The subject matter herein generally relates to printed circuit boards, in particular to a high-frequency circuit board and a method for manufacturing the same.
In high-frequency electronic signal transmissions, attenuation of the transmission signal is mainly a result of dielectric losses. Dielectric loss is positively correlated with dielectric loss factor and dielectric constant. In order to reduce the transmission loss, a liquid crystal polymer with a low dielectric constant can be used as the substrate layer covering the signal line. However, such material still has a relatively high dielectric loss.
Implementations of the present technology will now be described, by way of embodiment, with reference to the attached figures.
Implementations of the disclosure will now be described, by way of embodiments only, with reference to the drawings. The disclosure is illustrative only, and changes may be made in the detail within the principles of the present disclosure. It will, therefore, be appreciated that the embodiments may be modified within the scope of the claims.
Unless otherwise defined, all technical terms used herein have the same meaning as commonly understood by one of ordinary skill in the art. The technical terms used herein are to provide a thorough understanding of the embodiments described herein, but are not to be considered as limiting the scope of the embodiments.
The inner circuit board 10 is a single-sided circuit board, and includes a first substrate layer 11 and a first conductor layer 13 disposed on a surface of the first substrate layer 11.
As shown in
As shown in
The first substrate layer 11 may be a rigid resin layer, such as a prepreg (PP) layer including glass fiber and epoxy resin, or may be a flexible resin layer, such as a polyethylene naphthalate (PEN) layer, a polyimide (PI) layer, a polyethylene terephthalate (PET) layer, a polytetrafluoroethylene (Teflon) layer, a polythiamine (PA) layer, a poly methyl methacrylate (PMMA) layer, a polycarbonate (PC) layer, or a polyimide-polyethylene-terephthalate copolymer layer. In one embodiment, the first substrate layer 11 is made of a material having a dielectric constant of less than 3.5, such as polyethylene naphthalate.
The two outer circuit boards 30 are arranged at outer sides of the first substrate layer 11 and the first conductor layer 13. Each of the two outer circuit boards 30 includes a second substrate layer 31 and a second conductor layer 33. The second substrate layer 31 is in contact with the inner circuit board 10, and the second conductor layer 33 covers a surface of the second substrate layer 31 away from the inner circuit board 10.
As shown in
The second through holes 314 are not aligned with the first through holes 114, preventing copper foils of a copper laminate from collapsing during the pressing of the copper laminate on the inner circuit board 10. In one embodiment, in a thickness direction of the high-frequency circuit board 100, projections of the second through holes 314 and projections of the first through holes 114 alternate with each other.
The second substrate layer 31 may be a rigid resin layer or a flexible resin layer. The second substrate layer 31 and the first substrate layer 11 may be made of the same or different materials. In one embodiment, the second substrate layer 31 is made of a material having a dielectric constant of less than 3.5.
In an alternative embodiment, the high-frequency circuit board 100 further includes two adhesive layers 40. The two adhesive layers 40 attach the two outer circuit boards 30 to the inner circuit board 10. One adhesive layer 40 is sandwiched between the first substrate layer 11 and the second substrate layer 31 of one outer circuit board 30, and the other adhesive layer 40 is sandwiched between the first conductor layer 13 and the second substrate layer 31 of the other outer circuit board 30. Each of the adhesive layers 40 defines an opening 41. In the width direction of the high-frequency circuit board 100, a width of the opening 41 is greater than the width of the signal line 131 and is less than a straight-line distance between the two ground lines 132. The signal line 131 is in the opening 41 of one adhesive layer 40, and the adhesive layer 40 partially infills the slots 134.
The second conductor layers 33 function as shielding layers of the signal line 131. The high-frequency circuit board 100 further includes a plurality of conductive pillars 60 on both sides of signal line 131. The conductive pillars 60 are electrically connected to the second conductor layers 33 and the ground lines 132. The conductive pillars 60, the second conductor layers 33, and the ground lines 132 surround the signal line 131 and together act as a shield preventing electromagnetic interference from the environment in the signal line 131. Some conductive pillars 60 located on one side of the signal line 131 are arranged at equal or non-equal distances along the length direction of the signal line 131. In one embodiment, each of the conductive pillars 60 penetrates the first substrate layer 11, two adhesive layers, and two second substrate layers 31, and is electrically connected to one ground line 132 and two second conductor layers 33.
The high-frequency circuit board 100 further includes two protective layers 70. The two protective layers 70 are arranged on two outer sides of the two outer circuit boards 30, and protect the second conductor layers 33. In one embodiment, the protective layers 70 are covering layers. In other embodiment, the protective layers 70 may be solder resisting layers. The two protective layers 70 may be attached to the outer sides of the two outer circuit boards 30 by adhesive layers 40.
One embodiment of a method for manufacturing a high-frequency circuit board includes the steps of:
S1, providing an inner circuit board including a first substrate layer and a first conductor layer on a surface of the first substrate layer, the first conductor layer including a signal line and two ground lines arranged at intervals on both sides of the signal line, and the first substrate layer having a plurality of first through holes corresponding to the signal line;
S2, providing two copper clad laminates, each of the two copper clad laminates including a second substrate layer and a copper foil on a surface of the second substrate layer, the second substrate layer having a plurality of second through holes;
S3, pressing together the two copper clad laminates on two sides of the inner circuit board, the second substrate layer abutting the inner circuit board, and the second through holes non-aligned with the first through holes;
S4, forming a second conductor layer on the copper foil to obtain the high-frequency circuit board.
As shown in
The first conductor layer 13 is made of copper, and includes a signal line 131 and two ground lines 132. The first conductor layer 13 defines slots 134 passing through the first conductor layer 13. Each slot 134 isolates one ground line 132 from the signal line 131. The first substrate layer 11 covers one side of the first conductor layer 13.
The substrate layer 11 includes a first opening region 111 and a first non-opening region 113 connected to each other. The first opening region 111 corresponds in position to the signal line 131. In a width direction W of the high-frequency circuit board 100, a width of the first opening region 111 is not greater than a width of the signal line 131. The first opening region 111 defines first through holes 114, and the signal line 131 is exposed in the first through holes 114. Each of the first through holes 114 penetrates a surface of the first substrate layer 11 abutting the first conductor layer 13 and a surface of the first substrate layer 11 away from the first conductor layer 13. A cross-section of each of the first through holes 114 may be round, slot-like, or the like. The first through holes 114 are arranged at intervals along a length direction of the signal line 131. The first through holes 114 may be formed by laser cutting or punching.
The first substrate layer 11 may be a rigid resin layer, such as a prepreg (PP) layer including glass fiber and epoxy resin, or may be a flexible resin layer, such as a polyethylene naphthalate (PEN) layer, a polyimide (PI) layer, a polyethylene terephthalate (PET) layer, a polytetrafluoroethylene (Teflon) layer, a polythiamine (PA) layer, a poly methyl methacrylate (PMMA) layer, a polycarbonate (PC) layer, or a polyimide-polyethylene-terephthalate copolymer layer. In one embodiment, the first substrate layer 11 is made of a material having a dielectric constant of less than 3.5, such as polyethylene naphthalate.
As shown in
The second substrate layer 31 includes a second opening region 311 and a second non-opening region 313 connected to each other. The second opening region 311 corresponds in position to the signal line 131. In the width direction W of the high-frequency circuit board 100, a width of the second opening region 311 is not less than the width of the signal line 131. The second opening region 311 defines second through holes 314. The second through holes 314 may be formed by laser cutting or punching.
The second substrate layer 31 may be a rigid resin layer or a flexible resin layer. The second substrate layer 31 and the first substrate layer 11 may be made of the same or different materials. In one embodiment, the second substrate layer 31 is made of a material having a dielectric constant of less than 3.5.
As shown in
In an alternative embodiment, the two copper clad laminates 80 are adhered to two sides of the inner circuit board 10 by adhesive layers 40. One adhesive layer 40 is sandwiched between the first substrate layer 11 and the second substrate layer 31 of one outer circuit board 30, and the other adhesive layer 40 is sandwiched between the first conductor layer 13 and the second substrate layer 31 of the other outer circuit board 30. The adhesive layers 40 may be prepregs. Each of the adhesive layers 40 defines an opening 41. In the width direction of the high-frequency circuit board 100, a width of the opening 41 is greater than the width of the signal line 131 but less than a straight-line distance between the two ground lines 132. After being pressed together, the signal line 131 is in the opening 41 of one adhesive layer 40, and the adhesive layer 40 partially infills the slots 134.
As shown in
Specifically, each of the conductive pillars 60 is formed by forming a via 61 on the first substrate 11, the two adhesive layers 40, and the two substrate layers 31, the ground line 132 being exposed in the via 61. The via 61 is infilled or electroplated with conductive materials to form the conductive pillar 60.
As shown in
After forming the second conductor layers 33, the method further includes the step of forming two protective layers 70 on two outer sides of the two outer circuit boards 30. The protective layers 70 protect the second conductor layers 33. In one embodiment, the protective layers 70 are covering layers. In other embodiment, the protective layers 70 may be solder resisting layers. The two protective layers 70 may be attached to the outer sides of the two outer circuit boards 30 by two adhesive layers 40.
In the high-frequency circuit board 100, the first substrate layer 11 of the inner circuit board 10 and the second substrate layers 31 of the outer circuit boards 30 all define through holes corresponding to the signal line 131. The signal line 131 is at least in part surrounded by air, air having a very low dielectric constant, attenuation of the signal line 131 during transmission is thereby reduced. The second through holes 314 are non-aligned with the first through holes 114, so as to prevent the copper foils 81 of the copper laminates 80 from collapsing during the pressing together of the copper laminates 80 on the inner circuit board 10.
While the present disclosure has been described with reference to particular embodiments, the description is illustrative of the disclosure and is not to be construed as limiting the disclosure. Therefore, those of ordinary skill in the art can make various modifications to the embodiments without departing from the scope of the disclosure as defined by the appended claims.
Number | Date | Country | Kind |
---|---|---|---|
202010494280.1 | Jun 2020 | CN | national |
Number | Name | Date | Kind |
---|---|---|---|
9485859 | Hu | Nov 2016 | B1 |
10820457 | Kishi | Oct 2020 | B1 |
20030116343 | Adachi | Jun 2003 | A1 |
20030173633 | Barnes | Sep 2003 | A1 |
20030173640 | Ando | Sep 2003 | A1 |
20040263290 | Sherrer | Dec 2004 | A1 |
20060164190 | Sherrer | Jul 2006 | A1 |
20100052993 | Kim | Mar 2010 | A1 |
20140266515 | Sherrer | Sep 2014 | A1 |
20160381786 | Hu | Dec 2016 | A1 |
20170188451 | Hu | Jun 2017 | A1 |
20200037439 | Kim | Jan 2020 | A1 |