1. Field of the Invention
The invention in general relates to the packaging of electronic circuits, and particularly to those including MEMS devices.
2. Description of Related Art
A variety of MEMS (microelectromechanical systems) switches are in use, or proposed for use, in biomedical systems, in radar and communication systems, as well as other high frequency circuits for controlling RF signals. These MEMS switches are popular insofar as they can have a relatively high off impedance, with a low off capacitance, and a relatively low on impedance, with a high on capacitance, leading to desirable high cutoff frequencies and wide bandwidth operation. Additionally, the MEMS switches have a small footprint, can operate at high RF voltages and are compatible with conventional integrated circuit fabrication techniques.
For example, electronic circuits including MEMS switches are generally fabricated and tested on a large scale wafer which is subsequently cut up (diced) into individual circuits. These individual circuits are then packaged and placed into other systems.
Many of these MEMS switches generally have electrostatic elements, such as opposed electrodes, which are attracted to one another upon application of a pull down control voltage. At least one of these pull down electrodes is on the wafer and an opposing electrode is defined on the underside of a moveable bridge, or cantilever, above the wafer. Upon application of the pull down control voltage, the bridge, or cantilever is deflected down and the electrical impedance is severely reduced (either by capacitive coupling or by direct ohmic contact), between first and second spaced apart RF conductors on the wafer thus allowing a signal to propagate between the first and second RF conductors.
In view of the fact that these MEMS switches have electrically movable components, such as the bridge, it is imperative that movement of these components be completely unimpeded. However, after the fabrication process, in a wafer processing clean room, it is possible that unwanted debris blocks the normal movement of the bridge. This debris can occur particularly as a result of the dicing and packaging steps or in an application environment.
The MEMS device is not only sensitive to air borne particulates but also to moisture to which the MEMS device may be subject after it leaves the wafer processing clean room.
The present invention provides for a wafer scale packaging resulting in a hermetically sealed unit which eliminates the problems of conventional fabrication. In addition, the present invention is conducive to assembly under desired controlled ambient conditions.
A wafer scale package for electronic circuits is described and includes a base wafer having a plurality of locations each accommodating an electronic circuit, each circuit including at least one electronic device and associated signal lines. A cover wafer is provided having a corresponding like plurality of locations each including at least one cavity of sufficient size to accommodate the electronic device. Each location of the cover wafer includes a plurality of electrically conducting vias for establishing electrical continuity with the signal lines, at the bottom of the vias. A multilayer metallic seal surrounds each location to provide a peripheral hermetic seal and a multilayer metallic seal surrounds each bottom of the vias to provide a via hermetic seal. The peripheral hermetic seal is of sufficient width to enable dicing along the peripheral hermetic seal to form individual die packages, each containing a hermetically sealed electronic circuit.
Further scope of applicability of the present invention will become apparent from the detailed description provided hereinafter. It should be understood, however, that the detailed description and specific example, while disclosing the preferred embodiment of the invention, is provided by way of illustration only, since various changes and modifications within the spirit and scope of the invention will become apparent to those skilled in the art, from the detailed description.
The present invention will become more fully understood from the detailed description provided hereinafter and the accompanying drawings, which are not necessarily to scale, and are given by way of illustration only. In addition, the use of spatial terms such as top, bottom, above, below etc. is for ease of explanation and not as structural or orientation limitations.
Referring now to
In
A pad metalization 30 is deposited on base wafer 10 and makes electrical contact with line 24 and pad metalization 31 is deposited and makes electrical contact with line 25. Not seen in
Another metalization 34 straddles the juncture between adjacent locations 12, and completely surrounds the location. This will form part of a die package peripheral hermetic seal, when the assembly process (to be described) is completed. For ease of fabrication and to reduce processing costs, the pads 30, 31 and 32, and peripheral seal metalization 34 may be constituted of the same metal layers and may be applied in the same process step.
Extending from the top surface to the bottom surface of the wafer 14 are a plurality of vias 40 each having a metal deposition 42 on the inner wall thereof. A top via pad 44 and bottom via pad 45 are electrically integral with the via wall metal deposition 42. For RF applications, a ground plane 48 is provided on the top surface of the cover wafer 14 and surrounds the top via pads 44.
A cover peripheral seal includes metalization 50 which extends completely around the location 12 and is commensurate with peripheral seal metalization 34 on the base wafer 10. In addition, a via seal metalization 52 completely surrounds the bottom of each via 40, and is deposited over the bottom via pad 45. Again, for ease of fabrication and to reduce processing costs, the various metal layers in the peripheral seal 50 may be constituted of the same metal layers (to be described) in the bottom via pad 45 as well as the via seal metalization 52, and may be applied in the same process steps.
Potential contamination is an important consideration, particularly if the electronic device 22 has a moving part, such as in a MEMS switch. By way of example,
In
A moveable metallic bridge member in the form of cantilever 68 is electrically connected to one of the conductors, for example output conductor 63, and is positioned over input conductor 62. Cantilever 68 is provided with a voltage reference, for example DC ground, by a connection through output conductor 63.
When a DC pull down voltage is applied to pull down electrode 65, electrostatic attraction causes the cantilever to make contact either directly with input conductor 62, or with an oxide coating thereon, thus completing the RF circuit and allowing signal propagation. When the pull down voltage is removed, the cantilever resumes the position illustrated in
A bonding metal layer arrangement includes a layer 80 of titanium, a layer 81 of nickel, a layer 82 of indium and a layer 83 of gold. Deposited on the surface of base wafer 10 is a layer 84 of titanium, a layer 85 of nickel and a layer 86 of gold.
As previously stated, the via metal arrangement is formed simultaneously with the metal layer deposition of the peripheral seal. This ensures for planar alignment of the base and cover wafers. Accordingly, the bottom via pad 45 is comprised of metallic layers 78 and 79, the via seal 52 is comprised of metallic layers 80, 81, 82 and 83, and the pad metalization 30 is comprised of metallic layers 84, 85 and 86.
Typical thickness ranges for the metallic layers are as follows:
After the electronic circuit or circuits, along with associated signal lines have been deposited, and after the base and cover wafers 10 and 14 have been metalized, alignment and bonding apparatus is used to attach the base and cover wafers. This may be accomplished under a pressure of around 30 to 80 psi at a processing temperature of around 120° to 200° C. under vacuum or within an ambient atmosphere such as nitrogen, by way of example. The pressurization time is around 1 to 3 hours.
After the prescribed time, the bonding process is brought to atmospheric pressure and ambient temperature. The described selected metal layers and bonding process results in an exceptionally strong hermetic seal. Post fabrication analysis of the peripheral hermetic seal 53 reveals that the indium and nickel actually fuse together to form an indium-nickel alloy, lending strength to the seal, while the titanium promotes good adhesion to the quartz wafers.
The foregoing detailed description merely illustrates the principles of the invention. It will thus be appreciated that those skilled in the art will be able to devise various arrangements which, although not explicitly described or shown herein, embody the principles of the invention and are thus within its spirit and scope.
This application is a Division of U.S. Ser. No. 10/396,572, filed in the United States Patent and Trademark Office on Mar. 26, 2003 now U.S. Pat.No. 6,812,558, and is assigned to the same assignee as Ser. No. 10/396,572.
Number | Name | Date | Kind |
---|---|---|---|
5448014 | Kong et al. | Sep 1995 | A |
5668033 | Ohara et al. | Sep 1997 | A |
6383833 | Silverbrook | May 2002 | B1 |
6452238 | Orcutt et al. | Sep 2002 | B1 |
6479314 | Shibahara et al. | Nov 2002 | B2 |
6479320 | Gooch | Nov 2002 | B1 |
6559487 | Kang et al. | May 2003 | B1 |
6677187 | Salaville | Jan 2004 | B2 |
6777263 | Gan et al. | Aug 2004 | B1 |
6784020 | Lee et al. | Aug 2004 | B2 |
20020000646 | Gooch et al. | Jan 2002 | A1 |
20020179986 | Orcutt et al. | Dec 2002 | A1 |
20040077117 | Ding et al. | Apr 2004 | A1 |
Number | Date | Country | |
---|---|---|---|
20040191957 A1 | Sep 2004 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 10396572 | Mar 2003 | US |