STRESS-FREE LEAD FRAME

Abstract
The present invention relates to a stress-free lead frame (1) for a semiconductor. The stress-free lead frame (1) is provided with a stress-relief means (15) and an interlocking means (16) at the outer periphery. The stress-relief means (15) is capable of accommodating expansion and compression while the interlocking means (16) take care of shock and vibration during handling to thereby eliminate delamination of the lead frame (10).
Description
FIELD OF THE INVENTION

The present invention relates generally to a lead frame, especially to a stress-free lead frame for semiconductor provided with a stress-relief means and an interlocking means for eliminating delamination of leads during packaging.


BACKGROUND OF THE INVENTION

The process of manufacturing semiconductor devices involves several steps whereby an integrated circuit chip is bonded to a foil-type lead frame and encapsulated in epoxy or other moulded resin. The lead frame comprises of a plurality of leads etched or stamped out of a thin metallic foil sheet, and the inner ends of the leads are usually bonded to the solder bumps of the integrated circuit chip by a thermal compression method. The chip is then encapsulated in plastic by a transfer moulding process that results in a chip package having the outer ends of the leads expose to the outside for connection to a circuit board.


In a typical prior art system for bonding and encapsulating integrated circuits, a plurality of such circuits is linearly arranged in a single workpiece, which contains a series of identical lead frames etched or stamped on a strip of metallic substrate. A chip is bonded to each of the pre-manufactured lead frames and they are loaded to a bottom mould with the number of lead frames in a single batch being determined by the mould size and the capacity of the moulding equipment being used. A top mould is moved into place atop the bottom mould and some means is provided within the moulding equipment to heat the moulds to a proper moulding temperature, and to subsequently cool them for curing purposes. The heated moulds are clamped together by the moulding equipment and when the temperature is right, usually at approximately 175° C., the moulding material such as epoxy in pellet form is placed in the mould set through pots formed either in the top or bottom mould. Plungers are then inserted into the pots of the mould and a pressurizing force is applied to the plungers. The combination of the pressurizing force and the heat causes the epoxy pellets to liquify and flow into cavities provided in the mould set, which determines the configuration and the location of the moulded plastic that encapsulate the integrated circuits. Upon completion of this step, the mould set is cooled to induce curing to the epoxy, then the plungers are pulled from the mould set, the mould set is unclamped, and the top mould is lifted from the bottom mould. The lead frames are then removed from the bottom mould and the next station may be trimming, forming, sawing and otherwise operations on them to finish fabrication of the electronic circuit packages. Typically the outer leads of each package need to be bent (formed) to conform to requirements of the printed circuit board for which they are designed.


Delamination, that is separation of the metal lead frame from the moulded epoxy has been reported to happen during handling of the MLP. This is undesirable as it will cause damage and thus render the MLP a reject.


The moulding step also subjects the lead frame to tremendous structural stresses caused by the difference in expansion and compression of the moulded metallic foil that the lead frame and the unmoulded metallic foil that is its outer periphery. This causes bending, waving and twisting of the leads, resulting in delamination of the leads or separation of the metallic lead frame and the epoxy which will results in reliability failure of the package.


Therefore there exists a need for an improved lead frame design that may eliminate delamination problem as mentioned above.


BRIEF SUMMARY OF THE INVENTION

Accordingly, it is the primary object of the present invention to provide a stress-free lead frame having a stress-relief and an interlocking means for eliminating delamination of leads during packaging.


It is another object of the present invention to provide a stress-free lead frame having a stress-relief means that can be produced using existing moulding machine.


It is yet another object of the present invention to provide a stress-free lead frame having a stress-relief means that is of simple design for easy production.


These and other objects of the present invention are accomplished by,


A stress-free lead frame (1) comprising;


a plurality of integrated circuits areas (11), each of said plurality of integrated circuit areas having a die pad (12) and a plurality of leads (13); and


a peripheral pad (14) surrounding said plurality of integrated circuit areas,


said peripheral pad (14) being provided with a plurality of stress-relief means (15).




BRIEF DESCRIPTION OF THE DRAWINGS

Other aspect of the present invention and their advantages will be discerned after studying the Detailed Description in conjunction with the accompanying drawings in which:



FIG. 1 showing a lead frame of the prior art having a multiple integrated circuit units.



FIG. 2 showing a stress-free lead frame having a stress-relief means according to one embodiment of the present invention.




DETAILED DESCRIPTION OF THE INVENTION

Referring now to FIG. 1 showing a lead frame of the prior art having a multiple integrated circuit units. A lead frame (2) of the prior art consists of a plurality of integrated circuits (20), each having a die pad (21) and a plurality of leads (22) projecting outwardly from the die pad (21). The integrated circuits (20) are connected together by connecting bars (23). At the outer periphery of the lead frame (2), there is an inactive portion of the lead frame (2) called a peripheral pad (not shown). When the lead frame (2) is moulded to form the MLP, about half of the peripheral pad is left unmoulded causing different expansions and thus delamination to the plurality of leads (22) adjacent to the peripheral pad.


Referring to FIG. 2 showing a stress-free lead frame having a stress-relief means according to one embodiment of the present invention. The stress-free lead frame (1) comprises a lead frame (10) having a plurality of integrated circuit areas or integrated circuits (11) joined together by connecting bars (12). Each of the integrated circuits (11) has a plurality of die pads (not shown) and leads (not shown) projecting outwardly from the die pads. A peripheral pad (14) surrounds the lead frame (10).


The lead frame (10) is preferably of a metallic foil base, like copper or other suitable materials. The metallic foil is either etched or stamped to form the lead frame (10) that contain a plurality of integrated circuits (11). Each of the integrated circuit (11) has a die pad (not shown) for attaching a die and a plurality of leads (not shown) projecting away from the die pads. The lead frame (10) is surrounded by a peripheral pad (14) that is an inactive part of the metallic foil. The peripheral pad (14) is provided with a plurality of stress-relief means and a plurality of interlocking means in the form of holes and slots. Extensive research and experimentation has revealed that for best result, at least three rows of stress-relief means, a first row (15), a second row (17) and a third row (18), and a row of interlocking means (16) are needed. The first and the third row of the stress-relief means (15 and 18 respectively) are provided with slots while the second row (17) is provided with holes, preferably square hole. The holes and slots are arranged side by side in equal intervals for equal expansion and compression distribution. For the interlocking means (16), a plurality of slots are arranged at equal intervals in between the second and the third row of the stress-relief means (17 and 18 respectively).


During moulding, the lead frame (10) and the peripheral pad (14) containing the stress-relief means (15) and the interlocking means (16) is moulded to form the MLP. The heat produced during this process causes the leads to expand and to compress when cooled. In prior art practice, this produces delamination that causes many of the resulting integrated circuits a reject. However, the provision of the stress-relief means (15) can easily accommodate the expansion and compression of the leads. Further, the interlocking means (16) holds firmly the lead frame (10) to the moulded epoxy thus eliminating altogether delamination in the leads caused either by expansion and contraction of the metal lead frame or during handling of the MLP.


While the preferred embodiment of the present invention and their advantages have been disclosed in the above Detailed Description, the invention is not limited thereto but only by the spirit and scope of the appended claim.

Claims
  • 1. A method of manufacturing a plurality of integrated circuit packages, the method comprising: providing a lead frame strip comprising (i) an outer frame having a plurality of elongated openings regularly-spaced and arranged end to end around a circumference of an inner portion of the outer frame and a plurality of positioning holes along an outer portion of the outer frame, and (ii) a plurality of horizontal and vertical connecting bars attached to the outer frame and arranged in a manner that defines a plurality of inner frames arranged in a matrix pattern within the outer frame, each inner frame comprising a die pad and a plurality of leads arranged around the die pad; placing an integrated circuit die on each die pad, and for each integrated circuit die, electrically connecting the integrated circuit die to the plurality of leads surrounding its respective die pad; applying encapsulant material over the lead frame strip so that the plurality of inner frames including each integrated circuit placed on each die pad within the plurality of inner frames and the plurality of elongated openings are covered by the encapsulant material; severing individual integrated circuit packages from the lead frame strip to create the plurality of integrated circuit packages.
  • 2. The method of claim 1 wherein the plurality of elongated openings comprise a plurality of rows of elongated openings.
  • 3. A lead frame strip for use in making an integrated circuit die package, the lead frame strip comprising: a rectangular outer frame comprising four sides, a plurality of elongated openings arranged end-to-end along each of the four sides, and a plurality of positioning holes located on at least two of the four sides; and a plurality of inner frames arranged in a matrix pattern within the outer frame, each inner frame comprising connecting bars attached to the outer frame, a die pad and a plurality of tabs attached to the connecting bars, the plurality of tabs spaced apart from and arranged around the die pad, wherein the plurality of elongated openings do not extend along the inner frame connecting bars.
  • 4. The lead frame strip of claim 3 wherein the plurality of elongated openings includes a first plurality of elongated openings regularly spaced along rows on each of the four sides of the outer frame.
  • 5. The lead frame strip of claim 3 wherein the outer frame comprises a plurality of rows of elongated openings around the circumference of the outer frame.
  • 6. A lead frame strip for use in making an integrated circuit die package, the lead frame strip comprising: an outer frame, a plurality of regularly-spaced openings around the circumference of an inner portion of the outer frame outside of the plurality of connecting bars and a plurality of positioning holes along an outer portion of the outer frame; and a plurality of horizontal and vertical connecting bars attached to the outer frame and defining a plurality of inner frames arranged in a matrix pattern within the outer frame, each inner frame comprising a die pad and a plurality of tabs spaced apart from and arranged around the die pad, wherein the plurality of regularly-spaced openings do not extend along the horizontal or vertical connecting bars attached to the outer frame.
  • 7. The lead frame strip of claim 6 wherein the plurality of regularly spaced openings comprises a plurality of rows of elongated openings.
  • 8. The lead frame strip of claim 7 wherein the plurality of rows of openings comprises at least one row comprising a plurality of elongated openings.
  • 9. The lead frame strip of claim 7 wherein the plurality of regularly spaced openings further comprises a row comprising a plurality of non elongated holes.
Priority Claims (1)
Number Date Country Kind
PI 20004237 Sep 2000 MY national
CROSS-REFERENCES TO RELATED APPLICATIONS

This application is a division of U.S. application Ser. No. 11/022,071, filed Dec. 23, 2004; which is a continuation of U.S. application Ser. No. 09/909,934, filed Jul. 20, 2001, entitled “Stress-Free Lead Frame,” having Lee Kock Huat et al. listed as coinventors. The disclosures of 11/022,071 and 09/909,934 are herein incorporated herein by reference in their entirety.

Divisions (1)
Number Date Country
Parent 11022071 Dec 2004 US
Child 11868294 Oct 2007 US
Continuations (1)
Number Date Country
Parent 09909934 Jul 2001 US
Child 11022071 Dec 2004 US