The present invention relates to Microelectromechanical Systems (MEMS) devices, and more particularly, to fabrication of MEMS devices with portions exposed to the outside environment.
Many MEMS devices, specifically those measuring or modifying aspects of the environment outside of the device (e.g. pressure sensors, microphones, speakers, chemical sensors, biological sensors, optical sensors etc.) require a portion of the MEMS structure exposed to the outside environment. There is a strong need for a cost-effective and efficient fabrication process that implements and improves operation of such MEMS devices by fabricating devices with portions exposed to the outside environment. The present invention addresses such a need.
A method and system for providing a MEMS device with a portion exposed to an outside environment are disclosed. In a first aspect, the method comprises bonding a handle wafer to a device wafer to form a MEMS substrate with a dielectric layer disposed between the handle and device wafers. The method includes lithographically defining at least one standoff on the device wafer and bonding the at least one standoff to an integrated circuit substrate to form a sealed cavity between the MEMS substrate and the integrated circuit substrate. The method includes etching at least one opening in the handle wafer to expose a portion of the dielectric layer and etching the exposed portion of the dielectric layer to expose a portion of the device wafer to the outside environment.
In a second aspect, the MEMS device comprises a CMOS substrate and a MEMS substrate bonded to the CMOS substrate. The MEMS substrate includes a handle substrate bonded to a device substrate with a dielectric layer disposed between the handle and device substrates. The MEMS device includes at least one opening in the handle substrate, wherein the at least one opening exposes a surface of the device substrate to the outside environment.
The accompanying figures illustrate several embodiments of the invention and, together with the description, serve to explain the principles of the invention. One of ordinary skill in the art readily recognizes that the particular embodiments illustrated in the figures are merely exemplary, and are not intended to limit the scope of the present invention.
a illustrates the first MEMS device with an optional third etch of the device wafer in accordance with an embodiment.
b illustrates the first MEMS device where the etched opening is located over a stand-off frame, such that the dimensions of a flexible portion of the device wafer are defined by the location of the stand-off frame rather than the location and dimensions of the etched opening.
a illustrates a MEMS device in accordance with an embodiment.
b illustrates a second MEMS device in accordance with an embodiment.
The present invention relates to Microelectromechanical Systems (MEMS) devices, and more particularly, to fabrication of MEMS devices with portions exposed to the outside environment. The following description is presented to enable one of ordinary skill in the art to make and use the invention and is provided in the context of a patent application and its requirements. Various modifications to the described embodiments and the generic principles and features described herein will be readily apparent to those skilled in the art. Thus, the present invention is not intended to be limited to the embodiments shown but is to be accorded the widest scope consistent with the principles and features described herein.
A CMOS-MEMS integrated process can be utilized to create hermetically sealed MEMS devices that are integrated with CMOS wafers/substrates through wafer bonding. The resulting MEMS devices are sealed inside the resulting enclosure and do not have direct exposure to the environment. For some devices including but not limited to pressure sensors, optical MEMS, biological sensors, it is desirable for the MEMS structure to directly interface with the environment.
A method and system in accordance with the present invention provides a process for fabricating a MEMS device with a portion exposed to an outside environment. By bonding a MEMS substrate to an integrated circuit substrate and etching a portion of the MEMS substrate, the portion of the MEMS substrate is then exposed to the outside environment. The portion of the MEMS substrate that is exposed to the outside environment may be thinner than the remaining structural device layers of the MEMS substrate to enable the creation of a pressure sensor or related MEMS device that requires enhanced sensitivity. The integration of such pressure sensor or related MEMS devices with other MEMS devices including but not limited to motion sensors is also achieved by the fabrication process.
To describe the features of the present invention in more detail, refer now to the following description in conjunction with the accompanying Figures.
Thus, MEMS device 100 is a starting CMOS-MEMS bonded wafer that is created through a standard process. A top surface of the MEMS substrate is coated by a photoresist material and an opening is photolithographically defined over a region of the MEMS substrate that is to be exposed to the outside environment. In one embodiment, the starting wafer has a portion of the MEMS structural device layer thinned to a desired thickness prior to bonding with the CMOS wafer.
a illustrates the MEMS device 400a with an optional third etch 206 of the handle wafer 102 in accordance with an embodiment. In one embodiment, the third etch 206 is a membrane DRIE etch through the device wafer 106 that stops when it reaches a desired membrane thickness. One of ordinary skill in the art readily recognizes that the desired membrane thickness can vary in accordance with differing needs and applications and that would be within the spirit and scope of the present invention. Each of the first, second, and third etches 202-206 can be timed so as to stop the etch process at predetermined time periods and exacting thickness levels. Additionally, each of the first, second, and third etches 202-206 are selectively etched using a wet or dry etch.
b is an embodiment where the lateral membrane dimensions are determined by a contiguous standoff frame, 112. The diameter of the membrane, 116, is determined by the inner dimensions of the standoff frame. This membrane size definition may have superior lateral dimensional control than membranes defined by the first, second, and, third etches patterned from the topside of handle wafer, 102
In one embodiment, the device wafer 106 comprises two layers of silicon, a top structural layer and a bottom structural layer, fusion bonded through a dielectric.
In
In one embodiment, an additional substrate with fluidic or gas channels is bonded to a top surface of the MEMS substrate to create a fluidic or gas interface to an exposed portion of the MEMS device. One of ordinary skill in the art readily recognizes that the additional substrate can be bonded to a variety of surfaces including but not limited to a top surface of the handle wafer of the MEMS substrate and that would be within the spirit and scope of the present invention. In another embodiment, the opening in the handle wafer and oxide layers is created by non-etching means including but not limited to saw dicing, laser drilling, laser-assisted etching, and mechanical drilling.
In one embodiment, the wafer-level packaging process is done using TSV from the MEMS substrate side which allows the process that etches the handle wafer to simultaneously create a port to expose the structural layer and define a via for the TSV contacts required for the wafer-level packaging process. In this embodiment, great care must be taken to protect the MEMS membrane layers from metallization and solder mask deposition.
The wafer-level packaging process 700 includes depositing a Silicon Dioxide (SiO2) insulator layer 702 using chemical vapor deposition (CVD) or a sputter method. The SiO2 insulator layer 702 is deposited over the entire top surface of the handle wafer 102 of the MEMS device 100 including each surface within the two openings that were previously etched. Only the bottom surfaces 704 of the two openings 750 and 760 that included the deposited SiO2 layer are etched. A first photoresist patterning is deposited in the opening 760 and then a redistribution layer (RDL) 706 is deposited using a lift-off process. An electroplating top metal 708 is deposited on top of the RDL 706. In one embodiment, the electroplating top metal 708 is Copper (Cu).
A second photoresist patterning is deposited in both the opening 760 and on a top surface on a left side of the handle wafer 702 and then an insulating solder mask layer 710 is deposited using a lift-off process. Finally, a solder ball 712 is deposited into the insulating solder mask layer 710 using screen/stencil printing. One of ordinary skill in the art readily recognizes that the solder ball 712 can be deposited by a variety of methodologies and that would be within the spirit and scope of the present invention.
A MEMS device can also be packaged in a plastic-molded package with a handle wafer that is combined with a mold cap that acts like a dam to prevent a mold compound from entering an opening/cavity in the handle wafer and contacting an exposed device layer. In one embodiment, the mold cap uses a soft material including but not limited to tape which enhances sealing of the opening/cavity in the handle wafer.
The plastic-molding packaging process 900 includes singulating die of the MEMS device and attaching the die to the package lead frame 914 via the wire bonding 910. The plastic-molding packaging process 900 includes coupling a mold cap 916 to a top surface of the handle wafer 902 of the MEMS device. Once a molding compound 918 is applied to the MEMS device, the mold cap 916 prevents the molding compound 918 from entering an opening of the handle wafer 902 and coming in contact with exposed device layers of the MEMS device. After the molding compound 918 application has completed, the mold cap 916 is removed and the MEMS device is singulated.
In one embodiment, the etch process of the MEMS device is done on an area of the handle wafer that is located above the exposed device layers.
In one embodiment, a section of a device wafer of the MEMS device is exposed to the outside environment by extending an upper cavity of the MEMS device to a dicing lane edge so that the upper cavity is exposed to the outside environment when the MEMS device is singulated, thus creating a side-channel exposed to the outside environment. One of ordinary skill in the art readily recognizes that this embodiment can be utilized in a variety of applications including but not limited to exposing a pressure-sensor flexible plate to outside environment pressure and that would be within the spirit and scope of the present invention.
In this embodiment, a cavity seal of the MEMS device is maintained during all pre-singulation wafer processing preventing the need to protect the openings in the handle wafer/MEMS device from process liquids, gasses, and residues. In another embodiment, the side-channel remains sealed by a variety of mechanisms including but not limited to a narrow side plate and a fusion bond after singulation to protect the side-channel from singulation residues. The narrow side plate or fusion bond is then opened at a later stage through a puncturing process including but not limited to laser machining and laser dicing.
The device layer or substrate of the aforementioned MEMS devices is thinned during the aforementioned fabrication processes. In one embodiment, a portion of the device wafer to be exposed to the outside environment is thinned prior to fusion bonding to the handle wafer.
The fabrication process 1800 includes further processing and thinning of the device layer/MEMS substrate wafer by forming a plurality of standoffs on the device wafer, depositing Germanium or another material, and patterning and etching the device layer, via step 1808.
In one embodiment, port openings in the aforementioned MEMS devices that are exposed to the outside environment are fully or partially filled with a porous material including but not limited to Gortex to allow gasses or liquids to still penetrate to the MEMS portion while protecting the MEMS device from larger particles and objects.
As above described, the method and system allow for the fabrication of more efficient and more accurate force sensing and force exerting MEMS devices. By coupling an integrated circuit substrate to a MEMS substrate and utilizing an open handle wafer cavity, a top surface of the MEMS substrate structural layer is exposed to the outside environment. On one side of a flexible plate of the MEMS substrate is a hermetically sealed cavity/chamber while the other side is exposed to the surrounding ambient environment.
The approach disclosed in accordance with an embodiment allows wafer-level integration of environment-exposed MEMS structures with CMOS wafers and also allows the integration of such structures with other non-exposed structures on a same die that has varying levels of thickness. Specifically, the structural layer thickness of the exposed device on the die may be different (e.g. thinner) than that of the structural layer thickness of the other devices on the die. This enables the exposed device to benefit from increased sensitivities. Additionally, the method and system provide wafer-level packaging of these MEMS devices without damaging or compromising the exposed structural layer.
Although the present invention has been described in accordance with the embodiments shown, one of ordinary skill in the art will readily recognize that there could be variations to the embodiments and those variations would be within the spirit and scope of the present invention. Accordingly, many modifications may be made by one of ordinary skill in the art without departing from the spirit and scope of the appended claims.
This application claims the benefit of U.S. Provisional Patent Application No. 61/502,603, filed on Jun. 29, 2011, entitled “MEMS DEVICE, FABRICATION PROCESS, INTEGRATED SENSORS, PRESSURE SENSORS, OPTICAL SENSORS, MICRO-FLUIDIC, ACCELEROMETER,” which is incorporated herein by reference in its entirety. This application is related to U.S. Provisional Patent Application No. 61/502,616 filed Jun. 29, 2011, docket # IVS-156PR (5028PR), titled “HERMITICALLY SEALED MEMS DEVICE WITH A PORTION EXPOSED TO THE ENVIRONMENT AND WITH VERTICALLY INTERGRATED ELECTRONIC,” and U.S. patent application Ser. No. ______ docket # IVS-156 (5028P), entitled “HERMETICALLY SEALED MEMS DEVICE WITH A PORTION EXPOSED TO THE ENVIRONMENT WITH VERTICALLY INTEGRATED ELECTRONICS,” filed concurrently herewith and assigned to the assignee of the present invention, all of which are incorporated herein in their entireties.
Number | Date | Country | |
---|---|---|---|
61502603 | Jun 2011 | US |