The present disclosure relates to methods for the manufacture of microelectronic workpieces, and in particular, methods to etch material layers on microelectronic workpieces.
Device formation within microelectronic workpieces typically involves a series of manufacturing techniques related to the formation, patterning, and removal of a number of layers of material on a substrate. To meet the physical and electrical specifications of current and next generation semiconductor devices, processing flows are being requested to reduce feature size while maintaining structure integrity for various patterning processes.
Extreme ultra-violet (EUV) techniques have been used for photolithography processes to achieve reduced feature size in the manufacture of microelectronic workpieces. Because EUV photoresist patterns have very small dimensions, patterned photoresist (PR) is often unable to maintain its pattern during subsequent etch processes. Further, increases in aspect ratios for patterned structures from further scaling and greater density promotes the onset of pattern collapse. Prior solutions have tried to reduce the risk of pattern collapse by changing the photoresist hardness through composition or molecular configuration (bonding) changes. However, pattern collapse has still occurred with these prior solutions.
Embodiments are described herein for selective atomic layer deposition (ALD) of protective caps to enhance EUV processes for the manufacture of microelectronic workpieces. The disclosed methods and related systems use these selective ALD caps to make photoresists, such as EUV photoresists, more resistant to etch erosion without changing the patterning dimensions. Different or additional features, variations, and embodiments can also be implemented, and related systems and methods can be utilized as well.
For one embodiment, a method of processing microelectronic workpieces is disclosed including depositing a protective material on a patterned extreme ultraviolet (EUV) photoresist layer using selective atomic layer deposition (ALD) to form protective caps on top regions for the patterned EUV photoresist layer and transferring a pattern for the patterned EUV photoresist layer to one or more underlying layers using one or more etch processes.
In additional embodiments, the protective caps allow a target level of erosion to be achieved for the patterned EUV photoresist layer during the transferring. In further embodiments, an erosion of 2 percent or less of the height of the patterned EUV photoresist layer above an underlying layer is achieved.
In additional embodiments, the method also includes forming an EUV photoresist layer over the one or more underlying layers and patterning the EUV photoresist layer to form the patterned EUV photoresist layer. In further embodiments, the patterning includes depositing an EUV material, exposing a first portion of the EUV material to EUV radiation, and removing a second portion of the EUV material not exposed to the EUV radiation to form the patterned EUV photoresist layer.
In additional embodiments, the method also includes removing the protective caps and the patterned EUV photoresist layer. In further embodiments, the protective material includes at least one of aluminum oxide (Al2O3), silicon oxide (SiO2), or titanium oxide (TiO2). In further embodiments, the patterned photoresist layer includes an argon fluoride (ArF) photoresist. In still further embodiments, the depositing forms protective caps without covering exposed regions of an underlying layer.
In additional embodiments, the depositing includes positioning the microelectronic workpiece in an ALD processing tool and rotating the microelectronic workpiece through a plurality of processing regions within the ALD processing tool to deposit the protective material. In further embodiments, the protective material includes at least one of aluminum oxide (Al2O3), silicon oxide (SiO2), or titanium oxide (TiO2). In still further embodiments, the depositing of the protective material forms a coating of 1 to 10 nanometers.
In additional embodiments, the method also includes rotating the microelectronic workpiece through a precursor adsorption region, a separation region of nitrogen N2 flow, and an oxidation and plasma treatment region to complete each layer of deposition. In further embodiments, the method includes also rotating the microelectronic workpiece through a final separation region of N2 flow for each layer of deposition.
In additional embodiments, the protective material is aluminum oxide (Al2O3), and TMA (trimethyl aluminum) is used for the precursor absorption region for the ALD processing tool. In further embodiments, a supply for the TMA is reduced in the precursor absorption region to facilitate selective deposition of the protective material to the top regions of the patterned EUV photoresist layer.
In additional embodiments, the rotating occurs at a rate sufficient to the selectively deposit the protective material on the top regions of the patterned EUV photoresist layer. In further embodiments, the rotating occurs at a rotations-per-minute (rpm) of 200 rpm or greater. In further embodiments, the protective material is 20-40% thicker at the top regions of the patterned EUV photoresist layer as compared to other regions where the protective material is deposited. In still further embodiments, the top regions include up to thirty percent of the height that the patterned EUV photoresist layer extends above an underlying layer immediately below the patterned EUV photoresist layer.
A more complete understanding of the present inventions and advantages thereof may be acquired by referring to the following description taken in conjunction with the accompanying drawings, in which like reference numbers indicate like features. It is to be noted, however, that the accompanying drawings illustrate only exemplary embodiments of the disclosed concepts and are therefore not to be considered limiting of the scope, for the disclosed concepts may admit to other equally effective embodiments.
As described herein, an ALD thin film can be selectively deposited on the top of photoresist patterns, such as patterned EUV photoresist layers, to provide a protective cap against etch damage during pattern transfer. Some deposition of the protective material on the sidewalls of the photoresist pattern is acceptable, and any deposition on exposed regions of an underlying layer below the patterned photoresist layer is preferably thinner than the deposition at the top of the photoresist pattern. No deposition of the protective material on the exposed regions of the underlying layer is considered optimal, although is not a requirement for the disclosed embodiments. Protecting patterned photoresist layers from etch damage as described herein provides more photoresist options. Further, the selective deposition increases the flexibility of options to improve etch resistance for various processes/materials. It is further noted that the selective deposition of protective caps on photoresist structures can be implemented, for example, through the application of high-rotation speeds to spatial ALD techniques as described herein. Other advantages and implementations can also be achieved while still taking advantage of the process techniques described herein.
EUV lithography is one of the candidates for enabling next generation devices by cost friendly processes to achieve sub-22 nanometer (nm) half-pitch dimensions and below. For such sub-22 nm processes, two critical problems that have become difficult to control are photoresist erosion and pattern collapse. Photoresist erosion degrades the ability to transfer the resist feature patterns by etch processes to underlying layers due to decreases in resist thickness. Pattern collapse is promoted by the increase of aspect ratio that comes from further scaling down of feature sizes in next generation devices. Aspect ratio is a term used to describe the dimensions of resist critical dimension (CD) width to the resist height and expressing it in ratio form. One technique to overcome the pattern collapse is to reduce the resist thickness to achieve lower aspect ratios. The reduction of the resist thickness to achieve lower aspect ratios, however, also reduces the ability to fully transfer resist patterns by etch processes to underlying layers, particularly where erosion to the photoresist occurs during pattern transfer etch processes.
The embodiments disclosed herein enable low aspect ratio resist with sufficient etch transfer during etch processes by protecting patterned photoresist layers through selective atomic layer deposition (ALD) of protective caps to enhance EUV processes for the manufacture of microelectronic workpieces. The disclosed embodiments in part provide for the selective deposition of a protective cap material onto the top region of a patterned photoresist layer as protective caps to preserve the pattern during etch transfer of the pattern to the underlying layers. The material for the protective caps can be aluminum oxide (Al2O3), silicon oxide (SiO2), titanium oxide (TiO2), and/or other suitable protective cap material that provides a compatible deposition material. The disclosed techniques are particular useful to protect patterned EUV photoresist layers, such as patterned argon fluoride (ArF) photoresist layers, and/or other patterned photoresist layers.
It is noted that the selective deposition is preferably used to deposit the protective material to caps only on the top regions of the patterned layers, and not on the sidewalls or bottom substrate regions. However, where deposition does occur on the sidewalls or bottom substrate regions, the deposition is preferably thicker at the top of the patterned layer and thinner on the sidewall or bottom substrate. For example, the protective material deposited on the patterned photoresist layer is preferably 20 to 40 percent thicker at the top regions of patterned photoresist layers. It is also noted that the top regions for the patterned photoresist layer represents the top five to thirty percent of the height that the patterned photoresist layer extends above the next underlying layer. As such, the pattern can be transferred to the substrate or underlying layer with an etch process before breaking through to the patterned photoresist layer.
It is again noted that the top regions for the patterned photoresist layer 202 represent the top five to thirty percent of the height that the patterned photoresist layer 202 extends above the underlying layer 204. It is further noted that the patterned photoresist layer 202 can be made from an EUV photoresist material and can be patterned by depositing an EUV material, exposing a first portion of the EUV material to EUV radiation, and removing a second portion of the EUV material not exposed to the EUV radiation to form the patterned photoresist layer 202. It is further noted that EUV radiation is electromagnetic radiation having wavelengths of 200 nm or less and preferable 20 nm or less.
This spatial ALD processing tool, for example, can transfer the microelectronic workpieces 504 through a sequence of processing regions to complete a layer of deposition including a precursor adsorption region, followed by a separation region of nitrogen (N2) flow, followed by an oxidation and plasma treatment region. These regions can also be followed by a final separation region of N2 flow for the deposition of each layer. This sequence of processing through different ALD processing regions can be repeated until a selected number of layers have been deposited.
For the embodiments described herein, the rotation of the susceptor 502 is performed at a relative high rate of 200 rotations-per-minute (rpm) or greater. More generally, the rotation is provided at a rate sufficient to selectively deposit the protective material preferentially on the top regions of the patterned EUV photoresist layer in order to form protective caps. In addition for some embodiments, the precursor exposure region and the oxidation exposure region have dedicated exhaust systems designed to prevent precursor and oxidation mixing even at high wafer rotation rates. Other variations could also be implemented.
The selectivity of the deposition of the protective material (e.g., AlOx) to the top of the pattern from deposition can also be enhanced using various techniques. For example, reducing the TMA (trimethyl aluminum) supply in the precursor region for the spatial ALD processing tool helps to deplete the AlOx deposition as it reaches the pattern from the top of the features and thereby provides for selective ALOx deposition to the top to the pattern. For example, TMA supply reduction can be achieved by combining two methods: (1) pulsing the TMA during the high rate (e.g., 240 rpm, 200 rpm or greater) deposition process and (2) increasing the N2 co-flow through the TMA injector, which effectively reduces the vacuum pressure seen by the TMA in the source ampoule.
It is noted that one or more deposition processes can be used to form the material layers described herein. For example, one or more depositions can be implemented using chemical vapor deposition (CVD), plasma enhanced CVD (PECVD), physical vapor deposition (PVD), atomic layer deposition (ALD), and/or other deposition processes. For a plasma deposition process, a precursor gas mixture can be used including but not limited to hydrocarbons, fluorocarbons, or nitrogen containing hydrocarbons in combination with one or more dilution gases (e.g., argon, nitrogen, etc.) at a variety of pressure, power, flow and temperature conditions. Lithography processes with respect to PR layers can be implemented using optical lithography, extreme ultra-violet (EUV) lithography, and/or other lithography processes. The etch processes can be implemented using plasma etch processes, discharge etch processes, and/or other desired etch processes. For example, plasma etch processes can be implemented using plasma containing fluorocarbons, oxygen, nitrogen, hydrogen, argon, and/or other gases. In addition, operating variables for process steps can be controlled to ensure that CD target parameters for vias are achieved during via formation. The operating variables may include, for example, the chamber temperature, chamber pressure, flowrates of gases, frequency and/or power applied to electrode assembly in the generation of plasma, and/or other operating variables for the processing steps. Variations can also be implemented while still taking advantage of the techniques described herein.
It is noted that reference throughout this specification to “one embodiment” or “an embodiment” means that a particular feature, structure, material, or characteristic described in connection with the embodiment is included in at least one embodiment of the invention, but do not denote that they are present in every embodiment. Thus, the appearances of the phrases “in one embodiment” or “in an embodiment” in various places throughout this specification are not necessarily referring to the same embodiment of the invention. Furthermore, the particular features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments. Various additional layers and/or structures may be included and/or described features may be omitted in other embodiments.
“Microelectronic workpiece” as used herein generically refers to the object being processed in accordance with the invention. The microelectronic workpiece may include any material portion or structure of a device, particularly a semiconductor or other electronics device, and may, for example, be a base substrate structure, such as a semiconductor substrate or a layer on or overlying a base substrate structure such as a thin film. Thus, workpiece is not intended to be limited to any particular base structure, underlying layer or overlying layer, patterned or unpatterned, but rather, is contemplated to include any such layer or base structure, and any combination of layers and/or base structures. The description below may reference particular types of substrates, but this is for illustrative purposes only and not limitation.
The term “substrate” as used herein means and includes a base material or construction upon which materials are formed. It will be appreciated that the substrate may include a single material, a plurality of layers of different materials, a layer or layers having regions of different materials or different structures in them, etc. These materials may include semiconductors, insulators, conductors, or combinations thereof. For example, the substrate may be a semiconductor substrate, a base semiconductor layer on a supporting structure, a metal electrode or a semiconductor substrate having one or more layers, structures or regions formed thereon. The substrate may be a conventional silicon substrate or other bulk substrate comprising a layer of semi-conductive material. As used herein, the term “bulk substrate” means and includes not only silicon wafers, but also silicon-on-insulator (“SOI”) substrates, such as silicon-on-sapphire (“SOS”) substrates and silicon-on-glass (“SOG”) substrates, epitaxial layers of silicon on a base semiconductor foundation, and other semiconductor or optoelectronic materials, such as silicon-germanium, germanium, gallium arsenide, gallium nitride, and indium phosphide. The substrate may be doped or undoped.
Systems and methods for processing a microelectronic workpiece are described in various embodiments. One skilled in the relevant art will recognize that the various embodiments may be practiced without one or more of the specific details, or with other replacement and/or additional methods, materials, or components. In other instances, well-known structures, materials, or operations are not shown or described in detail to avoid obscuring aspects of various embodiments of the invention. Similarly, for purposes of explanation, specific numbers, materials, and configurations are set forth in order to provide a thorough understanding of the invention. Nevertheless, the invention may be practiced without specific details. Furthermore, it is understood that the various embodiments shown in the figures are illustrative representations and are not necessarily drawn to scale.
Further modifications and alternative embodiments of the described systems and methods will be apparent to those skilled in the art in view of this description. It will be recognized, therefore, that the described systems and methods are not limited by these example arrangements. It is to be understood that the forms of the systems and methods herein shown and described are to be taken as example embodiments. Various changes may be made in the implementations. Thus, although the inventions are described herein with reference to specific embodiments, various modifications and changes can be made without departing from the scope of the present inventions. Accordingly, the specification and figures are to be regarded in an illustrative rather than a restrictive sense, and such modifications are intended to be included within the scope of the present inventions. Further, any benefits, advantages, or solutions to problems that are described herein with regard to specific embodiments are not intended to be construed as a critical, required, or essential feature or element of any or all the claims.
This application claims priority to the following co-pending provisional application: U.S. Provisional Patent Application Ser. No. 62/688,960, filed Jun. 22, 2018, and entitled “SELECTIVE ALD CAP TO ENHANCE EUV ETCH RESISTANCE,” and U.S. Provisional Patent Application Ser. No. 62/741,415, filed Oct. 4, 2018, and entitled “SELECTIVE ATOMIC LAYER DEPOSITION (ALD) OF PROTECTIVE CAPS TO ENHANCE EXTREME ULTRA-VIOLET (EUV) ETCH RESISTANCE,” which are hereby incorporated by reference in their entirety.
| Number | Date | Country | |
|---|---|---|---|
| 62688960 | Jun 2018 | US | |
| 62741415 | Oct 2018 | US |