Atomic layer deposition methods

Abstract
The invention includes an atomic layer deposition method of forming a layer of a deposited composition on a substrate. The method includes positioning a semiconductor substrate within an atomic layer deposition chamber. On the substrate, an intermediate composition monolayer is formed, followed by a desired deposited composition from reaction with the intermediate composition, collectively from flowing multiple different composition deposition precursors to the substrate within the deposition chamber. A material adheres to a chamber internal component surface from such sequentially forming. After such sequentially forming, a reactive gas flows to the chamber which is different in composition from the multiple different deposition precursors and which is effective to react with such adhering material. After the reactive gas flowing, such sequentially forming is repeated. Further implementations are contemplated.
Description
TECHNICAL FIELD

This invention relates to atomic layer deposition methods.


BACKGROUND OF THE INVENTION

Semiconductor processing in the fabrication of integrated circuitry typically includes the deposition of layers on semiconductor substrates. One such method is atomic layer deposition (ALD) which involves the deposition of successive monolayers over a substrate within a deposition chamber typically maintained at subatmospheric pressure. With typical ALD, successive mono-atomic layers are adsorbed to a substrate and/or reacted with the outer layer on the substrate, typically by successive feeding of different deposition precursors to the substrate surface.


Atomic layer depositions are typically conducted within chambers or reactors which retain a single substrate upon a wafer holder or susceptor. The chambers include internal walls and other internal components which can undesirably have deposition product deposited thereupon in addition to the substrate. One existing method of protecting or preserving the internal chamber walls and other components is to shield such from the deposition material with one or more removable liners or shields. The liners might be received immediately adjacent or against the internal chamber walls or other surfaces. Alternately, the liners might be displaced from the wall or other surfaces, thereby defining an appreciably reduced volume chamber, or subchamber, within which the substrate is received for deposition. One advantage of using liners and shields is that they can be periodically replaced with new or cleaned liners, thereby extending the life of the deposition chambers and components therein. Further and regardless, the spent liners and shields can typically be removed and replaced much more quickly than the time it would take to clean the internal chamber walls and other components at given cleaning intervals.


An exemplary ALD method includes feeding a single vaporized precursor to a deposition chamber effective to form a first monolayer over a substrate received therein. Thereafter, the flow of the first deposition precursor is ceased and an inert purge gas is flowed through the chamber effective to remove any remaining first precursor which is not adhering to the substrate from the chamber. Subsequently, a second vapor precursor different from the first is flowed to the chamber effective to form a second monolayer on/with the first monolayer. The second monolayer might react with the first monolayer. Additional precursors can form successive monolayers, or the above process can be repeated until a desired thickness and composition layer has been formed over the substrate.


It is a desired intent or effect of the purging to remove unreacted gas or reaction by-products from the chamber to provide a clean reactive surface on the substrate for the subsequent precursor. In the context of this document, a reaction by-product is any substance (whether gas, liquid, solid or mixture thereof) which results from reaction of any deposition precursor flowing to the chamber and that is not desired to be deposited on the substrate. Further in the context of this document, an intermediate reaction by-product or reaction intermediate by-product is a reaction by-product formed by less than desired complete reaction of a precursor to form a desired monolayer on the substrate. Where there is a great degree of varying topography and/or there are high aspect ratio features on the substrate, it can be difficult to move the unreacted gases or reaction by-products from deep within openings for ultimate removal from the chamber. Further, certain reaction by-products, particularly intermediate reaction by-products, may not be gaseous and may not completely react to form gaseous reaction by-products in the typical short precursor pulse times. Accordingly, the purge gas pulse may not be effective or sufficient in removing such intermediate reaction by-products from the substrate and chamber.


For example, consider that in an atomic layer deposition of titanium nitride using TiCl4 and NH3, the desired deposition product is TiN with HCl gas being the desired principle gaseous by-product. Consider also that there might be reaction intermediate by-products which might, even if gaseous, be difficult to remove from substrate openings. Further, if certain reaction intermediate by-products are solid and/or liquid phase prior to HCl formation, complete removal can be even more problematic where less than complete reaction to TiN and HCl occurs.


Consider also the atomic layer deposition of Al2O3 using trimethylaluminum (TMA) and ozone as alternating deposition precursors. Apparently in such deposition, achieving an effective ozone precursor feed can be somewhat of a challenge due to the limited lifetime of ozone within the chamber. Specifically, an ozone molecule is in an inherently unstable, reactive form of oxygen which can rapidly dissociate and/or combine with another ozone molecule to form three O2molecules. Regardless, a desired goal in the ozone feed is to result in oxygen atoms from the O3 bonding to the surface of the substrate with O2 as the reaction by-product which is driven off. Of course, the O2 which forms deep within openings on the substrate has to be removed therefrom while more 03 needs to get into the openings to desirably form a complete monolayer of oxygen atoms adhered and projecting from the substrate. In other words, the O2 which forms is trying to get out while more O3 is desirably trying to get in.


While the invention was motivated in addressing the above issues and improving upon the above-described drawbacks, it is in no way so limited. The invention is only limited by the accompanying claims as literally worded (without interpretative or other limiting reference to the above background art description, remaining portions of the specification or the drawings) and in accordance with the doctrine of equivalents.


SUMMARY

The invention includes an atomic layer deposition method of forming a layer of a deposited composition on a substrate. The method includes positioning a semiconductor substrate within an atomic layer deposition chamber. On the substrate, an intermediate composition monolayer is formed, followed by a desired deposited composition from reaction with the intermediate composition, collectively from flowing multiple different composition deposition precursors to the substrate within the deposition chamber. A material adheres to a chamber internal component surface from such sequential forming. After such sequential forming, a reactive gas flows to the chamber which is different in composition from the multiple different deposition precursors and which is effective to react with such adhering material. After the reactive gas flowing, such sequential forming is repeated.


Further implementations are contemplated.





BRIEF DESCRIPTION OF THE DRAWINGS

Preferred embodiments of the invention are described below with reference to the following accompanying drawings.



FIG. 1 is a diagrammatic depiction of flow versus time of one atomic layer deposition process in accordance with an aspect of the invention.



FIG. 2 is a diagrammatic depiction of flow versus time of one atomic layer deposition process in accordance with an aspect of the invention.



FIG. 3 is a diagrammatic depiction of flow versus time of one atomic layer deposition process in accordance with an aspect of the invention.





DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

This disclosure of the invention is submitted in furtherance of the constitutional purposes of the U.S. Patent Laws “to promote the progress of science and useful arts” (Article 1, Section 8).


An atomic layer deposition method in accordance with an aspect of the invention includes positioning a semiconductor substrate within an atomic layer deposition chamber. In the context of this document, the term “semiconductor substrate” or “semiconductive substrate” is defined to mean any construction comprising semiconductive material, including, but not limited to, bulk semiconductive materials such as a semiconductive wafer (either alone or in assemblies comprising other materials thereon), and semiconductive material layers (either alone or in assemblies comprising other materials). The term “substrate” refers to any supporting structure, including, but not limited to, the semiconductive substrates described above.


An intermediate composition monolayer is formed on the substrate from one or more deposition precursors flowed to the substrate within the deposition chamber. Then, one or more different composition deposition precursors is flowed to the substrate within the deposition chamber effective to react with the first monolayer and form a monolayer comprising a desired deposited composition of the ultimate layer being formed, with “desired” herein referring to at least at this point in time with respect to the preferred method. In other words, such deposited layer might be subsequently annealed, implanted, exposed to plasma, or otherwise processed in a manner which does not significantly modify its overall composition. Any deposition precursor gases are contemplated whether existing or yet-to-be developed. By way of example only where a desired ultimate deposition product or layer is TiN, exemplary different composition precursors include TiCl4 or NH3 to deposit a TiN comprising layer. Further by way of example only where the ultimate layer or product being formed is to be Al2O3, exemplary different composition deposition precursors include trimethylaluminum and ozone. Further by way of example only, an exemplary first monolayer intermediate composition utilizing TiCl4 would include titanium or a titanium complex, whereas with respect to NH3 such would at least include nitrogen. With respect to trimethylaluminum, the first monolayer intermediate composition would include an aluminum complex, and with ozone typically adhered oxygen atoms. Any suitable temperature, pressure, flow rate or other operating parameters, with or without plasma, can be selected and optimized by the artisan, of course, with no particular set of the same being preferred or constituting a part of the invention.


By way of example only, FIG. 1 depicts an exemplary plot of flow rate versus time of but one process in accordance with an aspect of the invention. A first precursor gas is flowed to the substrate within the atomic layer deposition chamber effective to form a first monolayer on the substrate. Such is designated by a precursor flowing P1. After forming the first monolayer of intermediate composition on the substrate, a second precursor gas, different in composition from the first precursor gas, is flowed to the substrate within the deposition chamber effective to react with the first monolayer and form a monolayer comprising the desired deposited composition. Such second precursor gas flowing is designated by P2. The particular lengths and rates of the respective flowings, and the times therebetween, can also be optimized by the artisan, of course, and do not constitute material or preferred aspects of the inventions disclosed herein. Further, the exemplary FIG. 1 and other figure depictions contemplate any processing occurring before or after the depicted flowings, including any additional processing intermediate the respective gas pulses, unless such is specifically precluded by the particular claim under analysis as literally worded, without interpretative or limiting reference to the background art description, remaining portions of the specification or the drawings, and yet in accordance with the doctrine of equivalents.


In the course of one or both of the above-described precursor flowings, some material may adhere to a chamber internal component surface. In the context of this document, a “chamber internal component surface” comprises any surface of hardware received within the deposition chamber that is subjected to multiple processings of semiconductor substrates within the chamber. Examples include an actual internal wall surface of the chamber, a surface of a chamber liner apparatus which forms a deposition subchamber within the chamber, and a surface of a portion of a substrate support received internally of the chamber walls.


By way of example only, the adhering material might be derived totally or at least primarily from a deposition precursor flow which forms the intermediate composition monolayer. Alternately by way of example only, such material might be derived totally or at least primarily from a deposition precursor flow which reacts with the intermediate composition monolayer and forms the desired deposited composition. The adhering material and the intermediate composition might be of a common composition relative one another or of different composition. The material might also adhere to the substrate within the chamber which is the focus of the deposition, although the invention is principally directed to contending with material which adheres to chamber internal component surfaces. Further by way of example only, and during the formation of the intermediate composition monolayer, intermediate reaction by-product might be formed, for example in any of gaseous, liquid and deposited states. Such adhering material might be of common composition with one or more of the intermediate reaction by-products, or be different in composition from all intermediate reaction by-products.


In one non-limiting consideration, such adhering material might be reactive with one or a multiple of the deposition precursors. In such event, it might be desirable to remove such adhering material from the substrate so it will not react with subsequent flowing precursor, or at least in some way passivate such adhering material to preclude its reaction with subsequently flowing deposition precursors. Further by way of example only, the adhering material might result, in part, from the reaction of deposition precursor with material of the chamber internal component surface, thus forming material adhering thereto. Such might constitute a monolayer or eventually considerably thicker layers from the successive formation of repeated monolayers.


By way of example only, an exemplary adhered material might comprise oxygen atoms adhering to a metal internal surface of a deposition chamber. Such could manifest by the feeding of ozone in any of the above-described exemplary processes involving the deposition of Al2O3. Alternately by way of example only, such might encompass any of TiCl2, TiCl3 and NH3 complexes with respect to TiCl4 and NH3 deposition precursor flows.


After forming at least the initially desired deposited composition of the layer being formed, a reactive gas is flowed to the chamber which is different in composition from the multiple different deposition precursors effective to react with the adhering material. Further in one preferred embodiment, such reactive gas flowing preferably occurs prior to forming any further monolayer on the substrate.


In one aspect, the reactive gas reacts to modify the composition of the adhering material, with such modified composition material adhering to the chamber internal component surface(s). By way of example only, and where the adhering material comprises TiCl, TiCl2 and/or TiCl3, an exemplary reactive gas would be O2 to modify the adhering material composition to TiO2, which still adheres to the chamber internal component surface.


In one aspect, the reactive gas reacts to effectively remove the adhered material, and any reaction by-product thereof, from adhering to the chamber internal component surface. For example and by way of example only, where the adhering material comprises TiCl, TiCl2 and/or TiCl3, an exemplary reactive gas includes Cl2, which would effectively etch or otherwise vaporize the adhering material from the substrate (i.e., to TiCl4) and be exhausted from the chamber.


In one aspect, the reactive gas is not capable under conditions of the reactive gas flowing of reaction with the desired deposited composition. In one aspect, and under conditions of the reactive gas flowing, the reactive gas is capable of reaction with the intermediate composition, and regardless of whether any intermediate composition is exposed during the reactive gas flowing, either on the substrate or on any chamber internal component surface.


The conditions (i.e., temperature, pressure, flow rate, etc.) of the reactive gas flowing can be optimized by the artisan and are not otherwise particularly germane or preferred to any aspect of the invention. By way of example only, such conditions might be the same as, or different from, any of a first precursor gas flow, a second precursor gas flow and/or inert purge gas flow. In one aspect, the reactive gas flow is plasma-enhanced, for example either by plasma generation within the chamber, plasma generation remote of the chamber, or both.


The particular reactive gas selected, whether a single constituent or a mixture of constituents, will depend as a minimum upon at least some portion or component of the adhering material which will be capable of reaction with the reactive gas under conditions of the reactive gas flowing. By way of example only, possible reactive gas components include Cl2, O2 and H2. For example and by way of example only where the adhering material comprises oxygen atoms, such might be removed in the presence of O2 to form ozone and/or with H2 to form H2O, which is exhausted from the chamber.



FIG. 1 depicts an exemplary such reactive gas flowing in the form of a discrete pulse RG. After the reactive gas flowing, the sequential forming is repeated, whereby an intermediate composition monolayer is formed, then a desired deposited composition from reaction with the intermediate composition collectively from flowing multiple different composition deposition precursors to the substrate within the deposition chamber. FIG. 1 depicts such exemplary processing by subsequent P1 and P2 pulsings. In one preferred embodiment, thereafter the reactive gas flowing is repeated (FIG. 2). Further in one aspect, the repeating of one or both of the sequential formings, as just so stated, and/or the reactive gas flowing, are sequentially repeated multiple times. Further in one aspect, the invention contemplates repeating the sequentially forming multiple times and repeating the reactive gas flowing only periodically after a plurality of consecutive sequential forming repetitions. In other words, such reactive gas flowing does not necessarily occur intermediate each desired deposited composition monolayer forming, but rather after multiple formings thereof.


Further more typically and preferably, inert gas flows are interposed between some or all of the respective deposition precursor and reactive gas flowings. By way of example only, such is depicted in FIG. 3. There illustrated is a two-sequence repetition, with inert gas flows being indicated by IN and which are interposed between the respective precursor and reactive gas flows.


In compliance with the statute, the invention has been described in language more or less specific as to structural and methodical features. It is to be understood, however, that the invention is not limited to the specific features shown and described, since the means herein disclosed comprise preferred forms of putting the invention into effect. The invention is, therefore, claimed in any of its forms or modifications within the proper scope of the appended claims appropriately interpreted in accordance with the doctrine of equivalents.

Claims
  • 1. An atomic layer deposition method, comprising: leaving a material on a chamber internal component surface while forming a composition on a substrate received within the chamber by atomic layer deposition using multiple different composition deposition precursors, said chamber internal component surface comprising a surface other than a surface of the substrate;with the substrate in the chamber, flowing a reactive gas to the chamber effective to react with the material left on the chamber internal component surface, the reactive gas being different in composition from the multiple different deposition precursors; andafter flowing the reactive gas, again forming the composition on the substrate within the chamber by atomic layer deposition using said multiple different composition deposition precursors.
  • 2. The method of claim 1 wherein the material is also left on the substrate and the reactive gas reacts with such material left on the substrate.
  • 3. The method of claim 1 wherein the material is also left on the substrate and the reactive gas reacts with such material left on the substrate effective to remove it from the substrate.
  • 4. The method of claim 1 wherein the reactive gas reacts to modify composition of the material left on the chamber internal component surface, with such modified composition material remaining on the chamber internal component surface.
  • 5. The method of claim 1 wherein the reactive gas flowing is plasma enhanced.
  • 6. The method of claim 1 wherein the reactive gas flowing is plasma enhanced by plasma generation within the chamber.
  • 7. The method of claim 1 wherein the reactive gas flowing is plasma enhanced by plasma generation remote of the chamber.
  • 8. The method of claim 1 wherein the reactive gas comprises Cl2.
  • 9. The method of claim 1 wherein the reactive gas comprises O2.
  • 10. The method of claim 1 wherein the reactive gas comprises H2.
  • 11. The method of claim 1 wherein the material left on the chamber internal component surface comprises oxygen atoms.
RELATED PATENT DATA

This patent resulted from a continuation application of U.S. patent application Ser. No. 10/222,282, filed Aug. 15, 2002, now U.S. Pat. No. 6,753,271 entitled “Atomic Layer Deposition Methods”, naming Demetrius Sarigiannis, Garo J. Derderian, Cem Basceri, Gurtej S. Sandhu, F. Daniel Gealy and Chris M. Carison as inventors, the disclosure of which is incorporated by reference.

US Referenced Citations (68)
Number Name Date Kind
5225032 Golecki Jul 1993 A
5879459 Gadgil et al. Mar 1999 A
5925411 van de Ven et al. Jul 1999 A
5972430 DiMeo, Jr. et al. Oct 1999 A
6015597 David Jan 2000 A
6174377 Doering et al. Jan 2001 B1
6197120 David Mar 2001 B1
6200893 Sneh Mar 2001 B1
6270572 Kim et al. Aug 2001 B1
6287965 Kang et al. Sep 2001 B1
6301434 McDiarmid et al. Oct 2001 B1
6305314 Sneh et al. Oct 2001 B1
6355561 Sandhu et al. Mar 2002 B1
6387185 Doering et al. May 2002 B2
6391785 Satta et al. May 2002 B1
6403156 Jang et al. Jun 2002 B2
6426307 Lim Jul 2002 B2
6451119 Sneh et al. Sep 2002 B2
6451695 Sneh Sep 2002 B2
6468924 Lee et al. Oct 2002 B2
6475276 Elers et al. Nov 2002 B1
6475286 Frijlink Nov 2002 B1
6475910 Sneh Nov 2002 B1
6482262 Elers Nov 2002 B1
6482476 Liu Nov 2002 B1
6534395 Werkhoven et al. Mar 2003 B2
6585823 Van Wijck Jul 2003 B1
6586343 Ho et al. Jul 2003 B1
6589886 Kim et al. Jul 2003 B2
6590251 Kang et al. Jul 2003 B2
6602784 Sneh Aug 2003 B2
6613587 Carpenter et al. Sep 2003 B1
6613695 Pomarede et al. Sep 2003 B2
6620253 Dando et al. Sep 2003 B1
6620723 Byun Sep 2003 B1
6630401 Sneh Oct 2003 B2
6638862 Sneh Oct 2003 B2
6664192 Satta et al. Dec 2003 B2
6673701 Marsh et al. Jan 2004 B1
6696157 David Feb 2004 B1
6696368 Derraa et al. Feb 2004 B2
6720027 Yang et al. Apr 2004 B2
6727169 Raaijmakers et al. Apr 2004 B1
6730367 Sandhu May 2004 B2
6746952 Derraa et al. Jun 2004 B2
6753271 Sarigiannis et al. Jun 2004 B2
6821347 Carpenter et al. Nov 2004 B2
20010024387 Raaijmakers et al. Sep 2001 A1
20010041250 Werkhoven et al. Nov 2001 A1
20010050039 Park Dec 2001 A1
20010054381 Umotoy et al. Dec 2001 A1
20020086111 Byun et al. Jul 2002 A1
20020108570 Lindfors Aug 2002 A1
20020108714 Doering et al. Aug 2002 A1
20020173054 Kim Nov 2002 A1
20020173130 Pomerede et al. Nov 2002 A1
20020187256 Elers Dec 2002 A1
20030031807 Elers et al. Feb 2003 A1
20030032281 Werkhoven et al. Feb 2003 A1
20030082307 Chung et al. May 2003 A1
20030085424 Bryant et al. May 2003 A1
20030108674 Chung et al. Jun 2003 A1
20030129826 Werkhoven et al. Jul 2003 A1
20030143328 Chen et al. Jul 2003 A1
20030183171 Sneh et al. Oct 2003 A1
20040083959 Carpenter et al. May 2004 A1
20040137728 Gallagher et al. Jul 2004 A1
20050037597 Nguyen et al. Feb 2005 A1
Foreign Referenced Citations (5)
Number Date Country
WO 0127347 Apr 2001 WO
WO 0129280 Apr 2001 WO
WO 0129893 Apr 2001 WO
WO 0166832 Sep 2001 WO
WO 2004011693 Feb 2004 WO
Related Publications (1)
Number Date Country
20040224527 A1 Nov 2004 US
Continuations (1)
Number Date Country
Parent 10222282 Aug 2002 US
Child 10863048 US