This application is the U.S. National Phase of PCT Appln. No. PCT/EP2020/061882 filed Apr. 29, 2020, which claims priority to German Application No. 10 2019 207 772.2 filed May 28, 2019, the disclosures of which are incorporated in their entirety by reference herein.
The subject matter of the invention is a method for depositing an epitaxial layer on the front side of a wafer composed of monocrystalline material, this involving a provided wafer being arranged on a susceptor and being heated to a deposition temperature by means of thermal radiation and a deposition gas being conducted across a front side of the wafer. The subject matter of the invention is furthermore a device for depositing an epitaxial layer on a front side of a wafer composed of monocrystalline material.
The deposition of an epitaxial layer on the front side of a wafer is usually done by means of CVD (chemical vapour deposition) in a CVD reactor, often in a single-wafer reactor. Such a CVD reactor is described in US 2014/0 251 208 A1 for example. Provided in a single-wafer reactor between an upper and a lower dome is a reaction space in which a susceptor is held by susceptor support arms of a susceptor support shaft on susceptor support pins. The susceptor and a wafer rested on top is heated by means of thermal radiation by lamp arrays arranged above and below the domes, while a deposition gas is conducted across the front side of the wafer that is facing the upper dome.
US 2008/0118712 A1 describes a susceptor comprising a susceptor ring and a susceptor base. The susceptor ring has a ledge for resting a wafer in the edge region of the back side of the wafer. The susceptor ring is rested on the susceptor base in order to deposit a layer on the front side of the wafer.
US 2007/0227441 A1 refers to periodic variations in thickness in the edge region of epitaxially coated silicon wafers. This is because of the different growth rates with which the epitaxial layer grows. The different growth rates are linked to the crystal orientation of the front side of the wafer. The front side of the wafer is that face of the wafer on which the epitaxial layer is deposited. To homogenize the thickness of the epitaxial layer in the edge region, US 2007/0227441 A1 proposes that the structure of the susceptor be changed with the period of variations in thickness.
With the same goal, US 2015/0184314 A1 proposes limiting the width of the edge region of the wafer. This teaching takes no account of the fact that wafers in which the mentioned variations in thickness are regarded as problematic are provided with an orientation notch in the edge region. In the case of silicon wafers with <100> orientation of the front side, the orientation notch is usually situated on one of the four sites at which an epitaxial layer grows comparatively rapidly and marks one of four <110> crystal directions. Occasionally, the orientation notch is also situated 45° away from such a site and marks one of four <100> crystal directions.
It is an object of the present invention to improve the flatness of wafers having a deposited epitaxial layer in the edge region, especially in the region of the notch, and, at the same time, to reduce periodic variations in thickness in the edge region without having to change, to this end, the susceptor or the shape of the edge region of the wafer.
The object of the invention is achieved by the methods and devices described in the claims.
The features specified with regard to the above-mentioned embodiments of the method according to the invention can be applied mutatis mutandis to the device according to the invention. Conversely, the features specified with regard to the above-mentioned embodiments of the device according to the invention can be applied mutatis mutandis to the method according to the invention. These and other features of the embodiments according to the invention are elucidated in the description of the figures and in the claims. The individual features can be realized either separately or in combination as embodiments of the invention. Furthermore, they can describe advantageous designs which are independently protectable.
A device for depositing an epitaxial layer onto a front side of a wafer having an orientation notch contains a rotatable support shaft and susceptor support arms for holding and rotating a susceptor comprising a susceptor ring having a resting face for receiving the wafer and supporting the wafer in an edge region thereof. A ring held by the susceptor support arms lies below and spaced apart from the susceptor ring. This ring has azimuthal projections which reduce deposition along crystal orientations having increased deposition rates, resulting in wafers having improved thickness uniformities at these azimuthal positions.
A device (
Preferably, an inner edge (404, 504) of the projection (403, 503) of the ring (401, 501) is situated at a radial position, the distance of which in relation to a centre Z of the ring (401, 501) is not less than 140 mm, preferably not less than 145 mm and particularly preferably 148 mm to 150 mm.
In addition, a wafer (704, 804) can preferably be positioned in the susceptor ring (701, 801) such that the position with the greatest width of the resting face W1 (802) coincides with the position of the orientation notch (803).
In addition, the stepped boundary (
Preferably, the azimuthal position of an inwardly pointing bulge of the stepped boundary (902) adjacent to the rest is identical to the azimuthal position of the inwardly pointing projection of the resting face (403, 503).
To deposit an epitaxial layer on a front side of a wafer composed of monocrystalline material, the wafer is preferably arranged in the described device such that the orientation notch of the wafer has the same azimuthal position as a projection of the ring. Thereafter, the wafer is brought to a deposition temperature by means of thermal radiation which is directed towards a front side and towards a back side of the wafer and deposition gases are conducted across the front side of the wafer.
Said deposition gases preferably contain silanes, chlorosilanes or mixtures thereof, diluted in a carrier gas (preferably hydrogen).
What is understood by said deposition temperature is the temperature at which a layer is deposited on the wafer under the given boundary conditions.
The means of the described device ensure the selective reduction of the intensity of a portion of the thermal radiation which is directed towards the back side of the wafer, the result being that first subregions on the edge of the wafer, in which a growth rate of the epitaxial layer at uniform temperature of the wafer is greater because of the orientation of the monocrystalline material, are heated more weakly than in adjacent second subregions.
The above description of exemplary embodiments is to be understood exemplarily. The disclosure made thereby firstly enables a person skilled in the art to understand the present invention and the associated advantages and secondly encompasses alterations and modifications to the described structures and methods that are also obvious in the understanding of a person skilled in the art. Therefore, all such alterations and modifications and also equivalents are to be covered by the scope of protection of the claims.
Number | Date | Country | Kind |
---|---|---|---|
10 2019 207 772.2 | May 2019 | DE | national |
Filing Document | Filing Date | Country | Kind |
---|---|---|---|
PCT/EP2020/061882 | 4/29/2020 | WO |
Publishing Document | Publishing Date | Country | Kind |
---|---|---|---|
WO2020/239347 | 12/3/2020 | WO | A |
Number | Name | Date | Kind |
---|---|---|---|
9401271 | Pitney et al. | Jul 2016 | B2 |
20070026148 | Arai et al. | Feb 2007 | A1 |
20070227441 | Narahara et al. | Oct 2007 | A1 |
20080118712 | Schauer et al. | May 2008 | A1 |
20120270407 | Werner | Oct 2012 | A1 |
20140251208 | Samir et al. | Sep 2014 | A1 |
20140283748 | Higashi et al. | Sep 2014 | A1 |
20150184314 | Narahara et al. | Jul 2015 | A1 |
20170117228 | Schauer et al. | Apr 2017 | A1 |
20180002830 | Yudovsky et al. | Jan 2018 | A1 |
20200144035 | Wu et al. | May 2020 | A1 |
20200294794 | Haberecht et al. | Sep 2020 | A1 |
20200318234 | Haberecht | Oct 2020 | A1 |
20200365443 | Schauer | Nov 2020 | A1 |
20220267926 | Haberecht et al. | Aug 2022 | A1 |
Number | Date | Country |
---|---|---|
101111934 | Jan 2008 | CN |
205821452 | Dec 2016 | CN |
109451743 | Mar 2019 | CN |
213538160 | Jun 2021 | CN |
2004217809 | Aug 2004 | JP |
2005207997 | Aug 2005 | JP |
2007214531 | Aug 2007 | JP |
2009088088 | Apr 2009 | JP |
2014212244 | Nov 2014 | JP |
2015516685 | Jun 2015 | JP |
2017195301 | Oct 2017 | JP |
201715641 | May 2017 | TW |
201839187 | Nov 2018 | TW |
201906064 | Feb 2019 | TW |
2006068805 | Jun 2006 | WO |
2019110386 | Jun 2019 | WO |
Number | Date | Country | |
---|---|---|---|
20220267926 A1 | Aug 2022 | US |