Embodiments relate to the field of etching processes for semiconductor manufacturing and, in particular, to systems and methods for providing real time etch rate monitoring in radical only etching processes.
In semiconductor etching processes, it is often difficult to monitor the etch rate in real time. As such, etch rates can typically only be determined by calculating the difference between a starting thickness of a film and an ending thickness of the film and dividing the difference by the total processing time. However, it is to be appreciated that monitoring the etch rate in real time provides additional information that may be used to tune etching processes so that they are precise and have a higher degree of repeatability, among other advantages.
Some solutions to provide real time etch rate monitoring have been developed. For example, optical emission spectroscopy (OES) and absorption spectroscopy are solutions that have been used in traditional plasma etching chambers. In OES, the intensity of the optical emission from the plasma may be correlated to the etch rate. In absorption spectroscopy a line of sight path through the process volume is needed. However, a line of sight through the process volume is often not available in high volume manufacturing equipment.
Embodiments include a real time etch rate sensor and methods of for using a real time etch rate sensor. In an embodiment, the real time etch rate sensor includes a resonant system and a conductive housing. The resonant system may include a resonating body, a first electrode formed over a first surface of the resonating body, a second electrode formed over a second surface of the resonating body, and a sacrificial layer formed over the first electrode. In an embodiment, at least a portion of the first electrode is not covered by the sacrificial layer. In an embodiment, the conductive housing may secure the resonant system. Additionally, the conductive housing contacts the first electrode, and at least a portion of an interior edge of the conductive housing may be spaced away from the sacrificial layer.
Additional embodiments may include a radical only etching process tool. In an embodiment, the radical only etching process tool may include a remote plasma chamber and a main processing chamber coupled to the remote plasma chamber. In an embodiment, the main processing chamber include an upper portion and a lower portion that is separated from the upper portion by an ion filter, and a pump liner formed around a pedestal in the lower portion. In an embodiment, the radical only etching process tool may also include a real time etch rate sensor located in the lower portion of the main processing chamber. In an embodiment, the real time etch rate sensor includes a resonant system and a conductive housing. The resonant system may include a resonating body, a first electrode formed over a first surface of the resonating body, a second electrode formed over a second surface of the resonating body, and a sacrificial layer formed over the first electrode. In an embodiment, at least a portion of the first electrode is not covered by the sacrificial layer. In an embodiment, the conductive housing may secure the resonant system. Additionally, the conductive housing contacts the first electrode, and at least a portion of an interior edge of the conductive housing may be spaced away from the sacrificial layer.
Additional embodiments may include methods for etching a substrate with a closed loop process recipe. In an embodiment, the method may include executing the process recipe on a substrate in a processing chamber. The process recipe may include one or more process parameters and an endpoint criterion that is determinable from outputs obtained from a real time etch rate sensor located in the processing chamber. The method may then continue by determining whether the endpoint criterion is satisfied by analyzing one or more outputs from the real time etch rate sensor. Embodiments may then include terminating the process recipe once the endpoint criterion is satisfied. In some embodiments, the endpoint criterion is a total thickness of material removed, and the one or more outputs from the real time etch rate sensor that are used to determine if the endpoint criterion is satisfied may be a resonance frequency of the real time etch rate sensor prior to executing the process recipe and a present resonance frequency of the real time etch rate sensor after the process recipe has been initiated.
Systems and methods for using a sensor for real time etch rate monitoring in a radical only etching process are described in accordance with various embodiments. In the following description, numerous specific details are set forth in order to provide a thorough understanding of embodiments. It will be apparent to one skilled in the art that embodiments may be practiced without these specific details. In other instances, well-known aspects are not described in detail in order to not unnecessarily obscure embodiments. Furthermore, it is to be understood that the various embodiments shown in the accompanying drawings are illustrative representations and are not necessarily drawn to scale.
As noted above, real time etch rate monitoring provides information that may be used to improve various process outcomes of the etching process. While OES and absorption spectroscopy have been used in plasma etching operations, they are significantly limited in radical only etching processes. For example, in a radical only etching process OES is not feasible, because there is not a significant optical emission from the radical species in the process volume where the substrate is etched. In absorption spectroscopy, in addition to line of sight requirements described above, the absorption of light by many radical species used for etching is strongest in the deep ultra violet (UV) frequencies. Accordingly, the optics needed for measurements are complex and expensive. Furthermore, the signal to noise ratio in absorption spectroscopy is poor because there are relatively few radicals compared to background parent molecules.
As used herein, a radical only etching process is an etching process that relies substantially on radical species to remove a material.
According to an embodiment, the ion filter 122 may prevent ions 124 from passing to the lower region 118 of the main processing chamber 116, while at the same time allowing the radical species 126 to pass through to the lower region 118 of the main processing chamber 116. For example, in the upper region 117 the ratio of radical species 126 to ions 124 may be approximately 1:1, and in the lower region 118 the ratio of radical species 126 to ions 124 may be approximately 25,000:1 or greater. In some embodiments, the ratio of radical species 126 to ions 124 may be approximately 100,000:1 or greater. Due to the high ratio of radicals 126 to ions 124, etching processes using such a processing tool 100 may be considered a radical only etching process. The radical species 126 may then interact with a surface of a substrate 105 positioned on a pedestal 106. In an embodiment, a pump liner 108 may be formed around the perimeter of the pedestal 106 in order to direct the flow of radicals 126 towards the substrate 105. It is to be appreciated that radical only etching process tool 100 illustrated in
Since OES and absorption spectroscopy are not viable solutions for real time etch rate monitoring in such radical only etching processes, embodiments described herein include a sensor that uses a resonant system for etch rate monitoring. A resonant system measures a change in the resonance frequency of a resonating body. As the mass of the resonant system changes, the resonance frequency of the resonating body changes monotonically. When such a sensor is used to monitor the etch rate in a radical only etching process, the resonant system may include a sacrificial film that is formed over one face of the resonating body and is exposed to the radicals in the processing tool 100. The radicals etch away the sacrificial film, and the overall mass of the resonant system decreases. The decrease in mass of the resonant system causes an increase in the resonance frequency of the resonating body, which is measured in real time, and the rate of change of resonance frequency is converted to a rate of change of mass of the resonant system. The rate of change of mass of the resonant system may then be converted to a rate of change of thickness since the density of the film material is known.
Sensors that use resonant systems have been used in the past to provide real time deposition rates for deposition processes (e.g., evaporation, sputtering, and the like). However, previous etching solutions were not able to utilize sensors that use resonant systems for various reasons. One reason is that previous etching processes (e.g., reactive ion etching (RIE)) are not purely a material removal process. For example, as a material is being removed, additional byproducts may redeposit onto the substrate. For example, in a silicon etch with RIE a polymer may be redeposited onto the surfaces. This polymer improves anisotropic etching, but also adds to the mass of the substrate. Accordingly, if a sensor with a resonant system were used in such an etching process, the total mass of the film removed could not be accurately determined because there would also be an increase in mass that is attributed to the polymer redeposition. Additionally, the presence of the ions in the plasma and the RF power produce significant interference with the signal from the sensor. As such, a reliable reading with a suitable signal to noise ratio is much more difficult to obtain compared to the process environment in a radical only etching process.
Referring now to
The resonating body 262 may be a material that changes resonant frequency as the mass of the resonant system 261 changes. In an embodiment, the resonating body 262 may be a piezoelectric material. For example, the resonating body 262 may be quartz, sapphire, semiconducting materials, such as silicon, germanium, or other III-V semiconductor materials, lead zirconate titanate (PZT), or the like.
In an embodiment, the resonant system 261 may include a first electrode 264 formed on a first surface of the resonating body 262 and a second electrode 265 formed on a second surface of the resonating body 262 that is opposite from the first surface. The first electrode 264 and the second electrode 265 may be any suitable conductive material. In one embodiment, the first and second electrodes 264, 265 may be aluminum, or the like. In the illustrated embodiment, the first and second electrodes 264, 265 do not cover the entire surface of the resonating body 262, but it is to be appreciated that embodiments are not limited to such configurations. For example, the first and second electrodes 264, 265 may cover the entire surface of the resonating body 262 in some embodiments. Additionally, embodiments may include first and second electrodes 264, 265 that have different surface areas. For example, the second electrode 265 may have a smaller surface area than the first electrode 264. In yet another embodiment, the surface areas of the first and second electrodes 264, 265 may be substantially the same.
In an embodiment, the resonant system 261 may include a sacrificial layer 270 formed on a surface of the first electrode 264. The addition of the sacrificial layer 270 changes the mass of the resonant system 261 and, therefore, alters the resonance frequency of the resonating body 262. Accordingly, as the thickness of the sacrificial layer 270 is reduced during an etching process, the resonance frequency of the resonating body 262 changes monotonically, as described above. In an embodiment, the sacrificial film 270 is the same material that is to be etched with a radical only etching process. For example, the sacrificial film 270 may be a dielectric material, a semiconductor material, or a metallic material.
The sacrificial layer 270 may be formed with a known thickness T. In an embodiment, the thickness T of the sacrificial layer 270 may be greater than the thickness of the material that will subsequently be etched away from a substrate being processed. Since etching is a subtractive process, increasing the thickness T of the sacrificial layer 270 increases the lifespan of the sensor 250 before the sensor 250 needs to be replaced or refurbished. For example, the thickness T of the sacrificial layer 270 may be sufficient to run a given etching process recipe multiple times without needing to replace the sensor 250. In an embodiment, the thickness T of the sacrificial layer 270 may be chosen to allow for a process recipe to be run ten or more times before the sacrificial layer 270 is completely removed. Additional embodiments may allow for a process recipe to be run one hundred or more times before the sacrificial layer 270 is completely removed. Additional embodiments may allow for a process recipe to be run one thousand or more times before the sacrificial layer 270 is completely removed. In some embodiments, the sacrificial layer may have a thickness T that allows for a process recipe to be run ten thousand times before the sacrificial layer 270 is completely removed.
In an embodiment, the sacrificial layer 270 is formed over a portion of the first electrode 264 such that at least a portion of the first electrode 264 remains exposed. At least a portion of the first electrode is exposed in order to provide a location where an electrical contact to the first electrode 264 may be made. For example, the sacrificial layer 270 may be formed in the center of the first electrode 264, leaving an exposed portion of the first electrode 264 around the periphery of the sacrificial layer 270.
In an embodiment, the resonant system 261 may be secured by a housing 266. In an embodiment, the housing 266 may be a conductive material. In an embodiment, the housing 266 may provide an electrical connection between a frequency bridge 267 and the first electrode 264. In an embodiment, the second electrode 265 may be electrically coupled to the frequency bridge 267. In some embodiments, the housing 266 may be grounded so that the first electrode 264 is held at ground potential.
Referring now to
Since the first electrode 264 is exposed to the radicals in the radical only etching process, embodiments include a first electrode 264 that is formed with a material that is substantially resistant to the radical only etching process used to etch the sacrificial layer 270. Otherwise, the first electrode 264 may be etched along with the sacrificial layer 270, and several problems would arise. One such problem would be that the change in mass of the resonant system 261 would be the sum of the material loss of the first electrode 264 and the material loss of the sacrificial layer 270. As such, the change in resonance frequency of the resonating body 262 would not correspond to the etch rate of the sacrificial layer 270 only. Additionally, removal of the first electrode 264 and/or the housing 266 by the radical only etching process reduces the useable service life of the sensor 250.
In the illustrated embodiment, the sensor 250 is shown having resonant system 261 that includes a single sacrificial layer 270. However, embodiments are not limited to such configurations. For example, multiple sacrificial layers 2701-270n may be formed over the first electrode 264. In such embodiments, so long as each of the sacrificial layers have a high etch selectively with respect to each other, a single sensor 250 may be used to provide real time etch rates for several different etching recipes. For example, a first etch of a silicon oxide layer may be monitored and then a second etch of a silicon layer may be monitored without needing to change the QCM 250. Some exemplary embodiments that include multiple sacrificial layers 2701-270n are shown in the plan view illustrations in
In the embodiment illustrated in
Additional embodiments include a plurality of sacrificial layers 2701-270n that are formed in patterns over the surface of the first electrode 264 other than concentric rings. For example, in
Referring now to
In an additional embodiment illustrated in
For example, in some embodiments it may not be necessary to provide real time etch rate monitoring for every substrate that is processed in the processing tool 300 (e.g., the real time etch rate may only be monitored for a single substrate in each lot of substrates, the real time etch rate may be monitored for every second, third, fourth, fifth, etc., substrate, or any other desired sampling plan). As such, embodiments include retracting the sensor 250 into the antechamber 386 whenever active etch rate monitoring is not needed in order to extend the useable service life of the sensor 250. Since the antechamber 386 is able to be purged and pumped down to the processing pressure (i.e., the antechamber 386 may function similar to a load lock), the main processing chamber does not need to be depressurized between uses of the sensor 250. Furthermore, during an in situ chamber cleaning operation, the sensor 250 may be protected by being retracted into the antechamber 386. As such, a processing operation that may otherwise substantially reduce the useable service life of the sensor 250 due to an aggressive etching chemistry may be implemented without damaging the sensor 250.
In embodiments that include an antechamber 386 and gate valve 385, the sensor 250 may also be replaced without needing to depressurize and/or open the main processing chamber. Instead, the antechamber 386 may be depressurized and opened to retrieve the used sensor 250 and insert a replacement sensor 250. Since the antechamber 386 is smaller than the main processing chamber, the time needed to pump the antechamber 386 back down to the processing pressure is reduced. Furthermore, the main processing chamber does not need to be opened, and there is no need to season the main processing chamber after the sensor 250 is replaced.
As noted above, the ability to monitor etch rates in real time provides several advantages that improve various processing outcomes used during the processing of a single substrate or a plurality of substrates. For example, in some embodiments real time etch rate monitoring may allow for closed loop process control that allows for an etching process recipe to be dependent on the actual thickness of material removed. In another embodiment, chamber matching between multiple processing tools executing a single processing recipe may be implemented when real time etch rate monitoring is enabled. Additional embodiments may allow for refining an etching process recipe as multiple substrates are processed by using substrate to substrate feedforward control. Further embodiments may allow for chamber health monitoring that allows for more accurate determination of when process tool maintenance is needed.
In a particular embodiment, a sensor 250 substantially similar to those described above may be used to enable etching process recipes that are implemented with closed loop process control. Previously, when real time etch rate monitoring is not able to be implemented, the process recipe relies on a preset processing duration. Relying on a preset duration may be a problem because the conditions in the processing chamber may vary between substrates (e.g., due to variations in chamber conditions, inconsistent flow of radicals into the lower region, inconsistencies in previous processing operations on the substrates, etc.). However, embodiments that include a sensor 250, such as those described herein, provide the ability to implement closed loop process control that is not time dependent. Instead, the endpoint of the processing recipe may be determined by the actual thickness of material that is removed. For example, if the processing recipe is designed to remove 30 nm of material thickness, then the processing recipe may be terminated once the sensor 250 produces outputs that indicate 30 nm of material thickness has been removed from the substrate instead of approximating the removal of material from the substrate based on time. An exemplary process recipe that uses closed loop process control is shown in process flow chart 490 illustrated in
Starting with the processing operation 491, embodiments may include executing a radical only etching process recipe. In an embodiment, the processing recipe may include any number of processing parameters that are to be used in the etching process. For example, the processing recipe may include process parameters, such as the desired substrate temperature, the flow rate of one or more processing gasses, the pressure in the processing chamber, or the like. Additionally, the processing recipe may include one or more endpoint criteria. In a particular embodiment, one endpoint criterion may be a parameter that is determinable from outputs obtained from the sensor 250. For example, the endpoint criterion may be a total thickness of material removed from the substrate, which may be determined by the change in resonance frequency of the resonating body 262, as is described above.
Referring now to processing operation 492, embodiments may continue by analyzing the outputs obtained from the sensor 250 to determine if the one or more endpoint criteria are satisfied. For example, the sensor 250 may determine if the desired thickness of material has been removed from the substrate by comparing an initial resonance frequency of the resonating body 262 (prior to the initiation of the processing recipe) to the present resonance frequency of the resonating body 262. When the desired endpoint criterion is not satisfied, the process 490 may loop back to processing operation 491 and the processing recipe continues to be executed. In an embodiment, processing operation 492 may be implemented substantially continuously or at predetermined intervals (e.g., every 5 second or less, every 1 second or less, every 0.01 second or less, or any other desired interval). According to an embodiment, once the desired endpoint criteria has been satisfied, the process may continue to processing operation 493 and the processing recipe may be terminated.
In an additional embodiment, the sensor 250 may be utilized to provide chamber matching. Chamber matching allows for multiple processing tools to process a plurality of substrates in parallel. In properly matched chambers, the process outcome of each substrate is substantially the same even when they are processed in different chambers. Accordingly, the differences between different lots or batches of substrates may be minimized and process uniformity is improved. For example, when each processing tool utilizes a sensor 250 to implement a closed loop processing recipe similar to the processing described above with respect to
According to an additional embodiment, real time etch rate monitoring with a sensor 250 may also allow for substrate to substrate feedforward control of a processing recipe. Such an embodiment may be particularly beneficial because real time etch rate monitoring allows for the processing recipe to be modified after each substrate is processed. Therefore, even as processing conditions within the processing tool change (e.g., due to chamber cleanliness, or the like), a uniform process outcome may still be obtained. An example of a process for using substrate to substrate feedforward control of a processing recipe is illustrated in process flow 590 in
In an embodiment, the process may begin with processing operation 591 by executing a processing recipe on a first substrate in a processing chamber. In an embodiment, the processing recipe is a recipe for a radical only etching process. In an embodiment, the processing recipe may include any number of processing parameters that are to be used in the etching process. For example, the processing recipe may include processing parameters, such as the desired substrate temperature, the flow rate of one or more processing gasses, the pressure in the processing chamber, or the like. In an embodiment, the process recipe may include one or more endpoint criteria. In a particular embodiment, one endpoint criterion may be a parameter that is determinable from outputs obtained from the sensor 250. For example, the endpoint criterion may be a total thickness of material removed, which may be determined by the change in resonance frequency of the resonating body 262, as is described above.
In an embodiment, the process flow advances to processing operation 592 where the outputs of the sensor 250 are analyzed to determine whether the endpoint criterion has been satisfied. If the endpoint criterion has not been satisfied, the process may loop back to operation 591, as shown. When the endpoint criterion has been satisfied, the procedure may advance to processing operation 593 and the process recipe is terminated. Thereafter, the procedure may advance to processing operation 594 where data from the processing of the first substrate is fed forward and used to modify the processing recipe for use on a second substrate. In an embodiment, the processing recipe may be modified by changing one or more of the processing parameters of the process recipe. For example, if the endpoint criterion took longer than expected to reach during the execution of the process recipe, then one or more of the processing parameters of the processing recipe may be modified to decrease the time needed to reach the endpoint criteria (e.g., by increasing the substrate temperature, increasing the flow rate of the processing gasses, etc.). Therefore, embodiments may include using feed forward information from a processing recipe executed on a first substrate in order to modify the process recipe for use on a second substrate. As such, the process recipe may be refined to allow for a desired outcome to be obtained in a more efficient manner.
Furthermore, process flow 590 may be extended to allow for process chamber health monitoring. Particularly, embodiments may include the additional operation of comparing the modified process recipe with the original process recipe to determine if there is a significant enough variance such that chamber maintenance is needed, as illustrated in processing operation 595. For example, comparing the modified process recipe with the original process recipe may include calculating the differences between one or more of the processing parameters in the modified process recipe and the original process recipe. In an embodiment, the chamber maintenance may include any adjustment to the chamber conditions, such as a chamber clean or replacement and/or refurbishment of one or more components that have been determined to be at the end of their service life.
In an embodiment, a significant variation that indicates that a chamber clean is needed may be when the difference of one or more of the process parameters in the modified process recipe and the original process recipe exceeds a predetermined threshold value. In an embodiment, the predetermined threshold value may be a maximum percentage change in a given process parameter. For example, the predetermined threshold value may be a 25% change or greater in a given process parameter. In an embodiment, each process parameter may have a different predetermined threshold value. For example, the predetermined threshold value for the percentage change in the flow rate of a processing gas may be larger than the predetermined threshold value for the percentage change in the temperature of the substrate. In an additional embodiment, the predetermined threshold value may be a maximum or minimum value for a given processing parameter. For example, the predetermined threshold value for the substrate temperature may be a maximum temperature. In yet another embodiment, the type of predetermined threshold value may be dependent on the process parameter. For example, one or more process parameters in a processing recipe may have a predetermined threshold value that is given as a maximum percentage change of the process parameter and other process parameters in the processing recipe may have a predetermined threshold value that is given as a maximum and/or minimum value.
Referring now to
Computer system 660 may include a computer program product, or software 622, having a non-transitory machine-readable medium having stored thereon instructions, which may be used to program computer system 660 (or other electronic devices) to perform a process according to embodiments. A machine-readable medium includes any mechanism for storing or transmitting information in a form readable by a machine (e.g., a computer). For example, a machine-readable (e.g., computer-readable) medium includes a machine (e.g., a computer) readable storage medium (e.g., read only memory (“ROM”), random access memory (“RAM”), magnetic disk storage media, optical storage media, flash memory devices, etc.), a machine (e.g., computer) readable transmission medium (electrical, optical, acoustical or other form of propagated signals (e.g., infrared signals, digital signals, etc.)), etc.
In an embodiment, computer system 660 includes a system processor 602, a main memory 604 (e.g., read-only memory (ROM), flash memory, dynamic random access memory (DRAM) such as synchronous DRAM (SDRAM) or Rambus DRAM (RDRAM), etc.), a static memory 606 (e.g., flash memory, static random access memory (SRAM), etc.), and a secondary memory 618 (e.g., a data storage device), which communicate with each other via a bus 630.
System processor 602 represents one or more general-purpose processing devices such as a microsystem processor, central processing unit, or the like. More particularly, the system processor may be a complex instruction set computing (CISC) microsystem processor, reduced instruction set computing (RISC) microsystem processor, very long instruction word (VLIW) microsystem processor, a system processor implementing other instruction sets, or system processors implementing a combination of instruction sets. System processor 602 may also be one or more special-purpose processing devices such as an application specific integrated circuit (ASIC), a field programmable gate array (FPGA), a digital signal system processor (DSP), network system processor, or the like. System processor 602 is configured to execute the processing logic 626 for performing the operations described herein.
The computer system 660 may further include a system network interface device 608 for communicating with other devices or machines. The computer system 660 may also include a video display unit 610 (e.g., a liquid crystal display (LCD), a light emitting diode display (LED), or a cathode ray tube (CRT)), an alphanumeric input device 612 (e.g., a keyboard), a cursor control device 614 (e.g., a mouse), and a signal generation device 616 (e.g., a speaker).
The secondary memory 618 may include a machine-accessible storage medium 631 (or more specifically a computer-readable storage medium) on which is stored one or more sets of instructions (e.g., software 622) embodying any one or more of the methodologies or functions described herein. The software 622 may also reside, completely or at least partially, within the main memory 604 and/or within the system processor 602 during execution thereof by the computer system 660, the main memory 604 and the system processor 602 also constituting machine-readable storage media. The software 622 may further be transmitted or received over a network 620 via the system network interface device 608.
While the machine-accessible storage medium 631 is shown in an exemplary embodiment to be a single medium, the term “machine-readable storage medium” should be taken to include a single medium or multiple media (e.g., a centralized or distributed database, and/or associated caches and servers) that store the one or more sets of instructions. The term “machine-readable storage medium” shall also be taken to include any medium that is capable of storing or encoding a set of instructions for execution by the machine and that cause the machine to perform any one or more of the methodologies. The term “machine-readable storage medium” shall accordingly be taken to include, but not be limited to, solid-state memories, and optical and magnetic media.
In the foregoing specification, specific exemplary embodiments have been described. It will be evident that various modifications may be made thereto without departing from the scope of the following claims. The specification and drawings are, accordingly, to be regarded in an illustrative sense rather than a restrictive sense.
This application is a continuation of U.S. patent application Ser. No. 15/955,375, filed on Apr. 17, 2018, now U.S. Pat. No. 10,790,175, which is a continuation of U.S. patent application Ser. No. 15/351,437, filed on Nov. 14, 2016, now U.S. Pat. No. 9,978,621, issued May 22, 2018, the entire contents of which are hereby incorporated by reference herein.
| Number | Name | Date | Kind |
|---|---|---|---|
| 5282925 | Jeng et al. | Feb 1994 | A |
| 5665166 | Deguchi et al. | Sep 1997 | A |
| 6654659 | Lyons et al. | Nov 2003 | B1 |
| 7052622 | Chinn et al. | May 2006 | B2 |
| 7398671 | Brederlow et al. | Jul 2008 | B2 |
| 8575820 | Shirakawa | Nov 2013 | B2 |
| 20050039852 | Roche et al. | Feb 2005 | A1 |
| 20060211154 | Buehlmann | Sep 2006 | A1 |
| 20060263576 | Hirose | Nov 2006 | A1 |
| 20060283249 | Liu | Dec 2006 | A1 |
| 20070045228 | Kubota | Mar 2007 | A1 |
| 20070068456 | Grimbergen et al. | Mar 2007 | A1 |
| 20070074562 | Liu | Apr 2007 | A1 |
| 20070080611 | Yamada | Apr 2007 | A1 |
| 20070212807 | Yamada et al. | Sep 2007 | A1 |
| 20080216956 | Nakamoto et al. | Sep 2008 | A1 |
| 20090001848 | Umeda | Jan 2009 | A1 |
| 20090133470 | Whalen | May 2009 | A1 |
| 20100227420 | Banna et al. | Sep 2010 | A1 |
| 20100258796 | Horio et al. | Oct 2010 | A1 |
| 20100270262 | Hanawa et al. | Oct 2010 | A1 |
| 20100327994 | Choy | Dec 2010 | A1 |
| 20120161902 | Feng | Jun 2012 | A1 |
| 20120248941 | Shirakawa | Oct 2012 | A1 |
| 20130127300 | Umeda | May 2013 | A1 |
| 20140035440 | Aida | Feb 2014 | A1 |
| 20150041867 | Han | Feb 2015 | A1 |
| 20150380218 | Tan et al. | Dec 2015 | A1 |
| 20160099705 | Matsuda | Apr 2016 | A1 |
| Number | Date | Country |
|---|---|---|
| 1416247 | May 2004 | EP |
| S6355535 | Apr 1988 | JP |
| H02-248042 | Oct 1990 | JP |
| 2012-156261 | Aug 2012 | JP |
| 2016-153757 | Aug 2016 | JP |
| WO 0003421 | Jan 2000 | WO |
| Entry |
|---|
| Michael D. Baker, et al.: “A Novel in Situ Monitoring Technique for Reactive Ion Etching Using a Surface Micromachined Sensor.” IEEE Transactions on Semiconductor Manufacturing, IEEE Service Center, Piscataway, NJ, US, vol. 11, No. 2, May 1, 1998 (May 1, 1998). |
| Bryan G. Morris, et al.: “Design and Development of an Integrated MEMS Sensor for Real Time Control of Plasma Etching.” Technical Proceedings on the 2004 NSTI Nanotechnology Conference and Trade Show, Mar. 7, 2004, pp. 418-421. |
| Non-Final Office Action from U.S. Appl. No. 15/351,437, filed Nov. 14, 2016 dated Aug. 3, 2017, 18 pgs. |
| International Search Report and Written Opinion from PCT/US2017-056786 dated Feb. 2, 2018, 14 pgs. |
| International Preliminary Report on Patentability from PCT/US2017/056786 dated May 23, 2019, 11 pgs. |
| Non-Final Office Action from U.S. Appl. No. 15/955,375 dated Oct. 2, 2019, 12 pgs. |
| Final Office Action from U.S. Appl. No. 15/955,375 dated Jan. 16, 2020, 12 pgs. |
| Extended European Search Report for EP17870524 dated May 7, 2020, 11 pgs. |
| Preliminary Rejection from Korean Patent Application No. 10-2019-7016658 dated Jul. 21, 2020, 4 pgs. |
| Notice for Reasons of Rejection from Japanese Patent Application No. 2019-525878 dated Sep. 15, 2020, 6 pgs. |
| Notice of Preliminary Rejection from Korean Patent Application No. 10-2019-7016658 dated Jan. 29, 2021, 4 pgs. |
| Official Letter from Taiwan Patent Application No. 106139250 dated Mar. 31, 2021, 7 pgs. |
| Number | Date | Country | |
|---|---|---|---|
| 20200381280 A1 | Dec 2020 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 15955375 | Apr 2018 | US |
| Child | 16997807 | US | |
| Parent | 15351437 | Nov 2016 | US |
| Child | 15955375 | US |