An Application Data Sheet is filed concurrently with this specification as part of the present application. Each application that the present application claims benefit of or priority to as identified in the concurrently filed Application Data Sheet is incorporated by reference herein in its entirety and for all purposes.
This disclosure relates generally to integrated deposition and etch processes in fabrication of semiconductor devices and, more particularly, to integrated atomic layer deposition (ALD) and etch processes in critical dimension control in fabrication of integrated circuits.
As device and features size continue to shrink in the semiconductor industry, patterning features of small critical dimensions will continue to gain importance in fabrication of advanced integrated circuits (ICs). Current photolithography methods may be limited in its ability to pattern small critical dimension features.
This disclosure pertains to a method of critical dimension (CD) control. The method includes etching, in a plasma chamber, a first layer of a substrate to form a mask pattern of features, the mask pattern of features having a width that is less than a desired width of a plurality of structures to be formed by the mask pattern of features. The method further includes depositing, in the plasma chamber, a first passivation layer on the mask pattern of features by atomic layer deposition (ALD), the first passivation layer being deposited with a thickness that increases the width of the mask pattern of features to the desired width. The method further includes etching, in the plasma chamber, a second layer of the substrate to form the plurality of structures having the desired width.
In some implementations, the mask pattern of features includes one or more isolated features in an isolated feature region and one or more dense features in a dense feature region having a greater feature density than the isolated feature region. A CD gain between the one or more isolated features in the isolated feature region and the one or more dense features in the dense feature region may be the same or substantially similar after depositing the first passivation layer. A depth change between the isolated feature region and the dense feature region may be the same or substantially similar after etching the second layer of the substrate. In some implementations, the method further includes repeating operations of depositing by ALD and etching the second layer in the plasma chamber, where a CD gain between isolated features in the isolated feature region and dense features in the dense feature region is the same or substantially similar after repeating operations of depositing by ALD and etching the second layer. In some implementations, the mask pattern of features include one or more first features having a first material and one or more second features having a second material different than the first material, where a CD gain between the one or more first features and the one or more second features is the same or substantially similar after depositing the first passivation layer. In some implementations, operations of depositing by ALD and etching the second layer in the plasma chamber are performed without introducing a vacuum break in between operations. In some implementations, a thickness of the first passivation layer is between about 0.5 nm and about 3 nm. In some implementations, the method further includes depositing, in the plasma chamber, a second passivation layer on the plurality of structures by ALD after etching the second layer of the substrate, the second passivation layer being deposited with a thickness corresponding to a desired CD gain. In some implementations, the first passivation layer includes silicon oxide (SiOx). In some implementations, depositing the first passivation layer by ALD includes introducing a precursor into the plasma chamber to adsorb on the mask pattern of features, converting the precursor with plasma to form an adsorption-limited amount of the first passivation layer, and repeating operations of introducing the precursor and converting the precursor until the thickness of the first passivation layer is deposited on the mask pattern of features.
These and other aspects are described further below with reference to the drawings.
In the following description, numerous specific details are set forth to provide a thorough understanding of the presented embodiments. The disclosed embodiments may be practiced without some or all of these specific details. In other instances, well-known process operations have not been described in detail to not unnecessarily obscure the disclosed embodiments. While the disclosed embodiments will be described in conjunction with the specific embodiments, it will be understood that it is not intended to limit the disclosed embodiments.
In the present disclosure, the terms “semiconductor wafer,” “wafer,” “substrate,” “wafer substrate,” and “partially fabricated integrated circuit” are used interchangeably. One of ordinary skill in the art would understand that the term “partially fabricated integrated circuit” can refer to a silicon wafer during any of many stages of integrated circuit fabrication thereon. A wafer or substrate used in the semiconductor device industry typically has a diameter of 200 mm, or 300 mm, or 450 mm. The following detailed description assumes the present disclosure is implemented on a wafer. However, the present disclosure is not so limited. The work piece may be of various shapes, sizes, and materials. In addition to semiconductor wafers, other work pieces that may take advantage of the present disclosure include various articles such as printed circuit boards and the like.
Integrated Etch/ALD Processing Apparatus
As feature sizes shrink, pitch becomes smaller, and complementary metal-oxide-semiconductor (CMOS) technology scales to smaller nodes, thin conformal deposition techniques will continue to gain importance. Atomic layer deposition (ALD) is a film forming technique which is well-suited to the deposition of thin conformal films due to the fact that ALD deposits a single thin layer of material, the thickness being limited by the amount of one or more precursor reactants which may adsorb onto a substrate surface (i.e., forming an adsorption-limited layer) prior to film-forming chemical reaction itself. Each layer formed by ALD is thin and conformal, with the resulting film substantially conforming to the shape of underlying device structures and features.
Conventionally, ALD and etch processes are performed on separate tools or platforms. For example, ALD chambers do not run etch processes, and etch chambers do not run ALD processes. Plasma etch chambers that run a deposition process use a plasma-induced deposition process to form films that are not conformal and that are aspect ratio dependent.
Details regarding the processing apparatus 100 for performing etch and ALD operations are described in U.S. patent application Ser. No. 15/669,871, filed Aug. 4, 2017 to Zhou et al., and entitled “INTEGRATED ATOMIC LAYER PASSIVATION IN TCP ETCH CHAMBER AND IN-SITU ETCH-ALP METHOD,” which is incorporated by reference in its entirety and for all purposes.
The plasma chamber 132 may include an overall chamber structure that may be defined by chamber walls 114 and a window 106. The window 106 may be fabricated from quartz or other dielectric material. In some implementations, the plasma chamber 132 includes a substrate support 116 disposed inside the plasma chamber 132. In some implementations, the substrate support 116 is an electrostatic chuck for supporting a substrate 112 upon which a deposition/etch process is performed. The electrostatic chuck may include electrostatic electrodes for chucking and dechucking the substrate 112. A filter and DC clamp power supply (not shown) may be provided for this purpose. Other control systems for lifting the substrate 112 off the substrate support 116 may also be provided. The substrate support 116 is configured to receive and hold the substrate 112.
In some implementations, the substrate support 116 may include a heater (not shown) to heat the substrate 112. The substrate support 116 may operate at elevated temperatures, such as between about −20° C. and about 150° C. The temperature will depend on the process operation and specific recipe. In some implementations, the plasma chamber 132 may also operate at certain pressures, such as pressures in between about 1 mTorr and about 1 Torr.
In some implementations, the processing apparatus 100 may include a radio-frequency (RF) power supply 120 that may be used for biasing/charging the substrate support 116. The RF power supply 120 may be defined by one or more RF generators. If multiple RF generators are provided, different frequencies may be used to achieve various tuning characteristics. A bias matching circuitry 118 is coupled between the RF power supply 120 and the substrate support 116. In this manner, the RF power supply 120 is connected to the substrate support 116.
A coil 134 is positioned over the window 106. The coil 134 may be fabricated from an electrically conductive material and includes at least one complete turn. The coil 134 shown in
RF power is supplied from the RF power supply 121 to the coil 134 to cause an RF current to flow through the coil 134. The RF current flowing through the coil 134 may generate an electromagnetic field about the coil 134. The electromagnetic field generates an inductive current within the plasma chamber 132 that acts on the gas(es) present in the plasma chamber 132 to produce a plasma. Various ions and/or radicals from the plasma may interact with the substrate 112 to perform a deposition or etch operation.
In some implementations, the processing apparatus 100 optionally includes a plasma grid (not shown) that may be used to divide the plasma chamber 132 into an upper portion and a lower portion. The plasma grid may be used to limit the amount of hot electrodes into the lower portion of the plasma chamber 132. In some implementations, the processing apparatus 100 is designed to operate such that plasma present in the lower portion of the plasma chamber 132 is an ion-ion plasma and the plasma present in the upper portion of the plasma chamber 132 is an electron-ion plasma.
Process gases may be introduced into the plasma chamber 132 through a first gas injector 104 from the top of the plasma chamber 132 and/or through a second gas injector 110 from the side of the plasma chamber 132. Process gases may include vaporized liquid precursors or vaporized solid precursors, which may be vaporized in a solid source evaporator (not shown) upstream of the processing apparatus 100. One or more reactant gases may be supplied through the first gas injector 104 and/or second gas injector 110. In some implementations, the gas injectors 104, 110 may be replaced by showerheads. It will be understood that additional or other gas supplies may be provided for supplying different gases to the plasma chamber 132 for various types of operations.
The various ways of injecting gas(es) into the plasma chamber 132 show that process gases, vaporized liquid precursors, and/or vaporized solid precursors may be provided into the plasma chamber 132 from various locations. In some implementations, only the first gas injector 104 is used. In some other implementations, only the second gas injector 110 is used. In some other implementations, both the first gas injector 104 and the second gas injector 110 are used. In some implementations, manifolds 122 control which gases are supplied to each of the different gas lines. Manifolds 122 allow for any type of gas (reactant, carrier, precursor, etc.) to be provided from any of the different gas lines. In some implementations, carrier gases can include gases such as oxygen (O2), nitrogen (N2), and helium (He). The gases may be introduced into the plasma chamber 132 without mixing or may be mixed with other gases before introduction into the plasma chamber 132.
Manifolds 122 may be used for selecting, switching, and/or mixing outputs from respective delivery systems in a delivery system 128. The delivery system 128 may, in some implementations, include an etch gas delivery system 127 and a liquid delivery system 129. The etch gas delivery system 127 may be configured to output etchant gases. Examples of etchant gases include but are not limited to chlorine (Cl2), hydrogen bromide (HBr), and sulfur hexafluoride (SF6). The liquid delivery system 129 may be configured to provide liquid precursor that is vaporized and delivered in vapor form in an ALD process. The vaporized liquid precursor may be introduced into the plasma chamber 132 and may adsorb onto a surface of the substrate 112. The adsorbed precursor may be converted to form an adsorption-limited amount of film using a plasma. An example liquid precursor may have a chemical composition of the formula: CxHyNzOaSib.
A vacuum pump 130 is connected to the plasma chamber 132 and may be used to draw out process gases from the plasma chamber 132 and to maintain a certain pressure within the plasma chamber 132. A valve 126 may be disposed between an exhaust 124 and the vacuum pump 130 to control the amount of vacuum suction being applied to the plasma chamber 132. In some implementations, the vacuum pump 130 can be a one or two stage mechanical dry pump and/or turbomolecular pump. In some implementations, the vacuum pump 130 may be activated after each time an ALD process is completed to purge the plasma chamber 132.
The processing apparatus 100 may be coupled to facilities (not shown) when installed in a clean room or a fabrication facility. Facilities include plumbing that provide processing gases, vacuum, temperature control, and environmental particle control. These facilities may be coupled to the processing apparatus 100 when installed in the target fabrication facility. Additionally, the processing apparatus 100 may be coupled to a transfer chamber that allows robotics to transfer substrates into and out of the plasma chamber 132 using automation.
In some implementations, a system controller 108 (which may include one or more physical or logical controllers) controls some or all of the operations of the processing apparatus 100. The system controller 108 may include one or more memory devices and one or more processors. The processor may include a central processing unit (CPU) or computer, analog and/or digital input/output connections, stepper motor controller boards, and other like components. Instructions for implementing appropriate control operations are executed on the processor. These instructions may be stored on the memory devices associated with the system controller 108 they may be provided over a network. In certain implementations, the system controller 108 executes system control software.
The system control software may include instructions for controlling the timing of application and/or magnitude of any one or more of the following chamber operational conditions: the mixture and/or composition of gases, chamber pressure, chamber temperature, wafer/wafer support temperature, the bias applied to the substrate (which in various implementations may be zero), the frequency and power applied to coils or other plasma generation components, substrate position, substrate movement speed, and other parameters of a particular process performed by the tool. System control software may be configured in any suitable way. For example, various process tool component subroutines or control objects may be written to control operations of the process tool components necessary to carry out various process tool processes. System control software may be coded in any suitable compute readable programming language.
In some embodiments, system control software includes input/output control (IOC) sequencing instructions for controlling the various parameters described above. For example, each phase of a semiconductor fabrication process may include one or more instructions for execution by the system controller 108. The instructions for setting process conditions for a phase may be included in a corresponding recipe phase, for example. In some implementations, the recipe phases may be sequentially arranged, such that steps in a doping process are executed in a certain order for that process phase. For example, a recipe may be configured to perform etch operations and include one or more cycles of an ALD process performed in between each of the etch operations.
In some implementations, the system controller 108 is configured with instructions for performing one or more of the following operations: etching, in the plasma chamber 132, a first layer of a substrate 112 to form a mask pattern of features, the mask pattern of features having a width that is less than a desired width of a plurality of structures to be formed by the mask pattern of features; depositing, in the plasma chamber 132, a first passivation layer on the mask pattern of features by ALD, the first passivation layer being deposited with a thickness that increases the width of the mask pattern of features to the desired width; and etching, in the plasma chamber 132, a second layer of the substrate 112 to form the plurality of structures having the desired width. The etching and depositing operations are performed without introducing a vacuum break in the plasma chamber 132. In some implementations, the system controller 108 is further configured to perform the following operation: repeating operations of depositing by ALD and etching in the plasma chamber 132.
Other computer software and/or programs may be employed in some embodiments. Examples of programs or sections of programs for this purpose include substrate positioning program, a process gas composition control program, a pressure control program, a heater control program, and an RF power supply control program.
In some cases, the system controller 108 controls gas concentration, substrate movement, and/or the power supplied to the coil 134 and/or substrate support 116. The system controller 108 may control the gas concentration by, for example, opening and closing relevant valves to produce one or more inlet gas stream that provide the necessary reactant(s) at the proper concentration(s). The substrate movement may be controlled by, for example, directing a substrate positioning system to move as desired. The power supplied to the coil 134 and/or substrate support 116 may be controlled to provide particular RF power levels. If a grid is used, the RF powers may be adjusted by the system controller 108 to create an electron-ion plasma in an upper portion of the plasma chamber 132 and ion-ion plasma in a lower portion of the plasma chamber 132. Further, the system controller 108 may be configured to supply power to the substrate support 116 under conditions such that an electron-ion plasma does not form in the lower portion of the plasma chamber 132.
The system controller 108 may control these and other aspects based on sensor output (e.g., when power, potential, pressure, etc. reach a certain threshold), the timing of an operation (e.g., opening valves at certain times in a process), or based on received instructions from the user.
In some implementations, a system controller 108 is part of a system, which may be part of the above-described examples. Such systems can comprise semiconductor processing equipment, including a processing tool or tools, chamber or chambers, a platform or platforms for processing, and/or specific processing components (a wafer pedestal, a gas flow system, etc.). These systems may be integrated with electronics for controlling their operation before, during, and after processing of a semiconductor wafer or substrate. The electronics may be referred to as the “controller,” which may control various components or subparts of the system or systems. The system controller 108, depending on the processing requirements and/or the type of system, may be programmed to control any of the processes disclosed herein, including the delivery of processing gases, temperature settings (e.g., heating and/or cooling), pressure settings, vacuum settings, power settings, RF generator settings, RF matching circuit settings, frequency settings, flow rate settings, fluid delivery settings, positional and operation settings, substrate transfers into and out of a tool and other transfer tools and/or load locks connected to or interfaced with a specific system.
Broadly speaking, the system controller 108 may be defined as electronics having various integrated circuits, logic, memory, and/or software that receive instructions, issue instructions, control operation, enable cleaning operations, enable endpoint measurements, and the like. The integrated circuits may include chips in the form of firmware that store program instructions, digital signal processors (DSPs), chips defined as application specific integrated circuits (ASICs), and/or one or more microprocessors, or microcontrollers that execute program instructions (e.g., software). Program instructions may be instructions communicated to the system controller 108 in the form of various individual settings (or program files), defining operational parameters for carrying out a particular process on or for a semiconductor substrate or to a system. The operational parameters may, in some embodiments, be part of a recipe defined by process engineers to accomplish one or more processing steps during the fabrication of one or more layers, materials, metals, oxides, silicon, silicon dioxide, surfaces, circuits, and/or dies of a substrate.
The system controller 108, in some implementations, may be a part of or coupled to a computer that is integrated with, coupled to the system, otherwise networked to the system, or a combination thereof. For example, the system controller 108 may be in the “cloud” or all or a part of a fab host computer system, which can allow for remote access of the substrate processing. The computer may enable remote access to the system to monitor current progress of fabrication operations, examine a history of past fabrication operations, examine trends or performance metrics from a plurality of fabrication operations, to change parameters of current processing, to set processing steps to follow a current processing, or to start a new process. In some examples, a remote computer (e.g. a server) can provide process recipes to a system over a network, which may include a local network or the Internet. The remote computer may include a user interface that enables entry or programming of parameters and/or settings, which are then communicated to the system from the remote computer. In some examples, the system controller 108 receives instructions in the form of data, which specify parameters for each of the processing steps to be performed during one or more operations. It should be understood that the parameters may be specific to the type of process to be performed and the type of tool that the system controller 108 is configured to interface with or control. Thus as described above, the system controller 108 may be distributed, such as by comprising one or more discrete controllers that are networked together and working towards a common purpose, such as the processes and controls described herein. An example of a distributed system controller 108 for such purposes would be one or more integrated circuits on a chamber in communication with one or more integrated circuits located remotely (such as at the platform level or as part of a remote computer) that combine to control a process on the chamber.
Without limitation, example systems may include a plasma etch chamber or module, a deposition chamber or module, a spin-rinse chamber or module, a metal plating chamber or module, a clean chamber or module, a bevel edge etch chamber or module, a physical vapor deposition (PVD) chamber or module, a chemical vapor deposition (CVD) chamber or module, an atomic layer deposition (ALD) chamber or module, an atomic layer etch (ALE) chamber or module, an ion implantation chamber or module, a track chamber or module, and any other semiconductor processing systems that may be associated or used in the fabrication and/or manufacturing of semiconductor substrates.
As noted above, depending on the process step or steps to be performed by the tool, the system controller 108 might communicate with one or more of other tool circuits or modules, other tool components, cluster tools, other tool interfaces, adjacent tools, neighboring tools, tools located throughout a factory, a main computer, another system controller 108, or tools used in material transport that bring containers of substrates to and from tool locations and/or load ports in a semiconductor manufacturing factory.
Patterning and Critical Dimensions
With shrinking device features and smaller pitches in semiconductor devices, it has become more important to control and finely tune a critical dimension (CD) of substrate features. CD may also be referred to as “minimum feature size” or “target design rule.” In some implementations, CD may refer to the size of the smallest geometrical feature (e.g., width of interconnect lines, contacts, trenches, etc.). In some implementations, CD may refer to the narrowest width that a patterning process can achieve.
Patterning methods are used in many semiconductor manufacturing processes to achieve desired critical dimensions. A mask, such as a photoresist pattern or hard mask, may have a CD that is the width of the smallest feature. In some implementations, features may be formed when an etching operation is performed through the mask.
In pursuing features with smaller CD, masks with smaller CDs are desired. Photoresist masks generally have optical properties dependent on wavelength, with longer wavelength photoresist masks exposed to longer wavelength light having larger theoretical CDs and shorter wavelength photoresist masks exposed to shorter wavelength light having smaller theoretical CDs. However, the use of shorter wavelength photoresist masks may present additional problems over longer wavelength photoresist masks. For example, shorter wavelength photoresist masks may not have a selectivity as high as longer wavelength photoresist masks and may more easily deform under plasma etch conditions.
Masks of the present disclosure may be formed or otherwise provided using various patterning schemes, such as single patterning or multiple patterning. In particular, multiple patterning has been used to extend lithographic technology beyond its optical limits. Double patterning and quad patterning are example technologies used to extend lithographic technology beyond its optical limits and double patterning is now widely used in the industry for pitches less than about 80 nm. Current double patterning technologies often use sidewall spacers with two masking steps to pattern trenches. Methods of double patterning, particularly line patterning, in both positive and negative double patterning processes have involved the use of spacers and masks. Spacers can be deposited by ALD or by plasma-enhanced atomic layer deposition (PEALD) on a patterned core and may be used to create a smaller pitch pattern.
As shown in
The pattern of the second spacers 221 may be transferred to the second layer 205. Multiple patterning techniques, such as a technique shown in
The use of separate chambers for deposition and etch increases processing time, processing steps, and costs, thereby having an adverse impact on throughput. Furthermore, the use of separate chambers requires transporting substrates from one chamber to another chamber, which entails vacuum breaks and increases the likelihood of unwanted materials or particles coming into contact with the substrates. This may result in the loss of material functionality and/or integrity on the substrate. Moreover, as shown in
To achieve smaller CDs while avoiding the problems associated with performing etch steps and deposition steps in different tools, a plasma etch chamber may be utilized and adapted to perform deposition. Such deposition processes may include chemical vapor deposition (CVD) and plasma enhanced chemical vapor deposition (PECVD) processes. However, such deposition processes typically deposit films that are not conformal. More specifically, the deposition processes are dependent on aspect ratio and deposit more material in more open spaces or wider pitches, resulting in non-uniform deposition across structures or features of different aspect ratios. Specifically, more deposition would take place in isolated features than in dense features, where a CD bias for isolated features is greater than a CD bias for dense features.
Implementations of the present disclosure relate to the integration of ALD steps and etch steps in a plasma chamber. By using in-situ ALD rather than ALD conducted in a separate chamber and rather than using CVD/PECVD in the same chamber, standalone ALD tools and additional cleaning tools are eliminated. Furthermore, processing time and costs are reduced by eliminating additional substrate transfers and clean time. In addition, using in-situ ALD avoids vacuum breaks between substrate transfers (e.g., between ex-situ deposition and clean), which may expose the substrate to unwanted materials, atmosphere, and/or moisture. Using in-situ ALD also reduces the impact of non-uniform deposition across structures or features of different aspect ratios. In-situ ALD may refer to the ALD performed in a plasma etch chamber, such as a plasma chamber in the processing apparatus 100 of
Critical Dimension Control with In-Situ ALD and Etch
Implementations of the present disclosure relate to a method of CD control using in-situ ALD and etch. Specifically, cycles of ALD and etch steps are performed in the same process chamber or tool. In some implementations, the cycles of ALD and etch steps are performed in a plasma processing apparatus as described in
At block 410 of the process 400, a first layer of a substrate is etched to form a mask pattern of features in a plasma chamber. The plasma chamber may be configured to perform subsequent etch and deposition processes. Aspects of the plasma chamber may be described with respect to the processing apparatus 100 in
In some implementations of the process 400, a substrate is provided in the plasma chamber. The substrate may be positioned on a substrate support in the plasma chamber. In some implementations, the substrate can be a semiconductor substrate, such as a 200-mm, 300-mm, or 450-mm substrate, including silicon substrates. In some implementations, the substrate is provided in the plasma chamber pre-patterned with the mask pattern of features.
In some implementations, the mask pattern of features may include one or more isolated features in an isolated feature region of the substrate and one or more dense features in a dense feature region of the substrate. The one or more dense features have greater feature density in the dense feature region than the one or more isolated features in the isolated feature region. The one or more dense features may provide features with higher aspect ratios than the one or more isolated features.
In some implementations, the mask pattern of features may include one or more features having a first material and one or more other features having a second material different than the first material. The mask pattern of features may include two different materials, where the two different materials may react differently in a passivation process or etch process. Two different materials may be used to create a mask or masks with different pitches. For example, the first material may include silicon and the second material may include silicon-germanium or germanium.
In some implementations, at least some of the mask pattern of features may have a tapered profile. Patterning processes may produce a mask profile having some degree of taper. In some implementations, the etch performed in block 410 may straighten the tapered profile and reduce any pinch-off or merging caused by subsequent deposition. In some implementations, the process 400 further includes anisotropically etching at least a portion of the mask pattern of features with the tapered profile to modify the tapered profile before subsequent deposition.
The mask pattern of features may include a plurality of geometric structures, spacers, or features, each having a width that corresponds to a critical dimension (CD) of the mask pattern of features. In some implementations, each of the geometric structures, spacers, or features of the mask pattern of features has a width that is the same or is substantially similar. With respect to the width or CD of the mask pattern of features, “substantially similar” throughout this disclosure refers to values within plus or minus 5% of a stated value. Thus, the CD or space CD of the mask pattern of features is relatively consistent or constant across the mask pattern of features as provided on the substrate. In some implementations, the CD or space CD between one or more isolated features and one or more dense features may be the same or substantially similar. In some implementations, a space CD of the mask pattern of features is equal to or less than about 5 nm.
After etching the first layer to form the mask pattern of features, the CD of the mask pattern of features will typically not be equal to the CD of a plurality of structures to be formed using the mask pattern of features. This may be attributable to effects of faceting, erosion of the mask, and undercutting due to lateral etching. In some cases, a higher degree of overetch is performed intentionally to increase a process window of a mask open etch process, at the expense of smaller CD. As a result, the CD of the plurality of structures to be formed using the mask pattern of features may be less than the CD of the mask pattern of features.
Passivation techniques may be applied on a mask to minimize CD loss due to etching. Plasma-based passivation in the form of, for example, “flash” passivation or etch byproduct re-deposition has been used to minimize effects of faceting, erosion of the mask, and undercutting due to lateral etching. Plasma-based passivation techniques, however, are generally aspect ratio dependent, meaning that more passivating material is loaded in isolated features than dense features. Plasma-based techniques are also material dependent, meaning that more or less passivating material is loaded between different materials. Furthermore, plasma-based passivation techniques, such as an oxygen “flash” passivation, consumes material on the target feature through oxidation and causes CD loss. “Flash” passivation can refer to striking a gas such as oxygen (O2) and/or nitrogen (N2) to form a plasma of dissociated radicals to react with a surface and form a passivating layer of material (e.g., oxide or nitride) on a surface. Passivation techniques in general may minimize effects of faceting, erosion of the mask, and undercutting due to lateral etching but does not control CD or finely tune CD. In other words, CD loss may be limited using conventional passivation techniques but the passivation technique itself is not applied to precisely tune CD.
At block 420 of the process 400, a first passivation layer is deposited on the mask pattern of features by atomic layer deposition (ALD) in the plasma chamber. The first passivation layer is deposited with a thickness that increases the width of the mask pattern of features to the desired width. ALD at block 420 is performed in the same plasma chamber as etch at block 410 without introducing a vacuum break in between operations.
ALD is a technique that deposits thin layers of material using sequential self-limiting reactions. Typically, an ALD cycle includes operations to deliver and adsorb at least one reactant to the substrate surface, and then react the adsorbed reactant with one or more reactants to form the partial layer of film. Unlike a CVD technique, ALD processes use surface-self-limited deposition reactions to deposit films on a layer-by-layer basis. A typical ALD cycle may include: (i) dosing that delivers and adsorbs precursor material onto a substrate surface, (ii) purging excess precursor material from the chamber and leaving a self-limited monolayer on the substrate surface, (iii) delivery of reactant material to react with the adsorbed precursor material, and (iv) purging of unreacted reactant material or reaction byproducts from the chamber. The dose step may adsorb precursor material in a self-limiting manner such that once active sites are occupied by the precursor material, little or no additional precursor material will be adsorbed on the substrate surface. The reactant material may likewise react with the precursor material in a self-limiting or adsorption-limiting manner. Purge steps may be optionally performed to remove excess precursor material, reaction byproducts, and/or unreacted reactant material from the chamber, thereby completing an ALD cycle. ALD may be used to provide highly conformal films with high step coverage even in high aspect ratio features.
The first passivation layer may be conformally deposited by ALD on the mask pattern of features. The ALD process for conformally depositing the first passivation layer may occur in one or more cycles, where each cycle produces an adsorption-limited amount of passivation material on the mask pattern of features. Each cycle may include a dose step where a controlled amount of precursor material is delivered to a substrate surface to adsorb on the substrate surface in a self-limiting manner. This is also known as “soaking” the substrate surface to saturation. Each cycle may further include a conversion step following the dose step where reactant material is provided to react with the precursor material on the substrate surface and form an adsorption-limited amount of passivation material. The reactant material may include a reactant gas, where an RF power source generates plasma of the reactant gas in the plasma chamber. The reactant gas may include, for example, an oxygen-containing gas (e.g., O2) or a nitrogen-containing gas (e.g., N2 or NH3). Radicals and other charged species of the reactant gas react with the precursor material to convert the precursor material to the adsorption-limited amount of passivation material. In some implementations, the reactant gas is exposed to RF power delivery in a relatively short amount of time, such as between about 0.5 seconds and about 5 seconds, to form the plasma to convert the precursor material. This is also known as a “flash” operation to convert the precursor material on the substrate surface using plasma from RF power delivered in a relatively short amount of time. In some implementations, a purge step may remove excess precursor material, reaction byproducts, and/or unreacted reactant material from the plasma chamber to complete the cycle. In some implementations, the dose step and the conversion step may be repeated until a desired thickness of the first passivation layer is deposited.
The first passivation layer may include, for example, an oxide (e.g., SiOx) or a nitride (e.g., SixNy). The first passivation layer serves to protect the mask pattern of features, including sidewalls of the mask pattern of features, during a subsequent etch process such as an etch process described at block 430.
The first passivation layer is conformally deposited by ALD and may have a high step coverage, such as a step coverage of greater than 85%, greater than 90%, or greater than 95%. The high conformality of the first passivation layer provides a relatively uniform thickness of the first passivation layer along a surface and sidewalls of the mask pattern of features. In some implementations, the thickness of the first passivation layer may be between about 0.1 nm and about 5 nm or between about 0.5 nm and about 3 nm. The thickness of the first passivation layer may increase the width of the mask pattern of features to the desired width in a linear relationship, where the desired width corresponds to the desired CD of the plurality of structures to be subsequently formed. Accordingly, the CD of the mask pattern of features may be controlled by the thickness of the first passivation layer. In some implementations, any CD loss from etching at block 410 may be recovered by a thickness of the deposited first passivation layer. In some implementations, CD may be precisely tuned at block 420 to control the CD of the mask pattern of features, thereby controlling a CD of the plurality of structures or features to be subsequently formed. The relevant CD for CD control or recovery may depend on an application of the semiconductor device being fabricated. After etching, the CD of the remaining material may be the relevant CD in some cases, such as a gate or transistor size following a patterning and gate etch. Or, the CD (e.g., space CD) of the removed material may be the relevant CD in some cases, such as when a space, trench, or hole is opened following an etch, which may or may not be subsequently filled. CD gain from the deposited first passivation layer may be independent of aspect ratio and independent of material. Furthermore, CD may be tuned at block 420 without affecting subsequent etch performance. In other words, CD may be tuned with minimal or negligible impact on CD loading between isolated and dense features, and with minimal or negligible impact on depth loading between isolated and dense features.
At block 430 of the process 400, a second layer of the substrate is etched in the plasma chamber to form the plurality of structures having the desired width. Etch at block 430 is performed in the same plasma chamber as etch at block 410 and ALD at block 420 without introducing a vacuum break in between operations.
The second layer may be a target layer for patterning various geometric features of the substrate, where such geometric features may correspond to or may be defined by the plurality of structures. The geometric features may include, for example, interconnect lines, contacts, trenches, recesses, spaces, holes, etc. The plurality of structures may be defined using the mask pattern of features, where a CD of the plurality of structures is the same or substantially similar to the CD of the mask pattern of features. With respect to the CD difference between the mask pattern of features and the plurality of structures, “substantially similar” throughout this disclosure refers to values within plus or minus 5% of a stated value. In some implementations, the CD of the plurality of structures may be equal to or less than about 20 nm, equal to or less than about 15 nm, or equal to or less than about 10 nm. Though the CD being described refers to a CD of the plurality of structures defined by the mask pattern of features, it will be understood that the relevant CD may be a space CD of a plurality of geometric features such as trenches, recesses, spaces, and holes defined by the mask pattern of features.
The etch performed in the plasma chamber may be an anisotropic etch through the second layer to form features in the second layer. The etch may be selective to etch material of the second layer over material of the first layer and the first passivation layer. That way the etch performed at block 430 selectively etches the second layer without etching the mask pattern of features. In some implementations, the etch may extend through the second layer to a first depth, where the first depth is less than a final depth. For example, the first depth may be any suitable percentage of the final depth, such as 20%, 30%, 40%, 50%, 60%, etc. of the final depth. Thus, multiple etches may be performed to reach the final depth.
In some implementations, operations of ALD and etching in the plasma chamber are repeated until the final depth is achieved. The final depth may extend partially through the second layer or entirely through the second layer. In some implementations, the final depth may extend through additional underlying layers, such as a third layer, fourth layer, etc. The repeated etch operation may etch through the second layer or a third layer underlying the second layer. In some implementations, the operations of ALD and etching in the plasma chamber are repeated in a multiple patterning process. For example, each ALD operation following an etch operation may conformally deposit additional passivation layers such as a second passivation layer, third passivation layer, etc. to further tune or reduce a CD of substrate features. And, each etch operation following an ALD operation may etch through the second layer or underlying layers such as a third layer, fourth layer, fifth layer, etc. In some implementations, the process 400 further includes depositing a second passivation layer on the plurality of structures by ALD after etching the second layer of the substrate, the second passivation layer being deposited with a thickness corresponding to a desired CD gain. The process 400 may further include etching the second layer or a third layer of the substrate to form a plurality of features (e.g., trenches) having a desired CD. This kind of multiple patterning scheme may enable shrinking critical dimensions in a controlled manner without substrate transfers between etch-dep-etch operations.
The first passivation layer protects the mask pattern of features from the etch at block 430. The sidewalls and surface of the mask pattern of features are protected with minimal CD loss independent of aspect ratio and independent of material. Moreover, the sidewalls and surface of the mask pattern of features are protected with minimal CD loading between different materials and aspect ratios, minimal profile loading between different materials and aspect ratios, and minimal depth loading between different materials and aspect ratios.
In some implementations, operations of depositing by ALD in the plasma chamber at block 420 and etching the second layer in the plasma chamber at block 430 are repeated in the process 400. Where the mask pattern of features includes isolated and dense features, a CD gain is the same or substantially similar after repeating operations of depositing by ALD and etching the second layer. Where the mask pattern of features includes different materials, a CD gain is the same or substantially similar after repeating operations of depositing by ALD and etching the second layer.
Although the foregoing embodiments have been described in some detail for purposes of clarity of understanding, it will be apparent that certain changes and modifications may be practiced within the scope of the appended claims. It should be noted that there are many alternative ways of implementing the processes, systems, and apparatus of the present embodiments. Accordingly, the present embodiments are to be considered as illustrative and not restrictive, and the embodiments are not to be limited to the details given herein.
Number | Name | Date | Kind |
---|---|---|---|
8334083 | Luong et al. | Dec 2012 | B2 |
9171716 | Fukuda | Oct 2015 | B2 |
9269590 | Lucre et al. | Feb 2016 | B2 |
9543148 | Hudson et al. | Jan 2017 | B1 |
9576811 | Kanarik et al. | Feb 2017 | B2 |
9805941 | Kanarik et al. | Oct 2017 | B2 |
9806252 | Tan et al. | Oct 2017 | B2 |
9870899 | Yang et al. | Jan 2018 | B2 |
9997371 | Agarwal | Jun 2018 | B1 |
9997631 | Yang et al. | Jun 2018 | B2 |
10074543 | Mahorowala et al. | Sep 2018 | B2 |
10446394 | Abatchev et al. | Oct 2019 | B2 |
10515815 | Zhou et al. | Dec 2019 | B2 |
10658174 | Zhou et al. | May 2020 | B2 |
10734238 | Zhou | Aug 2020 | B2 |
20030192569 | Goto et al. | Oct 2003 | A1 |
20040144489 | Satoh et al. | Jul 2004 | A1 |
20050048785 | Kang et al. | Mar 2005 | A1 |
20060226120 | Rusu et al. | Oct 2006 | A1 |
20070196980 | Subramanian | Aug 2007 | A1 |
20080230947 | Chou et al. | Sep 2008 | A1 |
20090197420 | Luong et al. | Aug 2009 | A1 |
20090206443 | Juengling | Aug 2009 | A1 |
20090233446 | Sakao et al. | Sep 2009 | A1 |
20090246965 | Mori et al. | Oct 2009 | A1 |
20090275205 | Kiehlbauch et al. | Nov 2009 | A1 |
20100173496 | Zhong et al. | Jul 2010 | A1 |
20100323525 | Chi et al. | Dec 2010 | A1 |
20110089469 | Merckling | Apr 2011 | A1 |
20120264305 | Nakano | Oct 2012 | A1 |
20130189845 | Kim et al. | Jul 2013 | A1 |
20130323923 | Koehler et al. | Dec 2013 | A1 |
20140083978 | Mahadeswaraswamy et al. | Mar 2014 | A1 |
20140213037 | LiCausi et al. | Jul 2014 | A1 |
20140252478 | Doornbos et al. | Sep 2014 | A1 |
20150102386 | Chen et al. | Apr 2015 | A1 |
20150187602 | Kim | Jul 2015 | A1 |
20150249018 | Park et al. | Sep 2015 | A1 |
20150322569 | Kilpi et al. | Nov 2015 | A1 |
20150380272 | Wu et al. | Dec 2015 | A1 |
20160056270 | Dal | Feb 2016 | A1 |
20160064379 | Yu | Mar 2016 | A1 |
20160111309 | Lill et al. | Apr 2016 | A1 |
20160126243 | Weis | May 2016 | A1 |
20160307769 | Tseng et al. | Oct 2016 | A1 |
20160308112 | Tan | Oct 2016 | A1 |
20160336178 | Swaminathan et al. | Nov 2016 | A1 |
20160365425 | Chen et al. | Dec 2016 | A1 |
20160379824 | Wise et al. | Dec 2016 | A1 |
20170229314 | Tan et al. | Aug 2017 | A1 |
20170323831 | Jeong | Nov 2017 | A1 |
20180019387 | Tan et al. | Jan 2018 | A1 |
20180033635 | Kanarik et al. | Feb 2018 | A1 |
20180061650 | Mahorowala et al. | Mar 2018 | A1 |
20180090491 | Huang et al. | Mar 2018 | A1 |
20180240667 | Yu et al. | Aug 2018 | A1 |
20180308680 | Reddy et al. | Oct 2018 | A1 |
20190067120 | Ching | Feb 2019 | A1 |
20190109002 | Mattinen et al. | Apr 2019 | A1 |
20190122937 | Cheng | Apr 2019 | A1 |
20190148501 | Chen et al. | May 2019 | A1 |
20190157066 | Zhou et al. | May 2019 | A1 |
20190157095 | Zhou et al. | May 2019 | A1 |
20190157096 | Zhou et al. | May 2019 | A1 |
20190237330 | Abatchev et al. | Aug 2019 | A1 |
20200243326 | Zhou et al. | Jul 2020 | A1 |
Number | Date | Country |
---|---|---|
WO 2017048275 | Mar 2017 | WO |
Entry |
---|
U.S. Office Action dated Jul. 15, 2019 issued in U.S. Appl. No. 15/820,108. |
U.S. Final Office Action dated Jan. 6, 2020 issued in U.S. Appl. No. 15/820,108. |
U.S. Notice of Allowance dated Mar. 25, 2020 issued in U.S. Appl. No. 15/820,108. |
U.S. Office Action dated Dec. 11, 2018 issued in U.S. Appl. No. 15/820,263. |
U.S. Notice of Allowance dated Apr. 4, 2019 issued in U.S. Appl. No. 15/820,263. |
U.S. Notice of Allowance dated Sep. 16, 2019 issued in U.S. Appl. No. 15/820,263. |
U.S. Office Action dated Sep. 9, 2019 issued in U.S. Appl. No. 15/820,110. |
U.S. Notice of Allowance dated Jan. 16, 2020 issued in U.S. Appl. No. 15/820,110. |
U.S. Office Action dated Dec. 14, 2018 issued in U.S. Appl. No. 15/881,506. |
U.S. Notice of Allowance dated Mar. 8, 2019 issued in U.S. Appl. No. 15/881,506. |
U.S. Notice of Allowance dated Jul. 3, 2019 issued in U.S. Appl. No. 15/881,506. |
International Search Report and Written Opinion dated Mar. 6, 2019 in Application No. PCT/US2018/060732. |
International Search Report and Written Opinion dated Mar. 6, 2019 in Application No. PCT/US2018/060739. |
International Search Report and Written Opinion dated Mar. 5, 2019 in Application No. PCT/US2018/060743. |
International Search Report and Written Opinion dated May 14, 2019 in Application No. PCT/US2019/014580. |
U.S. Appl. No. 16/845,746, filed Apr. 10, 2020, Zhou et al. |
U.S. Office Action dated Feb. 3, 2021 issued in U.S. Appl. No. 16/845,746. |
International Preliminary Report on Patentability dated Jun. 4, 2020 in Application No. PCT/US2018/060732. |
International Preliminary Report on Patentability dated Jun. 4, 2020 in Application No. PCT/US2018/060739. |
International Preliminary Report on Patentability dated Jun. 4, 2020 in Application No. PCT/US2018/060743. |
International Preliminary Report on Patentability dated Aug. 6, 2020 in Application No. PCT/US2019/014580. |
U.S. Notice of Allowance dated Jul. 12, 2021 issued in U.S. Appl. No. 16/845,746. |
Number | Date | Country | |
---|---|---|---|
20200328087 A1 | Oct 2020 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 15820108 | Nov 2017 | US |
Child | 16946529 | US |