1. Field of Invention
The invention relates to a wafer level chip scale packaging structure and the method of fabricating the same. In particular, the invention relates to a wafer level chip scale packaging structure that uses a specially designed sacrificial layer material, interface crashes, or the elasticity of a suspension structure to remove the stress generated due to differential thermal expansion coefficients between the silicon (Si) wafer and the printed circuit board (PCB).
2. Related Art
The wafer level chip scale packaging is a very important technique for the packaging of wafers and PCB. The main difference from the conventional flip chip in package technique is: as the thermal expansion coefficients between the wafer (Si) and the PCB material is very large, it is likely to have some cracks at the solder ball joints during the reliability test after the wafer is assembled.
Therefore, one usually includes an underfill step in the technique of flip chip in package to protect the solder ball joint from being damaged. However, the underfill step is very time-consuming and it is very hard to repair once the process is completed. Therefore, the wafer level chip scale packaging is developed to replace the conventional flip chip in package technique. Since this kind of wafer level chip scale packaging techniques has superior electrical performance and lower manufacturing costs than other packaging forms and belongs to re-workable packaging techniques, it will play an important role in the production of future electronics.
We describe the developed wafer level chip scale packaging techniques in the following paragraphs.
In considering the reliability of the products, most packaging techniques can be applied to IC elements with a small pin number (smaller than 100 I/O ports) and area and cannot be used for future IC elements with a large pin number and area.
Therefore, for an optimized packaging (such as wafer level packaging) of future electronic devices that have a larger pin number, many functions, and a large chip size (such as system of single chip or system packaging), it is imperative to find a method to minimize the manufacturing cost and the packaging volume/surface.
In view of the foregoing, an objective of the invention is to provide a wafer level packaging structure and the method of fabricating it. The invention uses the usual semiconductor process to form a sacrificial layer below the bump using a normal semiconductor process. The bump is used to connect the signals between the Si wafer and the PCB. The interface between the sacrificial layer and the PCB or the sacrificial layer material is the weakest part in the whole structure. When the stress applied to the bump is overloaded, the interface between the sacrificial layer and the PCB or the sacrificial layer material will crash to remove the stress generated by different thermal expansion coefficients of the Si wafer and the PCB. The sacrificial layer can help avoid the crash occurring to the bump to protect the electrical conduction between the Si wafer and the PCB. The sacrificial layer can be removed to form a suspension part below the bump, the elasticity of which removes the stress generated by different thermal expansion coefficients of the Si wafer and the PCB.
The basic packaging structure of the invention includes: a substrate, an insulating layer, a metal wire, a bump, and a passivation layer. The substrate has electrical communications with the PCB via the bump.
The substrate part is the Si wafer. After forming the required circuit layout on the substrate using semiconductor processes, external signals can enter through the pads on its surface to control the actions of the substrate.
The insulating layer is formed on the substrate with a connection part and a suspension part. The connection part is directly connected to the substrate. The suspension part is suspended above the substrate and connected to the connection part.
Afterwards, the metal wire is pulled from the original pads to above the suspension part using the circuit redistribution layer technique. The bump is grown above the suspension part to electrically connect the pads and the bump. The substrate and the PCB thereabove are thus in electrical communications. Finally, a passivation layer is formed above the metal wire to protect the whole packaging structure from being damaged.
Since the wafer level packaging structure is fabricated using mature semiconductor processes, the structure and method can be used for mass production.
The invention will become more fully understood from the detailed description given hereinbelow illustration only, and thus are not limitative of the present invention, and wherein:
With reference to
The substrate 90 is usually a Si wafer. After forming the required circuit layout on the substrate 90 using semiconductor processes, external signals can enter through the pads 91 on its surface to control the actions of the substrate 90.
The insulating layer 100 is formed on the substrate 90 with a connection part 101 and a suspension part 102. The connection part 101 is directly formed on the substrate 90, exposing the surfaces of all the pads 91 for the connection of the metal wire 110. The suspension part 102 is suspended above the substrate 90 and connected to the connection part 101.
Since the pads 91 on the substrate 90 are formed using semiconductor processes, their pitch is very small. Although the same pitch can be fabricated on the PCB 130, it has a higher cost though.
To solve this problem, the redistribution layer (RDL) technique based upon the basic bump process is applied to wafers. Its primary objective is to widen the pitch on the PCB 130 through re-building the distribution of I/O ports (the bump 120 in the drawing). The ultimate goal is to reduce the fabrication cost of the PCB.
The metal wire 110 is pulled from the original pads 91 to above the suspension part 102 using the circuit RDL technique. The bump 120 is grown above the suspension part 102 to electrically connect the pads 91 and the bump 120. The substrate 90 and the PCB 130 thereabove are thus in electrical communications. Finally, a passivation layer 170 is formed above the metal wire 110 to protect the substrate 90 and the packaging structure from being damaged.
The invention uses the suspension part 102 as a protection pad (bump 120) design. When a stress is generated due to the different thermal expansion coefficients between the substrate 90 and the PCB 130, the tiny oscillations of the suspension 102 release such a stress. It prevents the cracks at the solder balls in the prior art. Therefore, the invention can protect the electrical connections between the pads 91 on the substrate 90 and the bump 120.
The connection part of the sacrificial layer 140 and the substrate 90 is weakest in the interfacial adhesive force or in the material of the complete structure. Therefore, when the stress on the bump 120 is too large, the connection part will break to release the stress between the substrate 90 and the PCB 130 while still keeping the electrical connection between the pads 91 on the substrate 90 and the bump 120.
The material of the sacrificial layer 140 can be metals, epoxy, organic polymers, inorganic oxides, etc, as long as the interfacial adhesive force with the substrate 90 or the sacrificial layer material has the weakest mechanical strength in the complete structure.
Likewise, the packaging structure in the third embodiment can have several suspension beams 111 (not shown) connecting to the bump 120. The suspension beams 111 are fabricated at the same time as the metal wire 110 (but without being connected to the pads 91) and installed above the insulating layer 100. They can further enhance the structural strength.
When the stress on the bump 120 is overloaded, it is absorbed by the elasticity of the elastic layer 150, protecting the electrical connection between the bump 120 and the pad 91. Likewise, the packaging structure in the fourth embodiment can be installed with several suspension beams 111 (not shown) connecting to the bump 120 to fortify the structural strength.
The substrate 90 contains pads 91 for external signals to enter and control the actions of the substrate 90.
The first insulating layer 103 is installed on the substrate 90 to expose all the pads 91. The second insulating layer 104 contains a first connection part 1041 and a second connection part 1042 connected with each other. The first connection part 1041 is installed on the first insulating layer 103. The second connection part 1042 is directly connected to the substrate 90. The adhesive force between the second connection part 1042 and the substrate 90 is smaller than that between the first connection part 1041 and the substrate 90. Therefore, when the stress between the substrate 90 and the PCB 130 is too large, the connection between the second connection part 1042 and the substrate 90 cracks to release the stress.
Likewise, there can be several suspension beams 111 (not shown) connecting to the bump 120 in the sixth embodiment to fortify the structural strength.
We use
As shown in
As shown in
As shown in
The fabricating method for the third embodiment is similar to the one for the first embodiment. One only needs to skip the step of removing the sacrificial layer 140 described in
Certain variations would be apparent to those skilled in the art, which variations are considered within the spirit and scope of the claimed invention.
Number | Date | Country | Kind |
---|---|---|---|
092131918 | Nov 2003 | TW | national |
Number | Date | Country | |
---|---|---|---|
Parent | 10765961 | Jan 2004 | US |
Child | 11152149 | Jun 2005 | US |