The invention relates to a showerhead electrode assembly of a plasma processing chamber in which semiconductor components can be manufactured.
According to one embodiment, a showerhead electrode assembly comprises a monolithic stepped electrode clamped to a backing plate wherein the showerhead electrode assembly comprises an upper electrode of a capacitively coupled plasma processing chamber. The stepped electrode is a circular plate having a plasma exposed surface on a lower face thereof and a mounting surface on an upper face thereof. The mounting surface includes a plurality of alignment pin recesses configured to receive alignment pins arranged in a pattern matching alignment pin holes in a backing plate against which the plate is held by cam locks and the plate includes process gas outlets arranged in a pattern matching gas supply holes in the backing plate. The upper face includes an outer recessed surface surrounding a planar inner surface, the plasma exposed surface including inner and outer inclined surfaces. A plurality of circumferentially spaced apart pockets in the outer recessed surface are configured to receive locking pins therein adapted to cooperate with cam locks to clamp the stepped electrode to the backing plate.
According to another embodiment, a showerhead electrode assembly of a capacitively coupled plasma processing chamber comprises a thermal control plate, a backing plate, a guard ring and a stepped electrode. The thermal control plate is supported by a temperature controlled wall of the plasma processing chamber, the thermal control plate having a diameter larger than a wafer to be processed in the plasma processing chamber and including annular projections on a lower side thereof with gas plenums between the annular projections. The backing plate is supported by the thermal control plate and has a diameter smaller than the thermal control plate, gas passages therethrough, and cam locks in horizontally extending bores. The shield ring has a height equal to a thickness of the outer periphery of the backing plate and at least one horizontally extending access bore passing through the shield ring, the shield ring being rotatable around the backing plate to align the access bore with at least one of the cam locks. The stepped electrode has gas passages therethrough in fluid communication with the gas passages in the backing plate The stepped electrode includes vertically extending locking pins which engage the cam locks, the stepped electrode supporting the shield ring and being removable by releasing the locking pins from the cam locks.
The fabrication of an integrated circuit chip typically begins with a thin, polished slice of high-purity, single-crystal semiconductor material substrate (such as silicon or germanium) called a “wafer.” Each wafer is subjected to a sequence of physical and chemical processing steps that form the various circuit structures on the wafer. During the fabrication process, various types of thin films may be deposited on the wafer using various techniques such as thermal oxidation to produce silicon dioxide films, chemical vapor deposition to produce silicon, silicon dioxide, and silicon nitride films, and sputtering or other techniques to produce other metal films.
After depositing a film on the semiconductor wafer, the unique electrical properties of semiconductors are produced by substituting selected impurities into the semiconductor crystal lattice using a process called doping. The doped silicon wafer may then be uniformly coated with a thin layer of photosensitive, or radiation sensitive material, called a “resist.” Small geometric patterns defining the electron paths in the circuit may then be transferred onto the resist using a process known as lithography. During the lithographic process, the integrated circuit pattern may be drawn on a glass plate called a “mask” and then optically reduced, projected, and transferred onto the photosensitive coating.
The lithographed resist pattern is then transferred onto the underlying crystalline surface of the semiconductor material through a process known as etching. Vacuum processing chambers are generally used for etching and chemical vapor deposition (CVD) of materials on substrates by supplying an etching or deposition gas to the vacuum chamber and application of a radio frequency (RF) field to the gas to energize the gas into a plasma state.
A reactive ion etching system typically consists of an etching chamber with an upper electrode or anode and a lower electrode or cathode positioned therein. The cathode is negatively biased with respect to the anode and the container walls. The wafer to be etched is covered by a suitable mask and placed directly on the cathode. A chemically reactive gas such as CF4, CHF3, CClF3, HBr, Cl2 and SF6 or mixtures thereof with O2, N2, He or Ar is introduced into the etching chamber and maintained at a pressure which is typically in the millitorr range. The upper electrode is provided with gas hole(s), which permit the gas to be uniformly dispersed through the electrode into the chamber. The electric field established between the anode and the cathode will dissociate the reactive gas forming plasma. The surface of the wafer is etched by chemical interaction with the active ions and by momentum transfer of the ions striking the surface of the wafer. The electric field created by the electrodes will attract the ions to the cathode, causing the ions to strike the surface in a predominantly vertical direction so that the process produces well-defined vertically etched sidewalls. The etching reactor electrodes may often be fabricated by bonding two or more dissimilar members with mechanically compliant and/or thermally conductive adhesives, allowing for a multiplicity of function.
The assembly 100 also includes a thermal control plate 102, and an upper (top) plate 104 having liquid flow channels therein and forming a temperature controlled wall of the chamber. The stepped electrode 110 is preferably a cylindrical plate and may be made of a conductive high purity material such as single crystal silicon, polycrystalline silicon, silicon carbide or other suitable material (such as aluminum or alloy thereof, anodized aluminum, yttria coated aluminum). The backing plate 140 is mechanically secured to the electrode 110 with mechanical fasteners described below. The guard ring 170 surrounds the backing plate 140 and provides access to cam locking members as described below.
The showerhead electrode assembly 100 as shown in
The upper electrode 110 is a consumable part which must be replaced periodically. To supply process gas to the gap between the wafer and the upper electrode, the upper electrode 110 is provided with a gas discharge passages 106, which are of a size and distribution suitable for supplying a process gas, which is energized by the electrode and forms plasma in a reaction zone beneath the upper electrode 110.
The showerhead electrode assembly 100 also includes a plasma confinement assembly (or wafer area plasma (WAP) assembly) 180, which surrounds the outer periphery of the upper electrode 110 and the backing plate 140. The plasma confinement assembly 180 is preferably comprised of a stack or plurality of spaced-apart quartz rings 190, which surrounds the outer periphery of upper electrode 110 and the backing plate 140. During processing, the plasma confinement assembly 180 causes a pressure differential in the reaction zone and increases the electrical resistance between the reaction chamber walls and the plasma thereby confining the plasma between the upper electrode 110 and the lower electrode (not shown).
During use, the confinement rings 190 confine the plasma to the chamber volume and controls the pressure of the plasma within the reaction chamber. The confinement of the plasma to the reaction chamber is a function of many factors including the spacing between the confinement rings 190, the pressure in the reaction chamber outside of the confinement rings and in the plasma, the type and flow rate of the gas, as well as the level and frequency of RF power. Confinement of the plasma is more easily accomplished if the spacing between the confinement rings 190 is very small. Typically, a spacing of 0.15 inches or less is required for confinement. However, the spacing of the confinement rings 190 also determines the pressure of the plasma, and it is desirable that the spacing can be adjusted to achieve the pressure required for optimal process performance while maintaining plasma. Process gas from a gas supply is supplied to electrode 110 through one or more passages in the upper plate 104 which permit process gas to be supplied to a single zone or multiple zones above the wafer.
The electrode 110 is preferably a planar disk or plate having a uniform thickness from center (not shown) to an area of increased thickness forming a step on the plasma exposed surface extending inwardly from an outer edge. The electrode 110 preferably has a diameter larger than a wafer to be processed, e.g., over 300 mm. The diameter of the upper electrode 110 can be from about 15 inches to about 17 inches for processing 300 mm wafers. The upper electrode 110 preferably includes multiple gas passages 106 for injecting a process gas into a space in a plasma reaction chamber below the upper electrode 110.
Single crystal silicon and polycrystalline silicon are preferred materials for plasma exposed surfaces of the electrode 110. High-purity, single crystal or polycrystalline silicon minimizes contamination of substrates during plasma processing as it introduces only a minimal amount of undesirable elements into the reaction chamber, and also wears smoothly during plasma processing, thereby minimizing particles. Alternative materials including composites of materials that can be used for plasma-exposed surfaces of the upper electrode 110 include aluminum (as used herein “aluminum” refers to pure Al and alloys thereof), yttria coated aluminum, SiC, SiN, and AlN, for example.
The backing plate 140 is preferably made of a material that is chemically compatible with process gases used for processing semiconductor substrates in the plasma processing chamber, has a coefficient of thermal expansion closely matching that of the electrode material, and/or is electrically and thermally conductive. Preferred materials that can be used to make the backing plate 140 include, but are not limited to, graphite, SiC, aluminum (Al), or other suitable materials.
The upper electrode 110 is attached mechanically to the backing plate 140 without any adhesive bonding between the electrode and backing plate, i.e., a thermally and electrically conductive elastomeric bonding material is not used to attach the electrode to the backing plate.
The backing plate 140 is preferably attached to the thermal control plate 102 with suitable mechanical fasteners, which can be threaded bolts, screws, or the like. For example, bolts (not shown) can be inserted in holes in the thermal control plate 102 and screwed into threaded openings in the backing plate 140. The thermal control plate 102 includes a flexure portion 184 and is preferably made of a machined metallic material, such as aluminum, an aluminum alloy or the like. The upper temperature controlled plate 104 is preferably made of aluminum or an aluminum alloy. The plasma confinement assembly (or wafer area plasma assembly (WAP)) 180 is positioned outwardly of the showerhead electrode assembly 100. A suitable plasma confinement assembly 180 including a plurality of vertically adjustable plasma confinement rings 190 is described in commonly owned U.S. Pat. No. 5,534,751, which is incorporated herein by reference in its entirety.
The upper electrode can be mechanically attached to the backing plate by a cam lock mechanism as described in commonly-owned U.S. application Ser. No. 61/036,862, filed Mar. 14, 2008, the disclosure of which is hereby incorporated by reference. With reference to
The electrode clamp includes a stud (locking pin) 205 mounted into a socket 213. The stud may be surrounded by a disc spring stack 215, such, for example, stainless steel Belleville washers. The stud 205 and disc spring stack 215 may then be press-fit or otherwise fastened into the socket 213 through the use of adhesives or mechanical fasteners. The stud 205 and the disc spring stack 215 are arranged into the socket 213 such that a limited amount of lateral movement is possible between the electrode 201 and the backing plate 203. Limiting the amount of lateral movement allows for a tight fit between the electrode 201 and the backing plate 203, thus ensuring good thermal contact, while still providing some movement to account for differences in thermal expansion between the two parts. Additional details on the limited lateral movement feature are discussed in more detail, below.
In a specific exemplary embodiment, the socket 213 is fabricated from bearing-grade Torlon®. Alternatively, the socket 213 may be fabricated from other materials possessing certain mechanical characteristics such as good strength and impact resistance, creep resistance, dimensional stability, radiation resistance, and chemical resistance may be readily employed. Various materials such as polyamides, polyimides, acetals, and ultra-high molecular weight polyethylene materials may all be suitable. High temperature-specific plastics and other related materials are not required for forming the socket 213 as 230° C. is a typical maximum temperature encountered in applications such as etch chambers. Generally, a typical operating temperature is closer to 130° C.
Other portions of the electrode clamp are comprised of a camshaft 207 surrounded at each end by a pair of camshaft bearings 209. The camshaft 207 and camshaft bearing assembly is mounted into a backing plate bore 211 machined into the backing plate 203. In a typical application for an etch chamber designed for 300 mm semiconductor wafers, eight or more of the electrode clamps may be spaced around the periphery of the electrode 201/backing plate 203 combination.
The camshaft bearings 209 may be machined from a variety of materials including Torlon®, Vespel®, Celcon®, Delrin®, Teflon®, Arlon®, or other materials such as fluoropolymers, acetals, polyamides, polyimides, polytetrafluoroethylenes, and polyetheretherketones (PEEK) having a low coefficient of friction and low particle shedding. The stud 205 and camshaft 207 may be machined from stainless steel (e.g., 316, 316L, 17-7, etc.) or any other material providing good strength and corrosion resistance.
Referring now to
In
The stud/socket assembly 303 illustrates an inside diameter in an upper portion of the socket 213 being larger than an outside diameter of a mid-section portion of the stud 205. The difference in diameters between the two portions allows for the limited lateral movement in the assembled electrode clamp as discussed above. The stud/disc spring assembly 301 is maintained in rigid contact with the socket 213 at a base portion of the socket 213 while the difference in diameters allows for some lateral movement. (See also,
With reference to
For example, with continued reference to
In an exemplary mode of operation, once the camshaft bearings are attached to the camshaft 207 and inserted into the backing plate bore 211, the camshaft 207 is rotated counterclockwise to its full rotational travel. The stud/socket assembly 303 (
With reference to
The electrode assembly 500 includes a thermal control plate 510 bolted from outside the chamber to a temperature controlled top wall 512 of the chamber. The electrode 502 is releasably attached to the backing plate from inside the chamber by cam-lock mechanisms 514 described earlier with reference to
In a preferred embodiment, the electrode 502 of the electrode assembly 500 can be disassembled by (a) rotating the guard ring 508 to a first position aligning four holes in the guard ring with four cam locks 514 located at spaced positions in the outer portion of the backing plate; (b) inserting a tool such as an allen wrench through each hole in the guard ring and rotating each cam lock to release a vertically extending locking pin of each respective cam lock; (c) rotating the guard ring 90° to a second position aligning the four holes in the guard ring with another four cam locks; and (d) inserting a tool such as an allen wrench through each hole in the guard ring and rotating each respective cam lock to release a locking pin of each respective cam lock; whereby the electrode 502 can be lowered and removed from the plasma chamber.
The upper face of the electrode includes 9 alignment pin holes with 3 pin holes near the center, 3 pin holes inward of the annular recess and 3 pin holes in the annular recess near the outer edge of the electrode. The 3 central pin holes are radially aligned and include a pin hole at the center of the inner electrode and 2 pin holes between the third and fourth rows of gas holes. The intermediate pin holes near the annular recess include one pin hole radially aligned with the central pin hole and two other pin holes spaced 120° apart. The outer 3 pin holes are spaced 120° apart at locations between adjacent pockets.
The electrode 502 includes an outer step (ledge) 536 which supports the guard ring 508, the upper face (mounting surface) 522 which engages a lower surface of the backing plate 506, the lower face (plasma exposed stepped surface) 530 which includes inner tapered surface 544, a horizontal surface 546, and an outer tapered surface 548 and 8 pockets 550 in upper face 540 in which the locking pins are mounted.
The mounting surface 522 of the electrode abuts an opposed surface of the backing plate 506 as a result of the clamping force exerted by the 8 locking pins held by the 8 cam locks in the backing plate. The guard ring 508 covers the mounting holes in the backing plate 506 and the access openings in the guard ring are filled with removable inserts made of plasma resistant polymer material such as Torlon®, Vespel®, Celcon®, Delrin®, Teflon®, Arlon®, or other materials such as fluoropolymers, acetals, polyamides, polyimides, polytetrafluoroethylenes, and polyetheretherketones (PEEK) having a low coefficient of friction and low particle shedding.
With reference to
While the invention has been described in detail with reference to specific embodiments thereof, it will be apparent to those skilled in the art that various changes and modifications can be made, and equivalents employed, without departing from the scope of the appended claims.