The present disclosure relates to substrate processing systems, and more particularly to substrate processing systems and methods for seamless feature fill.
The background description provided herein is for the purpose of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent the work is described in this background section, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure.
Shallow trench isolation (STI) provides electrical isolation between individual transistor devices in integrated circuits (ICs). STIs include trenches that are filled with high quality silicon (Si) oxide film. In some applications, an aspect ratio (AR) of the trench can be as high as 8:1 and an opening of the trench may narrow down to about 20 nm. Achieving void free STI fill is important because the film may be subjected to further processing in subsequent integration steps, which can expose the void. In some examples, the void may then be unintentionally filled with conductive material, which can lead to short circuits between different conductors on the chip.
In some applications, STIs are filled with film using high density plasma chemical vapor deposition (HDPCVD). However, for trenches with an AR that is higher than 4:1, it becomes very challenging for HDPCVD oxide to fill the STI without voids, even using a deposition-etch-deposition cyclic process.
Referring now to
While emerging flowable oxide methods provide liquid-like filling behavior, the requirement of flowability limits the achievable film density. Although post-deposition densification methods are available at extra cost, these methods have not proven successful. The alternative methods are not able to densify the film in a high aspect ratio structure due to the constraint of the surrounding sidewalls, which prevents the shrinkage required to fully densify the flowable oxide film.
ALD oxide may be used to gapfill deep trenches with high quality Si oxide film. However, a seam usually remains at a center of the trench after the film that is deposited on the side walls merges. Referring now to
This section provides a general summary of the disclosure, and is not a comprehensive disclosure of its full scope or all of its features.
A method for depositing film in a substrate processing system includes performing a first atomic layer deposition (AID) cycle in a processing chamber to deposit film on a substrate including a feature; after the first ALD cycle, exposing the substrate to an inhibitor plasma in the processing chamber for a predetermined period to create a varying passivated surface in the feature; and after the predetermined period, performing a second ALD cycle in the processing chamber to deposit film on the substrate.
In other features, prior to performing the first ALD cycle, the method includes exposing the substrate to the inhibitor plasma in the processing chamber. The first ALD cycle and the second ALD cycle include exposing the substrate to a first reactant during a first predetermined period; evacuating reactants from the processing chamber after the first predetermined period; exposing the substrate to a second reactant that is different than the first reactant during a second predetermined period; and evacuating reactants from the processing chamber after the second predetermined period.
In other features, the film includes silicon dioxide. Exposing the substrate to the inhibitor plasma includes supplying an inhibitor gas; striking the inhibitor plasma; maintaining the inhibitor plasma for the predetermined period; and after the predetermined period, turning the inhibitor plasma off.
In other features, the inhibitor plasma inhibits subsequent film deposition in an increasing manner in the feature as a depth of the feature decreases. The inhibitor plasma is created using molecular nitrogen as an inhibitor gas.
In other features, the varying passivated surface in the feature improves bottom-up fill of the feature to prevent a seam in the feature. The method further includes exposing the substrate to the inhibitor plasma and performing additional ALD cycles after the second ALD cycle to bottom-up fill the feature without a seam. The inhibitor plasma is created using a gas selected from a group consisting of molecular nitrogen, argon, helium, molecular hydrogen, ammonia or combinations thereof. The feature has an aspect ratio that is greater than 4:1 and an opening that is less than or equal to 30 nanometers.
In other features, the inhibitor plasma is generated using a first plasma source and the first ALD cycle is performed using the first plasma source. The inhibitor plasma is generated using a first plasma source and the first ALD cycle is performed using a second plasma source that is different than the first plasma source. The inhibitor plasma is generated using a first plasma source and the first ALD cycle and the second ALD cycle are performed without using plasma.
In other features, the method includes performing one or more ALD cycles prior to the first ALD cycle without using inhibitor plasma therebetween. The method includes using a process that is different than the first ALD cycle and the second ALD cycle to fill at least part of the feature with a material after performing the first ALD cycle and the second ALD cycle. The first ALD cycle and the second ALD cycle deposit dielectric film. The material includes another dielectric film that is different than the dielectric film. The material includes metal. The feature includes a trench. The feature includes a hole.
A substrate processing system for depositing film includes a processing chamber including a pedestal configured to support a substrate including a feature. A gas supply is configured to selectively supply atomic layer deposition (ALD) process gas to the processing chamber and to selectively supply inhibitor gas to the processing chamber. A plasma generator is configured to selectively generate inhibitor plasma in the processing chamber. A controller is configured to control the gas supply and the plasma generator. The controller is further configured to perform a first ALD cycle in the processing chamber to deposit film on the substrate; after the first ALD cycle, expose the substrate in the processing chamber to the inhibitor plasma generated using the inhibitor gas for a predetermined period to create a varying passivated surface in the feature; and after the predetermined period, perform a second ALD cycle in the processing chamber to deposit film on the substrate.
In other features, the controller is configured to expose the substrate to the inhibitor plasma prior to performing the first ALD cycle. During the first ALD cycle and the second ALD cycle, the controller is configured to expose the substrate to a first reactant for a first predetermined period; evacuate reactants from the processing chamber after the first predetermined period; expose the substrate to a second reactant that is different than the first reactant for a second predetermined period; and evacuate reactants from the processing chamber after the second predetermined period.
In other features, the film includes silicon dioxide. When exposing the substrate to the inhibitor plasma, the controller is configured to supply an inhibitor gas; strike the inhibitor plasma; maintain the inhibitor plasma for the predetermined period; and after the predetermined period, turn the inhibitor plasma off.
In other features, the inhibitor plasma inhibits subsequent film deposition in an increasing manner in the feature as a depth of the feature decreases. The inhibitor plasma is created using molecular nitrogen as the inhibiting gas. The varying passivated surface in the feature improves bottom-up fill of the feature to prevent a seam in the feature. The controller is further configured to expose the substrate to the inhibitor plasma and perform additional ALD cycles after the second ALD cycle to bottom-up fill the feature without a seam.
In other features, the inhibitor gas is selected from a group consisting of molecular hydrogen, ammonia or combinations thereof. The feature has an aspect ratio that is greater than 4:1 and an opening that is less than or equal to 30 nanometers.
Further areas of applicability will become apparent from the description provided herein. The description and specific examples in this summary are intended for purposes of illustration only and are not intended to limit the scope of the present disclosure.
In the drawings, reference numbers may be reused to identify similar and/or identical elements.
The present disclosure describes systems and methods for filling features on a substrate. In some examples, the features are formed below a field region of the substrate. In some examples, a seam that is formed in a hole or trench (such as a shallow trench insulator (STI)) during gapfill is eliminated using an atomic layer deposition (ALD) process. While STI applications are disclosed, the present disclosure applies to other applications requiring feature fill such as, but not limited to, pre-metal dielectric, 3D NAND, deep trenches, etc. The systems and methods described herein enhance bottom-up feature fill during the ALD process by exposing the substrate to inhibitor plasma between at least some ALD cycles performed during feature fill.
In some examples, the feature is substantially filled by the ALD cycles. In other examples, the feature is not completely filled by the ALD cycles and other material is used to fill the feature. Examples of other materials include metal or dielectric having a different composition.
The inhibitor plasma creates a passivated surface and increases a nucleation barrier of the deposited ALD film. When the inhibitor plasma interacts with material in the feature, the material at the bottom of the feature receives much less plasma treatment than material located closer to a top portion of the feature or the field because of the geometrical shadowing effect. As a result, deposition at the feature top is selectively inhibited and deposition in lower portions of the feature proceeds with less inhibition or without being inhibited. As a result, bottom-up fill is enhanced, which creates a more favorable sloped profile that mitigates the seam effect.
In some examples, molecular nitrogen (N2) may be used as the source gas for the inhibitor plasma, particularly when the deposited film is SiO2. As can be appreciated, ALD SiO2 nucleates at a slower rate on a nitride surface. In other examples, the inhibitor plasma source gas is selected from a group consisting of N2, argon (Ar), helium (He), molecular hydrogen (H2), ammonia (NH3), or combinations thereof.
The systems and methods described herein enable ALD Si oxide process to be used in STI or other applications. The ALD oxide process with N2 inhibitor plasma is capable of filling much more difficult structures such as those with higher AR or narrower feature sizes as compared to HDPCVD oxide due to the nature of conformal deposition. In some examples, the AR is greater than or equal to 4:1, 6:1, or 8:1. In some examples, the feature opening is less than or equal to 30 nm, 25 nm or 20 nm. Compared to the flowable oxide process, the ALD oxide process with inhibitor plasma provides improved film quality in terms of wet etch resistance and break down behavior.
Referring now to
A pedestal 318 supports a substrate 316. The pedestal 318 typically includes a chuck, a fork, or lift pins to hold and transfer the substrate during and between the deposition and/or plasma treatment reactions. The chuck may be an electrostatic chuck, a mechanical chuck or other type of chuck. The process gases are introduced via inlet 312. Multiple source gas lines 310 are connected to a manifold 308. The gases may be premixed or not. Appropriate valves and mass flow control mechanisms are employed to ensure that the correct gases are delivered during the deposition and plasma treatment phases of the process.
Process gases exit chamber 324 via an outlet 322. A vacuum pump 326 draws process gases out and maintains a suitably low pressure within the system by a flow restriction device, such as a throttle valve or a pendulum valve. A controller 340 may be provided to monitor process parameters and to control a gas mixture, plasma, pedestal heating, chuck and/or removal of reactants from the process chamber.
In some examples, the ALD cycles may include plasma-enhanced ALD (PEALD). If PEALD is used, the plasma sources for the ALD cycles and the inhibition plasma may be the same plasma source. In other examples, different plasma sources may be used. It may be desirable to have some directionality for the inhibitor plasma whereas it may be desirable for the deposition source to have little or no directionality. In other words there could be two plasma sources, or one common plasma source, or one plasma source only for the inhibitor plasma.
Referring now to
As can be seen in
Referring now to
Referring now to
Referring now to
The foregoing description is merely illustrative in nature and is in no way intended to limit the disclosure, its application, or uses. The broad teachings of the disclosure can be implemented in a variety of forms. Therefore, while this disclosure includes particular examples, the true scope of the disclosure should not be so limited since other modifications will become apparent upon a study of the drawings, the specification, and the following claims. As used herein, the phrase at least one of A, B, and C should be construed to mean a logical (A or B or C), using a non-exclusive logical OR. It should be understood that one or more steps within a method may be executed in different order (or concurrently) without altering the principles of the present disclosure.
In this application, including the definitions below, the term controller may be replaced with the term circuit. The term controller may refer to, be part of, or include an Application Specific Integrated Circuit (ASIC); a digital, analog, or mixed analog/digital discrete circuit; a digital, analog, or mixed analog/digital integrated circuit; a combinational logic circuit; a field programmable gate array (FPGA); a processor (shared, dedicated, or group) that executes code; memory (shared, dedicated, or group) that stores code executed by a processor; other suitable hardware components that provide the described functionality; or a combination of some or all of the above, such as in a system-on-chip.
The term code, as used above, may include software, firmware, and/or microcode, and may refer to programs, routines, functions, classes, and/or objects. The term shared processor encompasses a single processor that executes some or all code from multiple controllers. The term group processor encompasses a processor that, in combination with additional processors, executes some or all code from one or more controllers. The term shared memory encompasses a single memory that stores some or all code from multiple controllers. The term group memory encompasses a memory that, in combination with additional memories, stores some or all code from one or more controllers. The term memory is a subset of the term computer-readable medium. The term computer-readable medium, as used herein, does not encompass transitory electrical or electromagnetic signals propagating through a medium (such as on a carrier wave); the term computer-readable medium may therefore be considered tangible and non-transitory. Non-limiting examples of a non-transitory, tangible computer-readable medium include nonvolatile memory (such as flash memory), volatile memory (such as static random access memory and dynamic random access memory), magnetic storage (such as magnetic tape or hard disk drive), and optical storage.
The apparatuses and methods described in this application may be partially or fully implemented by one or more computer programs executed by one or more processors. The computer programs include processor-executable instructions that are stored on at least one non-transitory, tangible computer-readable medium. The computer programs may also include and/or rely on stored data.
This application claims the benefit of U.S. Provisional Application No. 61/944,871, filed on Feb. 26, 2014. The entire disclosure of the application referenced above is incorporated herein by reference.
Number | Date | Country | |
---|---|---|---|
61944871 | Feb 2014 | US |