A field of the disclosure is boron nitride deposition. Additional fields of the disclosure include high temperature ceramics, lubricants, and semiconductor fabrication, and particularly the deposition of ultra-thin oxides. Example technologies that can employ a high quality ALD boron nitride layer of the disclosure include insulating layers in a MISFET (metal-insulator-semiconductor field effect transistor), interconnect covering, such as copper, to help prevent power loss, lower resistivity, and prevent interconnect failure from power overloading. Other applications include finFETs, DRAM, flash memory, etc. Additional applications include as an interfacial layer of amorphous or crystalline BN that is deposited prior to dielectric deposition in MOSFET (metal-oxide-semiconductor FET) device architectures to prevent substrate diffusion into the high k material, thereby producing a device with a lower density of interfacial traps (Dit).
Nitrides are normally deposited using an activated NH3 source, such as a plasma source, usually at high substrate temperatures in excess of 500° C. Previous work has shown that ALD occurs at 600° C.-900° C. with a growth rate of 0.7 Å/cycle on sapphire and Si [1]. Above this window, the process was not self limiting. The precursors were triethylborane and ammonia with H2 carrier gas. George and coworkers showed that ALD with a growth rate of ˜1 Å/cycle of BN with BCl3 and NH3 on ZrO2 nanoparticles was possible at 500K, but it was likely with very large exposures. The process was low temperature, but the substrate was ZrO2 [2]. There has also been reports of laser-assisted ALD of BN using BBr3 and NH3 [3], as well as amorphous growth at 400° C. and turbostratic growth at 750° C. [4]. There are a couple patents from Samsung [5, 6] that discuss forming SiBN thin films with three precursors as well as forming nano-laminate structures of Si3N4 and BN, but these mainly discuss the formation of the films and nano-laminate structures using activated NH3 species or only on semiconducting substrates. There has also been recent work that shows low temperature ALD of hexagonal BN, but using an activated N2/H2 plasma [7].
The patent or application file contains at least one drawing executed in color. Copies of this patent or patent application publication with color drawings will be provided by the Office upon request and payment of the necessary fee.
Methods of the disclosure include a BN ALD process at low temperatures using a reactive nitrogen precursor, such as thermal N2H4, and a boron containing precursor, which allows for the deposition of ultra thin (less than 5 nm) films with precise thickness and composition control. Methods are self-limiting and provide saturating atomic layer deposition (ALD) of a boron nitride (BN) layer on various semiconductors and metallic substrates. The ALD occurs from the sequential exposures of a reactive nitrogen containing precursor such as hydrazine (N2H4) and a boron containing precursor. These precursors include, but are not limited to BCl3, BBr3, BF3, B2H6, borazine (BH)3(NH)3, as well as tris(dimethylamino)borane (TDMAB) and related organometallic compounds. The substrates that BN ALD can be performed on include, but are not limited to, semiconductors such as silicon, silicon germanium (SiGe), indium gallium arsenide (InGaAs), indium gallium antiminide (InGaSb), or indium gallium nitride (InGaN), with each compound substrate having varying alloy compositions. In addition, 2-dimensional semiconductor substrates such as highly ordered pyrolytic graphite (HOPG) and molybdenum disulfide (MoS2), as well as metallic substrates, such as copper, can be used.
BN (boron nitride) formed by a method of the disclosure can be an amorphous material. Amorphous BN acts as a diffusion barrier, and is especially useful on copper. BN can be formed via the disclosure in a crystalline form such as hexagonal or cubic. Crystalline BN has useful properties including high thermal conductivity, high chemical stability, a relatively low dielectric constant, and a wide bandgap.
Embodiments will be discussed with respect to experiments. Artisans will appreciate broader aspects and variations of the disclosure from the description of experiments.
Experiments have shown that depositing a thin (˜0.5 nm) interfacial layer of BN in a MOS architecture can lower Dit when compared to a similar device without the interfacial BN layer. The deposited films are uniform and pinhole free, a crucial requirement for ALD reactions, particularly in nm-sized devices. The deposited films are able to nucleate Al2O3 and are assumed to be able to nucleate any other gate oxides such as HfO2, ZrO2, and HfZrO. In effect, BN ALD has the ability to functionalize, passivate, and nucleate growth in each and every unit cell. Experiments also demonstrated a device with an interfacial layer of ˜0.5 nm BN with Al2O3 gate oxide. In addition, a device with ˜5 nm BN was fabricated on SiGe to see if a pinhole free film of BN was deposited. Atomic force microscopy (AFM) confirmed the presence of a uniform, pinhole free BN film. Deposition was also demonstrated on copper.
The experimental self-limiting atomic layer deposition procedure is based upon sequential exposures to a reactive nitrogen-containing precursor (N2H4 in our case) and a boron containing precursor (BCI3, BBr3, BF3, B2H6, (BH)3(NH)3, TDMAB). During the first half-cycle reaction of the substrate with N2H4, the surface terminates in N-Hx groups. During the second half cycle, exposure with the boron containing precursor (BCI3 is the only precursor we have tested), boron is added to the surface while a gaseous byproduct (HCI for BCI3) is formed. The surface reaction saturates when all surface hydrogen has reacted, and the surface is left terminated with B-CI groups. Upon the next exposure to N2H4, nitrogen is added to the surface again with the formation of a second gaseous byproduct (for example H-CI) that is pumped away. Similarly, the half-cycle reaction is completed when all surface CI has been reacted. Continued sequential exposures have shown that films upwards of 5 nm of nearly stoichiometric BN can be formed on SiGe with very minimal contamination. It is noted that on some substrates, the boron containing precursor will be more effective at nucleating the ALD (for example BCI3) than the N2H4 depending on if the substrate is electrophilic or nucleophilic. For example, on HOPG, the data is most consistent with ALD being nucleated by catalytic dissociation of BCI3 at step edges.
Anhydrous N2H4, courteous of Rasirc, Inc. was employed in these studies to prevent unwanted oxygen contamination during film deposition. A source containing the anhydrous hydrazine was charged with ultra-pure nitrogen to a pressure of 760 Torr, with subsequent pulses using the headspace N2H4/N2 gas mixture. Similarly, semiconductor grade (99.999% pure, Praxair) BCl3 was used to deposit contamination-free films. The self-limiting atomic layer deposition procedure can be seen in
All above data has discussed BN on SiGe. The following data discusses BN on HOPG. BN is isoelectronic to HOPG but has different electronic properties. Therefore, there has been research into depositing BN on HOPG to tune the electronic properties of devices, as well as gain the advantageous properties of BN.
BN deposition has also been performed on copper and MoS2 substrates in a very similar manner as on SiGe and HOPG discussed above.
BN ALD layers of the disclosure can be used as an interfacial layer in a gate oxide stack, or as a diffusion barrier on copper interconnects in devices, which can help prevent the interconnect form overheating. Due to its small bond length, a-BN should provide a better diffusion barrier than even Si3N4 or metal nitrides. While Si3N4 can readily be deposited by CVD and plasma enhanced ALD, the a-BN can be deposited by thermal ALD in accordance with the disclosure at low temperature, e.g., ˜350° C. or less, thereby providing a more conformal coating. Metal nitrides can be deposited by thermal ALD but these often require processing temperatures in excess of 350° C. while the ALD of a-BN can be done below 350° C. The-BN layer can be used in double, quadruple, etc. patterning since it can be deposited conformally on a feature and would have selective etching with respect to semiconductors or oxides (SiO2). While Si3N4 can readily be deposited by CVD and plasma enhanced ALD, the a-BN can be deposited by thermal ALD at ˜350° C. or less thereby providing a more conformal coating. There is also application for depositing BN as a low dielectric material, or it can serve as a selective etching material. It also has high mechanical resistance to chemical mechanical polishing (CMP) slurries, so depositing BN can help act as CMP stop layer. The ALD deposition of boron nitride is applicable for use as a semiconductor interfacial layer in MOSCAP, MOSFET, and FinFET device architectures. This interfacial layer can act as a surface protection layer from unwanted oxidation or surface contamination or act as diffusion barrier layer from substrate out-diffusion into the oxide. This application will serve useful during deposition and processing of gate stacks on FinFETs for MOSFETs.
While specific embodiments of the present disclosure have been shown and described, it should be understood that other modifications, substitutions and alternatives are apparent to one of ordinary skill in the art. Such modifications, substitutions and alternatives can be made without departing from the spirit and scope of the disclosure.
Various features of the disclosure are set forth in the appended claims.
The following references are hereby incorporated by reference in their entirety to the extent not inconsistent with the present disclosure.
1. Snure, M., et al., Optical characterization of nanocrystalline boron nitride thin films grown by atomic layer deposition. Thin Solid Films, 2014. 571, Part 1: p. 51-55.
2. Ferguson, J., A. Weimer, and S. George, Atomic layer deposition of boron nitride using sequential exposures of BCl3 and NH3. Thin Solid Films, 2002. 413(1): p. 16-25.
3. Olander, J., et al., Laser-Assisted Atomic Layer Deposition of Boron Nitride Thin Films. Chemical Vapor Deposition, 2005. 11(6-7): p. 330-337.
4. Mårlid, B., et al., Atomic layer deposition of BN thin films. Thin Solid Films, 2002. 402(1): p. 167-171.
5. Ahn, J. Y., et al., Insulating layers in semiconductor devices having a multi-layer nanolaminate structure of SiNx thin film and BN thin film and methods for forming the same. 2003, Google Patents.
6. Kim, Y. S., et al., Method for forming a thin film using an atomic layer deposition (ALD) process. 2004, Google Patents.
7. Haider, A., et al., Low-Temperature Deposition of Hexagonal Boron Nitride via Sequential Injection of Triethylboron and N2/H2 Plasma. Journal of the American Ceramic Society, 2014. 97(12): p. 4052-4059.
8. Cassabois, G., P. Valvin, and B. Gil, Hexagonal boron nitride is an indirect bandgap semiconductor. arXiv preprint arXiv:1512.02962, 2015.
9. Bath, A., et al., Plasma enhanced chemical vapor deposition and characterization of boron nitride gate insulators on InP. Journal of Applied Physics, 1991. 70(8): p. 4366-4370.
10. Liu, Z., et al., Direct Growth of Graphene/Hexagonal Boron Nitride Stacked Layers. Nano Letters, 2011. 11(5): p. 2032-2037.
This applications claims benefit of U.S. Provisional Patent Application Ser. No. 62/372,052, filed Aug. 8, 2016, which is herein incorporated by reference.
| Number | Name | Date | Kind |
|---|---|---|---|
| 6740977 | Ahn et al. | May 2004 | B2 |
| 6815350 | Kim et al. | Nov 2004 | B2 |
| 7648927 | Singh | Jan 2010 | B2 |
| 20070128858 | Haukka | Jun 2007 | A1 |
| 20100062149 | Ma | Mar 2010 | A1 |
| 20100108982 | Ping | May 2010 | A1 |
| 20110299720 | Nolen | Dec 2011 | A1 |
| 20150099360 | Yieh | Apr 2015 | A1 |
| Entry |
|---|
| Snure, M., et al., Optical characterization of nanocrystalline boron nitride thin films grown by atomic layer deposition. Thin Solid Films, 2014. 571, Part 1: p. 51-55. |
| Ferguson, J., A. Weimer, and S. George, Atomic layer deposition of boron nitride using sequential exposures of BCl 3 and NH3. Thin Solid Films, 2002. 413(1): p. 16-25. |
| Olander, J., et al., Laser-Assisted Atomic Layer Deposition of Boron Nitride Thin Films. Chemical Vapor Deposition, 2005. 11(6-7): p. 330-337. |
| Mårlid, B., et al., Atomic layer deposition of Bn thin films. Thin Solid Films, 2002. 402(1): p. 167-171. |
| Haider, A., et al., Low-Temperature Deposition of Hexagonal Boron Nitride via Sequential Injection of Triethylboron and N2/H2 Plasma. Journal of the American Ceramic Society, 2014. 97(12): p. 4052-4059. |
| Cassabois, G., P. Valvin, and B. Gil, Hexagonal boron nitride is an indirect bandgap semiconductor. arXiv preprint arXiv:1512.02962, 2015. |
| Bath, A., et al., Plasma enhanced chemical vapor deposition and characterization of boron nitride gate insulators on InP. Journal of Applied Physics, 1991. 70(8): p. 4366-4370. |
| Liu, Z., et al., Direct Growth of Graphene/Hexagonal Boron Nitride Stacked Layers. Nano Letters, 2011. 11(5): p. 2032-2037. |
| Number | Date | Country | |
|---|---|---|---|
| 20180040476 A1 | Feb 2018 | US |
| Number | Date | Country | |
|---|---|---|---|
| 62372052 | Aug 2016 | US |