This invention relates in general to an improved system and method for atomic layer deposition (“ALD” hereafter). In particular, the invention relates to a new method and system for ALD deposition processing and manufacture of end product by using self-limiting reaction condition to avoid need of enclosures and purge areas for separation of two or more reacting gases. Consequently, there is no need for dosing valves since precursor flows continuously, and there is 100% material utilization as part of the subject ALD method. Further, a low vapor pressure precursor can be used with a fast moving conveyance system; and there is no need for isolation of different reaction zones nor for use of system components having strict tolerance features either chemically or mechanically.
Among the techniques used to deposit thin films, chemical vapor deposition (“CVD” hereinafter) is a method that exposes substrates to one or more reacting gases. The non-volatile decomposition product is a solid material that accumulates on the substrate in the form of a thin film.
A variant of CVD is atomic layer deposition (“ALD” as previously noted). In this technique, surfaces are exposed to gaseous species that exhibit limited reactivity, that is, that the reaction and therefore the growth shuts itself down after all surface reacting sites are consumed. Conventional ALD is carried out by sequentially exposing surfaces to two or more different gaseous species. The growth during each exposure is self-limited, and this leads to homogeneous films.
In a more recent innovation of the ALD method, these sequential exposures mentioned above are separated not in time, but in space. In one configuration, a surface is moved across different enclosures, each of them containing a different gaseous species. In a second configuration, the surface is at rest, and a movable head containing two or more different enclosures is moved over the surface, resulting in alternate exposures to the reacting gases. Combinations of these two configurations also form part of the prior art.
All these prior art designs share a common feature: the need to physically isolate one gas from the other to avoid gas-phase reactions between the two species; and this feature would effectively kill the self-limited nature of ALD. Since there must be relative motion between the surface and the enclosure wherein the gas is dosed, it is not possible to have an airtight sealing of the gaseous species. Instead, a fraction of the species will diffuse out of the enclosure through the space between the moving substrate and the enclosure walls. Moreover, both the excess gas that does not react with the surface and the gas that escapes from the enclosure need to be removed from the system. This methodology requires the implementation of different purge strategies, including purge regions separating enclosures with two different kinds of gases to quickly remove the gas before it leads to undesired gas phase reactions or the use of high pressure gas to act as effective barriers between the different enclosures. Therefore, such prior art systems and methods require construction of complicated structures and highly demanding chemical processing conditions which make difficult and impractical the use of ALD for most commercial applications.
The method and system of the invention most preferably includes use of a fixed precursor gas being injected over a moving bed or conveyance coordinated such that the amount of precursor molecules released is less than the available reaction sites presented on a reaction surface by the moving bed/web incident to the flow. This methodology leads to the complete exhaustion of precursor gas with no need for removal ports, no precursor waste, and no purge stages being needed. The spacing of these injection ports is sufficient such that all precursor is adsorbed onto the moving bed/web surface before the next precursor injection port is encountered, and thus no purge stage is required. For multiple ALD layers, the bed/web can be made long enough to accommodate multiple precursor injection ports with sufficient spacing between them, or the bed/web can move back and forth under the fixed or even adjustable position injection ports.
Fixed, saturation ALD will lead to about 99%+ coverage (dependent on dwell time), while this invention, based on precursor exhaustion, will result in 95% coverage (with only random “holes” in the coverage). However, since operational ALD requires at least several passes, these coverage differences will be likely filled in or “washed out.” Since this invention's approach is so much simpler than present “spatial ALD” solutions, the method and system will result in much cheaper equipment to be used (no gas bearings, no purge system, no pump-out zones, no complicated injector timing, etc.). In addition, there will be much less need for precision tolerances for system set-up and maintenance, increased equipment up-time, lower equipment maintenance, higher throughput, elimination of expensive wasted precursor, elimination of waste precursor separation or disposal requirements, much tighter coverage distribution and thus much higher quality product with a much more easily controlled process.
These and other advantages and features of the invention, together with the organization and manner of operation thereof, will become apparent from the following detailed description when taken in conjunction with the accompanying drawings.
While the inputs 26 and 28 can include any valves and dosing mechanisms known in the prior art, including the ability to pulse the reactants, the embodiment of
Some advantages of this approach are:
1. 100% materials utilization: all the precursor is consumed as part of the ALD process.
2. Continuous operation: no need to pulse precursors.
3. Suitable for low vapor pressure precursors.
4. Reasonable reactor sizes, no small tolerances, robust against web vibration and other perturbations of a moving wall system.
5. Reactor size decreases with higher reaction probabilities: suitable for large surface area substrates.
A variety of operating regimes can exist for the system 10 illustrated in
Considering the steady state equations of a precursor flowing into the system 10 with moving walls and where the surface chemistry is given by a first-order irreversible Langmuir kinetics, two regimes can be distinguished. These two regimes depend on an excess number, defined as the number of molecules per surface site, and the ratio of the flow and web velocity:
Where S0 is the average area of a surface site, n0 is the precursor density at the entrance of the inputs 26 and 28, V and S are the volume and the surface of the system 10, u is the average flow velocity and ν is the surface (or web) velocity.
These regions of reaction are shown substantially in
Note that, while in conventional CVD methods, complete consumption of the precursor is expected after a long enough distance of travel in a reactor, the existence of such region is not guaranteed under ALD conditions. Only when the precursor flows are carefully chosen to ensure the self-extinguishing condition, it is then possible to run the system 10 such as that depicted in
The characteristic length for precursor decay can be determined and which is given by:
here u is the average flow velocity, c0 is the final coverage after all the precursor is consumed, νth is the average thermal velocity, β is the bare reaction probability, d is the vertical gap of the reactor (distance from injector to moving web or bed), and epsilon is the tolerance for precursor depletion. This expressions is obtained under the assumption of a first order irreversible Langmuir kinetics to represent ALD's self-limited chemistry.
The separation between the inputs 26 and 28 depends on the velocity of the web 15, the vertical dimension of the reactor zone of the system 10, the mean thermal velocity, the reaction probability, the coverage and the tolerance that is required for the process. Characteristic values are shown in
This formula above can further be used to estimate the distance between the inputs 26 and 28. Also, from the results obtained it is clear that one critical parameter in the design feature is the bare reaction probability of the precursor. Therefore, it is important to understand the chemistry of the precursor in order to adapt the experimental setup to a particular one of the system 10. Likewise, the design of the system 10 also can affect the distance between injectors. In
The distances shown in
While more complex simulations can be used to simulate the interaction between the flow and the moving walls of the web 14, the formula as presented above captures the main features of the system 10, and the ratio u/ν can be chosen from more accurate, and well known, computational fluid dynamic simulations.
The results show that a high reaction probability affects positively the distance between the inputs 26 and 28. This makes the method ideal to coat high surface area materials, since the effective reaction probability on high surface area materials is larger than that on planar substrates. In
In another embodiment, since the results above show a correlation between the dosing and the velocity of the surface of the web 14, in
In yet another embodiment shown in
In a further embodiment, shown in
In additional embodiments reasonable generalizations of the systems 10 described above, include, but are not limited to, the use of more than two channels 70 of the system 10, the variation of the spacing between the different channels 70, the use of more than one moving surfaces 54 of the web 15 and the adaptation of the reactor geometry to curved surfaces that could be used to treat surfaces directly on a roll.
The method and system adaptation described herein can be applied to any method or arrangement able to operate in an ALD mode, (thermal, plasma and radical assisted, and UV-assisted) and can be used for applications such as catalysis, photovoltaics, transparent electronics, energy storage, barrier coatings for organic photovoltaics and organic light-emitting diodes, and transparent conducting oxide materials. This method is particularly well suited for the coating of high surface area materials, for instance catalyst supports, and the coating of high-cost precursors where achieving a 100% materials utilization offers significant advantages in terms of the cost of the process.
The methodology of the invention therefore eliminates the stringent tight tolerances required in many existing spatial ALD approaches to avoid the cross-talk between different precursors in the ALD process. Instead, the method herein relies on the self-extinguishing nature of the pulse to eliminate the cross talk.
In another aspect of the methodology ALD can be used under continuous deposition of particles. The fact that the effective reaction or sticking probability becomes much larger in the presence of particles is extremely convenient for the instant invention since the speed of the continuous process relative to the size of the chamber is determined by the sticking probability.
However, the fact that the instant method does not require tight tolerances at the points where the web 15 or belt 30 crosses through the reaction embodiment means that the coating of the particles 32, as a form of the substrate in the ALD process, is enabled in the presence of mechanical agitation. This agitation greatly impacts the speed of the process by reducing the time required to achieve saturation and ensures that the particles 32 are coated homogenously. Examples of methods for increasing the mixing of the particles 32 would include including a device 80 (see
The present invention has been described herein with reference to the preferred embodiments and accompanying drawings. These embodiments and drawings do not serve to limit the invention, but are set forth for illustrative purposes. The scope of the invention is defined by the claims that follow. Those skilled in the art will appreciate that various modifications, additions and substitutions are possible, without departing from the scope and spirit of the invention as disclosed in the accompanying claims.
This application is a divisional of U.S. patent application Ser. No. 14/339,058 filed Jul. 23, 2014, which claims priority to U.S. Provisional Application No. 61/857,798 filed Jul. 24, 2013, which are incorporated by reference herein in their entirety.
The U.S. Government has rights in this invention pursuant to Contract No. W-31-109-ENG-38 between the U.S. Government and the University of Chicago and/or pursuant to DE-AC-02-06 CH11357 between the U.S. Government and the UChicago Argonne, LLC representing Argonne National Laboratory.
| Number | Date | Country | |
|---|---|---|---|
| 61857798 | Jul 2013 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 14339058 | Jul 2014 | US |
| Child | 15426789 | US |