The current invention is in the field of semiconductor manufacturing. Specifically, embodiments of the current invention relate to the formation of Vertical Not-AND (V-NAND) gate devices through atomic layer deposition (ALD), chemical vapor deposition (CVD), or interfacial pretreatment before semiconductor material deposition.
V-NAND devices are logic gates that can be built in a vertical three-dimensional structure for applications such as flash memory, for example. V-NAND devices include a channel used to conduct a signal. Currently, the channel is generally made of a poly-silicon layer, often deposited by low pressure chemical vapor deposition (LPCVD).
The channel may be formed in a narrow, deep cylindrical opening, approximately 80 nm wide and 2 μm deep. The channel itself may be approximately 10 nm thick. The remainder of the cylindrical opening may be filled with Silicon Dioxide (SiO2) in what may be considered a “macaroni” structure.
Conductivity of the poly-silicon channel may depend on the length and width of the channel. As V-NAND devices become further scaled to be smaller, the channel becomes longer in length and narrower in width. As a result, a current passing through the channel decreases, leading to a reduction in speed of the V-NAND device. In addition, other factors potentially affecting the conductivity of the poly-silicon channel include the intrinsic mobility of electrons in silicon and the resistance induced by the grain boundaries in poly-silicon.
The conductivity of the channel is critical as it can directly affect the read and write speed of the V-NAND device in memory devices. The conductivity is critical due to the structure of memory devices. Currently, memory cells are formed by a poly-silicon channel on top of a tunnel dielectric, a trapping material, a blocking oxide, and a control gate. This is essentially the channel of many transistors piled on top of each other vertically. A finished vertical channel may consist of a string of transistors, for example, 32 or more transistors. Therefore, with the potential of many transistors strung vertically, the conductivity of the channel or speed will become increasingly crucial.
In typical logical devices, a single crystalline channel material is preferred. However, no viable way to fabricate a single crystalline channel in a V-NAND channel currently exists. For example, a bottom-up selective epitaxial growth may take a very long time and be very expensive to manufacture. For these reasons, a conformal LPCVD poly-silicon layer is currently used for forming V-NAND devices. As a result, a method for forming a stable channel material for use in V-NAND devices with the requisite conductivity is desired.
In accordance with one embodiment of the invention, a method of forming a channel for use in a V-NAND device is disclosed, the method comprising: providing a substrate, the substrate having an opening; depositing a semiconducting material by atomic layer deposition in the opening to form a channel layer; and filling a remaining portion of the opening with a dielectric material.
In accordance with one embodiment of the invention, a method for forming a structure is disclosed, the method comprising: providing a substrate having a surface comprising an oxide; performing a pretreatment to the oxide surface; and depositing a semiconductor material on the oxide surface after the pretreatment; wherein the pretreatment comprises a gallium compound and oxygen compound.
In accordance with one embodiment of the invention, a method of forming a channel for use in a V-NAND device is disclosed, the method comprising: providing a substrate, the substrate having an opening; pretreating a surface formed in the opening; depositing a semiconductor material by atomic layer deposition inside the opening to form a channel layer; and filling a remaining portion of the opening with a dielectric material.
In accordance with one embodiment of the invention, a method of forming a channel for use in a V-NAND device is disclosed, the method comprising: providing a substrate, the substrate having an opening; depositing a first semiconductor material by atomic layer deposition in the opening to form a channel layer; and filling a remaining portion of the opening with a second semiconductor material.
In accordance with one embodiment of the invention, a method of forming a channel for use in a V-NAND device is disclosed, the method comprising: providing a substrate, the substrate having a cylindrical opening; pretreating surfaces formed in the cylindrical opening; depositing a first III-V material inside the cylindrical opening by atomic layer deposition to form a channel layer; and filling a remaining portion of the cylindrical opening with a second semiconductor material.
In accordance with one embodiment of the invention, a method of performing pretreatment prior to depositing a channel for use in a V-NAND device is disclosed, the method comprising: performing a cyclic pretreatment process comprising pulse of a first metal reactant and a pulse of non-metal reactant; and performing a second pulse comprising a second metal reactant within an opening in which a channel is to be deposited; wherein the cyclic pretreatment process improves adhesion of a material to be deposited in the opening.
For purposes of summarizing the invention and the advantages achieved over the prior art, certain objects and advantages of the invention have been described herein above. Of course, it is to be understood that not necessarily all such objects or advantages may be achieved in accordance with any particular embodiment of the invention. Thus, for example, those skilled in the art will recognize that the invention may be embodied or carried out in a manner that achieves or optimizes one advantage or group of advantages as taught or suggested herein without necessarily achieving other objects or advantages as may be taught or suggested herein.
All of these embodiments are intended to be within the scope of the invention herein disclosed. These and other embodiments will become readily apparent to those skilled in the art from the following detailed description of certain embodiments having reference to the attached figures, the invention not being limited to any particular embodiment(s) disclosed.
These and other features, aspects, and advantages of the invention disclosed herein are described below with reference to the drawings of certain embodiments, which are intended to illustrate and not to limit the invention.
It will be appreciated that elements in the figures are illustrated for simplicity and clarity and have not necessarily been drawn to scale. For example, the dimensions of some of the elements in the figures may be exaggerated relative to other elements to help improve understanding of illustrated embodiments of the present disclosure.
Although certain embodiments and examples are disclosed below, it will be understood by those in the art that the invention extends beyond the specifically disclosed embodiments and/or uses of the invention and obvious modifications and equivalents thereof. Thus, it is intended that the scope of the invention disclosed should not be limited by the particular disclosed embodiments described below.
Embodiments of the invention relate to methods of manufacturing or treating a V-NAND device. Specifically, the methods include manufacturing a channel material or treating the channel material in order to allow for optimum performance and stability. Embodiments of the invention may take place in in batch, mini-batch, or single-wafer reactors.
The method includes a step of depositing a first material to form a channel layer 110. The first material may be a compound semiconductor material. Appropriate compound semiconductor materials may include III-V materials, II-VI materials, and IV-VI materials. The depositing step 110 may be accomplished by atomic layer deposition (ALD), chemical vapor deposition (CVD), or other cyclical deposition processes, resulting in a layer for the channel layer, which is poly-crystalline in some embodiments. ALD may provide the advantage of a highly conformal deposition in high aspect ratio structures, similar to those in V-NAND applications. The III-V materials that may be used in the depositing step 110 include: gallium arsenide (GaAs); gallium antimonide (GaSb); indium phosphide (InP); gallium nitride (GaN); indium antimonide (InSb); indium gallium arsenide (InGaAs); or a combination of aluminum, gallium, or indium with nitride, phosphide, arsenide, or antimony. In some embodiments, the III-V material may be deposited by an ALD process comprising alkylsilyl-compounds of As or Sb and/or halides, such as chlorides, of the group 13 elements, like Al, Ga and In. The II-VI material that may be used in the depositing step 110 include: zinc sulfide (ZnS), zinc selenide (ZnSe), zinc telluride (ZnTe), cadmium sulfide (CdS), cadmium telluride (CdTe), and cadmium selenide (CdSe). The IV-VI material that may be used in the depositing step 110 include: tin sulfide (SnS), silicon selenide (SiSe), germanium selenide (GeSe), tin selenide (SnSe), silicon telluride (SiTe), germanium telluride (GeTe), and tin telluride (SnTe).
Other materials that can potentially be deposited through atomic layer deposition in the depositing step 110 may include semiconducting materials, such as germanium (Ge), silicon germanium (SiGe), germanium selenide (GeSe), zinc oxide (ZnO), zinc oxynitride (ZnON), indium gallium zinc oxide (IZGO), indium tin oxide (ITO), titanium oxide (TiOx), tin selenide (SnSe), carbon nanotubes, graphene, silicon carbide (SiC), germanium tin (GeSn), diamond, tungsten sulfide (WS2), or boron nitride carbide (BNC). The applicability of these above listed materials will depend on the availability of forming processes as well as sufficiently high intrinsic mobility.
The channel layer formed in depositing step 110 may be approximately 10 nm thick. The method also includes a step of filling a remaining opening with a second material 120. Materials that may be used in the filling step 120 include silicon oxides (such as silicon dioxide, hafnium oxides, or aluminum oxides), polysilicon, or other conductive materials. Each of the steps discussed above may be repeated and ordered in different sequences in order to allow formation of a desired channel.
The method includes a step of pretreatment, such as cyclic pretreatment, to improve adhesion 210. The step of pretreating 210 may be employed to assist the adhesion of ALD grown compound semiconductor film, such as III-V material, on a surface. In other embodiments, CVD or other cyclical deposition processes may be used. For example, the surface may comprise dielectric material, such as silicon oxide based dielectrics used as a tunnel oxide in V-NAND structure, resulting in greater stability of the formed V-NAND device. The pretreating step 210 may include a first pulse of a combination of a metal reactant and a non-metal reactant. The pretreating step 210 may then include a second pulse of a metal reactant.
In one embodiment in accordance with the invention, the pretreating step 210 may include several pulses of GaCl3 and H2O before starting a deposition of III-V material, such as GaSb, onto a thermal SiO2 substrate. The deposition may also take place on a high-k material as well. A pretreating step 210 may include a first pulse of gallium trichloride (GaCl3) and water. A deposition step 220 may follow, comprising a second pulse of Sb(SiMe3)3 and GaCl3. The first pulse or the second pulse may be repeated as necessary. Typical pulse lengths may range from about 0.05 to 20 seconds, from about 0.1 to 5 seconds, or from about 0.2 to 2 seconds. However, other pulse lengths may be utilized if necessary, such as where highly conformal step coverage over extremely high aspect ratio structures or structures having high surface area or other structures with complex surface morphology is needed or in case of batch reactors. Similarly, typical removal/purge times are from about 0.05 to 20 seconds, from about 0.5 to 10 seconds, or from about 1 to 5 seconds. However, other removal/purge times may be utilized if necessary, such as where highly conformal step coverage over extremely high aspect ratio structures or structures having high surface area or other structures with complex surface morphology is needed or in case of batch reactors.
Chemicals that may be used as a metal reactant for the first pulse of the pretreating step 210 include metal compounds. The metal compounds may include metal-organics or organometallic compounds, such as: metal-organic or organometallic compounds of group 13 or group 15 elements; metal-organic or organometallic compounds of gallium or antimony; or metal halides such as metal chlorides, semi-metal halides, semi-metal chlorides, gallium trichloride (GaCl3), and other gallium halides. Chemicals that may be used as a non-metal reactant for the second pulse of the pretreating step 210 include oxygen-containing reactants, such as H2O, H2O2, O3, and plasmas and radicals incorporating oxygen. Other non-metal reactants may include chemicals with a hydroxide group and others. The first and second pulses of the pretreating step 210 may be performed in any order. In some embodiments, the pretreating step 210 may deposit a material, such as Ga2O3, onto the substrate. In some embodiments, the pretreating step 210 may not deposit a substantial amount or a film of material, such as Ga2O3, onto the substrate. In some embodiments, the temperature of the pretreating step 210 is from about 20 to about 500° C., from about 40 to about 250° C., from about 50 to about 150° C., or from about 60 to about 130° C. In some embodiments, the temperature of the pretreating step 210 may be substantially the same as the temperature of the depositing step 220. In some embodiments, the temperature of the pretreating step 210 may be within less than a difference of about 100° C., within less than a difference of about 50° C., or within less than a difference of 20° C. from the temperature of the depositing step 220.
The method includes a step of depositing a first material to form a channel layer 220. The first material may comprise a compound semiconductor material. Appropriate compound semiconductor materials may include III-V materials, II-VI materials, and IV-VI materials. The depositing step 220 may be accomplished by atomic layer deposition (ALD), resulting in a layer for the channel layer, which in some embodiments is poly-crystalline. ALD may provide the advantage of a highly conformal deposition in high aspect ratio structures, similar to those in V-NAND applications. In other embodiments, CVD or other cyclical deposition processes may be used. The III-V materials that may be used in the depositing step 220 include: gallium arsenide (GaAs); gallium antimonide (GaSb); indium phosphide (InP); gallium nitride (GaN); indium antimonide (InSb); indium gallium arsenide (InGaAs); or a combination of aluminum, gallium, or indium with nitride, phosphide, arsenide, or antimony. In some embodiments, the III-V material is deposited by a deposition process comprising alkylsilyl-compounds of As or Sb and/or halides, such as chlorides, of the group 13 elements, like Al, Ga and In. The II-VI material that may be used in the depositing step 220 include: zinc sulfide (ZnS), zinc selenide (ZnSe), zinc telluride (ZnTe), cadmium sulfide (CdS), cadmium telluride (CdTe), and cadmium selenide (CdSe). The IV-VI material that may be used in the depositing step 220 include: tin sulfide (SnS), silicon selenide (SiSe), germanium selenide (GeSe), tin selenide (SnSe), silicon telluride (SiTe), germanium telluride (GeTe), and tin telluride (SnTe).
Other materials that can potentially be deposited in the depositing step 220 may include germanium (Ge), silicon germanium (SiGe), zinc oxide (ZnO), zinc oxynitride (ZnON), indium gallium zinc oxide (IZGO), indium tin oxide (ITO), titanium oxide (TiOx), carbon nanotubes, graphene, silicon carbide (SiC), germanium tin (GeSn), germanium selenide (GeSe), tin selenide (SnSe), diamond, tungsten sulfide (WS2), or boron nitride carbide (BNC). The applicability of these above listed materials will depend on the availability of forming processes as well as sufficiently high intrinsic mobility.
The channel layer formed in depositing step 220 may be approximately 10 nm thick. The method also includes a step of filling a remaining opening with a second material 230. The second material in the filling step 230 may include silicon oxides (such as silicon dioxide, hafnium oxides, or aluminum oxides), polysilicon, or other conductive materials. Each of the steps discussed above may be repeated and ordered in different sequences in order to allow formation of a desired channel.
The method includes a step of depositing a first material to form a channel layer 310. The first material may be a compound semiconductor material. Appropriate compound semiconductor materials may include III-V materials, II-VI materials, and IV-VI materials. The depositing step 310 may be accomplished by atomic layer deposition (ALD), resulting in a layer for the channel layer, which in some embodiments is poly-crystalline. ALD may provide the advantage of a highly conformal deposition in high aspect ratio structures, similar to those in V-NAND applications. In other embodiments, CVD or other cyclical deposition processes may be used. The III-V materials that may be used in the depositing step 310 include: gallium arsenide (GaAs); gallium antimonide (GaSb); indium phosphide (InP); gallium nitride (GaN); indium antimonide (InSb); indium gallium arsenide (InGaAs); or a combination of aluminum, gallium, or indium with nitride, phosphide, arsenide, or antimony. In some embodiments, the III-V material is deposited by an ALD process comprising alkylsilyl-compounds of As or Sb and/or halides, such as chlorides, of the group 13 elements, like Al, Ga and In. The II-VI material that may be used in the depositing step 310 include: zinc sulfide (ZnS), zinc selenide (ZnSe), zinc telluride (ZnTe), cadmium sulfide (CdS), cadmium telluride (CdTe), and cadmium selenide (CdSe). The IV-VI material that may be used in the depositing step 310 include: tin sulfide (SnS), silicon selenide (SiSe), germanium selenide (GeSe), tin selenide (SnSe), silicon telluride (SiTe), germanium telluride (GeTe), and tin telluride (SnTe).
Other materials that can potentially be deposited in the depositing step 310 may include germanium (Ge), silicon germanium (SiGe), zinc oxide (ZnO), zinc oxynitride (ZnON), indium gallium zinc oxide (IZGO), indium tin oxide (ITO), titanium oxide (TiOx), carbon nanotubes, graphene, silicon carbide (SiC), germanium tin (GeSn), germanium selenide (GeSe), tin selenide (SnSe), diamond, tungsten sulfide (WS2), or boron nitride carbide (BNC). The applicability of these above listed materials will depend on the availability of forming processes as well as sufficiently high intrinsic mobility.
The channel layer formed in depositing step 310 may be approximately 10 nm thick. The method also includes a step of filling a remaining opening with a second material, for example compound semiconductor material, like II-VI or III-V material 320. In some embodiments, the III-V material used in the filling step 320 may likely be different than the III-V material deposited in depositing step 310. In other embodiments, the III-V material used in the filling step 320 may be the same as the III-V material deposited in depositing step 310. Suitability of the material used in the filling step 320 may depend on the conductivity, band gap (either a higher, lower, or approximately same band gap), ability to integrate with dielectrics and/or III-V material of depositing step 310, electron and/or hole mobility, charge carrier density, and electron effective mass of the III-V materials. Each of the steps discussed above may be repeated and ordered in different sequences in order to allow formation of a desired channel.
The method includes a step of pretreating to improve adhesion 410. The step of pretreating 410 may be employed to assist the adhesion of ALD grown compound semiconductor film, such as III-V material, on a dielectric, such as silicon oxide based dielectrics used as a tunnel oxide in V-NAND structure, resulting in greater stability of the formed V-NAND device. In other embodiments, a CVD or other cyclical deposition process may be used. The pretreating step 410 may include a first pulse of a combination of a metal reactant and a non-metal reactant. The pretreating step 410 may then include a second pulse of a metal reactant.
In one embodiment in accordance with the invention, the pretreating step 410 may include several pulses of GaCl3 and H2O before starting a deposition of III-V material, such as GaSb, onto a thermal SiO2 substrate. A pretreating step 410 may include a first pulse of gallium trichloride (GaCl3) and water. A deposition step 420 may follow, comprising a second pulse of Sb(SiMe3)3 and GaCl3. The first pulse or the second pulse may be repeated as necessary. Typical pulse lengths may range from about 0.05 to 20 seconds, from about 0.1 to 5 seconds, or from about 0.2 to 2 seconds. However, other pulse lengths may be utilized if necessary, such as where highly conformal step coverage over extremely high aspect ratio structures or structures having high surface area or other structures with complex surface morphology is needed or in case of batch reactors. Similarly, typical removal/purge times are from about 0.05 to 20 seconds, from about 0.5 to 10 seconds, or from about 1 to 5 seconds. However, other removal/purge times may be utilized if necessary, such as where highly conformal step coverage over extremely high aspect ratio structures or structures having high surface area or other structures with complex surface morphology is needed or in case of batch reactors.
Chemicals that may be used as a metal reactant for the first pulse of the pretreating step 410 include metal compounds. The metal compounds may include metal-organics or organometallic compounds, such as: metal-organic or organometallic compounds of group 13 or group 15 elements; metal-organic or organometallic compounds of gallium or antimony; or metal halides such as metal chlorides, semi-metal halides, semi-metal chlorides, gallium trichloride (GaCl3), and other gallium halides. Chemicals that may be used as a non-metal reactant for the second pulse of the pretreating step 410 include oxygen-containing reactants, such as H2O, H2O2, O3, and plasmas and radicals incorporating oxygen. Other non-metal reactants may include chemicals with a hydroxide group and others. The first and second pulses of the pretreating step 410 may be performed in any order.
In some embodiments, the pretreating step 410 may deposit a material, such as Ga2O3, onto the substrate. In some embodiments, the pretreating step 410 may not deposit a substantial amount or a film of material, such as Ga2O3, onto the substrate. In some embodiments, the temperature of the pretreating step 410 is from about 20 to about 500° C., from about 40 to about 250° C., from about 50 to about 150° C., or from about 60 to about 130° C. In some embodiments, the temperature of the pretreating step 410 may be substantially the same as the temperature of the depositing step 420. In some embodiments, the temperature of the pretreating step 410 may be within less than a difference of about 100° C., within less than a difference of about 50° C., or within less than a difference of 20° C. from the temperature of the depositing step 420.
The method includes a step of depositing compound semiconductor materials to form a channel layer 420. Appropriate compound semiconductor materials may include III-V materials, II-VI materials, and IV-VI materials. The depositing step 420 may be accomplished by atomic layer deposition (ALD), resulting in a layer for the channel layer, which in some embodiments is poly-crystalline. ALD may provide the advantage of a highly conformal deposition in high aspect ratio structures, similar to those in V-NAND applications. In other embodiments, CVD or other cyclical deposition process may be used. The III-V materials that may be used in the depositing step 420 include: gallium antimonide (GaSb), gallium arsenide (GaAs); indium phosphide (InP); gallium nitride (GaN); indium antimonide (InSb); indium gallium arsenide (InGaAs); or a combination of aluminum, gallium, or indium with nitride, phosphide, arsenide, or antimony. In some embodiments, the III-V material is deposited by an ALD process comprising alkylsilyl-compounds of As or Sb and/or halides, such as chlorides, of the group 13 elements, like Al, Ga and In. The II-VI material that may be used in the depositing step 420 include: zinc sulfide (ZnS), zinc selenide (ZnSe), zinc telluride (ZnTe), cadmium sulfide (CdS), cadmium telluride (CdTe), and cadmium selenide (CdSe). The IV-VI material that may be used in the depositing step 420 include: tin sulfide (SnS), silicon selenide (SiSe), germanium selenide (GeSe), tin selenide (SnSe), silicon telluride (SiTe), germanium telluride (GeTe), and tin telluride (SnTe).
Other materials that can potentially be deposited in the depositing step 420 may include germanium (Ge), silicon germanium (SiGe), zinc oxide (ZnO), zinc oxynitride (ZnON), indium gallium zinc oxide (IZGO), indium tin oxide (ITO), titanium oxide (TiOx), carbon nanotubes, graphene, silicon carbide (SiC), germanium tin (GeSn), germanium selenide (GeSe), tin selenide (SnSe), diamond, tungsten sulfide (WS2), or boron nitride carbide (BNC). The applicability of these above listed materials will depend on the availability of forming processes as well as sufficiently high intrinsic mobility.
The channel layer formed in depositing step 420 may be approximately 10 nm thick. The method also includes a step of filling a remaining opening with additional semiconductor material, for example compound semiconductor material, like II-VI, III-V material, or IV-VI material 420. In some embodiments, the III-V material used in the filling step 420 may likely be different than the III-V material deposited in depositing step 410. In other embodiments, the III-V material used in the filling step 420 may be the same as the III-V material deposited in depositing step 410. Suitability of the material used in the filling step 420 may depend on the conductivity, band gap (either a higher, lower, or approximately same band gap), ability to integrate with dielectrics and/or III-V material of depositing step 410, electron and/or hole mobility, charge carrier density, and electron effective mass of the III-V materials. Each of the steps discussed above may be repeated and ordered in different sequences in order to allow formation of a desired channel.
The silicon oxide surface of step 500 may have hydroxyl (—OH) groups. As a result, the halide precursor of step 510 may convert the hydroxyl groups into Si—Cl bonds. The halide precursor of step 510 may comprise carbon tetrachloride (CCl4) or trichloromethane (CHCl3). The halide precursor of step 510 may also comprise a chemistry having a formula of CX4 or CHaX4-a, where X is a halide such as F, Cl, or Br, for example. The halide precursor of step 510 may comprise at least one of: Cl, Cl2, HCl, radicals, excited species, or plasmas comprising halides, such as chlorine.
The halide precursor pretreatment step 510 may comprise multiple cycles of exposure to the halide precursor, exceeding 10 cycles, 50 cycles, 100 cycles, 150 cycles, 200 cycles, or 250 cycles. The halide precursor pretreatment step 510 may involve exposures ranging between 0.1 and 10 seconds, between 1 and 8 seconds, or between 3 and 7 seconds, for those reactions occurring in a mini-batch or a single wafer reactor. In some embodiments, for example in batch reactors, the exposure and purge and other times may be longer.
The halide precursor pretreatment step 510 may also comprise a pre-stabilization lasting between 2 and 10 minutes. The pre-stabilization comprises waiting in the reactor before deposition of the precursors in steps 520 and 530. The benefits achieved from the pre-stabilization may include complete adhesion of the films and avoidance of any delamination. In addition, the halide precursor pretreatment step may occur at temperatures less than 500° C., less than 450° C., less than 400° C., or less than 350° C.
The alkyl-silyl compound precursor of step 520 may then react with the Si—Cl bonds. The step 520 may require a higher temperature exceeding approximately 100° C. in order to react with the alkyl-silyl compound precursor. The alkyl-silyl compound precursor may comprise alkylsilyl-compounds of As or Sb, such as Sb(SiMe3)3, for example. In addition, the alkyl-silyl compound precursor step may occur at temperatures less than 150° C., less than 130° C., less than 115° C., or less than 105° C.
After deposition of the alkyl-silyl compound precursor, a deposition of a metal halide precursor 520 may take place in order to form a III-V material. The metal halide precursor in step 520 may comprise halides, such as chlorides, of the group 13 elements, like Al, Ga and In. An example of the metal halide precursor in step 520 may be gallium trichloride (GaCl3). The III-V material formed may comprise: gallium antimonide (GaSb); gallium arsenide (GaAs); indium phosphide (InP); gallium nitride (GaN); indium antimonide (InSb); indium gallium arsenide (InGaAs); or a combination of aluminum, gallium, or indium with nitride, phosphide, arsenide, or antimony. In addition, the metal halide precursor step may occur at temperatures less than 150° C., less than 130° C., less than 115° C., or less than 105° C.
In some embodiments, a deposited compound semiconductor material may have a conformality greater than about 50%, greater than about 80%, greater than about 90%, greater than about 95%, greater than about 98%, or greater than about 99%. The deposited compound semiconductor material may have an aspect ratios (depth:width) of more than about 2, more than about 5, more than about 10, more than about 20, or in some instances even more than about 40, or more than about 80. It may be noted that aspect ratio may be difficult to determine for the V-NAND structures, but in this context, the aspect ratio could be understood to be the ratio of the total surface area of the structures in the wafer (or part of the wafer) in relation to the planar surface area of wafer (or part of the wafer).
In some embodiments, the reaction temperature for the deposition of the compound semiconductor material film (such as III-V material, like GaSb or GaAs, II-VI material, or a IV-VI material) may be less than about 700° C., may be less than about 500° C., less than about 400° C., less than about 300° C., less than about 200° C., or less than about 150° C.
In some embodiments, the growth rate of the deposited compound semiconductor materials may be less than about 3 Å/cycle, less than about 2 Å/cycle, less than about 1.5 Å/cycle, or less than about 1 Å/cycle. In some embodiments, the growth rate of the deposited compound semiconductor materials may range from about 0.05 Å/cycle to about 2 Å/cycle, or about 0.1 Å/cycle to about 1.5 Å/cycle.
In some embodiments, the compound semiconductor material may have impurities (i.e., other than materials in the compound semiconductor material itself) of less than about 20 at-%, less than about 10 at-%, less than about 5 at-%, or less than about 3 at-%. In some embodiments, the compound semiconductor materials may have halide impurities, such as chlorine, of less than about 5 at-%, less than about 2 at-%, less than about 1 at-%, or less than about 0.5 at-%. In some embodiments, the compound semiconductor materials may have hydrogen impurities of less than about 25 at-%, less than about 15 at-%, less than about 10 at-%, or less than about 5 at-%. In some embodiments, the compound semiconductor material may have silicon impurities of less than about 5 at-%, less than about 2 at-%, less than about 1 at-%, or less than about 0.5 at-%. In some embodiments, the compound semiconductor materials has carbon impurities, less than about 5 at-%, less than about 2 at-%, less than about 1 at-%, or less than about 0.5 at-%.
The examples set forth below are illustrative of various aspects of certain embodiments of the disclosure. The methods and various parameters reflected therein are intended only to exemplify various aspects and embodiments of the disclosure, and are not intended to limit the scope of the claimed invention.
The particular implementations shown and described are illustrative of the invention and its best mode and are not intended to otherwise limit the scope of the aspects and implementations in any way. Indeed, for the sake of brevity, conventional manufacturing, connection, preparation, and other functional aspects of the system may not be described in detail. Furthermore, the connecting lines shown in the various figures are intended to represent exemplary functional relationships and/or physical couplings between the various elements. Many alternative or additional functional relationship or physical connections may be present in the practical system, and/or may be absent in some embodiments.
It is to be understood that the configurations and/or approaches described herein are exemplary in nature, and that these specific embodiments or examples are not to be considered in a limiting sense, because numerous variations are possible. The specific routines or methods described herein may represent one or more of any number of processing strategies. Thus, the various acts illustrated may be performed in the sequence illustrated, in other sequences, or omitted in some cases.
The subject matter of the present disclosure includes all novel and nonobvious combinations and subcombinations of the various processes, systems, and configurations, and other features, functions, acts, and/or properties disclosed herein, as well as any and all equivalents thereof.
This application claims the benefit and priority of Provisional Application No. 62/272,345, filed on Dec. 29, 2015, entitled ATOMIC LAYER DEPOSITION OF III-V COMPOUNDS TO FORM V-NAND DEVICES, the contents of which are hereby incorporated by reference to the extent the contents do not conflict with the present disclosure.
Number | Name | Date | Kind |
---|---|---|---|
D30036 | Rhind | Jan 1899 | S |
D31889 | Gill | Nov 1899 | S |
D56051 | Cohn | Aug 1920 | S |
2059480 | Obermaier | Nov 1936 | A |
2161626 | Loughner et al. | Jun 1939 | A |
2240163 | Pick | Apr 1941 | A |
2266416 | Duclos | Dec 1941 | A |
2280778 | Anderson | Apr 1942 | A |
D142841 | D'Algodt | Nov 1945 | S |
2410420 | Bennett | Nov 1946 | A |
2441253 | Sarver | May 1948 | A |
2480557 | Cummins | Aug 1949 | A |
2563931 | Harrison | Aug 1951 | A |
2660061 | Lewis | Nov 1953 | A |
2745640 | Cushman | May 1956 | A |
2847320 | Bulloff | Aug 1958 | A |
2990045 | Root | Sep 1959 | A |
3038951 | Mead | Jun 1962 | A |
3089507 | Drake et al. | May 1963 | A |
3094396 | Flugge et al. | Jun 1963 | A |
3232437 | Hultgren | Feb 1966 | A |
3263502 | Springfield | Aug 1966 | A |
3332286 | Strong | Jul 1967 | A |
3410349 | Troutman | Nov 1968 | A |
3420622 | Donges et al. | Jan 1969 | A |
3588192 | Drutchas et al. | Jun 1971 | A |
3647387 | Benson | Mar 1972 | A |
3647716 | Koches | Mar 1972 | A |
3713899 | Sebestyen | Jan 1973 | A |
3718429 | Williamson | Feb 1973 | A |
3796182 | Rosler | Mar 1974 | A |
3814128 | Grantham | Jun 1974 | A |
3833492 | Bollyky | Sep 1974 | A |
3854443 | Baerg | Dec 1974 | A |
3862397 | Anderson et al. | Jan 1975 | A |
3867205 | Schley | Feb 1975 | A |
3885504 | Baermann | May 1975 | A |
3887790 | Ferguson | Jun 1975 | A |
3904371 | Neti | Sep 1975 | A |
3913058 | Nishio et al. | Oct 1975 | A |
3913617 | van Laar | Oct 1975 | A |
3947685 | Meinel | Mar 1976 | A |
3960559 | Suzuki | Jun 1976 | A |
3962004 | Sonneborn | Jun 1976 | A |
3997638 | Manning et al. | Dec 1976 | A |
4048110 | Vanderspurt | Sep 1977 | A |
4054071 | Patejak | Oct 1977 | A |
4058430 | Suntola et al. | Nov 1977 | A |
4079944 | Durley et al. | Mar 1978 | A |
4093491 | Whelpton et al. | Jun 1978 | A |
D249341 | Mertz | Sep 1978 | S |
4126027 | Smith et al. | Nov 1978 | A |
4134425 | Gussefeld et al. | Jan 1979 | A |
4145699 | Hu et al. | Mar 1979 | A |
4149237 | Freitas | Apr 1979 | A |
4152760 | Freitas et al. | May 1979 | A |
4157751 | Grundken et al. | Jun 1979 | A |
4164959 | Wurzburger | Aug 1979 | A |
4176630 | Elmer | Dec 1979 | A |
4179530 | Koppl et al. | Dec 1979 | A |
4181330 | Kojima | Jan 1980 | A |
4194536 | Stine et al. | Mar 1980 | A |
4217463 | Swearingen | Aug 1980 | A |
4229064 | Vetter et al. | Oct 1980 | A |
4234449 | Wolson et al. | Nov 1980 | A |
4314763 | Steigmeier et al. | Feb 1982 | A |
4322592 | Martin | Mar 1982 | A |
4324611 | Vogel et al. | Apr 1982 | A |
4333735 | Hardy | Jun 1982 | A |
4355912 | Haak | Oct 1982 | A |
4389973 | Suntola et al. | Jun 1983 | A |
D269850 | Preisler et al. | Jul 1983 | S |
4393013 | McMenamin | Jul 1983 | A |
4401507 | Engle | Aug 1983 | A |
4413022 | Suntola et al. | Nov 1983 | A |
4414492 | Hanlet | Nov 1983 | A |
4436674 | McMenamin | Mar 1984 | A |
4444990 | Villar | Apr 1984 | A |
D274122 | Stahel et al. | Jun 1984 | S |
4454370 | Voznick | Jun 1984 | A |
4455193 | Jeuch et al. | Jun 1984 | A |
4465716 | Baber et al. | Aug 1984 | A |
4466766 | Geren et al. | Aug 1984 | A |
4479831 | Sandow | Oct 1984 | A |
4484061 | Zelinka et al. | Nov 1984 | A |
4488506 | Heinecke et al. | Dec 1984 | A |
4495024 | Bok | Jan 1985 | A |
4499354 | Hill et al. | Feb 1985 | A |
4504439 | Elter et al. | Mar 1985 | A |
4512113 | Budinger | Apr 1985 | A |
4512841 | Cunningham et al. | Apr 1985 | A |
4527005 | McKelvey et al. | Jul 1985 | A |
4534816 | Chen et al. | Aug 1985 | A |
4537001 | Uppstrom | Aug 1985 | A |
4548688 | Mathews | Oct 1985 | A |
4560590 | Bok | Dec 1985 | A |
4570328 | Price et al. | Feb 1986 | A |
4575408 | Bok | Mar 1986 | A |
4575636 | Caprari | Mar 1986 | A |
4578560 | Tanaka et al. | Mar 1986 | A |
4579080 | Martin et al. | Apr 1986 | A |
4579378 | Snyders | Apr 1986 | A |
4579623 | Suzuki et al. | Apr 1986 | A |
4581520 | Vu et al. | Apr 1986 | A |
4590326 | Woldy | May 1986 | A |
4611966 | Johnson | Sep 1986 | A |
4620998 | Lalvani | Nov 1986 | A |
4622918 | Bok | Nov 1986 | A |
4624728 | Bithell et al. | Nov 1986 | A |
D288556 | Wallgren | Mar 1987 | S |
4653541 | Oehlschlaeger et al. | Mar 1987 | A |
4654226 | Jackson et al. | Mar 1987 | A |
4655592 | Allemand | Apr 1987 | A |
4662987 | Bok | May 1987 | A |
4664769 | Cuomo et al. | May 1987 | A |
4670126 | Messer et al. | Jun 1987 | A |
4681134 | Paris | Jul 1987 | A |
4693211 | Ogami et al. | Sep 1987 | A |
4707815 | Yamasaki | Nov 1987 | A |
4717461 | Strahl et al. | Jan 1988 | A |
4718637 | Contin | Jan 1988 | A |
4720407 | Sculke | Jan 1988 | A |
4721533 | Phillippi et al. | Jan 1988 | A |
4721534 | Phillippi et al. | Jan 1988 | A |
4722298 | Rubin et al. | Feb 1988 | A |
4724272 | Raniere et al. | Feb 1988 | A |
4725204 | Powell | Feb 1988 | A |
4735259 | Vincent | Apr 1988 | A |
4738618 | Massey et al. | Apr 1988 | A |
4738748 | Kisa | Apr 1988 | A |
4747367 | Posa | May 1988 | A |
4749416 | Greenspan | Jun 1988 | A |
4750520 | Heim et al. | Jun 1988 | A |
4753192 | Goldsmith et al. | Jun 1988 | A |
4753856 | Haluska et al. | Jun 1988 | A |
4756794 | Yoder | Jul 1988 | A |
4764076 | Layman et al. | Aug 1988 | A |
4770590 | Hugues et al. | Sep 1988 | A |
4771015 | Kanai | Sep 1988 | A |
4775281 | Prentakis | Oct 1988 | A |
4776744 | Stonestreet et al. | Oct 1988 | A |
4780169 | Stark et al. | Oct 1988 | A |
4781511 | Harada et al. | Nov 1988 | A |
4789294 | Sato et al. | Dec 1988 | A |
4790258 | Drage et al. | Dec 1988 | A |
4802441 | Waugh | Feb 1989 | A |
4808387 | Datta et al. | Feb 1989 | A |
4812201 | Sakai et al. | Mar 1989 | A |
4812217 | George et al. | Mar 1989 | A |
4821674 | deBoer et al. | Apr 1989 | A |
4827430 | Aid et al. | May 1989 | A |
4828224 | Crabb et al. | May 1989 | A |
4830515 | Cortes | May 1989 | A |
4837113 | Luttmer et al. | Jun 1989 | A |
4837185 | Yau et al. | Jun 1989 | A |
4854263 | Chang et al. | Aug 1989 | A |
4854266 | Simson et al. | Aug 1989 | A |
4857137 | Tachi et al. | Aug 1989 | A |
4857382 | Liu et al. | Aug 1989 | A |
4858557 | Pozzetti et al. | Aug 1989 | A |
4863374 | Vukovich | Sep 1989 | A |
4867629 | Iwasawa et al. | Sep 1989 | A |
4871523 | Datta et al. | Oct 1989 | A |
4874273 | Tokisue et al. | Oct 1989 | A |
4882199 | Sadoway et al. | Nov 1989 | A |
4916091 | Freeman et al. | Apr 1990 | A |
4917556 | Stark et al. | Apr 1990 | A |
4920918 | Adams et al. | May 1990 | A |
4925388 | Iseki et al. | May 1990 | A |
4934831 | Volbrecht | Jun 1990 | A |
4938815 | McNeilly | Jul 1990 | A |
D309702 | Hall | Aug 1990 | S |
4949848 | Kos | Aug 1990 | A |
4950624 | Inuzima et al. | Aug 1990 | A |
4956538 | Moslehi | Sep 1990 | A |
4958061 | Wakabayashi et al. | Sep 1990 | A |
D311126 | Crowley | Oct 1990 | S |
4962063 | Maydan et al. | Oct 1990 | A |
4976996 | Monkowski et al. | Dec 1990 | A |
4978567 | Miller | Dec 1990 | A |
4984904 | Nakano et al. | Jan 1991 | A |
4985114 | Okudaira | Jan 1991 | A |
4986215 | Yamada | Jan 1991 | A |
4987102 | Nguyen et al. | Jan 1991 | A |
4987856 | Hey | Jan 1991 | A |
4989992 | Piai | Feb 1991 | A |
4991614 | Hammel | Feb 1991 | A |
5002632 | Loewenstein et al. | Mar 1991 | A |
5013691 | Lory et al. | May 1991 | A |
5022961 | Izumi et al. | Jun 1991 | A |
5027746 | Frijlink | Jul 1991 | A |
5028366 | Harakal et al. | Jul 1991 | A |
D320148 | Andrews | Sep 1991 | S |
5049029 | Mitsui et al. | Sep 1991 | A |
5053247 | Moore | Oct 1991 | A |
5057436 | Ball | Oct 1991 | A |
5060322 | Delepine | Oct 1991 | A |
5061083 | Grimm et al. | Oct 1991 | A |
5062386 | Christensen | Nov 1991 | A |
5064337 | Asakawa et al. | Nov 1991 | A |
5065698 | Koike | Nov 1991 | A |
5067437 | Watanabe et al. | Nov 1991 | A |
5069591 | Kinoshita | Dec 1991 | A |
5071258 | Usher et al. | Dec 1991 | A |
5074017 | Toya et al. | Dec 1991 | A |
5082517 | Moslehi | Jan 1992 | A |
5084126 | McKee | Jan 1992 | A |
5088444 | Ohmine et al. | Feb 1992 | A |
5097890 | Nakao | Mar 1992 | A |
5098638 | Sawada | Mar 1992 | A |
5098865 | Machado | Mar 1992 | A |
5104514 | Quartarone | Apr 1992 | A |
5107170 | Ishikawa et al. | Apr 1992 | A |
5108192 | Mailliet et al. | Apr 1992 | A |
5110407 | Ono et al. | May 1992 | A |
5114683 | Hirase | May 1992 | A |
5116018 | Friemoth et al. | May 1992 | A |
D327534 | Manville | Jun 1992 | S |
5119760 | McMillan et al. | Jun 1992 | A |
5125358 | Ueda et al. | Jun 1992 | A |
5130003 | Conrad | Jul 1992 | A |
5134965 | Tokuda et al. | Aug 1992 | A |
5137286 | Whitford | Aug 1992 | A |
5151296 | Tokunaga | Sep 1992 | A |
5154301 | Kos | Oct 1992 | A |
5158128 | Inoue et al. | Oct 1992 | A |
D330900 | Wakegijig | Nov 1992 | S |
5167716 | Boitnott et al. | Dec 1992 | A |
5167761 | Westendorp et al. | Dec 1992 | A |
5174881 | Iwasaki et al. | Dec 1992 | A |
5176451 | Sasada | Jan 1993 | A |
5178639 | Nishi | Jan 1993 | A |
5178682 | Tsukamoto et al. | Jan 1993 | A |
5180273 | Sakaya et al. | Jan 1993 | A |
5180435 | Markunas et al. | Jan 1993 | A |
5181779 | Shia et al. | Jan 1993 | A |
5182232 | Chhabra et al. | Jan 1993 | A |
5183511 | Yamazaki et al. | Feb 1993 | A |
D333606 | Kanemitsu et al. | Mar 1993 | S |
5192717 | Kawakami | Mar 1993 | A |
5193912 | Saunders | Mar 1993 | A |
5193969 | Rush et al. | Mar 1993 | A |
5194401 | Adams et al. | Mar 1993 | A |
5199603 | Prescott | Apr 1993 | A |
5213650 | Wang et al. | May 1993 | A |
5221556 | Hawkins et al. | Jun 1993 | A |
5225366 | Yoder et al. | Jul 1993 | A |
5226383 | Bhat | Jul 1993 | A |
5226713 | Matsumura | Jul 1993 | A |
5226967 | Chen et al. | Jul 1993 | A |
5228114 | Suzuki | Jul 1993 | A |
5232508 | Arena et al. | Aug 1993 | A |
5234526 | Chen et al. | Aug 1993 | A |
5242539 | Kumihashi et al. | Sep 1993 | A |
5243195 | Nishi | Sep 1993 | A |
5243202 | Mori et al. | Sep 1993 | A |
5246218 | Yap et al. | Sep 1993 | A |
5246500 | Samata et al. | Sep 1993 | A |
5249960 | Monoe | Oct 1993 | A |
5259881 | Edwards et al. | Nov 1993 | A |
5261167 | Sakata | Nov 1993 | A |
5266526 | Aoyama | Nov 1993 | A |
5268989 | Moslehi et al. | Dec 1993 | A |
5271967 | Kramer et al. | Dec 1993 | A |
5273609 | Moslehi | Dec 1993 | A |
5277932 | Spencer | Jan 1994 | A |
5278494 | Obigane | Jan 1994 | A |
5279886 | Kawai et al. | Jan 1994 | A |
5279986 | Maloney et al. | Jan 1994 | A |
5281274 | Yoder | Jan 1994 | A |
5284519 | Gadgil | Feb 1994 | A |
5288684 | Yamazaki et al. | Feb 1994 | A |
5294572 | Granneman et al. | Mar 1994 | A |
5294778 | Carman et al. | Mar 1994 | A |
5305417 | Najm et al. | Apr 1994 | A |
5306666 | Izumi | Apr 1994 | A |
5306946 | Yamamoto | Apr 1994 | A |
5308650 | Krummel et al. | May 1994 | A |
5310456 | Kadomura | May 1994 | A |
5312245 | Brannen et al. | May 1994 | A |
5313061 | Drew et al. | May 1994 | A |
5314538 | Maeda et al. | May 1994 | A |
5314570 | Ikegaya et al. | May 1994 | A |
5315092 | Takahashi et al. | May 1994 | A |
5320218 | Yamashita et al. | Jun 1994 | A |
5326427 | Jerbic | Jul 1994 | A |
5328810 | Lowrey et al. | Jul 1994 | A |
5335309 | Fujii et al. | Aug 1994 | A |
5336327 | Lee | Aug 1994 | A |
5338362 | Imahashi | Aug 1994 | A |
5340261 | Oosawa et al. | Aug 1994 | A |
5346961 | Shaw et al. | Sep 1994 | A |
5348774 | Golecki et al. | Sep 1994 | A |
5350480 | Gray | Sep 1994 | A |
5354433 | Granneman et al. | Oct 1994 | A |
5354580 | Goela et al. | Oct 1994 | A |
5356478 | Chen et al. | Oct 1994 | A |
5356672 | Schmitt et al. | Oct 1994 | A |
5360269 | Ogawa et al. | Nov 1994 | A |
5364667 | Rhieu | Nov 1994 | A |
D353452 | Groenhoff | Dec 1994 | S |
5374315 | Deboer et al. | Dec 1994 | A |
D354898 | Nagy | Jan 1995 | S |
5380367 | Bertone | Jan 1995 | A |
5382311 | Ishikawa et al. | Jan 1995 | A |
5387265 | Kakizaki et al. | Feb 1995 | A |
5388945 | Garric et al. | Feb 1995 | A |
5393577 | Uesugi et al. | Feb 1995 | A |
5397395 | Sano et al. | Mar 1995 | A |
5403630 | Matsui et al. | Apr 1995 | A |
5404082 | Hernandez et al. | Apr 1995 | A |
5407449 | Zinger | Apr 1995 | A |
5407867 | Iwasaki et al. | Apr 1995 | A |
5413813 | Cruse et al. | May 1995 | A |
5414221 | Gardner | May 1995 | A |
5415753 | Hurwitt et al. | May 1995 | A |
5418382 | Blackwood et al. | May 1995 | A |
5421893 | Perlov | Jun 1995 | A |
5422139 | Fischer | Jun 1995 | A |
5423942 | Robbins et al. | Jun 1995 | A |
5426137 | Allen | Jun 1995 | A |
5427824 | Inushima et al. | Jun 1995 | A |
5430011 | Tanaka et al. | Jul 1995 | A |
5431734 | Chapple-Sokol et al. | Jul 1995 | A |
5443646 | Yamada et al. | Aug 1995 | A |
5443648 | Ohkase | Aug 1995 | A |
5443686 | Jones et al. | Aug 1995 | A |
5444217 | Moore | Aug 1995 | A |
5447294 | Sakata et al. | Sep 1995 | A |
5453124 | Moslehi et al. | Sep 1995 | A |
D363464 | Fukasawa | Oct 1995 | S |
5456207 | Gedridge et al. | Oct 1995 | A |
5461214 | Peck et al. | Oct 1995 | A |
5462899 | Ikeda | Oct 1995 | A |
5463176 | Eckert | Oct 1995 | A |
5464313 | Ohsawa | Nov 1995 | A |
5474410 | Ozawa et al. | Dec 1995 | A |
5474612 | Sato et al. | Dec 1995 | A |
5480488 | Bittner et al. | Jan 1996 | A |
5480818 | Matsumoto et al. | Jan 1996 | A |
5482559 | Imai et al. | Jan 1996 | A |
5484484 | Yamaga et al. | Jan 1996 | A |
5494439 | Goldstein et al. | Feb 1996 | A |
5494494 | Mizuno et al. | Feb 1996 | A |
5496408 | Motoda et al. | Mar 1996 | A |
5501740 | Besen et al. | Mar 1996 | A |
5503875 | Imai et al. | Apr 1996 | A |
5504042 | Cho et al. | Apr 1996 | A |
5510277 | Cunningham et al. | Apr 1996 | A |
5512102 | Yamazaki | Apr 1996 | A |
5514439 | Sibley | May 1996 | A |
5518549 | Hellwig | May 1996 | A |
5519234 | Paz de Araujo | May 1996 | A |
5520743 | Takahashi et al. | May 1996 | A |
5523616 | Yasuhide | Jun 1996 | A |
5527111 | Lysen et al. | Jun 1996 | A |
5527417 | Iida et al. | Jun 1996 | A |
5531218 | Krebs | Jul 1996 | A |
5531835 | Fodor et al. | Jul 1996 | A |
5537311 | Stevens | Jul 1996 | A |
5540059 | Yokokawa | Jul 1996 | A |
5540898 | Davidson | Jul 1996 | A |
5554557 | Koh | Sep 1996 | A |
5556275 | Sakata et al. | Sep 1996 | A |
5558717 | Zhao et al. | Sep 1996 | A |
5559046 | Oishi et al. | Sep 1996 | A |
5562383 | Iwai et al. | Oct 1996 | A |
5562947 | White et al. | Oct 1996 | A |
5562952 | Nakahigashi et al. | Oct 1996 | A |
5569402 | Meisser et al. | Oct 1996 | A |
5574247 | Nishitani et al. | Nov 1996 | A |
5576629 | Turner | Nov 1996 | A |
5577331 | Suzuki | Nov 1996 | A |
5583736 | Anderson et al. | Dec 1996 | A |
5586585 | Bonora et al. | Dec 1996 | A |
5589002 | Su | Dec 1996 | A |
5589110 | Motoda et al. | Dec 1996 | A |
5595606 | Fujikawa et al. | Jan 1997 | A |
5601641 | Stephens | Feb 1997 | A |
5602060 | Kobayashi et al. | Feb 1997 | A |
5604410 | Vollkommer et al. | Feb 1997 | A |
5611448 | Chen | Mar 1997 | A |
5616264 | Nishi et al. | Apr 1997 | A |
5616947 | Tamura | Apr 1997 | A |
5621982 | Yamashita | Apr 1997 | A |
5632919 | MacCracken et al. | May 1997 | A |
D380527 | Velez | Jul 1997 | S |
5650013 | Yamazaki | Jul 1997 | A |
5650351 | Wu | Jul 1997 | A |
5653807 | Crumbaker | Aug 1997 | A |
5656093 | Burkhart et al. | Aug 1997 | A |
5662470 | Huussen et al. | Sep 1997 | A |
5663899 | Zvonar et al. | Sep 1997 | A |
5665608 | Chapple-Sokol et al. | Sep 1997 | A |
5667592 | Boitnott et al. | Sep 1997 | A |
5670786 | Meyer et al. | Sep 1997 | A |
5679215 | Barnes et al. | Oct 1997 | A |
5681779 | Pasch et al. | Oct 1997 | A |
D386076 | Moore | Nov 1997 | S |
5683517 | Shan | Nov 1997 | A |
5685912 | Nishizaka | Nov 1997 | A |
5685914 | Hills et al. | Nov 1997 | A |
5695567 | Kordina | Dec 1997 | A |
5697706 | Ciaravino et al. | Dec 1997 | A |
5698036 | Ishii et al. | Dec 1997 | A |
5700729 | Lee et al. | Dec 1997 | A |
5708825 | Sotomayor | Jan 1998 | A |
5709745 | Larkin et al. | Jan 1998 | A |
5711811 | Suntola et al. | Jan 1998 | A |
5716133 | Hosokawa et al. | Feb 1998 | A |
5718574 | Shimazu | Feb 1998 | A |
5720927 | Cripe et al. | Feb 1998 | A |
D392855 | Pillow | Mar 1998 | S |
5724748 | Brooks | Mar 1998 | A |
5728223 | Murakarni et al. | Mar 1998 | A |
5728425 | Ebe et al. | Mar 1998 | A |
5730801 | Tepman et al. | Mar 1998 | A |
5730802 | Ishizumi et al. | Mar 1998 | A |
5732597 | Devenyi | Mar 1998 | A |
5732744 | Barr et al. | Mar 1998 | A |
5736314 | Hayes et al. | Apr 1998 | A |
5753835 | Gustin | May 1998 | A |
5754390 | Sandhu et al. | May 1998 | A |
5759281 | Gurary et al. | Jun 1998 | A |
5761328 | Solberg et al. | Jun 1998 | A |
5766365 | Umutoy et al. | Jun 1998 | A |
5768125 | Zinger et al. | Jun 1998 | A |
5769952 | Komino | Jun 1998 | A |
5775889 | Kobayashi et al. | Jul 1998 | A |
5777838 | Tamagawa et al. | Jul 1998 | A |
5779203 | Edlinger | Jul 1998 | A |
5781693 | Balance et al. | Jul 1998 | A |
5782979 | Kaneno | Jul 1998 | A |
5790750 | Anderson | Aug 1998 | A |
5791782 | Wooten et al. | Aug 1998 | A |
5792272 | Van Os et al. | Aug 1998 | A |
5796074 | Edelstein et al. | Aug 1998 | A |
5801104 | Schuegraf et al. | Sep 1998 | A |
5801945 | Commer | Sep 1998 | A |
5806980 | Berrian | Sep 1998 | A |
5813851 | Nakao | Sep 1998 | A |
5818716 | Chin et al. | Oct 1998 | A |
5819092 | Ferguson et al. | Oct 1998 | A |
5819434 | Herchen et al. | Oct 1998 | A |
5820366 | Lee | Oct 1998 | A |
5820685 | Kurihra et al. | Oct 1998 | A |
5820686 | Moore | Oct 1998 | A |
5826129 | Hasebe et al. | Oct 1998 | A |
5827420 | Shirazi et al. | Oct 1998 | A |
5827435 | Seiji | Oct 1998 | A |
5827757 | Robinson, Jr. et al. | Oct 1998 | A |
5836483 | Disel | Nov 1998 | A |
5837058 | Chen et al. | Nov 1998 | A |
5837320 | Hampden-Smith et al. | Nov 1998 | A |
5844683 | Pavloski et al. | Dec 1998 | A |
5846332 | Zhao et al. | Dec 1998 | A |
5851294 | Young et al. | Dec 1998 | A |
5851299 | Cheng et al. | Dec 1998 | A |
5852445 | Yoshikawa et al. | Dec 1998 | A |
5852879 | Schumaier | Dec 1998 | A |
5853484 | Jeong | Dec 1998 | A |
D403949 | Nakamura | Jan 1999 | S |
D404370 | Kimura | Jan 1999 | S |
D404372 | Ishii | Jan 1999 | S |
5855680 | Soininen et al. | Jan 1999 | A |
5855681 | Maydan et al. | Jan 1999 | A |
5855726 | Soraoka et al. | Jan 1999 | A |
5857777 | Schuh | Jan 1999 | A |
5861233 | Sekine et al. | Jan 1999 | A |
5862302 | Okase | Jan 1999 | A |
5863123 | Lee et al. | Jan 1999 | A |
5865205 | Wilmer | Feb 1999 | A |
5866795 | Wang et al. | Feb 1999 | A |
5872065 | Sivaramakrishnan | Feb 1999 | A |
5873942 | Park | Feb 1999 | A |
5877095 | Tamura et al. | Mar 1999 | A |
5879128 | Tietz et al. | Mar 1999 | A |
5879459 | Gadgil et al. | Mar 1999 | A |
5880980 | Rothacher et al. | Mar 1999 | A |
5882165 | Maydan et al. | Mar 1999 | A |
5884640 | Fishkin et al. | Mar 1999 | A |
5891251 | MacLeish et al. | Apr 1999 | A |
5893741 | Huang | Apr 1999 | A |
5897348 | Wu | Apr 1999 | A |
5897378 | Eriguchi | Apr 1999 | A |
5897379 | Ulrich et al. | Apr 1999 | A |
D409894 | McClurg | May 1999 | S |
5904170 | Harvey et al. | May 1999 | A |
D411516 | Imafuku et al. | Jun 1999 | S |
5908672 | Ryu | Jun 1999 | A |
5915200 | Tokumasu et al. | Jun 1999 | A |
5915562 | Nyseth et al. | Jun 1999 | A |
5916365 | Sherman | Jun 1999 | A |
D412270 | Fredrickson | Jul 1999 | S |
5920798 | Higuchi et al. | Jul 1999 | A |
5928426 | Aitchison | Jul 1999 | A |
D412512 | Boisvert | Aug 1999 | S |
5937142 | Moslehi et al. | Aug 1999 | A |
5937323 | Orczyk et al. | Aug 1999 | A |
5939886 | Turner et al. | Aug 1999 | A |
5947718 | Weaver | Sep 1999 | A |
5950327 | Peterson et al. | Sep 1999 | A |
5950925 | Fukunaga et al. | Sep 1999 | A |
5954375 | Trickle et al. | Sep 1999 | A |
5961775 | Fujimura | Oct 1999 | A |
5968275 | Lee et al. | Oct 1999 | A |
5970621 | Bazydola | Oct 1999 | A |
5972196 | Murphy et al. | Oct 1999 | A |
5975492 | Brenes | Nov 1999 | A |
5979506 | Aarseth | Nov 1999 | A |
5982931 | Ishimaru | Nov 1999 | A |
5984391 | Vanderpot et al. | Nov 1999 | A |
5987480 | Donohue et al. | Nov 1999 | A |
5989342 | Ikeda et al. | Nov 1999 | A |
5992453 | Zimmer | Nov 1999 | A |
5997588 | Goodwin | Dec 1999 | A |
5997768 | Scully | Dec 1999 | A |
5998870 | Lee et al. | Dec 1999 | A |
6000732 | Scheler et al. | Dec 1999 | A |
6001183 | Gurary et al. | Dec 1999 | A |
6001267 | Van Os et al. | Dec 1999 | A |
6004204 | Luxton et al. | Dec 1999 | A |
D419652 | Hall et al. | Jan 2000 | S |
6013553 | Wallace | Jan 2000 | A |
6013920 | Gordon et al. | Jan 2000 | A |
6014677 | Hayashi et al. | Jan 2000 | A |
6015459 | Jamison et al. | Jan 2000 | A |
6015465 | Kholodenko et al. | Jan 2000 | A |
6017779 | Miyasaka | Jan 2000 | A |
6017818 | Lu | Jan 2000 | A |
6024799 | Chen et al. | Feb 2000 | A |
6027163 | Longenecker et al. | Feb 2000 | A |
6029602 | Bhatnagar | Feb 2000 | A |
6030900 | Grassl et al. | Feb 2000 | A |
6035101 | Sajoto et al. | Mar 2000 | A |
6035804 | Arami et al. | Mar 2000 | A |
6039809 | Toyama et al. | Mar 2000 | A |
6042652 | Hyun | Mar 2000 | A |
6044860 | Nue | Apr 2000 | A |
6045260 | Schwartz et al. | Apr 2000 | A |
6048154 | Wytman | Apr 2000 | A |
6050506 | Guo et al. | Apr 2000 | A |
6053982 | Halpin et al. | Apr 2000 | A |
6053983 | Saeki et al. | Apr 2000 | A |
6054013 | Collins et al. | Apr 2000 | A |
6054678 | Miyazaki | Apr 2000 | A |
6060691 | Minami et al. | May 2000 | A |
6060721 | Huang | May 2000 | A |
6063196 | Li et al. | May 2000 | A |
6066204 | Haven | May 2000 | A |
6068441 | Raaijmakers et al. | May 2000 | A |
6071572 | Mosely et al. | Jun 2000 | A |
6072163 | Armstrong et al. | Jun 2000 | A |
6073973 | Boscaljon et al. | Jun 2000 | A |
6074154 | Ueda et al. | Jun 2000 | A |
6074443 | Venkatesh | Jun 2000 | A |
6074514 | Bjorkman et al. | Jun 2000 | A |
6077027 | Kawamura et al. | Jun 2000 | A |
6079356 | Umotoy et al. | Jun 2000 | A |
6079927 | Muka | Jun 2000 | A |
6083321 | Lei et al. | Jul 2000 | A |
6086677 | Umotoy et al. | Jul 2000 | A |
6090212 | Mahawili | Jul 2000 | A |
6090659 | Laibowitz et al. | Jul 2000 | A |
6091062 | Pfahnl et al. | Jul 2000 | A |
6093252 | Wengert et al. | Jul 2000 | A |
6093253 | Lofgren | Jul 2000 | A |
6095083 | Rice et al. | Aug 2000 | A |
6096133 | Yuuki et al. | Aug 2000 | A |
6096267 | Kishkovich | Aug 2000 | A |
6099302 | Hong et al. | Aug 2000 | A |
6099649 | Schmitt et al. | Aug 2000 | A |
6102565 | Kita et al. | Aug 2000 | A |
6104002 | Hirose et al. | Aug 2000 | A |
6104011 | Juliano | Aug 2000 | A |
6104401 | Parsons | Aug 2000 | A |
6106625 | Koai et al. | Aug 2000 | A |
6106678 | Shufflebotham | Aug 2000 | A |
6110531 | Paz de Araujo et al. | Aug 2000 | A |
6113703 | Anderson et al. | Sep 2000 | A |
6119710 | Brown | Sep 2000 | A |
6120008 | Littman et al. | Sep 2000 | A |
6121061 | Van Bilsen et al. | Sep 2000 | A |
6121158 | Benchikha et al. | Sep 2000 | A |
6122036 | Yamasaki et al. | Sep 2000 | A |
6124600 | Moroishi et al. | Sep 2000 | A |
6125789 | Gupta et al. | Oct 2000 | A |
6126744 | Hawkins et al. | Oct 2000 | A |
6126848 | Li et al. | Oct 2000 | A |
6127249 | Hu | Oct 2000 | A |
6129044 | Zhao et al. | Oct 2000 | A |
6129546 | Sada | Oct 2000 | A |
6132207 | Stoutjesdijk | Oct 2000 | A |
6134807 | Komino | Oct 2000 | A |
6135460 | Wise et al. | Oct 2000 | A |
6137240 | Bogdan et al. | Oct 2000 | A |
6139239 | Snijders | Oct 2000 | A |
6140252 | Cho et al. | Oct 2000 | A |
6143079 | Halpin | Nov 2000 | A |
6143082 | McInerney et al. | Nov 2000 | A |
6143659 | Leem | Nov 2000 | A |
6146463 | Yudovsky et al. | Nov 2000 | A |
6148761 | Majewski et al. | Nov 2000 | A |
6151446 | Hunter et al. | Nov 2000 | A |
6152070 | Fairbairn et al. | Nov 2000 | A |
6156151 | Komino et al. | Dec 2000 | A |
6158941 | Muka et al. | Dec 2000 | A |
6160244 | Ohashi | Dec 2000 | A |
6161500 | Kopacz et al. | Dec 2000 | A |
6162323 | Koshimizu | Dec 2000 | A |
6164894 | Cheng | Dec 2000 | A |
6174809 | Kang et al. | Jan 2001 | B1 |
6178918 | Van Os et al. | Jan 2001 | B1 |
6179955 | Shin et al. | Jan 2001 | B1 |
6180979 | Hofman et al. | Jan 2001 | B1 |
6182603 | Shang et al. | Feb 2001 | B1 |
6183564 | Reynolds et al. | Feb 2001 | B1 |
6183565 | Granneman et al. | Feb 2001 | B1 |
6187672 | Zhao | Feb 2001 | B1 |
6187691 | Fukuda | Feb 2001 | B1 |
6190037 | Das et al. | Feb 2001 | B1 |
6190113 | Bui et al. | Feb 2001 | B1 |
6190457 | Arai et al. | Feb 2001 | B1 |
6190634 | Lieber et al. | Feb 2001 | B1 |
6191399 | Van Bilsen | Feb 2001 | B1 |
6194037 | Terasaki et al. | Feb 2001 | B1 |
6200897 | Wang et al. | Mar 2001 | B1 |
6201999 | Jevtic | Mar 2001 | B1 |
6203613 | Gates et al. | Mar 2001 | B1 |
6203618 | Hashizume et al. | Mar 2001 | B1 |
6203969 | Ueda | Mar 2001 | B1 |
6207932 | Yoo | Mar 2001 | B1 |
6207936 | de Waard | Mar 2001 | B1 |
6209221 | Beulens | Apr 2001 | B1 |
6210485 | Zhao et al. | Apr 2001 | B1 |
6212789 | Kato | Apr 2001 | B1 |
6213708 | Allen | Apr 2001 | B1 |
6214122 | Thompson | Apr 2001 | B1 |
6214717 | Yan et al. | Apr 2001 | B1 |
6217658 | Orczyk et al. | Apr 2001 | B1 |
6218288 | Li et al. | Apr 2001 | B1 |
6225020 | Jung et al. | May 2001 | B1 |
6225602 | Buiijze et al. | May 2001 | B1 |
6225745 | Srivastava | May 2001 | B1 |
6230650 | Yamazaki | May 2001 | B1 |
6231290 | Kikuchi et al. | May 2001 | B1 |
6235858 | Swarup et al. | May 2001 | B1 |
6238734 | Senzaki et al. | May 2001 | B1 |
6240875 | Wijck et al. | Jun 2001 | B1 |
6241822 | Ide | Jun 2001 | B1 |
6242359 | Misra | Jun 2001 | B1 |
6243654 | Johnson et al. | Jun 2001 | B1 |
6245665 | Yokoyama | Jun 2001 | B1 |
6247245 | Ishii | Jun 2001 | B1 |
6250250 | Maishev et al. | Jun 2001 | B1 |
6255221 | Hudson et al. | Jul 2001 | B1 |
6257758 | Culbertson | Jul 2001 | B1 |
6261648 | Akiba et al. | Jul 2001 | B1 |
6264467 | Andreas et al. | Jul 2001 | B1 |
6265113 | Rosasco et al. | Jul 2001 | B1 |
6265311 | Hautala et al. | Jul 2001 | B1 |
6270572 | Kim et al. | Aug 2001 | B1 |
6271148 | Kao | Aug 2001 | B1 |
6274496 | Leusink et al. | Aug 2001 | B1 |
6274878 | Li et al. | Aug 2001 | B1 |
6281098 | Wang | Aug 2001 | B1 |
6281141 | Das et al. | Aug 2001 | B1 |
6283692 | Perlov et al. | Sep 2001 | B1 |
6284050 | Shi et al. | Sep 2001 | B1 |
6284149 | Li et al. | Sep 2001 | B1 |
6287965 | Kang et al. | Sep 2001 | B1 |
6287988 | Nagamine et al. | Sep 2001 | B1 |
6293700 | Lund et al. | Sep 2001 | B1 |
D449873 | Bronson | Oct 2001 | S |
6296710 | Allen et al. | Oct 2001 | B1 |
6296711 | Loan et al. | Oct 2001 | B1 |
6296909 | Spitsberg | Oct 2001 | B1 |
6297539 | Ma et al. | Oct 2001 | B1 |
6299133 | Waragai et al. | Oct 2001 | B2 |
6302964 | Umotoy et al. | Oct 2001 | B1 |
6303523 | Cheung | Oct 2001 | B2 |
6305898 | Yamagishi et al. | Oct 2001 | B1 |
6311016 | Yanagawa et al. | Oct 2001 | B1 |
6312525 | Bright et al. | Nov 2001 | B1 |
6315512 | Tabrizi et al. | Nov 2001 | B1 |
6316162 | Jung et al. | Nov 2001 | B1 |
6316371 | Oosterlaken et al. | Nov 2001 | B1 |
6320320 | Bailey et al. | Nov 2001 | B1 |
6321680 | Cook et al. | Nov 2001 | B2 |
6321780 | Iwabuchi | Nov 2001 | B1 |
D451893 | Robson | Dec 2001 | S |
D452220 | Robson | Dec 2001 | S |
6325858 | Wengert | Dec 2001 | B1 |
6326322 | Kim et al. | Dec 2001 | B1 |
6326597 | Lubomirsky et al. | Dec 2001 | B1 |
6328561 | Hasper et al. | Dec 2001 | B1 |
6329297 | Balish | Dec 2001 | B1 |
6333275 | Mayer et al. | Dec 2001 | B1 |
6335049 | Basceri | Jan 2002 | B1 |
6335240 | Kim et al. | Jan 2002 | B1 |
6342427 | Choi et al. | Jan 2002 | B1 |
6343239 | Toda et al. | Jan 2002 | B1 |
6344084 | Koinuma et al. | Feb 2002 | B1 |
6344232 | Jones et al. | Feb 2002 | B1 |
6346419 | Ryerson et al. | Feb 2002 | B1 |
6347636 | Xia | Feb 2002 | B1 |
6350391 | Livshits et al. | Feb 2002 | B1 |
6352049 | Yin et al. | Mar 2002 | B1 |
6352945 | Matsuki | Mar 2002 | B1 |
6357984 | Zinger et al. | Mar 2002 | B1 |
6363294 | Coronel et al. | Mar 2002 | B1 |
D455024 | Mimick et al. | Apr 2002 | S |
6367410 | Leahey et al. | Apr 2002 | B1 |
6368773 | Jung et al. | Apr 2002 | B1 |
6368987 | Kopacz et al. | Apr 2002 | B1 |
6370796 | Zucker | Apr 2002 | B1 |
6372583 | Tyagi | Apr 2002 | B1 |
6374831 | Chandran | Apr 2002 | B1 |
6375312 | Ikeda et al. | Apr 2002 | B1 |
6375749 | Boydston et al. | Apr 2002 | B1 |
6375750 | Van Os et al. | Apr 2002 | B1 |
6379466 | Sahin et al. | Apr 2002 | B1 |
D457609 | Piano | May 2002 | S |
6383300 | Saito et al. | May 2002 | B1 |
6383566 | Zagdoun | May 2002 | B1 |
6383955 | Matsuki | May 2002 | B1 |
6387207 | Janakiraman | May 2002 | B1 |
6387827 | Mertens et al. | May 2002 | B1 |
6390753 | de Ridder et al. | May 2002 | B1 |
6390754 | Yamaga et al. | May 2002 | B2 |
6391803 | Kim et al. | May 2002 | B1 |
6395650 | Callegari et al. | May 2002 | B1 |
6398184 | Sowada et al. | Jun 2002 | B1 |
6399022 | Schuler et al. | Jun 2002 | B1 |
6402806 | Schmitt et al. | Jun 2002 | B1 |
6410433 | Hautala et al. | Jun 2002 | B1 |
6410459 | Blalock et al. | Jun 2002 | B2 |
6410463 | Matsuki | Jun 2002 | B1 |
6413321 | Kim et al. | Jul 2002 | B1 |
6413583 | Moghadam et al. | Jul 2002 | B1 |
6420279 | Ono et al. | Jul 2002 | B1 |
6423949 | Chen et al. | Jul 2002 | B1 |
D461233 | Whalen | Aug 2002 | S |
D461882 | Piano | Aug 2002 | S |
6428859 | Chiang et al. | Aug 2002 | B1 |
6429465 | Yagi et al. | Aug 2002 | B1 |
6432206 | Tolt | Aug 2002 | B1 |
6432255 | Sun et al. | Aug 2002 | B1 |
6432479 | Chang et al. | Aug 2002 | B2 |
6432849 | Endo et al. | Aug 2002 | B1 |
6433298 | Ishii | Aug 2002 | B1 |
6435798 | Satoh | Aug 2002 | B1 |
6435865 | Tseng et al. | Aug 2002 | B1 |
6436819 | Zhang | Aug 2002 | B1 |
6437444 | Andideh | Aug 2002 | B2 |
6438502 | Awtrey | Aug 2002 | B1 |
6439822 | Kimura et al. | Aug 2002 | B1 |
6440261 | Tepman et al. | Aug 2002 | B1 |
6441350 | Stoddard et al. | Aug 2002 | B1 |
6445574 | Saw et al. | Sep 2002 | B1 |
6446573 | Hirayama et al. | Sep 2002 | B2 |
6447232 | Davis et al. | Sep 2002 | B1 |
6447651 | Ishikawa et al. | Sep 2002 | B1 |
6447937 | Murakawa et al. | Sep 2002 | B1 |
6448192 | Kaushik | Sep 2002 | B1 |
6450117 | Murugesh et al. | Sep 2002 | B1 |
6450757 | Saeki | Sep 2002 | B1 |
6451713 | Tay et al. | Sep 2002 | B1 |
6454860 | Metzner et al. | Sep 2002 | B2 |
6454909 | Matsuse et al. | Sep 2002 | B1 |
6455098 | Tran et al. | Sep 2002 | B2 |
6455225 | Kong et al. | Sep 2002 | B1 |
6455445 | Matsuki | Sep 2002 | B2 |
6460482 | Kuibira et al. | Oct 2002 | B1 |
6461435 | Littau et al. | Oct 2002 | B1 |
6461436 | Campbell et al. | Oct 2002 | B1 |
6461439 | Granneman et al. | Oct 2002 | B1 |
6468924 | Lee | Oct 2002 | B2 |
6471779 | Nishio et al. | Oct 2002 | B1 |
6472266 | Yu et al. | Oct 2002 | B1 |
6475276 | Elers et al. | Nov 2002 | B1 |
6475930 | Junker et al. | Nov 2002 | B1 |
6478872 | Chae et al. | Nov 2002 | B1 |
6481945 | Hasper et al. | Nov 2002 | B1 |
6482331 | Lu et al. | Nov 2002 | B2 |
6482663 | Buckland | Nov 2002 | B1 |
6483989 | Okada et al. | Nov 2002 | B1 |
6488774 | Hone et al. | Dec 2002 | B1 |
6490493 | Dharnipragada | Dec 2002 | B1 |
6492625 | Boguslayskiy et al. | Dec 2002 | B1 |
6494065 | Babbitt | Dec 2002 | B2 |
6494998 | Brcka | Dec 2002 | B1 |
6496819 | Bello et al. | Dec 2002 | B1 |
6497734 | Barber et al. | Dec 2002 | B1 |
6497767 | Okase et al. | Dec 2002 | B1 |
6498091 | Chen et al. | Dec 2002 | B1 |
6499533 | Yamada | Dec 2002 | B2 |
6500487 | Holst et al. | Dec 2002 | B1 |
6502530 | Turlot et al. | Jan 2003 | B1 |
6503079 | Kogano et al. | Jan 2003 | B2 |
6503330 | Sneh et al. | Jan 2003 | B1 |
6503365 | Kim et al. | Jan 2003 | B1 |
6503562 | Saito et al. | Jan 2003 | B1 |
6503826 | Oda | Jan 2003 | B1 |
6506009 | Nulman et al. | Jan 2003 | B1 |
6506253 | Sakuma | Jan 2003 | B2 |
6507410 | Robertson et al. | Jan 2003 | B1 |
6511539 | Raaijmakers | Jan 2003 | B1 |
6514313 | Spiegelman | Feb 2003 | B1 |
6514666 | Choi et al. | Feb 2003 | B1 |
6521295 | Remington | Feb 2003 | B1 |
6521547 | Chang et al. | Feb 2003 | B1 |
6527884 | Takakuwa et al. | Mar 2003 | B1 |
6528171 | Endler et al. | Mar 2003 | B1 |
6528430 | Kwan | Mar 2003 | B2 |
6528752 | Ishii et al. | Mar 2003 | B1 |
6528767 | Bagley et al. | Mar 2003 | B2 |
6530994 | Mahawili | Mar 2003 | B1 |
6531193 | Fonash et al. | Mar 2003 | B2 |
6531412 | Conti et al. | Mar 2003 | B2 |
6534133 | Kaloyeros et al. | Mar 2003 | B1 |
6534395 | Werkhoven et al. | Mar 2003 | B2 |
6536950 | Green | Mar 2003 | B1 |
6539891 | Kang et al. | Apr 2003 | B1 |
6540469 | Matsunaga et al. | Apr 2003 | B2 |
6540838 | Sneh et al. | Apr 2003 | B2 |
6544906 | Rotondaro et al. | Apr 2003 | B2 |
6552209 | Lei et al. | Apr 2003 | B1 |
6558517 | Basceri | May 2003 | B2 |
6558755 | Berry et al. | May 2003 | B2 |
6559026 | Rossman et al. | May 2003 | B1 |
6562094 | Denker et al. | May 2003 | B2 |
6565763 | Asakawa et al. | May 2003 | B1 |
6566278 | Harvey et al. | May 2003 | B1 |
6569239 | Arai et al. | May 2003 | B2 |
6569971 | Roh et al. | May 2003 | B2 |
6573030 | Fairbairn et al. | Jun 2003 | B1 |
6574644 | Hsu et al. | Jun 2003 | B2 |
6576062 | Matsuse | Jun 2003 | B2 |
6576064 | Griffiths et al. | Jun 2003 | B2 |
6576300 | Berry et al. | Jun 2003 | B1 |
6576564 | Agarwal | Jun 2003 | B2 |
6578589 | Mayusumi | Jun 2003 | B1 |
6579833 | McNallan et al. | Jun 2003 | B1 |
6580050 | Miller et al. | Jun 2003 | B1 |
6582174 | Hayashi | Jun 2003 | B1 |
6583048 | Vincent et al. | Jun 2003 | B1 |
6583572 | Veltrop et al. | Jun 2003 | B2 |
6587108 | Guerlain et al. | Jul 2003 | B1 |
6589352 | Yudovsky et al. | Jul 2003 | B1 |
6589707 | Lee et al. | Jul 2003 | B2 |
6589868 | Rossman | Jul 2003 | B2 |
6590251 | Kang et al. | Jul 2003 | B2 |
6594550 | Okrah | Jul 2003 | B1 |
6596653 | Tan | Jul 2003 | B2 |
6598559 | Vellore et al. | Jul 2003 | B1 |
6602806 | Xia et al. | Aug 2003 | B1 |
6607602 | Granneman et al. | Aug 2003 | B1 |
6607868 | Choi | Aug 2003 | B2 |
6607948 | Sugiyama et al. | Aug 2003 | B1 |
6608745 | Tsuruta et al. | Aug 2003 | B2 |
6610375 | Akiba et al. | Aug 2003 | B2 |
6613685 | Granneman et al. | Sep 2003 | B1 |
6616986 | Sherman | Sep 2003 | B2 |
6617253 | Chu et al. | Sep 2003 | B1 |
6620251 | Kitano | Sep 2003 | B2 |
6624064 | Sahin | Sep 2003 | B1 |
6627268 | Fair et al. | Sep 2003 | B1 |
6627503 | Ma et al. | Sep 2003 | B2 |
6630030 | Suntola et al. | Oct 2003 | B1 |
6632478 | Gaillard et al. | Oct 2003 | B2 |
6633364 | Hayashi | Oct 2003 | B2 |
6635115 | Fairbairn et al. | Oct 2003 | B1 |
6635117 | Kinnard et al. | Oct 2003 | B1 |
6635578 | Xu et al. | Oct 2003 | B1 |
6638839 | Deng et al. | Oct 2003 | B2 |
6640145 | Hoffberg et al. | Oct 2003 | B2 |
6645304 | Yamaguchi | Nov 2003 | B2 |
6648974 | Ogliari et al. | Nov 2003 | B1 |
6649921 | Cekic et al. | Nov 2003 | B1 |
6652924 | Sherman | Nov 2003 | B2 |
6656281 | Ueda | Dec 2003 | B1 |
6656282 | Kim et al. | Dec 2003 | B2 |
6660662 | Ishikawa et al. | Dec 2003 | B2 |
6662817 | Yamagishi | Dec 2003 | B2 |
6663332 | Sluijk et al. | Dec 2003 | B1 |
6673196 | Oyabu | Jan 2004 | B1 |
6676290 | Lu | Jan 2004 | B1 |
6679194 | Ham et al. | Jan 2004 | B2 |
6682971 | Tsuneda et al. | Jan 2004 | B2 |
6682973 | Paton et al. | Jan 2004 | B1 |
6683274 | Kwon et al. | Jan 2004 | B1 |
D486891 | Cronce | Feb 2004 | S |
6684659 | Tanaka et al. | Feb 2004 | B1 |
6684719 | Gehner et al. | Feb 2004 | B2 |
6686281 | Yamazaki et al. | Feb 2004 | B2 |
6688784 | Templeton | Feb 2004 | B1 |
6689220 | Nguyen | Feb 2004 | B1 |
6692575 | Omstead et al. | Feb 2004 | B1 |
6692576 | Halpin et al. | Feb 2004 | B2 |
6696367 | Aggarwal | Feb 2004 | B1 |
6699003 | Saeki | Mar 2004 | B2 |
6699399 | Qian et al. | Mar 2004 | B1 |
6700089 | Hirooka | Mar 2004 | B1 |
6709989 | Ramdani et al. | Mar 2004 | B2 |
6710364 | Guldi et al. | Mar 2004 | B2 |
6710857 | Kondo | Mar 2004 | B2 |
6713824 | Mikata | Mar 2004 | B1 |
6715949 | Fisher et al. | Apr 2004 | B1 |
6716571 | Gabriel | Apr 2004 | B2 |
6719499 | Kuznetsov et al. | Apr 2004 | B1 |
6720260 | Fair et al. | Apr 2004 | B1 |
6720531 | Jacobson et al. | Apr 2004 | B1 |
6722837 | Inui | Apr 2004 | B2 |
6723642 | Lim et al. | Apr 2004 | B1 |
6730614 | Lim et al. | May 2004 | B1 |
6732006 | Haanstra et al. | May 2004 | B2 |
6734090 | Agarwala et al. | May 2004 | B2 |
6734631 | Juestel et al. | May 2004 | B2 |
6737716 | Matsuo et al. | May 2004 | B1 |
6740853 | Johnson et al. | May 2004 | B1 |
6743475 | Skarp et al. | Jun 2004 | B2 |
6743738 | Todd et al. | Jun 2004 | B2 |
6745095 | Ben-Dov | Jun 2004 | B1 |
6746240 | de Ridder et al. | Jun 2004 | B2 |
6746308 | Bode et al. | Jun 2004 | B1 |
6749671 | Holst et al. | Jun 2004 | B2 |
6753507 | Fure et al. | Jun 2004 | B2 |
6755221 | Jeong et al. | Jun 2004 | B2 |
6756085 | Waldfried | Jun 2004 | B2 |
6756293 | Li et al. | Jun 2004 | B2 |
6756318 | Nguyen et al. | Jun 2004 | B2 |
6759098 | Han | Jul 2004 | B2 |
6760981 | Leap | Jul 2004 | B2 |
6767447 | Uno et al. | Jul 2004 | B2 |
D494552 | Tezuka et al. | Aug 2004 | S |
6780704 | Raaijmakers et al. | Aug 2004 | B1 |
6783875 | Yamada et al. | Aug 2004 | B2 |
6784033 | Yamazaki | Aug 2004 | B1 |
6784108 | Donohoe et al. | Aug 2004 | B1 |
D496008 | Takahashi et al. | Sep 2004 | S |
6786997 | Yamazaki | Sep 2004 | B1 |
D497536 | Fujiwara | Oct 2004 | S |
D497977 | Engelbrektsson | Nov 2004 | S |
6811960 | Lee et al. | Nov 2004 | B2 |
6812157 | Gadgil | Nov 2004 | B1 |
6815350 | Kim et al. | Nov 2004 | B2 |
6815352 | Tamura et al. | Nov 2004 | B1 |
6818864 | Ptak | Nov 2004 | B2 |
6820570 | Kilpela et al. | Nov 2004 | B2 |
6821910 | Adomaitis et al. | Nov 2004 | B2 |
6824665 | Shelnut et al. | Nov 2004 | B2 |
6825134 | Law et al. | Nov 2004 | B2 |
D499620 | Horner-Richardson et al. | Dec 2004 | S |
6827789 | Lee et al. | Dec 2004 | B2 |
6828235 | Takano | Dec 2004 | B2 |
6831004 | Byun | Dec 2004 | B2 |
6833024 | Holst et al. | Dec 2004 | B2 |
6835039 | Van Den Berg | Dec 2004 | B2 |
6838122 | Basceri et al. | Jan 2005 | B2 |
6841201 | Shanov et al. | Jan 2005 | B2 |
6843202 | Kusuda | Jan 2005 | B2 |
6846146 | Inui | Jan 2005 | B2 |
6846515 | Vrtis | Jan 2005 | B2 |
6846742 | Rossman | Jan 2005 | B2 |
6847014 | Benjamin et al. | Jan 2005 | B1 |
6849241 | Dauelsberg et al. | Feb 2005 | B2 |
6849857 | Ichiki et al. | Feb 2005 | B2 |
6858524 | Haukka et al. | Feb 2005 | B2 |
6858547 | Metzner | Feb 2005 | B2 |
6861642 | Ichiki et al. | Mar 2005 | B2 |
6863019 | Shamouilian | Mar 2005 | B2 |
6863281 | Endou et al. | Mar 2005 | B2 |
6864041 | Brown | Mar 2005 | B2 |
6867859 | Powell | Mar 2005 | B1 |
6872258 | Park et al. | Mar 2005 | B2 |
6872259 | Strang | Mar 2005 | B2 |
D504142 | Horner-Richardson et al. | Apr 2005 | S |
6874247 | Hsu | Apr 2005 | B1 |
6874480 | Ismailov | Apr 2005 | B1 |
6875477 | Trickett et al. | Apr 2005 | B2 |
6875677 | Conley, Jr. et al. | Apr 2005 | B1 |
6876017 | Goodner | Apr 2005 | B2 |
6876191 | de Ridder | Apr 2005 | B2 |
6878206 | Tzu et al. | Apr 2005 | B2 |
6878402 | Chiang et al. | Apr 2005 | B2 |
6883733 | Lind | Apr 2005 | B1 |
6884066 | Nguyen et al. | Apr 2005 | B2 |
6884295 | Ishii | Apr 2005 | B2 |
6884319 | Kim | Apr 2005 | B2 |
6884475 | Basceri | Apr 2005 | B2 |
D505590 | Greiner | May 2005 | S |
6889211 | Yoshiura et al. | May 2005 | B1 |
6889864 | Lindfors et al. | May 2005 | B2 |
6890596 | Sarigiannis et al. | May 2005 | B2 |
6895158 | Alyward et al. | May 2005 | B2 |
6899507 | Yamagishi et al. | May 2005 | B2 |
6902395 | Oosterlaken et al. | Jun 2005 | B2 |
6909839 | Wang et al. | Jun 2005 | B2 |
6911092 | Sneh | Jun 2005 | B2 |
6913152 | Zuk | Jul 2005 | B2 |
6913796 | Albano et al. | Jul 2005 | B2 |
6916398 | Chen et al. | Jul 2005 | B2 |
6916559 | Murakawa et al. | Jul 2005 | B2 |
6917755 | Nguyen et al. | Jul 2005 | B2 |
6924078 | Lee et al. | Aug 2005 | B2 |
6928890 | Gehner et al. | Aug 2005 | B2 |
6929699 | Whitesell | Aug 2005 | B2 |
6929700 | Tan et al. | Aug 2005 | B2 |
6930041 | Agarwal | Aug 2005 | B2 |
6930059 | Conley, Jr. et al. | Aug 2005 | B2 |
6935269 | Lee et al. | Aug 2005 | B2 |
6939579 | Bondestam et al. | Sep 2005 | B2 |
6939817 | Sandhu et al. | Sep 2005 | B2 |
6942753 | Choi et al. | Sep 2005 | B2 |
6949204 | Lenz et al. | Sep 2005 | B1 |
6951587 | Narushima | Oct 2005 | B1 |
6952656 | Cordova et al. | Oct 2005 | B1 |
6953609 | Carollo | Oct 2005 | B2 |
6955741 | Yamagishi | Oct 2005 | B2 |
6955836 | Kumagai et al. | Oct 2005 | B2 |
6955928 | Brennan | Oct 2005 | B1 |
6963052 | Kuibira et al. | Nov 2005 | B2 |
6972055 | Sferlazzo | Dec 2005 | B2 |
6972478 | Waite et al. | Dec 2005 | B1 |
6974781 | Timmermans et al. | Dec 2005 | B2 |
6975921 | Verhaar | Dec 2005 | B2 |
6976822 | Woodruff | Dec 2005 | B2 |
6981832 | Zinger et al. | Jan 2006 | B2 |
6982046 | Srivastava et al. | Jan 2006 | B2 |
6982103 | Basceri et al. | Jan 2006 | B2 |
6984591 | Buchanan et al. | Jan 2006 | B1 |
6984595 | Yamazaki | Jan 2006 | B1 |
6985788 | Haanstra et al. | Jan 2006 | B2 |
6986914 | Elers et al. | Jan 2006 | B2 |
6987155 | Roh et al. | Jan 2006 | B2 |
6990430 | Hosek | Jan 2006 | B2 |
7005227 | Yueh et al. | Feb 2006 | B2 |
7005391 | Min | Feb 2006 | B2 |
7008879 | Lee et al. | Mar 2006 | B2 |
7010580 | Fu et al. | Mar 2006 | B1 |
7017514 | Shepherd et al. | Mar 2006 | B1 |
7018941 | Cui et al. | Mar 2006 | B2 |
7021330 | Maula et al. | Apr 2006 | B2 |
7021881 | Yamagishi | Apr 2006 | B2 |
7036453 | Ishikawa et al. | May 2006 | B2 |
7041609 | Vaartstra | May 2006 | B2 |
7045430 | Ahn et al. | May 2006 | B2 |
7049226 | Chung et al. | May 2006 | B2 |
7049247 | Gates et al. | May 2006 | B2 |
7052584 | Basceri | May 2006 | B2 |
7053009 | Conley, Jr. et al. | May 2006 | B2 |
7055263 | Wu et al. | Jun 2006 | B2 |
7055875 | Bonora | Jun 2006 | B2 |
7062161 | Kusuda et al. | Jun 2006 | B2 |
7070178 | Van Der Toorn et al. | Jul 2006 | B2 |
7071051 | Jeon et al. | Jul 2006 | B1 |
7073834 | Matsumoto et al. | Jul 2006 | B2 |
7074690 | Gauri et al. | Jul 2006 | B1 |
7077614 | Hasper et al. | Jul 2006 | B1 |
7080545 | Dimeo et al. | Jul 2006 | B2 |
7084060 | Furukawa | Aug 2006 | B1 |
7084079 | Conti et al. | Aug 2006 | B2 |
7085623 | Siegers | Aug 2006 | B2 |
7086347 | Howald et al. | Aug 2006 | B2 |
7088003 | Gates et al. | Aug 2006 | B2 |
7090394 | Hashikura et al. | Aug 2006 | B2 |
7092287 | Beulens et al. | Aug 2006 | B2 |
7098149 | Lukas | Aug 2006 | B2 |
7098150 | Misra et al. | Aug 2006 | B2 |
7100459 | Gehner et al. | Sep 2006 | B2 |
7101763 | Anderson et al. | Sep 2006 | B1 |
7108753 | Wood | Sep 2006 | B2 |
7109098 | Ramaswamy et al. | Sep 2006 | B1 |
7109114 | Chen et al. | Sep 2006 | B2 |
7111232 | Bascom | Sep 2006 | B1 |
7115305 | Bronikowski et al. | Oct 2006 | B2 |
7115838 | Kurara et al. | Oct 2006 | B2 |
7122085 | Shero et al. | Oct 2006 | B2 |
7122222 | Xiao et al. | Oct 2006 | B2 |
7129165 | Basol et al. | Oct 2006 | B2 |
7132360 | Schaeffer et al. | Nov 2006 | B2 |
7135421 | Ahn et al. | Nov 2006 | B2 |
7140558 | McCracken et al. | Nov 2006 | B2 |
7141499 | Raaijmakers | Nov 2006 | B2 |
7143897 | Guzman et al. | Dec 2006 | B1 |
7144809 | Elers et al. | Dec 2006 | B2 |
7147766 | Uzoh et al. | Dec 2006 | B2 |
7153542 | Nguyen et al. | Dec 2006 | B2 |
7156380 | Soininen | Jan 2007 | B2 |
7163393 | Adachi et al. | Jan 2007 | B2 |
7163721 | Zhang et al. | Jan 2007 | B2 |
7163900 | Weber | Jan 2007 | B2 |
7168852 | Linnarsson | Jan 2007 | B2 |
7172497 | Basol et al. | Feb 2007 | B2 |
7173216 | Ptak | Feb 2007 | B2 |
7183229 | Yamanaka | Feb 2007 | B2 |
7186648 | Rozbicki | Mar 2007 | B1 |
7192824 | Ahn et al. | Mar 2007 | B2 |
7192892 | Ahn et al. | Mar 2007 | B2 |
7195479 | Beatty et al. | Mar 2007 | B2 |
7195693 | Cowans | Mar 2007 | B2 |
D541125 | Gaudron | Apr 2007 | S |
7198447 | Morimitsu et al. | Apr 2007 | B2 |
7199513 | Huber et al. | Apr 2007 | B2 |
7201943 | Park et al. | Apr 2007 | B2 |
7202148 | Chen et al. | Apr 2007 | B2 |
7202512 | Chen et al. | Apr 2007 | B2 |
7204886 | Chen et al. | Apr 2007 | B2 |
7204887 | Kawamura et al. | Apr 2007 | B2 |
7205246 | MacNeil et al. | Apr 2007 | B2 |
7205247 | Lee et al. | Apr 2007 | B2 |
7207763 | Lee | Apr 2007 | B2 |
7208198 | Basceri et al. | Apr 2007 | B2 |
7208389 | Tipton et al. | Apr 2007 | B1 |
7210925 | Adachi | May 2007 | B2 |
7211524 | Ryu et al. | May 2007 | B2 |
7211525 | Shanker | May 2007 | B1 |
7214630 | Varadarajan et al. | May 2007 | B1 |
7217617 | Basceri | May 2007 | B2 |
7223014 | Lojen | May 2007 | B2 |
7208413 | Byun et al. | Jun 2007 | B2 |
7234476 | Arai | Jun 2007 | B2 |
7235137 | Kitayama et al. | Jun 2007 | B2 |
7235482 | Wu | Jun 2007 | B2 |
7235501 | Ahn et al. | Jun 2007 | B2 |
7238596 | Kouvetakis et al. | Jul 2007 | B2 |
7238616 | Agarwal | Jul 2007 | B2 |
7238653 | Lee et al. | Jul 2007 | B2 |
7256375 | Oosterlaken | Aug 2007 | B2 |
7265061 | Cho et al. | Sep 2007 | B1 |
7274867 | Peukert | Sep 2007 | B2 |
D553104 | Oohashi et al. | Oct 2007 | S |
7279256 | Son | Oct 2007 | B2 |
7290813 | Bonora | Nov 2007 | B2 |
7294581 | Haverkort et al. | Nov 2007 | B2 |
7296460 | Dimeo et al. | Nov 2007 | B2 |
7297641 | Todd et al. | Nov 2007 | B2 |
7298009 | Yan et al. | Nov 2007 | B2 |
7301623 | Madsen et al. | Nov 2007 | B1 |
D556704 | Nakamura et al. | Dec 2007 | S |
D557226 | Uchino et al. | Dec 2007 | S |
D558021 | Lawrence | Dec 2007 | S |
7307028 | Goto et al. | Dec 2007 | B2 |
7307178 | Kiyomori et al. | Dec 2007 | B2 |
7312148 | Ramaswamy et al. | Dec 2007 | B2 |
7312162 | Ramaswamy et al. | Dec 2007 | B2 |
7312494 | Ahn et al. | Dec 2007 | B2 |
D559993 | Nagakubo et al. | Jan 2008 | S |
D559994 | Nagakubo et al. | Jan 2008 | S |
7320544 | Hsieh | Jan 2008 | B2 |
7323401 | Ramaswamy et al. | Jan 2008 | B2 |
7326656 | Brask et al. | Feb 2008 | B2 |
7326657 | Xia et al. | Feb 2008 | B2 |
7327948 | Shrinivasan | Feb 2008 | B1 |
7329947 | Adachi et al. | Feb 2008 | B2 |
7335611 | Ramaswamy et al. | Feb 2008 | B2 |
7351057 | Berenbak et al. | Apr 2008 | B2 |
7354482 | Konishi et al. | Apr 2008 | B2 |
7354847 | Chan et al. | Apr 2008 | B2 |
7354873 | Fukazawa et al. | Apr 2008 | B2 |
7356762 | van Driel | Apr 2008 | B2 |
7357138 | Ji et al. | Apr 2008 | B2 |
7361447 | Jung | Apr 2008 | B2 |
7375035 | Heden et al. | May 2008 | B2 |
7376520 | Wong | May 2008 | B2 |
7378618 | Sorabji et al. | May 2008 | B1 |
7379785 | Higashi et al. | May 2008 | B2 |
D571383 | Ota et al. | Jun 2008 | S |
D571831 | Ota et al. | Jun 2008 | S |
7381644 | Soubramonium et al. | Jun 2008 | B1 |
7387685 | Choi et al. | Jun 2008 | B2 |
7393207 | Imai | Jul 2008 | B2 |
7393418 | Yokogawa | Jul 2008 | B2 |
7393736 | Ahn et al. | Jul 2008 | B2 |
7393765 | Hanawa et al. | Jul 2008 | B2 |
7396491 | Marking et al. | Jul 2008 | B2 |
7399388 | Moghadam et al. | Jul 2008 | B2 |
7399570 | Lee et al. | Jul 2008 | B2 |
7402534 | Mahajani | Jul 2008 | B2 |
7405166 | Liang et al. | Jul 2008 | B2 |
7405454 | Ahn et al. | Jul 2008 | B2 |
D575713 | Ratcliffe | Aug 2008 | S |
7408225 | Shinriki et al. | Aug 2008 | B2 |
7410290 | Tanaka | Aug 2008 | B2 |
7410666 | Elers | Aug 2008 | B2 |
7411352 | Madocks | Aug 2008 | B2 |
7414281 | Fastow | Aug 2008 | B1 |
D576001 | Brunderman | Sep 2008 | S |
7422635 | Zheng et al. | Sep 2008 | B2 |
7422636 | Ishizaka | Sep 2008 | B2 |
7422653 | Blahnik et al. | Sep 2008 | B2 |
7422775 | Ramaswamy et al. | Sep 2008 | B2 |
7425224 | Nguyen | Sep 2008 | B2 |
7427571 | Lindeboom et al. | Sep 2008 | B2 |
7429532 | Ramaswamy et al. | Sep 2008 | B2 |
7431966 | Derderian et al. | Oct 2008 | B2 |
7432476 | Morita et al. | Oct 2008 | B2 |
7437060 | Wang et al. | Oct 2008 | B2 |
7442275 | Cowans | Oct 2008 | B2 |
7456429 | Levy | Nov 2008 | B2 |
D583395 | Ueda | Dec 2008 | S |
7467632 | Lee et al. | Dec 2008 | B2 |
7473655 | Wang et al. | Jan 2009 | B2 |
7475588 | Dimeo et al. | Jan 2009 | B2 |
7476291 | Wang et al. | Jan 2009 | B2 |
7479198 | Guffrey | Jan 2009 | B2 |
7482247 | Papasouliotis | Jan 2009 | B1 |
7482283 | Yamasaki et al. | Jan 2009 | B2 |
D585968 | Elkins et al. | Feb 2009 | S |
7489389 | Shibazaki et al. | Feb 2009 | B2 |
7494882 | Vitale | Feb 2009 | B2 |
7497614 | Gaff | Mar 2009 | B2 |
7498242 | Kumar et al. | Mar 2009 | B2 |
7501292 | Matsushita et al. | Mar 2009 | B2 |
7501355 | Bhatia et al. | Mar 2009 | B2 |
7503980 | Kida et al. | Mar 2009 | B2 |
7504344 | Matsuki et al. | Mar 2009 | B2 |
D590933 | Vansell | Apr 2009 | S |
7514058 | Hitzman et al. | Apr 2009 | B1 |
7514375 | Shanker et al. | Apr 2009 | B1 |
D593585 | Ota et al. | Jun 2009 | S |
D593969 | Li | Jun 2009 | S |
7541297 | Mallick et al. | Jun 2009 | B2 |
7544398 | Chang et al. | Jun 2009 | B1 |
7547363 | Tomiyasu et al. | Jun 2009 | B2 |
7547633 | Ravish et al. | Jun 2009 | B2 |
7550396 | Frohberg et al. | Jun 2009 | B2 |
D596476 | Welch | Jul 2009 | S |
7561982 | Rund et al. | Jul 2009 | B2 |
7563715 | Haukka et al. | Jul 2009 | B2 |
7566891 | Rocha-Alvarez et al. | Jul 2009 | B2 |
7569193 | Ferron et al. | Aug 2009 | B2 |
7575968 | Sadaka et al. | Aug 2009 | B2 |
7579285 | Zimmerman et al. | Aug 2009 | B2 |
7579785 | Shinmen et al. | Aug 2009 | B2 |
D600223 | Aggarwal | Sep 2009 | S |
7582555 | Lang | Sep 2009 | B1 |
7582575 | Fukazawa et al. | Sep 2009 | B2 |
7589003 | Kouvetakis et al. | Sep 2009 | B2 |
7589028 | Cho et al. | Sep 2009 | B1 |
7589029 | Derderian et al. | Sep 2009 | B2 |
7591601 | Matsuoka et al. | Sep 2009 | B2 |
7591907 | Chen et al. | Sep 2009 | B2 |
D602575 | Breda | Oct 2009 | S |
7598513 | Kouvetakis et al. | Oct 2009 | B2 |
7601223 | Lindfors et al. | Oct 2009 | B2 |
7601225 | Tuominen et al. | Oct 2009 | B2 |
7601652 | Singh et al. | Oct 2009 | B2 |
7611640 | Howald et al. | Nov 2009 | B1 |
7611751 | Elers | Nov 2009 | B2 |
7611980 | Wells et al. | Nov 2009 | B2 |
7618226 | Takizawa | Nov 2009 | B2 |
7621672 | Ripley | Nov 2009 | B2 |
7622369 | Lee et al. | Nov 2009 | B1 |
7622378 | Liu et al. | Nov 2009 | B2 |
7623940 | Huskamp et al. | Nov 2009 | B2 |
D606952 | Lee | Dec 2009 | S |
7625820 | Papasouliotis | Dec 2009 | B1 |
7629277 | Ghatnagar | Dec 2009 | B2 |
7632549 | Goundar | Dec 2009 | B2 |
7638951 | DeVincentis et al. | Dec 2009 | B2 |
7640142 | Tachikawa et al. | Dec 2009 | B2 |
7645341 | Kennedy et al. | Jan 2010 | B2 |
7645484 | Ishizaka | Jan 2010 | B2 |
7648895 | Kurokawa et al. | Jan 2010 | B2 |
7648927 | Singh et al. | Jan 2010 | B2 |
7651269 | Comendant | Jan 2010 | B2 |
7651583 | Kent et al. | Jan 2010 | B2 |
7651955 | Ravish et al. | Jan 2010 | B2 |
7651959 | Fukazawa et al. | Jan 2010 | B2 |
7651961 | Clark | Jan 2010 | B2 |
D609652 | Nagasaka | Feb 2010 | S |
D609655 | Sugimoto | Feb 2010 | S |
7661299 | Kusunoki | Feb 2010 | B2 |
7670432 | Li | Mar 2010 | B2 |
7674726 | Hasper et al. | Mar 2010 | B2 |
7678197 | Maki | Mar 2010 | B2 |
7678715 | Mungekar et al. | Mar 2010 | B2 |
7682454 | Sneh | Mar 2010 | B2 |
7682657 | Sherman | Mar 2010 | B2 |
D613829 | Griffin et al. | Apr 2010 | S |
D614153 | Fondurulia et al. | Apr 2010 | S |
D614267 | Breda | Apr 2010 | S |
D614268 | Breda | Apr 2010 | S |
D614593 | Lee | Apr 2010 | S |
7690881 | Yamagishi | Apr 2010 | B2 |
7691205 | Ikedo | Apr 2010 | B2 |
7692171 | Kaszuba et al. | Apr 2010 | B2 |
7695808 | Tuma | Apr 2010 | B2 |
D616390 | Sato | May 2010 | S |
D616394 | Sato | May 2010 | S |
7712435 | Yoshizaki et al. | May 2010 | B2 |
7713874 | Milligan | May 2010 | B2 |
7716993 | Ozawa et al. | May 2010 | B2 |
7718930 | Kawasaki et al. | May 2010 | B2 |
7720560 | Menser et al. | May 2010 | B2 |
7723648 | Tsukamoto et al. | May 2010 | B2 |
7725012 | Aggarwal et al. | May 2010 | B2 |
7727864 | Elers | Jun 2010 | B2 |
7732343 | Niroomand et al. | Jun 2010 | B2 |
7736437 | Cadwell et al. | Jun 2010 | B2 |
7736528 | Okita et al. | Jun 2010 | B2 |
7736600 | Clark et al. | Jun 2010 | B2 |
7737035 | Lind et al. | Jun 2010 | B1 |
7740437 | de Ridder et al. | Jun 2010 | B2 |
7740705 | Li | Jun 2010 | B2 |
7745346 | Hausmann et al. | Jun 2010 | B2 |
7748760 | Kushida | Jul 2010 | B2 |
7749563 | Zheng et al. | Jul 2010 | B2 |
7753584 | Gambino et al. | Jul 2010 | B2 |
7754621 | Putjkonen | Jul 2010 | B2 |
7758698 | Bang et al. | Jul 2010 | B2 |
7763869 | Matsushita et al. | Jul 2010 | B2 |
7767262 | Clark | Aug 2010 | B2 |
7771796 | Kohno et al. | Aug 2010 | B2 |
7780440 | Shibagaki et al. | Aug 2010 | B2 |
7780789 | Wu et al. | Aug 2010 | B2 |
7781352 | Fukazawa et al. | Aug 2010 | B2 |
7789559 | Waser et al. | Sep 2010 | B2 |
7789965 | Matsushita et al. | Sep 2010 | B2 |
7790633 | Tarafdar et al. | Sep 2010 | B1 |
7794546 | Li | Sep 2010 | B2 |
7798096 | Mahajani et al. | Sep 2010 | B2 |
7799300 | Lindfors et al. | Sep 2010 | B2 |
7799706 | Yeom et al. | Sep 2010 | B2 |
7803722 | Liang | Sep 2010 | B2 |
D625977 | Watson et al. | Oct 2010 | S |
7795160 | Wang et al. | Oct 2010 | B2 |
7806587 | Kobayashi | Oct 2010 | B2 |
7807566 | Tsuji et al. | Oct 2010 | B2 |
7807578 | Bencher et al. | Oct 2010 | B2 |
7816278 | Reed et al. | Oct 2010 | B2 |
7824492 | Tois et al. | Nov 2010 | B2 |
7825040 | Fukazawa et al. | Nov 2010 | B1 |
7829460 | Streck et al. | Nov 2010 | B2 |
7833348 | Wada et al. | Nov 2010 | B2 |
7833353 | Furukawahara et al. | Nov 2010 | B2 |
7838084 | Derderian et al. | Nov 2010 | B2 |
7842518 | Miyajima | Nov 2010 | B2 |
7842622 | Lee et al. | Nov 2010 | B1 |
D629874 | Hermans | Dec 2010 | S |
7850449 | Yang et al. | Dec 2010 | B2 |
7851019 | Tuominen et al. | Dec 2010 | B2 |
7851232 | van Schravendijk et al. | Dec 2010 | B2 |
7858519 | Liu et al. | Dec 2010 | B2 |
7858533 | Liu et al. | Dec 2010 | B2 |
7865070 | Nakamura | Jan 2011 | B2 |
7871198 | Rempe et al. | Jan 2011 | B2 |
7874726 | Jacobs et al. | Jan 2011 | B2 |
7884918 | Hattori | Feb 2011 | B2 |
7888233 | Gauri | Feb 2011 | B1 |
7894474 | Bell | Feb 2011 | B1 |
D634329 | Wastrom | Mar 2011 | S |
D634719 | Yasuda et al. | Mar 2011 | S |
7897215 | Fair et al. | Mar 2011 | B1 |
7897217 | Faguet | Mar 2011 | B2 |
7902009 | Simonelli et al. | Mar 2011 | B2 |
7902582 | Forbes et al. | Mar 2011 | B2 |
7906174 | Wu et al. | Mar 2011 | B1 |
7910288 | Abatchev et al. | Mar 2011 | B2 |
7910452 | Roh et al. | Mar 2011 | B2 |
7910494 | Dip et al. | Mar 2011 | B2 |
7915139 | Lang | Mar 2011 | B1 |
7915667 | Knoefler et al. | Mar 2011 | B2 |
7919142 | Yeom et al. | Apr 2011 | B2 |
7919416 | Lee et al. | Apr 2011 | B2 |
7923382 | Huotari et al. | Apr 2011 | B2 |
7925378 | Gilchrist et al. | Apr 2011 | B2 |
7935940 | Smargiassi | May 2011 | B1 |
7939447 | Bauer et al. | May 2011 | B2 |
7942969 | Riker et al. | May 2011 | B2 |
7946762 | Yednak | May 2011 | B2 |
7951262 | Koshiishi et al. | May 2011 | B2 |
7955516 | Chandrachood | Jun 2011 | B2 |
7955646 | Cruse et al. | Jun 2011 | B2 |
7955650 | Tsuji | Jun 2011 | B2 |
7957708 | Karschnia et al. | Jun 2011 | B2 |
7963736 | Takizawa et al. | Jun 2011 | B2 |
7967913 | Hua et al. | Jun 2011 | B2 |
7972980 | Lee et al. | Jul 2011 | B2 |
7977256 | Liu et al. | Jul 2011 | B2 |
7981751 | Zhu et al. | Jul 2011 | B2 |
D643055 | Takahashi | Aug 2011 | S |
7989365 | Park et al. | Aug 2011 | B2 |
7989736 | Park et al. | Aug 2011 | B2 |
7992318 | Kawaji | Aug 2011 | B2 |
7993457 | Krotov et al. | Aug 2011 | B1 |
7994070 | Dip et al. | Aug 2011 | B1 |
7994721 | Espiau et al. | Aug 2011 | B2 |
7997795 | Schwagerman et al. | Aug 2011 | B2 |
7998875 | DeYoung | Aug 2011 | B2 |
8003174 | Fukazawa | Aug 2011 | B2 |
8003919 | Goto et al. | Aug 2011 | B2 |
8004198 | Bakre et al. | Aug 2011 | B2 |
8020315 | Nishimura | Sep 2011 | B2 |
8030129 | Jeong | Oct 2011 | B2 |
8033771 | Gage et al. | Oct 2011 | B1 |
8038835 | Hayashi et al. | Oct 2011 | B2 |
8041197 | Kasai et al. | Oct 2011 | B2 |
8041450 | Takizawa et al. | Oct 2011 | B2 |
8043972 | Liu et al. | Oct 2011 | B1 |
8046193 | Yetter et al. | Oct 2011 | B2 |
8047711 | Ploechinger | Nov 2011 | B2 |
8048783 | Chung et al. | Nov 2011 | B2 |
8051799 | Itagaki et al. | Nov 2011 | B2 |
8052794 | Sumakeris et al. | Nov 2011 | B2 |
8055378 | Numakura | Nov 2011 | B2 |
8060252 | Gage et al. | Nov 2011 | B2 |
8083853 | Choi et al. | Nov 2011 | B2 |
RE43023 | Nakashima et al. | Dec 2011 | E |
D649986 | Fujikata et al. | Dec 2011 | S |
D651291 | Liebson et al. | Dec 2011 | S |
8071451 | Berry | Dec 2011 | B2 |
8071452 | Raisanen | Dec 2011 | B2 |
8072578 | Yasuda et al. | Dec 2011 | B2 |
8076230 | Wei | Dec 2011 | B2 |
8076237 | Uzoh | Dec 2011 | B2 |
8076250 | Rajagopalan | Dec 2011 | B1 |
8076251 | Akae et al. | Dec 2011 | B2 |
8078310 | Nishimoto et al. | Dec 2011 | B2 |
8082946 | Laverdiere et al. | Dec 2011 | B2 |
8084104 | Shinriki et al. | Dec 2011 | B2 |
8084372 | You et al. | Dec 2011 | B2 |
D652896 | Gether | Jan 2012 | S |
8092604 | Tomiyasu et al. | Jan 2012 | B2 |
8092606 | Park et al. | Jan 2012 | B2 |
8100583 | Aggarwal | Jan 2012 | B2 |
D653734 | Sisk | Feb 2012 | S |
D654882 | Honma et al. | Feb 2012 | S |
D654884 | Honma | Feb 2012 | S |
D655055 | Toll | Feb 2012 | S |
8110099 | Hersey et al. | Feb 2012 | B2 |
8114734 | Yang et al. | Feb 2012 | B2 |
8119466 | Avouris | Feb 2012 | B2 |
8119527 | Chadrashekar et al. | Feb 2012 | B1 |
D655260 | Honma et al. | Mar 2012 | S |
D655261 | Honma et al. | Mar 2012 | S |
D655599 | Durham | Mar 2012 | S |
8129290 | Balseanu et al. | Mar 2012 | B2 |
8137462 | Fondurulia et al. | Mar 2012 | B2 |
8137465 | Shrinivasan et al. | Mar 2012 | B1 |
8138104 | Balseanu et al. | Mar 2012 | B2 |
8138676 | Mills | Mar 2012 | B2 |
8142862 | Lee et al. | Mar 2012 | B2 |
8143174 | Xia et al. | Mar 2012 | B2 |
8147242 | Shibagaki et al. | Apr 2012 | B2 |
8152922 | Schmidt et al. | Apr 2012 | B2 |
8158512 | Ji et al. | Apr 2012 | B2 |
8172947 | Shibata et al. | May 2012 | B2 |
8173554 | Lee et al. | May 2012 | B2 |
8174400 | Park et al. | May 2012 | B2 |
8178436 | King et al. | May 2012 | B2 |
8187679 | Dickey et al. | May 2012 | B2 |
8187951 | Wang | May 2012 | B1 |
8192901 | Kageyama | Jun 2012 | B2 |
8196234 | Glunk | Jun 2012 | B2 |
8197915 | Oka et al. | Jun 2012 | B2 |
8198168 | Tanioku | Jun 2012 | B2 |
8202575 | Monsma et al. | Jun 2012 | B2 |
8206506 | Kadkhodayan et al. | Jun 2012 | B2 |
8216380 | White et al. | Jul 2012 | B2 |
8227032 | Dussarrat et al. | Jul 2012 | B2 |
8231799 | Bera et al. | Jul 2012 | B2 |
D665055 | Yanagisawa et al. | Aug 2012 | S |
8241991 | Hsieh et al. | Aug 2012 | B2 |
8241992 | Clevenger et al. | Aug 2012 | B2 |
8242028 | van Schravendijk | Aug 2012 | B1 |
8242031 | Mallick et al. | Aug 2012 | B2 |
8246900 | Kasai et al. | Aug 2012 | B2 |
8252114 | Vukovic | Aug 2012 | B2 |
8252659 | Huyghabaert et al. | Aug 2012 | B2 |
8252691 | Beynet et al. | Aug 2012 | B2 |
8267633 | Obikane | Sep 2012 | B2 |
8272516 | Salvador | Sep 2012 | B2 |
8278176 | Bauer et al. | Oct 2012 | B2 |
8282769 | Iizuka | Oct 2012 | B2 |
8282847 | Romano | Oct 2012 | B2 |
8282992 | Myo et al. | Oct 2012 | B2 |
8287648 | Reed et al. | Oct 2012 | B2 |
8291857 | Lam et al. | Oct 2012 | B2 |
8293016 | Bahng et al. | Oct 2012 | B2 |
8293642 | Kim | Oct 2012 | B2 |
8298336 | Wang et al. | Oct 2012 | B2 |
8298951 | Nakano | Oct 2012 | B1 |
8307472 | Saxon et al. | Nov 2012 | B1 |
8309173 | Tuominen et al. | Nov 2012 | B2 |
8318327 | O'Donnell | Nov 2012 | B2 |
8323413 | Son | Dec 2012 | B2 |
8328939 | Choi et al. | Dec 2012 | B2 |
8329599 | Fukazawa et al. | Dec 2012 | B2 |
8333839 | Oh | Dec 2012 | B2 |
8334219 | Lee et al. | Dec 2012 | B2 |
8338809 | Yang et al. | Dec 2012 | B2 |
8349083 | Takasuka et al. | Jan 2013 | B2 |
D676943 | Kluss | Feb 2013 | S |
8367528 | Bauer et al. | Feb 2013 | B2 |
8372204 | Nakamura | Feb 2013 | B2 |
8378464 | Kato et al. | Feb 2013 | B2 |
8382370 | Aggarwal et al. | Feb 2013 | B2 |
8382939 | Kutney et al. | Feb 2013 | B2 |
8393091 | Kawamoto | Mar 2013 | B2 |
8394466 | Hong et al. | Mar 2013 | B2 |
8398773 | Jdira et al. | Mar 2013 | B2 |
8402918 | Kadkhodayan et al. | Mar 2013 | B2 |
8404499 | Moffatt | Mar 2013 | B2 |
8415258 | Akae | Apr 2013 | B2 |
8415259 | Lee et al. | Apr 2013 | B2 |
8415587 | Millman et al. | Apr 2013 | B2 |
8419959 | Bettencourt et al. | Apr 2013 | B2 |
8425682 | Wang et al. | Apr 2013 | B2 |
8430620 | Blank et al. | Apr 2013 | B1 |
8440259 | Chiang et al. | May 2013 | B2 |
8444120 | Gregg et al. | May 2013 | B2 |
8445075 | Xu et al. | May 2013 | B2 |
8450191 | Wang | May 2013 | B2 |
8454749 | Li | Jun 2013 | B2 |
8465811 | Ueda | Jun 2013 | B2 |
8465903 | Weidman et al. | Jun 2013 | B2 |
8466411 | Arai | Jun 2013 | B2 |
8470187 | Ha | Jun 2013 | B2 |
8470718 | Lee | Jun 2013 | B2 |
8484846 | Dhindsa | Jul 2013 | B2 |
8492170 | Xie et al. | Jul 2013 | B2 |
8496377 | Harr et al. | Jul 2013 | B2 |
8496756 | Cruse et al. | Jul 2013 | B2 |
8497213 | Yasui et al. | Jul 2013 | B2 |
8501599 | Ueno et al. | Aug 2013 | B2 |
8506162 | Schick et al. | Aug 2013 | B2 |
8506713 | Takagi | Aug 2013 | B2 |
8524612 | Li et al. | Sep 2013 | B2 |
8529701 | Morita | Sep 2013 | B2 |
8535767 | Kimura | Sep 2013 | B1 |
8536068 | Weidman et al. | Sep 2013 | B2 |
D691974 | Osada et al. | Oct 2013 | S |
8551892 | Nakano | Oct 2013 | B2 |
8557712 | Antonelli et al. | Oct 2013 | B1 |
8562272 | Lenz | Oct 2013 | B2 |
8563443 | Fukazawa | Oct 2013 | B2 |
8569184 | Oka | Oct 2013 | B2 |
D693200 | Saunders | Nov 2013 | S |
8573152 | de la Llera et al. | Nov 2013 | B2 |
8573154 | Yorozuya | Nov 2013 | B2 |
8586484 | Matsuyama et al. | Nov 2013 | B2 |
8591659 | Fang et al. | Nov 2013 | B1 |
8592005 | Ueda | Nov 2013 | B2 |
D694790 | Matsumoto et al. | Dec 2013 | S |
D695240 | Iida et al. | Dec 2013 | S |
8608885 | Goto et al. | Dec 2013 | B2 |
8614047 | Ayothi et al. | Dec 2013 | B2 |
8616765 | Darabnia et al. | Dec 2013 | B2 |
8617411 | Singh | Dec 2013 | B2 |
D697038 | Matsumoto et al. | Jan 2014 | S |
8623770 | Gao et al. | Jan 2014 | B1 |
8633115 | Chang et al. | Jan 2014 | B2 |
D698904 | Milligan et al. | Feb 2014 | S |
8642488 | Liu et al. | Feb 2014 | B2 |
8647439 | Sanchez et al. | Feb 2014 | B2 |
8647722 | Kobayashi et al. | Feb 2014 | B2 |
8647993 | Lavoie et al. | Feb 2014 | B2 |
8651788 | Budde | Feb 2014 | B1 |
8664627 | Ishikawa et al. | Mar 2014 | B1 |
8667654 | Gros-Jean | Mar 2014 | B2 |
8668957 | Dussarrat et al. | Mar 2014 | B2 |
8669185 | Onizawa | Mar 2014 | B2 |
8679958 | Takamure et al. | Mar 2014 | B2 |
D702188 | Jacobs | Apr 2014 | S |
8683943 | Onodera et al. | Apr 2014 | B2 |
8697198 | Lee | Apr 2014 | B2 |
8703002 | Matsudo et al. | Apr 2014 | B2 |
8709162 | Leung et al. | Apr 2014 | B2 |
8710580 | Sakuma et al. | Apr 2014 | B2 |
8711338 | Liu et al. | Apr 2014 | B2 |
D705745 | Kurs et al. | May 2014 | S |
D705762 | Yu | May 2014 | S |
8664127 | Bhatia et al. | May 2014 | B2 |
8720965 | Hino et al. | May 2014 | B2 |
8721791 | Choi et al. | May 2014 | B2 |
8722510 | Watanabe et al. | May 2014 | B2 |
8722546 | Fukazawa et al. | May 2014 | B2 |
8726837 | Patalay et al. | May 2014 | B2 |
8728832 | Raisanen et al. | May 2014 | B2 |
8728956 | Lavoie et al. | May 2014 | B2 |
8741062 | Lindfors et al. | Jun 2014 | B2 |
8741065 | Odagiri et al. | Jun 2014 | B2 |
8742668 | Nakano et al. | Jun 2014 | B2 |
8758512 | Lee | Jun 2014 | B2 |
8759223 | Sapre et al. | Jun 2014 | B2 |
D709536 | Yoshimura et al. | Jul 2014 | S |
D709537 | Kuwabara et al. | Jul 2014 | S |
8764085 | Urabe | Jul 2014 | B2 |
8771791 | Lee et al. | Jul 2014 | B2 |
8771807 | Xiao et al. | Jul 2014 | B2 |
8779502 | Sakuma et al. | Jul 2014 | B2 |
8784950 | Fukazawa et al. | Jul 2014 | B2 |
8784951 | Fukazawa et al. | Jul 2014 | B2 |
8785215 | Kobayashi et al. | Jul 2014 | B2 |
8785311 | Miyoshi | Jul 2014 | B2 |
8790743 | Omari | Jul 2014 | B1 |
8790749 | Omori et al. | Jul 2014 | B2 |
8802201 | Raisanen et al. | Aug 2014 | B2 |
8809170 | Bauer | Aug 2014 | B2 |
D712358 | Allen et al. | Sep 2014 | S |
D712359 | Allen et al. | Sep 2014 | S |
8820809 | Ando et al. | Sep 2014 | B2 |
8821640 | Cleary et al. | Sep 2014 | B2 |
8821985 | Shao et al. | Sep 2014 | B2 |
8823672 | Kim | Sep 2014 | B2 |
8828886 | Samukawa et al. | Sep 2014 | B2 |
8841182 | Chen et al. | Sep 2014 | B1 |
8845806 | Aida et al. | Sep 2014 | B2 |
8846502 | Haukka et al. | Sep 2014 | B2 |
D715410 | Lohmann | Oct 2014 | S |
8859368 | Deniz | Oct 2014 | B2 |
8860955 | Rodnick et al. | Oct 2014 | B2 |
8864202 | Schrameyer | Oct 2014 | B1 |
8864375 | Abe et al. | Oct 2014 | B2 |
D716742 | Jang et al. | Nov 2014 | S |
8876974 | Wan | Nov 2014 | B2 |
8877300 | Lee | Nov 2014 | B2 |
8877655 | Shero et al. | Nov 2014 | B2 |
8882923 | Saido et al. | Nov 2014 | B2 |
8883270 | Shero et al. | Nov 2014 | B2 |
8895108 | Lee | Nov 2014 | B2 |
8900935 | Guo et al. | Dec 2014 | B2 |
8900999 | Wu et al. | Dec 2014 | B1 |
8901016 | Jeongseok et al. | Dec 2014 | B2 |
8911553 | Baluja et al. | Dec 2014 | B2 |
8911826 | Adachi et al. | Dec 2014 | B2 |
8912101 | Tsuji et al. | Dec 2014 | B2 |
D720838 | Yamagishi et al. | Jan 2015 | S |
8927906 | Tadokoro et al. | Jan 2015 | B2 |
8932802 | Wu et al. | Jan 2015 | B2 |
8933375 | Dunn et al. | Jan 2015 | B2 |
8940646 | Chandrasekharan | Jan 2015 | B1 |
D723153 | Borkholder | Feb 2015 | S |
8945305 | Marsh | Feb 2015 | B2 |
8945306 | Tsuda | Feb 2015 | B2 |
8945339 | Kakimoto | Feb 2015 | B2 |
8946830 | Jung et al. | Feb 2015 | B2 |
8956971 | Huakka | Feb 2015 | B2 |
8956983 | Swaminathan | Feb 2015 | B2 |
D723330 | York | Mar 2015 | S |
D724553 | Choi | Mar 2015 | S |
D724701 | Yamagishi et al. | Mar 2015 | S |
D725168 | Yamagishi | Mar 2015 | S |
8967608 | Mitsumori et al. | Mar 2015 | B2 |
8974868 | Ishikawa et al. | Mar 2015 | B2 |
8980006 | Huh et al. | Mar 2015 | B2 |
8986456 | Fondurulia et al. | Mar 2015 | B2 |
8991214 | Hoshino et al. | Mar 2015 | B2 |
8991887 | Shin et al. | Mar 2015 | B2 |
8993054 | Jung et al. | Mar 2015 | B2 |
8993457 | Ramkumar et al. | Mar 2015 | B1 |
D726365 | Weigensberg | Apr 2015 | S |
D726884 | Yamagishi et al. | Apr 2015 | S |
8999102 | Miyoshi et al. | Apr 2015 | B2 |
9004744 | Kemp | Apr 2015 | B1 |
9005539 | Halpin et al. | Apr 2015 | B2 |
9017481 | Pettinger et al. | Apr 2015 | B1 |
9017933 | Liu et al. | Apr 2015 | B2 |
9018093 | Tsuji et al. | Apr 2015 | B2 |
9018111 | Milligan et al. | Apr 2015 | B2 |
9018567 | de Ridder et al. | Apr 2015 | B2 |
9021985 | Alokozai et al. | May 2015 | B2 |
9023737 | Beynet et al. | May 2015 | B2 |
9023738 | Kato et al. | May 2015 | B2 |
9029244 | Won et al. | May 2015 | B2 |
9029253 | Milligan et al. | May 2015 | B2 |
9029272 | Nakano | May 2015 | B1 |
D732145 | Yamagishi | Jun 2015 | S |
D732644 | Yamagishi et al. | Jun 2015 | S |
D733257 | Schoenherr et al. | Jun 2015 | S |
D733261 | Yamagishi et al. | Jun 2015 | S |
D733262 | Kang | Jun 2015 | S |
9057388 | Comeau et al. | Jun 2015 | B2 |
9064815 | Zhang et al. | Jun 2015 | B2 |
D733843 | Yamagishi | Jul 2015 | S |
D734377 | Hirakida | Jul 2015 | S |
9076635 | Gross et al. | Jul 2015 | B2 |
9076726 | Kauerauf et al. | Jul 2015 | B2 |
D735836 | Yamagishi et al. | Aug 2015 | S |
D736348 | Tan | Aug 2015 | S |
9095869 | Kilpi et al. | Aug 2015 | B2 |
9096931 | Yednak et al. | Aug 2015 | B2 |
9099423 | Weeks et al. | Aug 2015 | B2 |
9099505 | Kusakabe et al. | Aug 2015 | B2 |
9111972 | Takeshita et al. | Aug 2015 | B2 |
9117657 | Nakano et al. | Aug 2015 | B2 |
9117866 | Marquardt et al. | Aug 2015 | B2 |
D739222 | Chadbourne | Sep 2015 | S |
9123510 | Nakano et al. | Sep 2015 | B2 |
9123577 | Fujimoto et al. | Sep 2015 | B2 |
9127358 | Inoue et al. | Sep 2015 | B2 |
9127362 | Scheible et al. | Sep 2015 | B2 |
9129897 | Pore et al. | Sep 2015 | B2 |
9136108 | Matsushita et al. | Sep 2015 | B2 |
9136180 | Machkaoutsan | Sep 2015 | B2 |
9142393 | Okabe et al. | Sep 2015 | B2 |
9142437 | Fosnight et al. | Sep 2015 | B2 |
9142764 | Wang | Sep 2015 | B1 |
9153441 | Takamure et al. | Oct 2015 | B2 |
9163310 | Lee | Oct 2015 | B2 |
9166012 | Sim et al. | Oct 2015 | B2 |
9169975 | Sarin et al. | Oct 2015 | B2 |
9171714 | Mori | Oct 2015 | B2 |
9171715 | Matero | Oct 2015 | B2 |
9171716 | Fukuda | Oct 2015 | B2 |
D742202 | Cyphers et al. | Nov 2015 | S |
D743357 | Vyne | Nov 2015 | S |
D743513 | Yamagishi | Nov 2015 | S |
9174178 | Yudovsky et al. | Nov 2015 | B2 |
9175394 | Berger et al. | Nov 2015 | B2 |
9177784 | Raisanen et al. | Nov 2015 | B2 |
9184047 | Liu et al. | Nov 2015 | B2 |
9184054 | Huang et al. | Nov 2015 | B1 |
9190263 | Ishikawa et al. | Nov 2015 | B2 |
9190264 | Yuasa et al. | Nov 2015 | B2 |
9196483 | Lee et al. | Nov 2015 | B1 |
D745641 | Blum | Dec 2015 | S |
9202727 | Dunn et al. | Dec 2015 | B2 |
9214333 | Sims et al. | Dec 2015 | B1 |
9219006 | Chatterjee | Dec 2015 | B2 |
9223203 | Farm et al. | Dec 2015 | B2 |
9228259 | Haukka et al. | Jan 2016 | B2 |
9240412 | Xie et al. | Jan 2016 | B2 |
9245742 | Haukka | Jan 2016 | B2 |
9252024 | Lam et al. | Feb 2016 | B2 |
9252238 | Trevino et al. | Feb 2016 | B1 |
9257274 | Kang et al. | Feb 2016 | B2 |
9263298 | Matsumoto et al. | Feb 2016 | B2 |
9267204 | Honma | Feb 2016 | B2 |
9267850 | Aggarwal | Feb 2016 | B2 |
D751176 | Schoenherr et al. | Mar 2016 | S |
9275834 | Park et al. | Mar 2016 | B1 |
9281277 | Baek et al. | Mar 2016 | B2 |
9284642 | Nakano | Mar 2016 | B2 |
9287273 | Ragnarsson et al. | Mar 2016 | B2 |
9297705 | Aggarwal | Mar 2016 | B2 |
9299557 | Tolle et al. | Mar 2016 | B2 |
9299595 | Dunn et al. | Mar 2016 | B2 |
D753269 | Yamagishi et al. | Apr 2016 | S |
D753629 | Plattard | Apr 2016 | S |
9305836 | Gates et al. | Apr 2016 | B1 |
9309598 | Wang et al. | Apr 2016 | B2 |
9309978 | Hatch et al. | Apr 2016 | B2 |
9310684 | Meyers et al. | Apr 2016 | B2 |
9312155 | Mori | Apr 2016 | B2 |
9315897 | Byun | Apr 2016 | B2 |
9324811 | Weeks | Apr 2016 | B2 |
9324846 | Camillo | Apr 2016 | B1 |
D756929 | Harck et al. | May 2016 | S |
9331200 | Wang et al. | May 2016 | B1 |
9337054 | Hunks et al. | May 2016 | B2 |
9337057 | Park et al. | May 2016 | B2 |
9341296 | Yednak | May 2016 | B2 |
9343297 | Fukazawa et al. | May 2016 | B1 |
9343308 | Isii | May 2016 | B2 |
9343343 | Mori | May 2016 | B2 |
9343350 | Arai | May 2016 | B2 |
9349620 | Kamata et al. | May 2016 | B2 |
9353440 | Ge et al. | May 2016 | B2 |
9353441 | Chung | May 2016 | B2 |
9355876 | Rejuter et al. | May 2016 | B2 |
9355882 | Wu et al. | May 2016 | B2 |
D759137 | Hassan | Jun 2016 | S |
9362107 | Thadani et al. | Jun 2016 | B2 |
9362137 | Kang et al. | Jun 2016 | B2 |
9362180 | Lee et al. | Jun 2016 | B2 |
9365924 | Nonaka | Jun 2016 | B2 |
9368352 | Takamure et al. | Jun 2016 | B2 |
9370863 | Tsuji et al. | Jun 2016 | B2 |
9378969 | Hsu et al. | Jun 2016 | B2 |
9384987 | Jung et al. | Jul 2016 | B2 |
9390909 | Pasquale et al. | Jul 2016 | B2 |
9394608 | Shero et al. | Jul 2016 | B2 |
9396934 | Tolle | Jul 2016 | B2 |
9396956 | Fukazawa | Jul 2016 | B1 |
9399228 | Breiling et al. | Jul 2016 | B2 |
D764196 | Handler et al. | Aug 2016 | S |
9404587 | Shugrue | Aug 2016 | B2 |
9412564 | Milligan | Aug 2016 | B2 |
9412581 | Thadani et al. | Aug 2016 | B2 |
9412582 | Sasaki et al. | Aug 2016 | B2 |
9418885 | Sung et al. | Aug 2016 | B2 |
9425078 | Tang et al. | Aug 2016 | B2 |
9443725 | Liu et al. | Sep 2016 | B2 |
9447498 | Shiba et al. | Sep 2016 | B2 |
9449793 | Shaji et al. | Sep 2016 | B2 |
9449795 | Sabri et al. | Sep 2016 | B2 |
9455138 | Fukazawa | Sep 2016 | B1 |
9455177 | Park et al. | Sep 2016 | B1 |
9464352 | Nakano et al. | Oct 2016 | B2 |
9472432 | Blank | Oct 2016 | B1 |
9474163 | Tolle et al. | Oct 2016 | B2 |
9478414 | Kobayashi et al. | Oct 2016 | B2 |
9478415 | Kimura | Oct 2016 | B2 |
D770993 | Yoshida et al. | Nov 2016 | S |
9484191 | Winkler | Nov 2016 | B2 |
9496225 | Adusumilli et al. | Nov 2016 | B1 |
9514927 | Tolle et al. | Dec 2016 | B2 |
9514932 | Mallick et al. | Dec 2016 | B2 |
9520289 | Park et al. | Dec 2016 | B2 |
9523148 | Pore et al. | Dec 2016 | B1 |
D777546 | Ishii et al. | Jan 2017 | S |
9543180 | Kamiya | Jan 2017 | B2 |
9556516 | Takamure | Jan 2017 | B2 |
9558931 | Tang | Jan 2017 | B2 |
9564312 | Henri et al. | Feb 2017 | B2 |
9564314 | Takamure et al. | Feb 2017 | B2 |
9570302 | Chang et al. | Feb 2017 | B1 |
9574268 | Dunn et al. | Feb 2017 | B1 |
9576952 | Joshi et al. | Feb 2017 | B2 |
9583333 | Chatterjee | Feb 2017 | B2 |
9583345 | Chen et al. | Feb 2017 | B2 |
D782419 | Willette | Mar 2017 | S |
9589770 | Winkler | Mar 2017 | B2 |
9605342 | Alokozai et al. | Mar 2017 | B2 |
9605343 | Winkler | Mar 2017 | B2 |
9607837 | Namba | Mar 2017 | B1 |
D783351 | Fujino et al. | Apr 2017 | S |
9613801 | Carcasi et al. | Apr 2017 | B2 |
9627221 | Zaitsu et al. | Apr 2017 | B1 |
D785766 | Sato | May 2017 | S |
D787458 | Kim et al. | May 2017 | S |
9640416 | Arai | May 2017 | B2 |
9640448 | Ikegawa et al. | May 2017 | B2 |
9640542 | Lee et al. | May 2017 | B2 |
9644266 | Nasu et al. | May 2017 | B2 |
9647114 | Margetis | May 2017 | B2 |
9657845 | Shugrue | May 2017 | B2 |
9659799 | Lawson | May 2017 | B2 |
9663857 | Nakano et al. | May 2017 | B2 |
9666528 | Bergendahl et al. | May 2017 | B1 |
D789888 | Jang et al. | Jun 2017 | S |
D790041 | Jang et al. | Jun 2017 | S |
9680268 | Finona | Jun 2017 | B1 |
9684234 | Darling et al. | Jun 2017 | B2 |
9685320 | Kang et al. | Jun 2017 | B2 |
9691668 | Chang et al. | Jun 2017 | B2 |
9691771 | Lansalot-Matms | Jun 2017 | B2 |
9698031 | Kobayashi et al. | Jul 2017 | B2 |
9708707 | Ditizio et al. | Jul 2017 | B2 |
9708708 | Isobe et al. | Jul 2017 | B2 |
9711345 | Shiba et al. | Jul 2017 | B2 |
D793352 | Hill | Aug 2017 | S |
D793572 | Kozuka et al. | Aug 2017 | S |
D793976 | Fukushima et al. | Aug 2017 | S |
D795208 | Sasaki et al. | Aug 2017 | S |
9735024 | Zaitsu | Aug 2017 | B2 |
9741546 | Carducci et al. | Aug 2017 | B2 |
9741559 | Shimura et al. | Aug 2017 | B2 |
9745658 | Kang et al. | Aug 2017 | B2 |
9748145 | Kannan et al. | Aug 2017 | B1 |
D796458 | Jang et al. | Sep 2017 | S |
D796670 | Dolk et al. | Sep 2017 | S |
9754779 | Ishikawa | Sep 2017 | B1 |
9754818 | Shin et al. | Sep 2017 | B2 |
9759489 | Kaneko | Sep 2017 | B2 |
9765432 | Ge et al. | Sep 2017 | B2 |
9773818 | Kimura | Sep 2017 | B2 |
9778561 | Marks et al. | Oct 2017 | B2 |
9780225 | Venkatasubramanian et al. | Oct 2017 | B2 |
9786491 | Suzuki et al. | Oct 2017 | B2 |
9786570 | Kang et al. | Oct 2017 | B2 |
9790595 | Jung et al. | Oct 2017 | B2 |
9793115 | Tolle | Oct 2017 | B2 |
9793135 | Zaitsu et al. | Oct 2017 | B1 |
9793148 | Yamagishi et al. | Oct 2017 | B2 |
9798308 | Mimura | Oct 2017 | B2 |
9799736 | Ebrish et al. | Oct 2017 | B1 |
D802546 | Jang et al. | Nov 2017 | S |
9808246 | Shelton et al. | Nov 2017 | B2 |
9812319 | Fukazawa et al. | Nov 2017 | B1 |
9812320 | Pore et al. | Nov 2017 | B1 |
9820289 | Pawar et al. | Nov 2017 | B1 |
9824884 | Sims et al. | Nov 2017 | B1 |
9824893 | Smith et al. | Nov 2017 | B1 |
9847221 | McLaughlin et al. | Dec 2017 | B1 |
D808254 | Deleu | Jan 2018 | S |
9859151 | Niskanen | Jan 2018 | B1 |
9865455 | Sims et al. | Jan 2018 | B1 |
9865456 | Pandey et al. | Jan 2018 | B1 |
9865815 | Hausmann | Jan 2018 | B2 |
9868131 | Kilpi et al. | Jan 2018 | B2 |
9870964 | Yoshino et al. | Jan 2018 | B1 |
9875891 | Henri et al. | Jan 2018 | B2 |
9875893 | Takamure et al. | Jan 2018 | B2 |
9881788 | Kim et al. | Jan 2018 | B2 |
D810705 | Krishnan et al. | Feb 2018 | S |
9887082 | Pore et al. | Feb 2018 | B1 |
9890456 | Tolle et al. | Feb 2018 | B2 |
9891521 | Kang et al. | Feb 2018 | B2 |
9892908 | Pettinger et al. | Feb 2018 | B2 |
9892913 | Margetis et al. | Feb 2018 | B2 |
9895715 | Haulcka et al. | Feb 2018 | B2 |
9899291 | Kato | Feb 2018 | B2 |
9899405 | Kim | Feb 2018 | B2 |
9905420 | Margetis et al. | Feb 2018 | B2 |
9905492 | Tang et al. | Feb 2018 | B2 |
9909214 | Suemori | Mar 2018 | B2 |
9909492 | Jeswine | Mar 2018 | B2 |
9911676 | Tang | Mar 2018 | B2 |
9916980 | Knaepen | Mar 2018 | B1 |
9920451 | Sivaramakrishnan et al. | Mar 2018 | B2 |
9922824 | Okada | Mar 2018 | B2 |
9929005 | Shimamoto et al. | Mar 2018 | B1 |
9929011 | Hawryluk et al. | Mar 2018 | B2 |
9951421 | Lind | Apr 2018 | B2 |
9960033 | Nozawa | May 2018 | B1 |
9960072 | Coomer | May 2018 | B2 |
9966299 | Tang et al. | May 2018 | B2 |
9984869 | Blanquart | May 2018 | B1 |
D819580 | Krishnan et al. | Jun 2018 | S |
9987747 | Hwang et al. | Jun 2018 | B2 |
9991138 | Lin et al. | Jun 2018 | B2 |
9996004 | Smith et al. | Jun 2018 | B2 |
9997357 | Arghavani et al. | Jun 2018 | B2 |
9997373 | Hudson | Jun 2018 | B2 |
10032628 | Xie et al. | Jun 2018 | B2 |
10014212 | Chen et al. | Jul 2018 | B2 |
10017856 | Arnepalli et al. | Jul 2018 | B1 |
10018920 | Chang et al. | Jul 2018 | B2 |
10023960 | Alokozai | Jul 2018 | B2 |
10032792 | Kim et al. | Jul 2018 | B2 |
10043661 | Kato et al. | Aug 2018 | B2 |
10047435 | Haukka et al. | Aug 2018 | B2 |
10053774 | Tolle et al. | Aug 2018 | B2 |
10060473 | Davey et al. | Aug 2018 | B2 |
D827592 | Ichino et al. | Sep 2018 | S |
10083836 | Milligan | Sep 2018 | B2 |
D830981 | Jeong et al. | Oct 2018 | S |
10087522 | Raisanen et al. | Oct 2018 | B2 |
10087525 | Schmotzer et al. | Oct 2018 | B2 |
10090316 | Ootsuka | Oct 2018 | B2 |
10103040 | Oosterlaken et al. | Oct 2018 | B1 |
10106892 | Siddiqui et al. | Oct 2018 | B1 |
RE47145 | Hashimoto | Nov 2018 | E |
10121671 | Fu et al. | Nov 2018 | B2 |
10134617 | Gurary et al. | Nov 2018 | B2 |
10134757 | Chun et al. | Nov 2018 | B2 |
RE47170 | Beynet et al. | Dec 2018 | E |
10147600 | Takamure et al. | Dec 2018 | B2 |
10167557 | Hawkins et al. | Jan 2019 | B2 |
10177024 | Gomm et al. | Jan 2019 | B2 |
10177025 | Pore | Jan 2019 | B2 |
10179947 | Fukazawa | Jan 2019 | B2 |
10186420 | Fukazawa | Jan 2019 | B2 |
10190213 | Zhu et al. | Jan 2019 | B2 |
10190214 | Shon et al. | Jan 2019 | B2 |
10190701 | Raj et al. | Jan 2019 | B2 |
10192734 | Sanchez et al. | Jan 2019 | B2 |
10193429 | Smith et al. | Jan 2019 | B2 |
D840364 | Ichino et al. | Feb 2019 | S |
10204788 | Ye et al. | Feb 2019 | B1 |
10211308 | Zhu et al. | Feb 2019 | B2 |
10229833 | Raisanen et al. | Mar 2019 | B2 |
10236177 | Kohen et al. | Mar 2019 | B1 |
10249524 | den Hartog Besselink et al. | Apr 2019 | B2 |
10249577 | Lee et al. | Apr 2019 | B2 |
10262859 | Margetis et al. | Apr 2019 | B2 |
10269558 | Blanquart et al. | Apr 2019 | B2 |
10276355 | White et al. | Apr 2019 | B2 |
D849662 | Rike | May 2019 | S |
10283353 | Kobayashi et al. | May 2019 | B2 |
10287684 | Yanai et al. | May 2019 | B2 |
10290508 | Kubota et al. | May 2019 | B1 |
10297440 | Yamazaki et al. | May 2019 | B2 |
RE47440 | Yudovsky et al. | Jun 2019 | E |
10312055 | Suzuki | Jun 2019 | B2 |
10312129 | Coomer | Jun 2019 | B2 |
10319588 | Mattinen et al. | Jun 2019 | B2 |
10322384 | Stumpf et al. | Jun 2019 | B2 |
10332963 | Xie | Jun 2019 | B1 |
D855089 | Hopkins | Jul 2019 | S |
10340125 | Winkler | Jul 2019 | B2 |
10340135 | Blanquart | Jul 2019 | B2 |
10343920 | Haukka | Jul 2019 | B2 |
10347547 | Varadarajan et al. | Jul 2019 | B2 |
10354873 | Ko et al. | Jul 2019 | B2 |
10361201 | Xie et al. | Jul 2019 | B2 |
10361366 | Hakamata et al. | Jul 2019 | B2 |
10367080 | Tang et al. | Jul 2019 | B2 |
10388513 | Blanquart | Aug 2019 | B1 |
10395917 | Niskanen et al. | Aug 2019 | B2 |
10395919 | Masaru et al. | Aug 2019 | B2 |
D859136 | Tenander et al. | Sep 2019 | S |
10400335 | Ge et al. | Sep 2019 | B2 |
10410943 | Jiang et al. | Sep 2019 | B2 |
10428419 | Huotari et al. | Oct 2019 | B2 |
10435790 | Fukazawa et al. | Oct 2019 | B2 |
D867867 | Tenander et al. | Nov 2019 | S |
10468244 | Li et al. | Nov 2019 | B2 |
10468251 | Ishikawa et al. | Nov 2019 | B2 |
10483154 | Smith et al. | Nov 2019 | B1 |
10510871 | More et al. | Dec 2019 | B1 |
10529554 | Ishikawa et al. | Jan 2020 | B2 |
D876504 | Lee et al. | Feb 2020 | S |
10590531 | Shirako et al. | Mar 2020 | B1 |
10600637 | Suzuki et al. | Mar 2020 | B2 |
D880437 | Lee et al. | Apr 2020 | S |
10622196 | Nagayama et al. | Apr 2020 | B2 |
10648788 | Boyd et al. | May 2020 | B2 |
10714335 | Kim et al. | Jul 2020 | B2 |
10763139 | Shindo | Sep 2020 | B2 |
D900036 | Wuester et al. | Oct 2020 | S |
D903477 | Goratela et al. | Dec 2020 | S |
20010000141 | Zhou et al. | Apr 2001 | A1 |
20010001953 | Griffiths et al. | May 2001 | A1 |
20010002581 | Nishikawa et al. | Jun 2001 | A1 |
20010003015 | Chang et al. | Jun 2001 | A1 |
20010003191 | Kovacs et al. | Jun 2001 | A1 |
20010004880 | Cho et al. | Jun 2001 | A1 |
20010006070 | Shang | Jul 2001 | A1 |
20010007246 | Ueda et al. | Jul 2001 | A1 |
20010007645 | Honma | Jul 2001 | A1 |
20010014267 | Yamaga et al. | Aug 2001 | A1 |
20010014514 | Geusic | Aug 2001 | A1 |
20010015343 | Sprey et al. | Aug 2001 | A1 |
20010016273 | Narasimhan et al. | Aug 2001 | A1 |
20010017103 | Takeshita et al. | Aug 2001 | A1 |
20010018267 | Shinriki et al. | Aug 2001 | A1 |
20010019777 | Tanaka et al. | Sep 2001 | A1 |
20010019900 | Hasegawa | Sep 2001 | A1 |
20010020715 | Yamasaki | Sep 2001 | A1 |
20010021591 | Srinivasan et al. | Sep 2001 | A1 |
20010022215 | Donohoe | Sep 2001 | A1 |
20010027026 | Dhindsa et al. | Oct 2001 | A1 |
20010028924 | Sherman | Oct 2001 | A1 |
20010031535 | Agnello et al. | Oct 2001 | A1 |
20010031541 | Madan et al. | Oct 2001 | A1 |
20010034097 | Lim et al. | Oct 2001 | A1 |
20010038783 | Nakashima et al. | Nov 2001 | A1 |
20010039922 | Nakahara | Nov 2001 | A1 |
20010039966 | Walpole et al. | Nov 2001 | A1 |
20010040511 | Bushner et al. | Nov 2001 | A1 |
20010041250 | Werkhoven et al. | Nov 2001 | A1 |
20010042511 | Liu et al. | Nov 2001 | A1 |
20010042594 | Shamouilian et al. | Nov 2001 | A1 |
20010046765 | Cappellani et al. | Nov 2001 | A1 |
20010047761 | Wijck et al. | Dec 2001 | A1 |
20010048981 | Suzuki | Dec 2001 | A1 |
20010049080 | Asano | Dec 2001 | A1 |
20010049202 | Maeda et al. | Dec 2001 | A1 |
20010054388 | Qian | Dec 2001 | A1 |
20020000195 | Bang et al. | Jan 2002 | A1 |
20020000202 | Yuda et al. | Jan 2002 | A1 |
20020001971 | Cho | Jan 2002 | A1 |
20020001974 | Chan | Jan 2002 | A1 |
20020001976 | Danek | Jan 2002 | A1 |
20020005400 | Gat et al. | Jan 2002 | A1 |
20020005943 | Voinalovich | Jan 2002 | A1 |
20020008270 | Marsh | Jan 2002 | A1 |
20020009119 | Matthew et al. | Jan 2002 | A1 |
20020009560 | Ozono | Jan 2002 | A1 |
20020009861 | Narwankar et al. | Jan 2002 | A1 |
20020011210 | Satoh et al. | Jan 2002 | A1 |
20020011211 | Halpin | Jan 2002 | A1 |
20020011310 | Kamarehi et al. | Jan 2002 | A1 |
20020013792 | Imielinski et al. | Jan 2002 | A1 |
20020014204 | Pyo | Feb 2002 | A1 |
20020014483 | Suzuki et al. | Feb 2002 | A1 |
20020016829 | Defosse | Feb 2002 | A1 |
20020020429 | Selbrede et al. | Feb 2002 | A1 |
20020023677 | Zheng | Feb 2002 | A1 |
20020025688 | Kato | Feb 2002 | A1 |
20020027945 | Hirano et al. | Mar 2002 | A1 |
20020030047 | Shao et al. | Mar 2002 | A1 |
20020031644 | Malofsky et al. | Mar 2002 | A1 |
20020041931 | Suntola et al. | Apr 2002 | A1 |
20020043337 | Goodman et al. | Apr 2002 | A1 |
20020045336 | Locati et al. | Apr 2002 | A1 |
20020048634 | Basceri | Apr 2002 | A1 |
20020081826 | Rotondaro et al. | Apr 2002 | A1 |
20020050648 | Kishida et al. | May 2002 | A1 |
20020062633 | Denker et al. | May 2002 | A1 |
20020064592 | Datta et al. | May 2002 | A1 |
20020064598 | Wang et al. | May 2002 | A1 |
20020066532 | Shih et al. | Jun 2002 | A1 |
20020068458 | Chiang et al. | Jun 2002 | A1 |
20020069222 | McNeely | Jun 2002 | A1 |
20020073922 | Frankel et al. | Jun 2002 | A1 |
20020073923 | Saito et al. | Jun 2002 | A1 |
20020076490 | Chiang et al. | Jun 2002 | A1 |
20020076507 | Chiang et al. | Jun 2002 | A1 |
20020076944 | Wang et al. | Jun 2002 | A1 |
20020078893 | Os et al. | Jun 2002 | A1 |
20020079714 | Soucy et al. | Jun 2002 | A1 |
20020086501 | O'Donnell et al. | Jul 2002 | A1 |
20020088542 | Nishikawa et al. | Jul 2002 | A1 |
20020090735 | Kishkovich et al. | Jul 2002 | A1 |
20020094378 | O'Donnell et al. | Jul 2002 | A1 |
20020094388 | Fonash et al. | Jul 2002 | A1 |
20020096211 | Zheng | Jul 2002 | A1 |
20020098627 | Pomarede et al. | Jul 2002 | A1 |
20020099470 | Zinger et al. | Jul 2002 | A1 |
20020100418 | Sandhu et al. | Aug 2002 | A1 |
20020104481 | Chiang et al. | Aug 2002 | A1 |
20020104751 | Drewery et al. | Aug 2002 | A1 |
20020108670 | Baker et al. | Aug 2002 | A1 |
20020108714 | Doering et al. | Aug 2002 | A1 |
20020109115 | Cederstav et al. | Aug 2002 | A1 |
20020110695 | Yang et al. | Aug 2002 | A1 |
20020110991 | Li | Aug 2002 | A1 |
20020112114 | Blair et al. | Aug 2002 | A1 |
20020114886 | Chou et al. | Aug 2002 | A1 |
20020115252 | Haukka et al. | Aug 2002 | A1 |
20020117113 | Tsuruno et al. | Aug 2002 | A1 |
20020122885 | Ahn | Sep 2002 | A1 |
20020123200 | Yamamoto et al. | Sep 2002 | A1 |
20020123230 | Hubacek | Sep 2002 | A1 |
20020123237 | Nguyen et al. | Sep 2002 | A1 |
20020124883 | Zheng | Sep 2002 | A1 |
20020124906 | Suzuki et al. | Sep 2002 | A1 |
20020127350 | Ishikawa et al. | Sep 2002 | A1 |
20020129768 | Carpenter et al. | Sep 2002 | A1 |
20020132408 | Ma et al. | Sep 2002 | A1 |
20020134511 | Ushioda et al. | Sep 2002 | A1 |
20020136214 | Do et al. | Sep 2002 | A1 |
20020136909 | Yang | Sep 2002 | A1 |
20020139775 | Chang | Oct 2002 | A1 |
20020146512 | Rossman | Oct 2002 | A1 |
20020151327 | Levitt | Oct 2002 | A1 |
20020152244 | Dean et al. | Oct 2002 | A1 |
20020155219 | Wang et al. | Oct 2002 | A1 |
20020155708 | Lo et al. | Oct 2002 | A1 |
20020157611 | Bondestam et al. | Oct 2002 | A1 |
20020160112 | Sakai et al. | Oct 2002 | A1 |
20020164420 | Derderian et al. | Nov 2002 | A1 |
20020164423 | Chiang et al. | Nov 2002 | A1 |
20020168870 | Matsuki | Nov 2002 | A1 |
20020170676 | Mitrovic et al. | Nov 2002 | A1 |
20020172768 | Endo et al. | Nov 2002 | A1 |
20020174106 | Martin | Nov 2002 | A1 |
20020179011 | Jonnalagadda et al. | Dec 2002 | A1 |
20020181612 | Warble et al. | Dec 2002 | A1 |
20020184111 | Swanson | Dec 2002 | A1 |
20020187650 | Blalock et al. | Dec 2002 | A1 |
20020187656 | Tan et al. | Dec 2002 | A1 |
20020188376 | Derderian et al. | Dec 2002 | A1 |
20020192370 | Metzner et al. | Dec 2002 | A1 |
20020197402 | Chiang et al. | Dec 2002 | A1 |
20020197849 | Mandal | Dec 2002 | A1 |
20030000647 | Yudovsky et al. | Jan 2003 | A1 |
20030002562 | Yerlikaya et al. | Jan 2003 | A1 |
20030003607 | Kagoshima | Jan 2003 | A1 |
20030003635 | Paranjpe et al. | Jan 2003 | A1 |
20030003696 | Gelatos et al. | Jan 2003 | A1 |
20030003719 | Lim et al. | Jan 2003 | A1 |
20030008528 | Xia et al. | Jan 2003 | A1 |
20030010355 | Nowak et al. | Jan 2003 | A1 |
20030010451 | Tzu | Jan 2003 | A1 |
20030010452 | Park et al. | Jan 2003 | A1 |
20030012632 | Saeki | Jan 2003 | A1 |
20030015141 | Takagi | Jan 2003 | A1 |
20030015294 | Wang | Jan 2003 | A1 |
20030015596 | Evans | Jan 2003 | A1 |
20030017265 | Basceri et al. | Jan 2003 | A1 |
20030017266 | Basceri et al. | Jan 2003 | A1 |
20030017268 | Hu | Jan 2003 | A1 |
20030019428 | Ku et al. | Jan 2003 | A1 |
20030019580 | Strang | Jan 2003 | A1 |
20030022468 | Shioya et al. | Jan 2003 | A1 |
20030022523 | Irino et al. | Jan 2003 | A1 |
20030023338 | Chin et al. | Jan 2003 | A1 |
20030024901 | Ishikawa | Feb 2003 | A1 |
20030025146 | Narwankar et al. | Feb 2003 | A1 |
20030026904 | Yadav et al. | Feb 2003 | A1 |
20030027431 | Sneh et al. | Feb 2003 | A1 |
20030029303 | Hasegawa et al. | Feb 2003 | A1 |
20030029381 | Nishibayashi | Feb 2003 | A1 |
20030029475 | Hua et al. | Feb 2003 | A1 |
20030032297 | Lindstrom et al. | Feb 2003 | A1 |
20030035002 | Moles | Feb 2003 | A1 |
20030035705 | Johnson | Feb 2003 | A1 |
20030036272 | Shamouilian et al. | Feb 2003 | A1 |
20030037800 | Bailey et al. | Feb 2003 | A1 |
20030040120 | Allen et al. | Feb 2003 | A1 |
20030040158 | Saitoh | Feb 2003 | A1 |
20030040196 | Lim et al. | Feb 2003 | A1 |
20030040841 | Nasr et al. | Feb 2003 | A1 |
20030041971 | Kido et al. | Mar 2003 | A1 |
20030042419 | Katsumata et al. | Mar 2003 | A1 |
20030045961 | Nakao | Mar 2003 | A1 |
20030049372 | Cook et al. | Mar 2003 | A1 |
20030049375 | Nguyen et al. | Mar 2003 | A1 |
20030049499 | Murakawa et al. | Mar 2003 | A1 |
20030049937 | Suzuki | Mar 2003 | A1 |
20030054670 | Wang et al. | Mar 2003 | A1 |
20030057848 | Yuasa et al. | Mar 2003 | A1 |
20030059535 | Luo et al. | Mar 2003 | A1 |
20030059980 | Chen et al. | Mar 2003 | A1 |
20030062359 | Ho et al. | Apr 2003 | A1 |
20030065413 | Liteplo et al. | Apr 2003 | A1 |
20030066482 | Pokharna et al. | Apr 2003 | A1 |
20030066541 | Sun et al. | Apr 2003 | A1 |
20030066826 | Lee et al. | Apr 2003 | A1 |
20030070617 | Kim et al. | Apr 2003 | A1 |
20030071015 | Chinn et al. | Apr 2003 | A1 |
20030072882 | Niinisto et al. | Apr 2003 | A1 |
20030075925 | Lindfors et al. | Apr 2003 | A1 |
20030077857 | Xia et al. | Apr 2003 | A1 |
20030077883 | Ohtake | Apr 2003 | A1 |
20030082296 | Elers et al. | May 2003 | A1 |
20030082307 | Chung et al. | May 2003 | A1 |
20030085663 | Horsky | May 2003 | A1 |
20030091938 | Fairbairn et al. | May 2003 | A1 |
20030094133 | Yoshidome et al. | May 2003 | A1 |
20030101938 | Ronsse et al. | Jun 2003 | A1 |
20030109107 | Hsieh et al. | Jun 2003 | A1 |
20030109951 | Hsiung et al. | Jun 2003 | A1 |
20030111013 | Oosterlaken et al. | Jun 2003 | A1 |
20030111963 | Tolmachev et al. | Jun 2003 | A1 |
20030116087 | Nguyen | Jun 2003 | A1 |
20030168750 | Basceri et al. | Jun 2003 | A1 |
20030121608 | Chen | Jul 2003 | A1 |
20030124792 | Jeon et al. | Jul 2003 | A1 |
20030124818 | Luo et al. | Jul 2003 | A1 |
20030124820 | Johnsgard et al. | Jul 2003 | A1 |
20030124842 | Hytros et al. | Jul 2003 | A1 |
20030127049 | Han et al. | Jul 2003 | A1 |
20030133854 | Tabata et al. | Jul 2003 | A1 |
20030134038 | Paranjpe | Jul 2003 | A1 |
20030140851 | Janakiraman et al. | Jul 2003 | A1 |
20030141527 | Joo et al. | Jul 2003 | A1 |
20030141820 | White et al. | Jul 2003 | A1 |
20030143328 | Chen | Jul 2003 | A1 |
20030145789 | Bauch et al. | Aug 2003 | A1 |
20030149506 | Haanstra et al. | Aug 2003 | A1 |
20030153177 | Tepman et al. | Aug 2003 | A1 |
20030153186 | Bar-Gadda | Aug 2003 | A1 |
20030157432 | Rottsegge | Aug 2003 | A1 |
20030157436 | Manger et al. | Aug 2003 | A1 |
20030159653 | Dando et al. | Aug 2003 | A1 |
20030159656 | Tan | Aug 2003 | A1 |
20030162412 | Chung | Aug 2003 | A1 |
20030168001 | Sneh | Sep 2003 | A1 |
20030168008 | Ohmi et al. | Sep 2003 | A1 |
20030168012 | Tamura et al. | Sep 2003 | A1 |
20030168699 | Honda | Sep 2003 | A1 |
20030168948 | Yamagishi et al. | Sep 2003 | A1 |
20030170153 | Bar-Gadda | Sep 2003 | A1 |
20030170583 | Nakashima | Sep 2003 | A1 |
20030170945 | Igeta et al. | Sep 2003 | A1 |
20030173030 | Ishii et al. | Sep 2003 | A1 |
20030173490 | Lappen | Sep 2003 | A1 |
20030176074 | Paterson et al. | Sep 2003 | A1 |
20030178145 | Anderson et al. | Sep 2003 | A1 |
20030180458 | Sneh | Sep 2003 | A1 |
20030183156 | Dando | Oct 2003 | A1 |
20030183856 | Wieczorek et al. | Oct 2003 | A1 |
20030188682 | Tois et al. | Oct 2003 | A1 |
20030188685 | Wang | Oct 2003 | A1 |
20030190804 | Glenn et al. | Oct 2003 | A1 |
20030192875 | Bieker et al. | Oct 2003 | A1 |
20030198587 | Kaloyeros | Oct 2003 | A1 |
20030201541 | Kim | Oct 2003 | A1 |
20030205096 | Gehner et al. | Nov 2003 | A1 |
20030205202 | Funaki et al. | Nov 2003 | A1 |
20030205327 | Howald et al. | Nov 2003 | A1 |
20030207032 | Ahn et al. | Nov 2003 | A1 |
20030209323 | Yokogaki | Nov 2003 | A1 |
20030209326 | Lee et al. | Nov 2003 | A1 |
20030209746 | Horii | Nov 2003 | A1 |
20030210901 | Donald et al. | Nov 2003 | A1 |
20030211735 | Rossman | Nov 2003 | A1 |
20030213435 | Okuda et al. | Nov 2003 | A1 |
20030213560 | Wang et al. | Nov 2003 | A1 |
20030213562 | Gondhalekar et al. | Nov 2003 | A1 |
20030215963 | AmRhein et al. | Nov 2003 | A1 |
20030217915 | Ouellet | Nov 2003 | A1 |
20030219972 | Green | Nov 2003 | A1 |
20030221780 | Lei et al. | Dec 2003 | A1 |
20030226840 | Dalton | Dec 2003 | A1 |
20030228772 | Cowans | Dec 2003 | A1 |
20030230986 | Horsky et al. | Dec 2003 | A1 |
20030231698 | Yamaguchi | Dec 2003 | A1 |
20030232138 | Tuominen et al. | Dec 2003 | A1 |
20030232491 | Yamaguchi | Dec 2003 | A1 |
20030232511 | Metzner et al. | Dec 2003 | A1 |
20030234371 | Ziegler | Dec 2003 | A1 |
20040002224 | Chono et al. | Jan 2004 | A1 |
20040005147 | Wang et al. | Jan 2004 | A1 |
20040009307 | Koh et al. | Jan 2004 | A1 |
20040009679 | Yeo et al. | Jan 2004 | A1 |
20040010772 | McKenna et al. | Jan 2004 | A1 |
20040011504 | Ku et al. | Jan 2004 | A1 |
20040013577 | Ganguli et al. | Jan 2004 | A1 |
20040013818 | Moon et al. | Jan 2004 | A1 |
20040015300 | Ganguli et al. | Jan 2004 | A1 |
20040016637 | Yang | Jan 2004 | A1 |
20040018304 | Chung et al. | Jan 2004 | A1 |
20040018307 | Park et al. | Jan 2004 | A1 |
20040018723 | Byun et al. | Jan 2004 | A1 |
20040018750 | Sophie et al. | Jan 2004 | A1 |
20040023125 | Nozawa et al. | Feb 2004 | A1 |
20040023516 | Londergan et al. | Feb 2004 | A1 |
20040025786 | Kontani et al. | Feb 2004 | A1 |
20040025787 | Selbrede et al. | Feb 2004 | A1 |
20040026372 | Takenaka et al. | Feb 2004 | A1 |
20040029052 | Park et al. | Feb 2004 | A1 |
20040031564 | Gottscho et al. | Feb 2004 | A1 |
20040035358 | Basceri et al. | Feb 2004 | A1 |
20040036129 | Forbes et al. | Feb 2004 | A1 |
20040037339 | Watson et al. | Feb 2004 | A1 |
20040037675 | Zinger et al. | Feb 2004 | A1 |
20040038525 | Meng et al. | Feb 2004 | A1 |
20040043149 | Gordon et al. | Mar 2004 | A1 |
20040043544 | Asai et al. | Mar 2004 | A1 |
20040048439 | Soman | Mar 2004 | A1 |
20040048452 | Sugawara et al. | Mar 2004 | A1 |
20040048492 | Ishikawa et al. | Mar 2004 | A1 |
20040050325 | Samoilov | Mar 2004 | A1 |
20040050496 | Iwai et al. | Mar 2004 | A1 |
20040052972 | Schmitt | Mar 2004 | A1 |
20040056017 | Renken | Mar 2004 | A1 |
20040062081 | Drewes | Apr 2004 | A1 |
20040063289 | Ohta | Apr 2004 | A1 |
20040065255 | Yang et al. | Apr 2004 | A1 |
20040069226 | Yoshida et al. | Apr 2004 | A1 |
20040071897 | Verplancken et al. | Apr 2004 | A1 |
20040077182 | Lim et al. | Apr 2004 | A1 |
20040079286 | Lindfors | Apr 2004 | A1 |
20040079960 | Shakuda | Apr 2004 | A1 |
20040080697 | Song | Apr 2004 | A1 |
20040082171 | Shin et al. | Apr 2004 | A1 |
20040083961 | Basceri | May 2004 | A1 |
20040083964 | Ingle et al. | May 2004 | A1 |
20040083975 | Tong et al. | May 2004 | A1 |
20040087141 | Ramanathan et al. | May 2004 | A1 |
20040087168 | Granneman et al. | May 2004 | A1 |
20040089078 | Gehner et al. | May 2004 | A1 |
20040089236 | Yokogawa et al. | May 2004 | A1 |
20040092073 | Cabral et al. | May 2004 | A1 |
20040092120 | Wicker | May 2004 | A1 |
20040093963 | Gehner et al. | May 2004 | A1 |
20040094206 | Ishida | May 2004 | A1 |
20040094402 | Gopalraja | May 2004 | A1 |
20040095074 | Ishii et al. | May 2004 | A1 |
20040099213 | Adomaitis et al. | May 2004 | A1 |
20040101622 | Park et al. | May 2004 | A1 |
20040103914 | Cheng et al. | Jun 2004 | A1 |
20040105738 | Ahn et al. | Jun 2004 | A1 |
20040106249 | Huotari | Jun 2004 | A1 |
20040115936 | DePetrillo et al. | Jun 2004 | A1 |
20040121620 | Pomarede et al. | Jun 2004 | A1 |
20040124131 | Aitchison | Jul 2004 | A1 |
20040124549 | Curran | Jul 2004 | A1 |
20040126213 | Pelzmann et al. | Jul 2004 | A1 |
20040126990 | Ohta | Jul 2004 | A1 |
20040127069 | Yamazaki et al. | Jul 2004 | A1 |
20040129211 | Blonigan et al. | Jul 2004 | A1 |
20040129671 | Ji et al. | Jul 2004 | A1 |
20040134429 | Yamanaka | Jul 2004 | A1 |
20040137756 | Li et al. | Jul 2004 | A1 |
20040142577 | Sugawara et al. | Jul 2004 | A1 |
20040144311 | Chen | Jul 2004 | A1 |
20040144323 | Kai | Jul 2004 | A1 |
20040144980 | Ahn et al. | Jul 2004 | A1 |
20040146644 | Xia et al. | Jul 2004 | A1 |
20040151844 | Zhang et al. | Aug 2004 | A1 |
20040151845 | Nguyen et al. | Aug 2004 | A1 |
20040152287 | Sherrill et al. | Aug 2004 | A1 |
20040159343 | Shimbara et al. | Aug 2004 | A1 |
20040168627 | Conley et al. | Sep 2004 | A1 |
20040168742 | Kim et al. | Sep 2004 | A1 |
20040168769 | Matsuoka et al. | Sep 2004 | A1 |
20040169032 | Murayama et al. | Sep 2004 | A1 |
20040185177 | Basceri et al. | Sep 2004 | A1 |
20040187304 | Chen et al. | Sep 2004 | A1 |
20040187777 | Okamoto et al. | Sep 2004 | A1 |
20040187784 | Sferlazzo | Sep 2004 | A1 |
20040187790 | Bader | Sep 2004 | A1 |
20040187928 | Ambrosina | Sep 2004 | A1 |
20040198069 | Metzner et al. | Oct 2004 | A1 |
20040200499 | Harvey et al. | Oct 2004 | A1 |
20040202786 | Wongsenakhum et al. | Oct 2004 | A1 |
20040203251 | Kawaguchi et al. | Oct 2004 | A1 |
20040206305 | Choi et al. | Oct 2004 | A1 |
20040208228 | Hashikura et al. | Oct 2004 | A1 |
20040208994 | Harkonen et al. | Oct 2004 | A1 |
20040209477 | Buxbaum et al. | Oct 2004 | A1 |
20040211357 | Gadgil | Oct 2004 | A1 |
20040212947 | Nguyen | Oct 2004 | A1 |
20040213921 | Leu | Oct 2004 | A1 |
20040214399 | Ahn et al. | Oct 2004 | A1 |
20040214445 | Shimizu et al. | Oct 2004 | A1 |
20040217217 | Han et al. | Nov 2004 | A1 |
20040219793 | Hishiya et al. | Nov 2004 | A1 |
20040220699 | Heden et al. | Nov 2004 | A1 |
20040221807 | Verghese et al. | Nov 2004 | A1 |
20040221808 | Kawano | Nov 2004 | A1 |
20040223893 | Tabata et al. | Nov 2004 | A1 |
20040226515 | Yendler et al. | Nov 2004 | A1 |
20040228968 | Basceri | Nov 2004 | A1 |
20040231600 | Lee | Nov 2004 | A1 |
20040231799 | Lee et al. | Nov 2004 | A1 |
20040238523 | Kuibira et al. | Dec 2004 | A1 |
20040241322 | Basceri et al. | Dec 2004 | A1 |
20040241998 | Hanson | Dec 2004 | A1 |
20040245091 | Karim et al. | Dec 2004 | A1 |
20040247779 | Selvamanickam et al. | Dec 2004 | A1 |
20040250600 | Bevers et al. | Dec 2004 | A1 |
20040253867 | Matsumoto | Dec 2004 | A1 |
20040261492 | Zarkar et al. | Dec 2004 | A1 |
20040261712 | Hayashi et al. | Dec 2004 | A1 |
20040261946 | Endoh et al. | Dec 2004 | A1 |
20040266011 | Lee et al. | Dec 2004 | A1 |
20050000428 | Shero et al. | Jan 2005 | A1 |
20050001062 | McCracken et al. | Jan 2005 | A1 |
20050003089 | Won et al. | Jan 2005 | A1 |
20050003600 | Kasai et al. | Jan 2005 | A1 |
20050003662 | Jurisch et al. | Jan 2005 | A1 |
20050008799 | Tomiyasu et al. | Jan 2005 | A1 |
20050009325 | Chung et al. | Jan 2005 | A1 |
20050016470 | Kang et al. | Jan 2005 | A1 |
20050016956 | Liu et al. | Jan 2005 | A1 |
20050017272 | Yamashita et al. | Jan 2005 | A1 |
20050019026 | Wang et al. | Jan 2005 | A1 |
20050019494 | Moghadam et al. | Jan 2005 | A1 |
20050019960 | Lee et al. | Jan 2005 | A1 |
20050020071 | Sonobe et al. | Jan 2005 | A1 |
20050023624 | Ahn et al. | Feb 2005 | A1 |
20050026402 | Jurgensen | Feb 2005 | A1 |
20050033075 | Chi et al. | Feb 2005 | A1 |
20050034664 | Koh et al. | Feb 2005 | A1 |
20050034674 | Ono | Feb 2005 | A1 |
20050037154 | Koh et al. | Feb 2005 | A1 |
20050037557 | Doczy et al. | Feb 2005 | A1 |
20050037578 | Chen et al. | Feb 2005 | A1 |
20050037610 | Cha | Feb 2005 | A1 |
20050037619 | Granneman et al. | Feb 2005 | A1 |
20050040144 | Sellers | Feb 2005 | A1 |
20050042778 | Peukert | Feb 2005 | A1 |
20050046825 | Powell et al. | Mar 2005 | A1 |
20050048797 | Fukazawa | Mar 2005 | A1 |
20050051093 | Makino et al. | Mar 2005 | A1 |
20050051100 | Chiang et al. | Mar 2005 | A1 |
20050054175 | Bauer | Mar 2005 | A1 |
20050054198 | Um | Mar 2005 | A1 |
20050054228 | March | Mar 2005 | A1 |
20050056218 | Sun et al. | Mar 2005 | A1 |
20050056780 | Miller et al. | Mar 2005 | A1 |
20050059261 | Basceri et al. | Mar 2005 | A1 |
20050059262 | Yin et al. | Mar 2005 | A1 |
20050059264 | Cheung | Mar 2005 | A1 |
20050061964 | Nagano et al. | Mar 2005 | A1 |
20050063451 | Abe et al. | Mar 2005 | A1 |
20050064207 | Senzaki et al. | Mar 2005 | A1 |
20050064719 | Liu | Mar 2005 | A1 |
20050066893 | Soininen | Mar 2005 | A1 |
20050069651 | Miyoshi | Mar 2005 | A1 |
20050070123 | Hirano | Mar 2005 | A1 |
20050070128 | Xia et al. | Mar 2005 | A1 |
20050070729 | Kiyomori et al. | Mar 2005 | A1 |
20050072357 | Shero et al. | Apr 2005 | A1 |
20050074576 | Chaiken et al. | Apr 2005 | A1 |
20050074983 | Shinriki et al. | Apr 2005 | A1 |
20050079691 | Kim et al. | Apr 2005 | A1 |
20050092247 | Schmidt | May 2005 | A1 |
20050092249 | Kilpela et al. | May 2005 | A1 |
20050092733 | Ito et al. | May 2005 | A1 |
20050095770 | Kumagai et al. | May 2005 | A1 |
20050095779 | Park et al. | May 2005 | A1 |
20050095859 | Chen et al. | May 2005 | A1 |
20050098107 | Du Bois et al. | May 2005 | A1 |
20050100669 | Kools et al. | May 2005 | A1 |
20050101154 | Huang | May 2005 | A1 |
20050101843 | Quinn et al. | May 2005 | A1 |
20050106762 | Chakrapani et al. | May 2005 | A1 |
20050106893 | Wilk | May 2005 | A1 |
20050107627 | Dussarrat et al. | May 2005 | A1 |
20050109461 | Sun | May 2005 | A1 |
20050110069 | Kil et al. | May 2005 | A1 |
20050112282 | Gordon et al. | May 2005 | A1 |
20050115946 | Shim et al. | Jun 2005 | A1 |
20050118804 | Byun et al. | Jun 2005 | A1 |
20050118837 | Todd | Jun 2005 | A1 |
20050120805 | Lane | Jun 2005 | A1 |
20050120962 | Ushioda et al. | Jun 2005 | A1 |
20050121145 | Du Bois et al. | Jun 2005 | A1 |
20050123690 | Derderian et al. | Jun 2005 | A1 |
20050130427 | Seok-Jun | Jun 2005 | A1 |
20050132957 | El-Raghy | Jun 2005 | A1 |
20050133160 | Kennedy et al. | Jun 2005 | A1 |
20050133161 | Carpenter et al. | Jun 2005 | A1 |
20050136188 | Chang | Jun 2005 | A1 |
20050139160 | Lei et al. | Jun 2005 | A1 |
20050141591 | Sakano | Jun 2005 | A1 |
20050142361 | Nakanishi | Jun 2005 | A1 |
20050145338 | Park et al. | Jul 2005 | A1 |
20050148162 | Chen et al. | Jul 2005 | A1 |
20050150601 | Srivastava | Jul 2005 | A1 |
20050151184 | Lee et al. | Jul 2005 | A1 |
20050153571 | Senzaki | Jul 2005 | A1 |
20050160987 | Kasai et al. | Jul 2005 | A1 |
20050161434 | Sugawara et al. | Jul 2005 | A1 |
20050172895 | Kijima et al. | Aug 2005 | A1 |
20050173003 | Laverdiere et al. | Aug 2005 | A1 |
20050175789 | Helms | Aug 2005 | A1 |
20050178333 | Loke et al. | Aug 2005 | A1 |
20050181535 | Yun et al. | Aug 2005 | A1 |
20050181555 | Haukka et al. | Aug 2005 | A1 |
20050183827 | White et al. | Aug 2005 | A1 |
20050186688 | Basceri | Aug 2005 | A1 |
20050187647 | Wang et al. | Aug 2005 | A1 |
20050191828 | Al-Bayati et al. | Sep 2005 | A1 |
20050193948 | Oohirabaru et al. | Sep 2005 | A1 |
20050199013 | Vandroux et al. | Sep 2005 | A1 |
20050199342 | Shajii et al. | Sep 2005 | A1 |
20050201908 | Nakamura et al. | Sep 2005 | A1 |
20050208217 | Shinriki et al. | Sep 2005 | A1 |
20050208219 | Basceri | Sep 2005 | A1 |
20050208718 | Lim et al. | Sep 2005 | A1 |
20050211167 | Gunji | Sep 2005 | A1 |
20050211384 | Hayashi | Sep 2005 | A1 |
20050212119 | Shero | Sep 2005 | A1 |
20050214457 | Schmitt et al. | Sep 2005 | A1 |
20050214458 | Meiere | Sep 2005 | A1 |
20050208778 | Li | Oct 2005 | A1 |
20050218462 | Ahn et al. | Oct 2005 | A1 |
20050221021 | Strang | Oct 2005 | A1 |
20050221618 | AmRhein et al. | Oct 2005 | A1 |
20050223982 | Park et al. | Oct 2005 | A1 |
20050223994 | Blomiley et al. | Oct 2005 | A1 |
20050227502 | Schmitt et al. | Oct 2005 | A1 |
20050229848 | Shinriki | Oct 2005 | A1 |
20050229849 | Silvetti et al. | Oct 2005 | A1 |
20050229972 | Hoshi et al. | Oct 2005 | A1 |
20050233477 | Yamazaki et al. | Oct 2005 | A1 |
20050238807 | Lin et al. | Oct 2005 | A1 |
20050241176 | Shero et al. | Nov 2005 | A1 |
20050241763 | Huang et al. | Nov 2005 | A1 |
20050241765 | Dhindsa et al. | Nov 2005 | A1 |
20050245058 | Lee et al. | Nov 2005 | A1 |
20050249876 | Kawahara et al. | Nov 2005 | A1 |
20050250340 | Chen et al. | Nov 2005 | A1 |
20050251990 | Choi | Nov 2005 | A1 |
20050252447 | Zhao et al. | Nov 2005 | A1 |
20050252449 | Nguyen et al. | Nov 2005 | A1 |
20050252455 | Moriya et al. | Nov 2005 | A1 |
20050253061 | Cameron et al. | Nov 2005 | A1 |
20050255257 | Choi et al. | Nov 2005 | A1 |
20050255327 | Chaney et al. | Nov 2005 | A1 |
20050258280 | Goto et al. | Nov 2005 | A1 |
20050260347 | Narwankar et al. | Nov 2005 | A1 |
20050260837 | Walther et al. | Nov 2005 | A1 |
20050260850 | Loke | Nov 2005 | A1 |
20050263072 | Balasubramanian et al. | Dec 2005 | A1 |
20050263075 | Wang et al. | Dec 2005 | A1 |
20050263719 | Ohdaira et al. | Dec 2005 | A1 |
20050263932 | Heugel | Dec 2005 | A1 |
20050268856 | Miller et al. | Dec 2005 | A1 |
20050271812 | Myo et al. | Dec 2005 | A1 |
20050271813 | Kher et al. | Dec 2005 | A1 |
20050272247 | Ikeda et al. | Dec 2005 | A1 |
20050274323 | Seidel et al. | Dec 2005 | A1 |
20050276928 | Okumura et al. | Dec 2005 | A1 |
20050277271 | Beintner | Dec 2005 | A1 |
20050280050 | Doczy et al. | Dec 2005 | A1 |
20050282101 | Adachi | Dec 2005 | A1 |
20050282350 | Chou et al. | Dec 2005 | A1 |
20050284573 | Egley et al. | Dec 2005 | A1 |
20050284991 | Saez | Dec 2005 | A1 |
20050285097 | Shang et al. | Dec 2005 | A1 |
20050287725 | Kitagawa | Dec 2005 | A1 |
20050287771 | Seamons et al. | Dec 2005 | A1 |
20060000411 | Seo | Jan 2006 | A1 |
20060006538 | Allman et al. | Jan 2006 | A1 |
20060009044 | Igeta et al. | Jan 2006 | A1 |
20060013674 | Elliott et al. | Jan 2006 | A1 |
20060013946 | Park et al. | Jan 2006 | A1 |
20060014384 | Lee et al. | Jan 2006 | A1 |
20060014397 | Seamons et al. | Jan 2006 | A1 |
20060016783 | Wu et al. | Jan 2006 | A1 |
20060019033 | Muthukrishnan et al. | Jan 2006 | A1 |
20060019502 | Park et al. | Jan 2006 | A1 |
20060021572 | Wolden | Feb 2006 | A1 |
20060021573 | Monsma et al. | Feb 2006 | A1 |
20060021703 | Umotoy et al. | Feb 2006 | A1 |
20060024439 | Tuominen et al. | Feb 2006 | A2 |
20060026314 | Franchuk et al. | Feb 2006 | A1 |
20060032443 | Hasebe et al. | Feb 2006 | A1 |
20060040054 | Pearlstein et al. | Feb 2006 | A1 |
20060040508 | Ji | Feb 2006 | A1 |
20060046518 | Hill et al. | Mar 2006 | A1 |
20060048710 | Horiguchi et al. | Mar 2006 | A1 |
20060051505 | Kortshagen et al. | Mar 2006 | A1 |
20060051520 | Behle et al. | Mar 2006 | A1 |
20060051925 | Ahn et al. | Mar 2006 | A1 |
20060057799 | Horiguchi et al. | Mar 2006 | A1 |
20060057828 | Omura | Mar 2006 | A1 |
20060060930 | Metz et al. | Mar 2006 | A1 |
20060062910 | Meiere | Mar 2006 | A1 |
20060063346 | Lee et al. | Mar 2006 | A1 |
20060068097 | Yamasaki et al. | Mar 2006 | A1 |
20060068104 | Ishizaka | Mar 2006 | A1 |
20060068121 | Lee et al. | Mar 2006 | A1 |
20060068125 | Radhakrishnan | Mar 2006 | A1 |
20060081558 | Collins et al. | Apr 2006 | A1 |
20060087638 | Hirayanagi | Apr 2006 | A1 |
20060090702 | Koo et al. | May 2006 | A1 |
20060093756 | Rajagopalan et al. | May 2006 | A1 |
20060094236 | Elkins et al. | May 2006 | A1 |
20060096540 | Choi | May 2006 | A1 |
20060099782 | Ritenour | May 2006 | A1 |
20060102968 | Bojarczuk et al. | May 2006 | A1 |
20060105566 | Waldfried et al. | May 2006 | A1 |
20060107898 | Blomberg | May 2006 | A1 |
20060108221 | Goodwin et al. | May 2006 | A1 |
20060108331 | Nozawa et al. | May 2006 | A1 |
20060110934 | Fukuchi | May 2006 | A1 |
20060113038 | Gondhalekar et al. | Jun 2006 | A1 |
20060113675 | Chang et al. | Jun 2006 | A1 |
20060113806 | Tsuji et al. | Jun 2006 | A1 |
20060118240 | Holber et al. | Jun 2006 | A1 |
20060125099 | Gordon et al. | Jun 2006 | A1 |
20060127067 | Wintenberger et al. | Jun 2006 | A1 |
20060128142 | Whelan et al. | Jun 2006 | A1 |
20060128168 | Ahn et al. | Jun 2006 | A1 |
20060130767 | Herchen | Jun 2006 | A1 |
20060137608 | Choi et al. | Jun 2006 | A1 |
20060137609 | Puchacz et al. | Jun 2006 | A1 |
20060141155 | Gordon et al. | Jun 2006 | A1 |
20060144820 | Sawin et al. | Jul 2006 | A1 |
20060147626 | Blomberg | Jul 2006 | A1 |
20060148180 | Ahn et al. | Jul 2006 | A1 |
20060151117 | Kasanami et al. | Jul 2006 | A1 |
20060154424 | Yang et al. | Jul 2006 | A1 |
20060156981 | Fondurulia | Jul 2006 | A1 |
20060162658 | Weidman | Jul 2006 | A1 |
20060162863 | Kim et al. | Jul 2006 | A1 |
20060163612 | Kouvetakis et al. | Jul 2006 | A1 |
20060163683 | Roth et al. | Jul 2006 | A1 |
20060165892 | Weidman | Jul 2006 | A1 |
20060166428 | Kamioka et al. | Jul 2006 | A1 |
20060172531 | Lin et al. | Aug 2006 | A1 |
20060175669 | Kim et al. | Aug 2006 | A1 |
20060177855 | Utermohlen | Aug 2006 | A1 |
20060182885 | Lei et al. | Aug 2006 | A1 |
20060185589 | Zehavi et al. | Aug 2006 | A1 |
20060188360 | Bonora et al. | Aug 2006 | A1 |
20060191555 | Yoshida et al. | Aug 2006 | A1 |
20060193979 | Meiere et al. | Aug 2006 | A1 |
20060196418 | Lindfors et al. | Sep 2006 | A1 |
20060196420 | Ushakov et al. | Sep 2006 | A1 |
20060196421 | Ronsse et al. | Sep 2006 | A1 |
20060199357 | Wan et al. | Sep 2006 | A1 |
20060205194 | Bauer | Sep 2006 | A1 |
20060205223 | Smayling | Sep 2006 | A1 |
20060205231 | Chou et al. | Sep 2006 | A1 |
20060208215 | Metzner et al. | Sep 2006 | A1 |
20060211243 | Ishizaka et al. | Sep 2006 | A1 |
20060211259 | Maes | Sep 2006 | A1 |
20060213437 | Ishizaka et al. | Sep 2006 | A1 |
20060213439 | Ishizaka | Sep 2006 | A1 |
20060216942 | Kim et al. | Sep 2006 | A1 |
20060219169 | Chen et al. | Oct 2006 | A1 |
20060219361 | Wang et al. | Oct 2006 | A1 |
20060219363 | Matsumoto et al. | Oct 2006 | A1 |
20060223301 | Vanhaelemeersch et al. | Oct 2006 | A1 |
20060226117 | Bertram et al. | Oct 2006 | A1 |
20060228496 | Choi | Oct 2006 | A1 |
20060228863 | Zhang et al. | Oct 2006 | A1 |
20060228888 | Lee et al. | Oct 2006 | A1 |
20060228898 | Wajda et al. | Oct 2006 | A1 |
20060236934 | Choi et al. | Oct 2006 | A1 |
20060240187 | Weidman | Oct 2006 | A1 |
20060240574 | Yoshie | Oct 2006 | A1 |
20060240662 | Conley et al. | Oct 2006 | A1 |
20060247404 | Todd | Nov 2006 | A1 |
20060249253 | Dando | Nov 2006 | A1 |
20060251827 | Nowak | Nov 2006 | A1 |
20060252228 | Jeng | Nov 2006 | A1 |
20060252351 | Kundracik | Nov 2006 | A1 |
20060254514 | Kang et al. | Nov 2006 | A1 |
20060257563 | Doh et al. | Nov 2006 | A1 |
20060257584 | Derderian et al. | Nov 2006 | A1 |
20060258078 | Lee et al. | Nov 2006 | A1 |
20060258173 | Xiao et al. | Nov 2006 | A1 |
20060260545 | Ramaswamy et al. | Nov 2006 | A1 |
20060263522 | Byun | Nov 2006 | A1 |
20060263540 | Ramaswamy et al. | Nov 2006 | A1 |
20060264060 | Ramaswamy et al. | Nov 2006 | A1 |
20060264066 | Bartholomew | Nov 2006 | A1 |
20060266289 | Verghese et al. | Nov 2006 | A1 |
20060269690 | Watanabe et al. | Nov 2006 | A1 |
20060269692 | Balseanu | Nov 2006 | A1 |
20060275710 | Yamazaki et al. | Dec 2006 | A1 |
20060275933 | Du Bois et al. | Dec 2006 | A1 |
20060278524 | Stowell | Dec 2006 | A1 |
20060283629 | Kikuchi et al. | Dec 2006 | A1 |
20060286774 | Singh et al. | Dec 2006 | A1 |
20060286775 | Singh et al. | Dec 2006 | A1 |
20060286817 | Kato et al. | Dec 2006 | A1 |
20060286818 | Wang et al. | Dec 2006 | A1 |
20060286819 | Seutter | Dec 2006 | A1 |
20060291982 | Tanaka | Dec 2006 | A1 |
20060292310 | Le et al. | Dec 2006 | A1 |
20060292845 | Chiang et al. | Dec 2006 | A1 |
20070004204 | Fukazawa et al. | Jan 2007 | A1 |
20070006806 | Imai | Jan 2007 | A1 |
20070010072 | Bailey et al. | Jan 2007 | A1 |
20070012402 | Sneh | Jan 2007 | A1 |
20070014919 | Hamalainen et al. | Jan 2007 | A1 |
20070020160 | Berkman et al. | Jan 2007 | A1 |
20070020167 | Han et al. | Jan 2007 | A1 |
20070020830 | Speranza | Jan 2007 | A1 |
20070020953 | Tsai et al. | Jan 2007 | A1 |
20070022954 | Iizuka et al. | Feb 2007 | A1 |
20070026148 | Arai et al. | Feb 2007 | A1 |
20070026162 | Wei et al. | Feb 2007 | A1 |
20070026540 | Nooten et al. | Feb 2007 | A1 |
20070028842 | Inagawa et al. | Feb 2007 | A1 |
20070031598 | Okuyama et al. | Feb 2007 | A1 |
20070031599 | Gschwandtner et al. | Feb 2007 | A1 |
20070032004 | Ramaswamy et al. | Feb 2007 | A1 |
20070032045 | Kasahara et al. | Feb 2007 | A1 |
20070032054 | Ramaswamy et al. | Feb 2007 | A1 |
20070032082 | Ramaswamy et al. | Feb 2007 | A1 |
20070032095 | Ramaswamy et al. | Feb 2007 | A1 |
20070034477 | Inui | Feb 2007 | A1 |
20070037343 | Colombo et al. | Feb 2007 | A1 |
20070037412 | Dip et al. | Feb 2007 | A1 |
20070042117 | Kupurao et al. | Feb 2007 | A1 |
20070042581 | Sano et al. | Feb 2007 | A1 |
20070044716 | Tetsuka et al. | Mar 2007 | A1 |
20070045244 | Lee et al. | Mar 2007 | A1 |
20070047384 | McLaughlin et al. | Mar 2007 | A1 |
20070048953 | Gealy et al. | Mar 2007 | A1 |
20070049053 | Mahajani | Mar 2007 | A1 |
20070051299 | Ong et al. | Mar 2007 | A1 |
20070051312 | Sneh | Mar 2007 | A1 |
20070051471 | Kawaguchi et al. | Mar 2007 | A1 |
20070054049 | Lindfors et al. | Mar 2007 | A1 |
20070054499 | Jang | Mar 2007 | A1 |
20070056843 | Ye et al. | Mar 2007 | A1 |
20070056850 | Ye et al. | Mar 2007 | A1 |
20070059948 | Metzner et al. | Mar 2007 | A1 |
20070062439 | Wada et al. | Mar 2007 | A1 |
20070062453 | Ishikawa | Mar 2007 | A1 |
20070062646 | Ogawa et al. | Mar 2007 | A1 |
20070065578 | McDougall | Mar 2007 | A1 |
20070066010 | Ando | Mar 2007 | A1 |
20070066038 | Sadjadi et al. | Mar 2007 | A1 |
20070066079 | Kolster et al. | Mar 2007 | A1 |
20070066084 | Wajda et al. | Mar 2007 | A1 |
20070074665 | Chacin et al. | Apr 2007 | A1 |
20070077355 | Chacin et al. | Apr 2007 | A1 |
20070082132 | Shinriki | Apr 2007 | A1 |
20070082500 | Norman et al. | Apr 2007 | A1 |
20070082508 | Chiang et al. | Apr 2007 | A1 |
20070084405 | Kim | Apr 2007 | A1 |
20070087296 | Kim et al. | Apr 2007 | A1 |
20070087579 | Kitayama et al. | Apr 2007 | A1 |
20070089670 | Ikedo | Apr 2007 | A1 |
20070095283 | Galewski | May 2007 | A1 |
20070095286 | Baek et al. | May 2007 | A1 |
20070096194 | Streck et al. | May 2007 | A1 |
20070098527 | Hall et al. | May 2007 | A1 |
20070107845 | Ishizawa et al. | May 2007 | A1 |
20070111470 | Smythe | May 2007 | A1 |
20070111545 | Lee et al. | May 2007 | A1 |
20070113788 | Nozawa et al. | May 2007 | A1 |
20070116872 | Li et al. | May 2007 | A1 |
20070116873 | Li et al. | May 2007 | A1 |
20070116887 | Faguet | May 2007 | A1 |
20070116888 | Faguet | May 2007 | A1 |
20070119370 | Ma et al. | May 2007 | A1 |
20070120275 | Liu | May 2007 | A1 |
20070123037 | Lee et al. | May 2007 | A1 |
20070123189 | Saito et al. | May 2007 | A1 |
20070125762 | Cui et al. | Jun 2007 | A1 |
20070128538 | Fairbairn et al. | Jun 2007 | A1 |
20070128858 | Haukka et al. | Jun 2007 | A1 |
20070128876 | Fukiage | Jun 2007 | A1 |
20070128888 | Goto et al. | Jun 2007 | A1 |
20070129621 | Kellogg et al. | Jun 2007 | A1 |
20070131168 | Gomi et al. | Jun 2007 | A1 |
20070134919 | Gunji et al. | Jun 2007 | A1 |
20070134942 | Ahn et al. | Jun 2007 | A1 |
20070137794 | Qiu et al. | Jun 2007 | A1 |
20070146621 | Yeom | Jun 2007 | A1 |
20070148347 | Hatanpaa et al. | Jun 2007 | A1 |
20070148350 | Rahtu | Jun 2007 | A1 |
20070148990 | Deboer et al. | Jun 2007 | A1 |
20070153625 | Lundgren et al. | Jun 2007 | A1 |
20070155138 | Tomasini et al. | Jul 2007 | A1 |
20070157466 | Kida et al. | Jul 2007 | A1 |
20070157683 | Li | Jul 2007 | A1 |
20070158026 | Amikura | Jul 2007 | A1 |
20070163440 | Kim et al. | Jul 2007 | A1 |
20070163625 | Lee | Jul 2007 | A1 |
20070163996 | Horiguchi | Jul 2007 | A1 |
20070166457 | Yamoto et al. | Jul 2007 | A1 |
20070166966 | Todd et al. | Jul 2007 | A1 |
20070166999 | Vaarstra | Jul 2007 | A1 |
20070170372 | Horsky | Jul 2007 | A1 |
20070173071 | Afzali-Ardakani et al. | Jul 2007 | A1 |
20070175393 | Nishimura et al. | Aug 2007 | A1 |
20070175397 | Tomiyasu et al. | Aug 2007 | A1 |
20070178235 | Yamada et al. | Aug 2007 | A1 |
20070181066 | Cadwell et al. | Aug 2007 | A1 |
20070184179 | Waghray et al. | Aug 2007 | A1 |
20070186849 | Furuya | Aug 2007 | A1 |
20070186952 | Honda et al. | Aug 2007 | A1 |
20070187362 | Nakagawa et al. | Aug 2007 | A1 |
20070187363 | Oka et al. | Aug 2007 | A1 |
20070190266 | Fu et al. | Aug 2007 | A1 |
20070190362 | Weidman | Aug 2007 | A1 |
20070190744 | Hiraiwa et al. | Aug 2007 | A1 |
20070190782 | Park | Aug 2007 | A1 |
20070199510 | Weiner et al. | Aug 2007 | A1 |
20070202678 | Plombon et al. | Aug 2007 | A1 |
20070207275 | Nowak et al. | Sep 2007 | A1 |
20070209588 | Li et al. | Sep 2007 | A1 |
20070209590 | Li | Sep 2007 | A1 |
20070210890 | Hsu et al. | Sep 2007 | A1 |
20070212484 | Li | Sep 2007 | A1 |
20070212811 | Hanawa et al. | Sep 2007 | A1 |
20070212827 | Girotra et al. | Sep 2007 | A1 |
20070215048 | Suzuki et al. | Sep 2007 | A1 |
20070215580 | Koshiishi et al. | Sep 2007 | A1 |
20070218200 | Suzuki et al. | Sep 2007 | A1 |
20070218705 | Matsuki et al. | Sep 2007 | A1 |
20070224777 | Hamelin | Sep 2007 | A1 |
20070224833 | Morisada et al. | Sep 2007 | A1 |
20070227665 | Matsumoto et al. | Oct 2007 | A1 |
20070231488 | Von Kaenel | Oct 2007 | A1 |
20070232031 | Singh et al. | Oct 2007 | A1 |
20070232071 | Balseanu et al. | Oct 2007 | A1 |
20070232501 | Tonomura | Oct 2007 | A1 |
20070234955 | Suzuki et al. | Oct 2007 | A1 |
20070237697 | Clark | Oct 2007 | A1 |
20070237698 | Clark | Oct 2007 | A1 |
20070237699 | Clark | Oct 2007 | A1 |
20070238305 | Delgadino et al. | Oct 2007 | A1 |
20070241688 | DeVancentis et al. | Oct 2007 | A1 |
20070243317 | Du Bois et al. | Oct 2007 | A1 |
20070247075 | Kim et al. | Oct 2007 | A1 |
20070248767 | Okura | Oct 2007 | A1 |
20070249131 | Allen et al. | Oct 2007 | A1 |
20070251444 | Gros-Jean et al. | Nov 2007 | A1 |
20070251456 | Herchen et al. | Nov 2007 | A1 |
20070252233 | Yamazaki et al. | Nov 2007 | A1 |
20070252244 | Srividya et al. | Nov 2007 | A1 |
20070252532 | DeVancentis et al. | Nov 2007 | A1 |
20070254414 | Miyanami | Nov 2007 | A1 |
20070258506 | Schwagerman et al. | Nov 2007 | A1 |
20070258855 | Turcot et al. | Nov 2007 | A1 |
20070259778 | Spencer et al. | Nov 2007 | A1 |
20070261868 | Gross | Nov 2007 | A1 |
20070264807 | Leone et al. | Nov 2007 | A1 |
20070266932 | Hiramatsu | Nov 2007 | A1 |
20070266945 | Shuto et al. | Nov 2007 | A1 |
20070269983 | Sneh | Nov 2007 | A1 |
20070275166 | Thridandam et al. | Nov 2007 | A1 |
20070277735 | Mokhesi et al. | Dec 2007 | A1 |
20070281082 | Mokhesi et al. | Dec 2007 | A1 |
20070281105 | Mokhesi et al. | Dec 2007 | A1 |
20070281496 | Ingle et al. | Dec 2007 | A1 |
20070286957 | Suzuki et al. | Dec 2007 | A1 |
20070289534 | Lubomirsky et al. | Dec 2007 | A1 |
20070292974 | Mizuno et al. | Dec 2007 | A1 |
20070295602 | Tiller et al. | Dec 2007 | A1 |
20070298362 | Rocha-Alvarez et al. | Dec 2007 | A1 |
20070298565 | Nieh et al. | Dec 2007 | A1 |
20080003425 | Spencer et al. | Jan 2008 | A1 |
20080003824 | Padhi et al. | Jan 2008 | A1 |
20080003838 | Haukka et al. | Jan 2008 | A1 |
20080006208 | Ueno et al. | Jan 2008 | A1 |
20080018004 | Steidl | Jan 2008 | A1 |
20080020591 | Balseanu et al. | Jan 2008 | A1 |
20080020593 | Wang et al. | Jan 2008 | A1 |
20080023436 | Gros-Jean et al. | Jan 2008 | A1 |
20080026162 | Dickey et al. | Jan 2008 | A1 |
20080026574 | Brcka | Jan 2008 | A1 |
20080026597 | Munro et al. | Jan 2008 | A1 |
20080029790 | Ahn et al. | Feb 2008 | A1 |
20080031708 | Bonora et al. | Feb 2008 | A1 |
20080035055 | Dip et al. | Feb 2008 | A1 |
20080035306 | White et al. | Feb 2008 | A1 |
20080035607 | O'Hara et al. | Feb 2008 | A1 |
20080036354 | Letz et al. | Feb 2008 | A1 |
20080038485 | Fuzakawa et al. | Feb 2008 | A1 |
20080038934 | Vrtis et al. | Feb 2008 | A1 |
20080042165 | Sugizaki | Feb 2008 | A1 |
20080042192 | Park et al. | Feb 2008 | A1 |
20080043803 | Bandoh | Feb 2008 | A1 |
20080044938 | England et al. | Feb 2008 | A1 |
20080050536 | Aing et al. | Feb 2008 | A1 |
20080050538 | Hirata | Feb 2008 | A1 |
20080054332 | Kim et al. | Mar 2008 | A1 |
20080054813 | Espiau et al. | Mar 2008 | A1 |
20080056860 | Natume | Mar 2008 | A1 |
20080057659 | Forbes et al. | Mar 2008 | A1 |
20080061667 | Gaertner et al. | Mar 2008 | A1 |
20080063798 | Kher et al. | Mar 2008 | A1 |
20080066778 | Matsushita et al. | Mar 2008 | A1 |
20080067146 | Onishi et al. | Mar 2008 | A1 |
20080069955 | Hong et al. | Mar 2008 | A1 |
20080072821 | Dalton et al. | Mar 2008 | A1 |
20080075562 | Maria et al. | Mar 2008 | A1 |
20080075838 | Inoue et al. | Mar 2008 | A1 |
20080075881 | Won et al. | Mar 2008 | A1 |
20080076070 | Koh et al. | Mar 2008 | A1 |
20080076266 | Fukazawa et al. | Mar 2008 | A1 |
20080076281 | Ciancanelli et al. | Mar 2008 | A1 |
20080081104 | Hasebe et al. | Apr 2008 | A1 |
20080081113 | Clark | Apr 2008 | A1 |
20080081121 | Morita et al. | Apr 2008 | A1 |
20080083710 | Chen et al. | Apr 2008 | A1 |
20080083948 | Lin et al. | Apr 2008 | A1 |
20080085226 | Fondurulia et al. | Apr 2008 | A1 |
20080085610 | Wang et al. | Apr 2008 | A1 |
20080087218 | Shimada et al. | Apr 2008 | A1 |
20080087642 | Sawin et al. | Apr 2008 | A1 |
20080087890 | Ahn et al. | Apr 2008 | A1 |
20080092815 | Chen et al. | Apr 2008 | A1 |
20080099147 | Myo et al. | May 2008 | A1 |
20080102203 | Wu | May 2008 | A1 |
20080102205 | Barry et al. | May 2008 | A1 |
20080102208 | Wu et al. | May 2008 | A1 |
20080102603 | Kobayashi et al. | May 2008 | A1 |
20080102630 | Saito | May 2008 | A1 |
20080105276 | Yeh et al. | May 2008 | A1 |
20080113094 | Casper | May 2008 | A1 |
20080113096 | Mahajani | May 2008 | A1 |
20080113097 | Mahajani et al. | May 2008 | A1 |
20080118334 | Bonora | May 2008 | A1 |
20080121177 | Bang et al. | May 2008 | A1 |
20080121626 | Thomas et al. | May 2008 | A1 |
20080121962 | Forbes et al. | May 2008 | A1 |
20080124197 | van der Meulen et al. | May 2008 | A1 |
20080124908 | Forbes et al. | May 2008 | A1 |
20080124945 | Miya et al. | May 2008 | A1 |
20080124946 | Xiao et al. | May 2008 | A1 |
20080128726 | Sakata et al. | Jun 2008 | A1 |
20080129209 | Deakins et al. | Jun 2008 | A1 |
20080132046 | Walther | Jun 2008 | A1 |
20080133154 | Krauss et al. | Jun 2008 | A1 |
20080134887 | Sherer | Jun 2008 | A1 |
20080142483 | Hua | Jun 2008 | A1 |
20080146033 | Park | Jun 2008 | A1 |
20080149031 | Chu et al. | Jun 2008 | A1 |
20080149593 | Bai et al. | Jun 2008 | A1 |
20080152463 | Chidambaram et al. | Jun 2008 | A1 |
20080153308 | Ogawa et al. | Jun 2008 | A1 |
20080153311 | Padhi et al. | Jun 2008 | A1 |
20080156769 | Weiner et al. | Jul 2008 | A1 |
20080157157 | Tonomura | Jul 2008 | A1 |
20080157365 | Ott et al. | Jul 2008 | A1 |
20080173237 | Collins | Jul 2008 | A1 |
20080173238 | Nakashima et al. | Jul 2008 | A1 |
20080173240 | Furukawahara | Jul 2008 | A1 |
20080173326 | Gu et al. | Jul 2008 | A1 |
20080176335 | Alberti et al. | Jul 2008 | A1 |
20080176375 | Erben et al. | Jul 2008 | A1 |
20080176412 | Komeda | Jul 2008 | A1 |
20080178608 | Tandou et al. | Jul 2008 | A1 |
20080178805 | Paterson et al. | Jul 2008 | A1 |
20080179104 | Zhang | Jul 2008 | A1 |
20080179291 | Collins et al. | Jul 2008 | A1 |
20080179715 | Coppa | Jul 2008 | A1 |
20080182075 | Chopra | Jul 2008 | A1 |
20080182390 | Lemmi et al. | Jul 2008 | A1 |
20080182411 | Elers | Jul 2008 | A1 |
20080191193 | Li et al. | Aug 2008 | A1 |
20080193643 | Dip | Aug 2008 | A1 |
20080194105 | Dominguez et al. | Aug 2008 | A1 |
20080194169 | Sterling et al. | Aug 2008 | A1 |
20080199977 | Weigel et al. | Aug 2008 | A1 |
20080202416 | Provencher | Aug 2008 | A1 |
20080202689 | Kim | Aug 2008 | A1 |
20080203487 | Hohage et al. | Aug 2008 | A1 |
20080205483 | Rempe et al. | Aug 2008 | A1 |
20080210278 | Orii et al. | Sep 2008 | A1 |
20080211423 | Shinmen et al. | Sep 2008 | A1 |
20080211526 | Shinma | Sep 2008 | A1 |
20080213696 | Meeus et al. | Sep 2008 | A1 |
20080214003 | Xia et al. | Sep 2008 | A1 |
20080216077 | Emani et al. | Sep 2008 | A1 |
20080216742 | Takebayashi | Sep 2008 | A1 |
20080216958 | Goto et al. | Sep 2008 | A1 |
20080220619 | Matsushita et al. | Sep 2008 | A1 |
20080223130 | Snell et al. | Sep 2008 | A1 |
20080224240 | Ahn et al. | Sep 2008 | A1 |
20080228306 | Yetter et al. | Sep 2008 | A1 |
20080230371 | McHugh | Sep 2008 | A1 |
20080233288 | Clark | Sep 2008 | A1 |
20080237572 | Chui et al. | Oct 2008 | A1 |
20080241052 | Hooper et al. | Oct 2008 | A1 |
20080241384 | Jeong | Oct 2008 | A1 |
20080241387 | Keto | Oct 2008 | A1 |
20080242116 | Clark | Oct 2008 | A1 |
20080248310 | Kim et al. | Oct 2008 | A1 |
20080248597 | Qin et al. | Oct 2008 | A1 |
20080257102 | Packer | Oct 2008 | A1 |
20080257494 | Hayashi et al. | Oct 2008 | A1 |
20080260345 | Mertesdorf et al. | Oct 2008 | A1 |
20080260963 | Yoon et al. | Oct 2008 | A1 |
20080261405 | Yang et al. | Oct 2008 | A1 |
20080261413 | Mahajani | Oct 2008 | A1 |
20080264337 | Sano et al. | Oct 2008 | A1 |
20080264443 | Shrinivasan et al. | Oct 2008 | A1 |
20080267598 | Nakamura | Oct 2008 | A1 |
20080268171 | Ma et al. | Oct 2008 | A1 |
20080268635 | Yu et al. | Oct 2008 | A1 |
20080272424 | Kim et al. | Nov 2008 | A1 |
20080274369 | Lee et al. | Nov 2008 | A1 |
20080277647 | Kouvetakis et al. | Nov 2008 | A1 |
20080277656 | Park et al. | Nov 2008 | A1 |
20080277715 | Ohmi et al. | Nov 2008 | A1 |
20080282970 | Heys et al. | Nov 2008 | A1 |
20080283962 | Dyer | Nov 2008 | A1 |
20080286463 | Tiner et al. | Nov 2008 | A1 |
20080289574 | Jacobs et al. | Nov 2008 | A1 |
20080289650 | Arena | Nov 2008 | A1 |
20080289767 | Tandou et al. | Nov 2008 | A1 |
20080291964 | Shrimpling | Nov 2008 | A1 |
20080295872 | Riker et al. | Dec 2008 | A1 |
20080298945 | Cox | Dec 2008 | A1 |
20080299326 | Fukazawa | Dec 2008 | A1 |
20080299758 | Harada et al. | Dec 2008 | A1 |
20080302303 | Choi et al. | Dec 2008 | A1 |
20080303744 | Hirayama et al. | Dec 2008 | A1 |
20080305014 | Honda | Dec 2008 | A1 |
20080305246 | Choi et al. | Dec 2008 | A1 |
20080305443 | Nakamura | Dec 2008 | A1 |
20080314319 | Hamano et al. | Dec 2008 | A1 |
20080314892 | Graham | Dec 2008 | A1 |
20080315292 | Ji et al. | Dec 2008 | A1 |
20080317972 | Hendriks | Dec 2008 | A1 |
20090000550 | Tran et al. | Jan 2009 | A1 |
20090000551 | Choi et al. | Jan 2009 | A1 |
20090000769 | Lin et al. | Jan 2009 | A1 |
20090004875 | Shen et al. | Jan 2009 | A1 |
20090011145 | Yun | Jan 2009 | A1 |
20090011150 | Jeon et al. | Jan 2009 | A1 |
20090011608 | Nabatame | Jan 2009 | A1 |
20090014879 | Park et al. | Jan 2009 | A1 |
20090017227 | Fu et al. | Jan 2009 | A1 |
20090017631 | Bencher | Jan 2009 | A1 |
20090017733 | Takahashi et al. | Jan 2009 | A1 |
20090020072 | Mizunaga et al. | Jan 2009 | A1 |
20090023229 | Matsushita | Jan 2009 | A1 |
20090029503 | Arai | Jan 2009 | A1 |
20090029528 | Sanchez et al. | Jan 2009 | A1 |
20090029564 | Yamashita et al. | Jan 2009 | A1 |
20090033907 | Watson | Feb 2009 | A1 |
20090035584 | Tran et al. | Feb 2009 | A1 |
20090035927 | Olsen et al. | Feb 2009 | A1 |
20090035947 | Horii | Feb 2009 | A1 |
20090036292 | Sun et al. | Feb 2009 | A1 |
20090039475 | Shioya | Feb 2009 | A1 |
20090041952 | Yoon et al. | Feb 2009 | A1 |
20090041984 | Mayers et al. | Feb 2009 | A1 |
20090042344 | Ye et al. | Feb 2009 | A1 |
20090042408 | Maeda | Feb 2009 | A1 |
20090045749 | Ganachev et al. | Feb 2009 | A1 |
20090045829 | Awazu | Feb 2009 | A1 |
20090047426 | Park et al. | Feb 2009 | A1 |
20090047433 | Kim et al. | Feb 2009 | A1 |
20090047447 | Sawin et al. | Feb 2009 | A1 |
20090050621 | Awazu | Feb 2009 | A1 |
20090052498 | Halpin et al. | Feb 2009 | A1 |
20090053023 | Wakabayashi | Feb 2009 | A1 |
20090053900 | Nozawa et al. | Feb 2009 | A1 |
20090053906 | Miya et al. | Feb 2009 | A1 |
20090056112 | Kobayashi | Mar 2009 | A1 |
20090056629 | Katz et al. | Mar 2009 | A1 |
20090057269 | Katz et al. | Mar 2009 | A1 |
20090061083 | Chiang et al. | Mar 2009 | A1 |
20090061644 | Chiang et al. | Mar 2009 | A1 |
20090061647 | Mallick et al. | Mar 2009 | A1 |
20090075490 | Dussarrat | Mar 2009 | A1 |
20090075491 | Liu et al. | Mar 2009 | A1 |
20090081879 | Sukekawa et al. | Mar 2009 | A1 |
20090084317 | Wu | Apr 2009 | A1 |
20090085156 | Dewey et al. | Apr 2009 | A1 |
20090087585 | Lee et al. | Apr 2009 | A1 |
20090087964 | Maeda et al. | Apr 2009 | A1 |
20090087967 | Todd | Apr 2009 | A1 |
20090090382 | Morisada | Apr 2009 | A1 |
20090093080 | Choi et al. | Apr 2009 | A1 |
20090093094 | Ye et al. | Apr 2009 | A1 |
20090095221 | Tam et al. | Apr 2009 | A1 |
20090104351 | Kakegawa | Apr 2009 | A1 |
20090104594 | Webb | Apr 2009 | A1 |
20090104789 | Mallick et al. | Apr 2009 | A1 |
20090107404 | Ogliari et al. | Apr 2009 | A1 |
20090108308 | Yang et al. | Apr 2009 | A1 |
20090112458 | Nakai | Apr 2009 | A1 |
20090115064 | Sandhu et al. | May 2009 | A1 |
20090116936 | Marubayashi et al. | May 2009 | A1 |
20090117717 | Tomasini et al. | May 2009 | A1 |
20090117746 | Masuda | May 2009 | A1 |
20090120580 | Kagoshima et al. | May 2009 | A1 |
20090122293 | Shibazaki | May 2009 | A1 |
20090122458 | Lischer et al. | May 2009 | A1 |
20090124131 | Breunsbach et al. | May 2009 | A1 |
20090130331 | Asai | May 2009 | A1 |
20090130859 | Itatani et al. | May 2009 | A1 |
20090136665 | Choi et al. | May 2009 | A1 |
20090136668 | Gregg et al. | May 2009 | A1 |
20090136683 | Fukasawa et al. | May 2009 | A1 |
20090137055 | Bognar | May 2009 | A1 |
20090139657 | Lee et al. | Jun 2009 | A1 |
20090142905 | Yamazaki | Jun 2009 | A1 |
20090142933 | Yajima et al. | Jun 2009 | A1 |
20090142935 | Fukazawa et al. | Jun 2009 | A1 |
20090146322 | Weling et al. | Jun 2009 | A1 |
20090147819 | Goodman et al. | Jun 2009 | A1 |
20090155488 | Nakano et al. | Jun 2009 | A1 |
20090156015 | Park et al. | Jun 2009 | A1 |
20090156017 | Fukazawa et al. | Jun 2009 | A1 |
20090159000 | Aggarwal et al. | Jun 2009 | A1 |
20090159002 | Bera et al. | Jun 2009 | A1 |
20090159424 | Liu et al. | Jun 2009 | A1 |
20090162647 | Sun et al. | Jun 2009 | A1 |
20090162996 | Ramaswarmy et al. | Jun 2009 | A1 |
20090163038 | Miyoshi | Jun 2009 | A1 |
20090165715 | Oh | Jul 2009 | A1 |
20090165721 | Pitney et al. | Jul 2009 | A1 |
20090165722 | Ha | Jul 2009 | A1 |
20090166616 | Uchiyama | Jul 2009 | A1 |
20090179365 | Lerner et al. | Jul 2009 | A1 |
20090183520 | Yukimoto | Jul 2009 | A1 |
20090186479 | Okabe et al. | Jul 2009 | A1 |
20090186571 | Haro | Jul 2009 | A1 |
20090194233 | Tamura et al. | Aug 2009 | A1 |
20090197015 | Kudela et al. | Aug 2009 | A1 |
20090197411 | Dussarrat et al. | Aug 2009 | A1 |
20090200494 | Hatem | Aug 2009 | A1 |
20090200547 | Griffin et al. | Aug 2009 | A1 |
20090204403 | Hollander et al. | Aug 2009 | A1 |
20090206056 | Xu | Aug 2009 | A1 |
20090209081 | Matero | Aug 2009 | A1 |
20090211523 | Kuppurao et al. | Aug 2009 | A1 |
20090211525 | Sarigiannis et al. | Aug 2009 | A1 |
20090214825 | Sun et al. | Aug 2009 | A1 |
20090217871 | Kim et al. | Sep 2009 | A1 |
20090221149 | Hammond et al. | Sep 2009 | A1 |
20090221151 | Honda et al. | Sep 2009 | A1 |
20090223441 | Arena et al. | Sep 2009 | A1 |
20090227094 | Bateman | Sep 2009 | A1 |
20090230211 | Kobayashi et al. | Sep 2009 | A1 |
20090232985 | Dussarrat et al. | Sep 2009 | A1 |
20090236014 | Wilson | Sep 2009 | A1 |
20090236276 | Kurth et al. | Sep 2009 | A1 |
20090239386 | Suzaki et al. | Sep 2009 | A1 |
20090242130 | Tian et al. | Oct 2009 | A1 |
20090242957 | Ma et al. | Oct 2009 | A1 |
20090246374 | Vukovic | Oct 2009 | A1 |
20090246399 | Goundar | Oct 2009 | A1 |
20090246971 | Reid et al. | Oct 2009 | A1 |
20090250004 | Yamada et al. | Oct 2009 | A1 |
20090250955 | Aoki | Oct 2009 | A1 |
20090255901 | Okita | Oct 2009 | A1 |
20090256127 | Feist et al. | Oct 2009 | A1 |
20090261331 | Yang et al. | Oct 2009 | A1 |
20090266296 | Tachibana et al. | Oct 2009 | A1 |
20090267135 | Tanaka et al. | Oct 2009 | A1 |
20090267225 | Eguchi | Oct 2009 | A1 |
20090269506 | Okura et al. | Oct 2009 | A1 |
20090269507 | Yu et al. | Oct 2009 | A1 |
20090269941 | Raisanen | Oct 2009 | A1 |
20090275205 | Kiehlbauch et al. | Nov 2009 | A1 |
20090275210 | Shanker et al. | Nov 2009 | A1 |
20090277510 | Shikata | Nov 2009 | A1 |
20090277874 | Rui et al. | Nov 2009 | A1 |
20090280248 | Goodman et al. | Nov 2009 | A1 |
20090283041 | Tomiyasu et al. | Nov 2009 | A1 |
20090283217 | Lubomirsky et al. | Nov 2009 | A1 |
20090284156 | Hanna et al. | Nov 2009 | A1 |
20090286400 | Heo et al. | Nov 2009 | A1 |
20090286402 | Xia et al. | Nov 2009 | A1 |
20090286405 | Okesaku et al. | Nov 2009 | A1 |
20090289300 | Sasaki et al. | Nov 2009 | A1 |
20090291208 | Gordon et al. | Nov 2009 | A1 |
20090297710 | Lindfors | Dec 2009 | A1 |
20090298257 | Lee et al. | Dec 2009 | A1 |
20090302002 | Collins et al. | Dec 2009 | A1 |
20090302434 | Pallem et al. | Dec 2009 | A1 |
20090304558 | Patton | Dec 2009 | A1 |
20090308315 | de Ridder | Dec 2009 | A1 |
20090308425 | Yednak | Dec 2009 | A1 |
20090311857 | Todd et al. | Dec 2009 | A1 |
20090314208 | Zhou et al. | Dec 2009 | A1 |
20090315093 | Li et al. | Dec 2009 | A1 |
20090317214 | Hsiao et al. | Dec 2009 | A1 |
20090320754 | Oya | Dec 2009 | A1 |
20090320881 | Aitchison | Dec 2009 | A1 |
20090324971 | De Vries et al. | Dec 2009 | A1 |
20090324989 | Witz et al. | Dec 2009 | A1 |
20090325391 | De Vusser et al. | Dec 2009 | A1 |
20090325469 | Koo et al. | Dec 2009 | A1 |
20100000608 | Goto et al. | Jan 2010 | A1 |
20100001409 | Humbert et al. | Jan 2010 | A1 |
20100003406 | Lam et al. | Jan 2010 | A1 |
20100006031 | Choi et al. | Jan 2010 | A1 |
20100006923 | Fujitsuka | Jan 2010 | A1 |
20100012036 | Silva et al. | Jan 2010 | A1 |
20100014479 | Kim | Jan 2010 | A1 |
20100015813 | McGinnis et al. | Jan 2010 | A1 |
20100018460 | Singh et al. | Jan 2010 | A1 |
20100018913 | Blum | Jan 2010 | A1 |
20100022097 | Yamoto et al. | Jan 2010 | A1 |
20100024727 | Kim et al. | Feb 2010 | A1 |
20100024872 | Kishimoto | Feb 2010 | A1 |
20100025766 | Nuttinck et al. | Feb 2010 | A1 |
20100025796 | Dabiran | Feb 2010 | A1 |
20100032587 | Hosch et al. | Feb 2010 | A1 |
20100032842 | Herdt et al. | Feb 2010 | A1 |
20100034719 | Dussarrat et al. | Feb 2010 | A1 |
20100040441 | Obikane | Feb 2010 | A1 |
20100041179 | Lee | Feb 2010 | A1 |
20100041243 | Cheng et al. | Feb 2010 | A1 |
20100046321 | McLaughlin et al. | Feb 2010 | A1 |
20100050943 | Kato et al. | Mar 2010 | A1 |
20100051584 | Okita et al. | Mar 2010 | A1 |
20100051597 | Morita et al. | Mar 2010 | A1 |
20100055312 | Kato et al. | Mar 2010 | A1 |
20100055316 | Honma | Mar 2010 | A1 |
20100055318 | Volf et al. | Mar 2010 | A1 |
20100055442 | Kellock | Mar 2010 | A1 |
20100055898 | Chang et al. | Mar 2010 | A1 |
20100058984 | Marubayashi | Mar 2010 | A1 |
20100065758 | Liu et al. | Mar 2010 | A1 |
20100068009 | Kimura | Mar 2010 | A1 |
20100068383 | Kato et al. | Mar 2010 | A1 |
20100068414 | Takahashi et al. | Mar 2010 | A1 |
20100068891 | Hatanaka et al. | Mar 2010 | A1 |
20100075037 | Marsh et al. | Mar 2010 | A1 |
20100075507 | Chang et al. | Mar 2010 | A1 |
20100078601 | Pallem et al. | Apr 2010 | A1 |
20100078746 | Jung | Apr 2010 | A1 |
20100081094 | Hasebe et al. | Apr 2010 | A1 |
20100081293 | Mallick et al. | Apr 2010 | A1 |
20100086703 | Mangum et al. | Apr 2010 | A1 |
20100087069 | Miya et al. | Apr 2010 | A1 |
20100089320 | Kim | Apr 2010 | A1 |
20100089870 | Hiroshima et al. | Apr 2010 | A1 |
20100090149 | Thompson et al. | Apr 2010 | A1 |
20100092679 | Lee et al. | Apr 2010 | A1 |
20100092696 | Shinriki | Apr 2010 | A1 |
20100093187 | Lee et al. | Apr 2010 | A1 |
20100094430 | Krumdieck | Apr 2010 | A1 |
20100098862 | Xu et al. | Apr 2010 | A1 |
20100101728 | Iwasaki | Apr 2010 | A1 |
20100102417 | Ganguli et al. | Apr 2010 | A1 |
20100105936 | Tada et al. | Apr 2010 | A1 |
20100111648 | Tamura et al. | May 2010 | A1 |
20100112496 | Nakajima et al. | May 2010 | A1 |
20100116207 | Givens | May 2010 | A1 |
20100116209 | Kato | May 2010 | A1 |
20100119439 | Shindou | May 2010 | A1 |
20100119727 | Takagi | May 2010 | A1 |
20100120261 | Kim et al. | May 2010 | A1 |
20100124610 | Aikawa et al. | May 2010 | A1 |
20100124618 | Kobayashi et al. | May 2010 | A1 |
20100124621 | Kobayashi et al. | May 2010 | A1 |
20100126415 | Ishino et al. | May 2010 | A1 |
20100126539 | Lee et al. | May 2010 | A1 |
20100126605 | Stones | May 2010 | A1 |
20100126666 | Tandou et al. | May 2010 | A1 |
20100129548 | Sneh | May 2010 | A1 |
20100129990 | Nishizawa et al. | May 2010 | A1 |
20100130015 | Nakajima et al. | May 2010 | A1 |
20100130017 | Luo et al. | May 2010 | A1 |
20100130105 | Lee | May 2010 | A1 |
20100134023 | Mills | Jun 2010 | A1 |
20100136216 | Tsuei et al. | Jun 2010 | A1 |
20100140221 | Kikuchi et al. | Jun 2010 | A1 |
20100140684 | Ozawa | Jun 2010 | A1 |
20100143609 | Fukazawa et al. | Jun 2010 | A1 |
20100144150 | Sills et al. | Jun 2010 | A1 |
20100144162 | Lee et al. | Jun 2010 | A1 |
20100144968 | Lee et al. | Jun 2010 | A1 |
20100145547 | Darabnia et al. | Jun 2010 | A1 |
20100151206 | Wu et al. | Jun 2010 | A1 |
20100159638 | Jeong | Jun 2010 | A1 |
20100159707 | Huang et al. | Jun 2010 | A1 |
20100162752 | Tabata et al. | Jul 2010 | A1 |
20100162956 | Murakami et al. | Jul 2010 | A1 |
20100163524 | Arai | Jul 2010 | A1 |
20100163937 | Clendenning | Jul 2010 | A1 |
20100166630 | Gu et al. | Jul 2010 | A1 |
20100168404 | Girolami et al. | Jul 2010 | A1 |
20100170441 | Won et al. | Jul 2010 | A1 |
20100170868 | Lin et al. | Jul 2010 | A1 |
20100173432 | White et al. | Jul 2010 | A1 |
20100178137 | Chintalapati et al. | Jul 2010 | A1 |
20100178423 | Shimizu et al. | Jul 2010 | A1 |
20100180819 | Hatanaka et al. | Jul 2010 | A1 |
20100183825 | Becker et al. | Jul 2010 | A1 |
20100184302 | Lee et al. | Jul 2010 | A1 |
20100186669 | Shin et al. | Jul 2010 | A1 |
20100189923 | Goundar et al. | Jul 2010 | A1 |
20100193501 | Zucker et al. | Aug 2010 | A1 |
20100193955 | Milligan et al. | Aug 2010 | A1 |
20100195392 | Freeman | Aug 2010 | A1 |
20100197107 | Matsuzaki | Aug 2010 | A1 |
20100202860 | Reed | Aug 2010 | A1 |
20100203242 | Borden | Aug 2010 | A1 |
20100206767 | Odashima et al. | Aug 2010 | A1 |
20100209598 | Xu et al. | Aug 2010 | A1 |
20100210108 | Ishizaka et al. | Aug 2010 | A1 |
20100219757 | Benzerrouk et al. | Sep 2010 | A1 |
20100221452 | Kang | Sep 2010 | A1 |
20100224130 | Smith et al. | Sep 2010 | A1 |
20100227458 | Chung et al. | Sep 2010 | A1 |
20100229795 | Tanabe | Sep 2010 | A1 |
20100229965 | Kashima et al. | Sep 2010 | A1 |
20100230051 | Iizuka | Sep 2010 | A1 |
20100230863 | Moench et al. | Sep 2010 | A1 |
20100233885 | Kushibiki et al. | Sep 2010 | A1 |
20100233886 | Yang et al. | Sep 2010 | A1 |
20100236691 | Yamazaki | Sep 2010 | A1 |
20100243166 | Hayashi et al. | Sep 2010 | A1 |
20100244688 | Braun et al. | Sep 2010 | A1 |
20100248465 | Yi et al. | Sep 2010 | A1 |
20100252434 | Roy | Oct 2010 | A1 |
20100255196 | Geisler et al. | Oct 2010 | A1 |
20100255198 | Cleary et al. | Oct 2010 | A1 |
20100255218 | Oka et al. | Oct 2010 | A1 |
20100255625 | De Vries | Oct 2010 | A1 |
20100255658 | Aggarwal | Oct 2010 | A1 |
20100259152 | Yasuda et al. | Oct 2010 | A1 |
20100266765 | White et al. | Oct 2010 | A1 |
20100267224 | Choi et al. | Oct 2010 | A1 |
20100267248 | Ma et al. | Oct 2010 | A1 |
20100270675 | Harada | Oct 2010 | A1 |
20100246630 | Kaszynski et al. | Nov 2010 | A1 |
20100275846 | Kitagawa | Nov 2010 | A1 |
20100279008 | Takagi | Nov 2010 | A1 |
20100279512 | Udea et al. | Nov 2010 | A1 |
20100282163 | Aggarwal et al. | Nov 2010 | A1 |
20100282170 | Nishizawa | Nov 2010 | A1 |
20100282645 | Wang | Nov 2010 | A1 |
20100285237 | Ditizio et al. | Nov 2010 | A1 |
20100285319 | Kwak et al. | Nov 2010 | A1 |
20100294199 | Tran et al. | Nov 2010 | A1 |
20100297391 | Kley | Nov 2010 | A1 |
20100301752 | Bakre et al. | Dec 2010 | A1 |
20100304047 | Yang et al. | Dec 2010 | A1 |
20100307415 | Shero et al. | Dec 2010 | A1 |
20100317177 | Huang et al. | Dec 2010 | A1 |
20100317198 | Antonelli | Dec 2010 | A1 |
20100322604 | Fondurulia et al. | Dec 2010 | A1 |
20100326358 | Choi | Dec 2010 | A1 |
20110000619 | Suh | Jan 2011 | A1 |
20110003087 | Soininen et al. | Jan 2011 | A1 |
20110003450 | Lee et al. | Jan 2011 | A1 |
20110005684 | Hayami et al. | Jan 2011 | A1 |
20110006402 | Zhou | Jan 2011 | A1 |
20110006406 | Urbanowicz et al. | Jan 2011 | A1 |
20110008950 | Xu | Jan 2011 | A1 |
20110014359 | Hashim | Jan 2011 | A1 |
20110014795 | Lee | Jan 2011 | A1 |
20110017139 | Chiang et al. | Jan 2011 | A1 |
20110021033 | Ikeuchi et al. | Jan 2011 | A1 |
20110027725 | Tsutsumi et al. | Feb 2011 | A1 |
20110027999 | Sparks et al. | Feb 2011 | A1 |
20110031562 | Lin et al. | Feb 2011 | A1 |
20110034039 | Liang et al. | Feb 2011 | A1 |
20110039419 | Date et al. | Feb 2011 | A1 |
20110041764 | Webb et al. | Feb 2011 | A1 |
20110042200 | Wilby | Feb 2011 | A1 |
20110045610 | van Schravendijk | Feb 2011 | A1 |
20110045676 | Park et al. | Feb 2011 | A1 |
20110046314 | Klipp et al. | Feb 2011 | A1 |
20110048642 | Mihara et al. | Mar 2011 | A1 |
20110048769 | Fujwara | Mar 2011 | A1 |
20110049100 | Han et al. | Mar 2011 | A1 |
20110052833 | Hanawa et al. | Mar 2011 | A1 |
20110053383 | Shero et al. | Mar 2011 | A1 |
20110056513 | Hombach et al. | Mar 2011 | A1 |
20110056626 | Brown et al. | Mar 2011 | A1 |
20110057248 | Ma et al. | Mar 2011 | A1 |
20110061810 | Ganguly et al. | Mar 2011 | A1 |
20110065289 | Asai | Mar 2011 | A1 |
20110067522 | Lai | Mar 2011 | A1 |
20110070380 | Shero et al. | Mar 2011 | A1 |
20110070740 | Bettencourt et al. | Mar 2011 | A1 |
20110076401 | Chao et al. | Mar 2011 | A1 |
20110081519 | Dillingh | Apr 2011 | A1 |
20110083496 | Lin et al. | Apr 2011 | A1 |
20110086516 | Lee et al. | Apr 2011 | A1 |
20110089166 | Hunter et al. | Apr 2011 | A1 |
20110089469 | Merckling | Apr 2011 | A1 |
20110092077 | Xu et al. | Apr 2011 | A1 |
20110097901 | Banna et al. | Apr 2011 | A1 |
20110098841 | Tsuda | Apr 2011 | A1 |
20110104395 | Kumagai et al. | May 2011 | A1 |
20110107512 | Gilbert | May 2011 | A1 |
20110108194 | Yoshioka et al. | May 2011 | A1 |
20110108424 | Puget et al. | May 2011 | A1 |
20110108741 | Ingram | May 2011 | A1 |
20110108929 | Meng | May 2011 | A1 |
20110114261 | Matsumoto et al. | May 2011 | A1 |
20110114601 | Lubomirsky et al. | May 2011 | A1 |
20110115378 | Lubomirsky et al. | May 2011 | A1 |
20110117490 | Bae et al. | May 2011 | A1 |
20110117492 | Yamada et al. | May 2011 | A1 |
20110117732 | Bauer et al. | May 2011 | A1 |
20110117737 | Agarwala et al. | May 2011 | A1 |
20110117749 | Sheu | May 2011 | A1 |
20110121503 | Burrows et al. | May 2011 | A1 |
20110121736 | Hirayama et al. | May 2011 | A1 |
20110124196 | Lee | May 2011 | A1 |
20110132542 | Ilzuka | Jun 2011 | A1 |
20110135842 | Faguet et al. | Jun 2011 | A1 |
20110139272 | Matsumoto et al. | Jun 2011 | A1 |
20110139748 | Donnelly et al. | Jun 2011 | A1 |
20110140172 | Chu | Jun 2011 | A1 |
20110140173 | Ramdani | Jun 2011 | A1 |
20110143032 | Vrtis et al. | Jun 2011 | A1 |
20110143461 | Fish et al. | Jun 2011 | A1 |
20110155264 | Minami et al. | Jun 2011 | A1 |
20110155322 | Himori et al. | Jun 2011 | A1 |
20110159200 | Kogure | Jun 2011 | A1 |
20110159202 | Matsushita | Jun 2011 | A1 |
20110159673 | Hanawa et al. | Jun 2011 | A1 |
20110159680 | Yoo | Jun 2011 | A1 |
20110168330 | Sakaue et al. | Jul 2011 | A1 |
20110171775 | Yamamoto et al. | Jul 2011 | A1 |
20110175011 | Ehrne et al. | Jul 2011 | A1 |
20110177648 | Tanner et al. | Jul 2011 | A1 |
20110180233 | Bera et al. | Jul 2011 | A1 |
20110183079 | Jackson et al. | Jul 2011 | A1 |
20110183269 | Zhu | Jul 2011 | A1 |
20110183527 | Cho | Jul 2011 | A1 |
20110185969 | Yang | Aug 2011 | A1 |
20110192820 | Yeom et al. | Aug 2011 | A1 |
20110198034 | Sun et al. | Aug 2011 | A1 |
20110198417 | Detmar et al. | Aug 2011 | A1 |
20110198736 | Shero et al. | Aug 2011 | A1 |
20110204025 | Tahara | Aug 2011 | A1 |
20110207332 | Liu et al. | Aug 2011 | A1 |
20110210468 | Shannon et al. | Sep 2011 | A1 |
20110217838 | Hsieh et al. | Sep 2011 | A1 |
20110220874 | Hanrath | Sep 2011 | A1 |
20110223334 | Yudovsky et al. | Sep 2011 | A1 |
20110226421 | Hayashi | Sep 2011 | A1 |
20110232678 | Shih et al. | Sep 2011 | A1 |
20110236201 | Shende | Sep 2011 | A1 |
20110236594 | Haverkamp et al. | Sep 2011 | A1 |
20110236600 | Fox et al. | Sep 2011 | A1 |
20110237040 | Ng et al. | Sep 2011 | A1 |
20110239936 | Suzaki et al. | Oct 2011 | A1 |
20110239940 | Benvenuti et al. | Oct 2011 | A1 |
20110244673 | Cho et al. | Oct 2011 | A1 |
20110253044 | Tam et al. | Oct 2011 | A1 |
20110254052 | Kouvetakis | Oct 2011 | A1 |
20110256675 | Avouris | Oct 2011 | A1 |
20110256724 | Chandrasekharan et al. | Oct 2011 | A1 |
20110256726 | Lavoie et al. | Oct 2011 | A1 |
20110256727 | Beynet et al. | Oct 2011 | A1 |
20110256734 | Hausmann et al. | Oct 2011 | A1 |
20110259519 | Kenworthy et al. | Oct 2011 | A1 |
20110262642 | Xiao et al. | Oct 2011 | A1 |
20110263107 | Chung et al. | Oct 2011 | A1 |
20110263115 | Ganguli et al. | Oct 2011 | A1 |
20110264250 | Nishimura et al. | Oct 2011 | A1 |
20110265549 | Cruse et al. | Nov 2011 | A1 |
20110265715 | Keller | Nov 2011 | A1 |
20110265725 | Tsuji | Nov 2011 | A1 |
20110265951 | Xu et al. | Nov 2011 | A1 |
20110266611 | Kim et al. | Nov 2011 | A1 |
20110269314 | Lee et al. | Nov 2011 | A1 |
20110275018 | Matteo et al. | Nov 2011 | A1 |
20110275166 | Shero et al. | Nov 2011 | A1 |
20110277690 | Rozenzon et al. | Nov 2011 | A1 |
20110281417 | Gordon et al. | Nov 2011 | A1 |
20110283933 | Makarov et al. | Nov 2011 | A1 |
20110291243 | Seamons | Dec 2011 | A1 |
20110294075 | Chen et al. | Dec 2011 | A1 |
20110294288 | Lee et al. | Dec 2011 | A1 |
20110298062 | Ganguli et al. | Dec 2011 | A1 |
20110300720 | Fu | Dec 2011 | A1 |
20110305102 | Berger et al. | Dec 2011 | A1 |
20110308453 | Su et al. | Dec 2011 | A1 |
20110308460 | Hong et al. | Dec 2011 | A1 |
20110312191 | Ohkura et al. | Dec 2011 | A1 |
20110318888 | Komatsu et al. | Dec 2011 | A1 |
20110318935 | Oyabu et al. | Dec 2011 | A1 |
20120001172 | Shang et al. | Jan 2012 | A1 |
20120003500 | Yoshida et al. | Jan 2012 | A1 |
20120003726 | Jones et al. | Jan 2012 | A1 |
20120003831 | Kang et al. | Jan 2012 | A1 |
20120006489 | Okita | Jan 2012 | A1 |
20120009802 | Lavoie | Jan 2012 | A1 |
20120012556 | Matsumoto et al. | Jan 2012 | A1 |
20120021252 | Lee | Jan 2012 | A1 |
20120024223 | Torres et al. | Feb 2012 | A1 |
20120024227 | Takasuka et al. | Feb 2012 | A1 |
20120024231 | Horino | Feb 2012 | A1 |
20120024478 | Huang et al. | Feb 2012 | A1 |
20120024479 | Palagashvili et al. | Feb 2012 | A1 |
20120028454 | Swaminathan et al. | Feb 2012 | A1 |
20120028469 | Onizawa et al. | Feb 2012 | A1 |
20120031333 | Kurita et al. | Feb 2012 | A1 |
20120031500 | Hirose et al. | Feb 2012 | A1 |
20120032311 | Gates | Feb 2012 | A1 |
20120033695 | Hayashi et al. | Feb 2012 | A1 |
20120034793 | Narushima et al. | Feb 2012 | A1 |
20120036732 | Varadaraj An | Feb 2012 | A1 |
20120040097 | Volf et al. | Feb 2012 | A1 |
20120040528 | Kim et al. | Feb 2012 | A1 |
20120043556 | Dube et al. | Feb 2012 | A1 |
20120043617 | Nakagawa et al. | Feb 2012 | A1 |
20120046421 | Darling et al. | Feb 2012 | A1 |
20120052681 | Marsh | Mar 2012 | A1 |
20120058270 | Winter et al. | Mar 2012 | A1 |
20120058630 | Quinn | Mar 2012 | A1 |
20120064690 | Hirota et al. | Mar 2012 | A1 |
20120064726 | Nozawa et al. | Mar 2012 | A1 |
20120064764 | Islam | Mar 2012 | A1 |
20120068242 | Shin | Mar 2012 | A1 |
20120070136 | Koelmel et al. | Mar 2012 | A1 |
20120070997 | Larson | Mar 2012 | A1 |
20120073400 | Wang | Mar 2012 | A1 |
20120074533 | Aoyama | Mar 2012 | A1 |
20120077349 | Li et al. | Mar 2012 | A1 |
20120080756 | Suzuki | Apr 2012 | A1 |
20120083134 | Wu et al. | Apr 2012 | A1 |
20120088031 | Neel | Apr 2012 | A1 |
20120090704 | Laverdiere et al. | Apr 2012 | A1 |
20120091522 | Ozaki et al. | Apr 2012 | A1 |
20120094468 | Bhatia et al. | Apr 2012 | A1 |
20120098107 | Raisanen et al. | Apr 2012 | A1 |
20120100464 | Kageyama | Apr 2012 | A1 |
20120103264 | Choi et al. | May 2012 | A1 |
20120103522 | Hohenwater | May 2012 | A1 |
20120103939 | Wu et al. | May 2012 | A1 |
20120104514 | Park et al. | May 2012 | A1 |
20120107607 | Takaki et al. | May 2012 | A1 |
20120108039 | Zajaji | May 2012 | A1 |
20120108048 | Lim et al. | May 2012 | A1 |
20120114877 | Lee | May 2012 | A1 |
20120115250 | Ariga et al. | May 2012 | A1 |
20120115257 | Matsuyam et al. | May 2012 | A1 |
20120119337 | Sasaki et al. | May 2012 | A1 |
20120121823 | Chhabra | May 2012 | A1 |
20120122275 | Koo et al. | May 2012 | A1 |
20120122302 | Weisman et al. | May 2012 | A1 |
20120122319 | Shimizu | May 2012 | A1 |
20120125258 | Lee | May 2012 | A1 |
20120126300 | Park et al. | May 2012 | A1 |
20120128897 | Xiao et al. | May 2012 | A1 |
20120135145 | Je et al. | May 2012 | A1 |
20120139009 | Ning et al. | Jun 2012 | A1 |
20120145078 | Huang et al. | Jun 2012 | A1 |
20120146113 | Suzuki et al. | Jun 2012 | A1 |
20120149207 | Graff | Jun 2012 | A1 |
20120149213 | Nittala | Jun 2012 | A1 |
20120156108 | Fondurulia et al. | Jun 2012 | A1 |
20120156890 | Yim et al. | Jun 2012 | A1 |
20120160172 | Wamura et al. | Jun 2012 | A1 |
20120160809 | Ishibashi et al. | Jun 2012 | A1 |
20120161126 | Yamazaki | Jun 2012 | A1 |
20120161405 | Mohn | Jun 2012 | A1 |
20120164327 | Sato | Jun 2012 | A1 |
20120164837 | Tan et al. | Jun 2012 | A1 |
20120164842 | Watanabe | Jun 2012 | A1 |
20120164846 | Ha et al. | Jun 2012 | A1 |
20120170170 | Gros-Jean | Jul 2012 | A1 |
20120171391 | Won | Jul 2012 | A1 |
20120171874 | Thridandam et al. | Jul 2012 | A1 |
20120175518 | Godet et al. | Jul 2012 | A1 |
20120175751 | Gatineau et al. | Jul 2012 | A1 |
20120180719 | Inoue et al. | Jul 2012 | A1 |
20120180954 | Yang et al. | Jul 2012 | A1 |
20120183689 | Suzuki et al. | Jul 2012 | A1 |
20120186521 | Iwasaki et al. | Jul 2012 | A1 |
20120186573 | Jdira et al. | Jul 2012 | A1 |
20120187083 | Hashizume | Jul 2012 | A1 |
20120187305 | Elam et al. | Jul 2012 | A1 |
20120190178 | Wang et al. | Jul 2012 | A1 |
20120190185 | Rogers | Jul 2012 | A1 |
20120190208 | Ozu et al. | Jul 2012 | A1 |
20120196048 | Ueda | Aug 2012 | A1 |
20120196450 | Balseanu et al. | Aug 2012 | A1 |
20120202358 | Gealy et al. | Aug 2012 | A1 |
20120206033 | Matsuyama | Aug 2012 | A1 |
20120207456 | Kim et al. | Aug 2012 | A1 |
20120212121 | Lin | Aug 2012 | A1 |
20120213947 | Lee | Aug 2012 | A1 |
20120214318 | Fukazawa et al. | Aug 2012 | A1 |
20120216743 | Itoh et al. | Aug 2012 | A1 |
20120219824 | Prolier et al. | Aug 2012 | A1 |
20120220139 | Lee et al. | Aug 2012 | A1 |
20120222815 | Sabri et al. | Sep 2012 | A1 |
20120225192 | Yudovsky et al. | Sep 2012 | A1 |
20120225561 | Watanabe | Sep 2012 | A1 |
20120231771 | Marcus | Sep 2012 | A1 |
20120232340 | Levy et al. | Sep 2012 | A1 |
20120238074 | Santhanam et al. | Sep 2012 | A1 |
20120240858 | Taniyama et al. | Sep 2012 | A1 |
20120241089 | Dielmann et al. | Sep 2012 | A1 |
20120241411 | Darling et al. | Sep 2012 | A1 |
20120244703 | Nakayama et al. | Sep 2012 | A1 |
20120247386 | Sanchez et al. | Oct 2012 | A1 |
20120252229 | Timans et al. | Oct 2012 | A1 |
20120258257 | Nguyen et al. | Oct 2012 | A1 |
20120263876 | Hauldca et al. | Oct 2012 | A1 |
20120263887 | Papasouliotis et al. | Oct 2012 | A1 |
20120264051 | Angelov et al. | Oct 2012 | A1 |
20120264305 | Nakano | Oct 2012 | A1 |
20120267048 | Moyama et al. | Oct 2012 | A1 |
20120269967 | Yudovsky et al. | Oct 2012 | A1 |
20120270339 | Xie et al. | Oct 2012 | A1 |
20120270393 | Pore et al. | Oct 2012 | A1 |
20120273052 | Ye et al. | Nov 2012 | A1 |
20120273162 | Mahadeswaraswamy | Nov 2012 | A1 |
20120288625 | Furuya et al. | Nov 2012 | A1 |
20120289053 | Holland et al. | Nov 2012 | A1 |
20120289056 | Bergman et al. | Nov 2012 | A1 |
20120289057 | DeDontney | Nov 2012 | A1 |
20120295427 | Bauer | Nov 2012 | A1 |
20120295449 | Fukazawa | Nov 2012 | A1 |
20120302055 | Pore et al. | Nov 2012 | A1 |
20120303313 | Moroi et al. | Nov 2012 | A1 |
20120304935 | Oosterlaken et al. | Dec 2012 | A1 |
20120305026 | Nomura et al. | Dec 2012 | A1 |
20120305196 | Mori et al. | Dec 2012 | A1 |
20120305987 | Hirler | Dec 2012 | A1 |
20120307588 | Hanada et al. | Dec 2012 | A1 |
20120309181 | Machkaoutsan et al. | Dec 2012 | A1 |
20120310440 | Darabnia et al. | Dec 2012 | A1 |
20120315113 | Hiroki | Dec 2012 | A1 |
20120315404 | Li et al. | Dec 2012 | A1 |
20120318334 | Bedell et al. | Dec 2012 | A1 |
20120318457 | Nguyen et al. | Dec 2012 | A1 |
20120318773 | Wu et al. | Dec 2012 | A1 |
20120319279 | Isobayashi | Dec 2012 | A1 |
20120321786 | Satitpunwaycha et al. | Dec 2012 | A1 |
20120322250 | Ganguli et al. | Dec 2012 | A1 |
20120322252 | Son et al. | Dec 2012 | A1 |
20120325148 | Yamagishi et al. | Dec 2012 | A1 |
20120328780 | Yamagishi et al. | Dec 2012 | A1 |
20130002121 | Ma | Jan 2013 | A1 |
20130005122 | Schwarzenbach et al. | Jan 2013 | A1 |
20130005147 | Angyal et al. | Jan 2013 | A1 |
20130008607 | Matsumoto et al. | Jan 2013 | A1 |
20130011983 | Tsai | Jan 2013 | A1 |
20130011984 | Wang et al. | Jan 2013 | A1 |
20130012034 | Ahn et al. | Jan 2013 | A1 |
20130014697 | Kanayama | Jan 2013 | A1 |
20130014896 | Shoji et al. | Jan 2013 | A1 |
20130017503 | de Ridder et al. | Jan 2013 | A1 |
20130019944 | Hekmatshoar-Tabai et al. | Jan 2013 | A1 |
20130019945 | Hekmatshoar-Tabai et al. | Jan 2013 | A1 |
20130019960 | Choi et al. | Jan 2013 | A1 |
20130020246 | Hoots et al. | Jan 2013 | A1 |
20130023120 | Yaehashi et al. | Jan 2013 | A1 |
20130023124 | Nemani et al. | Jan 2013 | A1 |
20130023129 | Reed | Jan 2013 | A1 |
20130025538 | Collins et al. | Jan 2013 | A1 |
20130025786 | Davidkovich et al. | Jan 2013 | A1 |
20130026451 | Bangsaruntip et al. | Jan 2013 | A1 |
20130032085 | Hanawa et al. | Feb 2013 | A1 |
20130037858 | Hong et al. | Feb 2013 | A1 |
20130037886 | Tsai et al. | Feb 2013 | A1 |
20130040447 | Swaminathan et al. | Feb 2013 | A1 |
20130040481 | Vallely et al. | Feb 2013 | A1 |
20130042811 | Shanker et al. | Feb 2013 | A1 |
20130048606 | Mao et al. | Feb 2013 | A1 |
20130052585 | Ayothi et al. | Feb 2013 | A1 |
20130052836 | Hirose et al. | Feb 2013 | A1 |
20130059078 | Gatineau et al. | Mar 2013 | A1 |
20130061755 | Frederick | Mar 2013 | A1 |
20130062753 | Nguyen et al. | Mar 2013 | A1 |
20130064973 | Chen et al. | Mar 2013 | A1 |
20130065189 | Yoshii et al. | Mar 2013 | A1 |
20130068727 | Okita | Mar 2013 | A1 |
20130068970 | Matsushita | Mar 2013 | A1 |
20130069052 | Sandhu | Mar 2013 | A1 |
20130070456 | Jang et al. | Mar 2013 | A1 |
20130075746 | Mallikarjunaswamy et al. | Mar 2013 | A1 |
20130078376 | Higashino et al. | Mar 2013 | A1 |
20130078392 | Xiao et al. | Mar 2013 | A1 |
20130081702 | Mohammed et al. | Apr 2013 | A1 |
20130082274 | Yang | Apr 2013 | A1 |
20130084156 | Shimamoto | Apr 2013 | A1 |
20130084408 | Nakao et al. | Apr 2013 | A1 |
20130084711 | Liang et al. | Apr 2013 | A1 |
20130084714 | Oka et al. | Apr 2013 | A1 |
20130089667 | Lai et al. | Apr 2013 | A1 |
20130089716 | Krishnamurthy et al. | Apr 2013 | A1 |
20130092085 | Lee | Apr 2013 | A1 |
20130093048 | Chang et al. | Apr 2013 | A1 |
20130093321 | Yoshikawa et al. | Apr 2013 | A1 |
20130095664 | Matero et al. | Apr 2013 | A1 |
20130095973 | Kroneberger et al. | Apr 2013 | A1 |
20130099318 | Adam et al. | Apr 2013 | A1 |
20130104988 | Yednak et al. | May 2013 | A1 |
20130104992 | Yednak et al. | May 2013 | A1 |
20130107415 | Banna et al. | May 2013 | A1 |
20130112251 | Hang et al. | May 2013 | A1 |
20130113085 | Michaelson et al. | May 2013 | A1 |
20130115383 | Lu et al. | May 2013 | A1 |
20130115763 | Takamure et al. | May 2013 | A1 |
20130115768 | Pore et al. | May 2013 | A1 |
20130118405 | Ho et al. | May 2013 | A1 |
20130118895 | Roozeboom et al. | May 2013 | A1 |
20130119018 | Kanarik et al. | May 2013 | A1 |
20130122712 | Kim et al. | May 2013 | A1 |
20130122722 | Cissell et al. | May 2013 | A1 |
20130126515 | Shero et al. | May 2013 | A1 |
20130129577 | Halpin et al. | May 2013 | A1 |
20130130490 | Lee et al. | May 2013 | A1 |
20130134148 | Tachikawa | May 2013 | A1 |
20130137279 | Yamamoto et al. | May 2013 | A1 |
20130143401 | Yu et al. | Jun 2013 | A1 |
20130143415 | Yudovsky et al. | Jun 2013 | A1 |
20130145587 | Adhiprakasha | Jun 2013 | A1 |
20130145984 | Zhang et al. | Jun 2013 | A1 |
20130152933 | Lischer et al. | Jun 2013 | A1 |
20130157409 | Vaidya | Jun 2013 | A1 |
20130157521 | Aldrich et al. | Jun 2013 | A1 |
20130160709 | White et al. | Jun 2013 | A1 |
20130161629 | Han et al. | Jun 2013 | A1 |
20130164458 | Soininen et al. | Jun 2013 | A1 |
20130168353 | Okita et al. | Jul 2013 | A1 |
20130168354 | Kanarik | Jul 2013 | A1 |
20130171818 | Kim et al. | Jul 2013 | A1 |
20130175596 | Cheng et al. | Jul 2013 | A1 |
20130177706 | Baluja et al. | Jul 2013 | A1 |
20130180448 | Sakaue et al. | Jul 2013 | A1 |
20130183814 | Huang et al. | Jul 2013 | A1 |
20130186340 | Omori et al. | Jul 2013 | A1 |
20130189635 | Lim et al. | Jul 2013 | A1 |
20130189854 | Hausmann et al. | Jul 2013 | A1 |
20130196502 | Haukka et al. | Aug 2013 | A1 |
20130196507 | Ma et al. | Aug 2013 | A1 |
20130200518 | Ahmed et al. | Aug 2013 | A1 |
20130202387 | Hiroki | Aug 2013 | A1 |
20130203266 | Hintze | Aug 2013 | A1 |
20130203267 | Pomarede et al. | Aug 2013 | A1 |
20130209940 | Sakamoto et al. | Aug 2013 | A1 |
20130210241 | Lavoie et al. | Aug 2013 | A1 |
20130214232 | Tendulkar et al. | Aug 2013 | A1 |
20130217239 | Mallick et al. | Aug 2013 | A1 |
20130217240 | Mallick et al. | Aug 2013 | A1 |
20130217241 | Underwood et al. | Aug 2013 | A1 |
20130217243 | Underwood et al. | Aug 2013 | A1 |
20130219853 | Little et al. | Aug 2013 | A1 |
20130224964 | Fukazawa | Aug 2013 | A1 |
20130228225 | Leeser | Sep 2013 | A1 |
20130228902 | Tomizawa et al. | Sep 2013 | A1 |
20130230814 | Dunn et al. | Sep 2013 | A1 |
20130234203 | Tsai et al. | Sep 2013 | A1 |
20130242287 | Schlezinger | Sep 2013 | A1 |
20130256265 | Darling et al. | Oct 2013 | A1 |
20130256838 | Sanchez et al. | Oct 2013 | A1 |
20130256962 | Ravish | Oct 2013 | A1 |
20130260371 | Holt | Oct 2013 | A1 |
20130264659 | Jung | Oct 2013 | A1 |
20130267045 | Lee et al. | Oct 2013 | A1 |
20130269609 | Leeser | Oct 2013 | A1 |
20130269612 | Cheng et al. | Oct 2013 | A1 |
20130270676 | Lindert et al. | Oct 2013 | A1 |
20130276978 | Bluck et al. | Oct 2013 | A1 |
20130280891 | Kim et al. | Oct 2013 | A1 |
20130285155 | Glass | Oct 2013 | A1 |
20130287526 | Bluck et al. | Oct 2013 | A1 |
20130288427 | Hung et al. | Oct 2013 | A1 |
20130288471 | Chi | Oct 2013 | A1 |
20130288480 | Sanchez et al. | Oct 2013 | A1 |
20130288485 | Liang et al. | Oct 2013 | A1 |
20130292047 | Tian et al. | Nov 2013 | A1 |
20130292676 | Milligan et al. | Nov 2013 | A1 |
20130292807 | Raisanen et al. | Nov 2013 | A1 |
20130295779 | Chandra et al. | Nov 2013 | A1 |
20130299944 | Lai et al. | Nov 2013 | A1 |
20130302520 | Wang et al. | Nov 2013 | A1 |
20130302999 | Won et al. | Nov 2013 | A1 |
20130303803 | Doerr et al. | Nov 2013 | A1 |
20130309876 | Ogawa | Nov 2013 | A1 |
20130312663 | Khosla et al. | Nov 2013 | A1 |
20130313656 | Tong | Nov 2013 | A1 |
20130319290 | Xiao et al. | Dec 2013 | A1 |
20130320429 | Thomas | Dec 2013 | A1 |
20130323435 | Xiao et al. | Dec 2013 | A1 |
20130323859 | Chen et al. | Dec 2013 | A1 |
20130323935 | Suzuki et al. | Dec 2013 | A1 |
20130330165 | Wimplinger | Dec 2013 | A1 |
20130330911 | Huang et al. | Dec 2013 | A1 |
20130330933 | Fukazawa et al. | Dec 2013 | A1 |
20130333619 | Omari | Dec 2013 | A1 |
20130337172 | Lee | Dec 2013 | A1 |
20130337583 | Kobayashi et al. | Dec 2013 | A1 |
20130337639 | Ivantsov | Dec 2013 | A1 |
20130337653 | Kovalgin et al. | Dec 2013 | A1 |
20130340619 | Tammera | Dec 2013 | A1 |
20130340678 | Wamura et al. | Dec 2013 | A1 |
20130344248 | Clark | Dec 2013 | A1 |
20140000843 | Dunn et al. | Jan 2014 | A1 |
20140001520 | Glass | Jan 2014 | A1 |
20140004274 | Thompson | Jan 2014 | A1 |
20140007808 | Okabe et al. | Jan 2014 | A1 |
20140014642 | Elliot et al. | Jan 2014 | A1 |
20140014644 | Akiba et al. | Jan 2014 | A1 |
20140015108 | Kim et al. | Jan 2014 | A1 |
20140015186 | Wessel et al. | Jan 2014 | A1 |
20140017408 | Gandikota et al. | Jan 2014 | A1 |
20140017414 | Fukazawa et al. | Jan 2014 | A1 |
20140017908 | Beynet et al. | Jan 2014 | A1 |
20140020619 | Vincent et al. | Jan 2014 | A1 |
20140020764 | Woelk et al. | Jan 2014 | A1 |
20140020839 | Kenney et al. | Jan 2014 | A1 |
20140023794 | Mahajani et al. | Jan 2014 | A1 |
20140027884 | Tang et al. | Jan 2014 | A1 |
20140030447 | Lee | Jan 2014 | A1 |
20140033978 | Adachi et al. | Feb 2014 | A1 |
20140034240 | Kim et al. | Feb 2014 | A1 |
20140034632 | Pan et al. | Feb 2014 | A1 |
20140036274 | Marquardt et al. | Feb 2014 | A1 |
20140045324 | Brabant et al. | Feb 2014 | A1 |
20140045342 | Mallick et al. | Feb 2014 | A1 |
20140047705 | Singh | Feb 2014 | A1 |
20140048765 | Ma et al. | Feb 2014 | A1 |
20140053866 | Baluja et al. | Feb 2014 | A1 |
20140056679 | Yamabe et al. | Feb 2014 | A1 |
20140056770 | Bedard et al. | Feb 2014 | A1 |
20140057454 | Subramonium | Feb 2014 | A1 |
20140058179 | Stevens et al. | Feb 2014 | A1 |
20140060147 | Sarin et al. | Mar 2014 | A1 |
20140060572 | Yasumuro et al. | Mar 2014 | A1 |
20140061770 | Lee | Mar 2014 | A1 |
20140062304 | Nakano et al. | Mar 2014 | A1 |
20140065841 | Matero | Mar 2014 | A1 |
20140067110 | Lawson et al. | Mar 2014 | A1 |
20140072710 | Valle | Mar 2014 | A1 |
20140072726 | Kim | Mar 2014 | A1 |
20140072925 | Kaneko | Mar 2014 | A1 |
20140073082 | Song | Mar 2014 | A1 |
20140073143 | Alokozai et al. | Mar 2014 | A1 |
20140076861 | Cornelius et al. | Mar 2014 | A1 |
20140077240 | Roucka et al. | Mar 2014 | A1 |
20140084341 | Weeks | Mar 2014 | A1 |
20140087490 | Kahlon | Mar 2014 | A1 |
20140087544 | Tolle | Mar 2014 | A1 |
20140087564 | Shimizu et al. | Mar 2014 | A1 |
20140094027 | Azumo et al. | Apr 2014 | A1 |
20140096716 | Chung et al. | Apr 2014 | A1 |
20140097468 | Okita | Apr 2014 | A1 |
20140099794 | Ingle et al. | Apr 2014 | A1 |
20140099798 | Tsuji | Apr 2014 | A1 |
20140103145 | White et al. | Apr 2014 | A1 |
20140106574 | Kang et al. | Apr 2014 | A1 |
20140110798 | Cai | Apr 2014 | A1 |
20140113457 | Sims | Apr 2014 | A1 |
20140116335 | Tsuji et al. | May 2014 | A1 |
20140117380 | Loboda et al. | May 2014 | A1 |
20140120487 | Kaneko | May 2014 | A1 |
20140120678 | Shinriki et al. | May 2014 | A1 |
20140120723 | Fu et al. | May 2014 | A1 |
20140120738 | Jung | May 2014 | A1 |
20140120750 | Johnson | May 2014 | A1 |
20140127405 | Li et al. | May 2014 | A1 |
20140127907 | Yang | May 2014 | A1 |
20140130687 | Shibusawa et al. | May 2014 | A1 |
20140138779 | Xie et al. | May 2014 | A1 |
20140141165 | Sato et al. | May 2014 | A1 |
20140141625 | Fukazawa et al. | May 2014 | A1 |
20140141674 | Galbreath et al. | May 2014 | A1 |
20140144375 | Kim et al. | May 2014 | A1 |
20140144500 | Cao et al. | May 2014 | A1 |
20140145332 | Ryan et al. | May 2014 | A1 |
20140147587 | Endo et al. | May 2014 | A1 |
20140148924 | Brak et al. | May 2014 | A1 |
20140158786 | Santo | Jun 2014 | A1 |
20140159170 | Raisanen et al. | Jun 2014 | A1 |
20140162401 | Kawano et al. | Jun 2014 | A1 |
20140167187 | Kuo et al. | Jun 2014 | A1 |
20140170335 | Shao et al. | Jun 2014 | A1 |
20140174354 | Arai | Jun 2014 | A1 |
20140174357 | Kim et al. | Jun 2014 | A1 |
20140174927 | Bashir et al. | Jun 2014 | A1 |
20140175054 | Carlson et al. | Jun 2014 | A1 |
20140179091 | Clark | Jun 2014 | A1 |
20140182053 | Huang | Jul 2014 | A1 |
20140182689 | Shareef et al. | Jul 2014 | A1 |
20140187045 | Hua et al. | Jul 2014 | A1 |
20140191389 | Lee et al. | Jul 2014 | A1 |
20140193983 | Lavoie | Jul 2014 | A1 |
20140202382 | Kim et al. | Jul 2014 | A1 |
20140202386 | Taga | Jul 2014 | A1 |
20140202388 | Um et al. | Jul 2014 | A1 |
20140209976 | Yang et al. | Jul 2014 | A1 |
20140213061 | Huang et al. | Jul 2014 | A1 |
20140217065 | Winkler et al. | Aug 2014 | A1 |
20140220247 | Haukka et al. | Aug 2014 | A1 |
20140225065 | Rachmady et al. | Aug 2014 | A1 |
20140227072 | Lee et al. | Aug 2014 | A1 |
20140227444 | Winter et al. | Aug 2014 | A1 |
20140227861 | Wu et al. | Aug 2014 | A1 |
20140227881 | Lubomirsky et al. | Aug 2014 | A1 |
20140231922 | Kim et al. | Aug 2014 | A1 |
20140234466 | Gao et al. | Aug 2014 | A1 |
20140234550 | Winter et al. | Aug 2014 | A1 |
20140234992 | Kubota et al. | Aug 2014 | A1 |
20140238607 | Nozawa et al. | Aug 2014 | A1 |
20140238608 | Sabri et al. | Aug 2014 | A1 |
20140242298 | Lansalot-Matras et al. | Aug 2014 | A1 |
20140242806 | Knapp et al. | Aug 2014 | A1 |
20140245948 | Nguyen et al. | Sep 2014 | A1 |
20140251788 | Ge et al. | Sep 2014 | A1 |
20140251953 | Winkler et al. | Sep 2014 | A1 |
20140251954 | Winkler et al. | Sep 2014 | A1 |
20140252134 | Chen | Sep 2014 | A1 |
20140252479 | Utomo et al. | Sep 2014 | A1 |
20140260684 | Christmann | Sep 2014 | A1 |
20140262028 | Kelekar | Sep 2014 | A1 |
20140262034 | Ishibashi et al. | Sep 2014 | A1 |
20140262193 | Im et al. | Sep 2014 | A1 |
20140263172 | Xie et al. | Sep 2014 | A1 |
20140263272 | Duan et al. | Sep 2014 | A1 |
20140264297 | Kumar et al. | Sep 2014 | A1 |
20140264444 | Guo | Sep 2014 | A1 |
20140264902 | Ting et al. | Sep 2014 | A1 |
20140265090 | Hou | Sep 2014 | A1 |
20140265832 | Kenney et al. | Sep 2014 | A1 |
20140272194 | Xiao et al. | Sep 2014 | A1 |
20140272341 | Duan et al. | Sep 2014 | A1 |
20140273428 | Shero | Sep 2014 | A1 |
20140273477 | Niskanen | Sep 2014 | A1 |
20140273497 | Payne et al. | Sep 2014 | A1 |
20140273510 | Chen et al. | Sep 2014 | A1 |
20140273528 | Niskanen | Sep 2014 | A1 |
20140273530 | Nguyen | Sep 2014 | A1 |
20140273531 | Niskanen | Sep 2014 | A1 |
20140283747 | Kasai et al. | Sep 2014 | A1 |
20140287164 | Xiao et al. | Sep 2014 | A1 |
20140287595 | Shimamoto et al. | Sep 2014 | A1 |
20140290573 | Okabe et al. | Oct 2014 | A1 |
20140290578 | Wamura et al. | Oct 2014 | A1 |
20140308108 | Fosnight et al. | Oct 2014 | A1 |
20140312767 | Tian et al. | Oct 2014 | A1 |
20140322862 | Xie et al. | Oct 2014 | A1 |
20140322885 | Xie et al. | Oct 2014 | A1 |
20140339981 | Komatsu et al. | Nov 2014 | A1 |
20140346142 | Chapuis et al. | Nov 2014 | A1 |
20140346650 | Raisanen et al. | Nov 2014 | A1 |
20140349033 | Nonaka et al. | Nov 2014 | A1 |
20140349068 | Inglis et al. | Nov 2014 | A1 |
20140357090 | Knaepen et al. | Dec 2014 | A1 |
20140363980 | Kawamata et al. | Dec 2014 | A1 |
20140363983 | Nakano et al. | Dec 2014 | A1 |
20140363985 | Jang et al. | Dec 2014 | A1 |
20140366804 | Pak et al. | Dec 2014 | A1 |
20140367043 | Bishara et al. | Dec 2014 | A1 |
20140367642 | Guo | Dec 2014 | A1 |
20140377960 | Koiwa | Dec 2014 | A1 |
20150004316 | Thompson et al. | Jan 2015 | A1 |
20150004317 | Dussarrat et al. | Jan 2015 | A1 |
20150004318 | Alasaarela et al. | Jan 2015 | A1 |
20150004798 | Chandrasekharan et al. | Jan 2015 | A1 |
20150007770 | Chandrasekharan et al. | Jan 2015 | A1 |
20150010381 | Cai | Jan 2015 | A1 |
20150011095 | Chandrasekharan et al. | Jan 2015 | A1 |
20150014632 | Kim et al. | Jan 2015 | A1 |
20150014823 | Mallikarjunan et al. | Jan 2015 | A1 |
20150017794 | Takamure | Jan 2015 | A1 |
20150021599 | Ridgeway | Jan 2015 | A1 |
20150024609 | Milligan et al. | Jan 2015 | A1 |
20150030766 | Lind et al. | Jan 2015 | A1 |
20150031218 | Karakawa | Jan 2015 | A1 |
20150041431 | Zafiropoulo et al. | Feb 2015 | A1 |
20150048485 | Tolle | Feb 2015 | A1 |
20150056815 | Fernandez | Feb 2015 | A1 |
20150056821 | Ishikawa | Feb 2015 | A1 |
20150064923 | Matsumoto et al. | Mar 2015 | A1 |
20150072509 | Chi et al. | Mar 2015 | A1 |
20150078874 | Sansoni | Mar 2015 | A1 |
20150079311 | Nakano | Mar 2015 | A1 |
20150086316 | Greenberg | Mar 2015 | A1 |
20150086716 | Park et al. | Mar 2015 | A1 |
20150087139 | O'Neill et al. | Mar 2015 | A1 |
20150087154 | Guha et al. | Mar 2015 | A1 |
20150091057 | Xie et al. | Apr 2015 | A1 |
20150091134 | Amaratunga et al. | Apr 2015 | A1 |
20150094470 | Sanchez et al. | Apr 2015 | A1 |
20150096973 | Dunn et al. | Apr 2015 | A1 |
20150099065 | Canizares et al. | Apr 2015 | A1 |
20150099072 | Takamure et al. | Apr 2015 | A1 |
20150099123 | Barbee et al. | Apr 2015 | A1 |
20150099342 | Tsai | Apr 2015 | A1 |
20150099374 | Kakimoto et al. | Apr 2015 | A1 |
20150099375 | Haripin et al. | Apr 2015 | A1 |
20150102466 | Colinge | Apr 2015 | A1 |
20150104574 | Lee et al. | Apr 2015 | A1 |
20150110147 | Mizuno | Apr 2015 | A1 |
20150111374 | Bao | Apr 2015 | A1 |
20150111395 | Hashimoto et al. | Apr 2015 | A1 |
20150114295 | Kim et al. | Apr 2015 | A1 |
20150118009 | Hsieh et al. | Apr 2015 | A1 |
20150118846 | Isii et al. | Apr 2015 | A1 |
20150118863 | Rathod et al. | Apr 2015 | A1 |
20150122180 | Chang et al. | May 2015 | A1 |
20150125628 | Kim et al. | May 2015 | A1 |
20150132212 | Winkler et al. | May 2015 | A1 |
20150140210 | Jung et al. | May 2015 | A1 |
20150144060 | Park | May 2015 | A1 |
20150147482 | Kang et al. | May 2015 | A1 |
20150147483 | Fukazawa | May 2015 | A1 |
20150147488 | Choi et al. | May 2015 | A1 |
20150147875 | Takamure et al. | May 2015 | A1 |
20150147877 | Jung | May 2015 | A1 |
20150152547 | Nakamura et al. | Jun 2015 | A1 |
20150152553 | Popp et al. | Jun 2015 | A1 |
20150155177 | Zhang et al. | Jun 2015 | A1 |
20150162168 | Oehrlien | Jun 2015 | A1 |
20150162185 | Pore | Jun 2015 | A1 |
20150162214 | Thompson | Jun 2015 | A1 |
20150167159 | Halpin et al. | Jun 2015 | A1 |
20150167161 | Canizares et al. | Jun 2015 | A1 |
20150167162 | Bank et al. | Jun 2015 | A1 |
20150167165 | Lindfors | Jun 2015 | A1 |
20150167705 | Lee et al. | Jun 2015 | A1 |
20150170914 | Haukka et al. | Jun 2015 | A1 |
20150170945 | Segawa et al. | Jun 2015 | A1 |
20150170947 | Bluck | Jun 2015 | A1 |
20150170954 | Agarwal | Jun 2015 | A1 |
20150170975 | Blatchford et al. | Jun 2015 | A1 |
20150171177 | Cheng et al. | Jun 2015 | A1 |
20150174768 | Rodnick | Jun 2015 | A1 |
20150175467 | Denifl et al. | Jun 2015 | A1 |
20150176126 | Ge et al. | Jun 2015 | A1 |
20150179415 | Sasaki et al. | Jun 2015 | A1 |
20150179501 | Jhaveri et al. | Jun 2015 | A1 |
20150179564 | Lee et al. | Jun 2015 | A1 |
20150179640 | Kim et al. | Jun 2015 | A1 |
20150184287 | Tsung et al. | Jul 2015 | A1 |
20150184291 | Alokozai et al. | Jul 2015 | A1 |
20150187559 | Sano | Jul 2015 | A1 |
20150187568 | Pettinger et al. | Jul 2015 | A1 |
20150187611 | Sato | Jul 2015 | A1 |
20150187908 | Zhang et al. | Jul 2015 | A1 |
20150203961 | Ha et al. | Jul 2015 | A1 |
20150203967 | Dhas et al. | Jul 2015 | A1 |
20150211124 | Nozawa et al. | Jul 2015 | A1 |
20150211125 | Yoshikawa et al. | Jul 2015 | A1 |
20150117456 | Tsuji et al. | Aug 2015 | A1 |
20150217330 | Haukka | Aug 2015 | A1 |
20150217456 | Tsuji et al. | Aug 2015 | A1 |
20150218695 | Odedra | Aug 2015 | A1 |
20150218698 | Yoon et al. | Aug 2015 | A1 |
20150218700 | Nguyen et al. | Aug 2015 | A1 |
20150221479 | Chen et al. | Aug 2015 | A1 |
20150221480 | Duan et al. | Aug 2015 | A1 |
20150221519 | Marks et al. | Aug 2015 | A1 |
20150225850 | Arora et al. | Aug 2015 | A1 |
20150228513 | Parkhe et al. | Aug 2015 | A1 |
20150228572 | Yang et al. | Aug 2015 | A1 |
20150228645 | Chuang et al. | Aug 2015 | A1 |
20150228749 | Ando et al. | Aug 2015 | A1 |
20150240357 | Tachibana et al. | Aug 2015 | A1 |
20150240359 | Jdira et al. | Aug 2015 | A1 |
20150240360 | Leeser | Aug 2015 | A1 |
20150241787 | Yaegashi | Aug 2015 | A1 |
20150243522 | Kitagaito et al. | Aug 2015 | A1 |
20150243542 | Yoshihara et al. | Aug 2015 | A1 |
20150243545 | Tang | Aug 2015 | A1 |
20150243563 | Lee et al. | Aug 2015 | A1 |
20150243658 | Joshi et al. | Aug 2015 | A1 |
20150249013 | Arghavani et al. | Sep 2015 | A1 |
20150255319 | Kikuchi et al. | Sep 2015 | A1 |
20150255324 | Li et al. | Sep 2015 | A1 |
20150255385 | Lee et al. | Sep 2015 | A1 |
20150259790 | Newman | Sep 2015 | A1 |
20150259801 | Matsumoto et al. | Sep 2015 | A1 |
20150262828 | Brand et al. | Sep 2015 | A1 |
20150263033 | Aoyama | Sep 2015 | A1 |
20150267294 | Itatani | Sep 2015 | A1 |
20150267295 | Hill et al. | Sep 2015 | A1 |
20150267297 | Shiba | Sep 2015 | A1 |
20150267298 | Saitou et al. | Sep 2015 | A1 |
20150267299 | Hawkins | Sep 2015 | A1 |
20150267301 | Hill et al. | Sep 2015 | A1 |
20150270140 | Gupta et al. | Sep 2015 | A1 |
20150270146 | Yoshihara et al. | Sep 2015 | A1 |
20150275357 | Kamakura et al. | Oct 2015 | A1 |
20150279665 | Zafiropoulo | Oct 2015 | A1 |
20150279681 | Knoops | Oct 2015 | A1 |
20150279682 | Nakatani et al. | Oct 2015 | A1 |
20150279708 | Kobayashi et al. | Oct 2015 | A1 |
20150279956 | Ozaki et al. | Oct 2015 | A1 |
20150280051 | Xu | Oct 2015 | A1 |
20150284848 | Nakano et al. | Oct 2015 | A1 |
20150287591 | Pore | Oct 2015 | A1 |
20150287612 | Luere et al. | Oct 2015 | A1 |
20150287626 | Arai | Oct 2015 | A1 |
20150287710 | Yun et al. | Oct 2015 | A1 |
20150291830 | Galbreath et al. | Oct 2015 | A1 |
20150292088 | Canizares | Oct 2015 | A1 |
20150299848 | Haukka et al. | Oct 2015 | A1 |
20150307982 | Firouzdor et al. | Oct 2015 | A1 |
20150308586 | Shugrue et al. | Oct 2015 | A1 |
20150311151 | Chi et al. | Oct 2015 | A1 |
20150303056 | Varadarajan et al. | Nov 2015 | A1 |
20150315704 | Nakano et al. | Nov 2015 | A1 |
20150322569 | Kilpi et al. | Nov 2015 | A1 |
20150325432 | Ishizaka | Nov 2015 | A1 |
20150332921 | Lee et al. | Nov 2015 | A1 |
20150340247 | Balakrishnan et al. | Nov 2015 | A1 |
20150340500 | Brunco | Nov 2015 | A1 |
20150340609 | Banno et al. | Nov 2015 | A1 |
20150343559 | Morikazu et al. | Dec 2015 | A1 |
20150343741 | Shibata et al. | Dec 2015 | A1 |
20150345018 | Detavernier et al. | Dec 2015 | A1 |
20150345022 | Yudovsky et al. | Dec 2015 | A1 |
20150348755 | Han et al. | Dec 2015 | A1 |
20150349073 | Kang | Dec 2015 | A1 |
20150353478 | Hoshino et al. | Dec 2015 | A1 |
20150354060 | Yabe et al. | Dec 2015 | A1 |
20150361550 | Yabe et al. | Dec 2015 | A1 |
20150361553 | Murakawa | Dec 2015 | A1 |
20150364347 | Nguyen et al. | Dec 2015 | A1 |
20150364371 | Yen | Dec 2015 | A1 |
20150364747 | Elam et al. | Dec 2015 | A1 |
20150367253 | Kanyal et al. | Dec 2015 | A1 |
20150368798 | Kwong | Dec 2015 | A1 |
20150371864 | Hsu et al. | Dec 2015 | A1 |
20150372056 | Seong et al. | Dec 2015 | A1 |
20150376211 | Girard | Dec 2015 | A1 |
20150376785 | Knaapen et al. | Dec 2015 | A1 |
20150380296 | Antonelli et al. | Dec 2015 | A1 |
20160002776 | Nal et al. | Jan 2016 | A1 |
20160002786 | Gatineau et al. | Jan 2016 | A1 |
20160005571 | Della Rosa et al. | Jan 2016 | A1 |
20160005595 | Liu et al. | Jan 2016 | A1 |
20160005839 | Yieh et al. | Jan 2016 | A1 |
20160013022 | Ayoub | Jan 2016 | A1 |
20160013024 | Milligan et al. | Jan 2016 | A1 |
20160013086 | Yang et al. | Jan 2016 | A1 |
20160017493 | Dhas | Jan 2016 | A1 |
20160020071 | Khaja et al. | Jan 2016 | A1 |
20160020092 | Kang et al. | Jan 2016 | A1 |
20160024655 | Yudovsky et al. | Jan 2016 | A1 |
20160024656 | White et al. | Jan 2016 | A1 |
20160035566 | LaVoie | Feb 2016 | A1 |
20160035596 | Kamiya | Feb 2016 | A1 |
20160042954 | Sung et al. | Feb 2016 | A1 |
20160051964 | Tolle et al. | Feb 2016 | A1 |
20160056074 | Na | Feb 2016 | A1 |
20160056156 | Ghani et al. | Feb 2016 | A1 |
20160060752 | Jacques et al. | Mar 2016 | A1 |
20160064208 | Zafiropoulo et al. | Mar 2016 | A1 |
20160064231 | Agarwal et al. | Mar 2016 | A1 |
20160069613 | Colgan et al. | Mar 2016 | A1 |
20160071750 | de Ridder et al. | Mar 2016 | A1 |
20160076949 | Sabah et al. | Mar 2016 | A1 |
20160079054 | Chen et al. | Mar 2016 | A1 |
20160085003 | Jaiswal | Mar 2016 | A1 |
20160087028 | Hirota et al. | Mar 2016 | A1 |
20160097123 | Shugrue et al. | Apr 2016 | A1 |
20160099150 | Tsai | Apr 2016 | A1 |
20160099166 | Yudovsky | Apr 2016 | A1 |
20160099250 | Rabkin et al. | Apr 2016 | A1 |
20160102214 | Dietz et al. | Apr 2016 | A1 |
20160111272 | Girard | Apr 2016 | A1 |
20160111438 | Tsutsumi et al. | Apr 2016 | A1 |
20160115590 | Haukka et al. | Apr 2016 | A1 |
20160118224 | Kohno et al. | Apr 2016 | A1 |
20160133307 | Lee et al. | May 2016 | A1 |
20160133628 | Xie | May 2016 | A1 |
20160141172 | Kang | May 2016 | A1 |
20160145738 | Liu et al. | May 2016 | A1 |
20160148800 | Henri et al. | May 2016 | A1 |
20160148801 | Yabe et al. | May 2016 | A1 |
20160148806 | Henri et al. | May 2016 | A1 |
20160148811 | Nakatani et al. | May 2016 | A1 |
20160148821 | Singh | May 2016 | A1 |
20160153088 | Tsuji et al. | Jun 2016 | A1 |
20160155629 | Hawryluk et al. | Jun 2016 | A1 |
20160163556 | Briggs et al. | Jun 2016 | A1 |
20160163558 | Hudson et al. | Jun 2016 | A1 |
20160163561 | Hudson et al. | Jun 2016 | A1 |
20160163711 | Arndt et al. | Jun 2016 | A1 |
20160163972 | Swaminathan et al. | Jun 2016 | A1 |
20160168699 | Fukazawa et al. | Jun 2016 | A1 |
20160172189 | Tapily | Jun 2016 | A1 |
20160172296 | Lim et al. | Jun 2016 | A1 |
20160175805 | Catchpole et al. | Jun 2016 | A1 |
20160177448 | Ikeda | Jun 2016 | A1 |
20160181117 | Arghavani et al. | Jun 2016 | A1 |
20160181128 | Mori | Jun 2016 | A1 |
20160181368 | Weeks | Jun 2016 | A1 |
20160190137 | Tsai et al. | Jun 2016 | A1 |
20160195331 | Hyon et al. | Jul 2016 | A1 |
20160196969 | Berry et al. | Jul 2016 | A1 |
20160196970 | Takamure et al. | Jul 2016 | A1 |
20160203995 | Kanarik et al. | Jul 2016 | A1 |
20160211135 | Noda et al. | Jul 2016 | A1 |
20160211147 | Fukazawa | Jul 2016 | A1 |
20160217857 | Paudel | Jul 2016 | A1 |
20160218028 | Schaller et al. | Jul 2016 | A1 |
20160222504 | Haukka et al. | Aug 2016 | A1 |
20160222509 | Honma | Aug 2016 | A1 |
20160222516 | Ikeda et al. | Aug 2016 | A1 |
20160225607 | Yamamoto et al. | Aug 2016 | A1 |
20160225632 | Shaikh et al. | Aug 2016 | A1 |
20160245704 | Osaka et al. | Aug 2016 | A1 |
20160256187 | Shelton et al. | Sep 2016 | A1 |
20160268102 | White | Sep 2016 | A1 |
20160268107 | White | Sep 2016 | A1 |
20160273101 | Komori et al. | Sep 2016 | A1 |
20160273106 | Kanjolia et al. | Sep 2016 | A1 |
20160276148 | Qian et al. | Sep 2016 | A1 |
20160276212 | Horikoshi | Sep 2016 | A1 |
20160281223 | Sowa et al. | Sep 2016 | A1 |
20160281230 | Varadarajan et al. | Sep 2016 | A1 |
20160284517 | Saido | Sep 2016 | A1 |
20160284542 | Noda et al. | Sep 2016 | A1 |
20160289828 | Shero et al. | Oct 2016 | A1 |
20160293398 | Danek et al. | Oct 2016 | A1 |
20160305015 | Nakamura et al. | Oct 2016 | A1 |
20160307739 | Lee et al. | Oct 2016 | A1 |
20160307766 | Jongbloed et al. | Oct 2016 | A1 |
20160312360 | Rasheed et al. | Oct 2016 | A1 |
20160314962 | Higashino et al. | Oct 2016 | A1 |
20160314964 | Tang et al. | Oct 2016 | A1 |
20160314967 | Tolle | Oct 2016 | A1 |
20160315168 | Dussarrat et al. | Oct 2016 | A1 |
20160334709 | Huli et al. | Nov 2016 | A1 |
20160336178 | Swaminathan et al. | Nov 2016 | A1 |
20160336392 | Tominaga et al. | Nov 2016 | A1 |
20160345384 | Zhang et al. | Nov 2016 | A1 |
20160351413 | Schmidt et al. | Dec 2016 | A1 |
20160351747 | Forrest et al. | Dec 2016 | A1 |
20160358772 | Xie | Dec 2016 | A1 |
20160362783 | Tolle et al. | Dec 2016 | A1 |
20160362813 | Bao et al. | Dec 2016 | A1 |
20160365280 | Brink et al. | Dec 2016 | A1 |
20160365414 | Peng et al. | Dec 2016 | A1 |
20160372321 | Krishnan et al. | Dec 2016 | A1 |
20160372365 | Tang et al. | Dec 2016 | A1 |
20160372744 | Essaki et al. | Dec 2016 | A1 |
20160376700 | Haukka | Dec 2016 | A1 |
20160376704 | Raisanen | Dec 2016 | A1 |
20160379826 | Arghavani et al. | Dec 2016 | A9 |
20160379851 | Swaminathan et al. | Dec 2016 | A1 |
20160381732 | Moench et al. | Dec 2016 | A1 |
20170009347 | Jang et al. | Jan 2017 | A1 |
20170009367 | Harris et al. | Jan 2017 | A1 |
20170011889 | Winkler et al. | Jan 2017 | A1 |
20170011926 | Harada et al. | Jan 2017 | A1 |
20170011950 | Schmotzer | Jan 2017 | A1 |
20170018477 | Kato | Jan 2017 | A1 |
20170018570 | Lue et al. | Jan 2017 | A1 |
20170025280 | Milligan | Jan 2017 | A1 |
20170025291 | Lin | Jan 2017 | A1 |
20170029945 | Kamakura | Feb 2017 | A1 |
20170032942 | Walfried | Feb 2017 | A1 |
20170032943 | Spaulding et al. | Feb 2017 | A1 |
20170032992 | Hoechbauer | Feb 2017 | A1 |
20170033004 | Siew et al. | Feb 2017 | A1 |
20170037513 | Haukka | Feb 2017 | A1 |
20170040164 | Wang et al. | Feb 2017 | A1 |
20170040206 | Schmotzer et al. | Feb 2017 | A1 |
20170044664 | Dussarrat et al. | Feb 2017 | A1 |
20170044665 | Shon et al. | Feb 2017 | A1 |
20170044666 | Jang et al. | Feb 2017 | A1 |
20170047446 | Margetis et al. | Feb 2017 | A1 |
20170051402 | Mori | Feb 2017 | A1 |
20170051405 | Fukazawa et al. | Feb 2017 | A1 |
20170051406 | Mori et al. | Feb 2017 | A1 |
20170051408 | Kosuke et al. | Feb 2017 | A1 |
20170053811 | Fung et al. | Feb 2017 | A1 |
20170058402 | Wenxu et al. | Mar 2017 | A1 |
20170062204 | Suzuki et al. | Mar 2017 | A1 |
20170062209 | Shiba | Mar 2017 | A1 |
20170062210 | Visser et al. | Mar 2017 | A1 |
20170062218 | Duan et al. | Mar 2017 | A1 |
20170062224 | Fu et al. | Mar 2017 | A1 |
20170062258 | Bluck | Mar 2017 | A1 |
20170069725 | Bhimarasetti et al. | Mar 2017 | A1 |
20170091320 | Psota et al. | Mar 2017 | A1 |
20170092469 | Kurita et al. | Mar 2017 | A1 |
20170092531 | Coomer | Mar 2017 | A1 |
20170092535 | Kimihiko et al. | Mar 2017 | A1 |
20170092847 | Kim et al. | Mar 2017 | A1 |
20170100742 | Pore et al. | Apr 2017 | A1 |
20170103907 | Chu et al. | Apr 2017 | A1 |
20170104061 | Peng et al. | Apr 2017 | A1 |
20170107621 | Suemori | Apr 2017 | A1 |
20170110313 | Tang et al. | Apr 2017 | A1 |
20170110601 | Blomberg et al. | Apr 2017 | A1 |
20170114460 | Kim et al. | Apr 2017 | A1 |
20170114464 | Iriuda | Apr 2017 | A1 |
20170114465 | Kalutarage et al. | Apr 2017 | A1 |
20170117141 | Zhu et al. | Apr 2017 | A1 |
20170117202 | Tang et al. | Apr 2017 | A1 |
20170117203 | Tang et al. | Apr 2017 | A1 |
20170117222 | Kim et al. | Apr 2017 | A1 |
20170121845 | Grutzmacher et al. | May 2017 | A1 |
20170130332 | Stumpf | May 2017 | A1 |
20170136578 | Yoshimura | May 2017 | A1 |
20170140925 | Suzuki et al. | May 2017 | A1 |
20170145564 | Bertuch et al. | May 2017 | A1 |
20170146909 | Smith et al. | May 2017 | A1 |
20170148918 | Ye et al. | May 2017 | A1 |
20170152968 | Raj et al. | Jun 2017 | A1 |
20170154757 | Winkler et al. | Jun 2017 | A1 |
20170154770 | Margetis et al. | Jun 2017 | A1 |
20170154895 | Huo | Jun 2017 | A1 |
20170159177 | Monsma et al. | Jun 2017 | A1 |
20170165624 | Ravoin et al. | Jun 2017 | A1 |
20170170033 | Okabe et al. | Jun 2017 | A1 |
20170173696 | Sheinman | Jun 2017 | A1 |
20170175290 | Chen et al. | Jun 2017 | A1 |
20170178899 | Kabansky et al. | Jun 2017 | A1 |
20170179036 | Chen et al. | Jun 2017 | A1 |
20170186621 | Zaitsu | Jun 2017 | A1 |
20170186754 | Blomberg et al. | Jun 2017 | A1 |
20170191159 | Polyak et al. | Jul 2017 | A1 |
20170191164 | Alokozai et al. | Jul 2017 | A1 |
20170191861 | Rondano et al. | Jul 2017 | A1 |
20170196562 | Shelton | Jul 2017 | A1 |
20170200622 | Shiokawa et al. | Jul 2017 | A1 |
20170204516 | Nguyen et al. | Jul 2017 | A1 |
20170216762 | Shugrue et al. | Aug 2017 | A1 |
20170226636 | Xiao | Aug 2017 | A1 |
20170232457 | Toshiki et al. | Aug 2017 | A1 |
20170233868 | Donoso et al. | Aug 2017 | A1 |
20170243734 | Ishikawa et al. | Aug 2017 | A1 |
20170250068 | Ishikawa | Aug 2017 | A1 |
20170250075 | Caymax et al. | Aug 2017 | A1 |
20170256417 | Chou | Sep 2017 | A1 |
20170256429 | Lawson et al. | Sep 2017 | A1 |
20170260649 | Coomer | Sep 2017 | A1 |
20170263437 | Li et al. | Sep 2017 | A1 |
20170267527 | Kim et al. | Sep 2017 | A1 |
20170267531 | Huakka | Sep 2017 | A1 |
20170271191 | Yoo et al. | Sep 2017 | A1 |
20170271256 | Inatsuka | Sep 2017 | A1 |
20170271501 | Avci et al. | Sep 2017 | A1 |
20170278705 | Murakami et al. | Sep 2017 | A1 |
20170278707 | Margetis et al. | Sep 2017 | A1 |
20170287681 | Nitadori et al. | Oct 2017 | A1 |
20170287744 | Kobayashi et al. | Oct 2017 | A1 |
20170294318 | Yoshida et al. | Oct 2017 | A1 |
20170294339 | Tapily | Oct 2017 | A1 |
20170294499 | Lu et al. | Oct 2017 | A1 |
20170301519 | Naim et al. | Oct 2017 | A1 |
20170301542 | Maes et al. | Oct 2017 | A1 |
20170303382 | Smith et al. | Oct 2017 | A1 |
20170306478 | Raisanen et al. | Oct 2017 | A1 |
20170306479 | Raisanen et al. | Oct 2017 | A1 |
20170306480 | Zhu et al. | Oct 2017 | A1 |
20170309490 | Ogawa | Oct 2017 | A1 |
20170309528 | Bansal et al. | Oct 2017 | A1 |
20170316933 | Xie et al. | Nov 2017 | A1 |
20170316940 | Ishikawa | Nov 2017 | A1 |
20170317194 | Tang et al. | Nov 2017 | A1 |
20170323783 | Sanchez et al. | Nov 2017 | A1 |
20170323784 | Faguet et al. | Nov 2017 | A1 |
20170338111 | Takamure et al. | Nov 2017 | A1 |
20170338133 | Tan et al. | Nov 2017 | A1 |
20170338134 | Tan et al. | Nov 2017 | A1 |
20170338192 | Lee et al. | Nov 2017 | A1 |
20170342559 | Fukazawa et al. | Nov 2017 | A1 |
20170343896 | Darling et al. | Nov 2017 | A1 |
20170345674 | Ranjan et al. | Nov 2017 | A1 |
20170350688 | Boyd et al. | Dec 2017 | A1 |
20170358445 | O'Shaughnessy et al. | Dec 2017 | A1 |
20170358482 | Chen et al. | Dec 2017 | A1 |
20170358670 | Kub et al. | Dec 2017 | A1 |
20170362710 | Ge et al. | Dec 2017 | A1 |
20170365467 | Shimamoto et al. | Dec 2017 | A1 |
20170372884 | Margetis et al. | Dec 2017 | A1 |
20170372919 | Manna et al. | Dec 2017 | A1 |
20170373188 | Mochizuki et al. | Dec 2017 | A1 |
20180005814 | Kumar et al. | Jan 2018 | A1 |
20180010243 | Lee et al. | Jan 2018 | A1 |
20180010247 | Niskanen | Jan 2018 | A1 |
20180011052 | Andersson et al. | Jan 2018 | A1 |
20180012792 | Zhu | Jan 2018 | A1 |
20180019165 | Baum et al. | Jan 2018 | A1 |
20180025890 | Choi et al. | Jan 2018 | A1 |
20180025907 | Kalutarage et al. | Jan 2018 | A1 |
20180025939 | Kovalgin et al. | Jan 2018 | A1 |
20180033614 | Chandra et al. | Feb 2018 | A1 |
20180033616 | Masaru | Feb 2018 | A1 |
20180033625 | Yoo | Feb 2018 | A1 |
20180033645 | Saido et al. | Feb 2018 | A1 |
20180033674 | Jeong | Feb 2018 | A1 |
20180033679 | Pore | Feb 2018 | A1 |
20180040746 | Johnson et al. | Feb 2018 | A1 |
20180044800 | Hendrix et al. | Feb 2018 | A1 |
20180047591 | Ogo | Feb 2018 | A1 |
20180047749 | Kim | Feb 2018 | A1 |
20180053660 | Jandl et al. | Feb 2018 | A1 |
20180053769 | Kim et al. | Feb 2018 | A1 |
20180057931 | Cha et al. | Mar 2018 | A1 |
20180057934 | Cooper et al. | Mar 2018 | A1 |
20180057937 | Lee et al. | Mar 2018 | A1 |
20180061628 | Ou et al. | Mar 2018 | A1 |
20180061851 | Ootsuka | Mar 2018 | A1 |
20180068844 | Chen et al. | Mar 2018 | A1 |
20180068862 | Terakura et al. | Mar 2018 | A1 |
20180068950 | Bruley et al. | Mar 2018 | A1 |
20180069019 | Kim et al. | Mar 2018 | A1 |
20180076021 | Fukushima et al. | Mar 2018 | A1 |
20180083435 | Redler | Mar 2018 | A1 |
20180087152 | Yoshida | Mar 2018 | A1 |
20180087154 | Pore et al. | Mar 2018 | A1 |
20180087156 | Kohei et al. | Mar 2018 | A1 |
20180090583 | Choi et al. | Mar 2018 | A1 |
20180094351 | Verghese et al. | Apr 2018 | A1 |
20180097076 | Cheng et al. | Apr 2018 | A1 |
20180102276 | Zhu et al. | Apr 2018 | A1 |
20180105930 | Kang et al. | Apr 2018 | A1 |
20180108587 | Jiang | Apr 2018 | A1 |
20180114680 | Kim et al. | Apr 2018 | A1 |
20180119283 | Fukazawa | May 2018 | A1 |
20180122642 | Raisanen | May 2018 | A1 |
20180122709 | Xie | May 2018 | A1 |
20180122959 | Calka et al. | May 2018 | A1 |
20180126379 | Ramsey et al. | May 2018 | A1 |
20180127876 | Tolle et al. | May 2018 | A1 |
20180130652 | Pettinger et al. | May 2018 | A1 |
20180130701 | Chun | May 2018 | A1 |
20180135172 | Nogami et al. | May 2018 | A1 |
20180135173 | Kim et al. | May 2018 | A1 |
20180135179 | Toshiyuki et al. | May 2018 | A1 |
20180138036 | Baldesseroni et al. | May 2018 | A1 |
20180142353 | Tetsuya et al. | May 2018 | A1 |
20180142357 | Yoshikazu | May 2018 | A1 |
20180148832 | Chatterjee et al. | May 2018 | A1 |
20180151346 | Blanquart | May 2018 | A1 |
20180151358 | Margetis et al. | May 2018 | A1 |
20180151588 | Tsutsumi et al. | May 2018 | A1 |
20180155832 | Hamalainen et al. | Jun 2018 | A1 |
20180155836 | Arai et al. | Jun 2018 | A1 |
20180158688 | Chen | Jun 2018 | A1 |
20180158716 | Konkola et al. | Jun 2018 | A1 |
20180163305 | Batzer et al. | Jun 2018 | A1 |
20180166258 | Kim et al. | Jun 2018 | A1 |
20180166315 | Coomer | Jun 2018 | A1 |
20180171475 | Maes et al. | Jun 2018 | A1 |
20180171477 | Kim et al. | Jun 2018 | A1 |
20180172172 | Oehler et al. | Jun 2018 | A1 |
20180173109 | Gronheid et al. | Jun 2018 | A1 |
20180174801 | Chen et al. | Jun 2018 | A1 |
20180174826 | Raaijmakers et al. | Jun 2018 | A1 |
20180179625 | Takagi et al. | Jun 2018 | A1 |
20180180509 | Sawachi et al. | Jun 2018 | A1 |
20180182613 | Blanquart et al. | Jun 2018 | A1 |
20180182618 | Blanquart et al. | Jun 2018 | A1 |
20180187303 | Gatineau et al. | Jul 2018 | A1 |
20180189923 | Zhong et al. | Jul 2018 | A1 |
20180190496 | Ashihara et al. | Jul 2018 | A1 |
20180195174 | Kim et al. | Jul 2018 | A1 |
20180204733 | Sherpa et al. | Jul 2018 | A1 |
20180211834 | Takamure et al. | Jul 2018 | A1 |
20180223047 | Xiao et al. | Aug 2018 | A1 |
20180223429 | Fukazawa et al. | Aug 2018 | A1 |
20180230595 | Suda et al. | Aug 2018 | A1 |
20180233372 | Vayrynen et al. | Aug 2018 | A1 |
20180245215 | Lei et al. | Aug 2018 | A1 |
20180246101 | Sasisekharan et al. | Aug 2018 | A1 |
20180254211 | Kosakai et al. | Sep 2018 | A1 |
20180258532 | Kato et al. | Sep 2018 | A1 |
20180269057 | Lei et al. | Sep 2018 | A1 |
20180277338 | Fukada et al. | Sep 2018 | A1 |
20180277423 | Lottes | Sep 2018 | A1 |
20180286638 | Susa | Oct 2018 | A1 |
20180286663 | Kobayashi et al. | Oct 2018 | A1 |
20180286668 | Baum et al. | Oct 2018 | A1 |
20180286672 | Van Aerde et al. | Oct 2018 | A1 |
20180286675 | Blomberg et al. | Oct 2018 | A1 |
20180286711 | Oosterlaken et al. | Oct 2018 | A1 |
20180294187 | Thombare et al. | Oct 2018 | A1 |
20180305247 | Feng et al. | Oct 2018 | A1 |
20180308686 | Xie et al. | Oct 2018 | A1 |
20180308701 | Na et al. | Oct 2018 | A1 |
20180312966 | Chan et al. | Nov 2018 | A1 |
20180315838 | Morrow et al. | Nov 2018 | A1 |
20180323055 | Woodruff et al. | Nov 2018 | A1 |
20180323056 | Woodruff et al. | Nov 2018 | A1 |
20180323059 | Bhargava et al. | Nov 2018 | A1 |
20180325414 | Marashdeh et al. | Nov 2018 | A1 |
20180331117 | Titus et al. | Nov 2018 | A1 |
20180337087 | Sandhu et al. | Nov 2018 | A1 |
20180350587 | Jia et al. | Dec 2018 | A1 |
20180350588 | Raisanen et al. | Dec 2018 | A1 |
20180350620 | Zaitsu et al. | Dec 2018 | A1 |
20180350653 | Jeong et al. | Dec 2018 | A1 |
20180355480 | Kondo | Dec 2018 | A1 |
20180355484 | Lansalot-Matras et al. | Dec 2018 | A1 |
20180358222 | Venkatasubramanian et al. | Dec 2018 | A1 |
20180363131 | Lee et al. | Dec 2018 | A1 |
20180363139 | Rajavelu et al. | Dec 2018 | A1 |
20180366314 | Niskanen et al. | Dec 2018 | A1 |
20180371610 | Banerjee et al. | Dec 2018 | A1 |
20190003050 | Dezelah et al. | Jan 2019 | A1 |
20190003052 | Shero et al. | Jan 2019 | A1 |
20190006797 | Paynter et al. | Jan 2019 | A1 |
20190013199 | Bhargava et al. | Jan 2019 | A1 |
20190019670 | Lin et al. | Jan 2019 | A1 |
20190027573 | Zhu et al. | Jan 2019 | A1 |
20190027583 | Margetis et al. | Jan 2019 | A1 |
20190027584 | Margetis et al. | Jan 2019 | A1 |
20190027605 | Tolle et al. | Jan 2019 | A1 |
20190032209 | Huggare | Jan 2019 | A1 |
20190032998 | Jdira et al. | Jan 2019 | A1 |
20190035605 | Suzuki | Jan 2019 | A1 |
20190035647 | Lee et al. | Jan 2019 | A1 |
20190035810 | Chun et al. | Jan 2019 | A1 |
20190040529 | Verbaas et al. | Feb 2019 | A1 |
20190046947 | Strohm et al. | Feb 2019 | A1 |
20190051544 | Verbaas | Feb 2019 | A1 |
20190051548 | den Hartog Besselink et al. | Feb 2019 | A1 |
20190051555 | Hill et al. | Feb 2019 | A1 |
20190057857 | Ishikawa | Feb 2019 | A1 |
20190057858 | Hausmann et al. | Feb 2019 | A1 |
20190058043 | Dewey et al. | Feb 2019 | A1 |
20190062907 | Kim et al. | Feb 2019 | A1 |
20190062917 | Sung et al. | Feb 2019 | A1 |
20190066978 | Um et al. | Feb 2019 | A1 |
20190066997 | Klaver et al. | Feb 2019 | A1 |
20190067003 | Zope et al. | Feb 2019 | A1 |
20190067004 | Kohen et al. | Feb 2019 | A1 |
20190067014 | Shrestha et al. | Feb 2019 | A1 |
20190067016 | Zhu et al. | Feb 2019 | A1 |
20190067085 | Kweskin | Feb 2019 | A1 |
20190067094 | Zope et al. | Feb 2019 | A1 |
20190067095 | Zhu et al. | Feb 2019 | A1 |
20190080903 | Abel et al. | Mar 2019 | A1 |
20190081072 | Chun et al. | Mar 2019 | A1 |
20190085451 | Lei et al. | Mar 2019 | A1 |
20190086807 | Kachel et al. | Mar 2019 | A1 |
20190088555 | Xie et al. | Mar 2019 | A1 |
20190089143 | Malone et al. | Mar 2019 | A1 |
20190093221 | Jdira et al. | Mar 2019 | A1 |
20190096708 | Sharma | Mar 2019 | A1 |
20190106788 | Hawkins et al. | Apr 2019 | A1 |
20190109002 | Mattinen et al. | Apr 2019 | A1 |
20190109009 | Longrie et al. | Apr 2019 | A1 |
20190112711 | Lyons et al. | Apr 2019 | A1 |
20190115206 | Kim et al. | Apr 2019 | A1 |
20190115237 | den Hartog Besselink et al. | Apr 2019 | A1 |
20190131124 | Kohen et al. | May 2019 | A1 |
20190140067 | Zhu et al. | May 2019 | A1 |
20190148224 | Kuroda et al. | May 2019 | A1 |
20190148398 | Kim | May 2019 | A1 |
20190153593 | Zhu et al. | May 2019 | A1 |
20190157054 | White et al. | May 2019 | A1 |
20190157067 | Bhuyan et al. | May 2019 | A1 |
20190163056 | Maes et al. | May 2019 | A1 |
20190164763 | Raisanen et al. | May 2019 | A1 |
20190181002 | Iijima et al. | Jun 2019 | A1 |
20190185999 | Shanbhag et al. | Jun 2019 | A1 |
20190189447 | Kamp et al. | Jun 2019 | A1 |
20190198359 | Kamimura et al. | Jun 2019 | A1 |
20190198571 | Xu et al. | Jun 2019 | A1 |
20190204029 | Tanabe | Jul 2019 | A1 |
20190217277 | Jeon et al. | Jul 2019 | A1 |
20190221433 | Raisanen et al. | Jul 2019 | A1 |
20190229008 | Rokkam et al. | Jul 2019 | A1 |
20190233940 | Guo et al. | Aug 2019 | A1 |
20190237325 | Wang et al. | Aug 2019 | A1 |
20190237327 | Kohen et al. | Aug 2019 | A1 |
20190244803 | Suzuki | Aug 2019 | A1 |
20190249300 | Hatanpaa et al. | Aug 2019 | A1 |
20190249303 | Kuroda et al. | Aug 2019 | A1 |
20190252195 | Haukka | Aug 2019 | A1 |
20190252196 | Vayrynen et al. | Aug 2019 | A1 |
20190259611 | Nakano et al. | Aug 2019 | A1 |
20190259612 | Nozawa et al. | Aug 2019 | A1 |
20190264324 | Shugrue et al. | Aug 2019 | A1 |
20190271078 | Raisanen et al. | Sep 2019 | A1 |
20190272981 | Xu et al. | Sep 2019 | A1 |
20190272993 | Mattinen et al. | Sep 2019 | A1 |
20190273133 | Agrawal et al. | Sep 2019 | A1 |
20190276934 | Verghese et al. | Sep 2019 | A1 |
20190287769 | Blomberg et al. | Sep 2019 | A1 |
20190295837 | Pore et al. | Sep 2019 | A1 |
20190301014 | Pierreux et al. | Oct 2019 | A1 |
20190304776 | Choi | Oct 2019 | A1 |
20190304780 | Kohen et al. | Oct 2019 | A1 |
20190304790 | Mousa et al. | Oct 2019 | A1 |
20190304821 | Pierreux et al. | Oct 2019 | A1 |
20190311894 | Girard et al. | Oct 2019 | A1 |
20190311897 | Kang et al. | Oct 2019 | A1 |
20190311940 | Choi et al. | Oct 2019 | A1 |
20190318923 | Blanquart et al. | Oct 2019 | A1 |
20190322812 | Wojtecki et al. | Oct 2019 | A1 |
20190330740 | Klaver | Oct 2019 | A1 |
20190333753 | Ueda et al. | Oct 2019 | A1 |
20190333761 | Tois et al. | Oct 2019 | A1 |
20190338418 | Goradia et al. | Nov 2019 | A1 |
20190346300 | Kim et al. | Nov 2019 | A1 |
20190348261 | Lin et al. | Nov 2019 | A1 |
20190348273 | Tang et al. | Nov 2019 | A1 |
20190348515 | Li et al. | Nov 2019 | A1 |
20190363006 | Min | Nov 2019 | A1 |
20190368040 | Kachel et al. | Dec 2019 | A1 |
20190368041 | Sreeram et al. | Dec 2019 | A1 |
20190371594 | Niskanen et al. | Dec 2019 | A1 |
20190371640 | Raisanen et al. | Dec 2019 | A1 |
20190375638 | Haukka | Dec 2019 | A1 |
20190376180 | Niskanen | Dec 2019 | A1 |
20190378916 | Tang et al. | Dec 2019 | A1 |
20190385907 | Gottheim et al. | Dec 2019 | A1 |
20190390338 | Raisanen et al. | Dec 2019 | A1 |
20190390343 | Min et al. | Dec 2019 | A1 |
20190393308 | Lo et al. | Dec 2019 | A1 |
20200002811 | Sreeram et al. | Jan 2020 | A1 |
20200002812 | Lee et al. | Jan 2020 | A1 |
20200013612 | Blanquart et al. | Jan 2020 | A1 |
20200013613 | Blanquart | Jan 2020 | A1 |
20200013626 | Longrie et al. | Jan 2020 | A1 |
20200013629 | de Roest et al. | Jan 2020 | A1 |
20200018421 | Shugrue | Jan 2020 | A1 |
20200040458 | Ma et al. | Feb 2020 | A1 |
20200048768 | Wiegers et al. | Feb 2020 | A1 |
20200052056 | Park et al. | Feb 2020 | A1 |
20200056282 | Raisanen et al. | Feb 2020 | A1 |
20200056286 | Shero et al. | Feb 2020 | A1 |
20200063262 | Katou et al. | Feb 2020 | A1 |
20200064737 | de Roest | Feb 2020 | A1 |
20200066552 | Susa | Feb 2020 | A1 |
20200080200 | Um et al. | Mar 2020 | A1 |
20200083054 | Väyrynen et al. | Mar 2020 | A1 |
20200083375 | Tolle et al. | Mar 2020 | A1 |
20200083469 | Lhullier | Mar 2020 | A1 |
20200102649 | Reed | Apr 2020 | A1 |
20200102653 | Muralidhar et al. | Apr 2020 | A1 |
20200105579 | Zhu | Apr 2020 | A1 |
20200105594 | Cheng et al. | Apr 2020 | A1 |
20200109472 | Um et al. | Apr 2020 | A1 |
20200111669 | Zaitsu et al. | Apr 2020 | A1 |
20200111690 | Oosterlaken | Apr 2020 | A1 |
20200118811 | Utsuno et al. | Apr 2020 | A1 |
20200118815 | Fukazawa et al. | Apr 2020 | A1 |
20200118817 | Blomberg et al. | Apr 2020 | A1 |
20200126771 | Roh et al. | Apr 2020 | A1 |
20200126840 | Roh et al. | Apr 2020 | A1 |
20200131634 | Gao et al. | Apr 2020 | A1 |
20200135512 | Oosterlaken et al. | Apr 2020 | A1 |
20200140995 | Blanquart et al. | May 2020 | A1 |
20200141003 | Lee et al. | May 2020 | A1 |
20200144058 | Kohen | May 2020 | A1 |
20200152473 | Tapily et al. | May 2020 | A1 |
20200152750 | Morrow et al. | May 2020 | A1 |
20200161129 | Mattinen et al. | May 2020 | A1 |
20200161438 | Tang et al. | May 2020 | A1 |
20200168485 | Fluit | May 2020 | A1 |
20200279758 | Sharma | May 2020 | A1 |
20200173020 | Huggare | Jun 2020 | A1 |
20200176244 | Lee et al. | Jun 2020 | A1 |
20200176246 | Huotari et al. | Jun 2020 | A1 |
20200181770 | Longrie et al. | Jun 2020 | A1 |
20200194253 | Banerjee et al. | Jun 2020 | A1 |
20200194268 | Sharma | Jun 2020 | A1 |
20200224309 | Sreeram et al. | Jul 2020 | A1 |
20200224311 | Niskanen et al. | Jul 2020 | A1 |
20200227243 | Kim et al. | Jul 2020 | A1 |
20200227250 | Pore et al. | Jul 2020 | A1 |
20200227325 | Xie et al. | Jul 2020 | A1 |
20200232096 | Hatanpää et al. | Jul 2020 | A1 |
20200234989 | Jeong | Jul 2020 | A1 |
20200251328 | Zaitsu et al. | Aug 2020 | A1 |
20200258766 | Garssen et al. | Aug 2020 | A1 |
20200266057 | Lee et al. | Aug 2020 | A1 |
20200266097 | Liu et al. | Aug 2020 | A1 |
20200266098 | Pore et al. | Aug 2020 | A1 |
20200266208 | Kim et al. | Aug 2020 | A1 |
20200270749 | Li et al. | Aug 2020 | A1 |
20200270752 | Pierreux et al. | Aug 2020 | A1 |
20200273729 | Verbaas et al. | Aug 2020 | A1 |
20200279721 | White et al. | Sep 2020 | A1 |
20200283893 | Byun et al. | Sep 2020 | A1 |
20200284467 | Lindeboom et al. | Sep 2020 | A1 |
20200286725 | Sharma et al. | Sep 2020 | A1 |
20200286726 | Shero et al. | Sep 2020 | A1 |
20200294789 | Woodruff et al. | Sep 2020 | A1 |
20200303180 | Kim et al. | Sep 2020 | A1 |
20200303196 | Chen et al. | Sep 2020 | A1 |
20200309455 | Fluit | Oct 2020 | A1 |
20200312652 | Kang et al. | Oct 2020 | A1 |
20200318237 | Fukazawa | Oct 2020 | A1 |
20200321209 | Ishikawa et al. | Oct 2020 | A1 |
20200332416 | Fluit | Oct 2020 | A1 |
20200340113 | Hatanpää et al. | Oct 2020 | A1 |
20200340138 | Tolle et al. | Oct 2020 | A1 |
20200343134 | Kovalgin et al. | Oct 2020 | A1 |
20200343358 | Zhu et al. | Oct 2020 | A1 |
20200350193 | Garssen | Nov 2020 | A1 |
20200354836 | Yednak et al. | Nov 2020 | A1 |
20200355296 | Shugrue et al. | Nov 2020 | A1 |
20200357631 | Ueda | Nov 2020 | A1 |
20200365391 | Blanquart et al. | Nov 2020 | A1 |
20200365433 | de Ridder et al. | Nov 2020 | A1 |
20200365434 | de Ridder | Nov 2020 | A1 |
20200365444 | Hill et al. | Nov 2020 | A1 |
20200373152 | Blanquart | Nov 2020 | A1 |
20200385861 | Deye et al. | Dec 2020 | A1 |
20200385867 | Kim et al. | Dec 2020 | A1 |
20200385868 | Kim et al. | Dec 2020 | A1 |
20200395209 | Yoshimoto et al. | Dec 2020 | A1 |
20200395444 | Lo et al. | Dec 2020 | A1 |
20210002762 | Jun et al. | Jan 2021 | A1 |
20210005449 | Blanquart et al. | Jan 2021 | A1 |
20210005450 | Mattinen et al. | Jan 2021 | A1 |
20210005723 | Tang et al. | Jan 2021 | A1 |
20210013010 | Yoshikawa et al. | Jan 2021 | A1 |
20210013037 | Sun et al. | Jan 2021 | A1 |
20210013042 | Väyrynen et al. | Jan 2021 | A1 |
20210013085 | Roh et al. | Jan 2021 | A1 |
20210020429 | Khazaka et al. | Jan 2021 | A1 |
20210020431 | Blanquart et al. | Jan 2021 | A1 |
20210020432 | Blanquart | Jan 2021 | A1 |
20210020467 | Sekiguchi | Jan 2021 | A1 |
20210020470 | Lee | Jan 2021 | A1 |
20210028021 | Mousa et al. | Jan 2021 | A1 |
20210017648 | Kubota et al. | Feb 2021 | A1 |
20210035785 | Jeong et al. | Feb 2021 | A1 |
20210035786 | Jeong et al. | Feb 2021 | A1 |
20210035802 | Tolle et al. | Feb 2021 | A1 |
20210035824 | de Ridder | Feb 2021 | A1 |
20210035839 | de Ridder | Feb 2021 | A1 |
20210035840 | de Ridder et al. | Feb 2021 | A1 |
20210035841 | Fluit | Feb 2021 | A1 |
20210035842 | de Ridder | Feb 2021 | A1 |
20210035854 | Yoo et al. | Feb 2021 | A1 |
20210040613 | White et al. | Feb 2021 | A1 |
20210040615 | White et al. | Feb 2021 | A1 |
20210041284 | Yednak | Feb 2021 | A1 |
20210043444 | Blanquart | Feb 2021 | A1 |
20210050231 | Oosterlaken | Feb 2021 | A1 |
Number | Date | Country |
---|---|---|
520629 | Jun 2019 | AT |
1186873 | Jul 1998 | CN |
2588350 | Nov 2003 | CN |
1563483 | Jan 2005 | CN |
1655362 | Aug 2005 | CN |
1664987 | Sep 2005 | CN |
1825535 | Aug 2006 | CN |
101142012 | Mar 2008 | CN |
101330015 | Dec 2008 | CN |
101522943 | Sep 2009 | CN |
101609858 | Dec 2009 | CN |
101681873 | Mar 2010 | CN |
101423937 | Sep 2011 | CN |
102383106 | Mar 2012 | CN |
103014846 | Apr 2013 | CN |
103515222 | Jan 2014 | CN |
102373440 | Jul 2014 | CN |
104244620 | Dec 2014 | CN |
105253917 | Jan 2016 | CN |
104201108 | Nov 2017 | CN |
108389798 | Aug 2018 | CN |
8902307 | Aug 1989 | DE |
3836696 | Dec 1989 | DE |
3626724 | Jun 1994 | DE |
10133013 | Jan 2003 | DE |
102008052750 | Jun 2009 | DE |
0058571 | Aug 1982 | EP |
0499004 | Aug 1992 | EP |
0550058 | Nov 1998 | EP |
0887632 | Dec 1998 | EP |
678909 | Jul 1999 | EP |
1061567 | Dec 2000 | EP |
0804631 | Sep 2002 | EP |
1889817 | Feb 2008 | EP |
2036600 | Mar 2009 | EP |
2426233 | Jul 2012 | EP |
686869 | Jul 1930 | FR |
1408266 | Aug 1965 | FR |
2233614 | Oct 1975 | FR |
2517790 | Jun 1983 | FR |
2610007 | Aug 1990 | FR |
752-277 | Jul 1956 | GB |
1186889 | Jun 1966 | GB |
1514921 | Jun 1978 | GB |
58-19462 | Apr 1983 | JP |
59-211779 | Nov 1984 | JP |
61038863 | Feb 1986 | JP |
S62237236 | Oct 1987 | JP |
S63136532 | Jun 1988 | JP |
H01296613 | Nov 1989 | JP |
H0130722 | Dec 1989 | JP |
H0293071 | Apr 1990 | JP |
H02-185038 | Jul 1990 | JP |
H02-217469 | Aug 1990 | JP |
03-044472 | Feb 1991 | JP |
H03-044472 | Feb 1991 | JP |
H03-155625 | Jul 1991 | JP |
H03-248427 | Nov 1991 | JP |
H0429313 | Jan 1992 | JP |
H04029313 | Jan 1992 | JP |
H04-115531 | Apr 1992 | JP |
H04115531 | Apr 1992 | JP |
H05-6880 | Jan 1993 | JP |
H05-23079 | Mar 1993 | JP |
405118928 | May 1993 | JP |
H05-118928 | May 1993 | JP |
H05-171446 | Jul 1993 | JP |
H05-291142 | Nov 1993 | JP |
H06-053210 | Feb 1994 | JP |
H0684888 | Mar 1994 | JP |
H06-140399 | May 1994 | JP |
H0616433 | Jun 1994 | JP |
6204231 | Jul 1994 | JP |
H06319177 | Nov 1994 | JP |
H06-338497 | Dec 1994 | JP |
H0729836 | Jan 1995 | JP |
H07297271 | Jan 1995 | JP |
07066267 | Mar 1995 | JP |
H07-74162 | Mar 1995 | JP |
H07-109576 | Apr 1995 | JP |
07-034936 | Aug 1995 | JP |
07034936 | Aug 1995 | JP |
H07-034936 | Aug 1995 | JP |
H07225214 | Aug 1995 | JP |
7-272694 | Oct 1995 | JP |
H07-283149 | Oct 1995 | JP |
H07283149 | Oct 1995 | JP |
H07-209093 | Nov 1995 | JP |
08-181135 | Jul 1996 | JP |
H08181135 | Jul 1996 | JP |
H08-335558 | Dec 1996 | JP |
H08335558 | Dec 1996 | JP |
H09064149 | Mar 1997 | JP |
9-89676 | Apr 1997 | JP |
H09148322 | Jun 1997 | JP |
H10-50635 | Feb 1998 | JP |
H1050800 | Feb 1998 | JP |
H10041096 | Feb 1998 | JP |
10-064696 | Mar 1998 | JP |
H10-064696 | Mar 1998 | JP |
H10-153494 | Jun 1998 | JP |
H10-227703 | Aug 1998 | JP |
10-0261620 | Sep 1998 | JP |
H10-0261620 | Sep 1998 | JP |
2845163 | Jan 1999 | JP |
H11-097163 | Apr 1999 | JP |
H11-118615 | Apr 1999 | JP |
H11-183264 | Jul 1999 | JP |
H11-183265 | Jul 1999 | JP |
H11-195688 | Jul 1999 | JP |
H11-287715 | Oct 1999 | JP |
2000068355 | Mar 2000 | JP |
2000182949 | Jun 2000 | JP |
2000269163 | Sep 2000 | JP |
2001-15698 | Jan 2001 | JP |
2001015698 | Jan 2001 | JP |
2001023872 | Jan 2001 | JP |
2001207265 | Jul 2001 | JP |
2001207268 | Jul 2001 | JP |
2001210602 | Aug 2001 | JP |
2001220677 | Aug 2001 | JP |
2001257199 | Sep 2001 | JP |
2001287180 | Oct 2001 | JP |
2001342570 | Dec 2001 | JP |
2002164342 | Jun 2002 | JP |
2002170781 | Jun 2002 | JP |
2002237375 | Aug 2002 | JP |
2003035574 | Feb 2003 | JP |
2003053688 | Feb 2003 | JP |
2003133300 | May 2003 | JP |
2003153706 | May 2003 | JP |
2003303814 | Oct 2003 | JP |
2004014952 | Jan 2004 | JP |
2004023043 | Jan 2004 | JP |
2004091848 | Mar 2004 | JP |
2004113270 | Apr 2004 | JP |
2004128019 | Apr 2004 | JP |
2004134553 | Apr 2004 | JP |
2004163293 | Jun 2004 | JP |
2004244661 | Sep 2004 | JP |
2004294638 | Oct 2004 | JP |
3589954 | Nov 2004 | JP |
2004310019 | Nov 2004 | JP |
2004538374 | Dec 2004 | JP |
2005033221 | Feb 2005 | JP |
2005079254 | Mar 2005 | JP |
2005507030 | Mar 2005 | JP |
2005172489 | Jun 2005 | JP |
3725100 | Dec 2005 | JP |
2006028572 | Feb 2006 | JP |
2006049352 | Feb 2006 | JP |
2006059931 | Mar 2006 | JP |
2006090762 | Apr 2006 | JP |
2006124832 | May 2006 | JP |
2006153706 | Jun 2006 | JP |
2006186271 | Jul 2006 | JP |
2006188729 | Jul 2006 | JP |
2006278058 | Oct 2006 | JP |
2006319261 | Nov 2006 | JP |
2007027777 | Feb 2007 | JP |
2008202107 | Sep 2007 | JP |
2007287902 | Nov 2007 | JP |
3140111 | Mar 2008 | JP |
2008060304 | Mar 2008 | JP |
2008066159 | Mar 2008 | JP |
2008085129 | Apr 2008 | JP |
2008089320 | Apr 2008 | JP |
2008172083 | Jul 2008 | JP |
2008527748 | Jul 2008 | JP |
2008198629 | Aug 2008 | JP |
2008202107 | Sep 2008 | JP |
2009016815 | Jan 2009 | JP |
2009088421 | Apr 2009 | JP |
2009239082 | Apr 2009 | JP |
2009099938 | May 2009 | JP |
2009194248 | Aug 2009 | JP |
2009251216 | Oct 2009 | JP |
2009252851 | Oct 2009 | JP |
2010067940 | Mar 2010 | JP |
2010097834 | Apr 2010 | JP |
2010205967 | Sep 2010 | JP |
2010251444 | Oct 2010 | JP |
2010255218 | Nov 2010 | JP |
2011049592 | Mar 2011 | JP |
2011162830 | Aug 2011 | JP |
2011181681 | Sep 2011 | JP |
2009010412 | Feb 2012 | JP |
2012089837 | May 2012 | JP |
2012146939 | Aug 2012 | JP |
2012164736 | Aug 2012 | JP |
2012195513 | Oct 2012 | JP |
2013026479 | Feb 2013 | JP |
2013196822 | Sep 2013 | JP |
2013235912 | Nov 2013 | JP |
2014522104 | Aug 2014 | JP |
D1422467 | Aug 2014 | JP |
2014222693 | Nov 2014 | JP |
2015115461 | Jun 2015 | JP |
2016098406 | May 2016 | JP |
2010123843 | Jun 2016 | JP |
2017183242 | Oct 2017 | JP |
6519897 | May 2019 | JP |
2016174158 | Jun 2019 | JP |
1998-0026850 | Jul 1998 | KR |
100253664 | Apr 2000 | KR |
10-2000-0031098 | Jun 2000 | KR |
10-2000-0045257 | Jul 2000 | KR |
100273261 | Dec 2000 | KR |
10-0295043 | Apr 2001 | KR |
10-2002-0027695 | Apr 2002 | KR |
10-2002-0064028 | Aug 2002 | KR |
2002-0086763 | Nov 2002 | KR |
10-0377095 | Mar 2003 | KR |
2003-0092305 | Dec 2003 | KR |
10-2005-0054122 | Jun 2005 | KR |
10-0547248 | Jan 2006 | KR |
10-0593960 | Jun 2006 | KR |
10-2006-0129566 | Dec 2006 | KR |
10-0688484 | Feb 2007 | KR |
10-2007-0079797 | Aug 2007 | KR |
10-2007-0084683 | Aug 2007 | KR |
20080058620 | Jun 2008 | KR |
10-2009-0039936 | Apr 2009 | KR |
10-2009-0055443 | Jun 2009 | KR |
10-2009-0056475 | Jun 2009 | KR |
10-2009-0086790 | Aug 2009 | KR |
10-2009-0105977 | Oct 2009 | KR |
10-0936694 | Jan 2010 | KR |
10-2010-0020834 | Feb 2010 | KR |
20100020834 | Feb 2010 | KR |
10-2010-0032812 | Mar 2010 | KR |
20100032812 | Mar 2010 | KR |
10-2010-0077442 | Jul 2010 | KR |
20100079920 | Jul 2010 | KR |
10-2010-0132779 | Dec 2010 | KR |
10-2011-0058534 | Jun 2011 | KR |
10-1114219 | Mar 2012 | KR |
20120111060 | Oct 2012 | KR |
10-2013-0007806 | Jan 2013 | KR |
10-2013-0067600 | Jun 2013 | KR |
10-1347962 | Jan 2014 | KR |
101491726 | Feb 2015 | KR |
10-1535573 | Jul 2015 | KR |
10-2019-0032077 | Mar 2019 | KR |
8600255 | Sep 1987 | NL |
8701549 | Feb 1989 | NL |
494614 | Feb 1976 | SU |
1408319 | Jul 1988 | SU |
1786406 | Jan 1993 | SU |
538327 | Jun 2003 | TW |
540093 | Jul 2003 | TW |
I226380 | Jan 2005 | TW |
M292692 | Jun 2006 | TW |
200701301 | Jan 2007 | TW |
200731357 | Aug 2007 | TW |
200903625 | Jan 2009 | TW |
201247690 | Dec 2012 | TW |
M446412 | Feb 2013 | TW |
201330086 | Jul 2013 | TW |
D162593 | Aug 2014 | TW |
D164568 | Dec 2014 | TW |
201531587 | Aug 2015 | TW |
M512254 | Nov 2015 | TW |
1514509 | Dec 2015 | TW |
201613231 | Apr 2016 | TW |
M553518 | Dec 2017 | TW |
D196097 | Feb 2019 | TW |
1987001508 | Mar 1987 | WO |
1990004045 | Apr 1990 | WO |
1991004522 | Apr 1991 | WO |
1991006975 | May 1991 | WO |
1992000477 | Jan 1992 | WO |
1994027315 | Nov 1994 | WO |
1996017107 | Jun 1996 | WO |
1997003223 | Jan 1997 | WO |
1998032893 | Jul 1998 | WO |
1999023690 | May 1999 | WO |
DM048579 | Jul 1999 | WO |
2004008491 | Jul 2002 | WO |
2004008827 | Jan 2004 | WO |
2004010467 | Jan 2004 | WO |
2004106584 | Dec 2004 | WO |
2005112082 | Nov 2005 | WO |
2006035281 | Apr 2006 | WO |
2006054854 | May 2006 | WO |
2006056091 | Jun 2006 | WO |
2006078666 | Jul 2006 | WO |
2006080782 | Aug 2006 | WO |
2006097525 | Sep 2006 | WO |
2006101857 | Sep 2006 | WO |
2006114781 | Nov 2006 | WO |
2007024720 | Mar 2007 | WO |
2007027165 | Mar 2007 | WO |
2007076195 | Jul 2007 | WO |
2007117718 | Oct 2007 | WO |
2007131051 | Nov 2007 | WO |
2007140376 | Dec 2007 | WO |
2008045972 | Apr 2008 | WO |
2008091900 | Jul 2008 | WO |
2008121463 | Oct 2008 | WO |
2008147731 | Dec 2008 | WO |
2009028619 | Mar 2009 | WO |
2009029532 | Mar 2009 | WO |
2009039251 | Mar 2009 | WO |
2009099776 | Aug 2009 | WO |
2009154889 | Dec 2009 | WO |
2009154896 | Dec 2009 | WO |
2010039363 | Apr 2010 | WO |
2010077533 | Jul 2010 | WO |
2010100702 | Sep 2010 | WO |
2010110558 | Sep 2010 | WO |
2010118051 | Oct 2010 | WO |
2010129428 | Nov 2010 | WO |
2010129430 | Nov 2010 | WO |
2010129431 | Nov 2010 | WO |
2010118051 | Jan 2011 | WO |
2011019950 | Feb 2011 | WO |
2011149640 | Dec 2011 | WO |
2012056592 | May 2012 | WO |
2012077590 | Jun 2012 | WO |
2013043330 | Mar 2013 | WO |
2013078065 | May 2013 | WO |
2013078066 | May 2013 | WO |
2014107290 | Jul 2014 | WO |
2015026230 | Feb 2015 | WO |
2015107009 | Jul 2015 | WO |
2015112728 | Jul 2015 | WO |
2018109553 | Jun 2016 | WO |
2018109554 | Jun 2016 | WO |
2017108713 | Jun 2017 | WO |
2017108714 | Jun 2017 | WO |
2017212546 | Dec 2017 | WO |
2018003072 | Jan 2018 | WO |
2018008088 | Jan 2018 | WO |
2018013778 | Jan 2018 | WO |
2018020316 | Feb 2018 | WO |
2018020318 | Feb 2018 | WO |
2018020320 | Feb 2018 | WO |
2018020327 | Feb 2018 | WO |
2008045972 | Apr 2018 | WO |
20181095 | Jun 2018 | WO |
2018105349 | Jun 2018 | WO |
2018109552 | Jun 2018 | WO |
2018178771 | Oct 2018 | WO |
2019030565 | Feb 2019 | WO |
2019103610 | May 2019 | WO |
2019103613 | May 2019 | WO |
2019142055 | Jul 2019 | WO |
2019158960 | Aug 2019 | WO |
2019217749 | Nov 2019 | WO |
2019229537 | Dec 2019 | WO |
2020002995 | Jan 2020 | WO |
2020003000 | Jan 2020 | WO |
Entry |
---|
USPTO; Office Action dated Jan. 10, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Restriction Requirment dated Oct. 29, 2013 in U.S. Appl. No. 13/439,528. |
USPTO; USPTO; Notice of Allowance dated Aug. 28, 2015 in U.S. Appl. No. 13/597,043. |
USPTO; Final Office Action dated Feb. 11, 2016 U.S. Appl. No. 14/090,750. |
USPTO; Non Final Office Action dated 112/21/2016 in U.S. Appl. No. 15/144,481. |
Chang et al. “Small-Subthreshold-Swing and Low-Voltage Flexible Organic Thin-Film Transistors Which Use HfLaO as the Gate Dielectric,” IEEE Electron Device Letters, pp. 133-135; vol. 30, No. 2; IEEE Electron Device Society (2009). |
Erjee et al., “Sub-100nm Gate Length Metal Gate NMOS Transistors Fabricated by a Replacement by a Replacement Gate Process,” IEEE Semiconductor Process and Device Center, 821-824 (1997). |
H.J. Yun et al., “Comparison of Atomic Scale Etching of Poly-Si in Inductively Coupled Ar and He Plasmas”, Korean Journal of Chemical Engineering, vol. 24, pp. 670-673 (2007). |
Jones et al., “Growth of Aluminium Films by Low Pressure Chemical Vapour Deposition Using Tritertiarybutylaluminium,” Journal of Crystal Growth 135, pp. 285-289, Elsevier Science B.V. (1994). |
Kim et al., “Characteristics of Low Temperaure High Quality Silicon Oxide by Plasma Enhanced Atomic Layer Deposition with In-Situ Plasma Densification Process,” The Electrochemical Society, ECS Transactions, College of Information and Communication Engineerign, Sungkyunkwan University, 53(1). |
Krenek et al. “IR Laser CVD of Nanodisperse Ge—Si—Sn Alloys Obtained by Dielectric Breakdown of GeH4/SiH4/SnH4 Mixtures”, NanoCon 2014, Nov. 5-7, Brno, Czech Republic, EU (2014). |
Liu et al., “Research, Design, and Experimen of End Effector for Wafer Transfer Robot,” Industrial Robot: An International Journal, 79-91 (2012). |
Marsik et al., “Effect of Ultraviolet Curing Wavelength on Low-k Dielectric Material Proerties and Plasma Damage Resistance,” Sciencedirect.com, 519, 11, 3619-3626 (2011). |
Nigamananda et al., “Low-Temperature (<200oC) Plasma Enhanced Atomic Deposition of Dense Titanium Nitride Thin Films.” (2012). |
Novaro et al. Theoretical Study on a Reaction Pathway of Ziegler-Natta-Type Catalysis, J. Chem. Phys. 68(5), p. 2337-2351 (1978). |
Okamoto et al., “Luminescent Properties of Pr3+- sensitized LaPO4: Gd3+ Ultraviolet-B Phosphor Under Vacuum-Ultraviolet Light Excitation,” J. App. Phys. 106, 013522 (2009). |
Presser, et al., “Effect of Pore Size on Carbon Dioxide Sorption by Carbide Derived Caton,” Energy & Environmental Science 4.8, 3059-3066 (2011). |
S.D. Athavale and D.J. Economou, “Realization of Atomic Layer Etching of Silicon”, Journal of Vacuum Science and Technology B, vol. 14, pp. 3702-3705 (1996). |
“Solid State Research, Quarterly Technical Report,” Massachusetts Institute of Technology, Lincoln Library, Aug. 10, 60 pages (1995). |
Wirths, et al, “SiGeSn Growth Studies Using Reduced Pressure Chemical Vapor Deposition Towards Optoeleconic Applications,” This Solid Films, 557, 183-187 (2014). |
USPTO; Notice of Allowance dated Jul. 26, 2005 in U.S. Appl. No. 10/033,058. |
USPTO; Non-Final Office Action dated Aug. 25, 2005 in U.S. Appl. No. 10/191,635. |
USPTO; Final Office Action dated Apr. 25, 2006 in U.S. Appl. No. 10/191,635. |
USPTO; Non-Final Office Action dated Nov. 20, 2006 in U.S. Appl. No. 10/191,635. |
USPTO; Notice of Allowance dated May 21, 2007 in U.S. Appl. No. 10/191,635. |
USPTO; Notice of Allowance dated Feb. 20, 2008 in U.S. Appl. No. 10/191,635. |
USPTO; Non-Final Office Action dated Oct. 22, 2003 in U.S. Appl. No. 10/222,229. |
USPTO; Final Office Action dated Mar. 22, 2004 in U.S. Appl. No. 10/222,229. |
USPTO; Advisory Action dated Oct. 7, 2004 in U.S. Appl. No. 10/222,229. |
USPTO; Non-Final Office Action dated Dec. 22, 2004 in U.S. Appl. No. 10/222,229. |
USPTO; Final Office Action dated Jun. 20, 2005 in U.S. Appl. No. 10/222,229. |
USPTO; Advisory Action dated Nov. 16, 2005 in U.S. Appl. No. 10/222,229. |
USPTO; Notice of Allowance dated Mar. 8, 2006 in U.S. Appl. No. 10/222,229. |
USPTO; Non-Final Office Action dated Jan. 26, 2005 in U.S. Appl. No. 10/838,510. |
USPTO; Notice of Allowance dated Jul. 12, 2005 in U.S. Appl. No. 10/838,510. |
USPTO; Office Action dated Aug. 27, 2010 in U.S. Appl. No. 12/118,596. |
USPTO; Office Action dated Feb. 15, 2011 in U.S. Appl. No. 12/118,596. |
USPTO; Notice of Allowance dated Aug. 4, 2011 in U.S. Appl. No. 12/118,596. |
USPTO; Non-Final Office Action dated Mar. 28, 2010 in U.S. Appl. No. 12/121,085. |
USPTO; Notice of Allowance dated Jul. 26, 2010 in U.S. Appl. No. 12/121,085. |
USPTO; Notice of Allowance dated Oct. 4, 2010 in U.S. Appl. No. 12/121,085. |
USPTO; Non-Final Office Action dated Sep. 13, 2010 in U.S. Appl. No. 12/140,809. |
USPTO; Final Office Action dated Dec. 28, 2010 in U.S. Appl. No. 12/140,809. |
USPTO; Notice of Allowance dated Mar. 17, 2011 in U.S. Appl. No. 12/140,809. |
USPTO; Non-Final Office Action dated Mar. 15, 2011 in U.S. Appl. No. 12/193,924. |
USPTO; Foma; Office Action dated Sep. 30, 2011 in U.S. Appl. No. 12/193,924. |
USPTO; Non-Final Office Action dated Oct. 24, 2012 in U.S. Appl. No. 12/193,924. |
USPTO; Final Office Action dated Apr. 17, 2013 in U.S. Appl. No. 12/193,924. |
USPTO; Advisory Action dated Jul. 9, 2013 in U.S. Appl. No. 12/193,924. |
USPTO; Non-Final Office Action dated Jul. 28, 2011 in U.S. Appl. No. 12/330,096. |
USPTO; Final Office Action dated Jan. 13, 2012 in U.S. Appl. No. 12/330,096. |
USPTO; Notice of Allowance dated Mar. 6, 2012 in U.S. Appl. No. 12/330,096. |
USPTO; Non-Final Office Action dated Mar. 20, 2012 in U.S. Appl. No. 12/330,096. |
USPTO; Notice of Allowance dated Jun. 7, 2012 in U.S. Appl. No. 12/330,096. |
USPTO; Non-Final Office Action dated Apr. 1, 2010 in U.S. Appl. No. 12/357,174. |
USPTO; Final Office Action dated Sep. 1, 2010 in U.S. Appl. No. 12/357,174. |
USPTO; Notice of Allowance dated Dec. 13, 2010 in U.S. Appl. No. 12/357,174. |
USPTO; Non-Final Office Action dated Dec. 29, 2010 in U.S. Appl. No. 12/362,023. |
USPTO; Non-Final Office Action dated Jul. 26, 2011 in U.S. Appl. No. 12/416,809. |
USPTO; Final Office Action dated Dec. 6, 2011 in U.S. Appl. No. 12/416,809. |
USPTO; Notice of Allowance dated Apr. 2, 2012 in U.S. Appl. No. 12/416,809. |
USPTO; Advisory Action dated Feb. 3, 2012 in U.S. Appl. No. 12/416,809. |
USPTO; Notice of Allowance dated Jun. 16, 2011 in U.S. Appl. No. 12/430,751. |
USPTO; Notice of Allowance dated Jul. 27, 2011 in U.S. Appl. No. 12/430,751. |
USPTO; Non-Final Office Action dated Aug. 3, 2011 in U.S. Appl. No. 12/436,300. |
USPTO; Final Office Action dated Jan. 23, 2012 in U.S. Appl. No. 12/436,300. |
USPTO; Advisory Action dated Mar. 6, 2012 in U.S. Appl. No. 12/436,300. |
USPTO; Non-Final Office Action dated May 22, 2012 in U.S. Appl. No. 12/436,300. |
USPTO; Notice of Allowance dated Nov. 28, 2012 in U.S. Appl. No. 12/436,300. |
USPTO; Restriction Requirement dated Dec. 20, 2011 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated Apr. 11, 2012 in U.S. Appl. No. 12/436,306. |
USPTO; Final Office Action dated Sep. 26, 2012 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated May 31, 2013 in U.S. Appl. No. 12/436,306. |
USPTO; Final Office Action dated Oct. 17, 2013 in U.S. Appl. No. 12/436,306. |
USPTO; Advisory Action dated Oct. 1, 2014 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated Feb. 4, 2014 in U.S. Appl. No. 12/436,306. |
USPTO; Final Office Action dated Jun. 23, 2014 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated Feb. 3, 2015 in U.S. Appl. No. 12/436,306. |
USPTO; Final Office Action dated May 13, 2015 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated Oct. 14, 2015 in U.S. Appl. No. 12/436,306. |
USPTO; Final Office Action dated Dec. 31, 2015 in U.S. Appl. No. 12/436,306. |
USPTO; Notice of Allowance dated Feb. 3, 2016 in U.S. Appl. No. 12/436,306. |
USPTO; Non-Final Office Action dated Aug. 3, 2011 in U.S. U.S. Appl. No. 12/436,315. |
USPTO; Notice of Allowance dated Nov. 17, 2011 in U.S. Appl. No. 12/436,315. |
USPTO; Notice of Allowance dated Oct. 1, 2010 in U.S. Appl. No. 12/467,017. |
USPTO; Non-Final Office Action dated Mar. 18, 2010 in U.S. Appl. No. 12/489,252. |
USPTO; Notice of Allowance dated Sep. 2, 2010 in U.S. Appl. No. 12/489,252. |
USPTO; Non-Final Office Action dated Dec. 15, 2010 in U.S. Appl. No. 12/553,759. |
USPTO; Final Office Action dated May 4, 2011 in U.S. Appl. No. 12/553,759. |
USPTO; Advisory Action dated Jul. 13, 2011 in U.S. Appl. No. 12/553,759. |
USPTO; Non-Final Office Action dated Sep. 6, 2011 in U.S. Appl. No. 12/553,759. |
USPTO; Notice of Allowance dated Jan. 24, 2012 in U.S. Appl. No. 12/553,759. |
USPTO; Non-Final Office Action dated Oct. 19, 2012 in U.S. Appl. No. 12/618,355. |
USPTO; Final Office Action dated May 8, 2013 in U.S. Appl. No. 12/618,355. |
USPTO; Advisory Action dated Jul. 23, 2013 in U.S. Appl. No. 12/618,355. |
USPTO; Non-Final Office Action dated Apr. 8, 2015 in U.S. Appl. No. 12/618,355. |
USPTO; Final Office Action dated Oct. 22, 2015 in U.S. Appl. No. 12/618,355. |
USPTO; Advisory Action dated Mar. 4, 2016 in U.S. Appl. No. 12/618,355. |
USPTO; Non-Final Office Action dated Jun. 30, 2016 in U.S. Appl. No. 12/618,355. |
USPTO; Final Office Action dated Feb. 10, 2017 in U.S. Appl. No. 12/618,355. |
USPTO; Advisory Action dated May 16, 2017 in U.S. Appl. No. 12/618,355. |
USPTO; Non-Final Office Action dated Nov. 29, 2017 in U.S. Appl. No. 12/618,355. |
USPTO; Final Office Action dated Aug. 10, 2018 in U.S. Appl. No. 12/618,355. |
USPTO; Non-Final Office Action dated Feb. 16, 2012 in U.S. Appl. No. 12/618,419. |
USPTO; Final Office Action dated Jun. 22, 2012 in U.S. Appl. No. 12/618,419. |
USPTO; Non-Final Office Action dated Nov. 27, 2012 in U.S. Appl. No. 12/618,419. |
USPTO; Advisory Action dated Aug. 9, 2012 in U.S. Appl. No. 12/618,419. |
USPTO; Notice of Allowance dated Apr. 12, 2013 in U.S. Appl. No. 12/618,419. |
USPTO; Notice of Allowance dated Oct. 9, 2013 in U.S. Appl. No. 12/618,419. |
USPTO; Requirement for Restriction dated Sep. 12, 2011 in U.S. Appl. No. 12/718,731. |
USPTO; Non-Final Office Action dated Dec. 6, 2011 in U.S. Appl. No. 12/718,731. |
USPTO; Notice of Allowance dated Mar. 16, 2012 in U.S. Appl. No. 12/718,731. |
USPTO; Restriction Requirement dated Jan. 15, 2013 in U.S. Appl. No. 12/754,223. |
USPTO; Office Action dated Feb. 26, 2013 in U.S. Appl. No. 12/754,223. |
USPTO; Final Office Action dated Jun. 28, 2013 in U.S. Appl. No. 12/754,223. |
USPTO; Office Action dated Feb. 25, 2014 in U.S. Appl. No. 12/754,223. |
USPTO; Final Office Action dated Jul. 14, 2014 in U.S. Appl. No. 12/754,223. |
USPTO; Non-Final Office Action dated Mar. 25, 2015 in U.S. Appl. No. 12/754,223. |
USPTO; Final Office Action dated Aug. 12, 2015 in U.S. Appl. No. 12/754,223. |
USPTO; Notice of Allowance dated May 23, 2016 in U.S. Appl. No. 12/754,223. |
USPTO; Office Action dated Apr. 23, 2013 in U.S. Appl. No. 12/763,037. |
USPTO; Final Office Action dated Oct. 21, 2013 in U.S. Appl. No. 12/763,037. |
USPTO; Office Action dated Oct. 8, 2014 in U.S. Appl. No. 12/763,037. |
USPTO; Notice of Allowance dated Jan. 27, 2015 in U.S. Appl. No. 12/763,037. |
USPTO; Non-Final Office Action dated Jan. 24, 2011 in U.S. Appl. No. 12/778,808. |
USPTO; Notice of Allowance dated May 9, 2011 in U.S. Appl. No. 12/778,808. |
USPTO; Notice of Allowance dated Oct. 12, 2012 in U.S. Appl. No. 12/832,739. |
USPTO; Non-Final Office Action dated Oct. 16, 2012 in U.S. Appl. No. 12/847,848. |
USPTO; Final Office Action dated Apr. 22, 2013 in U.S. Appl. No. 12/847,848. |
USPTO; Advisory Action dated Jul. 1, 2013 in U.S. Appl. No. 12/847,848. |
USPTO; Notice of Allowance dated Jan. 16, 2014 in U.S. Appl. No. 12/847,848. |
USPTO; Restriction Requirement dated Sep. 25, 2012 in U.S. Appl. No. 12/854,818. |
USPTO; Office Action dated Dec. 6, 2012 in U.S. Appl. No. 12/854,818. |
USPTO; Final Office Action dated Mar. 13, 2013 in U.S. Appl. No. 12/854,818. |
USPTO; Office Action dated Aug. 30, 2013 in U.S. Appl. No. 12/854,818. |
USPTO; Final Office Action dated Mar. 26, 2014 in U.S. Appl. No. 12/854,818. |
USPTO; Office Action dated Jun. 3, 2014 in U.S. Appl. No. 12/854,818. |
USPTO; Non-Final Office Action dated Jul. 11, 2012 in U.S. Appl. No. 12/875,889. |
USPTO; Notice of Allowance dated Jan. 4, 2013 in U.S. Appl. No. 12/875,889. |
USPTO; Notice of Allowance dated Jan. 9, 2012 in U.S. Appl. No. 12/901,323. |
USPTO; Requirement for Restriction dated Jul. 22, 2013 in U.S. Appl. No. 12/910,607. |
USPTO; Non-Final Office Action dated Nov. 20, 2013 in U.S. Appl. No. 12/910,607. |
USPTO; Final Office Action dated Apr. 28, 2014 in U.S. Appl. No. 12/910,607. |
USPTO; Advisory Action dated Jul. 9, 2014 in U.S. Appl. No. 12/910,607. |
USPTO; Notice of Allowance dated Aug. 15, 2014 in U.S. Appl. No. 12/910,607. |
USPTO; Non-Final Office Action dated Oct. 24, 2012 in U.S. Appl. No. 12/940,906. |
USPTO; Final Office Action dated Feb. 13, 2013 in U.S. Appl. No. 12/940,906. |
USPTO; Notice of Allowance dated Apr. 23, 2013 in U.S. Appl. No. 12/940,906. |
USPTO; Non-Final Office Action dated Dec. 7, 2012 in U.S. Appl. No. 12/953,870. |
USPTO; Final Office Action dated Apr. 22, 2013 in U.S. Appl. No. 12/953,870. |
USPTO; Advisory Action dated Jul. 8, 2013 in U.S. Appl. No. 12/953,870. |
USPTO; Non-Final Office Action dated Aug. 28, 2013 in U.S. Appl. No. 12/953,870. |
USPTO; Final Office Action dated Apr. 17, 2014 in U.S. Appl. No. 12/953,870. |
USPTO; Requirement for Restriction dated Sep. 10, 2010 in U.S. Appl. No. 12/148,956. |
USPTO; Non-Final Office Action dated Sep. 19, 2012 in U.S. Appl. No. 13/016,735. |
USPTO; Final Office Action dated Feb. 11, 2013 in U.S. Appl. No. 13/016,735. |
USPTO; Notice of Allowance dated Apr. 24, 2013 in U.S. Appl. No. 13/016,735. |
USPTO; Non-Final Office Action dated Apr. 4, 2012 in U.S. Appl. No. 13/030,438. |
USPTO; Final Office Action dated Aug. 22, 2012 in U.S. Appl. No. 13/030,438. |
USPTO; Notice of Allowance dated Oct. 24, 2012 in U.S. Appl. No. 13/030,438. |
USPTO; Non-Final Office Action dated Dec. 3, 2012 in U.S. Appl. No. 13/040,013. |
USPTO; Notice of Allowance dated May 3, 2013 in U.S. Appl. No. 13/040,013. |
USPTO; Notice of Allowance dated Sep. 13, 2012 in U.S. Appl. No. 13/085,698. |
USPTO; Non-Final Office Action dated Mar. 29, 2013 in U.S. Appl. No. 13/094,402. |
USPTO; Final Office Action dated Jul. 17, 2013 in U.S. Appl. No. 13/094,402. |
USPTO; Notice of Allowance dated Sep. 30, 2013 in U.S. Appl. No. 13/094,402. |
USPTO; Restriction Requirement dated May 8, 2013 in U.S. Appl. No. 13/102,980. |
USPTO; Office Action dated Oct. 7, 2013 in U.S. Appl. No. 13/102,980. |
USPTO; Final Office Action dated Mar. 25, 2014 in U.S. Appl. No. 13/102,980. |
USPTO; Advisory Action dated Jun. 12, 2014 in U.S. Appl. No. 13/102,980. |
USPTO; Notice of Allowance dated Jul. 3, 2014 in U.S. Appl. No. 13/102,980. |
USPTO; Notice of Allowance dated Sep. 17, 2014 in U.S. Appl. No. 13/102,980. |
USPTO; Requirement for Restriction dated Jun. 5, 2014 in U.S. Appl. No. 13/154,271. |
USPTO; Non-Final Office Action dated Jul. 17, 2014 in U.S. Appl. No. 13/154,271. |
USPTO; Final Office Action dated Jan. 2, 2015 in U.S. Appl. No. 13/154,271. |
USPTO; Non-Final Office Action dated May 27, 2015 in U.S. Appl. No. 13/154,271. |
USPTO; Final Office Action dated Nov. 23, 2015 in U.S. Appl. No. 13/154,271. |
USPTO; Notice of Allowance dated Feb. 10, 2016 in U.S. Appl. No. 13/154,271. |
USPTO; Requirement for Restriction dated Apr. 6, 2016 in U.S. Appl. No. 13/166,367. |
USPTO; Non-Final Office Action dated Jun. 27, 2016 in U.S. Appl. No. 13/166,367. |
USPTO; Final Office Action dated Dec. 30, 2016 in U.S. Appl. No. 13/166,367. |
USPTO; Advisory Action dated Apr. 21, 2017 in U.S. Appl. No. 13/166,367. |
USPTO; Requirement for Restriction dated Jun. 18, 2014 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Oct. 27, 2014 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated May 26, 2015 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Sep. 1, 2015 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated Mar. 3, 2016 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Jun. 9, 2016 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated Dec. 9, 2016 in U.S. Appl. No. 13/169,951. |
USPTO; Advisory Action dated May 13, 2016 in U.S. Appl. No. 13/169,951. |
USPTO; Advisory Action dated Feb. 15, 2017 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Apr. 26, 2017 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated Nov. 2, 2017 in U.S. Appl. No. 13/169,951. |
USPTO; Advisory Action dated Feb. 8, 2018 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Apr. 6, 2018 in U.S. Appl. No. 13/169,951. |
USPTO; Non-Final Office Action dated Jun. 24, 2014 in U.S. Appl. No. 13/181,407. |
USPTO; Final Office Action dated Sep. 24, 2014 in U.S. Appl. No. 13/181,407. |
USPTO; Advisory Action dated Dec. 17, 2014 in U.S. Appl. No. 13/181,407. |
USPTO; Non-Final Office Action dated Jan. 2, 2015 in U.S. Appl. No. 13/181,407. |
USPTO; Final Office Action dated Apr. 8, 2015 in U.S. Appl. No. 13/181,407. |
USPTO; Requirement for Restriction Sep. 25, 2012 in U.S. Appl. No. 13/184,351. |
USPTO; Non-Final Office Action dated Jan. 23, 2013 in U.S. Appl. No. 13/184,351. |
USPTO; Final Office Action dated Jul. 29, 2013 in U.S. Appl. No. 13/184,351. |
USPTO; Advisory Action dated Nov. 7, 2013 in U.S. Appl. No. 13/184,351. |
USPTO; Non-Final Office Action dated Jul. 16, 2014 in U.S. Appl. No. 13/184,351. |
USPTO; Final Office Action dated Feb. 17, 2015 in U.S. Appl. No. 13/184,351. |
USPTO; Advisory Action dated May 18, 2015 in U.S. Appl. No. 13/184,351. |
USPTO; Non-Final Office Action dated Aug. 10, 2015 in U.S. Appl. No. 13/184,351. |
USPTO; Final Office Action dated Feb. 12, 2016 in U.S. Appl. No. 13/184,351. |
USPTO; Non-Final Office Action dated Dec. 15, 2016 in U.S. Appl. No. 13/184,351. |
USPTO; Final Office Action dated Jun. 15, 2017 in U.S. Appl. No. 13/184,351. |
USPTO; Advisory Action dated Oct. 4, 2017 in U.S. Appl. No. 13/184,351. |
USPTO; Non-Final Office Action dated Jul. 26, 2018 in U.S. Appl. No. 13/184,351. |
USPTO; Restriction Requirement dated Aug. 21, 2014 in U.S. Appl. No. 13/187,300. |
USPTO; Non-Final Office Action dated Sep. 17, 2014 in U.S. Appl. No. 13/187,300. |
USPTO; Final Office Action dated Apr. 15, 2015 in U.S. Appl. No. 13/187,300. |
USPTO; Non-Final Office Action dated Apr. 7, 2016 in U.S. Appl. No. 13/187,300. |
USPTO; Final Office Acton dated Sep. 23, 2016 in U.S. Appl. No. 13/187,300. |
USPTO; Non-Final Office Action dated Jan. 30, 2017 in U.S. Appl. No. 13/187,300. |
USPTO; Final Office Action dated Aug. 9, 2017 in U.S. Appl. No. 13/187,300. |
USPTO; Non-Final Office Action dated Oct. 1, 2012 in U.S. Appl. No. 13/191,762. |
USPTO; Final Office Action dated Apr. 10, 2013 in U.S. Appl. No. 13/191,762. |
USPTO; Notice of Allowance dated Aug. 15, 2013 in U.S. Appl. No. 13/191,762. |
USPTO; Non-Final Office Action dated Oct. 22, 2012 in U.S. Appl. No. 13/238,960. |
USPTO; Final Office Action dated May 3, 2013 in U.S. Appl. No. 13/238,960. |
USPTO; Non-Final Office Action dated Apr. 26, 2013 in U.S. Appl. No. 13/250,721. |
USPTO; Notice of Allowance dated Sep. 11, 2013 in U.S. Appl. No. 13/250,721. |
USPTO; Non-Final Office Action dated Jul. 2, 2014 in U.S. Appl. No. 13/283,408. |
USPTO; Final Office Action dated Jan. 29, 2015 in U.S. Appl. No. 13/283,408. |
USPTO; Non-Final Office Action dated Jun. 17, 2015 in U.S. Appl. No. 13/283,408. |
USPTO; Final Office Action dated Dec. 18, 2015 in U.S. Appl. No. 13/283,408. |
USPTO; Advisory Action dated Mar. 28, 2016 in U.S. Appl. No. 13/283,408. |
USPTO; Notice of Allowance dated Mar. 28, 2016 in U.S. Appl. No. 13/283,408. |
USPTO; Restriction Requirement dated Dec. 16, 2013 in U.S. Appl. No. 13/284,642. |
USPTO; Restriction Requirement dated Apr. 21, 2014 in U.S. Appl. No. 13/284,642. |
USPTO; Office Action dated Jul. 30, 2014 in U.S. Appl. No. 13/284,642. |
USPTO; Notice of Allowance dated Feb. 11, 2015 in U.S. Appl. No. 13/284,642. |
USPTO; Restriction Requirement dated Oct. 2, 2013 in U.S. Appl. No. 13/312,591. |
USPTO; Office Action dated Jan. 28, 2014 in U.S. Appl. No. 13/312,591. |
USPTO; Final Office Action dated May 14, 2014 in U.S. Appl. No. 13/312,591. |
USPTO; Advisory Action dated Aug. 26, 2014 in U.S. Appl. No. 13/312,591. |
USPTO; Non-Final Office Action dated Nov. 26, 2014 in U.S. Appl. No. 13/312,591. |
USPTO; Final Office Action dated Mar. 20, 2015 in U.S. Appl. No. 13/312,591. |
USPTO; Notice of Allowance dated May 14, 2015 in U.S. Appl. No. 13/312,591. |
USPTO; Notice of Allowance dated Jun. 11, 2015 in U.S. Appl. No. 13/312,591. |
USPTO; Requirement for Restriction dated Nov. 26, 2013 in U.S. Appl. No. 13/333,420. |
USPTO; Non-Final Office Action dated Apr. 9, 2014 in U.S. Appl. No. 13/333,420. |
USPTO; Notice of Allowance dated Sep. 15, 2014 in U.S. Appl. No. 13/333,420. |
USPTO; Requirement for Restriction dated Jan. 10, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Office Action dated Feb. 11, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Final Office Action dated May 17, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Office Action dated Aug. 29, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Final Office Action dated Dec. 18, 2013 in U.S. Appl. No. 13/339,609. |
USPTO; Notice of Allowance dated Apr. 7, 2014 in U.S. Appl. No. 13/339,609. |
USPTO; Non-Final Office Action dated Oct. 10, 2012 in U.S. Appl. No. 13/406,791. |
USPTO; Final Office Action dated Jan. 31, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Advisory Action dated Mar. 27, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Non-Final Office Action dated Apr. 25, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Final Office Action dated Aug. 23, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Advisory Action dated Oct. 29, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Non-Final Office Action dated Dec. 4, 2013 in U.S. Appl. No. 13/406,791. |
USPTO; Final Office Action dated Apr. 21, 2014 in U.S. Appl. No. 13/406,791. |
USPTO; Non-Final Office Action dated Jan. 14, 2013 in U.S. Appl. No. 13/410,970. |
USPTO; Notice of Allowance dated Feb. 14, 2013 in U.S. Appl. No. 13/410,970. |
USPTO; Non-Final Office Action dated Feb. 13, 2014 in U.S. Appl. No. 13/411,271. |
USPTO; Non-Final Office Action dated Jul. 31, 2014 in U.S. Appl. No. 13/411,271. |
USPTO; Advisory Action dated Apr. 22, 2015 in U.S. Appl. No. 13/411,271. |
USPTO; Final Office Action dated Jan. 16, 2015 in U.S. Appl. No. 13/411,271. |
USPTO; Notice of Allowance dated Oct. 6, 2015 in U.S. Appl. No. 13/411,271. |
USPTO; Office Action dated Feb. 4, 2014 in U.S. Appl. No. 13/439,528. |
USPTO; Final Office Action dated Jul. 8, 2014 in U.S. Appl. No. 13/439,528. |
UPPTO; Notice of Allowance dated Oct. 21, 2014 in U.S. Appl. No. 13/439,528. |
USPTO; Non-Final Office Action dated Apr. 11, 2013 in U.S. Appl. No. 13/450,368. |
USPTO; Notice of Allowance dated Jul. 17, 2013 in U.S. Appl. No. 13/450,368. |
USPTO; Office Action dated May 23, 2013 in U.S. Appl. No. 13/465,340. |
USPTO; Final Office Action dated Oct. 30, 2013 in U.S. Appl. No. 13/465,340. |
USPTO; Notice of Allowance dated Feb. 12, 2014 in U.S. Appl. No. 13/465,340. |
USPTO; Non-Final Office Action dated Oct. 17, 2013 in U.S. Appl. No. 13/493,897. |
USPTO; Notice of Allowance dated Mar. 20, 2014 in U.S. Appl. No. 13/493,897. |
USPTO; Office Action dated Dec. 20, 2013 in U.S. Appl. No. 13/535,214. |
USPTO; Final Office Action dated Jun. 18, 2014 in U.S. Appl. No. 13/535,214. |
USPTO; Notice of Allowance dated Oct. 23, 2014 in U.S. Appl. No. 13/535,214. |
USPTO; Non-Final Office Action dated Sep. 11, 2013 in U.S. Appl. No. 13/550,419. |
USPTO; Final Office Action dated Jan. 27, 2014 in U.S. Appl. No. 13/550,419. |
USPTO; Advisory Action dated Mar. 31, 2014 in U.S. Appl. No. 13/550,419. |
USPTO; Notice of Allowance dated May 29, 2014 in U.S. Appl. No. 13/550,419. |
USPTO; Non-Final Office Action dated Aug. 8, 2014 in U.S. Appl. No. 13/563,066. |
USPTO; Final Office Action dated Feb. 12, 2015 in U.S. Appl. No. 13/563,066. |
USPTO; Advisory Action dated Apr. 16, 2015 in U.S. Appl. No. 13/563,066. |
USPTO; Notice of Allowance dated Jun. 12, 2015 in U.S. Appl. No. 13/563,066. |
USPTO; Notice of Allowance dated Jul. 16, 2015 in U.S. Appl. No. 13/563,066. |
USPTO; Non-Final Office Action dated May 28, 2013in U.S. Appl. No. 13/563,274. |
USPTO; Notice of Allowance dated Sep. 27, 2013 in U.S. Appl. No. 13/563,274. |
USPTO; Non-Final Office Action dated Nov. 7, 2013 in U.S. Appl. No. 13/565,564. |
USPTO; Final Office Action dated Feb. 28, 2014 in U.S. Appl. No. 13/565,564. |
USPTO; Advisory Action dated May 5, 2014 in U.S. Appl. No. 13/565,564. |
USPTO; Non-Final Office Action dated Jul. 2, 2014 in U.S. Appl. No. 13/565,564. |
USPTO; Notice of Allowance dated Nov. 3, 2014 in U.S. Appl. No. 13/565,564. |
USPTO; Notice of Allowance dated Sep. 13, 2013 in U.S. Appl. No. 13/566,069. |
USPTO; Non-Final Office Action dated Aug. 30, 2013 in U.S. Appl. No. 13/570,067. |
USPTO; Notice of Allowance dated Jan. 6, 2014 in U.S. Appl. No. 13/570,067. |
USPTO; Non-Final Office Action dated Oct. 15, 2014 in U.S. Appl. No. 13/597,043. |
USPTO; Final Office Action dated Mar. 13, 2015 in U.S. Appl. No. 13/597,043. |
USPTO;; Notice of Allowance dated Aug. 28, 2015 in U.S. Appl. No. 13/597,043. |
USPTO; Non-Final Office Action dated Feb. 12, 2015 in U.S. Appl. No. 13/597,108. |
USPTO; Final Office Action dated Jun. 1, 2015 in U.S. Appl. No. 13/597,108. |
USPTO; Advisory Action dated Sep. 2, 2015 in U.S. Appl. No. 13/597,108. |
USPTO; Non-Final Office Action dated Dec. 8, 2015 in U.S. Appl. No. 13/597,108. |
USPTO; Final Office Action dated Jun. 2, 2016 in U.S. Appl. No. 13/597,108. |
USPTO; Non-Final Office Action dated Sep. 15, 2016 in U.S. Appl. No. 13/597,108. |
USPTO; Notice of Allowance dated Mar. 7, 2017 in U.S. Appl. No. 13/597,108. |
USPTO; Notice of Allowance dated Mar. 27, 2014 in U.S. Appl. No. 13/604,498. |
USPTO; Restriction Requirement dated Jul. 9, 2013 in U.S. Appl. No. 13/612,538. |
USPTO; Office Action dated Nov. 15, 2013 in U.S. Appl. No. 13/612,538. |
USPTO; Office Action dated Jul. 10, 2014 in U.S. Appl. No. 13/612,538. |
USPTO; Notice of Allowance dated Feb. 25, 2015 in U.S. Appl. No. 13/612,538. |
USPTO; Requirement for Restriction dated Feb. 4, 2015 in U.S. Appl. No. 13/646,403. |
USPTO; Non-Final Office Action dated Apr. 15, 2015 in U.S. Appl. No. 13/646,403. |
USPTO; Final Office Action dated Oct. 15, 2015 in U.S. Appl. No. 13/646,403. |
USPTO; Notice of Allowance dated Feb. 2, 2016 in U.S. Appl. No. 13/646,403. |
USPTO; Requirement for Restriction dated Apr. 11, 2014 in U.S. Appl. No. 13/646,471. |
USPTO; Non-Final Office Action dated May 15, 2014 in U.S. Appl. No. 13/646,471. |
USPTO; Final Office Action dated Aug. 18, 2014 in U.S. Appl. No. 13/646,471. |
USPTO; Advisory Action dated Nov. 14, 2014 in U.S. Appl. No. 13/646,471. |
USPTO; Non-Final Office Action dated Dec. 16, 2014 in U.S. Appl. No. 13/646,471. |
USPTO; Final Office Action dated Apr. 21, 2015 in U.S. Appl. No. 13/646,471. |
USPTO; Non-Final Office Action dated Aug. 19, 2015 in U.S. Appl. No. 13/646,471. |
USPTO; Final Office Action dated Jan. 22, 2016 in U.S. Appl. No. 13/646,471. |
USPTO; Advisory Action dated Apr. 15, 2016 in U.S. Appl. No. 13/646,471. |
USPTO; Non-Final Office Action dated Jun. 2, 2016 in U.S. Appl. No. 13/646,471. |
USPTO; Final Office Action dated Oct. 20, 2016 in U.S. Appl. No. 13/646,471. |
USPTO; Restriction Requirement dated Mar. 4, 2015 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated May 28, 2015 in U.S. Appl. No. 13/651,144. |
USPTO; Final Office Action dated Dec. 14, 2017 in U.S. Appl. No. 13/651,144. |
USPTO; Final Office Action dated Nov. 19, 2015 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated May 10, 2016 in U.S. Appl. No. 13/651,144. |
USPTO; Final Office Action dated Sep. 20, 2016 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated May 17, 2017 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated Dec. 14, 2017 in U.S. Appl. No. 13/651,144. |
USPTO; Advisory Action dated Apr. 19, 2018 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated Nov. 19, 2015 in U.S. Appl. No. 14/659,437. |
USPTO; Final Office Action dated Mar. 17, 2016 in U.S. Appl. No. 14/659,437. |
USPTO; Notice of Allowance dated May 31, 2016 in U.S. Appl. No. 14/659,437. |
USPTO; Requirement for Restriction dated Dec. 24, 2014 in U.S. Appl. No. 13/665,366. |
USPTO; Non-Final Office Action dated Jun. 18, 2015 in U.S. Appl. No. 13/665,366. |
USPTO; Final Office Action dated Mar. 1, 2016 in U.S. Appl. No. 13/665,366. |
USPTO; Advisory Action dated May 13, 2016 in U.S. Appl. No. 13/665,366. |
USPTO; Non-Final Office Action dated Jun. 17, 2016 in U.S. Appl. No. 13/665,366. |
USPTO; Final Office Action dated May 3, 2017 in U.S. Appl. No. 13/665,366. |
USPTO; Non-Final Office Action dated Apr. 3, 2015 in U.S. Appl. No. 13/677,133. |
USPTO; Notice of Allowance dated Aug. 4, 2015 in U.S. Appl. No. 13/677,133. |
USPTO; Notice of Allowance dated Aug. 24, 2015 in U.S. Appl. No. 13/677,133. |
USPTO; Office Action dated Jun. 2, 2014 in U.S. Appl. No. 13/677,151. |
USPTO; Final Office Action dated Nov. 14, 2014 in U.S. Appl. No. 13/677,151. |
USPTO; Notice of Allowance dated Feb. 26, 2015 in U.S. Appl. No. 13/677,151. |
USPTO; Notice of Allowance dated Mar. 17, 2015 in U.S. Appl. No. 13/677,151. |
USPTO; Non-Final Office Action dated Aug. 20, 2013 in U.S. Appl. No. 13/679,502. |
USPTO; Final Office Action dated Feb. 25, 2014 in U.S. Appl. No. 13/679,502. |
USPTO; Notice of Allowance dated May 2, 2014 in U.S. Appl. No. 13/679,502. |
USPTO; Non-Final Office Action dated Jul. 21, 2015 in U.S. Appl. No. 13/727,324. |
USPTO; Final Office Action dated Jan. 22, 2016 in U.S. Appl. No. 13/727,324. |
USPTO; Advisory Action dated Apr. 6, 2016 in U.S. Appl. No. 13/727,324. |
USPTO; Non-Final Office Action dated May 25, 206 in U.S. Appl. No. 13/727,324. |
USPTO; Final Office Action dated Dec. 1, 2016 in U.S. Appl. No. 13/727,324. |
USPTO; Notice of Allowance dated Mar. 1, 2017 in U.S. Appl. No. 13/727,324. |
USPTO; Non-Final Office Action dated Oct. 24, 2013 in U.S. Appl. No. 13/749,878. |
USPTO; Non-Final Office Action dated Jun. 18, 2014 in U.S. Appl. No. 13/749,878. |
USPTO; Final Office Action dated Dec. 10, 2014 in U.S. Appl. No. 13/749,878. |
USPTO; Notice of Allowance Mar. 13, 2015 dated in U.S. Appl. No. 13/749,878. |
USPTO; Non-Final Office Action dated Sep. 16, 2013 in U.S. Appl. No. 13/760,160. |
USPTO; Final Office Action dated Dec. 27, 2013 in U.S. Appl. No. 13/760,160. |
USPTO; Non-Final Office Action dated Jun. 4, 2014 in U.S. Appl. No. 13/760,160. |
USPTO; Final Office Action dated Sep. 25, 2014 in U.S. Appl. No. 13/760,160. |
USPTO; Final Office Action dated Jan. 28, 2015 in U.S. Appl. No. 13/760,160. |
USPTO; Final Office Action dated May 12, 2015 in U.S. Appl. No. 13/760,160. |
USPTO; Notice of Allowance dated Oct. 21, 2015 in U.S. Appl. No. 13/760,160. |
USPTO; Notice of Allowance dated Jan. 20, 2016 in U.S. Appl. No. 13/760,160. |
USPTO; Office Action dated Apr. 23, 2014 in U.S. Appl. No. 13/784,362. |
USPTO; Notice of Allowance dated Aug. 13, 2014 in U.S. Appl. No. 13/784,362. |
USPTO; Non-Final Office Action dated Dec. 19, 2013 in U.S. Appl. No. 13/784,388. |
USPTO; Notice of Allowance dated Jun. 4, 2014 in U.S. Appl. No. 13/784,388. |
USPTO; Restriction Requirement dated May 8, 2014 in U.S. Appl. No. 13/791,246. |
USPTO; Non-Final Office Action dated Sep. 19, 2014 in U.S. Appl. No. 13/791,246. |
USPTO; Final Office Action dated Mar. 25, 2015 in U.S. Appl. No. 13/791,246. |
USPTO; Non-Final Office Action dated Oct. 26, 2015 in U.S. Appl. No. 13/791,246. |
USPTO; Final Office Action dated Apr. 20, 2016 in U.S. Appl. No. 13/791,246. |
USPTO; Advisory Action dated Jul. 13, 2016 in U.S. Appl. No. 13/791,246. |
USPTO; Non-Final Office Action dated Aug. 11, 2016 in U.S. Appl. No. 13/791,246. |
USPTO; Notice of Allowance dated Oct. 19, 2016 in U.S. Appl. No. 13/791,246. |
USPTO; Notice of Allowance dated Nov. 25, 2016 in U.S. Appl. No. 13/791,246. |
USPTO; Non-Final Office Action dated Nov. 6, 2015 in U.S. Appl. No. 13/791,339. |
USPTO; Final Office Action dated Apr. 12, 2016 in U.S. Appl. No. 13/791,339. |
USPTO; Advisory Action dated Jul. 14, 2016 in U.S. Appl. No. 13/791,339. |
USPTO; Notice of Allowance dated Aug. 24, 2016 in U.S. Appl. No. 13/791,339. |
USPTO; Non-Final Office Action dated Mar. 21, 2014 in U.S. Appl. No. 13/799,708. |
USPTO; Notice of Allowance dated Oct. 31, 2014 in U.S. Appl. No. 13/799,708. |
USPTO; Non-Final Office Action dated Sep. 1, 2016 in U.S. Appl. No. 14/827,177. |
USPTO; Restriction Requirement dated Jun. 26, 2014 in U.S. Appl. No. 13/874,708. |
USPTO; Non-Final Office Action dated Oct. 9, 2014 in U.S. Appl. No. 13/874,708. |
USPTO; Notice of Allowance dated Mar. 10, 2015 in U.S. Appl. No. 13/874,708. |
USPTO; Notice of Allowance dated Apr. 10, 2014 in U.S. Appl. No. 13/901,341. |
USPTO; Notice of Allowance dated Jun. 6, 2014 in U.S. Appl. No. 13/901,341. |
USPTO; Non-Final Office Action dated Jan. 2, 2015 in U.S. Appl. No. 13/901,372. |
USPTO; Final Office Action dated Apr. 16, 2015 in U.S. Appl. No. 13/901,372. |
USPTO; Notice of Allowance dated Aug. 5, 2015 in U.S. Appl. No. 13/901,372. |
USPTO; Advisory Action dated Jun. 29, 2015 in U.S. Appl. No. 13/901,372. |
USPTO; Non-Final Office Action dated Jul. 8, 2015 in U.S. Appl. No. 13/901,400. |
USPTO; Final Office Action dated Jan. 14, 2016 in U.S. Appl. No. 13/901,400. |
USPTO; Notice of Allowance dated Apr. 12, 2016 in U.S. Appl. No. 13/901,400. |
USPTO; Non-Final Office Action dated Apr. 24, 2014 in U.S. Appl. No. 13/912,666. |
USPTO; Final Office Action dated Sep. 25, 2014 in U.S. Appl. No. 13/912,666. |
USPTO; Advisory Action dated Dec. 11, 2014 in U.S. Appl. No. 13/912,666. |
USPTO; Non-Final Office Action dated Jan. 26, 2015 in U.S. Appl. No. 13/912,666. |
USPTO; Notice of Allowance dated Jun. 25, 2015 in U.S. Appl. No. 13/912,666. |
USPTO; Requirement for Restriction dated Sep. 4, 2014 in U.S. Appl. No. 13/915,732. |
USPTO; Non-Final Office Action dated Dec. 16, 2014 in U.S. Appl. No. 13/915,732. |
USPTO; Final Office Action dated Apr. 10, 2015 in U.S. Appl. No. 13/915,732. |
USPTO; Notice of Allowance dated Jun. 19, 2015 in U.S. Appl. No. 13/915,732. |
USPTO; Notice of Allowance dated Mar. 17, 2015 in U.S. Appl. No. 13/923,197. |
USPTO; Non-Final Office Action dated Sep. 12, 2014 in U.S. Appl. No. 13/941,134. |
USPTO; Notice of Allowance dated Jan. 20, 2015 in U.S. Appl. No. 13/941,134. |
USPTO; Restriction Requirement dated Apr. 30, 2015 in U.S. Appl. No. 13/941,216. |
USPTO; Non-Final Office Action dated Jul. 30, 2015 in U.S. Appl. No. 13/941,216. |
USPTO; Final Office Action dated Mar. 1, 2016 in U.S. Appl. No. 13/941,216. |
USPTO; Non-Final Office Action dated Jun. 15, 2016 in U.S. Appl. No. 13/941,216. |
USPTO; Notice of Allowance dated Sep. 13, 2016 in U.S. Appl. No. 13/941,216. |
USPTO; Notice of Allowance dated Nov. 14, 2016 in U.S. Appl. No. 13/941,216. |
USPTO; Non-Final Office Action dated Jan. 14, 2014 in U.S. Appl. No. 13/941,226. |
USPTO; Non-Final Office Action dated Jul. 8, 2014 in U.S. Appl. No. 13/941,226. |
USPTO; Non-Final Office Action dated Feb. 3, 2015 in U.S. Appl. No. 13/941,226. |
USPTO; Final Office Action dated Feb. 12, 2016 in U.S. Appl. No. 13/941,226. |
USPTO; Advisory Action dated Jul. 29, 2016 in U.S. Appl. No. 13/941,226. |
USPTO; Non-Final Office Action dated Aug. 8, 2017 in U.S. Appl. No. 13/941,226. |
USPTO; Restriction Requirement dated Sep. 16, 2014 in U.S. Appl. No. 13/948,055. |
USPTO; Non-Final Office Action dated Oct. 30, 2014 in U.S. Appl. No. 13/948,055. |
USPTO; Notice of Allowance dated Feb. 27, 2015 in U.S. Appl. No. 13/948,055. |
USPTO; Notice of Allowance dated Mar. 31, 2015 in U.S. Appl. No. 13/948,055. |
USPTO; Non-Final Office Action dated Jun. 29, 2015 in U.S. Appl. No. 13/966,782. |
USPTO; Final Office Action dated Jan. 4, 2016 in U.S. Appl. No. 13/966,782. |
USPTO; Notice of Allowance dated Mar. 21, 2016 in U.S. Appl. No. 13/966,782. |
USPTO; Notice of Allowance dated Oct. 7, 2015 in U.S. Appl. No. 13/973,777. |
USPTO; Non-Final Office Action dated Feb. 20, 2015 in U.S. Appl. No. 14/018,231. |
USPTO; Notice of Allowance dated Jul. 20, 2015 in U.S. Appl. No. 14/018,231. |
USPTO; Restriction Requirement Action dated Jan. 28, 2015 in U.S. Appl. No. 14/018,345. |
USPTO; Non-Final Office Action dated Apr. 7, 2015 in U.S. Appl. No. 14/018,345. |
USPTO; Final Office Action dated Sep. 14, 2015 in U.S. Appl. No. 14/018,345. |
USPTO; Notice of Allowance dated Jan. 14, 2016 in U.S. Appl. No. 14/018,345. |
USPTO; Notice of Allowance dated Mar. 17, 2016 in U.S. Appl. No. 14/018,345. |
USPTO; Non-Final Office Action dated Mar. 26, 2015 in U.S. Appl. No. 14/031,982. |
USPTO; Final Office Action dated Aug. 28, 2015 in U.S. Appl. No. 14/031,982. |
USPTO; Notice of Allowance dated Nov. 17, 2015 in U.S. Appl. No. 14/031,982. |
USPTO; Non-Final Office Action Restriction dated Jan. 2, 2015 in U.S. Appl. No. 14/040,196. |
USPTO; Non-Final Office Action dated Apr. 28, 2015 in U.S. Appl. No. 14/040,196. |
USPTO; Notice of Allowance dated Sep. 11, 2015 in U.S. Appl. No. 14/040,196. |
USPTO; Non-Final Action dated Dec. 3, 2015 in U.S. Appl. No. 14/050,150. |
USPTO; Final Office Action dated Jun. 15, 2016 in U.S. Appl. No. 14/050,150. |
USPTO; Final Office Action dated Jul. 8, 2016 in U.S. Appl. No. 14/050,150. |
USPTO; Notice of Allowance dated Oct. 20, 2016 in U.S. Appl. No. 14/050,150. |
USPTO; Non-Final Office Action dated Dec. 15, 2014 in U.S. Appl. No. 14/065,114. |
USPTO; Final Office Action dated Jun. 19, 2015 in U.S. Appl. No. 14/065,114. |
USPTO; Advisory Action dated Aug. 24, 2015 in U.S. Appl. No. 14/065,114. |
USPTO; Non-Final Office Action dated Oct. 7, 2015 in U.S. Appl. No. 14/065,114. |
USPTO; Notice of Allowance dated Feb. 22, 2016 in U.S. Appl. No. 14/065,114. |
USPTO; Non-Final Office Action dated Nov. 14, 2014 in U.S. Appl. No. 14/069,244. |
USPTO; Notice of Allowance dated Mar. 25, 2015 in U.S. Appl. No. 14/069,244. |
USPTO; Non-Final Office Action dated Mar. 19, 2015 in U.S. Appl. No. 14/079,302. |
USPTO; Final Office Action dated Sep. 1, 2015 in U.S. Appl. No. 14/079,302. |
USPTO; Non-Final Office Action dated Dec. 23, 2015 in U.S. Appl. No. 14/079,302. |
USPTO; Non-Final Office Action dated Apr. 27, 2016 in U.S. Appl. No. 14/079,302. |
USPTO; Final Office Action dated Aug. 22, 2016 in U.S. Appl. No. 14/079,302. |
USPTO; Notice of Allowance dated Dec. 14, 2016 in U.S. Appl. No. 14/079,302. |
USPTO; Requirement for Restriction dated Aug. 11, 2015 in U.S. Appl. No. 14/090,750. |
USPTO; Non-Final Office Action dated Sep. 9, 2015 in U.S. Appl. No. 14/090,750. |
USPTO; Final Office Action dated Feb. 11, 2016 in U.S. Appl. No. 14/090,750. |
USPTO; Advisory Action dated May 5, 2016 in U.S. Appl. No. 14/090,750. |
USPTO; Non-Final Office Action dated Jun. 14, 2016 in U.S. Appl. No. 14/090,750. |
USPTO; Advisory Action dated Dec. 21, 2016 in U.S. Appl. No. 14/090,750. |
USPTO; Advisory Action dated Jan. 30, 2018 in U.S. Appl. No. 14/090,750. |
USPTO; Final Office Action dated Sep. 28, 2016 in U.S. Appl. No. 14/090,750. |
USPTO; Non Final Office Action dated Jun. 23, 2017 in U.S. Appl. No. 14/090,750. |
USPTO; Final Office Action dated Nov. 17, 2017 in U.S. Appl. No. 14/090,750. |
USPTO; Non-Final Office Action dated Mar. 12, 2018 in U.S. Appl. No. 14/090,750. |
USPTO; Non-Final Office Action dated Mar. 19, 2015 in U.S. Appl. No. 14/166,462. |
USPTO; Notice of Allowance dated Sep. 3, 2015 in U.S. Appl. No. 14/166,462. |
USPTO; Non-Final Office Action dated Nov. 17, 2015 in U.S. Appl. No. 14/172,220. |
USPTO; Office Action dated May 29, 2014 in U.S. Appl. No. 14/183,187. |
USPTO; Final Office Action dated Nov. 7, 2014 in U.S. Appl. No. 14/183,187. |
USPTO; Advisory Action dated Feb. 20, 2015 in U.S. Appl. No. 14/183,187. |
USPTO; Non-Final Office Action dated Mar. 16, 2015 in U.S. Appl. No. 14/183,187. |
USPTO; Final Office Action dated Jul. 10, 2015 in U.S. Appl. No. 14/183,187. |
USPTO; Notice of Allowance dated Aug. 31, 2015 in U.S. Appl. No. 14/183,187. |
USPTO; Requirement for Restriction dated Sep. 24, 2015 in U.S. Appl. No. 14/188,760. |
USPTO; Non-Final Office Action dated Jan. 11, 2016 in U.S. Appl. No. 14/188,760. |
USPTO; Final Office Action dated Aug. 25, 2016 in U.S. Appl. No. 14/188,760. |
USPTO; Advisory Action dated Jan. 12, 2017 in U.S. Appl. No. 14/188,760. |
USPTO; Non-Final Office Action dated Mar. 23, 2017 in U.S. Appl. No. 14/188,760. |
USPTO; Final Office Action dated Oct. 5, 2017 in U.S. Appl. No. 14/188,760. |
USPTO; Advisory Action dated Jan. 3, 2018 in U.S. Appl. No. 14/188,760. |
USPTO; Non-Final Office Action dated Apr. 18, 2018 in U.S. Appl. No. 14/188,760. |
USPTO; Non-Final Office Action dated Oct. 8, 2015 in U.S. Appl. No. 14/218,374. |
USPTO; Final Office Action dated Feb. 23, 2016 in U.S. Appl. No. 14/218,374. |
USPTO; Advisory Action dated Apr. 29, 2016 in U.S. Appl. No. 14/218,374. |
USPTO; Notice of Allowance dated Aug. 5, 2016 in U.S. Appl. No. 14/218,374. |
USPTO; Restriction Requirement dated May 20, 2016 in U.S. Appl. No. 14/218,690. |
USPTO; Non-Final Office Action dated Jul. 15, 2016 in U.S. Appl. No. 14/218,690. |
USPTO; Final Office Action dated Nov. 14, 2016 in U.S. Appl. No. 14/218,690. |
USPTO; Non-Final Office Action dated Apr. 6, 2017 in U.S. Appl. No. 14/218,690. |
USPTO; Final Office Action dated Jul. 20, 2017 in U.S. Appl. No. 14/218,690. |
USPTO; Non-Final Office Action dated Jan. 11, 2018 in U.S. Appl. No. 14/218,690. |
USPTO; Final Office Action dated May 24, 2018 in U.S. Appl. No. 14/218,690. |
USPTO; Non-Final Office Action dated Sep. 22, 2015 in U.S. Appl. No. 14/219,839. |
USPTO; Final Office Action dated Mar. 25, 2016 in U.S. Appl. No. 14/219,839. |
USPTO; Non-Final Office Action dated Dec. 22, 2016 in U.S. Appl. No. 14/219,839. |
USPTO; Advisory Action dated Jun. 30, 2016 in U.S. Appl. No. 14/219,839. |
USPTO; Final Office Action dated Jul. 6, 2017 in U.S. Appl. No. 14/219,839. |
USPTO; Non-Final Office Action dated Mar. 27, 2018 in U.S. Appl. No. 14/219,839. |
USPTO; Non-Final Office Action dated Nov. 25, 2015 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office action dated May 19, 2016 in U.S. Appl. No. 14/219,879. |
USPTO; Advisory Action dated Aug. 22, 2016 in U.S. Appl. No. 14/219,879. |
USPTO; Non-Final Office Action dated Dec. 23, 2016 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office action dated Jul. 6, 2017 in U.S. Appl. No. 14/219,879. |
USPTO; Advisory Action dated Oct. 5, 2017 in U.S. Appl. No. 14/219,879. |
USPTO; Non-Final Office Action dated Apr. 6, 2018 in U.S. Appl. No. 14/219,879. |
USPTO; Non-Final Office Action dated Sep. 18, 2015 in U.S. Appl. No. 14/244,689. |
USPTO; Notice of Allowance dated Feb. 11, 2016 in U.S. Appl. No. 14/244,689. |
USPTO; Non-Final Office Action dated Oct. 7, 2015 in U.S. Appl. No. 14/246,969. |
USPTO; Final Office Action dated May 4, 2016 in U.S. Appl. No. 14/246,969. |
USPTO; Advisory Action dated Aug. 2, 2016 in U.S. Appl. No. 14/246,969. |
USPTO; Non Final Office Action dated Aug. 12, 2016 in U.S. Appl. No. 14/246,969. |
USPTO; Notice of Allowance dated Feb. 27, 2017 in U.S. Appl. No. 14/246,969. |
USPTO; Non-Final Office Action dated Nov. 20, 2015 in U.S. Appl. No. 14/260,701. |
USPTO; Notice of Allowance dated Jun. 2, 2016 in U.S. Appl. No. 14/260,701. |
USPTO; Notice of Allowance dated Feb. 23, 2016 in U.S. Appl. No. 14/327,134. |
USPTO; Requirement for Restriction dated Jun. 15, 2015 in U.S. Appl. No. 14/268,348. |
USPTO; Non-Final Office Action dated Aug. 19, 2015 in U.S. Appl. No. 14/268,348. |
USPTO; Non-Final Office Action dated Jan. 6, 2016 in U.S. Appl. No. 14/268,348. |
USPTO; Final Office Action dated Apr. 29, 2016 in U.S. Appl. No. 14/268,348. |
USPTO; Notice of Allowance dated Aug. 30, 2016 in U.S. Appl. No. 14/268,348. |
USPTO; Requirement for Restriction dated May 21, 2015 in U.S. Appl. No. 14/281,477. |
USPTO; Non-Final Office Action dated Oct. 20, 2015 in U.S. Appl. No. 14/281,477. |
USPTO; Advisory Action dated Mar. 28, 2016 in U.S. Appl. No. 14/281,477. |
USPTO; Non-Final Office Action dated Jan. 13, 2017 in U.S. Appl. No. 14/444,744. |
USPTO; Final Office Action dated Jul. 10, 2017 in U.S. Appl. No. 14/444,744. |
USPTO; Non-Final Office Action dated Nov. 29, 2017 in U.S. Appl. No. 14/444,744. |
USPTO; Final Office Action dated Mar. 28, 2018 in U.S. Appl. No. 14/444,744. |
USPTO; Non-Final Office Action dated Jul. 27, 2018 in U.S. Appl. No. 14/444,744. |
USPTO; Non-Final Office Action dated May 18, 2016 in U.S. Appl. No. 14/449,838. |
USPTO; Notice of Allowance dated Nov. 28, 2016 in U.S. Appl. No. 14/449,838. |
USPTO; Non-Final Office Action dated Feb. 12, 2015 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Action dated Jul. 14, 2015 in U.S. Appl. No. 14/457,058. |
USPTO; Non-Final Office Action dated Nov. 6, 2015 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Acton dated Jun. 17, 2016 in U.S. Appl. No. 14/457,058. |
USPTO; Advisory Action dated Sep. 21, 2016 in U.S. Appl. No. 14/457,058. |
USPTO; Non-Final Office Action dated Oct. 6, 2016 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Acton dated May 4, 2017 in U.S. Appl. No. 14/457,058. |
USPTO; Non-Final Office Action dated Oct. 19, 2017 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Action dated Jun. 14, 2018 in U.S. Appl. No. 14/457,058. |
USPTO; Non-Final Office Action dated Sep. 16, 2016 in U.S. Appl. No. 14/465,252. |
USPTO; Final Office Action dated Nov. 1, 2016 in U.S. Appl. No. 14/465,252. |
USPTO; Non-Final Office Action dated Mar. 6, 2017 in U.S. Appl. No. 14/465,252. |
USPTO; Final Office Action dated Jun. 9, 2017 in U.S. Appl. No. 14/465,252. |
USPTO; Notice of Allowance dated Oct. 3, 2017 in U.S. Appl. No. 14/465,252. |
USPTO; Non-Final Office Action dated May 31, 2018 in U.S. Appl. No. 15/491,726. |
USPTO; Requirement for Restriction dated Sep. 3, 2015 in U.S. Appl. No. 14/498,036. |
USPTO; Non-Final Office Action dated Nov. 24, 2015 in U.S. Appl. No. 14/498,036. |
USPTO; Final Office Action dated Apr. 5, 2016 in U.S. Appl. No. 14/498,036. |
USPTO; Advisory Action dated Jun. 16, 2016 in U.S. Appl. No. 14/498,036. |
USPTO; Notice of Allowance dated Aug. 17, 2016 in U.S. Appl. No. 14/498,036. |
USPTO; Requirement for Restriction dated Mar. 20, 2015 in U.S. Appl. No. 14/505,290. |
USPTO; Non-Final Office Action dated Apr. 10, 2015 in U.S. Appl. No. 14/505,290. |
USPTO; Notice of Allowance dated Aug. 21, 2015 in U.S. Appl. No. 14/505,290. |
USPTO; Non-Final Office Action dated Dec. 17, 2015 in U.S. Appl. No. 14/508,296. |
USPTO; Final Office Action dated May 26, 2016 in U.S. Appl. No. 14/508,296. |
USPTO; Advisory Action dated Aug. 17, 2016 in U.S. Appl. No. 14/508,296. |
USPTO; Non-Final Office Action dated Sep. 8, 2016 in U.S. Appl. No. 14/508,296. |
USPTO; Final Office Action dated Dec. 7, 2016 in U.S. Appl. No. 14/508,296. |
USPTO; Notice of Allowance dated Jan. 27, 2017 in U.S. Appl. No. 14/508,296. |
USPTO; Restriction for Requirement dated Dec. 30, 2016 in U.S. Appl. No. 14/508,489. |
USPTO; Non-Final Office Action dated Apr. 6, 2017 in U.S. Appl. No. 14/508,489. |
USPTO; Final Office Action dated Oct. 4, 2017 in U.S. Appl. No. 14/508,489. |
USPTO; Non-Final Office Action dated May 15, 2018 in U.S. Appl. No. 14/508,489. |
USPTO; Non-Final Office Action dated Jan. 16, 2015 in U.S. Appl. No. 14/563,044. |
USPTO; Final Office Action dated Jul. 16, 2015 in U.S. Appl. No. 14/563,044. |
USPTO; Notice of Allowance dated Oct. 15, 2015 in U.S. Appl. No. 14/563,044. |
USPTO; Notice of Allowance dated Dec. 2, 2015 in U.S. Appl. No. 14/563,044. |
USPTO; Non-Final Office Action dated May 4, 2016 in U.S. Appl. No. 14/568,647. |
USPTO; Final Office Action dated Sep. 29, 2016 in U.S. Appl. No. 14/568,647. |
USPTO; Advisory Action dated Dec. 21, 2016 in U.S. Appl. No. 14/568,647. |
USPTO; Non-Final Office Action dated Feb. 2, 2017 in U.S. Appl. No. 14/568,647. |
USPTO; Final Office Action dated May 19, 2017 in U.S. Appl. No. 14/568,647. |
USPTO; Non-Final Office Action dated Sep. 14, 2017 in U.S. Appl. No. 14/568,647. |
USPTO; Final Office Action dated Jan. 23, 2018 in U.S. Appl. No. 14/568,647. |
USPTO; Advisory Action dated Apr. 12, 2018 in U.S. Appl. No. 14/568,647. |
USPTO; Non-Final Office Action dated May 25, 2018 in U.S. Appl. No. 14/568,647. |
USPTO; Non-Final Office Action dated Oct. 1, 2015 in U.S. Appl. No. 14/571,126. |
USPTO; Final Office Action dated Feb. 22, 2016 in U.S. Appl. No. 14/571,126. |
USPTO; Notice of Allowance dated May 18, 2016 in U.S. Appl. No. 14/571,126. |
USPTO; Notice of Allowance dated Jun. 2, 2016 in U.S. Appl. No. 14/571,126. |
USPTO; Non-Final Office Action dated Nov. 25, 2015 in U.S. Appl. No. 14/598,532. |
USPTO; Notice of Allowance dated May 16, 2016 in U.S. Appl. No. 14/598,532. |
USPTO; Non-Final Office Action dated Jan. 15, 2016 in U.S. Appl. No. 14/606,364. |
USPTO; Restriction Requirement dated Mar. 7, 2016 in U.S. Appl. No. 14/606,364. |
USPTO; Final Office Action dated Jun. 14, 2016 in U.S. Appl. No. 14/606,364. |
USPTO; Advisory Action dated Aug. 25, 2016 in U.S. Appl. No. 14/606,364. |
USPTO; Non-Final Office Action dated Sep. 27, 2016 in U.S. Appl. No. 14/606,354. |
USPTO; Final Office Action dated Jan. 12, 2017 in U.S. Appl. No. 14/606,364. |
USPTO; Non-Final Office Action dated May 10, 2017 in U.S. Appl. No. 14/606,364. |
USPTO; Non-Final Office Action dated Mar. 3, 2016 in U.S. Appl. No. 14/622,603. |
USPTO; Notice of Allowance dated Aug. 2, 2016 in U.S. Appl. No. 14/622,603. |
USPTO; Notice of Allowance dated Feb. 16, 2016 in U.S. Appl. No. 14/634,342. |
USPTO; Non-Final Office Action dated Oct. 19, 2017 in U.S. Appl. No. 14/645,234. |
USPTO; Non-Final Office Action dated May 16, 2018 in U.S. Appl. No. 14/645,234. |
USPTO; Final Office Action dated Aug. 10, 2018 in U.S. Appl. No. 14/645,234. |
USPTO; Non-Final Office Action dated Jun. 7, 2017 in U.S. Appl. No. 14/656,588. |
USPTO; Final Office Action dated Dec. 26, 2017 in U.S. Appl. No. 14/656,588. |
USPTO; Non-Final Office Action dated Apr. 6, 2018 in U.S. Appl. No. 14/656,588. |
USPTO; Requirement for Restriction dated Oct. 26, 2015 in U.S. Appl. No. 14/659,152. |
USPTO; Non-Final Office Action dated Mar. 21, 2016 in U.S. Appl. No. 14/659,152. |
USPTO; Final Office Action dated Jul. 29, 2016 in U.S. Appl. No. 14/659,152. |
USPTO; Notice of Allowance dated Nov. 22, 2016 in U.S. Appl. No. 14/659,152. |
USPTO; Non-Final Office Action dated Sep. 7, 2017 in U.S. Appl. No. 14/660,755. |
USPTO; Restriction Requirement dated Sep. 11, 2017 in U.S. Appl. No. 14/660,755. |
USPTO; Notice of Allowance dated Oct. 2, 2017 in U.S. Appl. No. 14/660,755. |
USPTO; Notice of Allowance dated Mar. 25, 2016 in U.S. Appl. No. 14/693,138. |
USPTO; Requirement for Restriction dated Jul. 5, 2017 in U.S. Appl. No. 14/752,712. |
USPTO; Non-Final Office Action dated Aug. 3, 2017 in U.S. Appl. No. 14/752,712. |
USPTO; Final Office Action dated Nov. 29, 2017 in U.S. Appl. No. 14/752,712. |
USPTO; Advisory Action dated Feb. 15, 2018 in U.S. Appl. No. 14/752,712. |
USPTO; Non-Final Office Action dated Mar. 21, 2018 in U.S. Appl. No. 14/752,712. |
USPTO; Non-Final Office Action dated Nov. 29, 2017 in U.S. Appl. No. 14/793,323. |
USPTO; Final Office Action dated Mar. 29, 2018 in U.S. Appl. No. 14/793,323. |
USPTO; Non-Final Office Action dated Aug. 10, 2018 in U.S. Appl. No. 14/793,323. |
USPTO; Non-Final Office Action dated Jun. 16, 2017 in U.S. Appl. No. 14/798,136. |
USPTO; Notice of Allowance dated Oct. 5, 2017 in U.S. Appl. No. 14/798,136. |
USPTO; Non-Final Office Action dated Mar. 30, 2016 in U.S. Appl. No. 14/808,979. |
USPTO; Final Office Acton dated Sep. 30, 2016 in U.S. Appl. No. 14/808,979. |
USPTO; Non-Final Office Action dated Dec. 20, 2016 in U.S. Appl. No. 14/808,979. |
USPTO; Final Office Action dated Jun. 8, 2017 in U.S. Appl. No. 14/808,979. |
USPTO; Non-Final Office Action dated Sep. 21, 2017 in U.S. Appl. No. 14/808,979. |
USPTO; Final Office Action dated Mar. 14, 2018 in U.S. Appl. No. 14/808,979. |
USPTO; Notice of Allowance dated Jun. 27, 2018 in U.S. Appl. No. 14/808,979. |
USPTO; Non-Final Office Action dated Feb. 23, 2018 in U.S. Appl. No. 14/817,953. |
USPTO; Notice of Allowance dated Jul. 11, 2018 in U.S. Appl. No. 14/817,953. |
USPTO; Requirement for Restriction dated Mar. 17, 2016 in U.S. Appl. No. 14/827,177. |
USPTO; Notice of Allowance dated Jan. 27, 2017 in U.S. Appl. No. 14/827,177. |
USPTO; Requirement for Restriction dated Aug. 8, 2016 in U.S. Appl. No. 14/829,565. |
USPTO; Non-Final Office Action dated Sep. 9, 2016 in U.S. Appl. No. 14/829,565. |
USPTO; Final Office Action dated Feb. 9, 2017 in U.S. Appl. No. 14/829,565. |
USPTO; Advisory Action dated Apr. 20, 2017 in U.S. Appl. No. 14/829,565. |
USPTO; Non-Final Office Action dated Sep. 19, 2017 in U.S. Appl. No. 14/829,565. |
USPTO; Final Office Action dated Mar. 5, 2018 in U.S. Appl. No. 14/829,565. |
USPTO; Non-Final Office Action dated Apr. 29, 2016 in U.S. Appl. No. 14/835,637. |
USPTO; Final Office Action dated Nov. 25, 2016 in U.S. Appl. No. 14/835,637. |
USPTO; Advisory Action dated Feb. 14, 2017 in U.S. Appl. No. 14/835,637. |
USPTO; Notice of Allowance dated Apr. 25, 2017 in U.S. Appl. No. 14/835,637. |
USPTO; Non-Final Office Action dated Jul. 29, 2016 in U.S. Appl. No. 14/884,695. |
USPTO; Final Office Action dated Feb. 9, 2017 in U.S. Appl. No. 14/884,695. |
USPTO; Advisory Action dated Apr. 20, 2017 in U.S. Appl. No. 14/884,695. |
USPTO; Non-Final Office Action dated May 18, 2017 in U.S. Appl. No. 14/884,695. |
USPTO; Requirement for Restriction dated Dec. 1, 2016 in U.S. Appl. No. 14/886,571. |
USPTO; Non-Final Office Action dated May 18, 2017 in U.S. Appl. No. 14/886,571. |
USPTO; Final Office Action dated Sep. 21, 2017 in U.S. Appl. No. 14/886,571. |
USPTO; Notice of Allowance dated Dec. 6, 2017 in U.S. Appl. No. 14/886,571. |
USPTO; Requirement for Restriction dated Sep. 20, 2016 in U.S. Appl. No. 14/919,536. |
USPTO; Non-Final Office Action dated Dec. 1, 2016 in U.S. Appl. No. 14/919,536. |
USPTO; Final Office Action dated Mar. 28, 2017 in U.S. Appl. No. 14/919,536. |
USPTO; Non-Final Office Action dated Aug. 29, 2017 in U.S. Appl. No. 14/919,536. |
USPTO; Final Office Action dated May 11, 2018 in U.S. Appl. No. 14/919,536. |
USPTO; Non-Final Office Action dated May 3, 2016 in U.S. Appl. No. 14/937,053. |
USPTO; Notice of Allowance dated Jul. 26, 2016 in U.S. Appl. No. 14/937,053. |
USPTO; Requirement for Restriction dated Sep. 15, 2016 in U.S. Appl. No. 14/938,180. |
USPTO; Non-Final Office Action dated Dec. 15, 2016 in U.S. Appl. No. 14/938,180. |
USPTO; Notice of Allowance dated Nov. 9, 2017 in U.S. Appl. No. 14/938,180. |
USPTO; Non-Final Office Action dated Apr. 14, 2017 in U.S. Appl. No. 14/956,115. |
USPTO; Final Office Action dated Jul. 21, 2017 in U.S. Appl. No. 14/956,115. |
USPTO; Notice of Allowance dated Dec. 14, 2017 in U.S. Appl. No. 14/956,115. |
USPTO; Notice of Allowance dated Feb. 3, 2017 in U.S. Appl. No. 14/977,291. |
USPTO; Non-Final Office Action dated Aug. 12, 2016 in U.S. Appl. No. 14/981,434. |
USPTO; Notice of Allowance dated Nov. 21, 2016 in U.S. Appl. No. 14/981,434. |
USPTO; Non-Final Office Action dated Jan. 12, 2017 in U.S. Appl. No. 14/981,468. |
USPTO; Notice of Allowance dated Jun. 7, 2017 in U.S. Appl. No. 14/981,468. |
USPTO; Non-Final Office Action dated Mar. 22, 2016 in U.S. Appl. No. 14/987,420. |
USPTO; Non-Final Office Action dated Dec. 14, 2016 in U.S. Appl. No. 14/997,683. |
USPTO; Final Office Action dated Apr. 14, 2017 in U.S. Appl. No. 14/997,683. |
USPTO; Non-Final Office Action dated Sep. 1, 2017 in U.S. Appl. No. 14/997,683. |
USPTO; Final Office Action dated Feb. 6, 2018 in U.S. Appl. No. 14/997,683. |
USPTO; Advisory Action dated May 2, 2018 in U.S. Appl. No. 14/997,683. |
USPTO; Non-Final Office Action dated Jun. 20, 2018 in U.S. Appl. No. 14/997,683. |
USPTO; Non-Final Office Action dated Sep. 23, 2016 in U.S. Appl. No. 15/048,422. |
USPTO; Notice of Allowance dated May 4, 2017 in U.S. Appl. No. 15/048,422. |
USPTO; Requirement for Restriction dated Apr. 19, 2017 in U.S. Appl. No. 15/050,159. |
USPTO; Non-Final Office Action dated Aug. 4, 2017 in U.S. Appl. No. 15/050,159. |
USPTO; Notice of Allowance dated Feb. 7, 2018 in U.S. Appl. No. 15/050,159. |
USPTO; Non-Final Office Action dated Apr. 22, 2016 in U.S. Appl. No. 15/055,122. |
USPTO; Notice of Allowance dated Sep. 15, 2016 in U.S. Appl. No. 15/055,122. |
USPTO; Non-Final Office Action dated Feb. 20, 2018 in U.S. Appl. No. 15/060,412. |
USPTO; Requirement for Restriction dated Jun. 4, 2018 in U.S. Appl. No. 15/067,028. |
USPTO; Requirement for Restriction dated Jun. 28, 2018 in U.S. Appl. No. 15/074,813. |
USPTO; Non-Final Office Action dated Jan. 9, 2018 in U.S. Appl. No. 15/135,224. |
USPTO; Notice of Allowance dated Jun. 29, 2018 in U.S. Appl. No. 15/135,224. |
USPTO; Non-Final Office Action dated Jan. 9, 2018 in U.S. Appl. No. 15/135,258. |
USPTO; Final Office Action dated Jul. 6, 2018 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Jan. 9, 2018 in U.S. Appl. No. 15/135,333. |
USPTO; Non Final Office Action dated Nov. 21, 2016 in U.S. Appl. No. 15/144,481. |
USPTO; Final Office Action dated May 26, 2017 in U.S. Appl. No. 15/144,481. |
USPTO; Non-Final Office Action dated Sep. 21, 2017 in U.S. Appl. No. 15/144,481. |
USPTO; Notice of Allowance dated Apr. 11, 2018 in U.S. Appl. No. 15/144,481. |
USPTO; Non-Final Office Action dated Apr. 13, 2017 in U.S. Appl. No. 15/144,506. |
USPTO; Final Office Action dated Oct. 10, 2017 in U.S. Appl. No. 15/144,506. |
USPTO; Final Office Action dated Jul. 26, 2018 in U.S. Appl. No. 15/144,506. |
USPTO; Requirement for Restriction dated Jun. 22, 2018 in U.S. Appl. No. 15/182,504. |
USPTO; Non-Final Office Action dated Nov. 28, 2016 in U.S. Appl. No. 15/203,632. |
USPTO; Final Office Action dated Jun. 7, 2017 in U.S. Appl. No. 15/203,632. |
USPTO; Advisory Action dated Aug. 23, 2017 in U.S. Appl. No. 15/203,632. |
USPTO; Notice of Allowance dated Sep. 20, 2017 in U.S. Appl. No. 15/203,632. |
USPTO; Non-Final Office Action dated Nov. 29, 2016 in U.S. Appl. No. 15/203,642. |
USPTO; Final Office Action dated Apr. 13, 2017 in U.S. Appl. No. 15/203,642. |
USPTO; Advisory Action dated Jun. 22, 2017 in U.S. Appl. No. 15/203,642. |
USPTO; Notice of Allowance dated Aug. 7, 2017 in U.S. Appl. No. 15/203,642. |
USPTO; Non-Final Office Action dated Jun. 1, 2017 in U.S. Appl. No. 15/205,827. |
USPTO; Final Office Action dated Oct. 16, 2017 in U.S. Appl. No. 15/205,827. |
USPTO; Non-Final Office Action dated May 14, 2018 in U.S. Appl. No. 15/205,827. |
USPTO; Requirement for Restriction dated Jan. 26, 2017 in U.S. Appl. No. 15/205,890. |
USPTO; Non-Final Office Action dated Mar. 31, 2017 in U.S. Appl. No. 15/205,890. |
USPTO; Notice of Allowance dated Oct. 16, 2017 in U.S. Appl. No. 15/205,890. |
USPTO; Non-Final Office Action dated Jan. 20, 2017 in U.S. Appl. No. 15/210,256. |
USPTO; Notice of Allowance dated May 18, 2017 in U.S. Appl. No. 15/210,256. |
USPTO; Notice of Allowance dated Jul. 24, 2017 in U.S. Appl. No. 15/210,256. |
USPTO; Requirement for Restriction dated Apr. 3, 2017 in U.S. Appl. No. 15/222,715. |
USPTO; Non Final Office Action dated Apr. 21, 2017 in U.S. Appl. No. 15/222,715. |
USPTO; Notice of Allowance dated Jul. 14, 2017 in U.S. Appl. No. 15/222,715. |
USPTO; Notice of Allowance dated Sep. 27, 2017 in U.S. Appl. No. 15/222,715. |
USPTO; Non-Final Office Action dated Feb. 3, 2017 in U.S. Appl. No. 15/222,738. |
USPTO; Notice of Allowance dated Feb. 3, 2017 in U.S. Appl. No. 15/222,738. |
USPTO; Notice of Allowance dated Aug. 23, 2017 in U.S. Appl. No. 15/222,738. |
USPTO; Non-Final Office Action dated Jan. 17, 2017 in U.S. Appl. No. 15/222,749. |
USPTO; Final Office Action dated May 5, 2017 in U.S. Appl. No. 15/222,749. |
USPTO; Non-Final Office Action dated Sep. 7, 2017 in U.S. Appl. No. 15/222,749. |
USPTO: Final Office Action dated Jun. 4, 2018 in U.S. Appl. No. 15/222,749. |
USPTO; Non-Final Office Action dated Jan. 3, 2017 in U.S. Appl. No. 15/222,780. |
USPTO; Final Office Action dated May 5, 2017 in U.S. Appl. No. 15/222,780. |
USPTO; Non-Final Office Action dated Sep. 7, 2017 in U.S. Appl. No. 15/222,780. |
USPTO; Final Office Action dated May 17, 2018 in U.S. Appl. No. 15/222,780. |
USPTO; Requirement for Restriction dated Dec. 5, 2017 in U.S. Appl. No. 15/254,605. |
USPTO; Notice of Allowance dated Jul. 12, 2018 in U.S. Appl. No. 15/254,605. |
USPTO; Non-Final Office Action dated Aug. 28, 2017 in U.S. Appl. No. 15/254,724. |
USPTO; Notice of Allowance dated Jan. 17, 2018 in U.S. Appl. No. 15/254,724. |
USPTO; Notice of Allowance dated Apr. 2, 2018 in U.S. Appl. No. 15/254,724. |
USPTO; Non-Final Office Action dated May 22, 2018 in U.S. Appl. No. 15/262,990. |
USPTO; Non-Final Office Action dated Aug. 3, 2018 in U.S. Appl. No. 15/273,488. |
USTPO; Non-Final Office Action dated Jul. 2, 2018 in U.S. Appl. No. 15/286,503. |
USPTO; Requirement for Restriction dated Sep. 12, 2017 in U.S. Appl. No. 15/377,439. |
USPTO; Non-Final Office Action dated Oct. 23, 2017 in U.S. Appl. No. 15/377,439. |
USPTO; Final Office Action dated Apr. 16, 2018 in U.S. Appl. No. 15/377,439. |
USPTO; Advisory Action dated Aug. 8, 2018 in U.S. Appl. No. 15/377,439. |
USPTO; Notice of Allowance dated Aug. 8, 2017 in U.S. Appl. No. 15/380,895. |
USPTO; Notice of Allowance dated Oct. 11, 2017 in U.S. Appl. No. 15/380,895. |
USPTO; Non-Final Office Action dated Jan. 4, 2018 in U.S. Appl. No. 15/380,921. |
USPTO; Requirement for Restriction dated Sep. 21, 2017 in U.S. Appl. No. 15/380,921. |
USPTO; Final Office Action dated Jun. 28, 2018 in U.S. Appl. No. 15/380,921. |
USPTO; Final Office Action dated May 15, 2018 in U.S. Appl. No. 15/388,410. |
USPTO; Non-Final Office Action dated Aug. 11, 2017 in U.S. Appl. No. 15/397,237. |
USPTO; Notice of Allowance dated Dec. 22, 2017 in U.S. Appl. No. 15/397,237. |
USPTO; Non-Final Office Action dated Apr. 12, 2017 in U.S. Appl. No. 15/397,319. |
USPTO; Final Office Action dated Jul. 12, 2017 in U.S. Appl. No. 15/397,319. |
USPTO; Notice of Allowance dated Dec. 15, 2017 in U.S. Appl. No. 15/397,319. |
USPTO; Non-Final Office Action dated Aug. 7, 2018 in U.S. Appl. No. 15/428,808. |
USPTO; Non-Final Office Action dated Apr. 6, 2018 in U.S. Appl. No. 15/434,051. |
USPTO; Notice of Allowance dated Oct. 6, 2017 in U.S. Appl. No. 15/450,199. |
USPTO; Non-Final Office Action dated Dec. 15, 2017 in U.S. Appl. No. 15/466,149. |
USPTO; Notice of Allowance dated Apr. 20, 2018 in U.S. Appl. No. 15/466,149. |
USPTO; Non-Final Office Action dated Oct. 4, 2017 in U.S. Appl. No. 15/489,453. |
USPTO; Final Office Action dated Apr. 19, 2018 in U.S. Appl. No. 15/489,453. |
USPTO; Notice of Allowance dated Dec. 19, 2017 in U.S. Appl. No. 15/489,660. |
USPTO; Non-Final Office Action dated Apr. 6, 2018 in U.S. Appl. No. 15/472,750. |
USPTO; Non-Final Office Action dated Dec. 6, 2017 in U.S. Appl. No. 15/476,035. |
USPTO; Notice of Allowance dated Mar. 21, 2018 in U.S. Appl. No. 15/476,035. |
USPTO; Notice of Allowance dated Aug. 14, 2018 in U.S. Appl. No. 15/476,035. |
USPTO; Non-Final Office Action dated Jan. 16, 2018 in U.S. Appl. No. 15/499,647. |
USPTO; Notice of Allowance dated May 23, 2018 in U.S. Appl. No. 15/499,647. |
USPTO; Non-Final Office Action dated Jun. 21, 2018 in U.S. Appl. No. 15/499,647. |
USPTO; Office Action dated May 3, 2018 in U.S. Appl. No. 15/589,861. |
USPTO; Requirement of Restriction dated Mar. 30, 2018 in U.S. Appl. No. 15/589,849. |
USPTO; Office Action dated Aug. 30, 2018 in U.S. Appl. No. 15/589,849. |
USPTO; Non-Final Office Action dated Apr. 4, 2018 in U.S. Appl. No. 15/592,730. |
USPTO; Requirement for Restriction dated Aug. 1, 2018 in U.S. Appl. No. 15/627,189. |
USPTO; Non-Final Office Action dated Jun. 5, 2018 in U.S. Appl. No. 15/650,686. |
USPTO; Requirement for Restriction dated Apr. 6, 2018 in U.S. Appl. No. 15/659,631. |
USPTO; Non-Final Office Action dated Aug. 9, 2018 in U.S. Appl. No. 15/660,805. |
USPTO; Non-Final Office Action dated Jul. 27, 2018 in U.S. Appl. No. 15/673,110. |
USPTO; Non-Final Office Action dated Apr. 25, 2018 in U.S. Appl. No. 15/673,278. |
USPTO; Non-Final Office Action dated Jan. 18, 2018 in U.S. Appl. No. 15/683,701. |
USPTO; Final Office Action dated Aug. 24, 2018 in U.S. Appl. No. 15/683,701. |
USPTO; Non-Final Office Action dated Aug. 9, 2018 in U.S. Appl. No. 15/691,241. |
USPTO; Requirement for Restriction dated Jul. 11, 2018 in U.S. Appl. No. 15/707,786. |
USPTO; Requirement for Restriction dated May 11, 2018 in U.S. Appl. No. 15/711,989. |
USPTO; Non-Final Office Action dated Jun. 14, 2018 in U.S. Appl. No. 15/711,989. |
USPTO; Non-Final Office Action dated May 29, 2018 in U.S. Appl. No. 15/719,208. |
USPTO; Non-Final Office Action dated Apr. 19, 2018 in U.S. Appl. No. 15/726,959. |
USPTO; Non-Final Office Action dated May 17, 2018 in U.S. Appl. No. 15/729,485. |
USPTO; Non-Final Office Action dated Jun. 26, 2018 in U.S. Appl. No. 15/796,593. |
USPTO; Non-Final Office Action dated Dec. 26, 2017 in U.S. Appl. No. 15/798,120. |
USPTO; Notice of Allowance dated Jun. 13, 2018 in U.S. Appl. No. 15/798,120. |
USPTO; Requirement for Restriction dated Apr. 6, 2018 in U.S. Appl. No. 15/798,201. |
USPTO; Non-Final Office Action dated Aug. 9, 2018 in U.S. Appl. No. 15/798,201. |
USPTO; Non-Final Office Action dated Jul. 2, 2018 in U.S. Appl. No. 15/815,483. |
USPTO; Requirement for Restriction dated Mar. 21, 2018 in U.S. Appl. No. 15/863,340. |
USPTO; Non-Final Office Action dated Jul. 23, 2018 in U.S. Appl. No. 15/863,340. |
USPTO; Notice of Allowance dated May 14, 2012 in U.S. Appl. No. 29/411,637. |
USPTO; Notice of Allowance dated Oct. 2, 2013 in U.S. Appl. No. 29/412,887. |
USPTO; Non-Final Office Action dated Mar. 16, 2015 in U.S. Appl. No. 29/447,298. |
USPTO; Notice of Allowance dated Jul. 6, 2015 in U.S. Appl. No. 29/447,298. |
USPTO; Notice of Allowance dated Dec. 19, 2013 in U.S. Appl. No. 29/448,094. |
USPTO; Notice of Allowance dated Nov. 26, 2014 in U.S. Appl. No. 29/481,301. |
USPTO; Notice of Allowance dated Feb. 17, 2015 in U.S. Appl. No. 29/481,308. |
USPTO; Requirement for Restriction dated Dec. 1, 2014 in U.S. Appl. No. 29/481,312. |
USPTO; Notice of Allowance dated Jan. 12, 2015 in U.S. Appl. No. 29/481,312. |
USPTO; Requirement for Restriction dated Dec. 4, 2014 in U.S. Appl. No. 29/481,315. |
USPTO; Notice of Allowance dated Apr. 30, 2015 in U.S. Appl. No. 29/481,315. |
USPTO; Notice of Allowance dated May 11, 2015 in U.S. Appl. No. 29/511,011. |
USPTO; Notice of Allowance dated May 11, 2015 in U.S. Appl. No. 29/514,153. |
USPTO; Notice of Allowance dated Dec. 14, 2015 in U.S. Appl. No. 29/514,264. |
USPTO; Notice of Allowance dated Jun. 16, 2017 in U.S. Appl. No. 29/570,711. |
USPTO; Notice of Allowance dated Jun. 26, 2018 in U.S. Appl. No. 29/604,288. |
PCT; International Preliminary Report on Patentability dated Nov. 24, 2009 and International Search Report dated Jul. 31, 2008 in Application No. PCT/US2008/063919. |
PCT; International Preliminary Report on Patentability dated Feb. 24, 2010 in Application No. PCT/US2008/074063. |
PCT; International Preliminary Report on Patentability dated Nov. 26, 2009 in Application No. PCT/US2009/043454. |
PCT; International Preliminary Report on Patentability dated Jun. 14, 2011 in Application No. PCT/US2009/066377. |
PCT; International Search report and Written Opinion dated Nov. 12, 2010 in Application No. PCT/US2010/030126. |
PCT; International Preliminary Report on Patentability dated Oct. 11, 2011 Application No. PCT/US2010/030126. |
PCT; International Preliminary Report on Patentability dated Nov. 9, 2011 in Application No. PCT/US2010/033244. |
PCT; International Preliminary Report on Patentability dated Nov. 9, 2011 in Application No. PCT/US2010/033248. |
PCT; International Preliminary Report on Patentability dated Nov. 9, 2011 in Application No. PCT/US2010/033252. |
PCT; International Search report and Written Opinion dated Jan. 20, 2011 in Application No. PCT/US2010/045368. |
PCT; International Search report and Written Opinion dated Feb. 6, 2013 in Application No. PCT/US2012/065343. |
PCT; International Search report and Written Opinion dated Feb. 13, 2013 in Application No. PCT/US2012/065347. |
PCT; International Search Report and Written Opinion dated Nov. 16, 2017 in Application No. PCT/IB2017/001015. |
PCT; International Search Report and Written Opinion dated Nov. 13, 2017 in Application No. PCT/IB2017/001050. |
PCT; International Search Report and Written Opinion dated Nov. 30, 2017 in Application No. PCT/IB2017/001070. |
PCT; International Search Report and Written Opinion dated Jan. 25, 2018 in Application No. PCT/IB2017/001262. |
PCT: International Search Report and Written Opinion dated Jun. 1, 2018 in Application No. PCT/IB2017/001644. |
PCT: International Search Report and Written Opinion dated Jun. 1, 2018 in Application No. PCT/IB2017/001656. |
Chinese Patent Office; Office Action dated Jan. 10, 2013 in Application No. 201080015699.9. |
Chinese Patent Office; Office Action dated Aug. 1, 2013 in Application No. 201080015699.9. |
Chinese Patent Office; Office Action dated Jan. 21, 2014 in Application No. 201080015699.9. |
Chinese Patent Office; Office Action dated Jul. 24, 2014 in Application No. 201080015699.9. |
Chinese Patent Office; Office Action dated Jan. 12, 2015 in Application No. 201080015699.9. |
Chinese Patent Office; Office Action dated Dec. 10, 2013 in Application No. 201080020267.7. |
Chinese Patent Office; Office Action dated Jan. 21, 2013 in Application No. 201080020268.1. |
Chinese Patent Office; Office Action dated Sep. 26, 2013 in Application No. 201080020268.1. |
Chinese Patent Office; Office Action dated Apr. 3, 2014 in Application No. 201080020268.1. |
Chinese Patent Office; Office Action dated Sep. 23, 2014 in Application No. 201080020268.1. |
Chinese Patent Office; Office Action dated Apr. 7, 2015 in Application No. 201080020268.1. |
Chinese Patent Office; Office Action dated May 24, 2013 in Application No. 201080036764.6. |
Chinese Patent Office; Office Action dated Jan. 2, 2014 in Application No. 201080036764.6. |
Chinese Patent Office; Office Action dated Jul. 1, 2014 in Application No. 201080036764.6. |
Chinese Patent Office; Office Action dated Feb. 8, 2014 in Application No. 201110155056. |
Chinese Patent Office; Office Action dated Sep. 16, 2014 in Application No. 201110155056. |
Chinese Patent Office; Office Action dated Feb. 9, 2015 in Application No. 201110155056. |
Chinese Patent Office; Office Action dated Dec. 4, 2015 in Application No. 201210201995.9. |
Chinese Patent Office; Office Action dated Jul. 14, 2016 in Application No. 201210201995.9. |
Chinese Patent Office; Office Action dated Jan. 20, 2017 in Application No. 201210201995.9. |
Chinese Patent Office; Office Action dated Dec. 24, 2015 in Application No. 201280057466.4. |
Chinese Patent Office; Office Action dated Dec. 4, 2015 in Application No. 201280057542.1. |
Chinese Patent Office; Office Action dated May 16, 2016 in Application No. 201280057542.1. |
Chinese Patent Office; Office Action dated Sep. 9, 2016 in Application No. 201280057542.1. |
Chinese Patent Office; Office Action dated Dec. 5, 2016 in Application No. 201310412808.6. |
Chinese Patent Office; Office Action dated Feb. 5, 2018 in Application No. 201410331047.6. |
European Patent Office; Supplementary European Search Report and Opinion dated Nov. 9, 2012 in Application No. 08798519.8. |
European Patent Office; Office Action dated Jul. 18, 2016 in Application No. 08798519.8. |
European Patent Office; Extended European Search Report dated Dec. 9, 2016 in Application No. 9767208.3. |
European Patent Office; Supplementary European Search Report and Opinion dated Jan. 5, 2017 in Application No. 09836647.9. |
European Patent Office; Office Action dated Feb. 28, 2018 in Application No. 09836647.9. |
Japanese Patent Office; Office Action dated Dec. 20, 2011 in Application No. 2010-522075. |
Japanese Patent Office; Office Action dated Apr. 11, 2012 in Application No. 2010-522075. |
Japanese Patent Office; Office Action dated May 31, 2012 in Application No. 2011-514650. |
Japanese Patent Office; Office Action dated Sep. 11, 2012 in Application No. 2011-514650. |
Japanese Patent Office; Office Action dated Dec. 25, 2013 in Application No. 2012-504786. |
Japanese Patent Office; Office Action dated Jan. 25, 2014 in Application No. 2012-504786. |
Japanese Patent Office; Office Action dated Dec. 1, 2014 in Application No. 2012-504786. |
Japanese Patent Office; Office Action dated Mar. 11, 2013 in Application No. 2012-509857. |
Korean Patent Office; Office Action dated Dec. 10, 2015 in Application No. 10-2010-0028336. |
Korean Patent Office; Final Office Action dated Jun. 29, 2016 in Application No. 10-2010-0028336. |
Korean Patent Office; Office Action dated Mar. 3, 2016 in Application No. 10-2010-0067768. |
Korean Patent Office; Office Action dated Aug. 1, 2016 in Application No. 10-2010-0067768. |
Korean Patent Office; Office Action dated May 2, 2016 in Application No. 10-2010-0082446. |
Korean Patent Office; Office Action dated Sep. 19, 2016 in Application No. 10-2010-0082446. |
Korean Patent Office; Office Action dated Nov. 24, 2017 in Application No. 10-20110036449. |
Korean Patent Office; Office Action dated May 23, 2017 in Application No. 10-20110036449. |
Korean Patent Office; Office Action dated Sep. 4, 2017 in Application No. 10-2011-0087600. |
Korean Patent Office; Office Action dated Oct. 23, 2017 in Application No. 10-2011-0142924. |
Korean Patent Office; Office Action dated Dec. 11, 2015 in Application No. 10-20117023416. |
Korean Patent Office; Office Action dated Mar. 13, 2016 in Application No. 10-20117023416. |
Korean Patent Office; Office Action dated Oct. 30, 2017 in Application No. 10-2012-0041878. |
Korean Patent Office; Office Action dated Mar. 21, 2018 in Application No. 20120042518. |
Korean Patent Office; Office Action dated Mar. 21, 2018 in Application No. 10-2012-0064526. |
Korean Patent Office; Office Action dated Mar. 30, 2018 in Application No. 10-2012-0076564. |
Korean Patent Office; Office Action dated Apr. 30, 2018 in Application No. 10-2012-0103114. |
Korean Patent Office; Office Action dated Oct. 24, 2016 in Application No. 10-20127004062. |
Korean Patent Office; Office Action dated Jul. 24, 2017 in Application No. 10-20127004062. |
Korean Patent Office; Office Action dated Sep. 28, 2017 in Application No. 10-20147017112. |
Korean Patent Office; Office Action dated Nov. 9, 2016 in Application No. 10-20167023913. |
Korean Patent Office; Office Action dated Sep. 15, 2017 in Application No. 30-2017-0001320. |
Korean Patent Office; Office Action dated Jul. 11, 2018 in Application No. 30-2018-006016. |
Taiwanese Patent Office; Office Action dated Aug. 30, 2013 in Application No. 97132391. |
Taiwanese Patent Office; Office Action dated Dec. 20, 2013 in Application No. 98117513. |
Taiwan Patent Office; Office Action dated Jul. 4, 2014 in Application No. 099110511. |
Taiwanese Patent Office; Office Action dated Aug. 27, 2014 in Application No. 99114329. |
Taiwanese Patent Office; Office Action dated Dec. 26, 2014 in Application No. 99114330. |
Taiwanese Patent Office; Office Action dated Aug. 14, 2014 in Application No. 99114331. |
Taiwan Patent Office; Office Action dated Dec. 19, 2014 in Taiwan Application No. 099127063. |
Taiwanese Patent Office; Office Action received in Application No. 100113130. |
Taiwan Patent Office; Office Action dated May 13, 2016 in Taiwan Application No. 101142582. |
Taiwanese Patent Office; Office Action dated Aug. 1, 2016 in Application No. 101124745. |
Taiwanese Patent Office; Office Action received in Application No. 102113028. |
Taiwanese Patent Office; Office Action received in Application No. 102115605. |
Taiwanese Patent Office; Office Action dated Feb. 24, 2017 in Application No. 102115605. |
Taiwanese Patent Office; Office Action received in Application No. 102125191. |
Taiwanese Patent Office; Office Action dated Dec. 6, 2016 in Application No. 102126071. |
Taiwanese Patent Office; Office Action dated May 17, 2018 in Application No. 102126071. |
Taiwanese Patent Office; Office Action dated Feb. 10, 2017 in Application No. 102127065. |
Taiwanese Patent Office; Office Action dated Mar. 11, 2016 in Application No. 102129262. |
Taiwanese Patent Office; Office Action dated Dec. 29, 2016 in Application No. 102129397. |
Taiwanese Patent Office; Office Action dated Nov. 4, 2016 in Application No. 102131839. |
Taiwanese Patent Office; Office Action dated Dec. 2, 2016 in Application No. 102136496. |
Taiwanese Patent Office; Office Action dated Jan. 10, 2018 in Application No. 102136496. |
Taiwanese Patent Office; Office Action dated Nov. 11, 2016 in Application No. 102132952. |
Taiwanese Patent Office; Office Action dated Jul. 17, 2017 in Application No. 103101400. |
Taiwanese Patent Office; Office Action dated Feb. 23, 2017 in Application No. 103102563. |
Taiwanese Patent Office; Office Action dated Mar. 3, 2017 in Application No. 103105251. |
Taiwanese Patent Office; Office Action received in Application No. 103106021. |
Taiwanese Patent Office; Office Action dated Oct. 31, 2017 in Application No. 103106022. |
Taiwanese Patent Office; Office Action dated Jul. 5, 2017 in Application No. 103117477. |
Taiwanese Patent Office; Office Action dated Nov. 22, 2017 in Application No. 103117478. |
Taiwanese Patent Office; Office Action dated May 19, 2017 in Application No. 103120478. |
Taiwanese Patent Office; Office Action dated Nov. 8, 2017 in Application No. 103124509. |
Taiwanese Patent Office; Office Action dated Nov. 20, 2017 in Application No. 103127588. |
Taiwanese Patent Office; Office Action dated Sep. 19, 2017 in Application No. 103127734. |
Taiwanese Patent Office; Office Action dated Nov. 22, 2017 in Application No. 103134537. |
Taiwanese Patent Office; Office Action dated Aug. 24, 2017 in Application No. 103136251. |
Taiwanese Patent Office; Office Action dated Feb. 26, 2018 in Application No. 103138510. |
Taiwanese Patent Office; Office Action dated May 21, 2018 in Application No. 103139014. |
Taiwanese Patent Office; Office Action dated Jun. 22, 2018 in Application No. 104105533. |
Taiwanese Patent Office; Office Action dated Jun. 13, 2018 in Application No. 104111910. |
Taiwanese Patent Office; Office Action received in Application No. 106117181. |
Bearzotti, et al., “Fast Humidity Response of a Metal Halide-Doped Novel Polymer,” Sensors and Actuators B, 7, pp. 451-454, (1992). |
Becker et al., “Atomic Layer Deposition of Insulating Hafnium and Zirconium Nitrides,” Chem. Mater., 16, 3497-3501 (2004). |
Bhatnagar et al., “Copper Interconnect Advances to Meet Moore's Law Milestones,” Solid State Technology, 52, 10 (2009). |
Buriak, “Organometallic Chemistry on Silicon and Germanium Surfaces,” Chemical Reviews, 102, 5 (2002). |
Cant et al., “Chemisorption Sites on Porous Silica Glass and on Mixed-Oxide Catalysis,” Can. J. Chem. 46, 1373 (1968). |
Chang et al. “Small-Subthreshold-Swing and Low-Voltage Flexible Organic Thin-Film Transistors Which Use HfLaO as the Gate Dielectric,” IEEE Electron Device Letters, Feb. 2009, pp. 133-135; vol. 30, No. 2; IEEE Electron Device Society. |
Chatterjee et al., “Sub-100nm Gate Length Metal Gate NMOS Transistors Fabricated by a Replacement by a Replacement Gate Process,” IEEE Semiconductor Process and Device Center, 821-824 (1997). |
Chen et al., “A Self-Aligned Airgap Interconnect Scheme,” IEEE International Interconnect Technology Conference, vol. 1-3, 146-148 (2009). |
Choi et al., “Improvement of Silicon Direct Bonding using Surfaces Activated by Hydrogen Plasma Treatment,” Journal of the Korean Physical Society, 37, 6, 878-881 (2000). |
Choi et al., “Low Temperature Formation of Silicon Oxide Thin Films by Atomic Layer Deposition Using NH3/O2 Plasma,” ECS Solid State Letters, 2(12) p. 114-p. 116 (2013). |
Coates, “Process Analytical Technology: Spectroscopic Tools and Implementation Strategies for the Chemical and Pharmaceutical Industries.” Blackwell Publishing Ltd, 91-132, (2005). |
Crowell, “Chemical methods of thin film deposition: Chemical vapor deposition, atomic layer deposition, and related technologies,” Journal of Vacuum Science & Technology A 21.5, (2003): S88-S95. |
Cui et al., “Impact of Reductive N2/H2 Plasma on Porous Low-Dielectric Constant SiCOH Thin Films,” Journal of Applied Physics 97, 113302, 1-8 (2005). |
Dingemans et al., “Comparison Between Aluminum Oxide Surface Passivation Films Deposited with Thermal Aid,” Plasma Aid and Pecvd, 35th IEEE PVCS, Jun. 2010. |
Drummond et al., “Hydrophobic Radiofrequency Plasma-Deposited Polymer Films: Dielectric Properties and Surface Forces,” Colloids and Surfaces A, 129-130, 117-129 (2006). |
Easley et al., “Thermal Isolation of Microchip Reaction Chambers for Rapid Non-Contact DNA Amplification,” J. Micromech. Microeng. 17, 1758-1766 (2007). |
Elam et al., “New Insights into Sequential Infiltration Synthesis”, ECS Transactions, vol. 69, pp. 147-157 (2015). |
Ge et al., “Carbon Nanotube-Based Synthetic Gecko Tapes,” Department of Polymer Science, PNAS, 10792-10795 (2007). |
George et al., “Atomic Layer Deposition: An Overview,” Chem. Rev. 110, 111-131 (2010). |
Grill et al., “The Effect of Plasma Chemistry on the Damage Induced Porous SiCOH Dielectrics,” IBM Research Division, RC23683 (W0508-008), Materials Science, 1-19 (2005). |
Guan et al., “Voltage gated ion and molecule transport in engineered nanochannels: theory, fabrication and applications,” Nanotechnology 25 (2014) 122001. |
Gupta et al., “Conversion of Metal Carbides to Carbide Derived Carbon by Reactive Ion Etching in Halogen Gas,” Proceedings of SPIE—The International Society for Optical Engineering and Nanotechnologies for Space Applications, ISSN: 0277-786X (2006). |
Harrison et al., “Poly-gate Replacement Through Contact Hole (PRETCH): A New Method for High-K/ Metal Gate and Multi-Oxide Implementation on Chip,” IEEE (2004). |
Heo et al., “Structural Characterization of Nanoporous Low-Dielectric Constant SiCOH Films Using Organosilane Precursors,” NSTI-Nanotech, vol. 4, 122-123 (2007). |
Henke et al.., “X-Ray Interactions: Photo absorption, Scattering, Transmission, and Reflection at E=50-30,000 eV, Z=1-92,” Atomic Data and Nuclear Data Tables, 54, 181-342 (1993). |
H.J. Yun et al., “Comparison of Atomic Scale Etching of Poly-Si in Inductively Coupled Ar and He Plasmas”, Korean Journal of Chemical Engineering, vol. 24, 670-673 (2007). |
Hudis, “Surface Crosslinking of Polyethylene Using a Hydrogen Glow Discharge,” J. Appl. Polym. Sci., 16 (1972) 2397. |
Jones et al., “Growth of Aluminum Films by Low Pressure Chemical Vapour Deposition Using Tritertiarybutylaluminium,” Journal of Crystal Growth 135, pp. 285-289, Elsevier Science B.V. (1994). |
Jones et al., “Recent Developments in Metalorganic Precursors for Metalorganic Chemical Vapour Deposition,” Journal of Crystal Growth 146, pp. 503-510, Elsevier Science B.V. (1995). |
Jung et al., “Double Patterning of Contact Array with Carbon Polymer,” Proc. Of SPIE, 6924, 69240C, 1-10 (2008). |
Kim et al., “Passivation Effect on Low-k S/OC Dielectrics by H2 Plasma Treatment,” Journal of the Korean Physical Society, ″40, 1, 94-98 (2002). |
Kim et al., “Characteristics of Low Temperature High Quality Silicon Oxide by Plasma Enhanced Atomic Layer Deposition with In-Situ Plasma Densification Process,” The Electrochemical Society, ECS Transactions, College of Information and Communication Engineering, Sungkyunkwan University, 53(1), 321-329 (2013). |
King, Plasma Enhanced Atomic Layer Deposition of SiNx: H and SiO2, J. Vac. Sci. Technol., A29(4) (2011). |
Klug et al., “Atomic Layer Deposition of Amorphous Niobium Carbide-Based Thin Film Superconductors,” The Journal of Physical Chemistry C, vol. 115, pp. 25063-25071, (2011). |
Kobayshi, et al., “Temperature Dependence of SiO2 Film Growth with Plasma-Enhanced Atomic Layer Deposition,” regarding Thin Solid Films, published by Elsevier in the International Journal on the Science and Technology of Condensed Matter, in vol. 520, No. 11, 3994-3998 (2012). |
Koo et al., “Characteristics of A12O3 Thin Films Deposited Using Dimethylaluminum Isopropoxide and Trimethylaluminum Precursors by the Plasma-Enhanced Atomic-Layer Deposition Method,” Journal of Physical Society, 48, 1, 131-136 (2006),. |
Koutsokeras et al. “Texture and Microstructure Evolution in Single-Phase TixTal-xN Alloys of Rocksalt Structure,” Journal of Applied Physics, 110, pp. 043535-1-043535-6, (2011). |
Knoops et al., “Atomic Layer Deposition of Silicon Nitride from Bis(tert-butyloamino) silane and N2 Plasma,” Applied Materials & Interfaces, American Chemical Society, A-E (2015). |
Krenek et al. “IR Laser CVD of Nanodisperse Ge—Si—Sn Alloys Obtained by Dielectric Breakdown of GeH4/SiH4/SnH4 Mixtures”, NanoCon 2014, Nov. 5-7, Brno, Czech Republic, EU. |
Kurosawa et al., “Synthesis and Characterization of Plasma-Polymerized Hexamethyldisiloxane Films,” Thin Solid Films, 506-507, 176-179 (2006). |
Lanford et al., “The Hydrogen Content of Plasmadeposited Silicon Nitride,” J. Appl. Phys., 49, 2473 (1978). |
Lee et al., Layer Selection by Multi-Level Permutation in 3-D Stacked NAND Flash Memory, IEEE Electron Device Letters, vol. 37, No. 7, 866-869 (2016). |
Lieberman, et al., “Principles of Plasma Discharges and Materials Processing,” Second Edition, 368-381. |
Lim et al., “Low-Temperature Growth of SiO2 Films by Plasma-Enhanced Atomic Layer Deposition,” ETRI Journal, 27 (1), 118-121 (2005). |
Liu et al., “Research, Design, and Experiment of End Effector for Wafer Transfer Robot,” Industrial Robot: An International Journal, 79-91 (2012). |
Longrie et al., “Plasma-Enhanced ALD of Platinum with O2, N2 and NH3 Plasmas”, ECS Journal of Solid State Science and Technology, vol. 1, pp. Q123-Q129 (2012). |
Mackus et al., “Optical Emission Spectroscopy as a Tool for Studying Optimizing and Monitoring Plasma-Assisted Atomic Layer Deposition Processes,” Journal of Vacuum Science and Technology, 77-87 (2010). |
Maeno, “Gecko Tape Using Carbon Nanotubes,” Nitto Denko Gihou, 47, 48-51. |
Maeng et al. Electrical properties of atomic layer disposition Hf02 and HfOxNy on Si substrates with various crystal orientations, Journal of the Electrochemical Society, Apr. 2008, p. H267-H271, vol. 155, No. 4, Department of Materials Science and Engineering, Pohang University of Science and Technology, Pohang, Korea. |
Marsik et al., “Effect of Ultraviolet Curing Wavelength on Low-k Dielectric Material Properties and Plasma Damage Resistance,” Sciencedirect.com, 519, 11, 3619-3626 (2011). |
Mason et al., “Hydrolysis of Tri-tert-butylaluminum: The First Structural Characterization of Alkylalumoxanes [(R2A1)2O]n and (RAIO)n,” J. American Chemical Society, vol. 115, No. 12, pp. 4971-4984 (1993). |
Massachusetts Institute of Technology Lincoln Laboratory, “Solid State Research,” Quarterly Technical Report (1995). |
Maydannik et al., “Spatial atomic layer deposition: Performance of low temperature H2O and 03oxidant chemistry for flexible electronics encapsulation”, Journal of Vacuum Science and Technology: Part A AVS/ AIP, vol. 33 (1901). |
Meng et al., “Atomic Layer of Deposition of Silicon Nitride Thin Films: A Review of Recent Progress, Challenges, and Outlooks,” Materials, 9, 1007 (2016). |
Mix et al., “Characterization of plasma-polymerized allyl alcohol polymers and copolymers with styrene,” Adhes. Sci. Technol., 21 (2007), S. 487-507. |
Moeen, “Design, Modelling and Characterization of Si/SiGe Structures for IR Bolometer Applications,” KTH Royal Institute of Technology. Information and Communication Technology, Department of Integrated Devices and Circuits, Stockholm Sweden (2015). |
Morishige et al., “Thermal Desorption and Infrared Studies of Ammonia Amines and Pyridines Chemisorbed on Chromic Oxide,” J. Chem. Soc., Faraday Trans. 1, 78, 2947-2957 (1982). |
Mosleh et al., “Enhancement of Material Quality of (Si)GeSn Films Grown by SnC14 Precursor,” ECS Transactions, 69 (5), 279-285 (2015). |
Mukai et al., “A Study of CD Budget in Spacer Patterning Technology,” Proc. Of SPIE, 6924, 1-8 (2008). |
Nigamananda et al., “Low-Temperature (<200oC) Plasma. Enhanced Atomic Deposition of Dense Titanium Nitride Thin Films.” |
Nogueira et al., “Production of Highly Hydrophobic Films Using Low Frequency and High Density Plasma,” Revista Brasileira de Aplicacoes de Vacuo, 25(1), 45-53 (2006). |
Novaro et al. Theoretical Study on a Reaction Pathway of Ziegler-Natta-Type Catalysis, J. Chem. Phys. 68(5), Mar. 1, 1978 p. 2337-2351. |
S. Okamoto et al., “Luminescent Properties of Pr3+-sensitized LaPO4: Gd3+ Ultraviolet-B Phosphor Under Vacuum-Ultraviolet Light Excitation,” J. App. Phys. 106, 013522 (2009). |
Park,, “Substituted Aluminum Metal Gate on High-K Dielectric for Low Work-Function and Fermi-Level Pinning Free,” 4 pages, IEEE 0-7803-8684-1/04 (2004). |
Portet et al., “Impact of Synthesis Conditions on Surface Chemistry and Structure of Carbide-Derived Carbons,” Thermochimica Acta, 497, 137-142 (2010). |
Potts et al., “Low Temperature Plasma-Enhanced Atomic Layer Deposition of metal Oxide Thin Films,” Journal of the Electrochemical Society, 157, 66-74 (2010). |
Potts et al., “Room-Temperature Ald of Metal Oxide Thin Films by Energy-Enhanced ALD”, Chemical Vapor Deposition, vol. 19, pp. 125-133 (2013). |
Presser, et al., “Effect of Pore Size on Carbon Dioxide Sorption by Carbide Derived Carbon,” Energy & Environmental Science 4.8, 3059-3066 (2011). |
Provine et al., “Correlation of Film Density and Wet Etch Rate in Hydrofluoric Acid of Plasma Enhanced Atomic Layer Deposited Silicon Nitride,” AIP Advances, 6 (2016). |
Radamson et al. “Growth of Sn-alloyed Group IV Materials for Photonic and Electronic Applications”, Chapter 5 pp. 129-144, Manufacturing Nano Structures. |
Sakuma et al., “Highly Scalable Horizontal Channel 3-D NAND Memory Excellent in Compatibility with Conventional Fabrication Technology,” IEEE Electron Device Letters, vol. 34, No. 9, 1142-1144 (2013). |
Salim, “In-situ Fourier Transform Infrared Spectroscopy of Chemistry and Growth in Chemical Vapor Deposition,” Massachusetts Institute of Technology, 187 pages (1995). |
Salim et al., “In Situ Concentration Monitoring in a Vertical OMVPE Reactor by Fiber-Optics-Based Fourier Transform Infrared Spectroscopy,” Journal of Crystal Growth 169, pp. 443-449, Elsevier Science B.V. (1996). |
Schmatz et al., “Unusual Isomerization Reactions in 1.3-Diaza-2-Silcyclopentanes,” Organometallics, 23, 1180-1182 (2004). |
Scientific and Technical Information Center EIC 2800 Search Report dated Feb. 16, 2012. |
Selvaraj et al., “Selective Atomic Layer Deposition of Zirconia on Copper Patterned Silicon Substrates Using Ethanol as Oxygen Source as Well as Copper Reductant,” J. Vac. Sci. Technol. A32(1), (2014). |
Selvaraj et al., “Surface Selective Atomic Layer Deposition of Hafnium Oxide for Copper Diffusion Barrier Application Using Tetrakis (diethylamino) Hafnium and Ethanol,” 225th ECS Meeting, Meeting Abstract, (May 12, 2014). |
S.D. Athavale and D.J. Economou, “Realization of Atomic Layer Etching of Silicon”, Journal of Vacuum Science and Technology B, vol. 14, year 1996, pp. 3702-3705. |
Shamma et al., “PDL Oxide Enabled Doubling,” Proc. Of SPIE, 6924, 69240D, 1-10 (2008). |
Tseng et al., “Etch Properties of Resists Modified by Sequential Infiltration Synthesis,” American Vacuum Society (2011). |
Tseng et al., “Enhanced Block Copolymer Lithography Using Sequntial Infiltration Synthesis,” Journal of Physical Chemistry, vol. 5, 17725-17729 (2011). |
Varma, et al., “Effect of Metal Halides on Thermal, Mechanical, and Electrical Properties of Polypyromelitimide Films,” Journal of Applied Polymer Science, vol. 32, pp. 3987-4000, (1986). |
Voltaix, “Meterial Safety Data Sheet for: Trisilylamine”, pp. 1-8, (2014). |
Wang et al., “Tritertiarybutylaluminum as an Organometallic Source for Epitaxial Growth of AlGaSb,” Appl. Phys. Lett. 67 (10), Sep. 4, pp. 1384-1386, American Institute of Physics (1995). |
Wirths, et al, “SiGeSn Growth tudies Using Reduced Pressure Chemical Vapor Deposition Towards Optoeleconic Applications,” This Soid Films, 557, 183-187 (2014). |
Yoshida, et al., Threshold Voltage Tuning for 10NM and Beyond CMOS Integration, Solid State Technology, 57(7): 23-25 (2014). |
Yu et al., “Modulation of the Ni FUSI Workfunction by Yb Doping: from Midgap to N-Type Band-Edge,” 4 pages, IEEE 0-7803-9269-8/05 (2005). |
Yun et al., “Behavior of Various Organosilicon Molecules in PECVD Processes for Hydrocarbon-Doped Silicon Oxide Films,” Solid State Phenomena, vol. 124-126, 347-350 (2007). |
Yun et al., “Single-Crystalline Si Stacked Array (STAR) NAND Flash Memory,” IEEE Transactions on Electron Devices, vol. 58, No. 4, 1006-1014 (2011). |
Yun et al., “Effect of Plasma on Characteristics of Zirconium Oxide Films Deposited by Plasma-Enhanced Atomic Layer Deposition,” Electrochemical and Solid State Letters, 8(11) F47-F50 (2005). |
Yushin et al., “Carbon-Derived Carbon,” Department of Materials Science and Engineering, Taylor & Francis Group, LLC (2006). |
Chemistry Stack Exchange, “Why is CF4 Non-Polar and CHF Polar,” https://chemistry.stackexchange.com/questions/31604/why-is-cf4-non-polar-and-chf3-polar, (2015). |
USPTO; Notice of Allowance dated Jun. 28, 2017 in U.S. Appl. No. 13/166,367. |
USPTO; Non-Final Office Action dated Sep. 20, 2018 in U.S. Appl. No. 13/651,144. |
USPTO; Notice of Allowance dated Aug. 13, 2018 in U.S. Appl. No. 13/941,226. |
USPTO; Notice of Allowance dated Oct. 3, 2018 in U.S. Appl. No. 13/941,226. |
USPTO; Notice of Allowance dated Aug. 29, 2018 in U.S. Appl. No. 14/090,750. |
USPTO; Notice of Allowance dated Sep. 24, 2018 in U.S. Appl. No. 14/218,690. |
USPTO; Final Office Action dated Sep. 5, 2018 in U.S. Appl. No. 14/752,712. |
USPTO; Advisory Action dated Aug. 10, 2018 in U.S. Appl. No. 14/829,565. |
USPTO; Non-Final Office Action dated Sep. 6, 2018 in U.S. Appl. No. 14/829,565. |
USPTO; Notice of Allowance dated Oct. 20, 2017 in U.S. Appl. No. 14/884,695. |
USPTO; Notice of Allowance dated Oct. 4, 2018 in U.S. Appl. No. 14/919,536. |
USPTO; Non-Final Office Action dated Aug. 27, 2018 in U.S. Appl. No. 15/067,028. |
USPTO; Notice of Allowance dated Oct. 14, 2018 in U.S. Appl. No. 15/135,333. |
USPTO; Notice of Allowance dated May 22, 2017 in U.S. Appl. No. 15/222,738. |
USPTO; Notice of Allowance dated Sep. 10, 2018 in U.S. Appl. No. 15/222,749. |
USPTO; Non-Final Office Action dated Oct. 1, 2018 in U.S. Appl. No. 15/222,780. |
USPTO; Non-Final Office Action dated Sep. 13, 2018 in U.S. Appl. No. 15/262,990. |
USPTO; Non-Final Office Action dated Oct. 3, 2017 in U.S. Appl. No. 15/388,410. |
USPTO; Non-Final Office Action dated Sep. 20, 2018 in U.S. Appl. No. 15/410,503. |
USPTO; Final Office Action dated Aug. 29, 2018 in U.S. Appl. No. 15/434,051. |
USPTO; Non-Final Office Action dated Sep. 10, 2018 in U.S. Appl. No. 15/489,453. |
USPTO; Notice of Allowance dated Jul. 18, 2018 in U.S. Appl. No. 15/640,239. |
USPTO; Notice of Allowance dated Aug. 30, 2018 in U.S. Appl. No. 15/640,239. |
USPTO; Non-Final Office Action dated Sep. 21, 2017 in U.S. Appl. No. 15/659,631. |
USPTO; Non-Final Office Action dated Aug. 27, 2018 in U.S. Appl. No. 15/662,107. |
USPTO; Requirement for Restriction dated Sep. 11, 2018 in U.S. Appl. No. 15/672,063. |
USPTO; Requirement for Restriction dated Aug. 14, 2018 in U.S. Appl. No. 15/705,955. |
USPTO; Non-Final Office Action dated Oct. 4, 2018 in U.S. Appl. No. 15/726,222. |
USPTO; Restriction Requirement dated Aug. 31, 2018 in U.S. Appl. No. 15/795,056. |
USPTO; Non-Final Office Action dated Jun. 26, 2018 in U.S. Appl. No. 15/796,693. |
USPTO; Non-Final Office Action dated Sep. 10, 2018 in U.S. Appl. No. 15/836,547. |
European Patent Office; Office Action dated Aug. 10, 2018 in Application No. 09767208.3. |
Korean Patent Office; Office Action dated Apr. 2, 2018 in Application No. 10-2011-0036449. |
Korean Patent Office; Office Action dated Sep. 18, 2018 in Application No. 10-2012-0064526. |
Korean Patent Office; Office Action dated Sep. 27, 2018 in Application No. 10-2012-0076564. |
Korean Patent Office; Office Action dated Sep. 28, 2017 in Application No. 10-2017-7023740. |
Taiwanese Patent Office; Office Action Sep. 26, 2018 in Application No. 103132230. |
Taiwanese Patent Office; Office Action dated May 21, 2018 Application No. 103139014. |
Taiwanese Patent Office; Office Action dated Jul. 9, 2018 in Application No. 104107876. |
Taiwanese Patent Office; Office Action dates Aug. 7, 2018 Application No. 104107888. |
Taiwanese Patent Office; Office Action dated Jul. 9, 2018 in Application No. 104110326. |
Taiwanese Patent Office; Office Action dated Jul. 11, 2018 in Application No. 104124377. |
Taiwanese Patent Office; Office Action dated Jun. 25, 2018 in Application No. 106138800. |
Taiwanese Patent Office; Office Action dated Aug. 31, 2018 in Application No. 10720809210. |
WIPO; International Search Report and Written Opinion dated Jul. 9, 2018 in Application No. PCT/IB2018/000419. |
WIPO; International Search Report and Written Opinion dated Sep. 14, 2018 in Application No. PCT/IB2017/001640. |
Crystal IS “Application Note: Using UV Reflective Materials to Maximize Disinfection”; AN011; Jun. 16, 2016. |
Kukli et al., “Properties of hafnium oxide films grown by atomic layer deposition from hafnium tetraiodide and oxygen”. Journal of Applied Physics, vol. 92, No. 10, Nov. 15, 2002, pp. 5698-5703. |
Liang et al. “Conversion of Metal Carbides to Carbide Derived Carbon by Reactive Ion Etching in Halogen Gas” Micro (MEMS) and Nanotechnologies for Space Applications, Thomas George et al. vol. 6223, 2006 p. 62230J-I to 62230J-11 lines 3-14 in the “Abstract” section and lines 7-9 in the “Introduction” section of p. 1, lines 3-4 in the “Introduction” section and lines 3-4 in the “Experimental Procedure” section of p. 2. |
“Polyurethane HF”; webpage; no date. Cited in Notice of References dated May 18, 2017 in U.S. Appl. No. 14/884,695. |
Xu et al., “14NM Metal Gate Film Stack Development and Challenges,” Smic et al. (2016). |
EPO; Extended European Search Report dated Apr. 28, 2014 in Application No. 11162225.4. |
EPO; Notice of Allowance dated Feb. 3, 2015 in Application No. 11162225.4. |
IPOS; Notice of Allowance dated Aug. 14, 2017 in Application No. 10201401237. |
JPO; Office Action dated Mar. 27, 2012 in Application No. 2009-532567. |
JPO; Notice of Allowance dated Jul. 31, 2012 in Application No. 2009-532567. |
JPO; Office Action dated May 9, 2013 in Application No. 2010058415. |
JPO; Office Action dated Nov. 5, 2013 in Application No. 2010058415. |
JPO; Office Action dated Aug. 29, 2014 in Application No. 2010058415. |
JPO; Notice of Allowance dated Dec. 24, 2014 in Application No. 2010058415. |
JPO; Office Action dated Aug. 26, 2013 in Application No. 2010-153754. |
JPO; Office Action dated Nov. 5, 2013 in Application No. 2010-193285. |
JPO; Notice of Allowance dated Apr. 2, 2013 in Application No. 2010-509478. |
JPO; Office Action dated Aug. 31, 2015 in Application No. 2011-284831. |
JPO; Notice of Allowance dated Mar. 9, 2016 in Application No. 2011-284831. |
JPO; Notice of Allowance dated Dec. 21, 2012 in Application No. 2011-514650. |
JPO; Office Action dated Dec. 15, 2014 in Application No. 2011090067. |
JPO; Notice of Allowance dated May 1, 2015 in Application No. 2011090067. |
JPO; Office Action dated Jul. 19, 2016 in Application No. 2012-153698. |
JPO; Notice of Allowance dated Oct. 26, 2016 in Application No. 2012-153698. |
JPO; Notice of Allowance dated Jun. 12, 2015 in Application No. 2012-504786. |
JPO; Notice of Allowance dated Jul. 2, 2013 in Application No. 2012-509857. |
JPO; Office Action dated May 31, 2017 in Application No. 2013-160173. |
JPO; Notice of Allowance dated Aug. 25, 2017 in Application No. 2013-160173. |
JPO; Office Action dated Jun. 15, 2017 in Application No. 2013-178344. |
JPO; Office Action dated Jan. 29, 2018 in Application No. 2013-178344. |
JPO; Notice of Allowance dated Aug. 21, 2018 in Application No. 2013-178344. |
JPO; Office Action dated Apr. 10, 2018 in Application No. 2014-120675. |
JPO; Notice of Allowance dated Jun. 12, 2018 in Application No. 2014-120675. |
JPO; Office Action dated Apr. 3, 2018 in Application No. 2014-188835. |
JPO; Notice of Allowance dated Jun. 12, 2018 in Application No. 2014-188835. |
JPO; Office Action dated May 8, 2018 in Application No. 2014-205548. |
JPO; Notice of Allowance dated May 22, 2018 in Application No. 2014-216540. |
JPO; Office Action dated Jul. 31, 2018 in Application No. 2015-034774. |
KIPO; Notice of Allowance dated Sep. 29, 2016 in Application No. 10-2010-0028336. |
KIPO; Notice of Allowance dated Dec. 1, 2016 in Application No. 10-2010-0067768. |
KIPO; Notice of Allowance dated Mar. 7, 2017 in Application No. 10-2010-0082446. |
KIPO; Office Action dated Mar. 13, 2017 in Application No. 20110034612. |
KIPO; Office Action dated Jul. 20, 2017 in Application No. 20110034612. |
KIPO; Notice of Allowance dated Sep. 1, 2017 in Application No. 20110034612. |
KIPO; Notice of Allowance dated Oct. 24, 2018 in Application No. 10-2011-0036449. |
KIPO; Notice of Allowance dated Jan. 11, 2018 in Application No. 10-2011-0087600. |
KIPO; Notice of Allowance dated Mar. 14, 2018 in Application No. 10-2011-0142924. |
KIPO; Notice of Allowance dated Jun. 2, 0216 in Application No. 10-2011-7023416. |
KIPO; Notice of Allowance dated Feb. 28, 2018 in Application No. 10-2012-0041878. |
KIPO; Notice of Allowance dated May 30, 2018 in Application No. 10-2012-0042518. |
KIPO; Office Action dated Dec. 13, 2018 in Application No. 10-2012-0064526. |
KIPO; Notice of Allowance dated Nov. 22, 2018 in Application No. 10-2012-0103114. |
KIPO; Notice of Allowance dated Feb. 23, 2018 in Application No. 10-2014-7017112. |
KIPO; Notice of Allowance dated May 30, 2017 in Application No. 10-2016-7023913. |
KIPO; Notice of Allowance dated Jul. 19, 2018 in Application No. 20187013945. |
KIPO; Notice of Allowance dated Jan. 19, 2018 in Application No. 30-2017-0001320. |
KIPO; Notice of Allowance dated Jul. 1, 2018 in Application No. 30-2017-0052872. |
KIPO; Notice of Allowance dated Oct. 16, 2018 in Application No. 30-2018-0006016. |
SIPO; Notice of Allowance dated May 8, 2015 in Application No. 201080015699.9. |
SIPO; Notice of Allowance dated Aug. 22, 2014 in Application No. 201080020267.7. |
SIPO; Notice of Allowance dated Oct. 16, 2015 in Application No. 201080020268.1. |
SIPO; Notice of Allowance dated Oct. 24, 2014 in Application No. 201080036764.6. |
SIPO; Notice of Allowance dated Aug. 26, 2015 in Application No. 201110155056. |
SIPO; Notice of Allowance dated Apr. 13, 2017 in Application No. 201210201995.9. |
SIPO; Notice of Allowance dated Jun. 16, 2016 in Application No. 201280057466.4. |
SIPO; Notice of Allowance dated Jan. 3, 2017 in Application No. 201280057542.1. |
SIPO; Notice of Allowance dated Jul. 20, 2017 in Application No. 201310412808.6. |
SIPO; Notice of Allowance dated May 25, 2017 in Application No. 201730010308.9. |
SIPO; Notice of Allowance dated Oct. 24, 2018 in Application No. 201830060972.9. |
TIPO; Notice of Allowance dated Jun. 12, 2014 in Application No. 98117513. |
TIPO; Notice of Allowance dated Feb. 24, 2016 in Application No. 99110511. |
TIPO; Notice of Allowance dated Apr. 28, 2015 in Application No. 99114330. |
TIPO; Notice of Allowance dated Oct. 16, 2015 in Application No. 99114331. |
TIPO; Notice of Allowance dated Mar. 14, 2016 in Application No. 99127063. |
TIPO; Notice of Allowance dated Jun. 29, 2016 in Applicaton No. 100113130. |
TIPO; Notice of Allowance dated Oct. 14, 2015 in Application No. 100130472. |
TIPO; Notice of Allowance dated Oct. 19, 2016 in Application No. 101124745. |
TIPO; Notice of Allowance dated Nov. 2, 2016 in Application No. 101142581. |
TIPO; Notice of Allowance dated Sep. 9, 2016 in Application No. 101142582. |
TIPO; Notice of Allowance dated Feb. 13, 2017 in Application No. 102113028. |
TIPO; Notice of Allowance dated Dec. 26, 2017 in Application No. 102115605. |
TIPO; Notice of Allowance dated May 3, 2017 in Application No. 102129262. |
TIPO; Notice of Allowance dated Aug. 24, 2018 in Application No. 102126071. |
TIPO; Notice of Allowance dated Jul. 18, 2017 in Application No. 102127065. |
TIPO; Notice of Allowance dated Aug. 29, 2017 in Application No. 102129397. |
TIPO; Notice of Allowance dated Jan. 26, 2017 in Application No. 102131839. |
TIPO; Notice of Allowance dated Apr. 19, 2017 in Application No. 102132952. |
TIPO; Notice of Allowance dated Jan. 24, 2018 in Application No. 103101400. |
TIPO; Notice of Allowance dated Nov. 30, 2017 in Application No. 103102563. |
TIPO; Notice of Allowance dated Oct. 20, 2017 in Application No. 103105251. |
TIPO; Notice of Allowance dated Apr. 10, 2018 in Application No. 103106021. |
TIPO; Notice of Allowance dated Apr. 10, 2018 in Application No. 103106022. |
TIPO; Notice of Allowance dated Jan. 22, 2018 in Application No. 103117477. |
TIPO; Notice of Allowance dated Mar. 13, 2018 in Application No. 103117478. |
TIPO; Notice of Allowance dated Sep. 25, 2017 in Application No. 103120478. |
TIPO; Office Action dated Sep. 20, 2018 in Application No. 103123439. |
TIPO; Office Action dated Apr. 25, 2018 in Application No. 103124509. |
TIPO; Notice of Allowance dated Jun. 19, 2018 in Application No. 103127588. |
TIPO; Notice of Allowance dated Dec. 11, 2017 in Application No. 103127734. |
TIPO; Notice of Allowance dated Apr. 19, 2018 in Application No. 103134537. |
TIPO; Notice of Allowance dated Oct. 17, 2017 in Application No. 103136251. |
TIPO; Notice of Allowance dated Jun. 13, 2018 in Application No. 103138510. |
TIPO; Notice of Allowance dated Sep. 11, 2018 in Application No. 103139014. |
TIPO; Notice of Allowance dated Sep. 18, 2018 in Application No. 104111910. |
TIPO; Notice of Allowance dated Dec. 5, 2017 in Application No. 105308015. |
TIPO; Notice of Allowance dated Jun. 5, 2018 in Application No. 106117181. |
TIPO; Office Action dated Sep. 28, 2018 in Application No. 106119537. |
TIPO; Office Action dated Aug. 31, 2018 in Application No. 106138119. |
TIPO; Office Action dated Oct. 3, 2018 in Application No. 106142731. |
TIPO; Office Action dated Sep. 28, 2018 in Application No. 107112951. |
TIPO; Notice of Allowance dated Aug. 29, 2018 in Application No. 107300633. |
TIPO; Notice of Allowance dated Apr. 11, 2018 in Application No. 105308015D01. |
USPTO; Non-Final Office Action dated Feb. 15, 2012 in U.S. Appl. No. 13/085,531. |
USPTO; Notice of Allowance dated Jul. 12, 2012 in U.S. Appl. No. 13/085,531. |
USPTO; Final Office Action dated Nov. 2, 2018 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated Nov. 1, 2018 in U.S. Appl. No. 14/219,839. |
USPTO; Final Office Action dated Nov. 2, 2018 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office Action dated Nov. 28, 2018 in U.S. Appl. No. 14/508,489. |
USPTO; Notice of Allowance dated Nov. 19, 2018 in U.S. Appl. No. 14/656,588. |
USPTO; Notice of Allowance dated Nov. 19, 2018 in U.S. Appl. No. 14/919,536. |
USPTO; Final Office Action dated Dec. 10, 2018 in U.S. Appl. No. 14/997,683. |
USPTO; Final Office Action dated Oct. 19, 2018 in U.S. Appl. No. 15/060,412. |
USPTO; Non-Final Office Action dated Sep. 26, 2018 in U.S. Appl. No. 15/074,813. |
USPTO; Non-Final Office Action dated Nov. 23, 2018 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Oct. 9, 2018 in U.S. Appl. No. 15/182,504. |
USPTO; Final Office Action dated Oct. 9, 2018 in U.S. Appl. No. 15/205,827. |
USPTO; Non-Final Office Action dated Nov. 14, 2018 in U.S. Appl. No. 15/377,439. |
USPTO; Notice of Allowance dated Nov. 14, 2018 in U.S. Appl. No. 15/388,410. |
USPTO; Notice of Allowance dated Dec. 28, 2018 in U.S. Appl. No. 15/388,410. |
USPTO; Restriction Requirement dated Dec. 5, 2018 in U.S. Appl. No. 15/402,993. |
USPTO; Advisory Action dated Dec. 4, 2018 in U.S. Appl. No. 15/434,051. |
USPTO; Notice of Allowance dated Nov. 30, 2018 in U.S. Appl. No. 15/472,750. |
USPTO; Notice of Allowance dated Nov. 1, 2018 in U.S. Appl. No. 15/499,647. |
USPTO; Notice of Allowance dated Nov. 15, 2018 in U.S. Appl. No. 15/499,647. |
USPTO; Final Office Action dated Nov. 16, 2018 in U.S. Appl. No. 15/592,730. |
USPTO; Restriction Requirement dated Oct. 10, 2018 in U.S. Appl. No. 15/615,489. |
USPTO; Non-Final Office Action dated Nov. 9, 2018 in U.S. Appl. No. 15/636,307. |
USPTO; Final Office Action dated Nov. 20, 2018 in U.S. Appl. No. 15/650,686. |
USPTO; Non-Final Office Action dated Dec. 4, 2018 in U.S. Appl. No. 15/672,063. |
USPTO; Restriction Requirement dated Oct. 15, 2018 in U.S. Appl. No. 15/672,119. |
USPTO; Advisory Action dated Nov. 26, 2018 in U.S. Appl. No. 15/683,701. |
USPTO; Non-Final Office Action dated Dec. 18, 2018 in U.S. Appl. No. 15/690,017. |
USPTO; Non-Final Office Action dated Dec. 6, 2018 in U.S. Appl. No. 15/705,955. |
USPTO; Notice of Allowance dated Dec. 6, 2018 in U.S. Appl. No. 15/711,989. |
USPTO; Final Office Action dated Dec. 13, 2018 in U.S. Appl. No. 15/719,208. |
USPTO; Final Office Action dated Nov. 14, 2018 in U.S. Appl. No. 15/726,959. |
USPTO; Non-Final Office Action dated Nov. 28, 2018 in U.S. Appl. No. 15/795,056. |
USPTO; Non-Final Office Action dated Sep. 26, 2018 in U.S. Appl. No. 15/832,188. |
USPTO; Notice of Allowance dated Dec. 10, 2018 in U.S. Appl. No. 15/863,340. |
USPTO; Restriction Requirement dated Dec. 13, 2018 in U.S. Appl. No. 15/886,225. |
USPTO; Non-Final Office Action dated Nov. 15, 2018 in U.S. Appl. No. 15/890,037. |
USPTO; Restriction Requirement dated Oct. 9, 2018 in U.S. Appl. No. 15/892,756. |
USPTO; Restriction Requirement dated Nov. 26, 2018 in U.S. Appl. No. 15/917,262. |
USPTO; Restriction Requirement dated Nov. 2, 2018 in U.S. Appl. No. 16/018,692. |
WIPO; International Search Report and Written Opinion dated Nov. 6, 2018 in Application No. PCT/IB2017/001652. |
Beynet et al. “Low temperature plasma-enhanced ALD enables cost-effective spacer defined double patterning,” Proceedings of SPIE, 7520, (2009). |
Gupta et al., “Charge carrier transport and electroluminescence in atomic layer deposited poly-GaN/c-Si heterojunction diodes,” Journal of Applied Physics, 124, 084503 (2018). |
Mackenzie et al. “Stress Control of Si-Based PEVCD Dielectrics,” Proc. Symp. Silicon Nitrode and Silicon Dioxide Thin Insulating Films & Other Emerging Dielectrics VIII, 148-159 (2005). |
CNIPA; Office Action dated Dec. 14, 2018 in Application No. 201410331047.6. |
CNIPA; Notice of Allowance dated Jun. 14, 2019 in Application No. 201410331047.6. |
CNIPA; Office Action dated Jun. 28, 2019 in Application No. 201510765170.3. |
CNIPA; Office Action dated Oct. 19, 2018 in Application No. 201510765170.3. |
CNIPA; Office Action dated Oct. 31, 2018 in Application No. 201510765406.3. |
CNIPA; Office Action dated Jun. 28, 2019 in Application No. 201510765406.3. |
CNIPA; Office Action dated Mar. 14, 2019 in Application No. 201610141027.1. |
CNIPA; Office Action dated Dec. 20, 2018 in Application No. 201710738549.4. |
CNIPA; Office Action dated Jun. 20, 2019 in Application No. 201711120632.1. |
CNIPA; Notice of Allowance dated Nov. 1, 2018 in Application No. 201830397219.9. |
EPO; Office Action dated Jan. 11, 2019 in Application No. 09836647.9. |
JPO; Office Action dated Aug. 10, 2009 in Application No. 2003029767. |
JPO; Office Action dated Apr. 13, 2010 in Application No. 2003029767. |
JPO; Notice of Allowance dated Jun. 24, 2010 in Application No. 2003029767. |
JPO; Office Action dated Oct. 30, 2008 in Application No. 2004558313. |
JPO; Office Action dated Feb. 19, 2009 in Application No. 2004558313. |
JPO; Notice of Allowance dated Jun. 30, 2009 in Application No. 2004558313. |
JPO; Notice of Allowance dated Dec. 19, 2018 in Application No. 2014205548. |
JPO; Office Action dated Jun. 27, 2019 in Application No. 2015034774. |
JPO; Office Action dated Jan. 30, 2019 in Application No. 2015052198. |
JPO; Notice of Allowance dated Apr. 5, 2019 in Application No. 2015052198. |
KIPO; Office Action dated Jan. 12, 2019 in Application No. 10-2012-0064526. |
KIPO; Office Action dated Mar. 27, 2019 in Application No. 10-2012-0076564. |
KIPO; Office Action dated May 30, 2019 in Application No. 10-2012-7004062. |
KIPO; Decision of Intellectual Property Trial and Appeal Board dated May 13, 2019 in Application No. 10-2012-7004062. |
KIPO; Office Action dated Apr. 19, 2019 in Application No. 10-2013-0101944. |
KIPO; Office Action dated Apr. 24, 2019 in Application No. 10-2013-0036823. |
KIPO; Office Action dated May 31, 2019 in Application No. 10-2013-0050740. |
KIPO; Office Action dated Mar. 27, 2019 in Application No. 10-2013-0084459. |
KIPO; Office Action dated Apr. 30, 2019 in Application No. 10-2013-0088450. |
KIPO; Office Action dated May 21, 2019 in Application No. 10-2013-0121554. |
KIPO; Office Action dated Jan. 22, 2019 in Application No. 10-2014-7017110. |
KIPO; Notice of Allowance dated Feb. 27, 2018 in Application No. 10-2017-0175442. |
KIPO; Office Action dated Jan. 30, 2019 in Application No. 30-2018-0033442. |
KIPO; Notice of Allowance dated Apr. 1, 2019 in Application No. 30-2018-0033442. |
TIPO; Notice of Allowance dated Jan. 28, 2015 in Application No. 99114329. |
TIPO; Office Action dated Jun. 20, 2017 in Application No. 102125191. |
TIPO; Notice of Allowance dated Jan. 30, 2019 in Application No. 103132230. |
TIPO; Office Action dated Feb. 22, 2019 in Application No. 104105533. |
TIPO; Office Action dated Nov. 19, 2018 in Application No. 104105965. |
TIPO; Notice of Allowance dated May 9, 2019 in Application No. 104107876. |
TIPO; Notice of Allowance dated Apr. 26, 2019 in Application No. 104107888. |
TIPO; Office Action dated May 6, 2019 in Application No. 104108277. |
TIPO; Notice of Allowance dated May 8, 2019 in Application No. 104110326. |
TIPO; Office Action dated Apr. 29, 2019 in Application No. 104122889. |
TIPO; Office Action dated Jan. 30, 2019 in Application No. 104122890. |
TIPO; Notice of Allowance dated Jun. 19, 2019 in Application No. 104124377. |
TIPO; Office Action dated Jan. 7, 2019 in Application No. 104132991. |
TIPO; Notice of Allowance dated Apr. 12, 2019 in Application No. 104132991. |
TIPO; Office Action dated Apr. 25, 2019 in Application No. 104141679. |
TIPO; Office Action dated Apr. 25, 2019 in Application No. 105101536. |
TIPO; Notice of Allowance dated May 7, 2019 in Application No. 105104453. |
TIPO; Office Action dated Dec. 26, 2018 in Application No. 106127690. |
TIPO; Office Action dated Jan. 7, 2019 in Application No. 106138800. |
TIPO; Office Action dated Nov. 20, 2018 in Application No. 107118271. |
TIPO; Office Action dated Jun. 4, 2019 in Application No. 107123992. |
TIPO; Office Action dated May 28, 2019 in Application No. 107125586. |
TIPO; Notice of Allowance dated Feb. 21, 2019 in Application No. 107303723. |
TIPO; Office Action dated May 31, 2019 in Application No. 108102146. |
USPTO; Notice of Allowance dated Apr. 4, 2019 in U.S. Appl. No. 12/618,355. |
USPTO; Advisory Action dated Feb. 4, 2019 in U.S. Appl. No. 13/169,951. |
USPTO; Notice of Allowance dated Apr. 4, 2019 in U.S. Appl. No. 13/169,951. |
USPTO; Final Office Action dated Dec. 28, 2018 in U.S. Appl. No. 13/184,351. |
USPTO; Final Office Action dated Mar. 15, 2019 in U.S. Appl. No. 13/651,144. |
USPTO; Final Office Action dated Jan. 25, 2019 in U.S. Appl. No. 14/188,760. |
USPTO; Advisory Action dated Jan. 22, 2019 in U.S. Appl. No. 14/219,839. |
USPTO; Non-Final Office Action dated Jul. 15, 2019 in U.S. Appl. No. 14/219,839. |
USPTO; Advisory Action dated Jan. 22, 2019 in U.S. Appl. No. 14/219,879. |
USPTO; Non-Final Office Action dated Jun. 24, 2019 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office Action dated Feb. 7, 2019 in U.S. Appl. No. 14/444,744. |
USPTO; Non-Final Office Action dated Jan. 11, 2019 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Action dated Jun. 25, 2019 in U.S. Appl. No. 14/457,058. |
USPTO; Non-Final Office Action dated Apr. 4, 2019 in U.S. Appl. No. 14/508,489. |
USPTO; Non-Final Office Action dated Dec. 28, 2018 in U.S. Appl. No. 14/752,712. |
USPTO; Notice of Allowance dated Jun. 11, 2019 in U.S. Appl. No. 14/752,712. |
USPTO; Final Office Action dated Feb. 25, 2019 in U.S. Appl. No. 14/793,323. |
UPSTO; Non-Final Office Action dated Jun. 27, 2019 in U.S. Appl. No. 14/793,323. |
USPTO; Final Office Action dated Apr. 18, 2019 in U.S. Appl. No. 14/829,565. |
USPTO; Advisory Action dated Jul. 22, 2019 in U.S. Appl. No. 14/829,565. |
USPTO; Notice of Allowance dated Mar. 25, 2019 in U.S. Appl. No. 14/997,683. |
USPTO; Non-Final Office Action dated Jun. 3, 2019 in U.S. Appl. No. 15/060,412. |
USPTO; Notice of Allowance dated Dec. 21, 2018 in U.S. Appl. No. 15/067,028. |
USPTO; Notice of Allowance dated Feb. 25, 2019 in U.S. Appl. No. 15/074,813. |
USPTO; Final Office Action dated Mar. 14, 2019 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Jul. 19, 2019 in U.S. Appl. No. 15/135,258. |
USPTO; Notice of Allowance dated Mar. 13, 2019 in U.S. Appl. No. 15/144,506. |
USPTO; Final Office Action dated Mar. 28, 2019 in U.S. Appl. No. 15/182,504. |
USPTO; Notice of Allowance dated Jul. 17, 2019 in U.S. Appl. No. 15/182,504. |
USPTO; Non-Final Office Action dated Mar. 28, 2019 in U.S. Appl. No. 15/205,827. |
USPTO; Notice of Allowance dated Apr. 19, 2019 in U.S. Appl. No. 15/222,780. |
USPTO; Non-Final Office Action dated Jan. 30, 2019 in U.S. Appl. No. 15/262,990. |
USPTO; Final Office Action dated May 13, 2019 in U.S. Appl. No. 15/262,990. |
USPTO; Advisory Action dated Jul. 22, 2019 in U.S. Appl. No. 15/262,990. |
USPTO; Final Office Action dated Jan. 11, 2019 in U.S. Appl. No. 15/273,488. |
USPTO; Notice of Allowance dated Apr. 19, 2019 in U.S. Appl. No. 15/273,488. |
USPTO; Final Office Action dated Feb. 7, 2019 in U.S. Appl. No. 15/286,503. |
USPTO; Non-Final Office Action dated Jun. 27, 2019 in U.S. Appl. No. 15/286,503. |
USPTO; Non-Final Office Action dated Dec. 14, 2018 in U.S. Appl. No. 15/340,512. |
USPTO; Notice of Allowance dated May 24, 2019 in U.S. Appl. No. 15/340,512. |
USPTO; Final Office Action dated Jun. 25, 2019 in U.S. Appl. No. 15/377,439. |
USPTO; Non-Final Office Action dated May 31, 2019 in U.S. Appl. No. 15/380,909. |
USPTO; Non-Final Office Action dated Feb. 25, 2019 in U.S. Appl. No. 15/380,921. |
USPTO; Non-Final Office Action dated Feb. 5, 2019 in U.S. Appl. No. 15/402,993. |
USPTO; Final Office Action dated May 21, 2019 in U.S. Appl. No. 15/402,993. |
USPTO; Final Office Action dated Feb. 4, 2019 in U.S. Appl. No. 15/410,503. |
USPTO; Non-Final Office Action dated Apr. 25, 2019 in U.S. Appl. No. 15/410,503. |
USPTO; Final Office Action dated Jan. 11, 2019 in U.S. Appl. No. 15/428,808. |
USPTO; Notice of Allowance dated Apr. 25, 2019 in U.S. Appl. No. 15/428,808. |
USPTO; Non-Final Office Action dated Jan. 25, 2019 in U.S. Appl. No. 15/434,051. |
USPTO; Notice of Allowance dated Jun. 3, 2019 in U.S. Appl. No. 15/434,051. |
USPTO; Final Office Action dated Feb. 27, 2019 in U.S. Appl. No. 15/489,453. |
USPTO; Non-Final Office Action dated Jun. 5, 2019 in U.S. Appl. No. 15/489,453. |
USPTO; Final Office Action dated May 1, 2019 in U.S. Appl. No. 15/491,726. |
USPTO; Final Office Action dated Mar. 6, 2019 in U.S. Appl. No. 15/589,849. |
USPTO; Non-Final Office Action dated Jun. 28, 2019 in U.S. Appl. No. 15/589,849. |
USPTO; Non-Final Office Action dated Dec. 21, 2018 in U.S. Appl. No. 15/589,861. |
USPTO; Final Office Action dated Jun. 26, 2019 in U.S. Appl. No. 15/589,861. |
USPTO; Advisory Action dated Mar. 15, 2019 in U.S. Appl. No. 15/592,730. |
USPTO; Non-Final Office Action dated Mar. 7, 2019 in U.S. Appl. No. 15/598,169. |
USPTO; Final Office Action dated Jun. 25, 2019 in U.S. Appl. No. 15/598,169. |
USPTO; Ex Parte Quayle Action dated Mar. 21, 2019 in U.S. Appl. No. 15/615,489. |
USPTO; Non-Final Office Action dated Feb. 1, 2019 in U.S. Appl. No. 15/627,189. |
USPTO; Notice of Allowance dated May 21, 2019 in U.S. Appl. No. 15/627,189. |
USPTO; Final Office Action dated Mar. 6, 2019 in U.S. Appl. No. 15/636,307. |
USPTO; Non-Final Office Action dated Jul. 16, 2019 in U.S. Appl. No. 15/636,307. |
USPTO; Notice of Allowance dated Jun. 24, 2019 in U.S. Appl. No. 15/650,686. |
USPTO; Notice of Allowance dated Feb. 21, 2019 in U.S. Appl. No. 15/659,631. |
USPTO; Non-Final Office Action dated Mar. 1, 2019 in U.S. Appl. No. 15/660,805. |
USPTO; Notice of Allowance dated Feb. 21, 2019 in U.S. Appl. No. 15/662,107. |
USPTO; Notice of Allowance dated Mar. 20, 2019 in U.S. Appl. No. 15/672,063. |
USPTO; Non-Final Office Action dated Feb. 8, 2019 in U.S. Appl. No. 15/672,119. |
USPTO; Final Office Action dated Jul. 16, 2019 in U.S. Appl. No. 15/672,119. |
USPTO; Notice of Allowance dated Jan. 9, 2019 in U.S. Appl. No. 15/673,110. |
USPTO; Notice of Allowance dated May 6, 2019 in U.S. Appl. No. 15/673,278. |
USPTO; Notice of Allowance dated Jan. 9, 2019 in U.S. Appl. No. 15/683,701. |
USPTO; Non-Final Office Action dated Mar. 19, 2019 in U.S. Appl. No. 15/691,241. |
USPTO; Final Office Action dated Jan. 11, 2019 in U.S. Appl. No. 15/691,241. |
USPTO; Notice of Allowance dated Apr. 16, 2019 in U.S. Appl. No. 15/705,955. |
USPTO; Non-Final Office Action dated Feb. 11, 2019 in U.S. Appl. No. 15/707,786. |
USPTO; Non-Final Office Action dated Jun. 25, 2019 in U.S. Appl. No. 15/719,208. |
USPTO; Notice of Allowance dated Apr. 19, 2019 in U.S. Appl. No. 15/726,222. |
USPTO; Notice of Allowance dated Jan. 23, 2019 in U.S. Appl. No. 15/729,485. |
USPTO; Final Office Action dated Apr. 19, 2019 in U.S. Appl. No. 15/795,056. |
USPTO; Final Office Action dated Feb. 21, 2019 in U.S. Appl. No. 15/796,593. |
USPTO; Non-Final Office Action dated Dec. 21, 2018 in U.S. Appl. No. 15/798,150. |
USPTO; Notice of Allowance dated May 14, 2019 in U.S. Appl. No. 15/798,150. |
USPTO; Final Office Action dated Dec. 14, 2018 in U.S. Appl. No. 15/798,201. |
USPTO; Final Office Action dated Mar. 7, 2019 in U.S. Appl. No. 15/815,483. |
USPTO; Notice of Allowance dated Dec. 5, 2017 in U.S. Appl. No. 15/832,188. |
USPTO; Non-Final Office Action dated Mar. 13, 2019 in U.S. Appl. No. 15/836,547. |
USPTO; Non-Final Office Action dated Jan. 11, 2019 in U.S. Appl. No. 15/879,209. |
USPTO; Non-Final Office Action dated Jan. 22, 2019 in U.S. Appl. No. 15/879,209. |
USPTO; Non-Final Office Action dated Apr. 17, 2019 in U.S. Appl. No. 15/886,225. |
USPTO; Final Office Action dated May 2, 2019 in U.S. Appl. No. 15/890,037. |
USPTO; Notice of Allowance dated Feb. 8, 2019 in U.S. Appl. No. 15/892,756. |
USPTO; Non-Final Office Action dated Apr. 24, 2019 in U.S. Appl. No. 15/896,986. |
USPTO; Non-Final Office Action dated May 30, 2019 in U.S. Appl. No. 15/900,425. |
USPTO; Non-Final Office Action dated Mar. 8, 2019 in U.S. Appl. No. 15/917,224. |
USPTO; Non-Final Office Action dated Feb. 8, 2019 in U.S. Appl. No. 15/917,262. |
USPTO; Final Office Action dated Jun. 14, 2019 in U.S. Appl. No. 15/917,262. |
USPTO; Non-Final Office Action dated May 8, 2019 in U.S. Appl. No. 15/925,532. |
USPTO; Non-Final Office Action dated Mar. 29, 2019 in U.S. Appl. No. 15/940,801. |
USPTO; Notice of Allowance dated May 31, 2019 in U.S. Appl. No. 15/957,565. |
USPTO; Non-Final Office Action dated Apr. 19, 2019 in U.S. Appl. No. 15/985,298. |
USPTO; Non-Final Office Action dated Feb. 21, 2019 in U.S. Appl. No. 15/987,755. |
USPTO; Non-Final Office Action dated Jul. 16, 2019 in U.S. Appl. No. 16/014,981. |
USPTO; Non-Final Office Action dated Jan. 24, 2019 in U.S. Appl. No. 16/018,692. |
USPTO; Notice of Allowance dated Apr. 9, 2019 in U.S. Appl. No. 16/026,711. |
USPTO; Non-Final Office Action dated Apr. 25, 2019 in U.S. Appl. No. 16/038,024. |
USPTO; Non-Final Office Action dated Apr. 2, 2019 in U.S. Appl. No. 16/147,047. |
USPTO; Notice of Allowance dated Apr. 17, 2019 in U.S. Appl. No. 16/171,098. |
USPTO; Notice of Allowance dated May 1, 2019 in U.S. Appl. No. 16/171,098. |
USPTO; Non-Final Office Action dated Apr. 2, 2019 in U.S. Appl. No. 16/188,690. |
USPTO; Notice of Allowance dated Jun. 13, 2019 in U.S. Appl. No. 16/396,475. |
USPTO; Non-Final Office Action dated Apr. 16, 2019 in U.S. Appl. No. 29/604,101. |
USPTO; Non-Final Office Action dated Feb. 20, 2019 in U.S. Appl. No. 29/646,377. |
WIPO; International Search Report and Written Opinion dated Jan. 25, 2019 in Application No. PCT/IB2018/000192. |
WIPO; International Search Report and Written Opinion dated Jan. 4, 2019 in Application No. PCT/IB2018/000936. |
WIPO; International Search Report and Written Opinion dated Dec. 20, 2018 in Application No. PCT/IB2018/001003. |
WIPO; International Search Report and Written Opinion dated Dec. 20, 2018 in Application No. PCT/IB2018/001022. |
WIPO; International Search Report and Written Opinion dated May 23, 2019 in Application No. PCT/IB2019/050974. |
Arita et al. “Electrical and optical properties of germanium-doped zinc oxide thin films” Materials Transactions, vol. 45, No. 11, pp. 3180-3183 (2004). |
Arnold et al., “Novel single-layer vanadium sulphide phases” 2D Materials, 5, 045009, 11 pages. |
Boscher et al., “Atmosphere Pressure Chemical Vapour Deposition of NbSe2 Thin Films on Glass” Eur. J. Inorg. Chem., pp. 1255-1259 (2006). |
Carmalt et al., “Chemical Vapor Deposition of Niobium Disulfide Thin Films” Eur. J. Inorg. Chem., pp. 4470-4476 (2004). |
Casey et al. “Chemical Vapor Deposition of Mo onto Si” J. Electrochem. Soc.: Solid State Science, 114 (2), pp. 201-204 (1967). |
Chen et al., “Develop Gap-fill Process of Shallow Trench Isolation in 450mm Wafer by Advanced Flowable CVD Technology for Sub-20nm Node,” 2016 27th Annual Semi Advanced Semiconductor Manufacturing Conference (ASMC), IEEE, May 16, 2016, pp. 157-159 (2016). |
Cheng et al., “Effect of carrier gas on the structure and electric properties of low dielectric constant SiCOH film using trimethylsilane prepared by plasma enhanced chemical vapor deposition,” Thin Solid Films vol. 469-470, pp. 178-183 (2004). |
Conroy et al., “The Preparation and Properties of Single Crystals of the 1S and 2S Polymorphs of Tantalum Disulfide” J. Solid State Chemistry, 4, pp. 345-350 (1972). |
De Silva et al., “Inorganic Hardmask Development for Extreme Ultraviolet Patterning,” Journal of Micro/Nanolithography, MEMS, and MOEMS 18(1) (2018). |
Duffey et al., “Raman Scattering from 1T-TaS2” Solid State Communications 20, pp. 617-621. |
Elers et al. “Film Uniformity in Atomic Layer Deposition,” Chemical Vapor Deposition, 12, pp. 13-24 (2006). |
Fu et al., “Controlled Synthesis of Atomically Thin 1T-TaS2 for Tunable Charge Density Wave Phase Transitions” Chem. Mater. 28, pp. 7613-7618 (2016). |
Gesheva et al. “Composition and Microstructure of Black Molybdenum Photothermal Converter Layers Deposited by the Pyrolytic Hydrogen Reduction of MoO2Cl2” Thin Solid Films, 79, pp. 39-49 (1981). |
Gole et al. “Preparation of Nickel Sulfide Thin Films and Nanociystallites Using Nickel Furfuraldehyde Thiosemicarbazone as Single-source Precursor,” Advanced Materials Research, vols. 383-390, pp. 3828-3834 (2012). |
Habib et al. “Atmospheric oxygen plasma activation of silicon (100) surfaces,” American Vacuum Society, 28(3), pp. 476-485 (2010). |
Han et al., “van der Waals Metallic Transition Metal Dichalcogenides” Chem. Rev. 118, pp. 6297-6336 (2018). |
Heyne et al., “The conversion mechanism of amorphous silicon to stoichiometric W52” J. Materials Chemistry C, 6, pp. 4122-4130 (2018). |
Hossain et al., “Recent Advances in Two-Dimensional Materials with Charge Density Waves: Synthesis, Characterization and Applications” Crystals 7, 298, 19 pages (2017). |
Johansson et al. “Towards absolute asymmetric synthesis. Synthesis and crystal structure of stereochemically labile MC12 (M=Co, Ni, Cu, Zn) complexes with diamine ligands,” Inorganica Chimica Acta 358, pp. 3293-3302 (2005). |
Jung et al. “New Mechanisms for Ozone-Based ALO Growth of High-k Dielectrics via Nitrogen-Oxygen Species” ECS Transactions, 33(2), pp. 91-99 (2010). |
Kern et al., “Chemically Vapor-Deposited Borophosphosilicate Glasses for Silicon Device Applications” RCE Review, 43, 3, pp. 423-457 (1982). |
Kerrigan et al. “Low Temperature, Selective Atomic Layer Deposition of Cobalt Metal Films Using Bis(1,4-di-tert-butyl-1,3-diazadienyl)cobalt and Alkylamine Precursors,” Chem. Materials, 29, pp. 7458-7466 (2017). |
Kim et al., “Novel Flowable CVD Process Technology for sub-20nm Interlayer Dielectrics,” IEEE International Interconnect Conference (IITC 2012), San Jose, California, USA, Jun. 4-6, 2012, pp. 1-3 (2012). |
Kogelschatz et al. “Ozone Generation from Oxygen and Air: Discharge Physics and Reaction Mechanisms” Ozone Science & Engineering, 10, pp. 367-378 (1998). |
Kukli et al., “Influence of atomic layer deposition parameters on the phase content of Ta2O5 films” J. Crystal Growth, 212, pp. 459-468 (2000). |
Kukli et al. “Properties of tantalum oxide thin films grown by atomic layer deposition” Thin Solid Films, 260, pp. 135-142 (1995). |
Kwon et al., “Substrate Selectivity of (tBu-Allyl)Co(CO)3 during Thermal Atomic Layer Deposition of Cobalt,” Chem. Materials, 24, pp. 1025-1030 (2012). |
Lee et al., “Characteristics of Low-K Sioc Films Deposited Via Atomic Layer Deposition,” Thin Solid Films 645, pp. 334-339 (2018). |
Levy et al., “Reflow Mechanisms of Contact Vias in VLSI Processing” J. Electrochem. Soc.: Solid-State Science and Technology, 133, 7, pp. 1417-1424 (1986). |
Li et al., “Metallic Transition-Metal Dichalcogenide Nanocatalysts for Energy Conversion” Chem. 4, pp. 1510-1537 (2018). |
Lieberman, et al., “Principles of Plasma Discharges and Materials Processing” Second Edition, 368-381 (2005). |
Lim et al. “Synthesis and Characterization of Volatile, Thermally Stable, Reactive Transistion Metal Amidinates,” Inorg. Chem., 42, pp. 7951-7958 (2003). |
Liu et al., “Van der Waals metal-semiconductor junction: Weak Fermi level pinning enables effective tuning of Schottky barrier” Sci. Adv. 2: e1600069, 7 pages (2016). |
Maeno, “Gecko Tape Using Carbon Nanotubes,” Nitto Denko Gihou, 47, 48-51 (2009). |
Makela et al. “Thermal Atomic Layer Deposition of Continuous and Highly Conducting Gold Thin Films,” Chem. Materials, 29, pp. 6130-6136 (2017). |
Mattinen et al., “Crystalline tungsten sulfide thin films by atomic layer deposition and mild annealing” J. Vac. Sci. Tech. 37, 020921, 35 pages (2019). |
Nakano et al., “Layer-by-Layer Epitaxial Growth of Scalable WSe2 on Sapphire by Molecular Beam Epitaxy” Nano. Lett. 17, pp. 5595-5599 (2017). |
Ngo et al. “Atomic layer deposition of photoactive CoO/SrTiO3 and CoO/TiO2 on Si(001) for visible light driven photoelectrochemical water oxidation,” J. Applied Physics, 114, 9 pages (2013). |
Ohchi et al. “Reducing damage to Si substrates during gate etching processes.” Japanese Journal of Applied Physics 47.7R 5324 (2008). |
Radamson et al. “Growth of Sn-alloyed Group IV Materials for Photonic and Electronic Applications” Chapter 5 pp. 129-144, Manufacturing Nano Structures (2014). |
Ryu et al., “Persistent Charge-Density-Wave Order in Single-Layer TaSe2” Nano. Lett. 18, pp. 689-694 (2018). |
Samal et al., “Low-Temperature (<200° C.) Plasma Enhanced Atomic Deposition of Dense Titanium Nitride Thin Films” (2012). |
Sanders et al., “Crystalline and electronic structure of single-layer TaS2” Phys. Rev. B. 94, 081404, 6 pages (2016). |
Schindler, Dissertation, Next Generation High-k Dielectrics for DRAM Produced by Atomic Layer Deposition Studied by Transmission Electron Microscopy (2015). |
Sellers, Making Your Own Timber Dogs, Paul Sellers blog, Published on Nov. 18, 2014, [online], [site visted Jun. 10, 2017]. Available from Internet, <URL: https://paulsellers.com/2014/11/making-your-own-timber-dogs/>. |
Seshadri et al., “Ultrathin Extreme Ultraviolet Patterning Stack Using Polymer Brush As an Adhesion Promotion Layer,” Journal of Micro/Nanolithography, MEMS, and MOEMS 16(3) (2017). |
Simchi et al., “Sulfidation of 2D transition metals (Mo, W, Re, Nb, Ta): thermodynamics, processing, and characterization” J. Materials Science 52: 17, 9 pages (2017). |
Stanley et al. “Feedgas for Modern High-Performance Ozone Generators” Ozonia Ltd., Duebendorf, Switzerland. 7 pages. Available Jul. 14, 2017 online at: http://www.degremont-technologies.com/cms_medias/podf/tech_ozonia_feedgas.pdf (1999). |
Svetin et al., “Three-dimensional resistivity and switching between correlated electronic states in 1T-TaS2” Nature, Scientific Reports Apr. 12, 2017, 7:46048, 10 pages (2017). |
Tatehaba et al., “Adhesion Energy of Polystyrene and Substrate in Function Water,” 5th International Symposium of Cleaning Technology in Semiconductor Device Manufacturing, pp. 560-565 (1998). |
Todi et al., “Characterization of Pt—Ru Binary Alloy Thin Films for Work Function Tuning,” IEEE Electron Device Letters, vol. 27, No. 7, pp. 542-545 (2006). |
Ueda et al. “Enhanced Sidewall Grown (ESG) process: towards PEALD with conformality above 100%,” Extended Abstracts of the 2011 International Conference on Solid State Devices and Materials, Nagoya, pp. 34-35 (2011). |
Vasilev, “Borophosphosilicate Glass Films in Silicon Microelectronics, Part 1: Chemical Vapor Deposition, Composition, and Properties” Russian Microelectronics, vol. 33, No. 5, pp. 271-284 (2004). |
Xing et al., “Ising Superconductivity and Quantum Phase Transition in Macro-Size Monolayer NbSe2” Nano. Lett. 17, pp. 6802-6807 (2017). |
Xu et al., “Contacts between Two- and Three-Dimensional Materials: Ochmic, Schottky, and p-n Heterojunctions” ACS Nano 10, pp. 4895-4919 (2016). |
Yuan et al., “Facile Synthesis of Single Crystal Vanadium Disulfide Nanosheets by Chemical Vapor Deposition for Efficient Hydrogen Evolution Reaction” Adv. Mater. 27, pp. 5605-5609 (2015). |
Zhou et al., “A library of atomically thin metal chalcogenides” Nature 556, pp. 355-361 (2018). |
CNIPA; Notice of Allowance dated Sep. 3, 2019 in Application No. 201610141027.1. |
CNIPA; Notice of Allowance dated Sep. 30, 2010 in Application No. 201510765170.3. |
CNIPA; Office Action dated Jul. 23, 2019 in Application No. 201610897958.4. |
EPO; Notice of Allowance dated Aug. 1, 2019 in Application No. 09767208.3. |
JPO; Office Action dated Aug. 29, 2019 in Application No. 2016001928. |
KIPO; Notice of Allowance dated Jul. 5, 2019 in Application No. 10-2012-0064526. |
KIPO; Notice of Allowance dated Aug. 29, 2019 in Application No. 10-2013-0036823. |
KIPO; Office Action dated Aug. 27, 2019 in Application No. 10-2013-0049598. |
KIPO; Office Action dated Aug. 27, 2019 in Application No. 10-2013-0089998. |
KIPO; Notice of Allowance dated Oct. 8, 2019 in Application No. 10-2013-0101944. |
KIPO; Office Action dated Aug. 15, 2019 in Application No. 10-2013-0109390. |
KIPO; Office Action dated Oct. 7, 2019 in Application No. 10-2013-0114079. |
KIPO; Notice of Allowance dated Aug. 26, 2019 in Application No. 10-2014-7017110. |
KIPO; Final Office Action dated Jun. 17, 2019 in Application No. 10-2017-7023740. |
TIPO; Office Action dated Aug. 16, 2019 in Application No. 102136496. |
TIPO; Notice of Allowance dated Jul. 10, 2019 in Application No. 103123439. |
TIPO; Notice of Allowance dated Sep. 27, 2019 in Application No. 104105533. |
TIPO; Notice of Allowance dated Sep. 23, 2019 in Application No. 104105965. |
TIPO; Notice of Allowance dated Oct. 4, 2019 in Application No. 104122889. |
TIPO; Notice of Allowance dated Jul. 19, 2019 in Application No. 104122890. |
TIPO; Office Action dated Jul. 5, 2019 in Application No. 105112363. |
TIPO; Office Action dated Sep. 9, 2019 in Application No. 105115513. |
TIPO; Notice of Allowance dated Sep. 20, 2019 in Application No. 106138800. |
TIPO; Office Action dated Aug. 27, 2019 in Application No. 107116804. |
TIPO; Office Action dated Jun. 28, 2019 in Application No. 108102948. |
USPTO; Non-Final Office Action dated Aug. 19, 2019 in U.S. Appl. No. 13/184,351. |
USPTO; Advisory Action dated Feb. 12, 2016 in U.S. Appl. No. 13/651,144. |
USPTO; Advisory Action dated Dec. 29, 2016 in U.S. Appl. No. 13/651,144. |
USPTO; Non-Final Office Action dated Sep. 18, 2019 in U.S. Appl. No. 13/651,144. |
USPTO; Advisory Action dated Jun. 26, 2015 in U.S. Appl. No. 13/791,246. |
USPTO; Notice of Allowance dated Apr. 22, 2016 in U.S. Appl. No. 14/172,220. |
USPTO; Non-Final Office Action dated Aug. 8, 2019 in U.S. Appl. No. 14/188,760. |
USPTO; Notice of Allowance dated Aug. 19, 2016 in U.S. Appl. No. 14/268,348. |
USPTO; Non-Final Office Action dated Aug. 8, 2019 in U.S. Appl. No. 14/444,744. |
USPTO; Advisory Action dated Nov. 6, 2015 in U.S. Appl. No. 14/457,058. |
USPTO; Notice of Allowance dated Aug. 16, 2017 in U.S. Appl. No. 14/606,364. |
USPTO; Notice of Allowance dated Aug. 15, 2019 in U.S. Appl. No. 14/645,234. |
USPTO; Non-Final Office Action dated Sep. 19, 2019 in U.S. Appl. No. 14/829,565. |
USPTO; Final Office Action dated Jun. 10, 2016 in U.S. Appl. No. 14/987,420. |
USPTO; Notice of Allowance dated Mar. 26, 2018 in U.S. Appl. No. 15/144,481. |
USPTO; Final Office Action dated Aug. 9, 2019 in U.S. Appl. No. 15/205,827. |
USPTO; Non-Final Office Action dated Aug. 5, 2019 in U.S. Appl. No. 15/262,990. |
USPTO; Advisory Action dated Jul. 29, 2019 in U.S. Appl. No. 15/402,993. |
USPTO; Notice of Allowance dated Aug. 14, 2019 in U.S. Appl. No. 15/410,503. |
USPTO; Final Office Action dated Aug. 20, 2019 in U.S. Appl. No. 14/508,489. |
USPTO; Notice of Allowance dated Aug. 21, 2019 in U.S. Appl. No. 15/592,730. |
USPTO; Notice of Allowance dated Sep. 11, 2019 in U.S. Appl. No. 15/598,169. |
USPTO; Non-Final Office Action dated Sep. 4, 2019 in U.S. Appl. No. 15/615,489. |
USPTO; Non-Final Office Action dated Jul. 29, 2019 in U.S. Appl. No. 15/660,797. |
USPTO; Notice of Allowance dated Aug. 22, 2019 in U.S. Appl. No. 15/660,805. |
USPTO; Final Office Action dated Jul. 26, 2019 in U.S. Appl. No. 15/690,017. |
USPTO; Final Office Action dated Aug. 12, 2019 in U.S. Appl. No. 15/707,786. |
USPTO; Non-Final Office Action dated Jul. 8, 2019 in U.S. Appl. No. 15/726,959. |
USPTO; Final Office Action dated Jul. 31, 2019 in U.S. Appl. No. 15/795,056. |
UPSTO; Non-Final Office Action dated Oct. 2, 2019 in U.S. Appl. No. 15/798,201. |
USPTO; Non-Final Office Action dated Aug. 20, 2019 in U.S. Appl. No. 15/815,483. |
USPTO; Notice of Allowance dated Aug. 16, 2019 in U.S. Appl. No. 15/836,547. |
USPTO; Non-Final Office Action dated Jul. 31, 2019 in U.S. Appl. No. 15/860,564. |
USPTO; Final Office Action dated Aug. 21, 2019 in U.S. Appl. No. 15/879,209. |
USPTO; Notice of Allowance dated Sep. 23, 2019 in U.S. Appl. No. 15/886,225. |
USPTO; Non-Final Office Action dated Sep. 19, 2019 in U.S. Appl. No. 15/897,578. |
USPTO; Final Office Action dated Aug. 28, 2019 in U.S. Appl. No. 15/917,224. |
USPTO; Notice of Allowance dated Aug. 30, 2019 in U.S. Appl. No. 15/917,262. |
USPTO; Non-Final Office Action dated Jul. 22, 2019 in U.S. Appl. No. 15/940,759. |
USPTO; Notice of Allowance dated Aug. 26, 2019 in U.S. Appl. No. 15/940,801. |
USPTO; Notice of Allowance dated Aug. 22, 2019 in U.S. Appl. No. 15/985,298. |
USPTO; Notice of Allowance dated Jul. 31, 2019 in U.S. Appl. No. 15/987,755. |
USPTO; Non-Final Office Action dated Jul. 29, 2019 in U.S. Appl. No. 16/000,125. |
USPTO; Final Office Action dated Aug. 23, 2019 in U.S. Appl. No. 16/018,692. |
USPTO; Non-Final Office Action dated Aug. 7, 2019 in U.S. Appl. No. 16/024,390. |
USPTO; Notice of Allowance dated Jul. 10, 2019 in U.S. Appl. No. 16/046,218. |
USPTO; Final Office Action dated Sep. 25, 2019 in U.S. Appl. No. 16/147,047. |
USPTO; Non-Final Office Action dated Aug. 6, 2019 in U.S. Appl. No. 16/158,077. |
USPTO; Final Office Action dated Sep. 26, 2019 in U.S. Appl. No. 16/188,690. |
USPTO; Non-Final Office Action dated Aug. 29, 2019 in U.S. Appl. No. 16/161,744. |
USPTO; Non-Final Office Action dated Aug. 16, 2019 in U.S. Appl. No. 16/167,225. |
USPTO; Non-Final Office Action dated Aug. 19, 2019 in U.S. Appl. No. 16/208,062. |
USPTO; Non-Final Office Action dated Sep. 16, 2019 in U.S. Appl. No. 16/213,702. |
USPTO; Non-Final Office Action dated Aug. 21, 2019 in U.S. Appl. No. 29/634,768. |
WIPO; International Search Report and Written Opinion dated Jun. 28, 2019 in Application No. PCT/IB2019/000084. |
Bark et al. “Large-area niobium disulfide thin films as transparent electrodes for devices based on two-dimensional materials,” Nanoscale, published online, 7 pages (2012). |
Barreca et al. “Cobalt oxide nanomaterials by vapor phase synthesis for fast and reversible lithium storage” J Phys Chem C,114, 10054-10060 (2010). |
Basuvalingam et al. “Ns-WeA6—Low Temperature ALD for Phase-controlled Synthesis of 2D Transition Metal (M=Ti, Nb) di-(MX2) and Tri-(MX3) Sulfides,” AVS 19th International Conference on Atomic Layer Deposition (ALD 2019)), Jul. 22, 2019, Abstract, 1 page (2019). |
Cahiez et al. “Cobalt-Catalyzed cross coupling reaction between functionalized primary and secondary alkyl halides and aliphatic grignard reagents” Adv. Synth. Catal, 350, 1484-1488 (2008). |
“Fiji F200 200mm Thermal/Plasma ALD Systems: Installation and Use Manual.” CAW-02635 Rev. 0.6 (Mar. 13, 2012). Cambridge NanoTech Inc. pp. 1-164 (2012). |
Ge et al. “Large-scale synthesis of NbS2 nanosheets with controlled orientation on graphene by ambient pressure CVD,” Nanoscale, vol. 5, 5773-5778 (2013). |
Gordon et al. “A Kinetic Model for Step Coverage by Atomic Layer Deposition in Narrow Holes or Trenches.” Chemical Vapor Deposition. 9 [2]. pp. 73-78 (2003). |
Hansen. “A Primer on Vacuum Pressure Measurement.” Vacuum Technology & Coating. Jun. 2009. pp. 36-42 (2009). |
Hansen. “Speed, Pressure and Throughput: Part 1 System Diagnostics.” Vacuum Technology & Coating. Sep. 2011. pp. 14-17 (2011). |
Hansen. “Speed, Pressure and Throughput: Part 2 Managing Gas Flow in High Vacuum Systems.” Vacuum Technology & Coating. Oct. 2011. pp. 19-22 (2011). |
Hansen. “Speed, Pressure and Throughput: Part 3 Automating the Pressure Control Process.” Vacuum Technology & Coating. Nov. 2011. pp. 22-25 (2011). |
Hansen. “Speed, Pressure and Throughput: Part 4 Outgassing and Base Pressure.” Vacuum Technology & Coating. Dec. 2011. pp. 22-25 (2011). |
Hansen. “Speed, Pressure and Throughput: Part 5 Leaks and Gas Flow in Leak Detection.” Vacuum Technology & Coating. Jan. 2012. pp. 18-21 (2011). |
Khandelwal et al. “Low-temperature Ar/N2 remote plasma nitridation of SiO2 thin films,” J. Vacuum Science & Technology A, 20(6), pp. 1989-1996 (2002). |
Kucheyev et al. “Mechanisms of Atomic Layer Deposition on Substrates with Ultrahigh Aspect Ratios.” Langmuir. 24 [3]. pp. 943-948 (2008). |
Londergan et al. “Engineered Low Resistivity Titanium-Tantalum Nitride Films by Atomic Layer Deposition,” Mat. Res. Soc. Symp. Proc., vol. 714E, pp. L5.3.1-L5.3.6 (2001). |
Naito et al. “Electrical Transport Properties in 2H—NbS2, -NbSe2, -TaS2 and -TaSe2,” J. of Physical Society of Japan, vol. 51, No. 1, 219-227 (1982). |
Pichler. “Intrinsic Point Defects, Impurities and Their Diffusion in Silicon,” Springer-Verlag Wien, p. 367 (2004). |
Tidman et al. “Resistivity of thin TaS2 crystals,” Can. J. Phys., vol. 54, 2306-2309 (1976). |
Trumbore et al. “Solid solubilities of aluminum and gallium in germanium,” J. of Physics and Chemistry of Solids, vol. 11, Issues 3-4, 239-240 (1959). |
CNIPA; Notice of Allowance dated Dec. 27, 2019 in Application No. 201510765406.3. |
CNIPA; Office Action dated Nov. 4, 2019 in Application No. 201610898822.5. |
CNIPA; Office Action dated Nov. 11, 2019 in Application No. 201810379112.0. |
EPO; Extended European Search Report dated Nov. 29, 2019 in Application No. 19188826.2. |
JPO; Notice of Allowance dated Nov. 20, 2019 in Application No. JP2015034774. |
JPO; Notice of Allowance dated Dec. 17, 2019 in Application No. 2016001928. |
KIPO; Office Action dated Nov. 29, 2019 in Application No. 10-2013-0088450. |
KIPO; Notice of Allowance dated Jan. 13, 2020 in Application No. 10-2013-0088450. |
KIPO; Notice of Allowance dated Oct. 30, 2019 in Application No. 10-2013-0084459. |
KIPO; Office Action dated Dec. 4, 2019 in Application No. 10-2013-0098575. |
KIPO; Office Action dated Feb. 3, 2020 in Application No. 10-2014-0021615. |
KIPO; Office Action dated Feb. 15, 2020 in Application No. 10-2014-0027305. |
TIPO; Notice of Allowance dated Jan. 7, 2020 in Application No. 102136496. |
TIPO; Notice of Allowance dated Nov. 27, 2019 in Application No. 104141679. |
TIPO; Office Action dated Dec. 13, 2019 in Application No. 105101536. |
TIPO; Office Action dated Dec. 13, 2019 in Application No. 105111990. |
TIPO; Notice of Allowance dated Dec. 10, 2019 in Application No. 105112363. |
TIPO; Notice of Allowance dated Feb. 10, 2020 in Application No. 105115513. |
TIPO; Notice of Allowance dated Feb. 13, 2020 in Application No. 105122715. |
TIPO; Office Action dated Jan. 20, 2020 in Application No. 105122394. |
TIPO; Notice of Allowance dated Jan. 16, 2020 in Application No. 107116804. |
TIPO; Office Action dated Nov. 13, 2019 in Application No. 108115406. |
USPTO; Notice of Allowance dated Feb. 10, 2020 in U.S. Appl. No. 13/651,144. |
USPTO; Notice of Allowance dated Feb. 10, 2020 in U.S. Appl. No. 14/188,760. |
USPTO; Final Office Action dated Jan. 27, 2020 in U.S. Appl. No. 14/219,839. |
USPTO; Final Office Action dated Jan. 13, 2020 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office Action dated Dec. 26, 2019 in U.S. Appl. No. 15/060,412. |
USPTO; Advisory Action dated Jan. 3, 2020 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Feb. 13, 2020 in U.S. Appl. No. 15/135,258. |
USPTO; Notice of Allowance dated Dec. 3, 2019 in U.S. Appl. No. 15/205,827. |
USPTO; Final Office Action dated Nov. 19, 2019 in U.S. Appl. No. 15/262,990. |
USPTO; Advisory Action dated Jan. 30, 2020 in U.S. Appl. No. 15/262,990. |
USPTO; Final Office Action dated Jan. 6, 2020 in U.S. Appl. No. 15/286,503. |
USPTO; Final Office Action dated Dec. 12, 2019 in U.S. Appl. No. 15/380,909. |
USPTO; Non-Final Office Action dated Jan. 15, 2020 in U.S. Appl. No. 15/380,921. |
USPTO; Final Office Action dated Jan. 8, 2020 in U.S. Appl. No. 15/589,849. |
USPTO; Non-Final Office Action dated Jan. 13, 2020 in U.S. Appl. No. 15/589,861. |
USPTO; Advisory Action dated Jan. 17, 2020 in U.S. Appl. No. 15/636,307. |
USPTO; Notice of Allowance dated Feb. 7, 2020 in U.S. Appl. No. 15/672,119. |
USPTO; Final Office Action dated Jan. 24, 2020 in U.S. Appl. No. 15/691,241. |
USPTO; Notice of Allowance dated Jan. 29, 2020 in U.S. Appl. No. 15/719,208. |
USPTO; Final Office Action dated Jan. 7, 2020 in U.S. Appl. No. 15/726,959. |
USPTO; Notice of Allowance dated Jan. 6, 2020 in U.S. Appl. No. 15/727,432. |
USPTO; Non-Final Office Action dated Jun. 14, 2019 in U.S. Appl. No. 15/796,593. |
USPTO; Notice of Allowance dated Dec. 31, 2019 in U.S. Appl. No. 15/796,593. |
USPTO; Final Office Action dated Jan. 13, 2020 in U.S. Appl. No. 15/815,483. |
USPTO; Advisory Action dated Jan. 21, 2020 in U.S. Appl. No. 15/860,564. |
USPTO; Notice of Allowance dated Jan. 16, 2020 in U.S. Appl. No. 15/879,209. |
USPTO; Advisory Action dated Feb. 7, 2020 in U.S. Appl. No. 15/896,986. |
USPTO; Notice of Allowance dated Dec. 17, 2019 in U.S. Appl. No. 15/900,425. |
USPTO; Advisory Action dated Nov. 27, 2019 in U.S. Appl. No. 15/917,224. |
USPTO; Non-Final Office Action dated Dec. 23, 2019 in U.S. Appl. No. 15/923,834. |
USPTO; Final Office Action dated Nov. 27, 2019 in U.S. Appl. No. 15/925,532. |
USPTO; Non-Final Rejection dated Nov. 29, 2019 in U.S. Appl. No. 15/949,990. |
USPTO; Non-Final Office Action dated Jan. 31, 2020 in U.S. Appl. No. 15/962,980. |
USPTO; Non-Final Office Action dated Jan. 16, 2020 in U.S. Appl. No. 15/985,261. |
USPTO; Final Office Action dated Jan. 13, 2020 in U.S. Appl. No. 16/000,125. |
USPTO; Non-Final Office Action dated Jan. 16, 2020 in U.S. Appl. No. 16/014,981. |
USPTO; Non-Final Office Action dated Dec. 11, 2019 in U.S. Appl. No. 16/018,692. |
USPTO; Notice of Allowance dated Jan. 30, 2020 in U.S. Appl. No. 16/018,692. |
USPTO; Notice of Allowance dated Nov. 26, 2019 in U.S. Appl. No. 16/024,390. |
USPTO; Final Office Action dated Nov. 29, 2019 in U.S. Appl. No. 16/038,024. |
USPTO; Final Office Action dated Jan. 28, 2020 in U.S. Appl. No. 16/039,867. |
USPTO; Non-Final Office Action dated Feb. 6, 2020 in U.S. Appl. No. 16/117,530. |
USPTO; Non-Final Office Action dated Jan. 6, 2020 in U.S. Appl. No. 16/132,142. |
USPTO; Notice of Allowance dated Jan. 3, 2020 in U.S. Appl. No. 16/147,047. |
USPTO; Non-Final Office Action dated Nov. 5, 2019 in U.S. Appl. No. 16/152,260. |
USPTO; Final Office Action dated Dec. 16, 2019 in U.S. Appl. No. 16/167,225. |
USPTO; Notice of Allowance dated Dec. 16, 2019 in U.S. Appl. No. 16/188,690. |
USPTO; Notice of Allowance dated Jan. 28, 2020 in U.S. Appl. No. 16/208,062. |
USPTO; Notice of Allowance dated Dec. 9, 2019 in U.S. Appl. No. 16/213,702. |
USPTO; Non-Final Office Action dated Jan. 8, 2020 in U.S. Appl. No. 16/219,555. |
USPTO; Non-Final Office Action dated Jan. 30, 2020 in U.S. Appl. No. 16/245,006. |
USPTO; Final Office Action dated Jan. 10, 2020 in U.S. Appl. No. 16/251,534. |
USPTO; Non-Final Office Action dated Dec. 18, 2019 in U.S. Appl. No. 16/280,964. |
USPTO; Non-Final Office Action dated Jan. 9, 2020 in U.S. Appl. No. 16/317,774. |
USPTO; Non-Final Office Action dated Dec. 26, 2019 in U.S. Appl. No. 16/417,938. |
USPTO; Non-Final Office Action dated Dec. 31, 2019 in U.S. Appl. No. 16/427,288. |
USPTO; Non-Final Office Action dated Dec. 31, 2019 in U.S. Appl. No. 16/455,406. |
USPTO; Ex Parte Quayle Action dated Dec. 17, 2019 in U.S. Appl. No. 29/615,000. |
USPTO; Notice of Allowance dated Jan. 23, 2020 in U.S. Appl. No. 29/634,768. |
WIPO; International Search Report and Written Opinion dated Nov. 19, 2019 in Application No. PCT/IB2019/000127. |
WIPO; International Search Report and Written Opinion dated Jan. 10, 2020 in Application No. PCT/IB2019/000729. |
WIPO; International Search Report and Written Opinion dated Dec. 20, 2019 in Application No. PCT/IB2019/000805. |
WIPO; International Search Report and Written Opinion dated Dec. 20, 2019 in Application No. PCT/IB2019/000817. |
Alen, “Atomic layer deposition of TaN, NbN and MoN films for Cu Metallizations,” University of Helsinki Finland, 72 pages, (2005). |
Hamalainen et al., “Atomic Layer Deposition of Rhenium Disulfide,” Adv. Mater. 30.24, 6 pages (2018). |
Hargreaves et al., “New Fluorides and Oxyfluorides of Rhenium,” J. Chem. Soc., pp. 1099-1103 (1960). |
IPS Water Heater Pan Adapter Kit, Nov. 1, 2015, [online], [site visited Dec. 4, 2019]; URL: http://es.ipscorp.com/watertite/protectivesystem/whpanadapter (2015). |
Qin et al., “Chemical Vapor Deposition Growth of Degenerate p-Type Mo-Doped ReS2 Films and Their Homojunction,” ACS Appl. Mater. Interfaces, 9(18), pp. 15583-15591 (2007). |
Rhenium trioxide; https://en.wikipedia.org/wiki/Rhenium_trioxide [online]; last edited on Feb. 18, 2017. |
Saeki et al. “Reaction Process of Vanadium Tetrachloride with Ammonia in the Vapor Phase and Properties of the Vanadium Nitride Formed” Bull. Chem. Soc. Jpn., 55, pp. 3446-3449 (1982). |
EPO; Notice of Allowance dated Oct. 16, 2019 in Application No. 09836647.9. |
KIPO; Notice of Allowance dated Sep. 27, 2019 in Application No. 10-2012-7004062. |
KIPO; Office Action dated Nov. 27, 2019 in Application No. 10-2013-0050740. |
KIPO; Office Action dated Nov. 12, 2019 in Application No. 10-2013-0102026. |
KIPO; Notice of Allowance dated Oct. 21, 2019 in Application No. 10-2013-0109390. |
KIPO; Notice of Allowance dated Oct. 28, 2019 in Application No. 10-2013-0121554. |
KIPO; Notice of Allowance dated Nov. 29, 2019 in Application No. 10-2019-0127773. |
TIPO; Office Action dated Nov. 6, 2019 in Application No. 105101537. |
TIPO; Office Action dated Oct. 1, 2019 in Application No. 105114105. |
TIPO; Office Action dated Oct. 3, 2019 in Application No. 105119533. |
TIPO; Office Action dated Oct. 28, 2019 in Application No. 105122715. |
USPTO; Non-Final Office Action dated Oct. 31, 2019 in U.S. Appl. No. 14/457,058. |
USPTO; Advisory Action dated Oct. 28, 2019 in U.S. Appl. No. 14/508,489. |
USPTO; Notice of Allowance dated Nov. 14, 2019 in U.S. Appl. No. 14/793,323. |
USPTO; Final Office Action dated Oct. 24, 2019 in U.S. Appl. No. 15/135,258. |
USPTO; Advisory Action dated Oct. 22, 2019 in U.S. Appl. No. 15/205,827. |
USPTO; Non-Final Office Action dated Nov. 7, 2019 in U.S. Appl. No. 15/377,439. |
USPTO; Final Office Action dated Sep. 18, 2019 in U.S. Appl. No. 15/380,921. |
USPTO; Non-Final Office Action dated Oct. 24, 2019 in U.S. Appl. No. 15/402,993. |
USPTO; Notice of Allowance dated Oct. 7, 2019 in U.S. Appl. No. 15/489,453. |
USPTO; Non-Final Office Action dated Oct. 3, 2019 in U.S. Appl. No. 15/491,726. |
USPTO; Advisory Action dated Sep. 20, 2019 in U.S. Appl. No. 15/589,861. |
USPTO; Final Office Action dated Nov. 12, 2019 in U.S. Appl. No. 15/636,307. |
USPTO; Notice of Allowance dated Nov. 7, 2019 in U.S. Appl. No. 15/660,797. |
USPTO; Non-Final Office Action dated Oct. 10, 2019 in U.S. Appl. No. 15/672,096. |
USPTO; Advisory Action dated Sep. 23, 2019 in U.S. Appl. No. 15/672,119. |
USPTO; Non-Final Office Action dated Nov. 20, 2019 in U.S. Appl. No. 15/690,017. |
USPTO; Notice of Allowance dated Nov. 7, 2019 in U.S. Appl. No. 15/707,786. |
USPTO; Non-Final Office Action dated Sep. 26, 2019 in U.S. Appl. No. 15/727,432. |
USPTO; Non-Final Office Action dated Nov. 20, 2019 in U.S. Appl. No. 15/795,056. |
USPTO; Non-Final Office Action dated Nov. 15, 2019 in U.S. Appl. No. 15/802,154. |
USPTO; Final Office Action dated Nov. 13, 2019 in U.S. Appl. No. 15/860,564. |
USPTO; Advisory Action dated Nov. 5, 2019 in U.S. Appl. No. 15/879,209. |
USPTO; Non-Final Office Action dated Oct. 24, 2019 in U.S. Appl. No. 15/890,037. |
USPTO; Final Office Action dated Nov. 19, 2019 in U.S. Appl. No. 15/896,986. |
USPTO; Non-Final Office Action dated Jul. 25, 2019 in U.S. Appl. No. 16/039,867. |
USPTO; Notice of Allowance dated Oct. 3, 2019 in U.S. Appl. No. 16/200,100. |
USPTO; Non-Final Office Action dated Sep. 24, 2019 in U.S. Appl. No. 16/251,534. |
USPTO; Notice of Allowance dated Oct. 30, 2019 in U.S. Appl. No. 29/604,101. |
USPTO; Final Office Action dated Jul. 15, 2019 in U.S. Appl. No. 29/646,377. |
USPTO; Notice of Allowance dated Nov. 14, 2019 in U.S. Appl. No. 29/646,377. |
Ellis et al. “Nitrous Oxide (N2O) Processing for Silicon Oxynitride Gate Dielectrics.” IBM Journal of Research and Development. 1999. 43[3]. pp. 287-300. (1999). |
Hayashi et al. “Spectroscopic properties of nitrogen doped hydrogenated amorphous carbon films grown by radio frequency plasma-enhanced chemical vapor deposition,” Journal of Applied Physics. vol. 89, No. 12, pp. 7924-7931 (2001). |
Miller et al. “Carbon nitrides: synthesis and characterization of a new class of functional materials,” Phys.Chem.Chem.Phys., 19, pp. 15613-15638 (2017). |
Ohtsu et al. “Influences of Gap Distance on Plasma Characteristics in Narrow Gap Capacitatively Coupled Radio-Frequency Discharge,” vol. 43, No. 2, pp. 795-799 (2004). |
CNIPA; Office Action dated Jan. 21, 2020 in Application No. 201610028064.1. |
CNIPA; Office Action dated Feb. 28, 2020 in Application No. 201610897958.4. |
EPO; Extended European Search Report dated Mar. 3, 2020 in Application No. 19205558.0. |
KIPO; Office Action dated Feb. 28, 2020 in Application No. 10-2013-0049598. |
KIPO; Notice of Allowance dated Feb. 27, 2020 in Application No. 10-2013-0089998. |
KIPO; Notice of Allowance dated Mar. 4, 2020 in Application No. 10-2013-0114079. |
KIPO; Office Action dated Mar. 30, 2020 in Application No. 10-2014-0011764. |
KIPO; Office Action dated Mar. 11, 2020 in Application No. 10-2014-0103853. |
KIPO; Office Action dated Feb. 12, 2020 in Application No. 10-2020-7000992. |
TIPO; Notice of Allowance dated Feb. 20, 2020 in Application No. 102125191. |
TIPO; Office Action dated Jan. 17, 2020 in Application No. 104108277. |
TIPO; Notice of Allowance dated Jan. 15, 2020 in Application No. 105114105. |
TIPO; Notice of Allowance dated Mar. 13, 2020 in Application No. 105119533. |
TIPO; Office Action dated Jan. 17, 2020 in Application No. 105122586. |
TIPO; Office Action dated Jan. 17, 2020 in Application No. 107127688. |
TIPO; Office Action dated Feb. 3, 2020 in Application No. 108114221. |
TIPO; Notice of Allowance dated Mar. 12, 2020 in Application No. 108129100. |
USPTO; Final Office Action dated Feb. 20, 2020 in U.S. Appl. No. 14/444,744. |
USPTO; Non-Final Office Action dated Mar. 5, 2020 in U.S. Appl. No. 14/508,489. |
USPTO; Final Office Action dated Mar. 3, 2020 in U.S. Appl. No. 14/829,565. |
USPTO; Notice of Allowance dated Mar. 5, 2020 in U.S. Appl. No. 15/060,412. |
USPTO; Advisory Action dated Mar. 31, 2020 in U.S. Appl. No. 15/286,503. |
USPTO; Final Office Action dated Feb. 19, 2020 in U.S. Appl. No. 15/402,993. |
USPTO; Advisory Action dated Apr. 2, 2020 in U.S. Appl. No. 15/402,993. |
USPTO; Notice of Allowance dated Feb. 28, 2020 in U.S. Appl. No. 15/589,849. |
USPTO; Non-Final Office Action dated Mar. 10, 2020 in U.S. Appl. No. 15/611,707. |
USPTO; Notice of Allowance dated Feb. 28, 2020 in U.S. Appl. No. 15/615,489. |
USPTO; Non-Final Office Action dated Mar. 11, 2020 in U.S. Appl. No. 15/636,307. |
USPTO; Final Office Action dated Mar. 27, 2020 in U.S. Appl. No. 15/672,096. |
USPTO; Advisory Action dated Mar. 16, 2020 in U.S. Appl. No. 15/726,959. |
USPTO; Non-Final Office Action dated Apr. 3, 2020 in U.S. Appl. No. 15/726,959. |
USPTO; Notice of Allowance dated Mar. 12, 2020 in U.S. Appl. No. 15/795,056. |
USPTO; Final Office Action dated Mar. 19, 2020 in U.S. Appl. No. 15/798,201. |
USPTO; Final Office Action dated Mar. 11, 2020 in U.S. Appl. No. 15/802,154. |
USPTO; Advisory Action dated Mar. 25, 2020 in U.S. Appl. No. 15/815,483. |
USPTO; Non-Final Office Action dated Mar. 17, 2020 in U.S. Appl. No. 15/835,328. |
USPTO; Non-Final Office Action dated Feb. 20, 2020 in U.S. Appl. No. 15/835,352. |
USPTO; Non-Final Office Action dated Mar. 30, 2020 in U.S. Appl. No. 15/860,564. |
USPTO; Non-Final Office Action dated Mar. 20, 2020 in U.S. Appl. No. 15/861,418. |
USPTO; Final Office Action dated Feb. 26, 2020 in U.S. Appl. No. 15/890,037. |
USPTO; Non-Final Office Action dated Mar. 24, 2020 in U.S. Appl. No. 15/896,986. |
USPTO; Notice of Allowance dated Mar. 27, 2020 in U.S. Appl. No. 15/897,578. |
USPTO; Final Office Action dated Mar. 12, 2020 in U.S. Appl. No. 15/923,834. |
USPTO; Final Office Action dated Feb. 19, 2020 in U.S. Appl. No. 15/940,759. |
USPTO; Notice of Allowance dated Mar. 12, 2020 in U.S. Appl. No. 15/949,990. |
USPTO; Non-Final Office Action dated Apr. 2, 2020 in U.S. Appl. No. 15/974,948. |
USPTO; Notice of Allowance dated Apr. 3, 2020 in U.S. Appl. No. 15/985,261. |
USPTO; Non-Final Office Action dated Apr. 1, 2020 in U.S. Appl. No. 15/997,445. |
USPTO; Non-Final Office Action dated Mar. 3, 2020 in U.S. Appl. No. 16/000,109. |
USPTO; Advisory Action dated Apr. 3, 2020 in U.S. Appl. No. 16/000,125. |
USPTO; Non-Final Office Action dated Mar. 4, 2020 in U.S. Appl. No. 16/036,692. |
USPTO; Advisory Action dated Feb. 28, 2020 in U.S. Appl. No. 16/038,024. |
USPTO; Notice of Allowance dated Mar. 23, 2020 in U.S. Appl. No. 16/038,024. |
USPTO; Notice of Allowance dated Apr. 3, 2020 in U.S. Appl. No. 16/039,867. |
USPTO; Non-Final Office Action dated Feb. 20, 2020 in U.S. Appl. No. 16/105,745. |
USPTO; Non-Final Office Action dated Feb. 24, 2020 in U.S. Appl. No. 16/105,761. |
USPTO; Non-Final Office Action dated Mar. 19, 2020 in U.S. Appl. No. 16/105,802. |
USPTO; Non-Final Office Action dated Mar. 16, 2020 in U.S. Appl. No. 16/116,708. |
USPTO; Non-Final Office Action dated Feb. 28, 2020 in U.S. Appl. No. 16/137,974. |
USPTO; Final Office Action dated Mar. 2, 2020 in U.S. Appl. No. 16/158,077. |
USPTO; Final Office Action dated Mar. 17, 2020 in U.S. Appl. No. 16/161,744. |
USPTO; Notice of Allowance dated Mar. 5, 2020 in U.S. Appl. No. 16/167,225. |
USPTO; Non-Final Office Action dated Feb. 19, 2020 in U.S. Appl. No. 16/242,829. |
USPTO; Advisory Action dated Apr. 3, 2020 in U.S. Appl. No. 16/251,534. |
USPTO; Notice of Allowance dated Apr. 15, 2020 in U.S. Appl. No. 16/317,774. |
USPTO; Non-Final Office Action dated Mar. 2, 2020 in U.S. Appl. No. 16/356,394. |
USPTO; Notice of Allowance dated Mar. 30, 2020 in U.S. Appl. No. 16/417,938. |
USPTO; Final Office Action dated Jan. 10, 2020 in U.S. Appl. No. 16/674,894. |
WIPO; International Search Report and Written Opinion dated Apr. 17, 2019 in Application No. PCT/NL2018/050787. |
Rossing et al. “Acoustics of Eastern and Western bells, Old and New” J of Acoustical Society of Japan; 10(5); pp. 241-252 (1989). |
CNIPA; Notice of Allowance dated May 22, 2020 in Application No. 201610028064.1. |
CNIPA; Office Action dated Mar. 26, 2020 in Application No. 201610131743.1. |
CNIPA; Office Action dated May 18, 2020 in Application No. 201610982040.X. |
CNIPA; Office Action dated May 29, 2020 in Application No. 201710131319.1. |
CNIPA; Office Action dated Jun. 1, 2020 in Application No. 201710173292.2. |
CNIPA; Notice of Allowance dated May 14, 2020 in Application No. 201930615780.4. |
CNIPA; Notice of Allowance dated Apr. 27, 2020 in Application No. 201930660355.7. |
CNIPA; Notice of Allowance dated Jun. 2, 2020 in Application No. 202030048819.1. |
CNIPA; Notice of Allowance dated May 15, 2020 in Application No. 202030048854.3. |
CNIPA; Notice of Allowance dated May 15, 2020 in Application No. 202030053560.X. |
CNIPA; Notice of Allowance dated May 20, 2020 in Application No. 202030053634.X. |
KIPO; Notice of Allowance dated Apr. 23, 2020 in Application No. 10-2013-0050740. |
KIPO; Office Action dated Jun. 19, 2020 in Application No. 10-2013-0098575. |
KIPO; Notice of Allowance dated May 14, 2020 in Application No. 10-2013-0102026. |
KIPO; Office Action dated May 21, 2020 in Application No. 10-2014-0086902. |
KIPO; Office Action dated May 21, 2020 in Application No. 10-2014-0091092. |
KIPO; Offie Action dated Apr. 22, 2020 in Application No. 10-2020-0009462. |
TIPO; Notice of Allowance dated May 4, 2020 in Application No. 105101536. |
TIPO; Office Action dated Apr. 14, 2020 in Application No. 105129977. |
TIPO; Office Action dated Mar. 17, 2020 in Application No. 105130130. |
TIPO; Office Action dated Feb. 21, 2020 in Application No. 108120947. |
USPTO; Advisory Action dated Apr. 24, 2020 in U.S. Appl. No. 14/219,839. |
USPTO; Advisory Action dated Apr. 24, 2020 in U.S. Appl. No. 14/219,879. |
USPTO; Non-Final Office Action dated Apr. 28, 2020 in U.S. Appl. No. 14/444,744. |
USPTO; Final Office Action dated May 15, 2020 in U.S. Appl. No. 14/457,058. |
USPTO; Advisory Action dated Jun. 22, 2020 in U.S. Appl. No. 14/829,565. |
USPTO; Final Office Action dated Jun. 1, 2020 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Apr. 16, 2020 in U.S. Appl. No. 15/286,503. |
USPTO; Final Office Action dated May 13, 2020 in U.S. Appl. No. 15/377,439. |
USPTO; Non-Final Office Action dated May 27, 2020 in U.S. Appl. No. 15/402,993. |
USPTO; Final Office Action dated Apr. 17, 2020 in U.S. Appl. No. 15/491,726. |
USPTO; Final Office Action dated Jun. 16, 2020 in U.S. Appl. No. 15/636,307. |
USPTO; Notice of Allowance dated May 20, 2020 in U.S. Appl. No. 15/672,096. |
USPTO; Final Office Action dated May 27, 2020 in U.S. Appl. No. 15/690,017. |
USPTO; Advisory Action dated Jun. 19, 2020 in U.S. Appl. No. 15/691,241. |
USPTO; Advisory Action dated May 26, 2020 in U.S. Appl. No. 15/798,201. |
USPTO; Advisory Action dated May 19, 2020 in U.S. Appl. No. 15/802,154. |
USPTO; Non-Final Office Action dated Apr. 24, 2020 in U.S. Appl. No. 15/815,483. |
USPTO; Final Office Action dated Jun. 11, 2020 in U.S. Appl. No. 15/861,418. |
USPTO; Advisory Action dated Jun. 5, 2020 in U.S. Appl. No. 15/890,037. |
USPTO; Final Office Action dated Jun. 15, 2020 in U.S. Appl. No. 15/896,986. |
USPTO; Non-Final Office Action dated May 1, 2020 in U.S. Appl. No. 15/917,224. |
USPTO; Advisory Action dated May 15, 2020 in U.S. Appl. No. 15/923,834. |
USPTO; Non-Final Office Action dated May 1, 2020 in U.S. Appl. No. 15/925,532. |
USPTO; Advisory Action dated Apr. 23, 2020 in U.S. Appl. No. 15/940,759. |
USPTO; Final Office Action dated Apr. 30, 2020 in U.S. Appl. No. 15/962,980. |
USPTO; Non-Final Office Action dated May 15, 2020 in U.S. Appl. No. 15/974,988. |
USPTO; Non-Final Office Action dated Jun. 12, 2020 in U.S. Appl. No. 15/985,539. |
USPTO; Non-Final Office Action dated Feb. 20, 2020 in U.S. Appl. No. 15/996,286. |
USPTO; Non-Final Office Action dated Jun. 5, 2020 in U.S. Appl. No. 16/000,125. |
USPTO; Non-Final Office Action dated Apr. 22, 2020 in U.S. Appl. No. 16/000,156. |
USPTO; Non-Final Office Action dated May 7, 2020 in U.S. Appl. No. 16/004,041. |
USPTO; Notice of Allowance dated Jun. 24, 2020 in U.S. Appl. No. 16/014,981. |
USPTO; Notice of Allowance dated May 26, 2020 in U.S. Appl. No. 16/036,692. |
USPTO; Non-Final Office Action dated Apr. 30, 2020 in U.S. Appl. No. 16/055,532. |
USPTO; Non-Final Office Action dated May 27, 2020 in U.S. Appl. No. 16/100,012. |
USPTO; Final Office Action dated Jun. 23, 2020 in U.S. Appl. No. 16/105,745. |
USPTO; Final Office Action dated Apr. 21, 2020 in U.S. Appl. No. 16/105,761. |
USPTO; Final Office Action dated Jun. 26, 2020 in U.S. Appl. No. 16/105,802. |
USPTO; Non-Final Office Action dated Jun. 22, 2020 in U.S. Appl. No. 16/128,282. |
USPTO; Non-Final Office Action dated Apr. 21, 2020 in U.S. Appl. No. 16/130,798. |
USPTO; Final Office Action dated Jun. 5, 2020 in U.S. Appl. No. 16/132,142. |
USPTO; Advisory Action dated Jun. 9, 2020 in U.S. Appl. No. 16/158,077. |
USPTO; Notice of Allowance dated Jun. 19, 2020 in U.S. Appl. No. 16/161,744. |
USPTO; Non-Final Office Action dated May 29, 2020 in U.S. Appl. No. 16/205,899. |
USPTO; Final Office Action dated Jun. 19, 2020 in U.S. Appl. No. 16/219,555. |
USPTO; Final Office Action dated Jun. 15, 2020 in U.S. Appl. No. 16/242,829. |
USPTO; Notice of Allowance dated May 29, 2020 in U.S. Appl. No. 16/245,006. |
USPTO; Non-Final Office Action dated Apr. 24, 2020 in U.S. Appl. No. 16/251,534. |
USPTO; Non-Final Office Action dated May 27, 2020 in U.S. Appl. No. 16/252,567. |
USPTO; Non-Final Office Action dated Apr. 16, 2020 in U.S. Appl. No. 16/255,639. |
USPTO; Non-Final Office Action dated Jun. 30, 2020 in U.S. Appl. No. 16/258,187. |
USPTO; Notice of Allowance dated May 21, 2020 in U.S. Appl. No. 16/280,964. |
USPTO; Notice of Allowance dated Apr. 16, 2020 in U.S. Appl. No. 16/427,288. |
USPTO; Non-Final Office Action dated May 12, 2020 in U.S. Appl. No. 16/454,063. |
USPTO; Notice of Allowance dated Apr. 17, 2020 in U.S. Appl. No. 16/455,406. |
USPTO; Non-Final Office Action dated Jun. 11, 2020 in U.S. Appl. No. 16/598,768. |
USPTO; Notice of Allowance dated Apr. 21, 2020 in U.S. Appl. No. 16/674,894. |
USPTO; Non-Final Office Action dated Apr. 13, 2020 in U.S. Appl. No. 16/833,279. |
USPTO; Notice of Allowance dated Jun. 10, 2020 in U.S. Appl. No. 29/615,000. |
USPTO; Non-Final Office Action dated Apr. 24, 2020 in U.S. Appl. No. 29/726,623. |
WIPO; International Search Report and Written Opinion dated Apr. 29, 2019 in Application No. PCT/NL2018/050791. |
Chatterjee et al. “Chemical Vapor Deposition of Boron Nitride Nanosheets on Metallic Substrates via Decaborane/Ammonia Reactions”, Chem. Mater. 23, pp. 4414-4416 (2011). |
Fallica et al., “Dynamic Absorption Coefficients of Chemically Amplified Resists and Nonchemically Amplified Resists At Extreme Ultraviolet”, J. Micro/Nanolith. MEMS MOEMS 15(3), pp. 033506-1-033506-7 (2016). |
Glass et al. “The Chemical Vapor Deposition of Metal Boride Thin Films from Polyhedral Cluster Species”, Winter and Hoffman, Inorganic Materials Synthesis. ACS Symposium Series; American Cemical Society: Washington DC, Chapter 10, pp. 130-143 (1999). |
Jensen et al. “Titanium, Zirconium, and Hafnium Tetrahydroborates as “Tailored” CVD Precursors for Metal Diboride Thin Films”, J. Am. Chem. Soc. 110, pp. 1643-1644 (1988). |
Kliem et al. “Silyl Group Migrations Between Oxygen and Nitrogen in Aminosiloxanes”; Organosilicon Chemistry VI: from Molecules to Materials; pp. 216-221 (2005). |
Lewis et al. “Hawley's Condensed Chemical Dictionary” 12th Edition; excerpt pp. 1027-1038 (2005). |
Roddy, “Transport Reactions and Vaporization Studies of Some Vanadium Halides”, Iowa State university of Science and Technology dissertation, 207 pages (1962). |
Spear et al., “Chemical Transport Reactions in the Vanadium-Silicon-Oxygen System and the Ternary Phase Diagram”, Journal of the Less-Common Metals, 14, pp. 69-75 (1968). |
Su et al. “A Polymer Precursor Route to Metal Borides”, Chem. Mater., 5, pp. 1659-1668 (1993). |
CNIPA; Office Action dated Oct. 16, 2020 in Application No. 201610131743.1. |
CNIPA; Office Action dated Jun. 16, 2020 in Application No. 201610897958.4. |
CNIPA; Office Action dated Jul. 3, 2020 in Application No. 201610898822.5. |
CNIPA; Notice of Allowance dated Oct. 9, 2020 in Application No. 201610898822.5. |
CNIPA; Notice of Allowance dated Nov. 4, 2020 in Application No. 201710173292.2. |
CNIPA; Office Action dated Aug. 31, 2020 in Application No. 201780044761.9. |
CNIPA; Office Action dated Apr. 27, 2020 in Application No. 201810379112.0. |
CNIPA; Office Action dated Apr. 27, 2020 in Application No. 201810836604.8. |
CNIPA; Office Action dated Jul. 30, 2020 in Application No. 201810836604.8. |
CNIPA; Office Action dated Apr. 22, 2020 in Application No. 201810994464.7. |
CNIPA; Notice of Allowance dated Aug. 7, 2020 in Application No. 202030053609.1. |
EPO; Office Action dated Jul. 29, 2008 in Application No. 00902194.0. |
EPO; Office Action dated Jun. 27, 2003 in Application No. 97929595.3. |
EPO; Office Action dated Feb. 18, 2004 in Application No. 97929595.3. |
EPO; Notice of Allowance dated Apr. 29, 2004 in Application No. 97929595.3. |
EPO; Notice of Allowance dated Jan. 10, 2001 in Application No. 98911263.6. |
EPO; Office Action dated Jun. 6, 2001 in Application No. 98911277.6. |
EPO; Office Action dated Jun. 27, 2003 in Application No. 98967122.7. |
EPO; Notice of Allowance dated Feb. 23, 2004 in Application No. 98967122.7. |
EPO; Office Action dated Sep. 22, 2003 in Application No. 99946447.2. |
EPO; Office Action dated Nov. 25, 2003 in Application No. 99946447.2. |
EPO; Office Action dated Mar. 30, 2004 in Application No. 99946447.2. |
EPO; Office Action dated Jul. 19, 2004 in Application No. 99946447.2. |
EPO; Notice of Allowance dated Sep. 22, 2004 in Application No. 99946447.2. |
EPO; Supplementary European Search Report dated May 27, 2002 in Application No. 99973123. |
EPO; Notice of Allowance dated Jun. 11, 2004 in Application No. 99973123. |
JPO; Office Action dated Jun. 1, 2020 in Application No. 2016-206625. |
JPO; Office Action dated Aug. 28, 2020 in Application No. 2017-139817. |
JPO; Notice of Allowance dated Jul. 1, 2020 in Application No. 2019-025168. |
JPO; Office Action dated Aug. 24, 2020 in Application No. 2019-119908. |
JPO; Office Action dated Jun. 29, 2020 in Application No. 2020-502653. |
KIPO; Decision of Intellectual Property Trial and Appeal Board dated Jun. 23, 2020 in Application No. 10-2012-0076564. |
KIPO; Notice of Allowance dated Sep. 25, 2020 in Application No. 10-2013-0049598. |
KIPO; Notice of Allowance dated Aug. 13, 2020 in Application No. 10-2013-0098575. |
KIPO; Notice of Allowance dated Oct. 27, 2020 in Application No. 10-2014-0011764. |
KIPO; Office Action dated Jul. 21, 2020 in Application No. 10-2014-0011765. |
KIPO; Notice of Allowance dated Sep. 8, 2020 in Application No. 10-2014-0021615. |
KIPO; Office Action dated Oct. 26, 2020 in Application No. 10-2014-0027217. |
KIPO; Notice of Allowance dated Oct. 12, 2020 in Application No. 10-2014-0027305. |
KIPO; Office Action dated Jul. 9, 2020 in Application No. 10-2014-0060120. |
KIPO; Office Action dated Aug. 18, 2020 in Application No. 10-2014-0071653. |
KIPO; Notice of Allowance dated Oct. 19, 2020 in Application No. 10-2014-0086902. |
KIPO; Notice of Allowance dated Sep. 27, 2020 in Application No. 10-2014-0091092. |
KIPO; Office Action dated Oct. 5, 2020 in Application No. 10-2014-0103853. |
KIPO; Office Action dated Oct. 7, 2020 in Application No. 10-2014-0128626. |
KIPO; Office Action dated Jul. 21, 2020 in Application No. 10-2017-0087308. |
KIPO; Notice of Allowance dated Oct. 26, 2020 in Application No. 10-2017-0087308. |
KIPO; Office Action dated Jun. 30, 2020 in Application No. 10-2019-0044213. |
KIPO; Notice of Allowance dated Oct. 28, 2020 in Application No. 10-2020-0009462. |
KIPO; Notice of Allowance dated Jul. 20, 2020 in Application No. 10-2020-7000992. |
KIPO; Notice of Allowance dated Oct. 20, 2020 in Application No. 30-2019-0054013 M001. |
KIPO; Notice of Allowance dated Oct. 20, 2020 in Application No. 30-2019-0054013 M002. |
KIPO; Notice of Allowance dated Oct. 22, 2020 in Application No. 30-2019-0058076. |
TIPO; Notice of Allowance dated Jul. 1, 2020 in Application No. 105101537. |
TIPO; Notice of Allowance dated Sep. 4, 2020 in Application No. 105111990. |
TIPO; Office Action dated Sep. 7, 2020 in Application No. 105122394. |
TIPO; Notice of Allowance dated Aug. 31, 2020 in Application No. 105122586. |
TIPO; Office Action dated Sep. 18, 2020 in Application No. 105129977. |
TIPO; Notice of Allowance dated Sep. 25, 2020 in Application No. 105130130. |
TIPO; Office Action in Application No. 105131284. |
TIPO; Office Action dated Aug. 25, 2020 in Application No. 105131896. |
TIPO; Office Action dated Sep. 30, 2020 in Application No. 105142668. |
TIPO; Office Action dated Aug. 11, 2020 in Application No. 106100823. |
TIPO; Office Action dated Jun. 17, 2020 in Application No. 106108152. |
TIPO; Office Action dated Oct. 7, 2020 in Application No. 106108522. |
TIPO; Office Action dated Aug. 21, 2020 in Application No. 106111548. |
TIPO; Office Action dated Oct. 8, 2020 in Application No. 106111693. |
TIPO; Office Action dated Jul. 15, 2020 in Application No. 106120365. |
TIPO; Office Action dated Nov. 12, 2020 in Application No. 106120365. |
TIPO; Office Action dated Nov. 18, 2020 in Application No. 106120902. |
TIPO; Office Action dated Oct. 8, 2020 in Application No. 106123203. |
TIPO; Office Action dated Jun. 24, 2020 in Application No. 108135004. |
TIPO; Office Action dated Jun. 29, 2020 in Application No. 108137226. |
TIPO; Office Action dated Jul. 9, 2020 in Application No. 108137227. |
TIPO; Office Action dated Aug. 17, 2020 in Application No. 108139018. |
TIPO; Notice of Allowance dated Oct. 19, 2020 in Application No. 108306935. |
TIPO; Notice of Allowance dated Oct. 19, 2020 in Application No. 108306935D01. |
TIPO; Notice of Allowance dated Jul. 15, 2020 in Application No. 108307027. |
TIPO; Notice of Allowance dated Oct. 19, 2020 in Application No. 108307027D01. |
TIPO; Notice of Allowance dated Sep. 15, 2020 in Application No. 108307301. |
TIPO; Notice of Allowance dated Sep. 25, 2020 in Application No. 108307759. |
USPTO; Non-Final Office Action dated Mar. 28, 2001 in U.S. Appl. No. 09/452,844. |
USPTO; Final Office Action dated Sep. 11, 2001 in U.S. Appl. No. 09/452,844. |
USPTO; Advisory Action dated Jan. 24, 2002 in U.S. Appl. No. 09/452,844. |
USPTO; Non-Final Office Action dated Apr. 9, 2002 in U.S. Appl. No. 09/452,844. |
USPTO; Final Office Action dated Sep. 27, 2002 in U.S. Appl. No. 09/452,844. |
USPTO; Notice of Allowance dated Jun. 17, 2003 in U.S. Appl. No. 09/452,844. |
USPTO; Non-Final Office Action dated Oct. 31, 2003 in U.S. Appl. No. 09/452,844. |
USPTO; Notice of Allowance dated Mar. 26, 2004 in U.S. Appl. No. 09/452,844. |
USPTO; Non-Final Office Action dated Dec. 10, 2002 in U.S. Appl. No. 09/771,673. |
USPTO; Final Office Action dated May 29, 2003 in U.S. Appl. No. 09/771,673. |
USPTO; Final Office Action dated Feb. 6, 2004 in U.S. Appl. No. 09/771,673. |
USPTO; Advisory Action dated Apr. 20, 2004 in U.S. Appl. No. 09/771,673. |
USPTO; Notice of Allowance dated Jul. 29, 2004 in U.S. Appl. No. 09/771,673. |
USPTO; Non-Final Office Action dated Jan. 3, 2002 in U.S. Appl. No. 09/807,580. |
USPTO; Final Office Action dated Jun. 21, 2002 in U.S. Appl. No. 09/807,580. |
USPTO; Advisory Action dated Aug. 27, 2002 in U.S. Appl. No. 09/807,580. |
USPTO; Non-Final Action dated Nov. 27, 2002 in U.S. Appl. No. 09/807,580. |
USPTO; Final Office Action dated May 27, 2003 in U.S. Appl. No. 09/807,580. |
USPTO; Advisory Action dated Oct. 22, 2003 in U.S. Appl. No. 09/807,580. |
USPTO; Examiner's Answer to Appeal Brief dated May 6, 2004 in U.S. Appl. No. 09/807,580. |
USPTO; Decision on Appeal dated Feb. 16, 2005 in U.S. Appl. No. 09/807,580. |
USPTO; Non-Final Action dated May 19, 2005 in U.S. Appl. No. 09/807,580. |
USPTO; Final Action dated Nov. 21, 2005 in U.S. Appl. No. 09/807,580. |
USPTO; Notice of Allowance dated Feb. 23, 2006 in U.S. Appl. No. 09/807,580. |
USPTO; Non-Final Office Action dated May 13, 2003 in U.S. Appl. No. 10/222,229. |
USPTO; Non-Final Office Action dated Feb. 9, 2004 in U.S. Appl. No. 10/603,515. |
USPTO; Notice of Allowance dated Jun. 18, 2004 in U.S. Appl. No. 10/603,515. |
USPTO; Non-Final Office Action dated Oct. 17, 2006 in U.S. Appl. No. 10/932,633. |
USPTO; Non-Final Office Action dated Apr. 19, 2007 in U.S. Appl. No. 10/932,633. |
USPTO; Notice of Allowance dated Sep. 10, 2007 in U.S. Appl. No. 10/932,633. |
USPTO; Notice of Allowance dated Jul. 6, 2020 in U.S. Appl. No. 13/184,351. |
USPTO; Examiner's Answer to Appeal Brief dated Apr. 20, 2018 in U.S. Appl. No. 13/187,300. |
USPTO; Patent Board Decision dated Sep. 23, 2019 in U.S. Appl. No. 13/187,300. |
USPTO; Advisory Action dated Nov. 10, 2015 in U.S. Appl. No. 14/079,302. |
USPTO; Notice of Allowance dated Sep. 3, 2020 in U.S. Appl. No. 14/444,744. |
USPTO; Notice of Allowance dated Aug. 6, 2020 in U.S. Appl. No. 14/457,058. |
USPTO; Final Office Action dated Aug. 20, 2020 in U.S. Appl. No. 14/508,489. |
USPTO; Notice of Allowance dated Nov. 3, 2020 in U.S. Appl. No. 14/508,489. |
USPTO; Non-Final Office Action dated Aug. 3, 2020 in U.S. Appl. No. 14/829,565. |
USPTO; Notice of Allowance dated Aug. 18, 2020 in U.S. Appl. No. 15/135,258. |
USPTO; Non-Final Office Action dated Oct. 6, 2020 in U.S. Appl. No. 15/262,990. |
USPTO; Final Office Action dated Oct. 2, 2020 in U.S. Appl. No. 15/286,503. |
USPTO; Non-Final Office Action dated Sep. 2, 2020 in U.S. Appl. No. 15/377,439. |
USPTO; Non-Final Office Action dated Jul. 1, 2020 in U.S. Appl. No. 15/380,909. |
USPTO; Final Office Action dated Jul. 23, 2020 in U.S. Appl. No. 15/380,921. |
USPTO; Final Office Action dated Sep. 8, 2020 in U.S. Appl. No. 15/402,993. |
USPTO; Advisory Action dated Nov. 9, 2020 in U.S. Appl. No. 15/402,993. |
USPTO; Non-Final Office Action dated Sep. 30, 2020 in U.S. Appl. No. 15/491,726. |
USPTO; Final Office Action dated Jul. 8, 2020 in U.S. Appl. No. 15/589,861. |
USPTO; Notice of Allowance dated Oct. 16, 2020 in U.S. Appl. No. 15/589,861. |
USPTO; Final Office Action dated Sep. 16, 2020 in U.S. Appl. No. 15/611,707. |
USPTO; Advisory Action dated Nov. 20, 2020 in U.S. Appl. No. 15/611,707. |
USPTO; Non-Final Office Action dated Sep. 3, 2020 in U.S. Appl. No. 15/636,307. |
USPTO; Notice of Allowance dated Jul. 2, 2020 in U.S. Appl. No. 15/672,096. |
USPTO; Advisory Action dated Aug. 6, 2020 in U.S. Appl. No. 15/690,017. |
USPTO; Non-Final Office Action dated Aug. 24, 2020 in U.S. Appl. No. 15/690,017. |
USPTO; Non-Final Office Action dated Oct. 6, 2020 in U.S. Appl. No. 15/691,241. |
USPTO; Final Office Action dated Sep. 24, 2020 in U.S. Appl. No. 15/726,959. |
USPTO; Non-Final Office Action dated Jul. 10, 2020 in U.S. Appl. No. 15/798,201. |
USPTO; Notice of Allowance dated Oct. 21, 2020 in U.S. Appl. No. 15/798,201. |
USPTO; Non-Final Office Action dated Jul. 2, 2020 in U.S. Appl. No. 15/802,154. |
USPTO; Notice of Allowance dated Oct. 26, 2020 in U.S. Appl. No. 15/802,154. |
USPTO; Notice of Allowance dated Sep. 30, 2020 in U.S. Appl. No. 15/815,483. |
USPTO; Final Office Action dated Sep. 17, 2020 in U.S. Appl. No. 15/835,328. |
USPTO; Final Office Action dated Aug. 6, 2020 in U.S. Appl. No. 15/835,352. |
USPTO; Notice of Allowance dated Aug. 17, 2020 in U.S. Appl. No. 15/843,899. |
USPTO; Notice of Allowance dated Jun. 30, 2020 in U.S. Appl. No. 15/860,564. |
USPTO; Notice of Allowance dated Aug. 19, 2020 in U.S. Appl. No. 15/861,418. |
USPTO; Non-Final Office Action dated Sep. 2, 2020 in U.S. Appl. No. 15/890,037. |
USPTO; Notice of Allowance dated Aug. 26, 2020 in U.S. Appl. No. 15/896,986. |
USPTO; Non-Final Office Action dated Sep. 9, 2020 in U.S. Appl. No. 15/909,705. |
USPTO; Final Office Action dated Sep. 24, 2020 in U.S. Appl. No. 15/917,224. |
USPTO; Non-Final Office Action dated Jul. 6, 2020 in U.S. Appl. No. 15/923,834. |
USPTO; Final Office Action dated Oct. 19, 2020 in U.S. Appl. No. 15/923,834. |
USPTO; Final Office Action dated Oct. 15, 2020 in U.S. Appl. No. 15/925,532. |
USPTO; Non-Final Office Action dated Oct. 6, 2020 in U.S. Appl. No. 15/940,729. |
USPTO; Non-Final Office Action dated Aug. 3, 2020 in U.S. Appl. No. 15/940,759. |
USPTO; Advisory Action dated Jul. 2, 2020 in U.S. Appl. No. 15/962,980. |
USPTO; Non-Final Office Action dated Sep. 14, 2020 in U.S. Appl. No. 15/962,980. |
USPTO; Non-Final Office Action dated Oct. 6, 2020 in U.S. Appl. No. 15/967,146. |
USPTO; Final Office Action dated Sep. 3, 2020 in U.S. Appl. No. 15/974,948. |
USPTO; Notice of Allowance dated Oct. 14, 2020 in U.S. Appl. No. 15/974,988. |
USPTO; Final Office Action dated Nov. 25, 2020 in U.S. Appl. No. 15/985,539. |
USPTO; Final Office Action dated Jul. 24, 2020 in U.S. Appl. No. 15/996,286. |
USPTO; Advisory Action dated Oct. 7, 2020 in U.S. Appl. No. 15/996,286. |
USPTO; Final Office Action dated Oct. 2, 2020 in U.S. Appl. No. 15/997,445. |
USPTO; Notice of Allowance dated Jul. 10, 2020 in U.S. Appl. No. 15/998,775. |
USPTO; Final Office Action dated Sep. 14, 2020 in U.S. Appl. No. 16/000,109. |
USPTO; Final Office Action dated Oct. 6, 2020 in U.S. Appl. No. 16/000,125. |
USPTO; Final Office Action dated Oct. 22, 2020 in U.S. Appl. No. 16/000,156. |
USPTO; Final Office Action dated Oct. 15, 2020 in U.S. Appl. No. 16/004,041. |
USPTO; Non-Final Office Action dated Sep. 8, 2020 in U.S. Appl. No. 16/039,817. |
USPTO; Non-Final Office Action dated Aug. 4, 2020 in U.S. Appl. No. 16/042,791. |
USPTO; Final Office Action dated Jul. 30, 2020 in U.S. Appl. No. 16/055,532. |
USPTO; Final Office Action dated Nov. 3, 2020 in U.S. Appl. No. 16/055,532. |
USPTO; Notice of Allowance dated Sep. 14, 2020 in U.S. Appl. No. 16/100,012. |
USPTO; Advisory Action dated Aug. 25, 2020 in U.S. Appl. No. 16/105,745. |
USPTO; Non-Final Office Action dated Nov. 25, 2020 in U.S. Appl. No. 16/105,745. |
USPTO; Advisory Action dated Jul. 8, 2020 in U.S. Appl. No. 16/105,761. |
USPTO; Non-Final Office Action dated Nov. 25, 2020 in U.S. Appl. No. 16/105,761. |
USPTO; Final Office Action dated Nov. 17, 2020 in U.S. Appl. No. 16/105,802. |
USPTO; Non-Final Office Action dated Sep. 8, 2020 in U.S. Appl. No. 16/108,950. |
USPTO; Final Office Action dated Sep. 2, 2020 in U.S. Appl. No. 16/116,708. |
USPTO; Advisory Action dated Nov. 17, 2020 in U.S. Appl. No. 16/116,708. |
USPTO; Final Office Action dated Nov. 19, 2020 in U.S. Appl. No. 16/128,282. |
USPTO; Notice of Allowance dated Aug. 5, 2020 in U.S. Appl. No. 16/130,798. |
USPTO; Advisory Action dated Aug. 24, 2020 in U.S. Appl. No. 16/132,142. |
USPTO; Non-Final Office Action dated Oct. 16, 2020 in U.S. Appl. No. 16/132,142. |
USPTO; Final Office Action dated Aug. 20, 2020 in U.S. Appl. No. 16/137,974. |
USPTO; Notice of Allowance dated Nov. 3, 2020 in U.S. Appl. No. 16/137,974. |
USPTO; Non-Final Office Action dated Jul. 30, 2020 in U.S. Appl. No. 16/151,074. |
USPTO; Advisory Action dated Sep. 16, 2020 in U.S. Appl. No. 16/152,260. |
USPTO; Final Office Action dated Jul. 15, 2020 in U.S. Appl. No. 16/152,260. |
USPTO; Non-Final Office Action dated Nov. 9, 2020 in U.S. Appl. No. 16/152,260. |
USPTO; Notice of Allowance dated Jul. 24, 2020 in U.S. Appl. No. 16/158,077. |
USPTO; Non-Final Office Action dated Jul. 23, 2020 in U.S. Appl. No. 16/167,164. |
USPTO; Non-Final Office Action dated Aug. 7, 2020 in U.S. Appl. No. 16/172,535. |
USPTO; Final Office Action dated Oct. 16, 2020 in U.S. Appl. No. 16/172,535. |
USPTO; Non-Final Office Action dated Nov. 4, 2020 in U.S. Appl. No. 16/176,517. |
USPTO; Non-Final Office Action dated Oct. 29, 2020 in U.S. Appl. No. 16/183,258. |
USPTO; Notice of Allowance dated Jul. 28, 2020 in U.S. Appl. No. 16/193,789. |
USPTO; Notice of Allowance dated Jul. 7, 2020 in U.S. Appl. No. 16/194,041. |
USPTO; Final Office Action dated Nov. 27, 2020 in U.S. Appl. No. 16/205,899. |
USPTO; Non-Final Office Action dated Jul. 15, 2020 in U.S. Appl. No. 16/210,922. |
USPTO; Advisory Action dated Sep. 11, 2020 in U.S. Appl. No. 16/219,555. |
USPTO; Non-Final Office Action dated Sep. 30, 2020 in U.S. Appl. No. 16/219,555. |
USPTO; Advisory Action dated Aug. 11, 2020 in U.S. Appl. No. 16/242,829. |
USPTO; Notice of Allowance dated Sep. 23, 2020 in U.S. Appl. No. 16/242,829. |
USPTO; Non-Final Office Action dated Sep. 3, 2020 in U.S. Appl. No. 16/242,852. |
USPTO; Final Office Action dated Oct. 14, 2020 in U.S. Appl. No. 16/251,534. |
USPTO; Final Office Action dated Nov. 18, 2020 in U.S. Appl. No. 16/252,567. |
USPTO; Notice of Allowance dated Aug. 6, 2020 in U.S. Appl. No. 16/255,639. |
USPTO; Notice of Allowance dated Aug. 5, 2020 in U.S. Appl. No. 16/258,187. |
USPTO; Final Office Action dated Jun. 30, 2020 in U.S. Appl. No. 16/356,394. |
USPTO; Notice of Allowance dated Aug. 31, 2020 in U.S. Appl. No. 16/356,394. |
USPTO; Non-Final Office Action dated Aug. 5, 2020 in U.S. Appl. No. 16/397,045. |
USPTO; Non-Final Office Action dated Aug. 19, 2020 in U.S. Appl. No. 16/400,814. |
USPTO; Notice of Allowance dated Sep. 18, 2020 in U.S. Appl. No. 16/454,063. |
USPTO; Non-Final Office Action dated Nov. 27, 2020 in U.S. Appl. No. 16/468,258. |
USPTO; Non-Final Office Action dated Nov. 5, 2020 in U.S. Appl. No. 16/546,543. |
USPTO; Notice of Allowance dated Sep. 16, 2020 in U.S. Appl. No. 16/598,768. |
USPTO; Non-Final Office Action dated Oct. 16, 2020 in U.S. Appl. No. 16/679,885. |
USPTO; Non-Final Office Action dated Nov. 16, 2020 in U.S. Appl. No. 16/713,311. |
USPTO; Final Office Action dated Oct. 2, 2020 in U.S. Appl. No. 16/833,279. |
USPTO; Non-Final Office Action dated Jul. 9, 2020 in U.S. Appl. No. 16/897,158. |
USPTO; Notice of Allowance dated Nov. 12, 2020 in U.S. Appl. No. 16/897,158. |
USPTO; Non-Final Office Action dated Aug. 4, 2020 in U.S. Appl. No. 16/926,192. |
USPTO; Final Office Action dated Sep. 9, 2020 in U.S. Appl. No. 29/726,623. |
WIPO; International Search Report dated Oct. 13, 1998 in Application No. PCT/FI1998/000571. |
WIPO; International Search Report dated Jul. 13, 1990 in Application No. PCT/NL1990/000027. |
WIPO; International Search Report dated Jan. 11, 1990 in Application No. PCT/NL1990/000042. |
WIPO; International Search Report dated Feb. 26, 1991 in Application No. PCT/NL1990/000166. |
WIPO; International Search Report dated Oct. 25, 1991 in Application No. PCT/NL1991/000108. |
WIPO; International Search Report dated Oct. 17, 1997 in Application No. PCT/NL1997/000398. |
WIPO; International Preliminary Examination Report dated Oct. 2, 1998 in Application No PCT/NL1997/000398. |
WIPO; International Search Report dated Apr. 24, 1998 in Application No. PCT/NL1998/000055. |
WIPO; International Preliminary Examination Report dated Feb. 24, 1999 in Application No. PCT/NL1998/000055. |
WIPO; International Search Report dated May 27, 1998 in Application No. PCT/NL1998/000105. |
WIPO; International Search Report dated May 8, 1998 in Application No. PCT/NL1998/000151. |
WIPO; International Preliminary Examination Report dated Mar. 23, 1999 in Application No. PCT/NL1998/000151. |
WIPO; International Search Report dated May 27, 1998 in Application No. PCT/NL1998/000167. |
WIPO; International Preliminary Examination Report dated Jul. 13, 1999 in Application No. PCT/NL1998/000167. |
WIPO; International Search Report dated Jul. 8, 1998 in Application No. PCT/NL1998/000204. |
WIPO; International Search Report dated Aug. 21, 1998 in Application No. PCT/NL1998/000246. |
WIPO; International Search Report dated Oct. 16, 1998 in Application No. PCT/NL1998/000383. |
WIPO; International Preliminary Examination Report dated Sep. 16, 1999 in Application No. PCT/NL1998/000383. |
WIPO; International Search Report dated Apr. 15, 1999 in Application No. PCT/NL1999/000047. |
WIPO; International Search Report dated Oct. 12, 1999 in Application No. PCT/NL1999/000487. |
WIPO; International Search Report dated Dec. 16, 1999 in Application No. PCT/NL1999/000583. |
WIPO; Written Opinion dated Jul. 24, 2000 in Application No. PCT/NL1999/000583. |
WIPO; International Preliminary Examination Report dated Jan. 22, 2001 in Application No. PCT/NL1999/000583. |
WIPO; International Search Report dated Apr. 19, 2000 in Application No. PCT/NL2000/000020. |
WIPO; Written Opinion dated Oct. 17, 2000 in Application No. PCT/NL2000/000020. |
WIPO; International Search Report dated Dec. 16, 1999 in Application No. PCT/RU1999/000328. |
WIPO; International Preliminary Examination Report dated Jun. 29, 2001 in Application No. PCT/RU1999/000328. |
Akiyama et al. “Macro- and micro-scale simulation of growth rate and composition in MOCVD of yttria-stabilized zirconia” J. Crystal Growth 241, pp. 352-362 (2002). |
Altiere et al. “Review Article: Plasma-surface interactions at the atomic scale for patterning metals” J. Vac. Sci. Technol. A 35, 05C203, 13 pages (2017). |
Ande et al. “Role of Surface Termination in Atomic Layer Deposition of Silicon Nitride” J. Phys. Chem. Lett., 6(18), 16 pages (2015). |
Atta et al. “The Catalytic Activity of Ruthenates ARuO3 (A=Ca, Sr or Ba) for the Hydrogen Evolution Reaction in Acidic Medium” Int. J. Electrochem. Sci. 7, pp. 725-746 (2012). |
Ballal “Mass Transfer in Porous Solids under Pulsating Pressure Conditions” SLJ International, vol. 35, Nov. 4, pp. 446-448 (1995). |
Brewin et al. “UPS to deploy Bluetooth, wireless LAN network” Internet, pp. 1-5 (2001). |
Bulletin Plasma Source—12/02: Type AX7610—Downstream Plasma Source. Source location: MKS Instruments, Inc. http://www.mksinst.com/. Accessed: Aug. 6, 2015. pp. 1-4 (2002). |
Bulletin ASTRONe—4/02: Type AX7680—Reactive Gas Generator. Source location: MKS Instruments, Inc. http://www.mksinst.com/. Accessed: Aug. 6, 2015. pp. 1-2 (2002). |
Bulletin ASTRONex-7/09: Type AX7685—Reactive Gas Generator. Source location: MKS Instruments, Inc. http://www.mksinst.com/. Accessed: Aug. 6, 2015. pp. 1-2 (2002). |
Bulletin Astron hf-s—3/05: Type AX7645—Reactive Gas Generator. Source location: MKS Instruments, Inc. http://www.mksinst.com/. Accessed: Aug. 6, 2015. pp. 1-2 (2005). |
Bulletin ENG-XSTREAM-340-09 OM 8/06: Xstream with Active Matching Network Remote Plasma Source. Advanced Energy Industries, Inc. http://www.advanced-energy.net.cn/upload/File/Sources/ENG-Xstream-340-09. pdf. Accessed: Jul. 19, 2016. pp. 1-4 (2006). |
Bulletin R*evolution—9/06: Type AX7690—Remote Plasma Source. Source location: MKS Instruments, Inc. http://www.mksinst.com/. Accessed: Aug. 6, 2015. pp. 1-2 (2006). |
Callaghan et al. “Magnetic Interactions in Ternary Ruthenium Oxides” Inorganic Chemistry, vol. 5, No. 9, pp. 1572-1576 (1966). |
Choi et al. “UV irradiation effects on the bonding structure and electrical properties of ultra low-k SiOC(-H) thin films for 45 nm technology node” Current Applied Physics, 11, S109-S113 (2011). |
Closser et al., “Molecular Layer Deposition of a Highly Stable Silicon Oxycarbide Thin Film Using an Organic Chlorosilane and Water,” ACS Applied Materials & Interfaces 10, pp. 24266-24274 (2018). |
Crystal IS “Application Note: Using UV Reflective Materials to Maximize Disinfection”; AN011; Jun. 16, 2016, found at https://www.klaran.com/using-uv-reflective-materials-to-maximize-disinfection. |
Dufond et al. “Quantifying the Extent of Ligand Incorporation and the Effect on Properties of TiO 2 Thin Films Grown by Atomic Layer Deposition Using an Alkoxide or an Alkylamide” Chemistry of Material, American Chemical Society 32(4), pp. 1393-1407 (2020). |
Dultsev et al. “Effect of UV radiation on the reactivity of porous methyl-doped SiO2 layers” Phys. Status Solidi C, 8, No. 6, pp. 1946-1949 (2011). |
Esposito et al. “Preparation and characterization of lead ruthenate based composite cathodes for SOFC applications” Mater. Res. Soc. Symp. Proc., vol. 835, 6 pages (2005). |
Fray et al. “Aspects of the Application of Electrochemistry to the Extraction of Titanium and Its Applications” Materials Transactions, vol. 58, No. 3, pp. 306-312 (2017). |
Freund et al. “Single crystal growth from separated educts and its application to lithum transition-metal oxides” Sci. Rep. 6, 35362, pp. 1-5 (2016). |
Frequestly Asked Question, “What is a load lock chamber?”, Kurt J. Lesker Company, www.lesker.com, p. 1 (2020). |
Hong et al. “Ultralow-dielectric-constant amoprhous boron nitride” Nature, vol. 582, 16 pages (2020). |
Hubert et al., “A Stacked SONOS Technology, up to 4 Levels and 6nm Crystalline Nanowires, With Gate-All-Around or Independent Gates (-Flash), Suitable for Full 3D Integration,” Minatec, IEDM09-637-640 (2009). |
Ivanova et al. “ALD of Sc2O3 using Sc(Cp)3 and a Novel Heteroleptic Precursors” Presented on the AVS 19th International Conference on Atomic Layer Deposition, Jul. 23, 2019, Abstract, 1 page (2019). |
Johnson et al. “A brief review of atomic layer deposition: from fundamentals to applications” Materials Today, vol. 17, Issue 5, pp. 236-246 (2014). |
Juppo et al. “Deposition of molybdenum thin films by an alternate supply of MoCl 5 and Zn” J of Vacuumn Science & Technology A, 16, pp. 2845-2850 (1998). |
Katamreddy et al., “ALD and Characterization of Aluminum Oxide Deposited on Si(100) using Tris(diethylamino) Aluminum and Water Vapor,” Journal of The Electrochemical Society, 153 (10) C701-C706 (2006). |
Kim et al. “Thermal Decomposition of Tetrakis(ethylmethylamido) Titanium for Chemical Vapor Deposition of Titanium Nitride” Bull. Korean Chem. Soc., vol. 27, No. 2, 5 pages (2006). |
Kirsch et al. “Dipole model explaining high-k/metal gate field effect transistor threshold voltage tuning” Applied Physics Letters 92, 092901, 3 pages (2008). |
Kjesbu, ABB Corporate Research, Internet, pp. 1-37 (2002). |
Kofuji et al. “Line-edge roughness increase due to wiggling enhanced by initial pattern waviness” Jpn. J. Appl. Phys. 53, 03DE01, pp. 1-7 (2014). |
Kofuji et al. “Mechanism of wiggling enhancement due to HBr gas addition during amorphous carbon etching” Jpn. J. Appl. Phys. 54, 06FH04, pp. 107 (2015). |
Kovalgin et al. “Hot-Wire Assisted ALD: A Study Powered by In Situ Spectroscopic Ellipsometry” Adv. Mater. Interfaces 4, 1700058, 11 pages (2017). |
Krumdieck et al. “Experimental Characterization and Modeling of Pulsed MOCVD with Ultrasonic Atomization of Liquid Precusor” Chem. Vap. Deposition, 7 (2), pp. 85-90 (2001). |
Krumdieck “Kinetic Model of Low Pressure Film Deposition from Single Precursor Vapor in a Well-Mixed, Cold-Wall Reactor” Acta mater., 49, pp. 583-588 (2001). |
Kuchumov et al. “Pulsed MO CVD Processes of MgO Layer Deposition from Mg(thd)2” ECS Trans. 25, pp. 927-934 (2009). |
Kukli et al. “Atomic Layer Deposition and Chemical Vapor Deposition of Tantalum Oxide by Successive and Simultaneous Pulsing of Tantalum Ethoxide and Tantalum Chloride” Chem. Mater. 12, pp. 1914-1920 (2000). |
Kukli et al. “Atomic Layer Epitaxy Growth of Tantalum Oxide Thin Films from Ta(OC2H5)5 and H20” The Electrochemical Society, vol. 142, No. 5, pp. 1670-1674 (1995). |
Kumar et al. “Bringing the benefits of Java to Bluetooth” http://www.allembedded.com/story/OEG20020519S001, pp. 1-3 (2002). |
Mameli et al. “Area-Selective Atomic Layer Deposition of SiO2 Using Acetylacetone as a Chemoselective Inhibitor in an ABC-Type Cycle” ACS Nano 11, pp. 9303-9311 (2017). |
Mameli et al. “Isotropic Atomic Layer Etching of ZnO Using Acetylacetone and O2 Plama” ACS Appl. Mater. Interfaces 10, pp. 38588-38595 (2018). |
Naslain et al. “Synthesis of highly tailored ceramic matrix composites by pressure-pulsed CVI” Solid State Ionics, 141-142, pp. 541-548 (2001). |
Niinisto et al. “Advanced electronic and optoelectronic materials by Atomic Layer Deposition: An overview with special emphasis on recent progress in processing of high-k dielectrics and other oxide materials” Pus. Stat. Sol. (a) 201, No. 7, pp. 1443-1452 (2004). |
Ohzawa et al. “Preparation of fibrous SiC shape using pressure-pulsed chemical vapour infiltration and its properties as a high-temperature filter” J. of Materials Processing Technology, 96, pp. 151-156 (1999). |
O'Malley et al. “Structure and properties of ordered Li2IrO3 and Li2PtO3” Journal of Solid State Chemistry 181, pp. 1803-1809 (2008). |
Park et al. “Atomic layer deposition of Y2O3 films using hetroleptic liquid (iPrCp)2Y(iPr-amd) precursor” J. Mater. Chem. C, 2, 9 pages (2014). |
Peters et al., “Aerosol-Assisted Chemical Vapor Deposition of NbS2 and TaS2 Thin Films from Pentakis(dimethylamido)metal Complexes and 2-Methylpropanethiol” Eur. J. Inorg. Chem., pp. 4179-4185 (2005). |
Posseme et al. “Alternative process for thin layer etching: Application to nitride spacer etching stopping on silicon germanium” Apply. Phys. Lett. 105, 051604, pp. 1-4 (2014). |
Provine et al. “Atomic Layer Deposition: Introduction to the Theory and Cambridge Nanotech Savannah & Fiji” NNIN ALD Roadshow Presentation, 49 pages (2012). |
Rosemount 1199 Diaphragm Seal Systems, Product Data Sheet, 92 pages (2008). |
Senateur et al. “Pulsed Injection MOCVD of Functional Electronic Oxides” Adv. Mater. Opt. Electron, 10, pp. 155-161 (2000). |
Shevtsov et al. “An Apparatus for Pulse Chemical Vapor Deposition of Layers” Instruments and Experimental Techniques, vol. 56, No. 3, pp. 353-357 (2013). |
Shevtsov et al. “Effect of Spatial Image Transfer in a Pulse MOCVD Process” Physics Procedia 46, pp. 27-32 (2013). |
Stannowski et al. “Growth process and properties of silicon nitride deposited by hot-wire chemical vapor deposition” J Applied Physics, vol. 93 No. 5, 9 pages (2013). |
Tomozeiu et al. “Effects of UV photon irradiation on SiOx (0<x<2) structural properties” Applied Surface Science 253, pp. 376-380 (2006). |
US PPA 60394086 filed Jul. 3, 2002 in the name of Jacques Schmitt, and entitled “ALD on a Rotary Susceptor” pp. 1-23 (2002). |
US PPA 62293897 filed Feb. 11, 2016 in the names of Bernardo Donoso et al., and entitled “Vapor Based Site-Isolated Processing Systems and Methods” pp. 1-51 (2016). |
Vallat et al. “Area selective deposition of TiO2 by intercalation of plasma etching cycles in PEALD process: A bottom up approach for the simplification of 3D integration scheme” Journal of Vacuum Science & Technology A 37(2), 12 pages (2019). |
Vallat et al. “Selective deposition of Ta2O5 by adding plasma etching super-cycles in plasma enhanced atomic layer deposition steps” Journal of Vacuum Science & Technology A 35(1), 7 pages (2016). |
Venkatesan et al. “A rugged lead-ruthenate pyrochlore membrane catalyst for highly seelctive oxidation of alcohols” J. Molecular Catalysis A: Chemical 250, pp. 87-93 (2006). |
Xiao “Introduction to Semiconductor Manufacturing Technology” SPIE Press, ISBN 978-0-08194-9092-6, pp. 237-245 (2012). |
Yuan et al. “A Bifunctional Air Electrode Catalyzed by Lead Ruthenate for Li-Air Batteries” ECS Transactions 69(19), pp. 23-32 (2015). |
Zhao et al. “Surface Chemistry of Thermal Dry Etching of Cobalt Thin Films Using Hexafluoroacetylacetone (hfacH)” Appl Surf Sci. 455, pp. 438-445 (2018). |
Zhao et al. “Thermal and Plasma-Enhanced Atomic Layer Deposition of Yttrium Oxide Films and the Properties of Water Wettability” Appl. Mater. Interfac. 12(2), 9 pages (2019). |
CNIPA; Notice of Allowance dated Dec. 21, 2020 in Application No. 201610982040.X. |
CNIPA; Office Action dated Nov. 20, 2020 in Application No. 201710762817.6. |
CNIPA; Notice of Allowance dated Dec. 28, 2020 in Application No. 201930704935.1. |
CNIPA; Notice of Allowance dated Dec. 10, 2020 in Application No. 202030352604.9. |
CNIPA; Office Action dated Jan. 25, 2021 in Application No. 202030579755.8. |
JPO; Notice of Allowance dated Nov. 27, 2020 in Application No. 2016-206625. |
JPO; Office Action dated Jan. 26, 2021 in Application No. 2017-139817. |
JPO; Notice of Allowance dated Nov. 26, 2020 in Application No. 2020-502653. |
KIPO; Office Action dated Jan. 25, 2021 in Application No. 10-2014-0011765. |
KIPO; Notice of Allowance dated Jan. 4, 2021 in Application No. 10-2014-0060120. |
KIPO; Notice of Allowance dated Jan. 4, 2021 in Application No. 10-2014-0071653. |
KIPO; Office Action dated Nov. 29, 2020 in Application No. 10-2014-0105478. |
KIPO; Office Action dated Feb. 17, 2021 in Application No. 10-2014-0122903. |
KIPO; Office Action dated Jan. 25, 2021 in Application No. 10-2014-0145220. |
KIPO; Office Action dated Jan. 6, 2021 in Application No. 10-2015-0025314. |
KIPO; Office Action dated Dec. 23, 2020 in Application No. 10-2019-0044213. |
KIPO; Office Action dated Nov. 14, 2020 in Application No. 10-2020-0101096. |
KIPO; Notice of Allowance dated Oct. 20, 2020 in Application No. 30-2019-0054642. |
KIPO; Notice of Allowance dated Oct. 22, 2020 in Application No. 30-2019-0058566 (M001). |
KIPO; Notice of Allowance dated Oct. 22, 2020 in Application No. 30-2019-0058566 (M002). |
KIPO; Notice of Allowance dated Dec. 1, 2020 in Application No. 30-2019-0061607. |
KIPO; Office Action dated Jan. 26, 2021 in Application No. 30-2020-0005953 (M001). |
KIPO; Office Action dated Jan. 26, 2021 in Application No. 30-2020-0005953 (M002). |
KIPO; Notice of Allowance dated Dec. 23, 2020 in Application No. 30-2020-0006059. |
KIPO; Notice of Allownace dated Dec. 25, 2020 in Application No. 30-2020-0006223. |
KIPO; Notice of Allowance dated Feb. 1, 2021 in Application No. 30-2020-0006385. |
KIPO; Notice of Allowance dated Feb. 1, 2021 in Application No. 30-2020-0006391. |
TIPO; Office Action dated Dec. 2, 2020 in Application No. 105131896. |
TIPO; Notice of Allowance dated Jan. 29, 2021 in Application No. 105142668. |
TIPO; Notice of Allowance dated Dec. 10, 2020 in Application No. 106108152. |
TIPO; Notice of Allowance dated Jan. 25, 2021 in Application No. 106111548. |
TIPO; Office Action dated Sep. 30, 2020 in Application No. 106113604. |
TIPO; Office Action dated Jan. 6, 2021 in Application No. 106115126. |
TIPO; Office Action dated Dec. 21, 2020 in Application No. 106122231. |
TIPO; Office Action dated Dec. 29, 2020 in Application No. 106124126. |
TIPO; Office Action dated Dec. 9, 2020 in Application No. 106124128. |
TIPO; Office Action dated Jan. 25, 2021 in Application No. 106124129. |
TIPO; Office Action dated Dec. 9, 2020 in Application No. 106124130. |
TIPO; Office Action dated Jan. 20, 2021 in Application No. 106129491. |
TIPO; Office Action dated Feb. 8, 2021 in Application No. 106133152. |
TIPO; Office Action dated Dec. 24, 2019 in Application No. 108105002. |
TIPO; Notice of Allowance dated Nov. 24, 2020 in Application No. 108307599. |
TIPO; Notice of Allowance dated Jan. 11, 2021 in Application No. 108307599D01. |
TIPO; Notice of Allowance dated Jan. 11, 2021 in Application No. 109300591. |
TIPO; Notice of Allowance dated Jan. 11, 2021 in Application No. 109300593. |
TIPO; Office Action dated Jan. 11, 2021 in Application No. 109300594. |
USPTO; Non-Final Office Action dated Dec. 1, 2020 in U.S. Appl. No. 14/219,879. |
USPTO; Final Office Action dated Feb. 1, 2021 in U.S. Appl. No. 14/829,565. |
USPTO; Non-Final Office Action dated Dec. 24, 2020 in U.S. Appl. No. 15/286,503. |
USPTO; Final Office Action dated Feb. 12, 2021 in U.S. Appl. No. 15/377,439. |
USPTO Non-Final Office Action dated Dec. 10, 2020 in U.S. Appl. No. 15/380,921. |
USPTO; Non-Final Office Action dated Feb. 3, 2021 in U.S. Appl. No. 15/611,707. |
USPTO; Final Office Action dated Jan. 19, 2021 in U.S. Appl. No. 15/636,307. |
USPTO; Non-Final Office Action dated Jan. 6, 2021 in U.S. Appl. No. 15/726,959. |
USPTO; Advisory Action dated Dec. 15, 2020 in U.S. Appl. No. 15/835,328. |
USPTO; Notice of Allowance dated Jan. 14, 2021 in U.S. Appl. No. 15/835,352. |
USPTO; Final Office Action dated Jan. 11, 2021 in U.S. Appl. No. 15/890,037. |
USPTO; Advisory Action dated Jan. 8, 2021 in U.S. Appl. No. 15/923,834. |
USPTO; Advisory Action dated Dec. 24, 2020 in U.S. Appl. No. 15/925,532. |
USPTO; Non-Final Office Action dated Jan. 25, 2021 in U.S. Appl. No. 15/925,532. |
USPTO; Final Office Action dated Feb. 18, 2021 in U.S. Appl. No. 15/940,729. |
USPTO; Final Office Action dated Jan. 12, 2021 in U.S. Appl. No. 15/940,759. |
USPTO; Final Office Action dated Dec. 15, 2020 in U.S. Appl. No. 15/962,980. |
USPTO; Advisory Action dated Oct. 27, 2020 in U.S. Appl. No. 15/974,948. |
USPTO; Advisory Action dated Dec. 10, 2020 in U.S. Appl. No. 16/000,109. |
USPTO; Advisory Action dated Dec. 15, 2020 in U.S. Appl. No. 16/000,125. |
USPTO; Advisory Action dated Dec. 14, 2020 in U.S. Appl. No. 16/000,156. |
USPTO; Advisory Action dated Dec. 22, 2020 in U.S. Appl. No. 16/004,041. |
USPTO; Non-Final Office Action dated Nov. 24, 2020 in U.S. Appl. No. 16/039,938. |
USPTO; Advisory Action dated Jan. 14, 2021 in U.S. Appl. No. 16/055,532. |
USPTO; Final Office Action dated Dec. 15, 2020 in U.S. Appl. No. 16/108,950. |
USPTO; Final Office Action dated Jan. 6, 2021 in U.S. Appl. No. 16/117,530. |
USPTO; Notice of Allowance dated Feb. 12, 2021 in U.S. Appl. No. 16/128,282. |
USPTO; Notice of Allowance dated Feb. 8, 2021 in U.S. Appl. No. 16/132,142. |
USPTO; Final Office Action dated Dec. 14, 2020 in U.S. Appl. No. 16/151,074. |
USPTO; Advisory Action dated Feb. 16, 2021 in U.S. Appl. No. 16/151,074. |
USPTO; Final Office Action dated Dec. 18, 2020 in U.S. Appl. No. 16/167,164. |
USPTO; Advisory Action dated Dec. 21, 2020 in U.S. Appl. No. 16/172,535. |
USPTO; Final Office Action dated Jan. 29, 2021 in U.S. Appl. No. 16/176,517. |
USPTO; Non-Final Office Action dated Dec. 11, 2021 in U.S. Appl. No. 16/202,941. |
USPTO; Final Office Action dated Dec. 9, 2020 in U.S. Appl. No. 16/210,922. |
USPTO; Notice of Allowance dated Dec. 15, 2020 in U.S. Appl. No. 16/242,852. |
USPTO; Advisory Action dated Jan. 22, 2021 in U.S. Appl. No. 16/252,567. |
USPTO; Final Office Action dated Dec. 8, 2020 in U.S. Appl. No. 16/397,045. |
USPTO; Advisory Action dated Jan. 27, 2021 in U.S. Appl. No. 16/397,045. |
USPTO; Final Office Action dated Dec. 14, 2020 in U.S. Appl. No. 16/400,814. |
USPTO; Non-Final Office Action dated Jan. 12, 2021 in U.S. Appl. No. 16/453,249. |
USPTO; Non-Final Office Action dated Dec. 28, 2020 in U.S. Appl. No. 16/517,122. |
USPTO; Non-Final Office Action dated Feb. 11, 2021 in U.S. Appl. No. 16/565,460. |
USPTO; Notice of Allowance dated Jan. 25, 2021 in U.S. Appl. No. 16/679,885. |
USPTO; Non-Final Office Action dated Feb. 8, 2021 in U.S. Appl. No. 16/685,787. |
USPTO; Non-Final Office Action dated Jan. 8, 2021 in U.S. Appl. No. 16/752,514. |
USPTO; Notice of Allowance dated Dec. 28, 2020 in U.S. Appl. No. 16/833,279. |
USPTO; Notice of Allowance dated Nov. 23, 2020 in U.S. Appl. No. 29/726,623. |
Aoyagi et al. “Laser-assisted atomic layer epitaxy” Materials Science and Engineering, pp. 121-132 (1991). |
Galesic et al. “Formation of vanadium nitride by rapid thermal processing” Thin Solid Films 349(1), 7 pages (1999). |
Kim et al. “High Growth Rate in Atomic Layer Deposition of TiO2 Thin Films by UV Irradiation” Electrochemical and Solid-State Letters, 14(4), pp. H146-H148 (2011). |
Lee et al. “Enahancement of Iodine Adsorption on Ruthenium Glue Layer for Seedless CECVD of Cu” Electrochemical and Solid-State Letters, 8(2) C39-C42 (2005). |
Lee et al. “Growth without Postannealing of Monoclinic VO2 Thin Film by Atomic Layer Deposition Using VC14 as Precursor” Coatings, 8, 431, pp. 1-11 (2018). |
Lee et al. “Photo-Induced Atomic Layer Deposition of Tantalum Oxide Thin Films from Ta(OC2H5)5 and O2” J of the Electrochemical Society. 151(1) pp. C52-C55 (2004). |
Merdrignac-Conanec et al. “Nitridation under ammonia of high surface area vanadium aerogels” Journal of Solid State Chemistry 178(1), 8 pages (2005). |
Nikolic et al. “The dependence of the work function of rare earth metals on their electron structure” Microelectronics Journal 27, 93-96 (1996). |
Putkonen et al. “Low-Temperature ALE Deposition of Y2O3 Thin Films from β-Diketonate Precursors” Chemical Vapor Deposition 7(1) pp. 44-50 (2001). |
US PPA 62274238 filed Jan. 1, 2016 in the names of Alexander S. Polyak et al., and entitled “Non-Metallic Thermal CVD/ALD Gas Injector and Purge System” pp. 1-63 (2016). |
Vayrynen et al. “Photo-Assisted Atomic Layer Deposition and Chemical Vapor Deposition of Metal and Metal Oxide Thin Films” Thesis, Oct. 2015, 146 pages (2005). |
Number | Date | Country | |
---|---|---|---|
20170186754 A1 | Jun 2017 | US |
Number | Date | Country | |
---|---|---|---|
62272345 | Dec 2015 | US |