The present disclosure relates generally to the field of semiconductor devices, and particularly to structures containing bonding pads that include self-aligned diffusion barrier layers and methods for forming the same.
Wafer bonding or die bonding can be employed to provide a bonded assembly of multiple semiconductor dies. For example, two semiconductor dies providing different functionalities can be bonded to provide a semiconductor chip having combined functionalities. Metal wiring inside each semiconductor die provides metal interconnection among components within a respective semiconductor die.
According to an embodiment of the present disclosure, a structure comprising a first semiconductor die is provided. The first semiconductor die includes at least one first semiconductor device located on a first substrate, a first pad-level dielectric layer which is a diffusion barrier overlying the at least one first semiconductor device, and first bonding structures including a respective first metallic bonding pad embedded in the first pad-level dielectric layer. Each of the first bonding structures includes a metallic fill material portion having a horizontal distal surface that is located within a horizontal plane including a horizontal distal surface of the first pad-level dielectric layer, and a metallic liner laterally surrounding the metallic fill material portion and vertically spaced from the horizontal plane by a vertical recess distance.
According to another embodiment of the present disclosure, a method of forming a structure including a first semiconductor die is provided. The method comprises: forming at least one first semiconductor device on a first substrate; forming a first pad-level dielectric layer over the at least one first semiconductor device; forming first cavities in the first pad-level dielectric layer; forming metallic liners in the first cavities, wherein each of the metallic liners is vertically recessed from a horizontal plane including a horizontal distal surface of the first pad-level dielectric layer toward the first substrate; and forming metallic fill material portions in remaining volumes of the first cavities on a respective one of the metallic liners, whereby first bonding structures comprising a respective first metallic bonding pad are formed, wherein each of the first bonding structures comprises a combination of a respective one of the metallic liners and a respective one of the metallic fill material portions.
Bonding pads including copper are prone to recesses in regions proximal to metallic diffusion barrier layers, which can accelerate copper migration induced void formation. Bonding pads without recesses near metallic diffusion barrier layers are desirable. The embodiments of the present disclosure are directed to structures containing bonding pads that include self-aligned diffusion barrier layers and methods for forming the same, the various aspects of which are described herein in detail. The self-aligned diffusion barrier layers reduce or prevent the recess and void formation and improve the quality of the bonding between the dies.
The drawings are not drawn to scale. Multiple instances of an element may be duplicated where a single instance of the element is illustrated, unless absence of duplication of elements is expressly described or clearly indicated otherwise. Ordinals such as “first,” “second,” and “third” are employed merely to identify similar elements, and different ordinals may be employed across the specification and the claims of the instant disclosure. The term “at least one” element refers to all possibilities including the possibility of a single element and the possibility of multiple elements.
The same reference numerals refer to the same element or similar element. Unless otherwise indicated, elements having the same reference numerals are presumed to have the same composition and the same function. Unless otherwise indicated, a “contact” between elements refers to a direct contact between elements that provides an edge or a surface shared by the elements. If two or more elements are not in direct contact with each other or among one another, the two elements are “disjoined from” each other or “disjoined among” one another. As used herein, a first element located “on” a second element can be located on the exterior side of a surface of the second element or on the interior side of the second element. As used herein, a first element is located “directly on” a second element if there exist a physical contact between a surface of the first element and a surface of the second element. As used herein, a first element is “electrically connected to” a second element if there exists a conductive path consisting of at least one conductive material between the first element and the second element. As used herein, a “prototype” structure or an “in-process” structure refers to a transient structure that is subsequently modified in the shape or composition of at least one component therein.
As used herein, a “layer” refers to a material portion including a region having a thickness. A layer may extend over the entirety of an underlying or overlying structure, or may have an extent less than the extent of an underlying or overlying structure. Further, a layer may be a region of a homogeneous or inhomogeneous continuous structure that has a thickness less than the thickness of the continuous structure. For example, a layer may be located between any pair of horizontal planes between, or at, a top surface and a bottom surface of the continuous structure. A layer may extend horizontally, vertically, and/or along a tapered surface. A substrate may be a layer, may include one or more layers therein, or may have one or more layer thereupon, thereabove, and/or therebelow.
As used herein, a first surface and a second surface are “vertically coincident” with each other if the second surface overlies or underlies the first surface and there exists a vertical plane or a substantially vertical plane that includes the first surface and the second surface. A substantially vertical plane is a plane that extends straight along a direction that deviates from a vertical direction by an angle less than 5 degrees. A vertical plane or a substantially vertical plane is straight along a vertical direction or a substantially vertical direction, and may, or may not, include a curvature along a direction that is perpendicular to the vertical direction or the substantially vertical direction.
As used herein, a “memory level” or a “memory array level” refers to the level corresponding to a general region between a first horizontal plane (i.e., a plane parallel to the top surface of the substrate) including topmost surfaces of an array of memory elements and a second horizontal plane including bottommost surfaces of the array of memory elements. As used herein, a “through-stack” element refers to an element that vertically extends through a memory level.
As used herein, a “semiconducting material” refers to a material having electrical conductivity in the range from 1.0×10−5 S/m to 1.0×105 S/m. As used herein, a “semiconductor material” refers to a material having electrical conductivity in the range from 1.0×10−5 S/m to 1.0 S/m in the absence of electrical dopants therein, and is capable of producing a doped material having electrical conductivity in a range from 1.0 S/m to 1.0×107 S/m upon suitable doping with an electrical dopant. As used herein, an “electrical dopant” refers to a p-type dopant that adds a hole to a valence band within a band structure, or an n-type dopant that adds an electron to a conduction band within a band structure. As used herein, a “conductive material” refers to a material having electrical conductivity greater than 1.0×105 S/m. As used herein, an “insulator material” or a “dielectric material” refers to a material having electrical conductivity less than 1.0×10−5 S/m. As used herein, a “heavily doped semiconductor material” refers to a semiconductor material that is doped with electrical dopant at a sufficiently high atomic concentration to become a conductive material either as formed as a crystalline material or if converted into a crystalline material through an anneal process (for example, from an initial amorphous state), i.e., to provide electrical conductivity greater than 1.0×105 S/m. A “doped semiconductor material” may be a heavily doped semiconductor material, or may be a semiconductor material that includes electrical dopants (i.e., p-type dopants and/or n-type dopants) at a concentration that provides electrical conductivity in the range from 1.0×10−5 S/m to 1.0×107 S/m. An “intrinsic semiconductor material” refers to a semiconductor material that is not doped with electrical dopants. Thus, a semiconductor material may be semiconducting or conductive, and may be an intrinsic semiconductor material or a doped semiconductor material. A doped semiconductor material may be semiconducting or conductive depending on the atomic concentration of electrical dopants therein. As used herein, a “metallic material” refers to a conductive material including at least one metallic element therein. All measurements for electrical conductivities are made at the standard condition.
A monolithic three-dimensional memory array is one in which multiple memory levels are formed above a single substrate, such as a semiconductor wafer, with no intervening substrates. The term “monolithic” means that layers of each level of the array are directly deposited on the layers of each underlying level of the array. In contrast, two dimensional arrays may be formed separately and then packaged together to form a non-monolithic memory device. For example, non-monolithic stacked memories have been constructed by forming memory levels on separate substrates and vertically stacking the memory levels, as described in U.S. Pat. No. 5,915,167 titled “Three-dimensional Structure Memory.” The substrates may be thinned or removed from the memory levels before bonding, but as the memory levels are initially formed over separate substrates, such memories are not true monolithic three-dimensional memory arrays. The substrate may include integrated circuits fabricated thereon, such as driver circuits for a memory device
The various three-dimensional memory devices of the embodiments of the present disclosure may include a monolithic three-dimensional NAND string memory device, and may be fabricated using the various embodiments described herein. The monolithic three-dimensional NAND string is located in a monolithic, three-dimensional array of NAND strings located over the substrate. At least one memory cell in the first device level of the three-dimensional array of NAND strings is located over another memory cell in the second device level of the three-dimensional array of NAND strings.
Generally, a semiconductor package (or a “package”) refers to a unit semiconductor device that may be attached to a circuit board through a set of pins or solder balls. A semiconductor package may include a semiconductor chip (or a “chip”) or a plurality of semiconductor chips that are bonded throughout, for example, by flip-chip bonding or another chip-to-chip bonding. A package or a chip may include a single semiconductor die (or a “die”) or a plurality of semiconductor dies. A die is the smallest unit that may independently execute external commands or report status. Typically, a package or a chip with multiple dies is capable of simultaneously executing as many number of external commands as the total number of dies therein. Each die includes one or more planes. Identical concurrent operations may be executed in each plane within a same die, although there may be some restrictions. In case a die is a memory die, i.e., a die including memory elements, concurrent read operations, concurrent write operations, or concurrent erase operations may be performed in each plane within a same memory die. In a memory die, each plane contains a number of memory blocks (or “blocks”), which are the smallest unit that may be erased by in a single erase operation. Each memory block contains a number of pages, which are the smallest units that may be selected for programming. A page is also the smallest unit that may be selected to a read operation.
A die may be in an isolated form (e.g., immediately after singulation from a structure including a plurality of dies), or may be connected to at least another die sharing a same substrate (such as a semiconductor wafer including a plurality of dies prior to singulation), or may be bonded to at least another die (for example, by metal-to-metal bonding among facing bonding pads or by an array of solder material portions located between two sets of bonding pads that face each other and embedded in different dies).
Referring to
A first etch stop dielectric layer 850 can be optionally formed over the top surface of the first device structure 840. The first etch stop dielectric layer 850 includes an etch stop dielectric material having a higher etch resistivity than the dielectric material to be subsequently deposited over the first etch stop dielectric layer 850. For example, the first etch stop dielectric layer 850 includes silicon nitride or a dielectric metal oxide such as aluminum oxide. The thickness of the first etch stop dielectric layer 850 can be in a range from 5 nm to 30 nm, although lesser and greater thicknesses can also be employed.
A first via-level dielectric layer 872 can be deposited over the top surface of the first etch stop dielectric layer 850. The first via-level dielectric layer 872 includes a dielectric material such as undoped silicate glass (i.e., silicon oxide), a doped silicate glass, or organosilicate glass. The thickness of the first via-level dielectric layer 872 can be in a range from 100 nm to 600 nm, although lesser and greater thicknesses can also be employed.
First via cavities 81 can be formed through the first via-level dielectric layer 872. For example, a photoresist layer can be applied over the top surface of the first via-level dielectric layer 872, and can be lithographically patterned to form discrete openings that overlie the electrically active nodes within the first device structure 840. An anisotropic etch process can be performed to form the first via cavities 81 underneath the discrete openings in the patterned photoresist layer. The photoresist layer can be removed, for example, by ashing.
Referring to
Excess portions of the at least one conductive material can be removed from above the horizontal plane including the top surface of the first via-level dielectric layer 872 by a planarization process. The planarization process can include a recess etch process and/or a chemical mechanical planarization process. Each remaining portion of the at least one conductive material comprises a conductive via structure, which is herein referred to as a first conductive via structure 88V. The first conductive via structure 88V can include a via-level metallic liner 82V, an optional via-level metallic seed layer 84V, and a via-level metallic fill portion 86V. The via-level metallic liner 82V is a remaining patterned portion of the continuous via-level metallic liner. The via-level metallic seed layer 84V is a remaining patterned portion of the continuous via-level metallic seed layer. The via-level metallic fill portion 86V is a remaining patterned portion of the continuous via-level metallic fill layer. Each contiguous combination of a via-level metallic seed layer 84V and a via-level metallic fill portion 86V constitutes a via-level metallic fill material portion (84V, 86V). Thus, each first conductive via structure 88V includes a combination of a via-level metallic liner 82V and a via-level metallic fill material portion (84V, 86V).
Referring to
A photoresist layer (not shown) can be applied over the top surface of the first pad-level dielectric layer 874, and can be lithographically patterned to form pad-shaped openings overlying a respective one of the first conductive via structures 88V. An anisotropic etch process can be performed employing the patterned photoresist layer as an etch mask layer. The pattern in the photoresist layer can be transferred through the first pad-level dielectric layer 874 by an anisotropic etch process to form first pad cavities 83. The first via-level dielectric layer 872 can be employed as an etch stop layer for the anisotropic etch process. A top surface of at least one first conductive via structure 88V can be physically exposed at the bottom of each first pad cavity 83. The maximum lateral dimension of each pad cavity 83 can be in a range from 2 microns to 100 microns, such as from 4 microns to 50 microns, although lesser and greater lateral dimensions can also be employed. Each first pad cavity 83 can have a horizontal cross-sectional shape of a polygon (such as a rectangle), a rounded polygon, a circle, an ellipse, or any other curvilinear two-dimensional shape having a closed periphery.
The sidewalls of the first pad cavities 83 can comprise surface of the material of the first pad-level dielectric layer 874, which may be a silicon carbide nitride material. The sidewalls of the first pad cavities 83 can be vertical, or may have a taper angle that is less than 20 degrees relative to the vertical direction. For example, the taper angle may be in a range from 0.1 degree to 5 degrees. A top surface of the first via-level dielectric layer 872 and a top surface of a first conductive via structure 88V can be physically exposed at the bottom of each first pad cavity 83.
Referring to
Referring to
Referring to
Referring to
Referring to
The pad-level metallic liners 82P are formed in the first pad cavities 83. Each of the pad-level metallic liners 82P is vertically recessed from the horizontal plane HP including the top surface of the first pad-level dielectric layer 874 toward the first substrate 808. Because the top surface of the first pad-level dielectric layer 874 is distal from the first substrate 808, the top surface of the first pad-level dielectric layer 874 is herein referred to as a horizontal distal surface of the first pad-level dielectric layer 874. In one embodiment, the pad-level metallic liners 82P comprise, and/or consist of, a metallic nitride material.
Referring to
Referring to
Referring to
First bonding structures 88 are formed in the first via-level dielectric layer 872 and in the first pad-level dielectric layer 874. Each first bonding structure 88 comprises a respective first metallic bonding pad 88P and a respective first conductive via structure 88V. Each of the first bonding structures comprises a pad-level metallic fill material portion (84P, 86P) having a horizontal distal surface that is located within a horizontal plane HP including a horizontal distal surface of the first pad-level dielectric layer 874, and a pad-level metallic liner 82P laterally surrounding the pad-level metallic fill material portion (84P, 86P) and is vertically spaced from the horizontal plane HP by a vertical recess distance vrd. Each contiguous combination of a pad-level metallic seed layer 84P and a pad-level metallic fill portion 86P constitutes a pad-level metallic fill material portion (84P, 86P). Thus, each first metallic bonding pad 88P includes a combination of a pad-level metallic liner 82P and a pad-level metallic fill material portion (84P, 86P).
The pad-level metallic fill material portions (84P, 86P) are formed in remaining volumes of the first pad cavities 83 that remain after formation of the pad-level metallic liners 82P. The pad-level metallic fill material portions (84P, 86P) can be formed directly on upper portions of the sidewalls of the first pad cavities 83. In one embodiment, the pad-level metallic fill material portions (84P, 86P) comprise copper. Each pad-level metallic liner 82P comprises a horizontally-extending portion contacting a horizontal surface of a pad-level metallic fill material portion (84P, 86P), and a vertically-extending portion adjoined to a periphery of the horizontally-extending portion and contacting a sidewall of the pad-level metallic fill material portion (84P, 86P). In one embodiment, the entirety of a sidewall of each pad-level metallic fill material portion (84P, 86P) may contact the first pad-level dielectric layer 874.
Presence of a metallic liner in proximity to a metallic fill material can cause edge recesses at a periphery of a remaining portion of the metallic fill material adjacent to the metallic liner. For example, if copper filling a cavity lined with a metallic liner material (such as TiN) is planarized employing a chemical mechanical planarization process, then a remaining portion of copper may have a peripheral recess that adjoins remaining sidewalls of the metallic liner material. According to an aspect of the present disclosure, vertical recessing of the pad-level metallic liners 82P below the horizontal plane HP including the top surface of the first pad-level dielectric layer 874 has the effect of reducing or preventing formation of such collaterally formed recesses in the pad-level metallic fill material portions (84P, 86P) that remain after the planarization process. In other words, by vertically recessing the pad-level metallic liners 82P relative to the top surface of the first pad-level dielectric layer 874, undesirable recesses at peripheral regions of the pad-level metallic fill material portions (84P, 86P) can be reduced or avoided during the planarization process that removes excess portions of the metallic fill materials from above the horizontal plane including the top surface of the first pad-level dielectric layer 874. Furthermore, if the first pad-level dielectric layer 874 includes a dielectric copper diffusion barrier material, such as a silicon carbide nitride, then this dielectric diffusion barrier material may prevent or reduce copper migration into the first pad-level dielectric layer 874. Elimination or reduction of recesses and copper migration reduces or prevents electromigration and/or stress induced voids in the copper containing materials of the pad-level metallic fill material portions (84P, 86P) after formation of a bonded assembly and during operation of the bonded assembly.
Generally, the first semiconductor die 800 can include a first pad-level dielectric layer 874 overlying the at least one first semiconductor device in the first device structure 840, and first bonding structures comprising a respective first metallic bonding pad 88P embedded in the first pad-level dielectric layer 874. Each of the first bonding structures can comprise a metallic fill material portion (such as a pad-level metallic fill material portion (84P, 86P) having a horizontal distal surface that is located within a horizontal plane HP including a horizontal distal surface of the first pad-level dielectric layer 874, and a metallic liner (such as a pad-level metallic liner 82P) laterally surrounding the metallic fill material portion and is vertically spaced from the horizontal plane HP by a vertical recess distance vrd. As used herein, a “distal surface” refers to a surface that is distal from a reference structure, such as the first substrate 808, and a “proximal surface” refers to a surface that is proximal to the reference structure.
In one embodiment, the metallic liner (such as the pad-level metallic liner 82P) comprises: a horizontally-extending portion contacting a horizontal surface of the metallic fill material portion (such as the pad-level metallic fill material portions (84P, 86P)), and a vertically-extending portion adjoined to a periphery of the horizontally-extending portion and contacting a sidewall of the metallic fill material portion (such as the pad-level metallic fill material portion (84P, 86P)).
In one embodiment, a sidewall of the metallic fill material portion (such as the pad-level metallic fill material portion (84P, 86P)) has a stepped profile such that a laterally-extending segment LES of the sidewall connects a first vertically-extending segment VES1 of the sidewall that extends to the horizontal plane HP to a second vertically-extending segment VES2 of the sidewall that extends to the horizontally-extending portion HS of the metallic liner (such as the pad-level metallic liner 82P).
In one embodiment, the laterally-extending segment LES of the metallic fill material portion (such as the pad-level metallic fill material portion (84P, 86P)) contacts a distal surface of the metallic liner (such as the pad-level metallic liner 82P) that is most distal from the first substrate 808 of all surfaces of the metallic liner. In one embodiment, the vertical recess distance vrd can be in a range from 10% to 90% of a vertical distance between the horizontal plane HP and a proximal surface of the horizontally-extending portion of the metallic liner (which is located within a horizontal interface between the pad-level metallic liner 82P and the first via-level dielectric layer 872).
In one embodiment, a first vertically-extending segment VES1 of a stepped sidewall of the metallic fill material portion (such as the pad-level metallic fill material portion (84P, 86P)) and an outer sidewall of the metallic liner (such as the pad-level metallic liner 82P) are located within a two-dimensional plane that is vertical or has a taper angle less than 20 degrees relative to a vertical direction, and a second vertically-extending segment VES2 the stepped sidewall of the metallic fill material portion contacts an inner sidewall of the metallic liner, and is parallel to the two-dimensional plane.
In one embodiment, the metallic liners (such as the pad-level metallic liners 82P) comprise a metallic nitride material, and the metallic fill material portions (such as the pad-level metallic fill material portions (84P, 86P)) comprise copper. In one embodiment, a sidewall of the metallic fill material portion (such as the pad-level metallic fill material portion (84P, 86P)) contacts the first pad-level dielectric layer 874, and a sidewall of the metallic liner (such as the pad-level metallic liners 82P) contacts the first pad-level dielectric layer 874. In one embodiment, the first pad-level dielectric layer 874 comprises silicon carbide nitride. In one embodiment, conductive via structures (such as first conductive via structures 88V) can underlie the first bonding structures 88P, and can contact a horizontal surface of a respective one of the first bonding structures 88P.
The sidewalls of the first metallic bonding pads 88P can comprise surfaces of the material of the first pad-level dielectric layer 874, which may be surfaces of a silicon carbide nitride material. The sidewalls of the first metallic bonding pads 88P can be vertical, or may have a taper angle that is less than 20 degrees relative to the vertical direction. For example, the taper angle may be in a range from 0.1 degree to 5 degrees.
Referring to
The second etch stop dielectric layer 950 can have the same material composition and the same thickness range as the first etch stop dielectric layer 850. The second via-level dielectric layer 972 can have the same material composition and the same thickness range as the first via-level dielectric layer 872. The second pad-level dielectric layer 974 can have the same material composition and the same thickness range as the first pad-level dielectric layer 874. The via-level metallic liners 92V in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the via-level metallic liners 82V in the first semiconductor die 800. The via-level metallic seed layers 94V in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the via-level metallic seed layers 84V in the first semiconductor die 800. The via-level metallic fill portions 96V in the second semiconductor die 900 can include any material that can be employed for the via-level metallic fill portions 86V in the first semiconductor die 800. The pad-level metallic liners 92P in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the pad-level metallic liners 82P in the first semiconductor die 800. The pad-level metallic seed layers 94P in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the pad-level metallic seed layers 84P in the first semiconductor die 800. The pad-level metallic fill portions 96P in the second semiconductor die 900 can include any material that can be employed for the pad-level metallic fill portions 86P in the first semiconductor die 800. The portions of the second semiconductor die 900 located above the second semiconductor structure 940 may be formed employing the same manufacturing methods that are employed to form the portions of the first semiconductor die 800 above the first semiconductor structure 840.
As discussed above, presence of a metallic liner in proximity to a metallic fill material may cause edge recesses at a periphery of a remaining portion of the metallic fill material adjacent to the metallic liner. According to an aspect of the present disclosure, vertical recessing of the pad-level metallic liners 92P below the horizontal plane including the top surface of the second pad-level dielectric layer 974 has the effect of reducing or preventing formation of such collaterally formed grooves in the pad-level metallic fill material portions (94P, 96P) that remain after the planarization process. Elimination or reduction of recessed regions from the polished surfaces of the pad-level metallic fill material portions (94P, 96P) may reduce or prevent electromigration and/or stress induced voids in the copper containing material of the pad-level metallic fill material portions (94P, 96P) after formation of a bonded assembly and during usage of the bonded assembly.
Referring to
A first etch stop dielectric layer 850 can be optionally formed over the top surface of the first device structure 840. The first etch stop dielectric layer 850 can be the same as in the first embodiment. A first via-level dielectric layer 872 can be deposited over the top surface of the first etch stop dielectric layer 850. The first via-level dielectric layer 872 can be the same as in the first embodiment. A first pad-level dielectric layer 874 can be deposited over the first via-level dielectric layer 872. The first pad-level dielectric layer 874 may include a dielectric copper diffusion barrier material, such as a silicon carbide nitride (i.e., silicon carbonitride, SiCN) material. The first pad-level dielectric layer 874 can be deposited by a conformal or a non-conformal deposition process. For example, the first pad-level dielectric layer 874 can be formed by a plasma-enhanced chemical vapor deposition process. The thickness of the first pad-level dielectric layer 874 can be in a range from 100 nm to 600 nm, although lesser and greater thicknesses can also be employed.
A first photoresist layer (not shown) can be applied over the top surface of the first pad-level dielectric layer 874, and can be lithographically patterned to form via cavity shaped openings. An anisotropic etch process can be performed employing the patterned first photoresist layer as an etch mask layer. The pattern in the first photoresist layer can be transferred through the first pad-level dielectric layer 874 and the first via-level dielectric layer 872 to form first via cavities 81. The first etch stop dielectric layer 850 can be employed as an etch stop layer for the anisotropic etch process. The etch may then be continued with a different etching gas or liquid through the first etch stop dielectric layer 850 to the first device structure 840. The maximum lateral dimension of each first via cavity 81 can be in a range from 2 microns to 100 microns, such as from 4 microns to 50 microns, although lesser and greater lateral dimensions can also be employed. Each first via cavity 81 can have a horizontal cross-sectional shape of a polygon (such as a rectangle), a rounded polygon, a circle, an ellipse, or any other curvilinear two-dimensional shape having a closed periphery. The first photoresist layer can be removed, for example, by ashing.
The sidewalls of the first via cavities 81 can comprise surface of the material of the first pad-level dielectric layer 874, which may be a silicon carbide nitride material, the first pad-level dielectric layer 874, which may be a silicon oxide layer, and optionally the first etch stop dielectric layer 850, which may be a silicon nitride material. The sidewalls of the first via cavities 81 can be vertical, or may have a taper angle that is less than 20 degrees relative to the vertical direction. For example, the taper angle may be in a range from 0.1 degree to 5 degrees. A top surface of the first device structure 840 can be physically exposed at the bottom of each first via cavity 81.
Referring to
Referring to
Referring to
Referring to
Referring to
Referring to
The pad-and-via-level metallic liners 82 are formed in the combined volumes of the first pad cavities 83 and the first via cavities 81. Each of the pad-and-via-level metallic liners 82 is vertically recessed from the horizontal plane HP including the top surface of the first pad-level dielectric layer 874 toward the first substrate 808. Because the top surface of the first pad-level dielectric layer 874 is distal from the first substrate 808, the top surface of the first pad-level dielectric layer 874 is herein referred to as a horizontal distal surface of the first pad-level dielectric layer 874. In one embodiment, the pad-and-via-level metallic liners 82 comprise, and/or consist of, a metallic nitride material.
Referring to
Referring to
Referring to
Each first bonding structure 88 comprises a respective first metallic bonding pad 88P. Each of the first bonding structures 88 comprises a pad-and-via-level metallic fill material portion (84, 86) having a horizontal distal surface that is located within a horizontal plane HP including a horizontal distal surface of the first pad-level dielectric layer 874, and a pad-and-via-level metallic liner 82 laterally surrounding the pad-and-via-level metallic fill material portion (84, 86) and is vertically spaced from the horizontal plane HP by a vertical recess distance vrd. Each contiguous combination of a pad-and-via-level metallic seed layer 84 and a pad-and-via-level metallic fill portion 86 constitutes a pad-and-via-level metallic fill material portion (84, 86). Thus, each first metallic bonding pad 88P includes a combination of a pad-and-via-level metallic liner 82 and a pad-and-via-level metallic fill material portion (84, 86).
The pad-and-via-level metallic fill material portions (84, 86) are formed in remaining volumes of the first pad cavities 83 and the first via cavities 81 that remain after formation of the pad-and-via-level metallic liners 82. The pad-and-via-level metallic fill material portions (84, 86) can be formed directly on upper portions of the sidewalls of the first pad cavities 83. In one embodiment, the pad-and-via-level metallic fill material portions (84, 86) comprise copper. Each pad-and-via-level metallic liner 82 comprises a horizontally-extending portion HS contacting a horizontal surface of a pad-and-via-level metallic fill material portion (84, 86), and a vertically-extending portion adjoined to a periphery of the horizontally-extending portion and contacting a sidewall of the pad-and-via-level metallic fill material portion (84, 86). In one embodiment, the entirety of a sidewall of each pad-level metallic fill material portion (84, 86) may contact the first pad-level dielectric layer 874.
Generally, the first semiconductor die 800 can include a first pad-level dielectric layer 874 overlying the at least one first semiconductor device in the first device structure 840, and first bonding structures comprising a respective first metallic bonding pad 88P embedded in the first pad-level dielectric layer 874 and the first via-level dielectric layer 872. Each of the first bonding structures can comprise a metallic fill material portion (such as a pad-and-via-level metallic fill material portion (84, 86)) having a horizontal distal surface that is located within a horizontal plane HP including a horizontal distal surface of the first pad-level dielectric layer 874, and a metallic liner (such as a pad-and-via-level metallic liner 82) laterally surrounding the metallic fill material portion and is vertically spaced from the horizontal plane HP by a vertical recess distance vrd.
In one embodiment, the metallic liner (such as the pad-and-via-level metallic liner 82) comprises: a horizontally-extending portion HS contacting a horizontal surface of the metallic fill material portion (such as the pad-and-via-level metallic fill material portions (84, 86)), and a vertically-extending portion adjoined to a periphery of the horizontally-extending portion and contacting a sidewall of the metallic fill material portion (such as the pad-and-via-level metallic fill material portion (84, 86)).
In one embodiment, a sidewall of the metallic fill material portion (such as the pad-and-via-level metallic fill material portion (84, 86)) has a stepped profile such that a laterally-extending segment LES of the sidewall connects a first vertically-extending segment VES1 of the sidewall that extends to the horizontal plane HP to a second vertically-extending segment VES2 of the sidewall that extends to the horizontally-extending portion HS of the metallic liner (such as the pad-and-via-level metallic liner 82).
In one embodiment, the laterally-extending segment LES of the metallic fill material portion (such as the pad-and-via-level metallic fill material portion (84, 86)) contacts a distal surface of the metallic liner (such as the pad-and-via-level metallic liner 82) that is most distal from the first substrate 808 among all surfaces of the metallic liner. In one embodiment, the vertical recess distance vrd can be in a range from 10% to 90% of a vertical distance between the horizontal plane HP and a proximal surface of the horizontally-extending portion of the metallic liner (which is located within a horizontal interface between the pad-and-via-level metallic liner 82 and the first via-level dielectric layer 872).
In one embodiment, a first vertically-extending segment VES1 of a stepped sidewall of the metallic fill material portion (such as the pad-and-via-level metallic fill material portion (84, 86)) and an outer sidewall of the metallic liner (such as the pad-and-via-level metallic liner 82) are located within a two-dimensional plane that is vertical or has a taper angle less than 20 degrees relative to a vertical direction, and a second vertically-extending segment VES2 the stepped sidewall of the metallic fill material portion contacts an inner sidewall of the metallic liner, and is parallel to the two-dimensional plane.
In one embodiment, the metallic liners (such as the pad-and-via-level metallic liners 82) comprise a metallic nitride material, and the metallic fill material portions (such as the pad-and-via-level metallic fill material portions (84, 86)) comprise copper. In one embodiment, a sidewall of the metallic fill material portion (such as the pad-and-via-level metallic fill material portion (84, 86)) contacts the first pad-level dielectric layer 874, and a sidewall of the metallic liner (such as the pad-and-via-level metallic liners 82) contacts the first pad-level dielectric layer 874. In one embodiment, the first pad-level dielectric layer 874 comprises silicon carbide nitride. In one embodiment, conductive via structures (such as first conductive via structures 88V) can underlie the first metallic bonding pads 88P, and can contact a horizontal surface of a respective one of the first metallic bonding pads 88P.
The sidewalls of the first metallic bonding pads 88P can contact surfaces of the first pad-level dielectric layer 874, which may include a silicon carbide nitride material. The sidewalls of the first metallic bonding pads 88P can be vertical, or may have a taper angle that is less than 20 degrees relative to the vertical direction. For example, the taper angle may be in a range from 0.1 degree to 5 degrees.
In one embodiment, the first bonding structures 88 can comprise an integrated pad and conductive via structure that includes a first conductive via structure 88V (i.e., a portion of a first bonding structure 88 located under the horizontal plane including the interface between the first via-level dielectric layer 872 and the first pad-level dielectric layer 874) that vertically protrudes from one of the first metallic bonding pads 88P. A metallic liner (such as a pad-and-via-level metallic liner 82) within each of the first bonding structures 88 vertically protrudes into a respective first conductive via structure 88V. A metallic fill material portion (such as a pad-and-via-level metallic fill material portion (84, 86)) within each of the first bonding structures 88 vertically protrudes into a respective first conductive via structure 88V.
Referring to
The second etch stop dielectric layer 950 can have the same material composition and the same thickness range as the first etch stop dielectric layer 850. The second via-level dielectric layer 972 can have the same material composition and the same thickness range as the first via-level dielectric layer 872. The second pad-and-via-level dielectric layer 974 can have the same material composition and the same thickness range as the first pad-level dielectric layer 874. The pad-and-via-level metallic liners 92 in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the pad-and-via-level metallic liners 82 in the first semiconductor die 800. The pad-and-via-level metallic seed layers 94 in the second semiconductor die 900 can include any material that can be employed for, and can have a thickness within a same thickness range as, the pad-and-via-level metallic seed layers 84 in the first semiconductor die 800. The pad-and-via-level metallic fill portions 96 in the second semiconductor die 900 can include any material that can be employed for the pad-and-via-level metallic fill portions 86 in the first semiconductor die 800. The portions of the second semiconductor die 900 located above the second semiconductor structure 940 may be formed employing the same manufacturing methods that are employed to form the portions of the first semiconductor die 800 above the first semiconductor structure 840.
In one embodiment, the second bonding structures 98 can comprise an integrated pad and conductive via structure that includes a second conductive via structure 98V (i.e., a portion of a second bonding structure 98 located under the horizontal plane including the interface between the second via-level dielectric layer 972 and the second pad-level dielectric layer 974) that vertically protrudes downward from one of the second metallic bonding pads 98P. A metallic liner (such as a pad-and-via-level metallic liner 92) within each of the second bonding structures 98 vertically protrudes into a respective second conductive via structure 98V. A metallic fill material portion (such as a pad-and-via-level metallic fill material portion (84, 96)) within each of the second bonding structures 98 vertically protrudes into a respective second conductive via structure 98V.
Referring to
Referring to
Generally, the second semiconductor devices 920 may comprise any semiconductor device known in the art. In one embodiment, the second semiconductor die 900 comprises a memory die, and may include memory devices, such as a three-dimensional NAND memory device. In an illustrative example, the second semiconductor devices 920 may include a vertically alternating stack of insulating layers 32 and electrically conductive layers 46, and a two-dimensional array of memory openings vertically extending through the vertically alternating stack (32, 46). The electrically conductive layers 46 may comprise word lines of the three-dimensional NAND memory device.
A memory opening fill structure 58 may be formed within each memory opening. A memory opening fill structure 58 may include a memory film and a vertical semiconductor channel contacting the memory film. The memory film may include a blocking dielectric, a tunneling dielectric and a charge storage material located between the blocking and tunneling dielectric. The charge storage material may comprise charge trapping layer, such as a silicon nitride layer, or a plurality of discrete charge trapping regions, such as floating gates or discrete portions of a charge trapping layer. In this case, each memory opening fill structure 58 and adjacent portions of the electrically conductive layers 46 constitute a vertical NAND string. Alternatively, the memory opening fill structures 58 may include any type of non-volatile memory elements such as resistive memory elements, ferroelectric memory elements, phase change memory elements, etc. The memory device may include an optional horizontal semiconductor channel layer 10 connected to the bottom end of each vertical semiconductor channel, and an optional dielectric spacer layer 910 that provides electrical isolation between the second substrate 908 and the horizontal semiconductor channel layer 10.
The electrically conductive layers 46 may be patterned to provide a terrace region in which each overlying electrically conductive layer 46 has a lesser lateral extent than any underlying electrically conductive layer 46. Contact conductive via structures (not shown) may be formed on the electrically conductive layers 46 in the terrace region to provide electrical connection to the electrically conductive layers 46. Dielectric material portions 65 may be formed around each vertically alternating stack (32, 46) to provide electrical isolation among neighboring vertically alternating stacks (32, 46).
The second dielectric material layers (290, 930) may include second contact-level dielectric layers 290 embedding contact conductive via structures (not expressly shown) and bit lines 978, and second interconnect-level dielectric layers 930 that embed a subset of the second metal interconnect structures 970 located above the second contact-level dielectric layers 290. The second dielectric material layers (290, 930) laterally extend along horizontal directions that are parallel to the top surface of the second substrate 908.
The bit lines 978 are a subset of the second metal interconnect structures 970 and may electrically contact drain regions located above the semiconductor channel at the top of the memory opening fill structures 58. The contact conductive via structures contact various nodes of the second semiconductor devices. Interconnect metal lines and interconnect metal conductive via structures, which are subsets of the second metal interconnect structures 970, may be embedded in the second interconnect-level dielectric layers 930. The second metal interconnect structures 970 may be located within the second interconnect-level dielectric layers 930. Each of the second contact-level dielectric layers 290 and the second interconnect-level dielectric layers 930 may include a dielectric material such as undoped silicate glass, a doped silicate glass, organosilicate glass, silicon nitride, a dielectric metal oxide, or a combination thereof. The second bonding structures 98 may have the second configuration illustrated in
Generally, the second semiconductor devices 920 in the second device structure 940 of the second semiconductor die 900 may comprise any semiconductor device that may be operated in conjunction with the first semiconductor devices in the first device structure 840 of the first semiconductor die 800 to provide enhanced functionality. In one embodiment, one of the first semiconductor die 800 and the second semiconductor die 900 can comprise a memory die including a three-dimensional array of memory elements, another of the first semiconductor die 800 and the second semiconductor die 900 comprises a logic die including a logic circuit configured to control operation of memory elements within the three-dimensional array of memory elements. In one embodiment, the first semiconductor die 800 comprises a logic die and the second semiconductor die 900 comprises a memory die. The logic die can include a support circuitry (i.e., driver or peripheral circuitry) for operation of memory devices (such as a three-dimensional array of memory elements, including a three-dimensional NAND memory device) within the memory die.
Referring to
Referring to
An anneal process at an elevated temperature to induce metal-to-metal bonding between each mating pair of a first metallic bonding pad 88P and a second metallic bonding pad 98P. If the pad-level metallic fill material portions (84P, 86P) of the first metallic bonding pads 88P and the pad-level metallic fill material portions (94P, 96P) of the second metallic bonding pads 98P include copper, the elevated temperature may be in a range from 200 degrees Celsius to 400 degrees Celsius. Metal-to-metal bonding is formed between each mating pair of a first metallic bonding pad 88P and a second metallic bonding pad 98P at a respective horizontal bonding interface. Thus, each of the second metallic bonding pads 98P can be bonded to a respective one of the first metallic bonding pads 88P.
Generally, the first bonding structures 88 comprise a respective first metallic bonding pad 88P embedded in the first pad-level dielectric layer 874 and bonded to a respective one of the second metallic bonding pads 98P. The second bonding structures 98 comprise a respective second metallic bonding pad 98P embedded in the second pad-level dielectric layer 974 and bonded to a respective one of the first metallic bonding pads 88P. Each of the first bonding structures 88 comprises a metallic fill material portion (such as a pad-level metallic fill material portion (84P, 86P) or a pad-and-via-level metallic fill material portion (84, 86)), and a respective metallic liner (such as a pad-level metallic liner 82P or a pad-and-via-level metallic liner 82) laterally surrounding the respective metallic fill material portion and is vertically spaced from the horizontal plane including the bonding interfaces by a vertical recess distance. Each of the second bonding structures 98 comprises a respective additional metallic fill material portion (such as a pad-level metallic fill material portion (94P, 96P) or a pad-and-via-level metallic fill material portion (94, 96)) that is bonded to a respective one of the metallic material portions (such as a pad-level metallic fill material portion (84P, 86P) or a pad-and-via-level metallic fill material portion (84, 86)) at the horizontal plane including the bonding interfaces, and a respective additional metallic liner (such as a pad-level metallic liner 92P or a pad-and-via-level metallic liner 92) laterally surrounding the respective additional metallic fill material portion and is vertically spaced from the horizontal plane including the bonding interfaces by another vertical recess distance.
The various embodiments of the present disclosure can be employed to form a bonded assembly including a self-aligned diffusion barrier structure comprising the pad-level dielectric layers (874, 974). Specifically, the entire periphery of each metallic fill material portion {(84P, 86P), (84, 86), (94P, 96P), (94, 96)} can be laterally contacted by a combination of a respective pad-level dielectric layer (874, 974) and a respective metallic liner (82P, 82, 92P, 92) without any gap. The pad-level dielectric layer (874, 974) can include a dielectric diffusion barrier material such as a silicon nitride carbide material, and can function as a dielectric diffusion barrier structure. The metallic liners (82P, 82, 92P, 92) function as a metallic diffusion barrier material for the metallic fill material portions {(84P, 86P), (84, 86), (94P, 96P), (94, 96)}. By vertically recessing the metallic liners (82P, 82, 92P, 92) relative to the top surface of a pad-level dielectric layer (874, 974), undesirable recesses at peripheral portions of the metallic fill material portions {(84P, 86P), (84, 86), (94P, 96P), (94, 96)} can be avoided during the planarization process that removes excess portions of the metallic fill materials from above the horizontal plane including the top surface of the pad-level dielectric layer (874, 974).
Furthermore, since the first pad-level dielectric layer 874 and the second pad-level dielectric layer 974 can include a dielectric diffusion barrier material such a silicon carbide nitride, the diffusion of the metallic material of the metallic fill material portions {(84P, 86P), (84, 86), (94P, 96P), (94, 96)}, such as copper, through the first pad-level dielectric layer 874 and/or the second pad-level dielectric layer 974 can be prevented or suppressed. If the respective bonding pads of the first and second dies are partially misaligned, as shown in
Although the foregoing refers to particular embodiments, it will be understood that the disclosure is not so limited. It will occur to those of ordinary skill in the art that various modifications may be made to the disclosed embodiments and that such modifications are intended to be within the scope of the disclosure. Compatibility is presumed among all embodiments that are not alternatives of one another. The word “comprise” or “include” contemplates all embodiments in which the word “consist essentially of” or the word “consists of” replaces the word “comprise” or “include,” unless explicitly stated otherwise. Where an embodiment using a particular structure and/or configuration is illustrated in the present disclosure, it is understood that the present disclosure may be practiced with any other compatible structures and/or configurations that are functionally equivalent provided that such substitutions are not explicitly forbidden or otherwise known to be impossible to one of ordinary skill in the art. All of the publications, patent applications and patents cited herein are incorporated herein by reference in their entirety.
Number | Name | Date | Kind |
---|---|---|---|
5915167 | Leedy | Jun 1999 | A |
8492265 | Yang | Jul 2013 | B2 |
9027821 | Di Cioccio | May 2015 | B2 |
9224704 | Landru | Dec 2015 | B2 |
9728521 | Tsai | Aug 2017 | B2 |
10115681 | Ariyoshi | Oct 2018 | B1 |
10283493 | Nishida | May 2019 | B1 |
10354980 | Mushiga et al. | Jul 2019 | B1 |
10354987 | Mushiga et al. | Jul 2019 | B1 |
10381322 | Azuma et al. | Aug 2019 | B1 |
10381362 | Cui et al. | Aug 2019 | B1 |
10510738 | Kim et al. | Dec 2019 | B2 |
10685875 | Hatano | Jun 2020 | B2 |
20040251550 | Yoda | Dec 2004 | A1 |
20050151224 | Abe | Jul 2005 | A1 |
20070205482 | Yang | Sep 2007 | A1 |
20120068355 | Aoki | Mar 2012 | A1 |
20120171818 | Barth | Jul 2012 | A1 |
20140061914 | Dyer | Mar 2014 | A1 |
20140117546 | Liu | May 2014 | A1 |
20160013160 | Chun | Jan 2016 | A1 |
20170069593 | Chou et al. | Mar 2017 | A1 |
20170358553 | Kim | Dec 2017 | A1 |
20190109042 | Katkar | Apr 2019 | A1 |
20190221557 | Kim | Jul 2019 | A1 |
20190252361 | Nishida | Aug 2019 | A1 |
Number | Date | Country |
---|---|---|
10-2016-0007240 | Jan 2016 | KR |
10-2017-0139342 | Dec 2017 | KR |
Entry |
---|
U.S. Appl. No. 16/231,752, filed Dec. 24, 2018, SanDisk Technologies LLC. |
U.S. Appl. No. 16/242,216, filed Jan. 8, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/248,923, filed Jan. 16, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/249,423, filed Jan. 16, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/255,413, filed Jan. 23, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/269,301, filed Feb. 13, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/274,687, filed Feb. 13, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/275,668, filed Feb. 14, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/278,372, filed Feb. 18, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/284,502, filed Feb. 25, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/288,656, filed Feb. 28, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/291,220, filed Mar. 4, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/291,457, filed Mar. 4, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/291,504, filed Mar. 4, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/291,577, filed Mar. 4, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/295,292, filed Mar. 7, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/372,908, filed Apr. 2, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/385,010, filed Apr. 16, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/391,632, filed Apr. 23, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/409,593, filed May 10, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/417,913, filed May 21, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/440,183, filed Jun. 13, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/521,849, filed Jul. 25, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/523,029, filed Jul. 26, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/552,089, filed Aug. 27, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/589,404, filed Oct. 1, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/660,177, filed Oct. 22, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/666,522, filed Oct. 29, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/671,025, filed Oct. 31, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/682,848, filed Nov. 13, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/694,340, filed Nov. 25, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/694,400, filed Nov. 25, 2019, SanDisk Technologies LLC. |
U.S. Appl. No. 16/694,438, filed Nov. 25, 2019, SanDisk Technologies LLC. |
Notification of Transmittal of the International Search Report and Written Opinion of the International Search Authority for International Patent Application No. PCT/US2020/026182, dated Sep. 18, 2020, 9 pages. |
Number | Date | Country | |
---|---|---|---|
20210202382 A1 | Jul 2021 | US |