This application claims the benefit of Korean Patent Application No. 10-2008-0086737 filed with the Korea Intellectual Property Office on Sep. 3, 2008, the disclosure of which is incorporated herein by reference.
1. Field of the Invention
The present invention relates to a wafer level package and a method of manufacturing the same; and, more particularly, to a wafer level package including a metal post with a flexure hinge structure and a method of manufacturing the same.
2. Description of the Related Art
A packaging process includes many unit processes, for example, chip attaching, wire bonding, molding, trimming/forming or the like, and so a conventional method of manufacturing a package to perform the packaging process by each chip has a disadvantage of needing a very long time for packaging all chips when considering the number of the chips obtained from one wafer.
Therefore, recently, there has been suggested a method of manufacturing an individual package by firstly performing the packaging process in a wafer state and then cutting a wafer along a dicing line. The package manufactured by this method is referred to as a wafer level package.
The wafer level package has advantages of manufacturing the package as a finished product in a state of not separating individual chips from the wafer and using existing wafer manufacturing equipment and processes for manufacture equipment or processes used in manufacturing the package.
In the wafer level package according to the prior art, a molding resin such as an EMC(Epoxy Molding Compound) and a metal post connected to a die pad of the wafer are formed on the wafer and a solder ball is formed on a top surface of the metal post in a state of not dividing the wafer to the individual chips.
In the wafer level package according to the prior art, the metal post is generally formed in a cylindrical shape and used in a state of having large compliance by increasing a height of the metal post to improve reliability, however, in this case, a thickness of the entire molding resin is increased and a process cost is rising due to increment of a plating amount in a plating process for forming the metal post.
The present invention has been invented in order to overcome the above-described problems and it is, therefore, an object of the present invention to provide a wafer level package capable of reducing a process cost without the need for increasing a height of a metal post and allowing a metal post to play a role of a buffer to deformation of the package due to a CTE(Coefficient of Thermal Expansion) mismatch between the wafer level package and a wiring substrate by forming the metal post in a flexure hinge structure, and a method of manufacturing the same.
In accordance with one aspect of the present invention to achieve the object, there is provided a wafer level package including a wafer having a die pad; a redistribution line formed to be connected on a top surface of the die pad; a metal post connected to a top surface of the redistribution line and formed in a flexure hinge structure; and a molding resin formed between the metal posts.
Herein, the flexure hinge structure of the metal post may have a concave central portion.
And, the flexure hinge structure of the metal post may have a curved side surface and is spread upward.
Further, the wafer level package may further include a protection layer which is formed between the wafer and the redistribution line and has a via hole to expose a portion of a top surface of the die pad.
Further, the wafer level package may further include an external connection device formed at a top surface of the metal post.
Further, the external connection device may be a solder ball.
And, in accordance with another aspect of the present invention to achieve the object, there is provided a method for manufacturing a wafer level package including the steps of: forming a redistribution line connected to a top surface of a die pad on a wafer with the die pad; additionally preparing a carrier film having a metal post with a concave central portion on one surface; bonding the metal post to a top surface of the redistribution line; molding a space between the metal posts with a molding resin; and removing the carrier film.
Herein, the step of additionally preparing the carrier film having the metal post with the concave central portion includes the steps of: separately preparing a first silicon substrate and a second silicon substrate; separately forming first and second metal post filling spaces which have curved side surfaces and are spread upward by etching portions of the first and second silicon substrates; forming a silicon mold with a metal post filling space of which a central portion is concave by bonding the first silicon substrate to the second silicon substrate to contact bottom surfaces thereof to each other; adhering a carrier film coated with metal to one surface of the silicon mold; forming a metal post by plating the metal post filling space of the silicon mold with metal; and selectively removing the silicon mold.
Further, in the step of separately forming the first and second metal post filling spaces which have the curved side surfaces and are spread upward by etching portions of the first and second silicon substrates, the first and second silicon substrates may be etched by an RIE (Reactive Ion Etching) method.
Further, before forming the redistribution line, the method may further include a step of: forming a protection layer including a via hole to expose a portion of a top surface of a die pad on a wafer with the die pad.
Further, after removing the carrier film, the method may further include a step of: forming an external connection device on a top surface of the metal post.
And, in accordance with still another aspect of the present invention to achieve the object, there is provided a method for manufacturing a wafer level package including the steps of: forming a redistribution line connected to a top surface of a die pad on a wafer with the die pad; forming a molding resin with a metal post filling space, which exposes a portion of a top surface of the redistribution line, has a curved side surface, and is spread upward, on an upper part of the wafer having the redistribution line; and forming a metal post by plating the metal post filling space with metal.
Herein, the step of forming the molding resin with the metal post filling space may include the steps of: forming the molding resin on the entire surface of the wafer having the redistribution line; and imprinting the molding resin by using a mold provided with an uneven portion of the same shape as that of the metal post filling space on the surface.
These and/or other aspects and advantages of the present general inventive concept will become apparent and more readily appreciated from the following description of the embodiments, taken in conjunction with the accompanying drawings of which:
Hereinafter, a matter regarding to an operation effect including a technical configuration to achieve the object of a wafer level package and a method of manufacturing the same in accordance with the present invention will be appreciated clearly through the following detailed description with reference to the accompanying drawings illustrating preferable embodiments of the present invention.
A Structure of a Wafer Level Package
First of all, a wafer level package in accordance with an embodiment of the present invention will be described in detail with reference to
First of all, as shown in
Herein, the wafer 10 may use a silicon wafer or the like and the die pads 11 may be made of aluminum(Al) or the like.
The protection layer 12 may be formed by polyimide, a silicon nitride layer, a silicon oxide layer or the like.
The redistribution line 13 may be made of metal such as copper.
Further, the metal posts 15 may be formed through copper-plating or the like.
And, a molding resin 14, which is made of epoxy resin or the like, is formed between the metal posts 15.
An external connection device 16 for connection to a wiring substrate(not shown in the drawing) is formed on a top surface of the metal post 15. The external connection device 16 may be formed by a solder ball or the like.
Particularly, in the wafer level package in accordance with the embodiment of the present invention, the metal post 15 may have a flexure hinge structure.
Herein, the flexure hinge structure of the metal post 15, as shown in
For example,
Further, although not shown in the drawings, the metal post 15 may have a one-axis circular type or two-axis elliptical type flexure hinge structure or the like as well as the above-mentioned structures.
Further, the flexure hinge structure of the metal post 15, as shown in
As described above, in the wafer level package in accordance with the embodiment of the present invention, the metal post 15 can play a role of a buffer for preventing deformation of the package due to a CTE mismatch between the wafer level package and a wiring substrate(not shown in the drawings) although the metal post 150 is formed at a low height without the need for increasing the height of the metal post 15 by changing the structure of the metal post 15 into the flexure hinge structure with the concave central portion, and so on unlike a conventional cylindrical structure.
Therefore, the present invention has an advantage of securing reliability of the wafer level package without increasing the height of the metal post 15.
Further, the metal post 15 of the wafer level package in accordance with the embodiment of the present invention has excellent buffering capability to external impact by having the above-mentioned flexure hinge structure, thereby improving reliability of a drop test or the like.
And, it is possible to reduce a material cost and a time of a plating process in comparison with the cylindrical structure of the conventional metal post.
A Method of Manufacturing a Wafer Level Package
Hereinafter, a method of manufacturing the wafer level package shown in
First of all, although not shown in the drawings, a wafer 10 with die pads 11 on one surface is prepared. Then, after forming a protection layer 12 on the wafer with the die pads 11, via holes 12a are formed to expose a portion of a top surface of each of the die pads 11 by removing a portion of the protection layer 12.
Then, a redistribution line 13, which is connected to top surfaces of the die pads 11, is formed on the protection layer 12 including the via holes 12a.
As described above, after forming the redistribution line 13 connected to the top surfaces of the die pads 11 on the wafer 10 with the die pads 11, as shown in
Then, as shown in
Then, as shown in
Then, an adhesive 203 is coated on the one surfaces of the silicon molds 200.
Then, as shown in
The metal 204 may play a role of a plating seed layer in the following metal plating process. The carrier film 205 may be made of resin or the like.
Then, as shown in
Then, as shown in
Then, as shown in
Then, as shown in
Then, as shown in
As described above, in accordance with the embodiment of the present invention, it is possible to reduce a material cost of the metal post 15 or the like by forming the central portion of the metal post 15 in a concave shape, thereby reducing a manufacture cost of the wafer level package.
Further, the metal post 15 with the concave central portion can play a role of a buffer to deformation of the package due to a CTE mismatch between the wafer level package and the wiring substrate.
Hereinafter, a method of manufacturing the wafer level package shown in the above-mentioned
First of all, as shown in
Then, as shown in
Then, as shown in
Then, as shown in
Then, as shown in
Herein, the uneven portion 100a of the mold 100 has the same shape as that of the metal post 15 to be formed, for example, it is preferable that a side surface of the uneven portion is curved and the uneven portion is spread upward.
After the imprinting process is completed, as shown in
Then, after performing a demolding process to remove the mold 100, the molding resin 14 is cured.
Then, as shown in
As described above, the metal post 15 can play a role of a buffer to deformation of the package due to a CTE mismatch between the wafer level package and the wiring substrate and reduce a plating material cost, a lead time, and so on in comparison with a conventional cylindrical metal post by having the curved side surface and being spread upward.
Then, as shown in the above-mentioned
As described above, in accordance with the present invention, the wafer level package and the method of manufacturing the same can prevent the deformation of the package due to the CTE mismatch between the wafer level package and the wiring substrate although the height of the metal post is reduced by forming the metal post in the flexure hinge structure of which the central portion is concave or the like, thereby securing the reliability.
Further, the prevent invention can improve the buffering capability to the external impact by forming the metal post in the flexure hinge structure, thereby enhancing the reliability of the drop test of the package or the like.
In addition, the metal post structure of the present invention can reduce the material cost in the plating process for forming the metal post and the time of the plating process by reducing the volume and the height thereof in comparison with the conventional cylindrical structure.
As described above, although the preferable embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that substitutions, modifications and changes may be made in this embodiment without departing from the principles and spirit of the general inventive concept, the scope of which is defined in the appended claims and their equivalents.
Number | Date | Country | Kind |
---|---|---|---|
10-2008-0086737 | Sep 2008 | KR | national |