Method of making semiconductor package having redistribution layer

Abstract
The present invention relates to a semiconductor package and a method for making the same. The semiconductor package includes a substrate, a first passivation layer, a first metal layer, a second passivation layer, a second metal layer and a third metal layer. The substrate has a surface having at least one first pad and at least one second pad. The first passivation layer covers the surface of the substrate and exposes the first pad and the second pad. The first metal layer is formed on the first passivation layer and is electrically connected to the second pad. The second passivation layer is formed on the first metal layer and exposes the first pad and part of the first metal layer. The second metal layer is formed on the second passivation layer and is electrically connected to the first pad. The third metal layer is formed on the second passivation layer and is electrically connected to the first metal layer.
Description
BACKGROUND OF THE INVENTION

1. Field of the Invention


The present invention relates to a semiconductor package and a method for making the same, and more particularly to a semiconductor package having a redistribution layer and a method for making the same.


2. Description of the Related Art


There is a tendency of making smaller and lighter electrical products, so packages with higher intensity of pins and new packaging methods are developed. Those new packaging methods include: (1) Ball Grid Array (BGA), which uses solder balls to replace conventional pins, the solder balls being connected to a circuit board and disposed in array; (2) Flip Chip, which places an active surface of a chip downward to connect the chip and the substrate by Sn/Pb bumps; (3) Quad Flat Package (QFP). Currently, the most advanced packaging technique is redistribution layer (RDL). In conventional packaging technique, a solder joint must go through the center of a chip. However, the redistribution layer redistributes a solder joint to the periphery, two sides or any side of a chip; as a result, multi-chips can be stacked perpendicularly, crisscross, or side by side.


In the design and production of the conventional redistribution layer, the power signal and the ground signal are redistributed by long and thin traces of a single-layered layout. However, when high speed and high frequency signals are transferred, the long and thin traces of the single-layered layout cannot steadily control the characteristic impedance, so a noise of power is produced and the signal is rebounded, which is the main disadvantage.


Moreover, when the numbers and the intensity of the devices in an IC chip increase, the consumption of electricity increases. Although the redistribution layer redistributes the solder joint to the periphery, two sides or any side of the chip by the long and thin traces, it causes difficulty in heat dissipation, which increases the temperature of the chip and influences the characteristic and function of the chip. Finally, it leads to lower yield rate of the chip, which is another disadvantage.


Therefore, redistributing the solder joint of the signal input and output terminal by the conventional redistribution layer with long and thin traces has the disadvantages of high parasitic impedance, lack of voltage, and uncontrolled characteristic impedance. Moreover, the long and thin traces also increase thermal resistance, and the yield rate of the chip is reduced.


SUMMARY OF THE INVENTION

The present invention provide a semiconductor package which is able to control the characteristic impedance of a high-speed and high-frequency IC chip with a redistribution layer. The present invention provides a semiconductor package which is able to reduce the parasitic impedance and the inductance value of the redistribution layer.


The present invention provides a semiconductor package which is able to reduce the thermal resistance value produced by the redistribution layer and provides a better heat dissipation path, so as to increase the reliability of the devices in the package.


The present invention provides a method for making a semiconductor package having the above-mentioned characteristics.


The present invention is directed to a semiconductor package comprising a substrate, a first passivation layer, a first metal layer, a second passivation layer, a second metal layer and a third metal layer. The substrate has a surface having at least one first pad and at least one second pad. The first passivation layer covers the surface of the substrate and exposes the first pad and the second pad. The first metal layer is formed on the first passivation layer and is electrically connected to the second pad. The second passivation layer is formed on the first metal layer and exposes the first pad and part of the first metal layer. The second metal layer is formed on the second passivation layer and is electrically connected to the first pad. The third metal layer is formed on the second passivation layer and is electrically connected to the first metal layer.


The present invention is further directed to a method for making a semiconductor package. The method comprises the following steps: (a) providing a substrate having a surface, wherein the surface has at least one first pad and at least one second pad; (b) forming a first passivation layer on the surface of the substrate, wherein the first passivation layer covers the surface of the substrate and exposes the first pad and the second pad; (c) forming a first metal layer on the first passivation layer, wherein the first metal layer is electrically connected to the second pad; (d) forming a second passivation layer on the first metal layer, wherein the second passivation layer exposes the first pad and part of the first metal layer; (e) forming a fourth metal layer on the second passivation layer; and (f) patterning the fourth metal layer, so as to form a second metal layer and a third metal layer, wherein the second metal layer is electrically connected to the first pad, and the third metal layer is electrically connected to the first metal layer.





BRIEF DESCRIPTION OF THE DRAWINGS


FIG. 1 is a schematic view according to a method for making a semiconductor package of the present invention after a first passivation layer is formed;



FIG. 2 is a schematic view according to the method for making a semiconductor package of the present invention after a first metal layer is formed;



FIG. 3 is a schematic view according to the method for making a semiconductor package of the present invention after a second passivation layer is formed;



FIG. 4 is a schematic view according to the method for making a semiconductor package of the present invention after a second metal layer is formed;



FIG. 5 is a schematic view according to the method for making a semiconductor package of the present invention after a third passivation layer is formed; and



FIG. 6 is a schematic view of a semiconductor package formed by the method of the present invention.





DETAILED DESCRIPTION OF THE INVENTION

The semiconductor package and method for making the same of the present invention will be described by illustrating the following embodiments with reference to accompanying FIGS. 1 to 6. It should be noted that, “on” and “under” are used to illustrate the provisional position in the figures, not to limit the present invention.



FIG. 1 shows a schematic view according to a method for making a semiconductor package of the present invention after a first passivation layer is formed. As shown in FIG. 1, a substrate 1, for example a wafer, is provided. The substrate 1 has a surface 100, which has at least one first pad 10 and at least one second pad 20 thereon. A first passivation layer 101 is then formed to cover the surface 100 of the substrate 1 and expose the first pad 10 and the second pad 20. The material of the first passivation layer 101 may be but is not limited to benzo-cyclo-butence or polyimide. The first pad 10 is a signal input and output terminal, and the second pad 20 is a ground terminal.


As shown in FIG. 2, a first metal layer 201 is formed on the first passivation layer 101, and is electrically connected to the second pad 20. Moreover, the first metal layer 201 exposes and surrounds the first pad 10, and is electrically isolated from the first pad 10. The material of the first metal layer 201 is selected from the group consisting of Au, Ag, Cu and an alloy thereof.


As shown in FIG. 3, a second passivation layer 102 is then formed on the first metal layer 201, and exposes the first pad 10 and part of the first metal layer 201 which surrounds the first pad 10. The material of the second passivation layer 102 may be but is not limited to benzo-cyclo-butence or polyimide.


As shown in FIG. 4, a second metal layer 202 is then formed on the second passivation layer 102, exposes part of the second passivation layer 102, and is electrically connected to the first pad 10. Moreover, a third metal layer 203 is formed on the second passivation layer 102, is electrically connected to the first metal layer 201, and exposes part of the second passivation layer 102. The second metal layer 202 is a redistribution layer, and the third metal layer 203 is an under bump metallurgy. The material of the second metal layer 202 and the third metal layer 203 is selected from the group consisting of Au, Ag, Cu and an alloy thereof. The second metal layer 202 and the third metal layer 203 may be formed by the following steps. First, a fourth metal layer (not shown in figure) is formed on the second passivation layer 102. Part of the fourth metal layer is then removed by patterning the fourth metal layer, and the remaining part of the fourth metal layer on the second passivation layer 102 forms the second metal layer 202 and the third metal layer 203.


As shown in FIG. 5, a third passivation layer 103 is then formed on the second passivation layer 102. The third passivation layer 103 covers the exposed part of the second passivation layer 102, the second metal layer 202 and the third metal layer 203, and exposes part of the second metal layer 202 and part of the third metal layer 203. The material of the third passivation layer 103 may be but is not limited to benzo-cyclo-butence or polyimide.



FIG. 6 shows a schematic view of a semiconductor package formed by the method of the present invention. The semiconductor package is formed by disposing a Pb/Sn bump 60 on a semi-finished semiconductor package as shown in FIG. 5, and the Pb/Sn bump 60 is disposed on the exposed part of the second metal layer 202 and the exposed part of the third metal layer 203.


As described above, the present invention provides a semiconductor package which is able to control the characteristic impedance of a high-speed and high-frequency IC chip with a redistribution layer, and a method for making the same.


Moreover, the semiconductor package and a method for making the same of the present invention are able to reduce the parasitic impedance and the inductance value of the redistribution layer. In addition, the design of the present invention is able to reduce the thermal resistance value produced by the redistribution layer and provide a better heat dissipation path, so as to increase the reliability of the devices in the package.


While several embodiments of the present invention have been illustrated and described, various modifications and improvements can be made by those skilled in the art. The embodiments of the present invention are therefore described in an illustrative but not restrictive sense. It is intended that the present invention should not be limited to the particular forms as illustrated, and that all modifications which maintain the spirit and scope of the present invention are within the scope defined in the appended claims.

Claims
  • 1. Method for making a semiconductor package, comprising: (a) providing a substrate having a surface, wherein the surface has at least one first pad and at least one second pad;(b) forming a first passivation layer on the surface of the substrate, wherein the first passivation layer covers the surface of the substrate and exposes the first pad and the second pad;(c) forming a first metal layer on the first passivation layer, wherein the first metal layer is electrically connected to the second pad and has an opening to expose the first pad;(d) forming a second passivation layer on the first metal layer, wherein the second passivation layer exposes the first pad and part of the first metal layer;(e) forming a fourth metal layer on the second passivation layer; and(f) patterning the fourth metal layer, so as to form a second metal layer and a third metal layer, wherein the second metal layer is electrically connected to the first pad, and the third metal layer is electrically connected to the first metal layer.
  • 2. The method as claimed in claim 1, further comprising a step of forming a third passivation layer on the second passivation layer, wherein the third passivation layer covers the second passivation layer, the second metal layer and the third metal layer and exposes part of the second metal layer and part of the third metal layer.
  • 3. The method as claimed in claim 2, wherein the third metal layer is an under bump metallurgy.
  • 4. The method as claimed in claim 2, further comprising a step of electrically connecting a Pb/Sn bump on the exposed part of the second metal layer and the exposed part of the third metal layer.
  • 5. The method as claimed in claim 1, wherein in step (c), the first metal layer surrounds the first pad, and is electrically isolated from the first pad.
  • 6. The method as claimed in claim 1, wherein the first pad is a signal input and output terminal, and the second pad is a ground terminal.
  • 7. The method as claimed in claim 1, wherein the second metal layer is a redistribution layer.
  • 8. A method for making a semiconductor package, comprising: (a) providing a substrate having a surface, wherein the surface has at least one first pad and at least one second pad;(b) forming a first passivation layer on the surface of the substrate, wherein the first passivation layer covers the surface of the substrate and has a first opening and a second opening, the first opening of the first passivation layer exposes the first pad, and the second opening of the first passivation layer exposes the second pad;(c) forming a first metal layer on the first passivation layer, wherein the first metal layer is electrically connected to the second pad;(d) forming a second passivation layer on the first metal layer, wherein the second passivation layer has a third opening and a fourth opening, the third opening of the second passivation layer overlaps the first opening of the first passivation layer so as to expose the first pad, and the fourth opening of the second passivation layer is vertically misaligned with the second opening of the first passivation layer and exposes part of the first metal layer;(e) forming a fourth metal layer on the second passivation layer; and(f) patterning the fourth metal layer, so as to form a second metal layer and a third metal layer, wherein the second metal layer is electrically connected to the first pad, and the third metal layer is electrically connected to the first metal layer.
  • 9. The method as claimed in claim 8, further comprising a step of forming a third passivation layer on the second passivation layer, wherein the third passivation layer covers the second passivation layer, the second metal layer and the third metal layer and exposes part of the second metal layer and part of the third metal layer.
  • 10. The method as claimed in claim 9, wherein the third metal layer is an under bump metallurgy.
  • 11. The method as claimed in claim 9, further comprising a step of electrically connecting a Pb/Sn bump on the exposed part of the second metal layer and the exposed part of the third metal layer.
  • 12. The method as claimed in claim 8, wherein in step (c), the first metal layer surrounds the first pad, and is electrically isolated from the first pad.
  • 13. The method as claimed in claim 8, wherein the first pad is a signal input and output terminal, and the second pad is a ground terminal.
  • 14. The method as claimed in claim 8, wherein the second metal layer is a redistribution layer.
  • 15. A method for making a semiconductor package, comprising: (a) providing a substrate having a surface, wherein the surface has at least one first pad and at least one second pad;(b) forming a first passivation layer on the surface of the substrate, wherein the first passivation layer covers the surface of the substrate and exposes the first pad and the second pad;(c) forming a first metal layer on the first passivation layer, wherein the first metal layer is electrically connected to the second pad and has a first portion extending outside a periphery of the second pad;(d) forming a second passivation layer on the first metal layer, wherein the second passivation layer exposes the first pad and part of the first portion of the first metal layer;(e) forming a fourth metal layer on the second passivation layer; and(f) patterning the fourth metal layer, so as to form a second metal layer and a third metal layer, wherein the second metal layer directly contacts the first pad, and the third metal layer directly connects the first portion of the first metal layer.
  • 16. The method as claimed in claim 15, further comprising a step of forming a third passivation layer on the second passivation layer, wherein the third passivation layer covers the second passivation layer, the second metal layer and the third metal layer and exposes part of the second metal layer and part of the third metal layer.
  • 17. The method as claimed in claim 16, wherein the third metal layer is an under bump metallurgy, and the second metal layer is a redistribution layer.
  • 18. The method as claimed in claim 16, further comprising a step of electrically connecting a Pb/Sn bump on the exposed part of the second metal layer and the exposed part of the third metal layer.
  • 19. The method as claimed in claim 15, wherein in step (c), the first metal layer surrounds the first pad, and is electrically isolated from the first pad.
  • 20. The method as claimed in claim 15, wherein the first pad is a signal input and output terminal, and the second pad is a ground terminal.
Priority Claims (1)
Number Date Country Kind
96148502 A Dec 2007 TW national
CROSS-REFERENCE TO RELATED APPLICATIONS

This application is a divisional of U.S. patent application Ser. No. 12/241,204, filed Sep. 30, 2008, and issued as U.S. Pat. No. 7,977,384 on Jul. 12, 2011, which claims the benefit of Taiwan Patent Application No. 096148502, filed Dec. 18, 2007, each of which is incorporated by reference herein.

US Referenced Citations (5)
Number Name Date Kind
6590295 Liao et al. Jul 2003 B1
8035226 Wilcoxen et al. Oct 2011 B1
20050017355 Chou et al. Jan 2005 A1
20080079150 Simon et al. Apr 2008 A1
20090212428 Yang et al. Aug 2009 A1
Related Publications (1)
Number Date Country
20110237032 A1 Sep 2011 US
Divisions (1)
Number Date Country
Parent 12241204 Sep 2008 US
Child 13156043 US