2. Prior Art
The manufacturer of integrated circuits in the production of semiconductor devices is an evolving field. Their high demand in commerce has required greater speed in their manufacture and further necessitates improvements in environmental control during their manufacture
The current manufacturer of such semiconductor devices is initially accomplished by the deposition of solder at discreet points on a silicon wafer or base carrier. Such production methods to date, are very involved, utilizing complicated automatic manufacturing techniques. For example, U.S. Pat. No. 6,832,747 to Cordes et al, shows a process for utilizing hybrid molds for a molten solder screening process. This process developed a pyramidal shaped cavity for producing solder balls on a substrate.
A further example of the prior art, is shown in U.S. Pat. No. 6,708,872 to Gruber et al. This particular prior art shows a plurality of steps for applying a solder to a substrate, utilizing a variety of steps including alignment plates and associated procedures therewith which makes the process somewhat complicated.
It is an object of the present invention to overcome the disadvantages of the prior art.
It is a further object of the present invention, to provide a method and an apparatus for applying a solder to a substrate, in an environmentally safe arrangement not shown or suggested by the prior art.
It is yet a further object of the present invention, to minimize the number of steps by the apparatus utilized in the production of a silicon substrate having solder bumps thereon.
The present invention relates to method and apparatus for generating, depositing and forming an accurate array of solder bumps on a substrate such as a wafer of for example, silicon, or on a layer of plate glass. These solder bumps are utilized to form an array of electrical contacts on that substrate, wafer of plate, for subsequent use in the electronics industry.
The apparatus of the present invention comprises a solder-loading assembly consisting of a first or lower plate and a second or upper plate. The first or lower plate of the assembly may be movably supported on lower plate drive and the second or upper plate may be supported by an upper plate drive for compressably advancing the lower and upper plates toward and apart from one another. The lower plate arrangement of the assembly may be removably disposed within a liquid solder bath or received within a solder deposition application arrangement.
A mold plate or pattern plate is arranged in proper alignment on the first or lower plate during operation of the solder-loading assembly. The pattern plate has a plurality of properly aligned “through-holes” disposed thereon. The pattern plate is alignably disposed on the first or lower plate in the solder bath or solder-deposition arrangement so as to supply completely void-free molten solder in those through-holes thereon. The first or lower plate and the second or upper plate are then brought pressingly together facing one another with the now solder-filled pattern plate sandwiched therebetween. During this compression stage between the first or lower plate and the second or upper plate, the pattern plate is chilled through a temperature sufficient to solidify the solder in the through-holes in that pattern plate.
The now solidified solder in the now excess-solder-clear pattern plate is transferred to an awaiting substrate such as for example, a silicon wafer, or a plate glass substrate, in proper alignment therewith. The wafer or substrate to which the pattern plate is disposed, may be resting upon or in contact with a wafer supporting base with a heater and or chill means arranged therewithin. The wafer substrate and pattern plate may then be heated to a temperature above the melting point of the solder within the through-holes of the pattern plate. The now aligned through-holes adheringly deposit their bumps of solder onto the aligned wafer therebeneath or thereadjacent. The patterned plate is then removed from the wafer substrate with the solder bumps on their particular pads on the now cooled wafer or substrate therebeneath or thereadjacent. That substrate or wafer with the solder bumps thereon may now be removed from its chill plate base for subsequent further processing.
In a further embodiment of the present apparatus, the first or lower compression plate may have a slightly convex or cylindrically shaped uppermost surface thereon and the second or upper plate may have a corresponding cylindrically or a somewhat convex shaped surface thereon so as to provide a rollable or rockable “squeegee” effect to a pattern plate supportably compressed therebetween. Such a curved upper plate and correspondingly curved lower support plate could be articulated side-to-side to provide a squeezing and excess solder-removal action to a pattern plate with its associated through-holes with temporarily molten solder. Such excess solder removal would thus shorten the manufacturing process by combining several steps into one operation of filling those through-hole and cleaning the surface of the pattern plate almost simultaneously.
A further embodiment of the compression operation as applied to a pattern plate, comprises the advancement of a pattern plate with its respective aligned through-holes therewith being pulled preferably vertically, from a solder bath, while being rolled or “squeegeed” between a pair of compressive members. Such compressive members in a preferred embodiment thereof, would comprise a pair of biasedly-opposed rollers compressing and advancing a pattern plate therebetween, thus compressing each individual through-hole therebetween and simultaneously “squeegeeing” any access molten solder therefrom. Such compression and squeegeeing would thus foreshorten such a manufacturing method. The biasedly opposed pair of roller apparatus or squeegee members may be correspondingly chilled, so as to chill the molten solder in those through-holes in that particular pattern plate.
Such a pattern plate may have in one example, a straight through-bore or hole therethrough. In another further embodiment of that pattern plate, the through-hole may be tapered, so as to create a tapered or conical shape to a solder bump subsequently applied to a substrate.
In yet a further embodiment of the through-hole configuration in a pattern plate, a hemispherical depression is arranged on one side of the pattern plate, with a through-hole in the other side of that pattern plate in communication with the hemispherical depression. A yet further embodiment of the through-hole configuration for a pattern plate would be a hour-glass or pinched-waist configuration to the through-hole, wherein that pattern plate may be etched away on deposition of that pinched-waist configuration of solder applied to a wafer or substrate.
A still further configuration of that through-hole in a pattern plate may be a straight bore therethrough with a slot arrangement disposed on both the top side and the lower side of the patterned plate to provide a “keyway” effect therewithin.
Alignment of a patterned plate and a wafer or substrate in the prior art is often an operation which consumes time and expense. One such apparatus for minimizing the expense, the time and the possible inaccuracies associated therewith, would be to present an apparatus for supporting the patterned plate in a hinged-correspondence to a plate for supporting the wafer. Moving the support for the patterned plate and the wafer via a hinged support arrangement, to provide automatic and prompt alignment therebetween preceding a heating and chilling operation therewith for the deposition of those solder bumps onto that wafer is presented herewith.
The invention thus comprises a process for the manufacture of a wafer substrate for use in the semiconductor industry, comprising one or more of the following steps: arranging a first compressive member and a second compressive member in an opposed, compressibly displacable, spaced-apart relationship, with a pattern plate disposed therebetween, the pattern plate having a plurality of aligned through-holes arranged thereon; filling the through-holes with a molten solder; compressing the solder and the pattern plate between the first and the second opposed compressive members to compact the solder therein and cleans the pattern plate of excess solder; chilling the pattern plate to solidify the molten solder in the through-holes; and removing the pattern plate from the spaced-apart compressive members. The process may include placing the pattern plate on the wafer substrate in an aligned manner; heating the solder in the through-holes in the pattern plate to as to melt and cause adherence of the solder to the wafer as solder bumps thereon. The first compressive member and the second compressive member may have correspondingly curved facing surfaces to effect an excess solder removal operation during compression of the pattern plate therebetween. The compressive members may be plates. The curved facing surfaces of the compressive members may be of convex shape. The curved facing surfaces of the compressive members may be of slightly cylindrical shape. The compressing of the pattern plate may occur in a generally vertical orientation. The compressive members may be comprised of rotatable rollers. The through-holes may be straight bores arranged through the pattern plate. The through-holes may be openings having a hemispherical depression on one side of the plate in communication with a bore from the side of the pattern plate. The through-holes may be openings through the pattern plate having a pinched waist portion. The bores may have a slot arranged thereacross to define a keyway on at least one side of the pattern plate. The first compressive member and the second compressive member may be hinged together on a hinge pair member arrangement to provide pre-aligned mating of the pattern plate and the wafer/substrate. The compressive members may be supported by an articulable support to move the compressive members side to side with respect to one another and the pattern plate pinched therebetween. The process may include pivoting the pattern plate into mating alignment with the wafer/substrate for initiation of transfer of solder from the pattern plate to the wafer/substrate. The process may include applying an energy field to said pattern plate to facilitate void free production of solder bumps in said pattern plate.
The invention also comprises an apparatus for the manufacture of a wafer substrate for use in the semiconductor industry, comprising: a first compressive member and a second compressive member arranged in an opposed, compressibly displaceable, spaced-apart relationship; a heatable, chillable pattern plate disposed between the compressive members, the pattern plate having a plurality of aligned through-holes arranged thereon; and wherein the first compressive member and the second compressive member have correspondingly curved facing surfaces to effect an excess solder removal operation during compression of said pattern plate therebetween. An activatable energy generator may be arranged within or in communication with the pattern plate to help fill the through holes in the pattern plate with solder. The through-holes may be of non-cylindrical shape. The first and second compressive members may be rotatable rollers.
The objects and advantages of the present invention will become more apparent when viewed in conjunction with the following drawings, in which:
Referring now to the drawings in detail, and particularly to
The initial apparatus of the present invention, represented in
A mold plate or pattern plate 32 is arranged in proper alignment on the first or lower plate 22 during operation of the solder-loading assembly 20. The pattern plate 32 has a plurality of properly aligned “through-holes” 34 disposed thereon. The pattern plate 32 is disposed on the first or lower plate 22 in the solder bath 30 or solder-deposition arrangement so as to supply completely void-free molten solder 36 in those through-holes 34 thereon. The first or lower plate 22 and the second or upper plate 24 are then brought pressingly together facing one another with the now solder-filled pattern plate 32 sandwiched therebetween, as represented in
The now solidified, void-free solder 36 in the now excess-solder free pattern plate 32 is transferred to an awaiting substrate 40 such as a silicon wafer, or a plate glass substrate, in proper alignment therewith, as represented in
In a further embodiment of the assembly 20 of the present apparatus as shown in
A further embodiment of the assembly 20 utilized in the compression operation as applied to a pattern plate 32, is represented in
The particular through-holes 34 may nave various cross-sectional configurations to suit particular wafer requirements. Such a pattern plate 32 in one embodiment, may have a straight through-bore or hole 34 therethrough, as is represented in the sectional view shown in
In yet a further embodiment of the through-hole configuration in a pattern plate 32, as represented in
A still further configuration of that through-hole in a pattern plate 32 may be a straight bore 78 therethrough with a slot arrangement 80 disposed on both the top side and the lower side of the patterned plate to provide a “keyway” effect therewithin, as is represented in
Alignment of a pattern plate 32 and a wafer or substrate 40 in the prior art is often an operation which consumes time and expense. One such apparatus for minimizing the expense, the time and the possible inaccuracies associated therewith, would be to present an apparatus 90 for supporting the patterned plate 32 in a hinged-correspondence to a base 92 for supporting the wafer 40. Pivotably moving the support 91 for the pre-aligned pattern plate 32 and the pre-aligned wafer 40 on a hinged support arrangement 94, to provide automatic and prompt pivotable self-alignment therebetween, preceding a heating and chilling operation of the pattern plate 32 with its solder 36 filled through-holes 34 therewith for the ultimate deposition of those solder 36 as “bumps” onto that wafer 40 is presented herewith, in
1. Field of the Invention The present invention relates to method and apparatus for forming solder bumps on substrates such as silicon wafers for utilization in chip manufacturing in the electronics industry, and this application is a divisional application of our U.S. patent application Ser. No. 12/653,454, filed Dec. 14, 2009, now U.S. Pat. No. 7,982,320, which is a divisional of Ser. No. 11/482,838, filed Jul. 7, 2006, now U.S. Pat. No. 7,632,750, each of which are incorporated herein by reference in its entirety.
Number | Name | Date | Kind |
---|---|---|---|
6056191 | Brouillette et al. | May 2000 | A |
6123248 | Tadauchi et al. | Sep 2000 | A |
6276589 | Watts et al. | Aug 2001 | B1 |
6329608 | Rinne et al. | Dec 2001 | B1 |
6425518 | Gruber et al. | Jul 2002 | B1 |
6452117 | Curcio et al. | Sep 2002 | B2 |
6540129 | Lee | Apr 2003 | B2 |
6609652 | MacKay et al. | Aug 2003 | B2 |
Number | Date | Country | |
---|---|---|---|
20120289042 A1 | Nov 2012 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 12653454 | Dec 2009 | US |
Child | 13135970 | US | |
Parent | 11482838 | Jul 2006 | US |
Child | 12653454 | US |