The present invention relates to Atomic Layer Deposition (ALD) apparatus and loading methods.
Atomic Layer Epitaxy (ALE) method was invented by Dr. Tuomo Suntola in the early 1970's. Another generic name for the method is Atomic Layer Deposition (ALD) and it is nowadays used instead of ALE. ALD is a special chemical deposition method based on the sequential introduction of at least two reactive precursor species to a substrate that is located within a heated reaction space. The growth mechanism of ALD relies on the bond strength differences between chemical adsorption (chemisorption) and physical adsorption (physisorption). ALD utilizes chemisorption and eliminates physisorption during the deposition process. During chemisorption a strong chemical bond is formed between atom(s) of a solid phase surface and a molecule that is arriving from the gas phase. Bonding by physisorption is much weaker because only van der Waals forces are involved. Physisorption bonds are easily broken by thermal energy when the local temperature is above the condensation temperature of the molecules.
By definition the reaction space of an ALD reactor comprises all the heated surfaces that can be exposed alternately and sequentially to each of the ALD precursor used for the deposition of thin films. A basic ALD deposition cycle consists of four sequential steps: pulse A, purge A, pulse B and purge B. Pulse A typically consists of metal precursor vapor and pulse B of non-metal precursor vapor, especially nitrogen or oxygen precursor vapor. Inactive gas, such as nitrogen or argon, and a vacuum pump are used for purging gaseous reaction by-products and the residual gaseous reactant molecules from the reaction space during purge A and purge B. A deposition sequence comprises at least one deposition cycle. Deposition cycles are repeated until the deposition sequence has produced a thin film of desired thickness.
Precursor species form through chemisorption a chemical bond to reactive sites of the heated surfaces. Conditions are typically arranged in such a way that no more than a molecular monolayer of a solid material forms on the surfaces during one precursor pulse. The growth process is thus self-terminating or saturative. For example, the first precursor can include ligands that remain attached to the adsorbed species and saturate the surface, which prevents further chemisorption. Reaction space temperature is maintained above condensation temperatures and below thermal decomposition temperatures of the utilized precursors such that the precursor molecule species chemisorb on the substrate(s) essentially intact. Essentially intact means that volatile ligands may come off the precursor molecule when the precursor molecules species chemisorb on the surface. The surface becomes essentially saturated with the first type of reactive sites, i.e. adsorbed species of the first precursor molecules. This chemisorption step is typically followed by a first purge step (purge A) wherein the excess first precursor vapor and possible reaction by-product vapors are removed from the reaction space. Second precursor vapor is then introduced into the reaction space. Second precursor molecules typically react with the adsorbed species of the first precursor molecules, thereby forming the desired thin film material. This growth terminates once the entire amount of the adsorbed first precursor has been consumed and the surface has essentially been saturated with the second type of reactive sites. The excess of second precursor vapor and possible reaction by-product vapors are then removed by a second purge step (purge B). The cycle is then repeated until the film has grown to a desired thickness. Deposition cycles can also be more complex. For example, the cycles can include three or more reactant vapor pulses separated by purging steps. All these deposition cycles form a timed deposition sequence that is controlled by a logic unit or a microprocessor.
Thin films grown by ALD are dense, pinhole free and have uniform thickness. For example, aluminum oxide grown from trimethylaluminum (CH3)3Al, also referred to as TMA, and water at 250-300° C. has usually about 1% non-uniformity over the 100-200 mm wafer. Metal oxide thin films grown by ALD are suitable for gate dielectrics, electroluminescent display insulators, capacitor dielectrics and passivation layers. Metal nitride thin films grown by ALD are suitable for diffusion barriers, e.g., in dual damascene structures.
Precursors suitable for ALD processes in various ALD reactors are disclosed, for example, in review article R. Puurunen, “Surface chemistry of atomic layer deposition: A case study for the trimethylaluminum/water process”, J. Appl. Phys., 97 (2005), p. 121301, which is incorporated herein by reference.
In a typical reactor, ALD deposition cycles are applied to a single wafer or substrate. While this kind of single wafer processing may be satisfactory for an R&D purpose, it does not meet, e.g., the requirements of affordable mass production, such as the through-put of the product or mean time between service.
The patent application U.S. Ser. No. 12/154,879 filed on 27 May 2008 and assigned to the same assignee as the present application, the contents of which is incorporated herein by reference, presents a solution improving a through-put of an ALD reactor. In that solution a batch of substrates is loaded into a vertical flow reactor in a substrate holder, and the whole batch of substrates in the reactor is processed simultaneously to improve through-put. Although this presents a major step towards mass production compared to single substrate reactors, there is a need to improve the through-put even more.
According to a first aspect of the invention there is provided an atomic layer deposition (ALD) reactor system comprising:
a plurality of ALD reactors placed in a pattern in relation to each other, each ALD reactor being configured to receive a batch of substrates for ALD processing, each ALD reactor comprising a reaction chamber accessible from the top; and
a loading robot comprising a gripping part and a motion arrangement, the loading robot being configured to perform a plurality of loading sequences for loading each of said plurality of ALD reactors, each loading sequence comprising:
picking up with said gripping part a substrate holder carrying a batch of substrates in a storage area or shelf; and
moving with said moving arrangement said substrate holder with said batch of substrates into the reaction chamber of the ALD reactor in question.
In certain embodiments, said loading robot is in each loading sequence configured to lower said substrate holder vertically into a reaction chamber from the top without passing a separate loading chamber. The number of ALD reactors of the system may be two or three or more.
In certain embodiments, a pre-filled cassette of wafers is loaded and unloaded with the aid of a loading robot.
In certain embodiments, the substrates are semiconductor wafers, such as silicon wafers, for example 3-12″ wafers.
In certain embodiments, the substrates comprise 10-100000 pieces of three-dimensional parts such as 2-10 mm metal, glass or silica spheres, the substrates being in the pre-filled cassette during the loading sequence, the deposition process and the unloading sequence.
In certain embodiments, each ALD reactor comprises:
a lid-system comprising a reactor lid or vacuum chamber lid integrated with a reaction chamber lid; and
a lifting arrangement configured for lifting said lid-system up for loading the reaction chamber.
In certain embodiments, the ALD reactor system comprises a high efficiency particulate air filter hood, such as a HEPA filter hood, surrounding said plurality of ALD reactors, loading robot and storage area or shelf.
In certain embodiments, the loading robot is further configured to perform a plurality of unloading sequences for unloading each of said plurality of ALD reactors after ALD processing, each unloading sequence comprising:
picking up with said gripping part a substrate holder carrying a batch of ALD processed substrates from an ALD reactor in question; and
moving with said motion arrangement said substrate holder with the batch of ALD processed substrates to said storage area or shelf.
According to a second aspect of the invention there is provided a method comprising:
operating a plurality of ALD reactors placed in a pattern in relation to each other, each ALD reactor being configured to receive a batch of substrates for ALD processing, and each ALD reactor comprising a reaction chamber accessible from the top;
performing a plurality of loading sequences with a loading robot for loading each of said plurality of ALD reactors, each loading sequence comprising:
picking up a substrate holder carrying a batch of substrates in a storage area or shelf; and
moving said substrate holder with said batch of substrates into the reaction chamber of the ALD reactor in question.
In certain embodiments, in each loading sequence said substrate holder is lowered by said loading robot vertically into a reaction chamber from the top without passing a separate loading chamber.
In certain embodiments, the method comprises arranging a high efficiency particulate air filter hood, such as a HEPA filter hood, to surround said plurality of ALD reactors, loading robot and said storage area or shelf.
In certain embodiments, said loading sequences are performed by a single robot without human operator.
In certain embodiments, the method further comprises performing a plurality of unloading sequences with the loading robot for unloading each of said plurality of ALD reactors after ALD processing, each unloading sequence comprising:
picking up a substrate holder carrying a batch of ALD processed substrates from an ALD reactor in question; and
moving said substrate holder with the batch of ALD processed substrates to said storage area or shelf.
In all embodiments, it is not necessary to have a plurality of ALD reactors but a single ALD reactor will suffice in certain embodiments. Accordingly, yet another aspect of the invention provides an atomic layer deposition (ALD) reactor system comprising:
an ALD reactor configured to receive a batch of substrates for ALD processing, and comprising a reaction chamber accessible from the top; and
a loading robot comprising a gripping part and a motion arrangement, the loading robot being configured to perform a loading sequence for loading said ALD reactor, the loading sequence comprising:
picking up with said gripping part a substrate holder carrying a batch of substrates in a storage area or shelf; and
moving with said moving arrangement said substrate holder with said batch of substrates into the reaction chamber of the ALD reactor.
Advantages of certain aspects and/or embodiments of the invention involve improving through-put in ALD reactors, cost-efficiency, and reducing ALD reactor loading (and unloading) time.
Various exemplary embodiments of the present invention are illustrated hereinafter in the detailed description of the invention as well as in the dependent claims appended hereto. The embodiments are illustrated with reference to selected aspects of the invention. A person skilled in the art appreciates that any embodiment of the invention may be combined with other embodiment(s) within the same aspect. Furthermore, any embodiment may apply to other aspects as well either alone or in combination with other embodiment(s).
The basics of an ALD growth mechanism are known to a skilled person. Details of ALD methods have also been described in the introductory portion of this patent application. These details are not repeated here but a reference is made to the introductory portion with that respect.
The loading robot 110 is attached to the base 105 from the lower part 111a of arm 111 by bolts or other suitable attachment. The upper part 111b of arm 111 and other parts of the loading robot 110 attached thereto are rotatable in a horizontal plane as depicted by arrow 151. The arm 112 is attached to arm 111 by a joint and is rotatable around rotation axis A as depicted by arrow 152. The arm 113 is attached to arm 112 by a joint and is rotatable around rotation axis B as depicted by arrow 153. The arm 114 is attached to arm 113 by a joint and is rotatable around rotation axis C as depicted by arrow 154. The arm 114 is also rotatable around its own longitudinal axis as depicted by arrow 155.
The arm 114 shown in
The T-shaped structure may comprise, as shown in
The substrate holder 120 material typically comprises stainless steel, nickel, titanium, silicon carbide (e.g. SiC made from graphite by chemical vapor infiltration) or quartz. In an embodiment the substrate holder 120 is coated with an amorphous thin film (e.g. 100-200 nm of Al2O3) to protect the holder surface against corrosive source chemicals before taking the substrate holder in use.
The system shown in
In the example shown in
The loading robot 110 receives or grips a substrate holder 120 carrying a batch of substrates to be ALD processed in a loading station (loading space/storage area or rack/shelf, not shown). In practice, the loading robot 110 may grip the substrate holder 120 with its gripping part or arm 114 having the suitable protrusion(s) 225 or 325, or similar. The movement of the loading robot 110 is controlled by a computerized control system (not shown) thereby producing a motion arrangement for moving the substrate holder 120 with substrates 130. The loading robot 110 carries the substrate holder 120 with the batch of substrates 130 from the loading station towards the ALD reactor 481. In the close proximity of ALD reactor 481 the loading robot 110 moves the substrate holder 120 mainly in a horizontal direction above the aperture leading into the reaction chamber. Subsequently, the loading robot 110 lowers the substrate holder 120 with the batch of substrates 130 in a mainly vertical direction onto the bottom of the reaction chamber. Thereupon, the loading robot 110 releases its grip of the substrate holder 120 and moves the arm 114 away from the reactor. The reactor lid is lowered into a closed position by the lifting mechanism 470. The reaction chamber is evacuated from room pressure to vacuum. The process pressure is adjusted with flowing inactive gas such as nitrogen gas typically to about 1-10 hPa. The substrate temperature can be stabilized to process temperature (typically to about +80 . . . +500° C.) within the (hot wall) reaction chamber.
The first ALD reactor 481 performs ALD processing (comprising a desired amount of ALD deposition cycles) to the loaded batch of substrates 130. After ALD processing, the reaction chamber is vented to room pressure, the reactor lid is raised by the lifting mechanism 470 into the upper position, and the loading robot 110 unloads the substrate holder 120 with the ALD processed batch of substrates 130 from the ALD reactor. The loading robot 110 carries the substrate holder 120 with said batch of substrates 130 to an unloading station (which may be the same or different station as the loading station mentioned in the preceding). The loading and unloading operations can be performed by a single loading robot 110. Suitable electronics of the ALD reactor(s) and the loading robot communicate with each other for carrying out proper sequences of operations.
The loading and unloading of the system's second ALD and any further reactor are performed similarly. All ALD reactors can be loaded first before ALD processing is started in any of the ALD reactors. Alternatively, the loading robot 110 may load or unload certain ALD reactors while others are processing in accordance with an appropriate operating schedule.
In an embodiment, the storage area or rack 606 comprises a computer-controlled positioning table such as a slide table for setting substrate holder(s) to an optimum handling position for the loading robot.
In this embodiment, although also applicable in other embodiments, a high efficiency particulate air (HEPA) filter hood 690 is arranged to surround the ALD reactor system (reactors, loading robot and storage area or shelf) for preventing impurity particles from entering the reactors or substrate holder(s). In this way a local clean room can be created. In an embodiment, cleaned air is guided from hood ceiling towards the floor to form preferably laminar air flow. The local clean room can be constructed, for example, within a bigger room. The loading, ALD processing and unloading operations are performed within said local clean room by the loading robot and ALD reactor(s) without a human operator's residence in the local clean room.
Various embodiments have been presented. It should be appreciated that in this document, words comprise, include and contain are each used as open-ended expressions with no intended exclusivity.
The foregoing description has provided by way of non-limiting examples of particular implementations and embodiments of the invention a full and informative description of the best mode presently contemplated by the inventors for carrying out the invention. It is however clear to a person skilled in the art that the invention is not restricted to details of the embodiments presented above, but that it can be implemented in other embodiments using equivalent means without deviating from the characteristics of the invention.
Furthermore, some of the features of the above-disclosed embodiments of this invention may be used to advantage without the corresponding use of other features. As such, the foregoing description should be considered as merely illustrative of the principles of the present invention, and not in limitation thereof. Hence, the scope of the invention is only restricted by the appended patent claims.