The present disclosure describes semiconductor dies suitable for coupling to a printed circuit board using a solder ball, and to methods of manufacture thereof. More specifically, the disclosure relates to a via structure for the semiconductor dies.
The present disclosure claims priority to U.S. Patent Application Ser. No. 62/839,066 filed Apr. 26, 2019, which is incorporated by reference herein in its entirety.
Ball Grid Array (BGA) packages of semiconductor devices have become increasingly popular. In a Ball Grid Array, a grid array of solder balls is applied to a printed circuit board, and an integrated circuit can be mounted to the printed circuit board by means of the solder balls. A solder ball of a BGA is stressed through excessive temperature cycling (TC) due to a mismatch between material properties, such as the Coefficients of Thermal Expansion (CTE) of the silicon in the integrated circuit die and the printed circuit board substrate to which the solder ball is connected.
The following table gives typical values for the Young's modulus, for the Coefficient of Thermal Expansion (CTE), and for the Poisson's ratio, for silicon and for a printed circuit board (PCB).
The difference in material properties causes the materials to react differently under temperature cycling, which places stress on the solder ball connecting the two materials.
As a result of this stress, a prevalent failure mode on board level packages is an electronic failure, caused by cracking in the vicinity of a solder ball. For example, the temperature cycling may result in cracking in the bulk of a solder ball, or may cause delamination of one or more layer (for example a Back End of Line (BEOL) layer) within the integrated circuit.
The issue of reliability is made more relevant by the desire for a higher BGA pin count and smaller solder balls, and smaller gaps between solder balls.
According to some embodiments there is provided a semiconductor die for coupling to a printed circuit board using a solder ball. The semiconductor die comprises a redistribution layer formed above a semiconductor chip. The semiconductor die also comprises a polymer layer formed on the redistribution layer, wherein the polymer layer comprises a plurality of vias. The semiconductor die also comprises an Under Bump Metallurgy (UBM) layer formed on the polymer layer, wherein the plurality of vias electrically couple the UBM layer to the redistribution layer, and wherein the entire UBM layer is deposited with a continuously flat upper surface for coupling to the solder ball.
The plurality of vias may be positioned such that they are centered on a point not central to the UBM layer.
According to some embodiments there is provided a method of manufacturing a semiconductor die. The method comprises forming a polymer layer on a redistribution layer of a semiconductor die, and drilling the polymer layer to provide a plurality of vias through the polymer layer to the redistribution layer. The method further comprises depositing an Under Bump Metallurgy (UBM) layer onto the polymer layer such that the plurality of vias electrically couple the UBM layer to the redistribution layer, and the entire UBM layer is deposited with a continuously flat upper surface for coupling to the solder ball.
According to some embodiments there is provided a semiconductor die for coupling to a printed circuit board using a solder ball. The semiconductor die comprises a redistribution layer formed above a semiconductor chip, and a polymer layer formed on the redistribution layer. The polymer layer comprises a plurality of vias. The semiconductor die further comprises an Under Bump Metallurgy (UBM) layer formed on the polymer layer. The plurality of vias electrically couple the UBM layer to the redistribution layer, and the plurality of vias are positioned such that the plurality of vias are centered on a point not central to the UBM layer.
The UBM layer may be an entire UBM layer deposited with a continuously flat upper surface for coupling to the solder ball.
According to some embodiments there is provided a method of manufacturing a semiconductor die. The method comprises forming a polymer layer on a redistribution layer of a semiconductor die, and drilling the polymer layer to provide a plurality of vias through the polymer layer to the redistribution layer such that the plurality of vias are centered on a point not central to the UBM layer. The method further comprises depositing an Under Bump Metallurgy (UBM) layer on to the polymer layer such that the plurality of vias electrically couple the UBM layer to the redistribution layer.
For a better understanding of the embodiments of the present disclosure, and to show how it may be put into effect, reference will now be made, by way of example only, to the accompanying drawings, in which:
The description below sets forth example embodiments according to this disclosure. Further example embodiments and implementations will be apparent to those having ordinary skill in the art. Further, those having ordinary skill in the art will recognize that various equivalent techniques may be applied in lieu of, or in conjunction with, the embodiments discussed below, and all such equivalents should be deemed as being encompassed by the present disclosure.
The present disclosure relates to a semiconductor device, and in particular to a semiconductor device that is intended to be mounted to a printed circuit board, as part of an electronic device such as a laptop or tablet computer, a smartphone, a camera, a smart speaker, a games controller, or indeed any suitable device.
The integrated circuit die is coupled to the PCB 10 using an example ball grid array of solder balls 14.
As discussed above, the material used to make the printed circuit board and the semiconductor material have different material properties, and in particular have different coefficients of thermal expansion. One effect of this material difference is that, as the device is heated (for example by heat generated while the device is in operation) and cooled, the printed circuit board 10 and the semiconductor die 20 expand and contract by different amounts. The result of this differing amount is that the solder balls 14 of the ball grid array are subjected to stresses.
In general terms, solder balls near the corners of the ball grid array are typically under more stress than solder balls near the center of the ball grid array during temperature cycling (TC). This stress can eventually result in fatigue cracking.
The semiconductor die 12 comprises an Under Bump Metallurgy (UBM) layer 30, a PBO2 polymer layer 32, a redistribution layer (RDL) 34, a PBO1 polymer layer 36, and a Back End of Line (BEOL) stack-up portion 38, formed on the semiconductor (e.g. silicon) substrate 40.
It will be appreciated that the semiconductor die 12 will typically be connected to the printed circuit board by means of many such solder balls 14, and that the structure shown in
It will be noted that the UBM layer 30 is formed with a substantially continuously flat upper surface 42 for coupling to the solder ball 14.
A plurality of vias, for example made of copper, are formed through the polymer layer 32, in order to connect the UBM layer 30 to the RDL 34.
A plurality of vias 46a, 46b, 46c, 46d, 46e are formed through the polymer layer 32, and connect the UBM layer 30 to the RDL 34.
By way of example, in one illustrative embodiment, the UBM layer 30 has a thickness of 5.6 μm, and the vias 46a, 46b, 46c, 46d, 46e have a height of 9 μm and a width of 10 μm.
In another illustrative embodiment, the UBM layer 30 has a thickness of 1 μm, and the vias 46a, 46b, 46c, 46d, 46e have a height of 9 μm and a width of 10 μm.
In another illustrative embodiment, the UBM layer 30 has a thickness of 1 μm, and the vias 46a, 46b, 46c, 46d, 46e have a height of 12 μm and a width of 10 μm.
A method of manufacturing the semiconductor die illustrated in
The semiconductor die illustrated in
For example, structures such as that shown in
In addition, the depositing of the flat UBM pad also removes any requirement for the etching of the PBO2 layer 32 during manufacture.
In some embodiments, the vias are positioned such that they are centered on a point that is not central to the UBM layer.
Similar to the embodiment shown in
The semiconductor die 12 comprises an Under Bump Metallurgy (UBM) layer 50, a PBO2 polymer layer 52, a redistribution layer (RDL) 54, a PBO1 polymer layer 56, and a Back End of Line (BEOL) stack-up portion 58, formed on the semiconductor (e.g. silicon) substrate 60.
Again, it will be appreciated that the semiconductor die 12 will typically be connected to the printed circuit board by means of many such solder balls 14, and that a structure similar to that shown in
It will be noted that the UBM layer 50 is formed with a substantially continuously flat upper surface 62 for coupling to the solder ball 14.
A plurality of vias 66a, 66b, 66c, 66d, 66e, 66f, 66g, 66h, 66i, for example made of copper, are formed through the polymer layer 52, and connect the UBM layer 50 to the RDL 54.
A method of manufacturing the semiconductor die illustrated in
As described with reference to
In the embodiment shown in
Although
Specifically,
It was noted with reference to
The vias that extend through the polymer layer in order to electrically couple the UBM layer to the redistribution layer have the effect of reducing that stress and so, in some embodiments, when the plurality of vias are positioned such that they are centered on a point that is not central to the UBM layer, they are positioned such that they are centered at a point that is towards the corner of the ball grid array.
Thus, by way of an illustrative example only, and referring back to
The UBM region 72 shown in
Because the vias are on average positioned in the region of the semiconductor device that suffers from the highest stress, this positioning has the effect that the stress reduction effect of the vias is maximized.
This principle may be applied to as much of the ball grid array as required.
For example, a non-centered arrangement of vias may be used in connection with the solder balls in some or all of the corners of the ball grid array. As another example, the non-centered arrangement of vias may be used in connection with multiple solder balls in some or all of the corner regions of the ball grid array.
As another example, a non-centered arrangement of vias may be used in connection with one or more solder balls along one or more edge of the ball grid array. In this case, the plurality of vias may be positioned such that they are centered on a point that is not central to the UBM layer, but rather is offset towards the edge of the ball grid array.
For ease of illustration, the semiconductor device is not shown in as much detail as in
Specifically,
When the device is cooled back to its normal temperature, the vias 96 contract to their normal lengths, as shown by the arrow 100, and the UBM layer returns to its normal position 102, as shown in dashed lines.
There are two vias 116a, 116b through the UBM region 112. For example, each via may have a width of 10 μm. They are centered on a point that is not central to the UBM region 112, but rather is offset towards the corner of the package.
There are six vias 126a, 126b, 126c, 126d, 126e, 126f through the UBM region 122. For example, each via may have a width of 10 μm. They are centered on a point that is not central to the UBM region 122, but rather is offset towards the corner of the package.
There are nine vias 136a, 136b, 136c, 136d, 136e, 136f, 136g, 136h, 136i through the UBM region 132. For example, each via may have a width of 10 μm. They are centered on a point that is not central to the UBM region 132, but rather is offset towards the corner of the package.
Specifically,
The semiconductor die 152 comprises an Under Bump Metallurgy (UBM) layer 158, a PBO2 polymer layer 160, a redistribution layer (RDL) 162, and a PBO1 polymer layer 164, formed on the semiconductor (e.g. silicon) substrate 166 that includes the BEOL stack-up (not specifically shown in
It will be appreciated that the semiconductor die 152 will typically be connected to the printed circuit board 156 by means of many such solder balls 154, and that such a structure of UBM layer, RDL and associated components will be provided under each of those solder balls.
It will be noted that the UBM layer 158 is formed with a substantially continuously flat lower surface 168 for coupling to the solder ball 154.
The three vias 136f, 136d, 136e, shown in
As described previously, the structure illustrated in
Therefore, in embodiments described above, an Under-Bump-Via (UBV) structure with vias drilled through a polymer layer has been provided to connect a UBM layer to an RDL.
It should be understood—especially by those having ordinary skill in the art with the benefit of this disclosure—that the various operations described herein, particularly in connection with the figures, may be implemented by other circuitry or other hardware components. The order in which each operation of a given method is performed may be changed, and various elements of the systems illustrated herein may be added, reordered, combined, omitted, modified, etc. It is intended that this disclosure embrace all such modifications and changes and, accordingly, the above description should be regarded in an illustrative rather than a restrictive sense.
Similarly, although this disclosure makes reference to specific embodiments, certain modifications and changes can be made to those embodiments without departing from the scope and coverage of this disclosure. Moreover, any benefits, advantages, or solutions to problems that are described herein with regard to specific embodiments are not intended to be construed as a critical, required, or essential feature or element.
Further embodiments likewise, with the benefit of this disclosure, will be apparent to those having ordinary skill in the art, and such embodiments should be deemed as being encompassed herein.
It should be noted that the above-mentioned embodiments illustrate rather than limit the invention, and that those skilled in the art will be able to design many alternative embodiments without departing from the scope of the appended claims. The word “comprising” does not exclude the presence of elements or steps other than those listed in a claim, “a” or “an” does not exclude a plurality, and a single feature or other unit may fulfil the functions of several units recited in the claims. Any reference numerals or labels in the claims shall not be construed so as to limit their scope.
Number | Date | Country | |
---|---|---|---|
62839066 | Apr 2019 | US |