For a more complete understanding of exemplary embodiments of the present invention and the advantages thereof, reference is now made to the following description taken in conjunction with the accompanying drawings, in which:
a shows a schematic cross-sectional view of a solid electrolyte memory device set to a first memory state;
b shows a schematic cross-sectional view of a solid electrolyte memory device set to a second memory state;
a shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
b shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
c shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
a shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
b shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
c shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
d shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
e shows a cross-sectional view of a processing state of a method of fabricating a solid electrolyte memory device according to one embodiment of the present invention;
a shows a perspective view of a memory module according to one embodiment of the present invention; and
b shows a perspective view of a memory module according to one embodiment of the present invention.
For sake of simplicity, it will be assumed in the following description that the memory device is a solid electrolyte memory device. However, it is to be understood that the embodiments discussed below are also applicable to other types of memory devices.
According to one embodiment of the present invention, a method of manufacturing a memory device includes generating a solid electrolyte layer including a first solid electrolyte layer area and a second solid electrolyte layer area, the height of the top surface of the solid electrolyte layer within the second solid electrolyte layer area being lower than the height of the top surface of the solid electrolyte layer within the first solid electrolyte layer area; generating a conductive layer above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area; planarizing the top surface of the conductive layer such that the solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area; patterning the exposed solid electrolyte layer within the first solid electrolyte layer area.
According to one embodiment of the present invention, a method of manufacturing an integrated circuit including a memory device is provided, the method including generating a solid electrolyte layer including a first solid electrolyte layer area and a second solid electrolyte layer area, the height of the top surface of the solid electrolyte layer within the second solid electrolyte layer area being lower than the height of the top surface of the solid electrolyte layer within the first solid electrolyte layer area generating a conductive layer above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area planarizing the top surface of the conductive layer such that the solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area; patterning the exposed solid electrolyte layer within the first solid electrolyte layer area.
Within the scope of the present invention, the term, a first layer is disposed “above” a second layer means that the first layer is directly arranged on the second layer, or means that at least one further layer is arranged between the first layer and the second layer.
According to one embodiment of the present invention, the portions of the solid electrolyte layer and the conductive layer located within the second solid electrolyte layer area constitute at least a part of at least one memory cell of the memory device.
According to one embodiment of the present invention, the generation of the solid electrolyte layer includes a process of patterning a solid electrolyte layer having a top surface of a uniform height such that the height of the top surface of the solid electrolyte layer within the second solid electrolyte layer area becomes lower than the height of the top surface of the solid electrolyte layer within the first solid electrolyte layer area.
According to one embodiment of the present invention, the patterning of the exposed solid electrolyte layer is carried out such that the solid electrolyte layer is completely removed within the first solid electrolyte layer area.
According to one embodiment of the present invention, the planarization of the top surface of the conductive layer is carried out using a chemical mechanical polishing process (CMP process).
According to one embodiment of the present invention, the solid electrolyte layer is a solid electrolyte layer composite structure including a first solid electrolyte layer, a second solid electrolyte layer disposed above the first solid electrolyte layer, and an intermediate layer sandwiched between the first solid electrolyte layer and the second solid electrolyte layer.
According to one embodiment of the present invention, the generation of the solid electrolyte layer includes, patterning the second solid electrolyte layer within the second solid electrolyte layer area until the top surface of the intermediate layer is exposed; patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed.
According to one embodiment of the present invention, the patterning of the exposed solid electrolyte layer within the first solid electrolyte layer includes, patterning the second solid electrolyte layer within the first solid electrolyte layer area until the top surface of the intermediate layer is exposed; patterning the exposed intermediate layer within the first solid electrolyte layer area until the top surface of the first solid electrolyte layer is exposed; patterning the first solid electrolyte layer.
According to one embodiment of the present invention, after having provided the conductive layer, a photo dissolution process and/or a thermal dissolution process is carried out driving metal ions out of the conductive layer into the solid electrolyte layer.
According to one embodiment of the present invention, the conductive layer includes an electrode layer and a contact layer disposed above the electrode layer.
According to one embodiment of the present invention, after having provided the electrode layer, a photo dissolution process and/or a thermal dissolution process is carried out driving metal ions out of the electrode layer into the solid electrolyte layer.
According to one embodiment of the present invention, the intermediate layer includes or consists of nitride or SiC.
According to one embodiment of the present invention, the electrode layer includes or consists of silver.
According to one embodiment of the present invention, the solid electrolyte layer includes or consists of chalcogenide.
According to one embodiment of the present invention, the thickness of the first solid electrolyte layer ranges from 10 nm to 100 nm or from 30 nm to 100 mn.
According to one embodiment of the present invention, the thickness of the second solid electrolyte layer ranges from 10 nm to 100 nm or from 30 nm to 100 mn.
According to one embodiment of the present invention, the thickness of the intermediate layer ranges from 10 Angstrom to 100 Angstrom.
According to one embodiment of the present invention, the thickness of the contact layer ranges from 50 nm to 300 mn.
According to one embodiment of the present invention, the thickness of the electrode layer ranges from 10 Angstrom to 100 Angstrom.
According to one embodiment of the present invention, the second solid electrolyte layer is patterned using an etching process, wherein the intermediate layer serves as an etching barrier during the etching process.
According to one embodiment of the present invention, the thickness of the first solid electrolyte layer corresponds to the target thickness of solid electrolyte layers of memory cells of the memory device.
All embodiments described above can also be applied to the embodiments described in the following.
According to one embodiment of the present invention, a method of manufacturing a memory device is provided, the method including patterning a composite structure including a first solid electrolyte layer, a second solid electrolyte layer disposed above the first solid electrolyte layer, and an intermediate layer sandwiched between the first solid electrolyte layer and the second solid electrolyte layer, the patterning of the composite structure including selectively patterning the second solid electrolyte layer within the second solid electrolyte layer area until the top surface of the intermediate layer is exposed, and selectively patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed; providing an electrode layer above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area; providing a contact layer above the electrode layer; planarizing the top surface of the contact layer such that the second solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area; patterning the composite structure within the first solid electrolyte layer area, the patterning including patterning the second solid electrolyte layer until the top surface of the intermediate layer is exposed, patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed, and patterning the first solid electrolyte layer.
According to one embodiment of the present invention, a method of manufacturing an integrated circuit including a memory device is provided, the method including patterning a composite structure including a first solid electrolyte layer, a second solid electrolyte layer disposed above the first solid electrolyte layer, and an intermediate layer sandwiched between the first solid electrolyte layer and the second solid electrolyte layer, the patterning of the composite structure including selectively patterning the second solid electrolyte layer within the second solid electrolyte layer area until the top surface of the intermediate layer is exposed, and selectively patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed; providing an electrode layer above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area; providing a contact layer above the electrode layer; planarizing the top surface of the contact layer such that the second solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area; patterning the composite structure within the first solid electrolyte layer area, the patterning including patterning the second solid electrolyte layer until the top surface of the intermediate layer is exposed, patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed, and patterning the first solid electrolyte layer.
According to one embodiment of the present invention, a memory device is provided including a memory cell, the memory cell including a memory cell solid electrolyte layer and a memory cell conductive layer disposed on or above the memory cell solid electrolyte layer, wherein the memory cell solid electrolyte layer and the memory cell conductive layer are generated as follows generating a solid electrolyte layer including a first solid electrolyte layer area and a second solid electrolyte layer area, the height of the top surface of the solid electrolyte layer within the second solid electrolyte layer area being lower than the height of the top surface of the solid electrolyte layer within the first solid electrolyte layer area; generating a conductive layer on or above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area; planarizing the top surface of the conductive layer such that the solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area; patterning the exposed solid electrolyte layer within the first solid electrolyte layer area, wherein the portions of the solid electrolyte layer and the conductive layer located within the first solid electrolyte layer area constitute the memory cell solid electrolyte layer and the memory cell conductive layer.
According to one embodiment of the present invention, an integrated circuit is provided comprising at least one memory device according to an embodiment of the present invention.
According to one embodiment of the present invention, a memory module is provided comprising at least one memory device according to an embodiment of the present invention. According to one embodiment of the present invention, the memory module is stackable.
Since the embodiments of the present invention can be applied to solid electrolyte devices like CBRAM (conductive bridging random access memory) devices, in the following description, making reference to
As shown in
In the context of this description, chalcogenide material (ion conductor) is to be understood, for example, as any compound containing oxygen, sulphur, selenium, germanium and/or tellurium. In accordance with one embodiment of the invention, the ion conducting material is, for example, a compound, which is made of a chalcogenide and at least one metal of the group I or group II of the periodic system, for example, arsenic-trisulfide-silver. Alternatively, the chalcogenide material contains germanium-sulfide (GeSx), germanium-selenide (GeSex), tungsten oxide (WOx), copper sulfide (CuSx) or the like. The ion conducting material may be a solid state electrolyte. Furthermore, the ion conducting material can be made of a chalcogenide material containing metal ions, wherein the metal ions can be made of a metal, which is selected from a group consisting of silver, copper and zinc or of a combination or an alloy of these metals.
If a voltage as indicated in
In order to determine the current memory status of a CBRAM cell, for example, a sensing current is routed through the CBRAM cell. The sensing current experiences a high resistance in case no conductive bridge 107 exists within the CBRAM cell, and experiences a low resistance in case a conductive bridge 107 exists within the CBRAM cell. A high resistance may, for example, represent “0”, whereas a low resistance represents “1”, or vice versa. The memory status detection may also be carried out using sensing voltages.
The solid electrolyte memory device 200 further comprises a second isolation layer 207 and a third isolation layer 208 arranged in this order on the first isolation layer 206. Bit lines 209 which contact first vias 202, second vias 210, a first wiring layer 211, a first plug 212, a second plug 213, and a third plug 214 are embedded into the second isolation layer 207 and the third isolation layer 208. The first plug 212, the second plug 213, and the third plug 214 are partly surrounded by interface material 215 which may be adhesive material and/or conductive material and/or insulating material. A fourth isolation layer 216, a fifth isolation layer 217, and a sixth isolation layer 218 are arranged on the third isolation layer 208 in this order. A third via 219 partially surrounded by interface material 215 (for example, tantalum or tantalum nitride (Ta/TaN)) is embedded into the composite structure formed by the fourth isolation layer 216, the fifth isolation layer 217, and the sixth isolation layer 218. Further, a solid electrolyte cell unit 221 is embedded into said composite structure. The solid electrolyte cell unit 221 comprises a fourth plug 222 functioning as bottom electrode of the solid electrolyte cell unit 221 and being partially surrounded by interface material 215, a layer of active material 223 (for example, chalcogenide material), a common top electrode layer 224 (for example, a silver layer) arranged on the active material layer 223, a common contacting layer 225 arranged on the common top electrode layer 224, and a fifth plug 241 being arranged on the common contacting layer 225 and being partially surrounded by the interface material 215. A seventh isolation layer 226 and an eighth isolation layer 227 are arranged on the sixth isolation layer 218 in this order. A second wiring layer 228 is embedded into the seventh isolation layer 226 and is partially surrounded by interface material 215. A sixth plug 229 is embedded into the eighth isolation layer 227 and is partially surrounded by interface material 215. A third wiring layer 231 is arranged on the eighth isolation layer 227 and is partially surrounded by interface material 215. The upper surface of the eighth isolation layer 227 as well as parts of the surface of the third wiring layer 231 are covered with a ninth isolation layer 232 and a tenth isolation layer 233.
The third wiring layer 231, the sixth plug 229, the second wiring layer 228, the third via 219, the second plug 213, the first plug 212, the first wiring layer 211, and some of the first vias 202 may be connected in a way that a conductive line is formed which guides electric currents between the semiconductor substrate 201 of the solid electrolyte memory device 200 and a substrate voltage/current terminal which is formed by the upper surface of the third wiring layer 231.
The fifth plug 241 and the second wiring layer 228 may be connected in a way that a conductive line is formed which guides electric currents or voltages between the common contacting layer 225 and a memory cell programming unit (not shown here) programming memory states of the memory cells or between the common contacting layer 225 and a memory cell reading unit (not shown here) determining the memory state of the memory cells. For sake of simplicity, only one fifth plug 241 is shown. However, a plurality of fifth plugs 241 may be provided, each fifth plug 241 being part of a conductive line guiding electric currents or voltages between the common contacting layer 225 and a memory cell programming unit/a memory cell reading unit. Further, the common contacting layer 225 and the common top electrode layer 224 may be patterned.
The third wiring layer 231, the sixth plug 229, the second wiring layer 228, the third via 219, the second plug 213, the first plug 212, and the first wiring layer 211 are located within a peripheral area 242 of the solid electrolyte memory device 200, whereas the fifth plug 241 and the second wiring layer 228 are located within a cell area 243 of the solid electrolyte memory device 200.
In the following description, making reference to
In a first process P1″, a solid electrolyte layer 300 comprising a first solid electrolyte layer area 301 and a second solid electrolyte layer area 302 is provided. The top surface 303 of the solid electrolyte layer 300 has a first height H1 within the first solid electrolyte layer area 301 and a second height H2 within the second solid electrolyte layer area 302. As a consequence, the top surface 303 shows a step at the border between the first solid electrolyte layer area 301 and the second solid electrolyte layer area 302.
In a second process P2″, a conductive layer 304 is provided on the top surface 303 of the solid electrolyte layer 300. The conductive layer 304 has a uniform thickness. Therefore, the top surface of the conductive layer 304 also shows a step near the border between the first solid electrolyte layer area 301 and the second solid electrolyte layer area 302.
In a third process P3″, the top surface 305 of the conductive layer 304 is planarized. The planarization process is carried out such that the solid electrolyte layer 300 is exposed within the first solid electrolyte layer area 301, however is covered by the conductive layer 304 within the second solid electrolyte layer area 302. In this way, the conductive layer 304 is completely removed within the first solid electrolyte layer area 301.
In a further process (not shown), the solid electrolyte layer 300 may be patterned within the first solid electrolyte layer area 301, i.e. within the area where the top surface of the solid electrolyte layer 300 is not covered by the conductive layer 304. This patterning process may, for example, be carried out using etching substances which chemically only react with the solid electrolyte layer 300, but not with the conductive layer 304.
In a first process P1, a solid electrolyte layer is generated including a first solid electrolyte layer area and a second solid electrolyte layer area, the height of the top surface of the solid electrolyte layer within the second solid electrolyte layer area being lower than the height of the top surface of the solid electrolyte layer within the first solid electrolyte layer area.
In a second process P2, a conductive layer is generated above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area.
In a third process P3, the top surface of the conductive layer is planarized such that the solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area.
In a fourth process P4, the exposed solid electrolyte layer is patterned within the first solid electrolyte layer area.
In a first process P1′, a composite structure is patterned including a first solid electrolyte layer, a second solid electrolyte layer disposed above the first solid electrolyte layer and an intermediate layer sandwiched between the first solid electrolyte layer and the second solid electrolyte layer. The patterning of the composite structure includes: a) patterning the second solid electrolyte layer within the second solid electrolyte layer area until the top surface of the intermediate layer is exposed, and b) patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed.
In a second process P2′, an electrode layer is provided above the top surfaces of the first solid electrolyte layer area and the second solid electrolyte layer area.
In a third process P3′, a contact layer is provided above the electrode layer.
In a fourth process P4′, the top surface of the contact layer is planarized such that the second solid electrolyte layer is exposed within the first solid electrolyte layer area, however is covered by the conductive layer within the second solid electrolyte layer area.
In a fifth process P5′, the composite structure is patterned within the first solid electrolyte layer area, wherein the patterning includes: a) patterning the second solid electrolyte layer until the top surface of the intermediate layer is exposed, b) patterning the exposed intermediate layer until the top surface of the first solid electrolyte layer is exposed, and c) patterning the first solid electrolyte layer.
In the following description, making reference to
a shows a first processing state A in which a first solid electrolyte layer 601, a second solid electrolyte layer 602, and an intermediate layer 603 sandwiched between the first solid electrolyte layer 601 and the second solid electrolyte layer 604 have been provided on an isolation layer 604 in this order. The first solid electrolyte layer 601 and the second solid electrolyte layer 602 may, for example, comprise or consist of chalcogenide. The thickness of the first solid electrolyte layer 601 may, for example, range from 10 nm to 100 nm or from 30 nm to 100 nm. In the same way, the thickness of the second solid electrolyte layer 602 may, for example, range from 10 nm to 100 nm or from 30 nm to 100 nm. The intermediate layer 603 may, for example, comprise or consist of nitride or SiC. The thickness of the intermediate layer 603 may, for example, range from 10 Angstrom to 100 Angstrom.
In a second processing state B shown in
In a third processing state C shown in
In a fourth processing state D shown in
In a fifth processing state E shown in
As shown in
As shown in
According to one embodiment of the present invention, the reliability of integrated circuits having a memory device is improved.
In the following description, further features of the present invention will be explained.
Under current processing, the CBRAM process includes a silver layer on top of the chalcogenide layer. The way to pattern the chalcogenide is done by an etching process including the etching of silver. The actual etching process is carried out using Ar plasma, a lot of residue is still present after the etching process; the etching process is not selective, and a huge pattern factor issue exists.
According to one embodiment of the present invention, a new solution is provided in order to pattern the chalcogenide, a deposition of a thicker chalcogenide followed by the inverse patterning of the chalcogenide; deposition of silver and the cap layer (also photo dissolution) and the contacting layer like tungsten; performing a CMP process stopping on the contacting layer; and finally selectively etching the chalcogenide: no silver etch is required. The actual process is a process using the etch integration scheme.
According to one embodiment of the present invention, a new PL Level integration scheme is provided. The new integration scheme uses, thicker chalcogenide with etch barrier (sandwich chalcogenide, barrier, chalcogenide); inverse litho-etch patterning; Silver+Cap layer deposition+Photo dissolution; contact layer deposition; CMP layer planarization; selective chalcogenide etch
According to one embodiment of the present invention, a new PL Level integration scheme is provided. The new integration scheme uses, Litho+Etch to the barrier; selective etch of the barrier; chalcogenide surface clean; silver deposition+Cap; photo dissolution; contact metal deposition (like W); CMP to contact metal; selective chalcogenide etch stop on barrier (Nitride or SiC); provide uniformity; barrier etch; selective chalcogenide etch stop on oxide.
As used herein, the terms “connected” and “coupled” are intended to include both direct and indirect connection and coupling, respectively.
The foregoing description has been presented for purposes of illustration and description. It is not intended to be exhaustive or to limit the invention to the precise form disclosed, and obviously many modifications and variations are possible in light of the disclosed teaching. The described embodiments were chosen in order to best explain the principles of the invention and its practical application to thereby enable others skilled in the art to best utilize the invention in various embodiments and with various modifications as are suited to the particular use contemplated. It is intended that the scope of the invention be defined solely by the claims appended hereto.
Number | Name | Date | Kind |
---|---|---|---|
6815818 | Moore et al. | Nov 2004 | B2 |
6838692 | Lung | Jan 2005 | B1 |
7115504 | Moore et al. | Oct 2006 | B2 |
7115992 | Moore et al. | Oct 2006 | B2 |
7151273 | Campbell et al. | Dec 2006 | B2 |
7167387 | Sugita et al. | Jan 2007 | B2 |
7332401 | Moore et al. | Feb 2008 | B2 |
7368314 | Ufert | May 2008 | B2 |
7374174 | Liu et al. | May 2008 | B2 |
7599211 | Blanchard | Oct 2009 | B2 |
7646007 | Campbell et al. | Jan 2010 | B2 |
7658773 | Pinnow | Feb 2010 | B2 |
7723713 | Campbell et al. | May 2010 | B2 |
20030096497 | Moore et al. | May 2003 | A1 |
20030173558 | Campbell | Sep 2003 | A1 |
20040149980 | Campbell | Aug 2004 | A1 |
20040232551 | Moore et al. | Nov 2004 | A1 |
20040238958 | Moore et al. | Dec 2004 | A1 |
20050167699 | Sugita et al. | Aug 2005 | A1 |
20060139989 | Gruning Von Schwerin et al. | Jun 2006 | A1 |
20060164880 | Sakamoto et al. | Jul 2006 | A1 |
20060199377 | Ufert | Sep 2006 | A1 |
20060279328 | Kozicki et al. | Dec 2006 | A1 |
20080029842 | Symanczyk | Feb 2008 | A1 |
20080248380 | Blanchard | Oct 2008 | A1 |
20080253164 | Blanchard | Oct 2008 | A1 |
20080253165 | Blanchard | Oct 2008 | A1 |
20080253168 | Blanchard et al. | Oct 2008 | A1 |
20080304307 | Gopalakrishnan | Dec 2008 | A1 |
20100259960 | Samachisa | Oct 2010 | A1 |
20100259961 | Fasoli et al. | Oct 2010 | A1 |
20100259962 | Yan et al. | Oct 2010 | A1 |
Number | Date | Country |
---|---|---|
10 2004 061 548 | Jun 2006 | DE |
10 2005 005 325 | Aug 2006 | DE |
1 780 728 | May 2007 | EP |
WO 2005041303 | May 2005 | WO |
Number | Date | Country | |
---|---|---|---|