This application claims priority to and the benefit of Korean Patent Application No. 10-2011-0040716 filed in the Korean Intellectual Property Office on Apr. 29, 2011, the entire contents of which are incorporated herein by reference.
(a) Field of the Invention
The present invention relates to a lateral flow atomic layer deposition device.
(b) Description of the Related Art
Efforts to improve an apparatus or process for forming a high quality thin film on a substrate in the field of semiconductor devices have been made. Atomic layer deposition (ALD) has recently been proposed, in which two or more reaction materials are temporally isolated and sequentially fed onto a substrate, and a thin film is grown thereon through a surface reaction, followed by repeating such a process so as to form a thin film with a desired thickness. As the film is formed through a surface reaction, a thin film with a uniform thickness is formed over the entire surface of the substrate irrespective of protrusions and depressions thereof, and impurities are prevented from intruding into the thin film, thereby ensuring excellent film characteristics.
Various structures of reactors have been developed so as to realize the atomic layer deposition (ALD) process that is widely applied to semiconductor processes. Regarding the ALD process, the basic gas supply order of source gas supply/purge and reaction gas supply/purge is repeated until a desired thickness of a film is deposited. To realize excellent characteristics of the ALD process, there must be no inter-reaction between reaction gases during a process, differing from the conventional deposition method such as CVD, and to increase productivity for commercialization, switching time between the reaction gases must be swift. Showerhead-structured reactors have already been developed, but such structures have a limit in reducing the switching time between the reaction gases because of a problem such as a complex gas passage in the showerhead, and particles can be generated in the showerhead because of a reaction between remaining reaction gases therein, leading to low yield of semiconductor chips, so the above-noted structure has limits in commercialization.
To solve the problem of the atomic layer deposition device with the showerhead structure, a lateral flow reactor was developed. The lateral flow reactor has an optimized small reaction space for an atomic layer deposition process. The lateral flow reactor is well-described in the Korea Patent 624030 by ASM Genitech Korea Ltd. and U.S. Pat. No. 6,539,891, its family patent. The lateral flow reactor can have a gas flow control plate installed to supply at least two kinds of gases in the reaction space inside the reactor through a top part of the reactor.
The lateral flow atomic layer deposition device will now be described with reference to
Referring to
Referring to
A gas flow distance in the center of the gas inlet channel 141 is greater than that on the edge thereof, and resultantly, the amount of gas supplied to the center of the substrate is less than that of gas supplied to the edge region of the substrate per unit time, leading to a thinner film thickness at the center of the substrate than at the edge of the substrate.
As described, the gases in the conventional lateral flow reactor are supplied to one side of the reaction space to flow in the lateral direction over the substrate, and are then discharged to the opposite side. However, in the above-described reactor, the gases flow to the edge of the substrate and a relatively smaller amount of gases are supplied to the center of the substrate to thus reduce the film thickness at the center of the substrate.
The above information disclosed in this Background section is only for enhancement of understanding of the background of the invention and therefore it may contain information that does not form the prior art that is already known in this country to a person of ordinary skill in the art.
The present invention has been made in an effort to provide a lateral flow atomic layer deposition device in which more gases are induced to the center of a substrate.
An exemplary embodiment of the present invention provides a lateral flow atomic layer deposition device in which gases flow horizontally over the substrate in a reaction space formed between the substrate and an opposite side facing the substrate, including: a reactor cover for defining a reaction space together with a substrate supporting plate; a gas inlet unit disposed on one side of the reaction space, and having an internal shape that becomes wider when approaching the substrate; a gas outlet unit disposed on another side of the reaction space facing the one side of the reaction space, and having an internal shape that becomes wider when approaching the substrate; a gas inlet connected to the gas inlet unit; and a gas outlet connected to the gas outlet unit.
The gas inlet unit and the gas outlet unit are formed in the reactor cover.
The reactor cover includes a top wall, a bottom wall, and a side wall, the side wall surrounds at least a part of the side of the top wall, and the gas inlet unit and the gas outlet unit are formed to face each other on the top wall.
The gas inlet includes a plurality of inlets.
The gas inlet is disposed to face the substrate, and the gas inlet unit has an internal shape that becomes wider when approaching the substrate from the gas inlet.
Regarding a gas flow path across the substrate from the gas inlet through the gas inlet unit, the path through a center of the substrate is shorter than the path via an edge of the substrate.
According to the embodiment of the present invention, the gas flow control plate is eliminated and shapes of a gas inlet unit and a gas outlet unit of the reactor cover are controlled such that a gas flow path through the center of the substrate can be shorter than a gas flow path via the edge of the substrate, thereby increasing the amount of gas supplied to the center of the substrate per unit area. Therefore, a reduction of the film thickness at the center of the substrate occurring in the conventional lateral flow reactor can be prevented. Also, the shape of the gas inlet unit is changeable in various ways to supply gas in a desired manner.
In addition, in the conventional lateral flow reactor with a gas flow control plate described in
Advantages and features of the present invention and methods to achieve them will be elucidated from exemplary embodiments described below in detail with reference to the accompanying drawings. However, the present invention is not limited to exemplary embodiment disclosed herein but may be implemented in various forms. The exemplary embodiments are provided by way of example only so that a person of ordinary skill in the art can fully understand the disclosures of the present invention and the scope of the present invention. Therefore, the present invention will be defined only by the scope of the appended claims.
A lateral flow atomic layer deposition device according to an exemplary embodiment of the present invention will now be described with reference to accompanying drawings.
A lateral flow atomic layer deposition device according to an exemplary embodiment of the present invention will now be described with reference to
Referring to
The gas inlet unit 230 and the gas outlet unit 240 of the lateral flow atomic layer deposition device are formed in the reactor cover 220 as one body, the process gas input into the gas inlet unit 230 flows along a first path (a) that is formed on one side of the reactor, passes through a second path a1 on the substrate (S), and is used for the process, and the remaining process gas flows along a third path a2 and is then discharged to the outside through the gas outlet unit 240. As described, the lateral flow atomic layer deposition device supplies gas to one side of the reactor cover 220 without the conventional gas flow control plate and discharges the gas through another side on the facing side such that a flow path of the gas is simplified. Therefore, recombination and decomposition of gases during gas supply on the gas path can be reduced and the switching time of the gases is reduced, thereby reducing the process time.
The gas inlet unit 230 and the gas outlet unit 240 of a lateral flow atomic layer deposition device according to an exemplary embodiment of the present invention will now be described with reference to
Referring to
The source gas, reaction gas, purge gas, or a mixed gas thereof is supplied through the gas supply lines 1 of the gas inlet unit 230. A source supply line and a reaction gas supply line are merged at the gas mixer 3. When source gas is supplied to the reactor through the gas mixer 3, purge gas is supplied to the gas mixer 3 through the reaction gas supply line to prevent the source gas from flowing backward to the reaction gas supply line. A reaction gas is supplied to the reactor through the gas mixer 3, and a purge gas is supplied to the gas mixer 3 to prevent the reaction gas from flowing backward to the source gas supply line. According to another exemplary embodiment of the present invention, a 2-way valve can be used as a gas mixer to prevent gas from flowing backward to other gas line, or another device to prevent backward flow can be used.
The gas having passed the gas mixer 3 is supplied to the reactor through the inlet port 5 and flows to the substrate, and the inlet port 5 becomes wider as it approaches the bottom of the reaction space where the substrate is loaded. Therefore, the gas path from the gas inlet unit 230 to the center of the substrate (S) becomes shorter than that from the gas inlet unit 230 to the edge of the substrate (S). Also, the inside of the inlet port 5 has a curved shape so the gas smoothly flows at the curve. That is, the inlet port 5 has an internally curved shape which becomes gradually wider from the inlet unit. According to the lateral flow atomic layer deposition device with above-described configuration, the gas flow path to the central portion of the substrate is shorter than the gas flow path to the edge of the substrate such that the amount of gas per unit area supplied to the center of the substrate is increased. Hence, a film thickness reduction at the center of the substrate in the conventional lateral flow reactor can be prevented.
The gas supplied through the gas inlet unit 230 flows over the substrate (S) and is used for the film deposition, and the remaining gas flows to the outlet port 6 and is discharged to the outside through the gas outlet line 2. Like the inlet port 5, the outlet port 6 has an internally curved shape which becomes gradually narrower until reaching the gas outlet line 2 from the inside of the reactor. By the above-noted configuration, the gas supplied to the center of the substrate (S) can be easily discharged through a short path. In addition, the internal part of the outlet port 6 has a curved shape so the gas smoothly flows at the curve.
The lateral flow atomic layer deposition device according to the exemplary embodiment of the present invention eliminates the gas flow control plate used in the conventional lateral flow atomic layer deposition device and changed the shapes of the gas input part and the gas output part in the reactor cover to make the gas flow path to the center of the substrate shorter than the gas flow path to the edge of the substrate and thereby increase the amount of gas per unit area supplied to the center of the substrate. Therefore, a film thickness reduction at the center of the substrate in the conventional lateral flow reactor can be prevented.
Further, the lateral flow atomic layer deposition device according to the exemplary embodiment of the present invention integrally forms the gas inlet unit and the gas outlet in one body, supplies the process gas to one side of the reactor, and outputs the same through another side thereof such that the gas flow path is simplified. Therefore, recombination and decomposition of the gas can be minimized and the switching time of gases is reduced to reduce time for depositing film.
The lateral flow atomic layer deposition device according to the exemplary embodiment of the present invention can supply the gas in various ways by changing the shapes of the inlet port and the outlet port of the gas inlet unit and the gas outlet, respectively.
A one-body reactor cover having a gas inlet and a gas outlet of a lateral flow atomic layer deposition device according to an exemplary embodiment of the present invention will now be described with reference to
Referring to
A result of an experimental example of the present invention will now be described with reference to
Therefore, in the lateral flow atomic layer deposition device according to the exemplary embodiment of the present invention, the amount of gas per unit area passing through the center area during the same process time is increased compared to that passing through the edge area, so the film thickness reduction in the center of the substrate is prevented.
Referring to
The atomic layer deposition device according to the exemplary embodiment of the present invention prevents reduction of the film thickness at the center of the substrate by controlling the length of the gas flow path by introducing the gas inlet port and the gas outlet port that are integrally formed in the reactor cover.
Further, the lateral flow atomic layer deposition device according to the exemplary embodiment of the present invention eliminates the conventional gas flow control plate and simplifies the gas supply structure and the gas flow path to reduce recombination and decomposition of gases flowing along the gas path, and reduces the switching time of gases to reduce the process time, contributing to higher productivity.
While this invention has been described in connection with what is presently considered to be practical exemplary embodiments, it is to be understood that the invention is not limited to the disclosed embodiments, but, on the contrary, is intended to cover various modifications and equivalent arrangements included within the spirit and scope of the appended claims.