This application is a translation of and claims the priority benefit of French patent application number 12/51362, filed on Feb. 14, 2012, entitled “CHIP ASSEMBLY SYSTEM,” which is hereby incorporated by reference to the maximum extent allowable by law.
The present disclosure relates to the field of three-dimensional integrated circuits. Indeed, to increase the integration level of semiconductor components, there is a tendency to form integrated circuits made of a stack of chips.
Opposite pads Pi1 and Pi2 of each of semiconductor elements W1, W2 must then be interconnected. This connection between pads may be achieved in various ways. For example, connection between pads may be achieved by conductive pillars or bumps, each bump or pillar being welded to two opposite pads.
Another technique which has developed to form this interconnection between opposite pads comprises very carefully polishing the opposite surfaces of two semiconductor elements W1, W2 and directly applying the two opposite surfaces against each other. An anneal is then carried out, for example at temperatures approximately ranging from 300 to 400° C. As a result, with no addition of external material (bump, pillar, welding . . . ), a connection between opposite surfaces is obtained. The bonding between the copper surfaces of opposite pads Pi1 and Pi2 results from the anneal, while the opposite insulating surfaces bond to each other by molecular bonding.
However, as illustrated in
To solve this problem, FR2963158 and US2011/084403 propose to change the SiO2 layer in which the copper pads are formed to a layer of a material in which copper does not diffuse. This solution necessitates an important change in the manufacturing steps of the wafers.
There thus is a need to improve procedures of assembly of semiconductor wafers while keeping the advantages of the previously-described simple and direct assembly.
To fulfill this need, an embodiment provides an assembly of semiconductor wafers/chips wherein the adjacent surfaces of two wafers/chips each comprise a silicon oxide layer having copper pads formed therein, wherein the silicon oxide layer is coated, outside of regions in which the copper pads are formed, with a silicon nitride or silicon carbon nitride layer thinner than the thickness of the copper pads.
According to an embodiment, the opposite surfaces of the copper pads are nitrided-silicided.
According to an embodiment, the opposite surfaces of the copper pads are coated with CoWP.
According to an embodiment, the pads are regularly distributed on each of the chips/wafers, at least some of the pads being electrically unconnected.
According to an embodiment, several first chips are associated with a same second chip.
According to an embodiment, the second chip belongs to a semiconductor wafer comprising an assembly of second chips.
The foregoing and other features and benefits will be discussed in detail in the following non-limiting description of specific embodiments in connection with the accompanying drawings.
For clarity, the same elements have been designated with the same reference numerals in the different drawings and, further, as usual in the representation of integrated circuits, the various drawings are not to scale.
In this embodiment, the pads are now formed in a silicon oxide layer covered with an insulating layer 20, 21 of a material having, on the one hand, like silicon oxide, the advantage that the two opposite polished surfaces bond to each other by molecular bonding and, on the other hand, the advantage that copper is not capable of diffusing therein. A preferred example of such a material is silicon nitride (Si3N4) or SiCN.
Other types of barrier layers may be used, for example, a CoWP layer.
As a dimensional example, it should be noted that each of the copper pads may have lateral dimensions ranging from 3 to 5 micrometers and a thickness ranging from 0.5 to 1 micrometer, the spacing between copper pads being of the same order of magnitude.
Further,
In practice, the connected copper pads will not necessarily be regularly arranged over the entire surface of the opposite elements. However, the present inventors have observed that a better bonding between the two assembled elements is obtained when the copper pads are regularly distributed. Thus, on each of the opposite surfaces of the two elements, regularly distributed copper pads will be provided, some of these pads being “dummy” pads, which are not connected to lower metal levels.
Such alterations, modifications, and improvements are intended to be part of this disclosure, and are intended to be within the spirit and the scope of the present invention. Accordingly, the foregoing description is by way of example only and is not intended to be limiting. The present invention is limited only as defined in the following claims and the equivalents thereto.
Number | Date | Country | Kind |
---|---|---|---|
12 51362 | Feb 2012 | FR | national |
Number | Name | Date | Kind |
---|---|---|---|
6596640 | Fishcer et al. | Jul 2003 | B1 |
20030015799 | Abiru et al. | Jan 2003 | A1 |
20060220197 | Kobrinsky et al. | Oct 2006 | A1 |
20060234473 | Wong et al. | Oct 2006 | A1 |
20070197023 | Widodo et al. | Aug 2007 | A1 |
20080116584 | Sitaram | May 2008 | A1 |
20110084403 | Yang et al. | Apr 2011 | A1 |
Number | Date | Country |
---|---|---|
2963158 | Jan 2012 | FR |
Number | Date | Country | |
---|---|---|---|
20130207268 A1 | Aug 2013 | US |