The present invention relates to the field of electronic devices and, more particularly, to methods for making electronic devices having redistribution layers (RDL).
Conventional semiconductor device packages are typically multi-layered structures. A conventional semiconductor device package may include, for example, a bottom layer of encapsulant material, a carrier, a semiconductor die, and a top layer of encapsulant material. In addition to being located above and beneath the semiconductor die and carrier, the encapsulant material of a conventional semiconductor device package may also laterally surround the semiconductor device and the carrier. In addition, a conventional semiconductor device package typically includes input/output elements to facilitate electrical connection of the semiconductor device thereof with external electronic components.
Leads are an example of conventional input/output elements. Leads typically contribute to the dimensions of the footprint of a conventional semiconductor device package and, thus, consume an undesirably large amount of real estate upon a substrate (e.g., a circuit board) to which the semiconductor device package is to be secured and electrically connected.
Other examples of such input/output elements include pins, solder balls or other discrete conductive structures (e.g., bumps, balls, columns, etc.), which contribute to the height of a conventional semiconductor device package. When coupled with the thicknesses that conventional encapsulants and carriers impart to the overall thickness of a conventional semiconductor device package, the added heights of such discrete conductive structures may result in a semiconductor device package which will protrude an undesirably large distance from a carrier substrate to which it is secured and electrically connected.
In order to keep up with the trend toward ever-decreasing the dimensions of electronic devices, various technologies have been developed to decrease the dimensions of packaged semiconductor devices. The result of many of these technologies is the “chip-scale package” (CSP), a packaged semiconductor device with lateral dimensions that are roughly the same as (i.e., slightly larger than) the corresponding lateral dimensions of the semiconductor die thereof.
Due to the relatively small, semiconductor die-dependent, lateral dimensions of CSPs, they are often formed at the so-called “wafer-scale,” meaning that packaging occurs prior to severing the semiconductor devices from a wafer or other large-scale substrate. Packaging semiconductor devices at the wafer-scale avoids the difficulties that may otherwise be associated with handling such small components during chip-scale packaging thereof.
Such wafer-scale packaging may include the formation of redistribution layers (RDL), which may rearrange or effectively expand the connection pattern of bond pads on the active surface of the semiconductor device to a redistributed connection pattern which is more suitable for connection to a substrate.
A semiconductor device including RDL is disclosed in U.S. Pat. No. 7,728,437 to Choi et al. Choi discloses a semiconductor package which includes a terminal disposed at intervals equal to or greater than a minimum pitch. The semiconductor package includes a semiconductor chip having a bottom surface on which a plurality of bumps are formed, with redistribution layer patterns formed under the semiconductor chip. Each redistribution layer includes a first part electrically connected to at least one of the bumps and a second part electrically connected to the first part. An encapsulation layer surrounds at least a top surface of the semiconductor chip, and a patterned insulating layer is formed below the redistribution layer patterns and exposes at least parts of the second parts of the redistribution layer patterns.
Further developments in methods of making electronic devices with redistribution layers are still desired, however.
In view of the foregoing background, it is therefore an object of the present invention to provide a method of transferring redistribution layers initially formed on a temporary substrate to a wafer comprising a plurality of electronic devices.
This and other objects, features, and advantages in accordance with the present invention are provided by a method of making redistributed electronic devices that includes providing a wafer comprising a plurality of electronic devices, each electronic device having a pattern of contact areas. To aid in the description of the present invention, this pattern of contact areas will be referred to as die pads.
The method includes forming redistribution layers on a temporary substrate. The redistribution layers contain a pattern of contact areas referred to as wafer bonding pads matching the die pads of the aforementioned wafer, coupled to a different pattern of contact areas referred to as redistributed pads. The die pads of the wafer of electronic devices are coupled to the wafer bonding pads of the temporary wafer containing the redistribution layers. The temporary substrate is then removed, exposing the redistributed pads.
In addition, the wafer and redistribution layers may be divided into a plurality of redistributed electronic devices after removal of the temporary substrate. Alternatively, the wafer and redistribution layers may be divided into the plurality of redistributed electronic devices before the temporary substrate is removed. After the dividing, then the temporary substrate is removed from each redistributed electronic device. A size of the temporary substrate corresponds to a size of the wafer comprising the plurality of electronic devices.
Forming the wafer and redistribution layers separately is particularly advantageous because an error in forming the wafer or redistribution layers does not result in destruction of the other, as typically occurs in prior art methods where the redistribution layers are formed directly on a wafer.
In some applications, prior to dividing the wafer, the method may include forming additional redistribution layers on an additional temporary substrate having a pattern of contact areas matching the original redistributed pads and an additional pattern of redistributed contact areas different than the original redistributed pads. The pattern of contact areas matching the original redistributed pads is coupled to the additional pattern of redistributed contact areas through the redistribution layers.
In such an application, the method may also include coupling the redistributed pads of the original redistribution layers to the pattern of contact areas matching the original redistributed pads of the additional redistribution layers and removing the additional temporary substrate from the additional redistribution layers. This may be performed multiple times in order to create the final device, which those skilled in the art will appreciate.
The present invention will now be described more fully hereinafter with reference to the accompanying drawings, in which preferred embodiments of the invention are shown. This invention may, however, be embodied in many different forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the invention to those skilled in the art. Like numbers refer to like elements throughout.
Referring initially to the flowchart 50 of
Next, the redistribution layers 29 are formed as a plurality of stacked conductive layers 23, 25, 27, with passivation layers 24, 26, 28 there between on a temporary substrate 20 (Block 56), as shown in
Next, optionally, the wafer 10 may be tested (Block 53). If at Block 54, the wafer 10 tests as being unsuitable for use, the method continues with providing a new wafer 10 as described above (Block 52). The new wafer 10 is then tested (Block 53), and the testing and providing a new wafer 10 continues until a good wafer is found. In other words, yield of good die on the wafer is greater than a threshold.
If at Block 54 the wafer tests as being suitable for use, the method proceeds to processing the redistribution layers on the temporary substrate 20, and then the redistribution layers 29 may optionally be tested (Block 57). If the redistribution layers 29 are unsuitable for use at Block 58, the method continues with forming new redistribution layers 29 on a new temporary substrate 20, as described above (Block 56).
These testing steps are particularly useful and represent an important advantage of the present invention over prior art methods. By forming the wafer 10 and redistribution layers 29 separately, as opposed to forming the redistribution layers directly on the wafer as in the prior art, the wafer and redistribution layers may be tested prior to their coupling. This way, if the wafer 10 or redistribution layers 29 are bad, non-functional, or unsuitable for use, can be replaced without having wasted the corresponding redistribution layers or wafer. In addition, forming the wafer 10 and redistribution layers 29 separately means that the wafer is not subjected to the thermal stresses caused by forming the redistribution layers directly on the wafer.
If the redistribution layers 29 are suitable for use at Block 58, the method continues with coupling the die pads 13 to the wafer bonding pads 27 (Block 60), as shown in
Next, the method continues with the removal of the temporary substrate 20 (Block 61), as shown in
Optionally, additional redistribution layers may be formed on additional temporary substrates using the methods described above. As shown in the flowchart 99 of
Forming these additional redistribution layers may be useful when the materials used to form the additional redistribution layers and original redistribution layers 29 are different and different processing temperatures are used. In these situations, forming the additional redistribution layers separately is more advantageous than making the original redistribution layers 29 more complicated.
Referring to
The wafer 10 and redistribution layers 29 are then divided into a plurality of redistributed electronic devices 31, 32 (Block 64) using techniques known to those of skill in the art, as shown in
Even though the illustrated flowchart shows Block 64 being performed after Block 61, the reverse order may occur. That is, the coupled wafers and redistribution layers may be divided into a plurality of redistributed electronic device before the temporary substrates are removed from the redistribution layers. The temporary substrate can then be removed for each individual redistributed electronic device. Even though the order of Blocks 61 and 64 are interchangeable, forming the interconnect structures on the redistributed pads in Block 63 needs to be performed after the temporary substrate has been removed in Block 61. This is regardless of when the redistributed wafer is divided in Block 64. For instance, processing in the order of Blocks 61, 64, 63 would be acceptable. Block 65 indicates the end of the method.
As discussed above, a wafer 10 comprising the electronic devices 11, 12 is coupled to the redistribution layers 29 on the temporary substrate 20. A size of the temporary substrate 20 corresponds to a size of the wafer 10 comprising the plurality of electronic devices 11, 12. This may be referred to as redistribution at the wafer level. After being coupled together, the wafer 10 and the temporary substrate 20 are then divided into redistributed electronic devices 31, 32. The dividing may be done before or after the temporary substrate 20 is removed. Since the electronic devices 11, 12 come from the same wafer 10, they typically have the same design, function and layout. In other words, the electronic devices 11 and 12 on the wafer 10 are equal to one another.
Referring now to
Since the electronic devices 14′, 15′ are each being handled on an individual basis, they may be different from one another in terms of design and function. This allows the electronic devices 14′, 15′ to be random from one another. Electronic devices as used herein broadly covers integrated circuits, dies and any components requiring a redistribution layer, as readily appreciated by those skilled in the art.
As illustrated in
The temporary substrate 20′ is formed with the redistribution layers 29a′, 29b′ being different from one another. The above description with respect to forming the redistribution layers 29 on a temporary substrate 20 is also applicable to forming the redistribution layers 29a′, 29b′ on a temporary substrate 20′, with the exception being that the pattern of contact areas on the redistribution layers 29a′, 29b′ are different from one another.
Alternatively, the temporary substrate may be formed so that the redistribution layers are all the same, as is the case for the temporary substrate 20 illustrated in
Another aspect is directed to the temporary substrate 20″ being sized so that it corresponds in size to an electronic device 14″ being bonded thereto, as illustrate in
In terms of removing the temporary substrate 20′ illustrated in
In terms of removing the temporary substrate 20″ illustrated in
A flowchart 100 illustrating a method for making an electronic device with a redistribution layer will now be discussed in reference to
Many modifications and other embodiments of the invention will come to the mind of one skilled in the art having the benefit of the teachings presented in the foregoing descriptions and the associated drawings. Therefore, it is understood that the invention is not to be limited to the specific embodiments disclosed, and that modifications and embodiments are intended to be included within the scope of the appended claims.
| Number | Name | Date | Kind |
|---|---|---|---|
| 3333326 | Thomas, Jr. et al. | Aug 1967 | A |
| 3726002 | Greenstein et al. | Apr 1973 | A |
| 5034091 | Trask et al. | Jul 1991 | A |
| 5192716 | Jacobs | Mar 1993 | A |
| 5311404 | Trask et al. | May 1994 | A |
| 5514613 | Santadrea et al. | May 1996 | A |
| 5521122 | Kuramochi | May 1996 | A |
| 5691245 | Bakhit et al. | Nov 1997 | A |
| 5998291 | Bakhit et al. | Dec 1999 | A |
| 6222212 | Lee et al. | Apr 2001 | B1 |
| 6514780 | Manyoki | Feb 2003 | B2 |
| 6746898 | Lin et al. | Jun 2004 | B2 |
| 6762074 | Draney et al. | Jul 2004 | B1 |
| 6875638 | Yoneda et al. | Apr 2005 | B2 |
| 6995044 | Yoneda et al. | Feb 2006 | B2 |
| 7208335 | Boon et al. | Apr 2007 | B2 |
| 7425458 | Seshan | Sep 2008 | B2 |
| 7435910 | Sakamoto et al. | Oct 2008 | B2 |
| 7728437 | Choi et al. | Jun 2010 | B2 |
| 7749814 | Lin et al. | Jul 2010 | B2 |
| 7807505 | Farnworth et al. | Oct 2010 | B2 |
| 20030122244 | Lin et al. | Jul 2003 | A1 |
| 20030122246 | Lin et al. | Jul 2003 | A1 |
| 20030124767 | Lee et al. | Jul 2003 | A1 |
| 20050233482 | Kirby et al. | Oct 2005 | A1 |
| 20070262436 | Kweon et al. | Nov 2007 | A1 |
| 20080132006 | Jiang et al. | Jun 2008 | A1 |
| 20080265367 | Tan et al. | Oct 2008 | A1 |
| 20080315372 | Kuan et al. | Dec 2008 | A1 |
| 20100068837 | Kumar et al. | Mar 2010 | A1 |
| 20110074028 | Pendse | Mar 2011 | A1 |
| 20120015532 | Markovich et al. | Jan 2012 | A1 |
| 20120098129 | Reed et al. | Apr 2012 | A1 |
| 20120146216 | Kang et al. | Jun 2012 | A1 |
| 20120187545 | Khan et al. | Jul 2012 | A1 |
| 20120306068 | Saito | Dec 2012 | A1 |
| 20130056880 | Wang et al. | Mar 2013 | A1 |
| 20130203240 | Reed et al. | Aug 2013 | A1 |
| Number | Date | Country |
|---|---|---|
| 9009093 | Aug 1990 | WO |
| 2004051737 | Jun 2004 | WO |
| Number | Date | Country | |
|---|---|---|---|
| 20130203190 A1 | Aug 2013 | US |