This invention relates to systems and methods that destroy active species of pre-cursor gases used in atomic layer deposition (ALD). More particularly, this invention relates to systems and methods that destroy active species of pre-cursor gases inside the reactor in which the ALD occurs.
ALD is a process in which atoms are deposited on a substrate, monolayer at a time, to grow a multi-layered thin film. In typical ALD processes, a first pre-cursor gas enters a reactor in which a substrate is placed. The first pre-cursor gas saturates the surface of the substrate forming a first monolayer. The reactor is then typically purged with an inert gas. Purging is required to prevent parasitic chemical vapor deposition (CVD) reactions from occurring between the first pre-cursor gas and a second pre-cursor gas that enters the chamber after purging. If most of the pre-cursor gas is not purged from the chamber, these reactions can form particles that will either ruin the thin film being grown, result in an undesired CVD-type deposition, or both. Problems associated with CVD-type deposition include poor step coverage and poor uniformity.
After the first pre-cursor gas is purged, a second pre-cursor gas enters the reactor and reacts with the adsorbed monolayer or partial monolayer (i.e., the first monolayer) to form a monolayer of the desired film. The reactor is again purged with an inert gas. This process is repeated until the thin film is grown to a desired thickness.
In some ALD reactions, one of the pre-cursors may include an active species. An active species is a molecule that is not in its most stable state. Active species will readily react to either accept or donate electrons in a reaction (e.g., O3, O*, or N* (where * denotes an excited state with excess energy)). Because most active species readily decay or recombine into a more stable state as temperature increases, they have a relatively short half-life in an ALD chamber operating at temperatures in excess of 400° C. However, in some cases, it may be advantageous to grow a film via ALD at lower temperatures such as 200° C. In this situation, the half-life of the active species is increased, and for a given purge time, there is a higher initial concentration of active species present to be purged from the reactor. This directly reduces the throughput of the reactor.
Variables that can affect the half-life of active species of gases include temperature and pressure. As temperature and pressure increase, the half-life of the active species decreases because of simple kinetics. Destruction of the active species is necessary because of their high reactivity. For example, an active species such as ozone can irritate the eyes and lungs, and so should be completely converted into O2 before being discharged to the atmosphere. ALD processes that require the use of an active species typically run at temperatures high enough to destroy (e.g., consume or decompose) most of the active species before they leave the chamber. This reduces the concentration level of the active species significantly.
However, current experience with ALD processes indicates that it may be advantageous to operate at temperatures lower than the high temperatures of many known ALD processes. For example, many of the metal-organic pre-cursors that may be used in the ALD of hafnium (Hf) oxide decompose at temperatures higher than 200° C. Therefore, in order to obtain a film with acceptable properties (e.g., step coverage, low carbon content) the reactor must be operated at a temperature close to or lower than 200° C. When ozone is used as an oxidizer in this process, these lower temperatures are not sufficient to decompose all of the ozone before it leaves the reactor.
For example, in the ALD of hafnium oxide, if ozone is supplied to a reactor and the chamber is running at 400° C., a certain percentage of the ozone, X, will be consumed by the reaction with the Hf pre-cursor and another percentage, Y, will be consumed by kinetic recombination of the O3 and O* to form O2. This kinetic recombination reaction is driven by temperature. The overall percentage of ozone remaining in the chamber will be Z. However, if the chamber is running at 200° C., the percentage of ozone that recombines will be far less than Y. Thus, the amount remaining to be purged will be greater than Z. This requires a longer purge time.
In view of the foregoing, it would be desirable to decrease the purge time of active species of pre-cursor gases from reactors used in ALD to improve throughput.
It is an object of this invention to decrease the purge time of active species of pre-cursor gases from reactors used in ALD to improve throughput.
Some active species of pre-cursor gases that do not readily decay at typical ALD reaction temperatures are known to readily decay at temperatures higher than the ALD reaction temperatures. For example, when aluminum oxide is deposited using trimethylaluminum (TMA) and ozone (ozone includes O3, O2, and O*), the active species of the ozone (i.e., O3 and O*) do not readily decay at the typical reaction temperature of about 300° C. That is, a large percentage of the active species remains active. In other words, a large concentration of the active species remains in the reactor. This hinders the throughput of the reactor. However, at higher temperatures (e.g., at temperatures equal to or greater than 400° C.) the active species of the ozone readily break down.
There are three ways to decrease the concentration of an active species in the reactor: i) consume more O3 in the surface reaction to grow film (in ALD this is limited because only one monolayer is grown at a time); ii) increase the temperature to destroy more active species via a kinetic recombination reaction; iii) purge for a longer time. The addition of a high temperature surface beyond the wafer but before the outlet will destroy more active species. This will drop the concentration of the active species to one that can be reduced more readily with a shorter purge time.
In accordance with this invention, a high-temperature surface is placed inside the reactor to significantly speed the decay of the active species and thus increase the throughput of the reactor. The high-temperature surface preferably has a high surface area. The high-temperature surface is preferably a metal, other material, or combination thereof that can be heated to a temperature high enough to induce the rapid decay of the active species of a pre-cursor gas used in ALD. The high-temperature surface may also include a material that catalyzes the active species to further increase the rate of decay. Alternatively, the surface may be coated with a catalyst. In the case of ozone as an active species, the high-temperature surface is preferably heatable to about 400° C. or higher.
The high-temperature surface is preferably placed inside the reactor downstream (with respect to the flow of gas) from the gas input and the substrate and upstream from the gas output. The high-temperature surface is preferably placed inside the reactor such that the temperature of the substrate is not substantially affected by the high-temperature surface. As the active species of a pre-cursor gas are purged, they are “de-activated” (i.e., destroyed) as they pass over the high-temperature surface.
Advantageously, more than one high-temperature surface may be placed inside the reactor according to the invention. In addition, the high-temperature surface or surfaces can be of various shapes. For example, the surface or surfaces may be a group of fins, a ring, a perforated plate, an ordered mesh of metal or other material, or a random mesh of metal or other material. The high-temperature surface is preferably shaped and situated inside the reactor such that the flow of gas through the reactor is not substantially impeded.
Advantageously, thin films may be grown on multiple substrates simultaneously according to the invention.
The above and other objects and advantages of the invention will be apparent upon consideration of the following detailed description, taken in conjunction with the accompanying drawings, in which like reference characters refer to like parts throughout, and in which:
Atomic layer deposition (ALD) processes are used to grow multi-layered thin films for use in a variety of semiconductor fabrication applications. Such applications include DRAMs, SiO2 dielectrics, and gate dielectrics. In typical ALD processes, pre-cursor gases enter a reactor one at a time via one or more gas inputs. Pre-cursor gases used in ALD are often chosen for their self-regulation properties with respect to growth. In some ALD systems, one of the pre-cursors is or includes an active species. For example, in a system to grow aluminum oxide, pre-cursors of trimethylaluminum (TMA) and ozone (ozone includes O3, O2, and O*) are alternately entered into a chamber. Ozone includes the active species O3 and O*.
When a pre-cursor gas reacts with a substrate inside the reactor, a portion of the pre-cursor gas saturates the substrate forming a monolayer of atoms on the substrate. After the pre-cursor gas reacts with the substrate, the pre-cursor and active species (if any) are purged out of the reactor. This is done by either pulling a vacuum on one or more gas outputs of the reactor, forcing an inert gas (e.g., argon) through the reactor, or both.
After the first monolayer is deposited and the first pre-cursor purged, a second pre-cursor gas enters the reactor. This second pre-cursor reacts with the deposited portion of the first pre-cursor gas (i.e., grows on top of the deposited portion of the first pre-cursor gas). The remaining pre-cursor gas and active species (if any) of the second pre-cursor gas are then purged from the reactor. This process is repeated until the film is grown to the desired thickness.
Inside reactor 100 is one or more heaters 140. Heater 140 is supported by heater column 144 and heater support 146. Substrate 130 rests on and is substantially flush with surface 142 of heater 140. Surface 142 should be heated to a temperature suitable for the ALD of the film being grown. That is, surface 142 should be at a temperature that causes a pre-cursor gas to react with the substrate. Substrate 130 may rest on surface 142 simply due to gravity or be held under a vacuum or by mechanical means, or any combination thereof. The surface of substrate 130 with which the pre-cursor gases react does not have to face upward or towards the gas input (however, it should not face down on surface 142). Alternatively, substrate 130 can be placed near heater 140, instead of on it.
Surface 142 is preferably larger in both length and width than the largest substrate to be placed on surface 142. Surface 142 and heater column 144 are preferably cylindrical. This allows gas to pass over substrate 130 and through reactor 100 more rapidly as compared to surfaces and columns of other shapes. However, surface 142 and heater column 144 can still be of other shapes such as square, hexagonal, or octagonal.
When growing ALD films, pre-cursor gases and their active species should be purged from the reactor as quickly as possible after the pre-cursor gases react with the substrate. When mass producing ALD films, purge time becomes an important factor in the number of films that can be produced in a given time.
Purging of active species may be difficult when they do not quickly decay into non-active species. This decreases the throughput of the reactor and the overall ALD process time. Non-active species are more readily purgeable because they are more stable and less reactive than active species.
To decrease the purge time of active species used in ALD, which are often temperature sensitive, a high-temperature surface is placed in the reactor in accordance with the invention. The high-temperature surface decreases the half-life of the active species and thus decreases purge time. For ALD reactions using, for example, trimethylaluminum (TMA) and ozone as the pre-cursor gases, the active species of ozone (O3 and O*) usually limit how fast the ALD reactions can be completed. At 250° C. (and 1 Torr) the half-life of ozone is about 76 seconds. The half-life drops to about 0.75 seconds at 400° C. (and 1 Torr), and to about 0.02 seconds at 600° C. (and 1 Torr).
The high-temperature surface is preferably positioned inside the reactor such that the pre-cursor gases react with the substrate before coming in the vicinity of, or in contact with, the high-temperature surface. In other words, the high-temperature surface is preferably downstream from the heater surface and substrate and upstream from the gas output. As the active species of a pre-cursor gas are purged, they are de-activated or “destroyed” (i.e., their reactivity is destroyed) as they pass over the high-temperature surface.
The reactors of
Furthermore, although the embodiments of
For example,
Inside reactor 900 is high temperature surface 980, which is a perforated plate with openings 982. Surface 980 is heated to a temperature high enough to destroy the active species of pre-cursor gases used in ALD processes.
Inside reactor 1100 are two substrates 1130 fixed to two respective heating surfaces 1140. Substrates 1130 may be held to heaters 1140 by, for example, vacuum. The surface of each substrate 1130 on which a film is to be grown preferably faces the center of reactor 1100. This ensures that substantially uniform monolayers of atoms are deposited on the substrate. A high-temperature surface 1180 is downstream (with respect to the flow of gas) from substrates 1130 and heaters 1140. Surface 1180 is heated to a temperature high enough to destroy the active species of pre-cursor gases used in ALD processes.
The reactors of the invention can be of any type suitable for ALD including depression reactors and barrel reactors.
High-temperature surfaces such as surfaces 280, 380, 480, 580, 680, 780, 980, 1080, 1180, and 1280 may be heated by, for example, an electrical power source external to the reactor in which the surface is located. High-temperature surfaces may also be heated by, for example, heat convection.
The above embodiments destroy active species of pre-cursor gases insitu by subjecting them to a high-temperature surface in the same reactor in which the ALD process occurs. In those ALD processes in which active species of pre-cursor gases can be destroyed by subjecting them to a cold-temperature surface, a cold-temperature surface may be alternatively placed inside the reactor. The cold-temperature surface may be the same shape as any of high-temperature surfaces 280, 380, 480, 580, 680, 780, 980, 1080, 1180, or 1280. The cold-temperature surface can be at any temperature below the reaction temperature of the ALD process that induces rapid decay of active species. For example, the cold-temperature surface can be about 100° C., room temperature, freezing, or below freezing, depending on the active species to be destroyed.
Note that although semiconductor substrates have been described herein with respect to ALD, the invention is not limited to them. Other workpieces appropriate for ALD are also within the scope of the invention.
In addition, although the ALD processes described herein have been described using only two pre-cursor gases, the invention is not limited to two pre-cursor gases. For example, three or four pre-cursor gases may be used.
Thus it is seen that systems and methods of insitu post atomic layer deposition destruction of active species are provided. One skilled in the art will appreciate that the invention can be practiced by other than the described embodiments, which are presented for purposes of illustration and not of limitation, and the invention is limited only by the claims which follow.
Number | Name | Date | Kind |
---|---|---|---|
6015590 | Suntola et al. | Jan 2000 | A |
6042652 | Hyun et al. | Mar 2000 | A |
6143659 | Leem | Nov 2000 | A |
6174377 | Doering et al. | Jan 2001 | B1 |
6174809 | Kang et al. | Jan 2001 | B1 |
6305314 | Sneh et al. | Oct 2001 | B1 |
6506352 | Lindfors et al. | Jan 2003 | B1 |
20020187084 | Lindfors et al. | Dec 2002 | A1 |
20030082296 | Elers et al. | May 2003 | A1 |
20030180458 | Sneh | Sep 2003 | A1 |
Number | Date | Country | |
---|---|---|---|
20040152304 A1 | Aug 2004 | US |