1. Field of the Invention
Embodiments of the invention generally relate to an apparatus and method for atomic layer deposition. More particularly, embodiments of the invention relate to an improved gas delivery apparatus and method for atomic layer deposition.
2. Description of the Related Art
Reliably producing submicron and smaller features is one of the key technologies for the next generation of very large scale integration (VLSI) and ultra large scale integration (ULSI) of semiconductor devices. However, as the fringes of circuit technology are pressed, the shrinking dimensions of interconnects in VLSI and ULSI technology have placed additional demands on the processing capabilities. The multilevel interconnects that lie at the heart of this technology require precise processing of high aspect ratio features, such as vias and other interconnects. Reliable formation of these interconnects is very important to VLSI and ULSI success and to the continued effort to increase circuit density and quality of individual substrates.
As circuit densities increase, the widths of interconnects, such as vias, trenches, contacts, and other features, as well as the dielectric materials between, decrease to 45 nm and 32 nm dimensions, whereas the thickness of the dielectric layers remain substantially constant, with the result of increasing the aspect ratios of the features. Many traditional deposition processes have difficulty filling submicron structures where the aspect ratio exceeds 4:1, and particularly where the aspect ratio exceeds 10:1. Therefore, there is a great amount of ongoing effort being directed at the formation of substantially void-free and seam-free submicron features having high aspect ratios.
Atomic layer deposition (ALD) is a deposition technique being explored for the deposition of material layers over features having high aspect ratios. One example of an ALD process includes the sequential introduction of pulses of gases. For instance, one cycle for the sequential introduction of pulses of gases may contain a pulse of a first reactant gas, followed by a pulse of a purge gas and/or a pump evacuation, followed by a pulse of a second reactant gas, and followed by a pulse of a purge gas and/or a pump evacuation. The term “gas” as used herein is defined to include a single gas or a plurality of gases. Sequential introduction of separate pulses of the first reactant and the second reactant may result in the alternating self-limiting absorption of monolayers of the reactants on the surface of the substrate and, thus, forms a monolayer of material for each cycle. The cycle may be repeated to a desired thickness of the deposited material. A pulse of a purge gas and/or a pump evacuation between the pulses of the first reactant gas and the pulses of the second reactant gas serves to reduce the likelihood of gas phase reactions of the reactants due to excess amounts of the reactants remaining in the chamber.
Therefore, there is a need for apparatuses and methods used to deposit material films during ALD processes.
Embodiments of the invention relate to apparatuses and methods for uniformly depositing materials on a substrate during an atomic layer deposition (ALD) process. The high degree of uniformity for the deposited materials may be attributed to exposing the substrate to a deposition gas having circular gas flow pattern, such as a vortex pattern. In one embodiment, a process chamber contains a chamber lid assembly containing a centralized expanding channel and a tapered bottom surface extending from the expanding channel to a peripheral portion of the chamber lid assembly. The tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface. Another embodiment of a chamber includes a chamber lid assembly containing a centralized gas dispersing channel containing a converging channel and a diverging channel. Another embodiment of a chamber includes a chamber lid assembly containing at least two gas passageways circumventing an expanding channel. A plurality of inlets extend from each gas passageway into the expanding channel and are positioned to provide a circular gas flow pattern through the expanding channel.
In one embodiment, a chamber for processing substrates is provided which includes a substrate support containing a substrate receiving surface and a chamber lid assembly. The chamber lid assembly contains a gas dispersing channel at a central portion of the chamber lid assembly, wherein a converging portion of the gas dispersing channel tapers towards a central axis of the gas dispersing channel, a diverging portion of the gas dispersing channel tapers away from the central axis, and a tapered bottom surface extending from the diverging portion of the gas dispersing channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface. The chamber lid assembly further contains a first conduit coupled to a first gas inlet within the converging portion of the gas dispersing channel and a second conduit coupled to a second gas inlet within the converging portion of the gas dispersing channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern through the gas dispersing channel.
In one example, the first conduit and the second conduit are independently positioned to direct gas at an inner surface of the converging portion of the gas dispersing channel. The circular gas flow pattern contains a flow pattern of a vortex, a helix, a spiral, a twirl, a twist, a coil, a whirlpool, derivatives thereof, or combinations thereof. In some examples, the circular gas flow pattern extends at least about 1 revolution around the central axis of the gas dispersing channel, preferably about 1.5, about 2, about 3, about 4, or more revolutions around the central axis of the gas dispersing channel.
In some embodiments, a first valve is coupled to the first conduit and a second valve is coupled to the second conduit, and a first gas source is in fluid communication to the first valve and a second gas source is in fluid communication to the second valve. The first and second valves enable an atomic layer deposition process with a pulse time of about 2 seconds or less, such as within a range from about 0.05 seconds to about 0.5 seconds. In other examples, the first conduit and the second conduit are independently positioned at an angle greater than 0° from the central axis of the gas dispersing channel in order to form a circular gas flow.
In one example, the process chamber may contain a reaction zone having a volume of about 3,000 cm3 or less, wherein the reaction zone is defined between the tapered bottom surface and the substrate receiving surface. Other examples provide that the volume may be about 1,500 cm3 or less, such as about 600 cm3 or less.
In another embodiment, a chamber for processing substrates is provided which includes a chamber lid assembly containing a gas dispersing channel at a central portion of the chamber lid assembly, wherein a converging portion of the gas dispersing channel tapers towards a central axis of the gas dispersing channel and a diverging portion of the gas dispersing channel tapers away from the central axis, a first conduit coupled to a first gas inlet within the converging portion of the gas dispersing channel, a second conduit coupled to a second gas inlet within the converging portion of the gas dispersing channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern, and a first valve coupled to the first conduit and a second valve coupled to the second conduit, where the first and second valves enable an atomic layer deposition process with a pulse time of about 2 seconds or less.
In one example, the chamber lid assembly further contains a tapered bottom surface extending from the diverging portion of the gas dispersing channel to a peripheral portion of the chamber lid assembly. The tapered bottom surface may be shaped and sized to substantially cover the substrate receiving surface. In other examples, a first gas source may be in fluid communication to the first valve and a second gas source may be in fluid communication to the second valve, and the first conduit and the second conduit are independently positioned to direct gas at an inner surface of the converging portion of the gas dispersing channel. The circular gas flow pattern contains a flow pattern of a vortex, a helix, a spiral, a twirl, a twist, a coil, a whirlpool, derivatives thereof, or combinations thereof. In other examples, a mean surface roughness of the inner surface of the expanding channel increases along the central axis through the expanding channel (e.g., from the second plurality of inlets extending into the expanding channel—towards the substrate support).
In another embodiment, a method for depositing a material on a substrate is provided which includes positioning a substrate on a substrate support within a process chamber containing a chamber body and a chamber lid assembly, wherein the chamber lid assembly contains a gas dispersing channel at a central portion of the chamber lid assembly, wherein a converging portion of the gas dispersing channel tapers towards a central axis of the gas dispersing channel and a diverging portion of the gas dispersing channel tapers away from the central axis, a tapered bottom surface extending from the diverging portion of the gas dispersing channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate, a first conduit coupled to a first gas inlet within the converging portion of the gas dispersing channel, and a second conduit coupled to a second gas inlet within the converging portion of the gas dispersing channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern, flowing at least one carrier gas through the first and second conduits to form a circular flowing gas, exposing the substrate to the circular flowing gas, pulsing at least one precursor into the circular flowing gas, and depositing a material containing at least one element derived from the at least one precursor onto the substrate.
In another embodiment, a chamber for processing substrates is provided which includes a chamber lid assembly containing an expanding channel extending along a central axis at a central portion of the chamber lid assembly, a tapered bottom surface extending from the expanding channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface. The chamber lid assembly further contains a first conduit coupled to a first gas passageway, wherein the first gas passageway circumvents the expanding channel and contains a first plurality of inlets extending into the expanding channel, and a second conduit coupled to a second gas passageway, wherein the second gas passageway circumvents the expanding channel, contains a second plurality of inlets extending into the expanding channel, and the first plurality of inlets and the second plurality of inlets are positioned to provide a circular gas flow pattern through the expanding channel.
In one example, the first gas passageway may be positioned directly above the second gas passageway and the first gas passageway and the second gas passageway are both circumventing an upper portion of the expanding channel. The first plurality of inlets and the second plurality of inlets may be independently positioned to direct gas at an inner surface of the expanding channel. The circular gas flow pattern contains a flow pattern of a vortex, a helix, a spiral, a twirl, a twist, a coil, a whirlpool, derivatives thereof, or combinations thereof. In other examples, a first valve may be coupled to the first conduit and a second valve may be coupled to the second conduit, and a first gas source is in fluid communication to the first valve and a second gas source is in fluid communication to the second valve. The first and second valves enable an atomic layer deposition process with a pulse time of about 2 seconds or less, such as about 1 second or less, or within a range from about 0.05 seconds to about 0.5 seconds.
In another embodiment, a chamber for processing substrates is provided which includes a chamber lid assembly containing an expanding channel extending along a central axis at a central portion of the chamber lid assembly, a first conduit coupled to a first gas passageway, wherein the first gas passageway circumvents the expanding channel and contains a first plurality of inlets extending into the expanding channel, a second conduit coupled to a second gas passageway, wherein the second gas passageway circumvents the expanding channel, contains a second plurality of inlets extending into the expanding channel, and the first plurality of inlets and the second plurality of inlets are positioned to provide a circular gas flow pattern through the expanding channel, and a first valve coupled to the first conduit and a second valve coupled to the second conduit, where the first and second valves enable an atomic layer deposition process with a pulse time of about 2 seconds or less, such as about 1 second or less, or within a range from about 0.05 seconds to about 0.5 seconds.
In another embodiment, a method for depositing a material on a substrate is provided which includes positioning a substrate on a substrate support within a process chamber containing a chamber lid assembly which contains an expanding channel extending along a central axis at a central portion of the chamber lid assembly, a tapered bottom surface extending from the expanding channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface, a first conduit coupled to a first gas passageway, wherein the first gas passageway circumvents the expanding channel and contains a first plurality of inlets extending into the expanding channel, and a second conduit coupled to a second gas passageway, wherein the second gas passageway circumvents the expanding channel, contains a second plurality of inlets extending into the expanding channel, and the first plurality of inlets and the second plurality of inlets are positioned to provide a circular gas flow pattern through the expanding channel, forming a circular flowing gas by flowing at least one carrier gas through the first plurality of inlets or the second plurality of inlets, exposing the substrate to the circular flowing gas, pulsing at least one precursor into the circular flowing gas, and depositing a material containing at least one element derived from the at least one precursor onto the substrate.
In another embodiment, a chamber for processing substrates is provided which includes a chamber lid assembly containing an expanding channel at a central portion of the chamber lid assembly, wherein an upper portion of the expanding channel extends substantially parallel along a central axis of the expanding channel and an expanding portion of the expanding channel tapers away from the central axis, an inner surface within the upper portion of the expanding channel has a lower mean surface roughness than an inner surface within the expanding portion of the expanding channel, a tapered bottom surface extending from the expanding portion of the expanding channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface, a first conduit coupled to a first gas inlet within the upper portion of the expanding channel, and a second conduit coupled to a second gas inlet within the upper portion of the expanding channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern through the expanding channel.
In other embodiments, the chamber for processing substrates is provided which includes a chamber lid assembly containing an expanding channel at a central portion of the chamber lid assembly, wherein an upper portion of the expanding channel extends substantially parallel along a central axis of the expanding channel and an expanding portion of the expanding channel tapers away from the central axis, a first conduit coupled to a first gas inlet within the upper portion of the expanding channel, a second conduit coupled to a second gas inlet within the upper portion of the expanding channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern, and a first valve coupled to the first conduit and a second valve coupled to the second conduit, where the first and second valves enable an atomic layer deposition process with a pulse time of about 2 seconds or less. The chamber lid assembly further contains a tapered bottom surface extending from the expanding portion of the expanding channel to a peripheral portion of the chamber lid assembly.
In another embodiment, a method for depositing a material on a substrate is provided which includes positioning a substrate on a substrate support within a process chamber containing a chamber body and a chamber lid assembly, wherein the chamber lid assembly contains an expanding channel at a central portion of the chamber lid assembly, wherein an upper portion of the expanding channel extends substantially parallel along a central axis of the expanding channel and an expanding portion of the expanding channel tapers away from the central axis, a tapered bottom surface extending from the expanding portion of the expanding channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate, a first conduit coupled to a first gas inlet within the upper portion of the expanding channel, and a second conduit coupled to a second gas inlet within the upper portion of the expanding channel, wherein the first conduit and the second conduit are positioned to provide a circular gas flow pattern, flowing at least one carrier gas through the first and second conduits to form a circular flowing gas, exposing the substrate to the circular flowing gas, pulsing at least one precursor into the circular flowing gas, and depositing a material containing at least one element derived from the at least one precursor onto the substrate. The circular gas flow pattern contains a flow pattern of a vortex, a helix, a spiral, a twirl, a twist, a coil, a whirlpool, derivatives thereof, or combinations thereof.
In some examples, the first conduit and the second conduit may be independently positioned to direct gas at an inner surface of the converging portion of the gas dispersing channel. Therefore, the first conduit and the second conduit may be independently positioned at an angle (e.g., >0°) from the central axis of the gas dispersing channel. Alternatively, the first plurality of inlets and the second plurality of inlets may be independently positioned to direct gas at an inner surface of the expanding channel. Therefore, the first plurality of inlets and the second plurality of inlets may be independently positioned at an angle (e.g., >0°) from the central axis of the expanding channel. The circular gas flow pattern may contain a flow pattern, such as a vortex pattern, a helix pattern, a spiral pattern, a twirl pattern, a twist pattern, a coil pattern, a whirlpool pattern, or derivatives thereof. The circular gas flow pattern may extend at least about 1.5 revolutions around the central axis of the gas dispersing channel or the expanding channel, preferably, about 2 revolutions, more preferably, about 3 revolutions, and more preferably, about 4 revolutions. In other examples, the chamber may contain a reaction zone defined between the tapered bottom surface and the substrate receiving surface. The reaction zone may have a volume of about 3,000 cm3 or less. In one example, the volume may be about 1,500 cm3 or less. In another example, the volume may be about 600 cm3 or less. The volume may be adjusted by laterally positioning the substrate support.
In another embodiment, a method for depositing a material on a substrate is provided which includes positioning a substrate on a substrate support within a process chamber containing a chamber body and a chamber lid assembly, wherein the chamber lid assembly contains a gas dispersing channel at a central portion of the chamber lid assembly. The gas dispersing channel may contain a converging portion of the gas dispersing channel that tapers towards a central axis of the gas dispersing channel and a diverging portion of the gas dispersing channel that tapers away from the central axis. The chamber lid assembly may further contain a tapered bottom surface extending from the diverging portion of the gas dispersing channel to a peripheral portion of the chamber lid assembly. The tapered bottom surface may be shaped and sized to substantially cover the substrate. Also, the chamber lid assembly may further contain a first conduit coupled to a first gas inlet within the converging portion of the gas dispersing channel and a second conduit coupled to a second gas inlet within the converging portion of the gas dispersing channel. The first conduit and the second conduit may be positioned to provide a circular gas flow pattern.
The method further provides flowing at least one carrier gas through the first and second conduits to form a circular flowing gas, exposing the substrate to the circular flowing gas, pulsing at least one precursor into the circular flowing gas, and depositing a material containing at least one element derived from the at least one precursor onto the substrate. In one example, at least two chemical precursors are sequentially pulsed into the circular flowing gas during an atomic layer deposition process. In another example, at least three chemical precursors are sequentially pulsed into the circular flowing gas during the atomic layer deposition process.
In another embodiment, a method for depositing a material on a substrate is provided which includes positioning a substrate on a substrate support within a process chamber containing a chamber body and a chamber lid assembly, wherein the chamber lid assembly contains an expanding channel extending along a central axis at a central portion of the chamber lid assembly. The chamber lid assembly may further contain a tapered bottom surface extending from the expanding channel to a peripheral portion of the chamber lid assembly, wherein the tapered bottom surface is shaped and sized to substantially cover the substrate receiving surface. Also, the chamber lid assembly may further contain a first conduit coupled to a first gas passageway, wherein the first gas passageway circumvents the expanding channel and contains a first plurality of inlets extending into the expanding channel, and a second conduit coupled to a second gas passageway, wherein the second gas passageway circumvents the expanding channel, contains a second plurality of inlets extending into the expanding channel, and the first plurality of inlets and the second plurality of inlets are positioned to provide a circular gas flow pattern through the expanding channel.
The method further provides forming a circular flowing gas by flowing at least one carrier gas through the first plurality of inlets or the second plurality of inlets, exposing the substrate to the circular flowing gas, pulsing at least one precursor into the circular flowing gas, and depositing a material containing at least one element derived from the at least one precursor onto the substrate. In one example, at least two chemical precursors are sequentially pulsed into the circular flowing gas during an atomic layer deposition process. In another example, at least three chemical precursors are sequentially pulsed into the circular flowing gas during the atomic layer deposition process.
In another embodiment, a method for depositing a material layer over a substrate structure is provided which includes delivering a first reactant gas and a first purge gas through a first gas conduit in which the first reactant gas is provided in pulses and the first purge gas is provided in a continuous flow. The method further contains delivering a second reactant gas and a second purge through a second gas conduit in which the second reactant gas is provided in pulses and the second purge gas is provided in a continuous flow.
In another embodiment, a method for depositing a material layer over a substrate structure is provided which includes delivering gases to a substrate in a substrate processing chamber contains providing one or more gases into the substrate processing chamber, reducing a velocity of the gases through non-adiabatic expansion, providing the gases to a central portion of the substrate, and directing the gases radially across the substrate from the central portion of the substrate to a peripheral portion of the substrate.
So that the manner in which the above recited features of the invention are attained and can be understood in detail, a more particular description of the invention, briefly summarized above, may be had by reference to the embodiments thereof which are illustrated in the appended drawings.
It is to be noted, however, that the appended drawings illustrate only typical embodiments of this invention and are therefore not to be considered limiting of its scope, for the invention may admit to other equally effective embodiments.
Embodiments of the invention provide apparatuses and methods that may be used to deposit materials during an atomic layer deposition (ALD) process. Embodiments include ALD process chambers and gas delivery systems which contain an expanding channel lid assembly, a converge-diverge lid assembly, a multiple injection lid assembly, or an extended cap lid assembly. Other embodiments provide methods for depositing materials using these gas delivery systems during ALD processes.
Expanding Channel Lid Assembly
A substrate support 212 supports substrate 210 on a substrate receiving surface 211 in process chamber 200. Substrate support 212 is mounted to a lift motor 214 to raise and lower substrate support 212 and a substrate 210 disposed thereon. Lift plate 216 connected to lift motor 218 is mounted in process chamber 200 and raises and lowers lift pins 220 movably disposed through substrate support 212. Lift pins 220 raise and lower substrate 210 over the surface of substrate support 212. Substrate support 212 may include a vacuum chuck (not shown), an electrostatic chuck (not shown), or a clamp ring (not shown) for securing substrate 210 to substrate support 212 during processing.
Substrate support 212 may be heated to heat a substrate 210 disposed thereon. For example, substrate support 212 may be heated using an embedded heating element, such as a resistive heater (not shown), or may be heated using radiant heat, such as heating lamps (not shown) disposed above substrate support 212. A purge ring 222 may be disposed on substrate support 212 to define a purge channel 224 which provides a purge gas to a peripheral portion of substrate 210 to prevent deposition thereon.
Gas delivery system 230 is disposed at an upper portion of chamber body 202 to provide a gas, such as a process gas and/or a purge gas, to process chamber 200. Vacuum system 278 is in communication with a pumping channel 279 to evacuate any desired gases from process chamber 200 and to help maintain a desired pressure or a desired pressure range inside pumping zone 266 of process chamber 200.
In one embodiment, the gas delivery system 230 contains a chamber lid assembly 232. Chamber lid assembly 232 includes an expanding channel 234 extending from a central portion of chamber lid assembly 232 and a lower surface 260 extending from expanding channel 234 to a peripheral portion of chamber lid assembly 232. Lower surface 260 is sized and shaped to substantially cover substrate 210 disposed on substrate support 212. Expanding channel 234 has gas inlets 236a, 236b to provide gas flows from two similar pairs of valves 242a/252a, 242b/252b, which may be provided together and/or separately.
In one configuration, valve 242a and valve 242b are coupled to separate reactant gas sources but are preferably coupled to the same purge gas source. For example, valve 242a is coupled to reactant gas source 238 and valve 242b is coupled to reactant gas source 239, and both valves 242a, 242b are coupled to purge gas source 240. Each valve 242a, 242b includes a delivery line 243a, 243b having a valve seat assembly 244a, 244b and each valves 252a, 252b includes a purge line 245a, 245b having a valve seat assembly 246a, 246b. Delivery line 243a, 243b is in fluid communication with reactant gas source 238, 239 and is in fluid communication with gas inlet 236a, 236b of expanding channel 234. Valve seat assembly 244a, 244b of delivery line 243a, 243b controls the flow of the reactant gas from reactant gas source 238, 239 to expanding channel 234. Purge line 245a, 245b is in fluid communication with purge gas source 240 and intersects delivery line 243a, 243b downstream of valve seat assembly 244a, 244b of delivery line 243a, 243b. Valve seat assembly 246a, 246b of purge line 245a, 245b controls the flow of the purge gas from purge gas source 240 to expanding channel 234. If a carrier gas is used to deliver reactant gases from reactant gas source 238, 239, preferably the same gas is used as a carrier gas and a purge gas (i.e., an argon gas used as a carrier gas and a purge gas).
Each valve seat assembly 244a, 244b, 246a, 246b may contain a diaphragm (not shown) and a valve seat (not shown). The diaphragm may be biased open or closed and may be actuated closed or open respectively. The diaphragms may be pneumatically actuated or may be electrically actuated. Pneumatically actuated valves include pneumatically actuated valves available from Fujikin, Inc. and Veriflo Division, Parker Hannifin, Corp. Electrically actuated valves include electrically actuated valves available from Fujikin, Inc. For example, an ALD valve that may be used is the Fujikin Model No. FPR-UDDFAT-21-6.35-PI-ASN or the Fujikin Model No. FPR-NHDT-21-6.35-PA-AYT. Programmable logic controllers 248a, 248b may be coupled to valves 242a, 242b to control actuation of the diaphragms of the valve seat assemblies 244a, 244b, 246a, 246b of valves 242a, 242b. Pneumatically actuated valves may provide pulses of gases in time periods as low as about 0.020 seconds. Electrically actuated valves may provide pulses of gases in time periods as low as about 0.005 seconds. An electrically actuated valve typically requires the use of a driver coupled between the valve and the programmable logic controller.
Each valve 242a, 242b may be a zero dead volume valve to enable flushing of a reactant gas from delivery line 243a, 243b when valve seat assembly 244a, 244b is closed. For example, purge line 245a, 245b may be positioned adjacent valve seat assembly 244a, 244b of delivery line 243a, 243b. When valve seat assembly 244a, 244b is closed, purge line 245a, 245b may provide a purge gas to flush delivery line 243a, 243b. In the embodiment shown, purge line 245a, 245b is positioned slightly spaced from the valve seat assembly 244a, 244b of delivery line 243a, 243b so that a purge gas is not directly delivered into valve seat assembly 244a, 244b when open. A zero dead volume valve as used herein is defined as a valve which has negligible dead volume (i.e., not necessary zero dead volume).
Each valve pair 242a/252a, 242b/252b may be adapted to provide a combined gas flow and/or separate gas flows of the reactant gas and the purge gas. In reference to valve pair 242a/252a, one example of a combined gas flow of the reactant gas and the purge gas includes a continuous flow of a purge gas from purge gas source 240 through purge line 245a and pulses of a reactant gas from reactant gas source 238 through delivery line 243a. The continuous flow of the purge gas may be provided by leaving the diaphragm of valve seat assembly 246a of the purge line 245a open. The pulses of the reactant gas from reactant gas source 238 may be provided by opening and closing the diaphragm of valve seat assembly 244a of delivery line 243a. In reference to valve pair 242a/252a, one example of separate gas flows of the reactant gas and the purge gas includes pulses of a purge gas from purge gas source 240 through purge line 245a and pulses of a reactant gas from reactant gas source 238 through delivery line 243a. The pulses of the purge gas may be provided by opening and closing the diaphragm of valve seat assembly 246a of purge line 245a. The pulses of the reactant gas from reactant gas source 238 may be provided by opening and closing the diaphragm of valve seat assembly 244a of delivery line 243a.
Delivery lines 243a, 243b of valves 242a, 242b may be coupled to gas inlets 236a, 236b through gas conduits 250a, 250b. Gas conduits 250a, 250b may be integrated or may be separate from valves 242a, 242b. In one aspect, valves 242a, 242b are coupled in close proximity to expanding channel 234 to reduce any unnecessary volume of delivery line 243a, 243b and gas conduits 250a, 250b between valves 242a, 242b and gas inlets 236a, 236b.
In reference to
Referring to
Not wishing to be bound by theory, it is believed that the diameter of expanding channel 234, which is gradually increasing from upper portion 237 to lower portion 235 of expanding channel 234, allows less of an adiabatic expansion of a gas through expanding channel 234 which helps to control the temperature of the gas. For instance, a sudden adiabatic expansion of a gas delivered through gas inlet 236a, 236b into expanding channel 234 may result in a drop in the temperature of the gas which may cause condensation of the gas and formation of droplets. On the other hand, a gradually expanding channel 234 according to embodiments of the invention is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 232). The gradually expanding channel 234 may contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas inlets 236a, 236b are located adjacent upper portion 237 of expanding channel 234. In other embodiments, one or more gas inlets 236a, 236b may be located along the length of expanding channel 234 between upper portion 237 and lower portion 235.
Not wishing to be bound by theory,
As shown in
In one embodiment, distance 410 between gas inlets 236a, 236b and substrate 210 is made long enough that vortex flow 402 dissipates to a downwardly flow as shown by arrows 404 as a spiral flow across the surface of substrate 210 may not be desirable. It is believed that vortex flow 402 and the downwardly flow 404 proceeds in a laminar manner efficiently purging the surface of chamber lid assembly 232 and substrate 210. In one specific embodiment the length of distance 410 between upper portion 237 of expanding channel 234 and substrate 210 is within a range from about 3 inches to about 8 inches, preferably, from about 3.5 inches to about 7 inches, and more preferably, from about 4 inches to about 6 inches, such as about 5 inches.
Referring to
Not wishing to be bound by theory,
Q/A=V (1)
In which, “Q” is the flow of the gas, “A” is the area of the flow section, and “V” is the velocity of the gas. The velocity of the gas is inversely proportional to the area “A” of the flow section (Hx2πR), in which “H” is the height of the flow section and “2πR” is the circumference of the flow section having a radius “R”. In other words, the velocity of a gas is inversely proportional to the height “H” of the flow section and the radius “R” of the flow section.
Comparing the velocity of the flow section at position 502 and position 504, assuming that the flow “Q” of the gas at all positions between lower surface 260 of chamber lid assembly 232 and the surface of substrate 210 is equal, the velocity of the gas may be theoretically made equal by having the area “A” of the flow sections equal. For the area of flow sections at position 502 and position 504 to be equal, the height H1 at position 502 must be greater than the height H2 at position 504.
In one aspect, lower surface 260 is downwardly sloping to help reduce the variation in the velocity of the gases as it travels between lower surface 260 of chamber lid assembly 232 and substrate 210 to help provide uniform exposure of the surface of substrate 210 to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 260 of chamber lid assembly 232 and the surface of substrate 210 is less than about 2, preferably less than about 1.5, more preferably less than about 1.3, and most preferably about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of substrate 210 helps provide a more uniform deposition of the gas on substrate 210. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on substrate 210 surface. Thus, a higher velocity of a gas at a first area of the surface of substrate 210 versus a second area of the surface of substrate 210 is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 232 having a downwardly sloping lower surface 260 provides for more uniform deposition of the gas across the surface of substrate 210 because the downwardly sloping lower surface 260 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of substrate 210.
In one specific embodiment, the spacing between choke 262 and substrate support 212 is between about 0.04 inches and about 2.0 inches, and preferably between 0.04 inches and about 0.2 inches. The spacing may vary depending on the gases being delivered and the process conditions during deposition. Choke 262 helps provide a more uniform pressure distribution within the volume or reaction zone 264 defined between chamber lid assembly 232 and substrate 210 by isolating reaction zone 264 from the non-uniform pressure distribution of pumping zone 266 (
Referring to
Since reaction zone 264 may contain a smaller volume when compared to the inner volume of a conventional CVD chamber, a smaller amount of gas is required to fill reaction zone 264 for a particular process in an atomic layer deposition sequence. For example, in one embodiment, the volume of reaction zone 264 is about 1,000 cm3 or less, preferably 500 cm3 or less, and more preferably 200 cm3 or less for a chamber adapted to process 200 mm diameter substrates. In one embodiment, the volume of reaction zone 264 is about 3,000 cm3 or less, preferably 1,500 cm3 or less, and more preferably 600 cm3 or less for a chamber adapted to process 300 mm diameter substrates. In one embodiment, substrate support 212 may be raised or lowered to adjust the volume of reaction zone 264 for deposition. Because of the smaller volume of reaction zone 264, less gas, whether a deposition gas or a purge gas, is necessary to be flowed into process chamber 200. Therefore, the throughput of process chamber 200 is greater and the waste may be minimized due to the smaller amount of gas used reducing the cost of operation.
Chamber lid assembly 232 has been shown in
Chamber lid assembly 232 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 232 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 232. For example, water channels (not shown) may be formed in chamber lid assembly 232 to cool chamber lid assembly 232. In another example, heating elements (not shown) may be embedded or may surround components of chamber lid assembly 232 to heat chamber lid assembly 232. In one embodiment, components of chamber lid assembly 232 may be individually heated or cooled. For example, referring to
Chamber lid assembly 232 contains components that may be made of stainless steel, aluminum, nickel-plated aluminum, nickel, or other suitable materials compatible with the processing to be performed. In one embodiment, lid cap 272 contains aluminum or stainless steel and lid plate 270 contains aluminum. In another embodiment, the optional additional plate disposed between lid plate 270 and lid cap 272 contains stainless steel.
In one embodiment, inner surface 261 of expanding channel 234 (including both inner surfaces of lid plate 270 and lid cap 272) and lower surface 260 of chamber lid assembly 232 may contain a mirror polished surface to help produce a laminar flow of a gas along expanding channel 234 and lower surface 260 of chamber lid assembly 232. In another embodiment, the inner surface of gas conduits 250a, 250b may be electropolished to help produce a laminar flow of a gas therethrough.
In an alternative embodiment, inner surface 261 of expanding channel 234 (including both inner surfaces of lid plate 270 and lid cap 272) and lower surface 260 of chamber lid assembly 232 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surface 261 and lower surface 260. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surface 261 and lower surface 260 to contaminate substrate 210. In one example, the mean roughness (Ra) of lower surface 260 and/or inner surface 261 may be at least about 10 microinches (μin), such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of lower surface 260 and/or inner surface 261 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
Returning to
The control unit 280 may be one of any form of general purpose computer processor that can be used in an industrial setting for controlling various chambers and sub-processors. The CPU 282 may use any suitable memory 1186, such as random access memory, read only memory, floppy disk drive, hard disk, or any other form of digital storage, local or remote. Various support circuits may be coupled to the CPU 282 for supporting process chamber 200. The control unit 280 may be coupled to another controller that is located adjacent individual chamber components, such as programmable logic controllers 248a, 248b of valves 242a, 242b. Bi-directional communications between the control unit 280 and various other components of process chamber 200 are handled through numerous signal cables collectively referred to as signal buses 288, some of which are illustrated in
Referring to
Process chamber 200 as illustrated in
For example,
In another example,
The gas delivery apparatuses 230, 830, 930 of
Gas delivery system 230 of
Embodiments of chambers 200, 800, and 900 with gas delivery apparatuses 230, 830, and 930 as described in
For clarity reasons, deposition of a layer by atomic layer deposition will be described in more detail in reference to the atomic layer deposition of a tantalum nitride layer utilizing process chamber 200 as described in
It is believed that the adsorption processes used to adsorb the monolayer of the reactants, such as the tantalum precursor and the nitrogen precursor, are self-limiting in that only one monolayer may be adsorbed onto the surface of the substrate structure during a given pulse because the surface of the substrate structure has a finite number of sites for adsorbing the reactants. Once the finite number of sites is occupied by the reactants, such as the tantalum precursor or the nitrogen precursor, further absorption of the reactants will be blocked. The cycle may be repeated to a desired thickness of the tantalum nitride layer.
Pulses of a tantalum precursor, such as pentakis(dimethylamido) tantalum (PDMAT; Ta(NMe2)5), may be introduced by gas source 238 through valve 242a. The tantalum precursor may be provided with the aid of a carrier gas, which includes, but is not limited to, helium (He), argon (Ar), nitrogen (N2), hydrogen (H2), and combinations thereof. Pulses of a nitrogen precursor, such as ammonia, may be introduced by gas source 239 through valve 242a. A carrier gas may also be used to help deliver the nitrogen precursor. A purge gas, such as argon, may be introduced by gas source 240 through valve 242a and/or through valve 242b. In one aspect, the flow of purge gas may be continuously provided by gas source 240 through valves 242a, 242b to act as a purge gas between the pulses of the tantalum precursor and of the nitrogen precursor and to act as a carrier gas during the pulses of the tantalum precursor and the nitrogen precursor. In one aspect, delivering a purge gas through two gas conduits 250a, 250b provides a more complete purge of reaction zone 264 rather than a purge gas provided through one of gas conduit 250a or 250b. In one aspect, a reactant gas may be delivered through one of gas conduits 250a or 250b since uniformity of flow of a reactant gas, such as a tantalum precursor or a nitrogen precursor, is not as critical as uniformity of the purge gas due to the self-limiting absorption process of the reactants on the surface of substrate structures. In other embodiments, a purge gas may be provided in pulses. In other embodiments, a purge gas may be provided in more or less than two gas flows. In other embodiments, a tantalum precursor gas may be provided in more than a single gas flow (i.e., two or more gas flows). In other embodiments, a nitrogen precursor gas may be provided in more than a single gas flow (i.e., two or more gas flows).
Other examples of tantalum precursors, include, but are not limited to, other metal-organic precursors or derivatives thereof, such as pentakis(ethylmethylamido) tantalum (PEMAT; Ta(N(Et)Me)5), pentakis(diethylamido) tantalum (PDEAT; Ta(NEt2)5), and derivatives of PEMAT, PDEAT, or PDMAT. Other tantalum precursors include without limitation TBTDET (Ta(NEt2)3NC4H9 or C16H39N4Ta) and tantalum halides, for example TaX5 where X is fluorine (F), bromine (Br) or chlorine (Cl), and/or derivatives thereof. Other nitrogen precursors may be used which include, but are not limited to, NxHy with x and y being integers (e.g., hydrazine (N2H4)), dimethyl hydrazine ((CH3)2N2H2), tertbutylhydrazine (C4H9N2H3), phenylhydrazine (C6H5N2H3), other hydrazine derivatives, a nitrogen plasma source (e.g., N2, N2/H2, NH3, or a N2H4 plasma), 2,2′-azotertbutane ((CH3)6C2N2), ethylazide (C2H5N3), and other suitable gases. Other examples of purge gases or carrier gases include, but are not limited to, helium (He), nitrogen (N2), hydrogen (H2), other gases, and combinations thereof.
The tantalum nitride layer formation is described as starting with the absorption of a monolayer of a tantalum precursor on the substrate followed by a monolayer of a nitrogen precursor. Alternatively, the tantalum nitride layer formation may start with the absorption of a monolayer of a nitrogen precursor on the substrate followed by a monolayer of the tantalum precursor. Furthermore, in other embodiments, a pump evacuation alone between pulses of reactant gases may be used to prevent mixing of the reactant gases.
The time duration for each pulse of the tantalum precursor, the time duration for each pulse of the nitrogen precursor, and the duration of the purge gas flow between pulses of the reactants are variable and depend on the volume capacity of a deposition chamber employed as well as a vacuum system coupled thereto. For example, (1) a lower chamber pressure of a gas will require a longer pulse time; (2) a lower gas flow rate will require a longer time for chamber pressure to rise and stabilize requiring a longer pulse time; and (3) a large-volume chamber will take longer to fill, longer for chamber pressure to stabilize thus requiring a longer pulse time. Similarly, time between each pulse is also variable and depends on volume capacity of the process chamber as well as the vacuum system coupled thereto. In general, the time duration of a pulse of the tantalum precursor or the nitrogen precursor should be long enough for absorption of a monolayer of the compound. In one aspect, a pulse of a tantalum precursor may still be in the chamber when a pulse of a nitrogen precursor enters. In general, the duration of the purge gas and/or pump evacuation should be long enough to prevent the pulses of the tantalum precursor and the nitrogen precursor from mixing together in the reaction zone.
Generally, a pulse time of about 1.0 second or less for a tantalum precursor and a pulse time of about 1.0 second or less for a nitrogen precursor are typically sufficient to adsorb alternating monolayers on a substrate structure. A time of about 1.0 second or less between pulses of the tantalum precursor and the nitrogen precursor is typically sufficient for the purge gas, whether a continuous purge gas or a pulse of a purge gas, to prevent the pulses of the tantalum precursor and the nitrogen precursor from mixing together in the reaction zone. Of course, a longer pulse time of the reactants may be used to ensure absorption of the tantalum precursor and the nitrogen precursor and a longer time between pulses of the reactants may be used to ensure removal of the reaction by-products.
During atomic layer deposition, substrate 210 may be maintained approximately below a thermal decomposition temperature of a selected tantalum precursor. An exemplary heater temperature range to be used with tantalum precursors identified herein is approximately between about 20° C. and about 500° C. at a chamber pressure less than about 100 Torr, preferably less than 50 Torr. When the tantalum containing gas is PDMAT, the heater temperature is preferably between about 100° C. and about 300° C., more preferably between about 175° C. and 250° C., and the chamber pressure is between about 1.0 Torr and about 5.0 Torr. In other embodiments, it should be understood that other temperatures and pressures may be used. For example, a temperature above a thermal decomposition temperature may be used. However, the temperature should be selected so that more than 50 percent of the deposition activity is by absorption processes. In another example, a temperature above a thermal decomposition temperature may be used in which the amount of decomposition during each precursor deposition is limited so that the growth mode will be similar to an atomic layer deposition growth mode.
One exemplary process of depositing a tantalum nitride layer by atomic layer deposition, in process chamber 200 of
In one embodiment, the layer, such as a tantalum nitride layer, is deposited to a sidewall coverage of about 50 Å or less. In another embodiment, the layer is deposited to a sidewall coverage of about 20 Å or less. In still another embodiment, the layer is deposited to a sidewall coverage of about 10 Å or less. A tantalum nitride layer with a thickness of about 10 Åor less is believed to be a sufficient thickness in the application as a barrier layer to prevent copper diffusion. In one aspect, a thin barrier layer may be used to advantage in filling submicron (e.g., less than 0.15 μm) and smaller features having high aspect ratios (e.g., greater than 5 to 1). Of course, a layer having a sidewall coverage of greater than 50 Å may be used.
Embodiments of atomic layer deposition have been described above as absorption of a monolayer of reactants on a substrate. The invention also includes embodiments in which the reactants are deposited to more or less than a monolayer. The invention also includes embodiments in which the reactants are not deposited in a self-limiting manner. The invention also includes embodiments in which deposition occurs in mainly a chemical vapor deposition process in which the reactants are delivered sequentially or simultaneously.
Coverage-Diverge Lid Assembly
Gas conduit cover 1052 contains at least one gas conduit, or may contain two, three, or more gas conduits.
Conduit 1050c is an optional conduit in some embodiments. Gas conduit 1050c may be coupled to and in fluid communication with lid cap 1072 on one end, while the other end of gas conduit 1050c extends through lid plate 1070 and may be coupled to and in fluid communication with an ALD valve and gas source, such as a carrier gas source, a purge gas source, a plasma gas, or a chemical precursor source. In another embodiment, conduit 1050c is may be coupled to and in fluid communication with the top surface of lid cap 1072. In another embodiment, conduit 1050c is may be combined with conduit 1050b, such as with a Y-joint, and may be coupled to and in fluid communication with gas conduit 1068b.
Chamber lid assembly 1032 has been shown in
Chamber lid assembly 1032 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1032 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1032. For example, coolant channel 1090 may be formed in chamber lid assembly 1032 to cool chamber lid assembly 1032. In another example, heating elements (not shown) may be embedded or may surround components of chamber lid assembly 1032 to heat chamber lid assembly 1032. In one embodiment, components of chamber lid assembly 1032 may be individually heated or cooled. For example, referring to
Chamber lid assembly 1032 contains components that may be made of stainless steel, aluminum, nickel-plated aluminum, nickel, or other suitable materials compatible with the processing to be performed. In one embodiment, lid cap 1072 and lid plate 1070 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof.
In one embodiment, gas dispersing channel 1028 and lower surface 1060 of chamber lid assembly 1032 may contain a mirror polished surface to help produce a laminar flow of a gas along gas dispersing channel 1028 and lower surface 1060 of chamber lid assembly 1032. In another embodiment, the inner surface of gas conduits 1050a, 1050b, 1150c, 1068a, or 1068b may be electropolished to help produce a laminar flow of a gas therethrough.
In one embodiment, inner surfaces 1035a, 1035b, and 1035c of dispersing channel 1028 and lower surface 1060 of chamber lid assembly 1032 may contain a mirror polished surface to help produce a laminar flow of a gas along dispersing channel 1028 and lower surface 1060 of chamber lid assembly 1032. In another embodiment, the inner surface of gas conduits 1050a, 1050b, and 1050c may be electropolished to help produce a laminar flow of a gas therethrough.
In an alternative embodiment, inner surfaces 1035a, 1035b, and 1035c of dispersing channel 1028 and lower surface 1060 of chamber lid assembly 1032 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surfaces 1035a, 1035b, and 1035c and lower surface 1060. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surfaces 1035a, 1035b, and 1035c and lower surface 1060 to contaminate substrate 1010. In one example, the mean roughness (Ra) of inner surfaces 1035a, 1035b, and/or 1035c and lower surface 1060 may be at least about 10 μin, such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of inner surfaces 1035a, 1035b, and/or 1035c and lower surface 1060 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
Processes gases, as circular gas flow 1020 depicted in
In one example, chamber lid assembly 1032 adapted to process 300 mm diameter substrates may have the following diameters. The diameter at upper portion 1037 of gas dispersing channel 1028 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch. The diameter at throttle 1036 of gas dispersing channel 1028 may be within a range from about 0.1 inches to about 1.5 inches, preferably, from about 0.3 inches to about 0.9 inches, and more preferably, from 0.5 inches to about 0.8 inches, for example, about 0.66 inches. The diameter at lower portion 1035 of gas dispersing channel 1028 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch.
In general, the above dimension apply to gas dispersing channel 1028 adapted to provide a total gas flow of between about 500 sccm and about 3,000 sccm. In other specific embodiments, the dimension may be altered to accommodate a certain gas flow therethrough. In general, a larger gas flow will require a larger diameter of gas dispersing channel 1028.
Not wishing to be bound by theory, it is believed that the diameter of gas dispersing channel 1028, which is gradually decreasing from upper portion 1037 of gas dispersing channel 1028 to throttle 1036 and increasing from throttle 1036 to lower portion 1035 of gas dispersing channel 1028, allows less of an adiabatic expansion of a gas through gas dispersing channel 1028 which helps to control the temperature of the process gas contained in circular flow gas 1020. For instance, a sudden adiabatic expansion of a gas delivered through gas inlet 1038A, 1038B into gas dispersing channel 1028 may result in a drop in the temperature of the gas which may cause condensation of the gas and formation of droplets. On the other hand, gas dispersing channel 1028 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1032). Gas dispersing channel 1028 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas inlets 1038A, 1038B are located adjacent upper portion 1037 of gas dispersing channel 1028, as depicted in
Each gas conduit 1050a, 1050b, 1050c, 1068a, or 1068b may be positioned at an angle α from the centerline of the gas conduit and from a radius line of gas dispersing channel 1028, similarly as depicted in
Not wishing to be bound by theory,
In one example, lower surface 1060 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1060 of chamber lid assembly 1032 and a substrate while assisting to provide uniform exposure of the surface of a substrate to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 1060 of chamber lid assembly 1032 and the surface of a substrate is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of a substrate helps provide a more uniform deposition of the gas on a substrate. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on a substrate surface. Thus, a higher velocity of a gas at a first area of the surface of a substrate versus a second area of the surface of a substrate is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1032 having lower surface 1060, downwardly sloping, provides for more uniform deposition of the gas across the surface of a substrate because lower surface 1060 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of a substrate.
Lid cap 1072, gas conduit 1050a, gas conduit cover 1052, and a portion of the upper surface of lid plate 1070 may be covered by chamber lid cover 1080 having handles 1082, as illustrated in
Substrate support 1112 supports substrate 1110 on substrate receiving surface 1111 in process chamber 1100. Substrate support 1112 is mounted to lift motor 1114 for raising and lowering substrate support 1112 and substrate 1110 disposed thereon. Lift plate 1116 connected to lift motor 1118 is mounted in process chamber 1100 and raises and lowers lift pins 1120 movably disposed through substrate support 1112. Lift pins 1120 raise and lower substrate 1110 over the surface of substrate support 1112. Substrate support 1112 may include a vacuum chuck (not shown), an electrostatic chuck (not shown), or a clamp ring (not shown) for securing substrate 1110 to substrate support 1112 during a deposition process.
The temperature of substrate support 1112 may be adjusted to control the temperature of substrate 1110 disposed thereon. For example, substrate support 1112 may be heated using an embedded heating element, such as a resistive heater (not shown), or may be heated using radiant heat, such as heating lamps (not shown) disposed above substrate support 1112. Purge ring 1122 may be disposed on substrate support 1112 to define purge channel 1124 which provides a purge gas to a peripheral portion of substrate 1110 to prevent deposition thereon.
Gas delivery system 1130 is disposed at an upper portion of chamber body 1102 to provide a gas, such as a process gas and/or a purge gas, to process chamber 1100.
In one embodiment, gas delivery system 1130 contains chamber lid assembly 1132 having gas dispersing channel 1128 extending through a central portion of chamber lid assembly 1132. Gas dispersing channel 1128 extends perpendicular to substrate receiving surface 1111 and also extends along central axis 1133 of gas dispersing channel 1128, through lid plate 1170, and to lower surface 1160. Converging channel 1134a is a portion of gas dispersing channel 1128 that tapers towards central axis 1133 within upper portion 1137 of gas dispersing channel 1128. Diverging channel 1134b is a portion of gas dispersing channel 1128 that tapers away from central axis 1133 within lower portion 1135 of gas dispersing channel 1128. Throttle 1131 is a narrow passage separating converging channel 1134a and diverging channel 1134b. Gas dispersing channel 1128 further extends pass lower surface 1160 and into reaction zone 1164. Lower surface 1160 extends from diverging channel 1134 to choke 1162. Lower surface 1160 is sized and shaped to substantially cover substrate 1110 disposed on substrate receiving surface 1111 of substrate support 1112.
Processes gases, as circular gas flow 1174, are forced to make more revolutions around central axis 1133 of gas dispersing channel 1128 while passing through throttle 1131, than in similarly configured process chamber in the absence of throttle 1131. Circular gas flow 1174 may contain a flow pattern, such as a vortex pattern, a helix pattern, a spiral pattern, a twirl pattern, a twist pattern, a coil pattern, a whirlpool pattern, or derivatives thereof. Circular gas flow 1174 may extend at least about 1 revolution around central axis 1133 of gas dispersing channel 1128, preferably, at least about 1.5 revolutions, more preferably, at least about 2 revolutions, more preferably, at least about 3 revolutions, and more preferably, about 4 revolutions or more.
Gas dispersing channel 1128 has gas inlets 1136a, 1136b to provide gas flows from two similar pairs of valves 1142a/1152a, 1142b/1152b, which may be provided together and/or separately. In one configuration, valve 1142a and valve 1142b are coupled to separate reactant gas sources but are preferably coupled to the same purge gas source. For example, valve 1142a is coupled to reactant gas source 1138 and valve 1142b is coupled to reactant gas source 1139, and both valves 1142a, 1142b are coupled to purge gas source 1140. Each valve 1142a, 1142b includes delivery line 1143a, 1143b having valve seat assembly 1144a, 1144b and each valve 1152a, 1152b includes purge line 1145a, 1145b having valve seat assembly 1146a, 1146b. Delivery line 1143a, 1143b is in fluid communication with reactant gas source 1138, 1143 and is in fluid communication with gas inlet 1136a, 1136b of gas dispersing channel 1128. Valve seat assembly 1144a, 1144b of the delivery line 1143a, 1143b controls the flow of the reactant gas from reactant gas source 1138, 1143 to gas dispersing channel 1128. Purge line 1145a, 1145b is in fluid communication with purge gas source 1140 and intersects delivery line 1143a, 1143b downstream of valve seat assembly 1144a, 1144b of delivery line 1143a, 1143b. Valve seat assembly 1146a, 1146b of purge line 1145a, 1145b controls the flow of the purge gas from purge gas source 1140 to gas dispersing channel 1128. If a carrier gas is used to deliver reactant gases from reactant gas source 1138, 1143, preferably the same gas is used as a carrier gas and a purge gas (i.e., an argon gas used as a carrier gas and a purge gas).
Each valve seat assembly 1144a, 1144b, 1146a, 1146b may contain a diaphragm (not shown) and a valve seat (not shown). The diaphragm may be biased open or closed and may be actuated closed or open respectively. The diaphragms may be pneumatically actuated or may be electrically actuated. Pneumatically actuated valves include pneumatically actuated valves available from Fujikin, Inc. and Veriflo Division, Parker Hannifin, Corp. Electrically actuated valves include electrically actuated valves available from Fujikin, Inc. For example, an ALD valve that may be used is the Fujikin Model No. FPR-UDDFAT-21-6.35-PI-ASN or the Fujikin Model No. FPR-NHDT-21-6.35-PA-AYT. Programmable logic controllers 1148a, 1148b may be coupled to valves 1142a, 1142b to control actuation of the diaphragms of valve seat assemblies 1144a, 1144b, 1146a, 1146b of valves 1142a, 1142b. Pneumatically actuated valves may provide pulses of gases in time periods as low as about 0.020 seconds. Electrically actuated valves may provide pulses of gases in time periods as low as about 0.005 seconds. An electrically actuated valve typically requires the use of a driver coupled between the valve and the programmable logic controller.
Each valve 1142a, 1142b may be a zero dead volume valve to enable flushing of a reactant gas from delivery line 1143a, 1143b when valve seat assembly 1144a, 1144b is closed. For example, purge line 1145a, 1145b may be positioned adjacent valve seat assembly 1144a, 1144b of delivery line 1143a, 1143b. When valve seat assembly 1144a, 1144b is closed, purge line 1145a, 1145b may provide a purge gas to flush delivery line 1143a, 1143b. In one embodiment, purge line 1145a, 1145b is positioned slightly spaced from valve seat assembly 1144a, 1144b of delivery line 1143a, 1143b so that a purge gas is not directly delivered into valve seat assembly 1144a, 1144b when open. A zero dead volume valve as used herein is defined as a valve which has negligible dead volume (i.e., not necessary zero dead volume).
Each valve pair 1142a/1152a, 1142b/1152b may be adapted to provide a combined gas flow and/or separate gas flows of the reactant gas and the purge gas. In reference to valve pair 1142a/1152a, one example of a combined gas flow of the reactant gas and the purge gas includes a continuous flow of a purge gas from purge gas source 1140 through purge line 1145a and pulses of a reactant gas from reactant gas source 1138 through delivery line 1143a. The continuous flow of the purge gas may be provided by leaving the diaphragm of valve seat assembly 1146a of purge line 1145a open. The pulses of the reactant gas from reactant gas source 1138 may be provided by opening and closing the diaphragm of valve seat assembly 1144a of delivery line 1143a. In reference to valve pair 1142a/1152a, one example of separate gas flows of the reactant gas and the purge gas includes pulses of a purge gas from purge gas source 1140 through purge line 1145a and pulses of a reactant gas from reactant gas source 1138 through delivery line 1143a. The pulses of the purge gas may be provided by opening and closing the diaphragm of valve seat assembly 1146a of purge line 1145a. The pulses of the reactant gas from reactant gas source 1138 may be provided by opening and closing the diaphragm of valve seat assembly 1144a of delivery line 1143a.
Delivery lines 1143a, 1143b of valves 1142a, 1142b may be coupled to gas inlets 1136a, 1136b through gas conduits 1150a, 1150b. Gas conduits 1150a, 1150b may be integrated or may be separate from valves 1142a, 1142b. In one aspect, valves 1142a, 1142b are coupled in close proximity to gas dispersing channel 1128 to reduce any unnecessary volume of delivery line 1143a, 1143b and gas conduits 1150a, 1150b between valves 1142a, 1142b and gas inlets 1136a, 1136b.
In general, the above dimension apply to gas dispersing channel 1128 adapted to provide a total gas flow of between about 500 sccm and about 3,000 sccm. In other specific embodiments, the dimension may be altered to accommodate a certain gas flow therethrough. In general, a larger gas flow will require a larger diameter of gas dispersing channel 1128.
Not wishing to be bound by theory, it is believed that the diameter of gas dispersing channel 1128, which is gradually decreasing from upper portion 1137 of gas dispersing channel 1128 to throttle 1131 and increasing from throttle 1131 to lower portion 1135 of gas dispersing channel 1128, allows less of an adiabatic expansion of a gas through gas dispersing channel 1128 which helps to control the temperature of the process gas contained in circular flow gas 1174. For instance, a sudden adiabatic expansion of a gas delivered through gas inlet 1136a, 1136b into gas dispersing channel 1128 may result in a drop in the temperature of the gas which may cause condensation of the gas and formation of droplets. On the other hand, gas dispersing channel 1128 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1132). Gas dispersing channel 1128 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas inlets 1136a, 1136b are located adjacent upper portion 1137 of gas dispersing channel 1128. In other embodiments, one or more gas inlets 1136a, 1136b may be located along the length of gas dispersing channel 1128 between upper portion 1137 and lower portion 1135.
Each gas conduit 1150a, 1150b may be positioned at an angle α from the centerline of the gas conduit 1150a, 1150b and from a radius line of gas dispersing channel 1128, similarly as depicted in
Not wishing to be bound by theory,
In one embodiment,
Distance 1177a as the length of converging channel 1134a along central axis 1133 within lid cap 1172 between upper portion 1137 of gas dispersing channel 1128 and throttle 1131 and distance 1177b as the length of diverging channel 1134b along central axis 1133 within lid cap 1172 between throttle 1131 and lower surface 1173 of lid cap 1172. In one example, distance 1177a may have a length within a range from about 1 inch to about 4 inches, preferably, from about 1.25 inches to about 3 inches, and more preferably, from 1.5 inches to about 2.5 inches, for example, about 2 inches and distance 1177b may have a length within a range from about 0.5 inches to about 4 inches, preferably, from about 1 inch to about 3 inches, and more preferably, from 1.25 inches to about 1.75 inches, for example, about 1.5 inches.
In one example, lower surface 1160 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1160 of chamber lid assembly 1132 and substrate 1110 while assisting to provide uniform exposure of the surface of substrate 1110 to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 1160 of chamber lid assembly 1132 and the surface of substrate 1110 is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of substrate 1110 helps provide a more uniform deposition of the gas on substrate 1110. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on substrate 1110 surface. Thus, a higher velocity of a gas at a first area of the surface of substrate 1110 versus a second area of the surface of substrate 1110 is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1132 having lower surface 1160, downwardly sloping, provides for more uniform deposition of the gas across the surface of substrate 1110 because lower surface 1160 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of substrate 1110.
In one specific embodiment, the spacing between choke 1162 and substrate support 1112 is between about 0.04 inches and about 2.0 inches, and preferably between 0.04 inches and about 0.2 inches. The spacing may vary depending on the gases being delivered and the process conditions during deposition. Choke 1162 helps provide a more uniform pressure distribution within the volume or reaction zone 1164 defined between chamber lid assembly 1132 and substrate 1110 by isolating reaction zone 1164 from the non-uniform pressure distribution of pumping zone 1166 (
Referring to
Since reaction zone 1164 may contain a smaller volume when compared to the inner volume of a conventional CVD chamber, a smaller amount of gas is required to fill reaction zone 1164 for a particular process in an atomic layer deposition sequence. For example, in one embodiment, the volume of reaction zone 1164 is about 1,000 cm3 or less, preferably 500 cm3 or less, and more preferably 200 cm3 or less for a chamber adapted to process 200 mm diameter substrates. In one embodiment, the volume of reaction zone 1164 is about 3,000 cm3 or less, preferably 1,500 cm3 or less, and more preferably 600 cm3 or less for a chamber adapted to process 300 mm diameter substrates. In one embodiment, substrate support 1112 may be raised or lowered to adjust the volume of reaction zone 1164 for deposition. Because of the smaller volume of reaction zone 1164, less gas, whether a deposition gas or a purge gas, is necessary to be flowed into process chamber 1100. Therefore, the throughput of process chamber 1100 is greater and the waste may be minimized due to the smaller amount of gas used reducing the cost of operation.
Chamber lid assembly 1132 contains lid cap 1172 and lid plate 1170 in which lid cap 1172 and lid plate 1170 form gas dispersing channel 1128, as depicted in
Chamber lid assembly 1132 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1132 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1132. For example, water channels (such as coolant channel 1090 in
The components and parts of chamber lid assembly 1132 may contain materials such as stainless steel, aluminum, nickel-plated aluminum, nickel, alloys thereof, or other suitable materials. In one embodiment, lid cap 1172 and lid plate 1170 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof.
In one embodiment, the inner surfaces of gas dispersing channel 1128 (including both inner surfaces of lid plate 1170 and lid cap 1172) and lower surface 1160 of chamber lid assembly 1132 may contain a mirror polished surface to help produce a laminar flow of a gas along gas dispersing channel 1128 and lower surface 1160 of chamber lid assembly 1132. In another embodiment, the inner surface of gas conduits 1150a, 1150b may be electropolished to help produce a laminar flow of a gas therethrough.
In an alternative embodiment, the inner surfaces of gas dispersing channel 1128 (including both inner surfaces of lid plate 1170 and lid cap 1172) and lower surface 1160 of chamber lid assembly 1132 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on the inner surfaces of lid plate 1170 and lid cap 1172 and lower surface 1160. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from lower surface 1160 and the inner surfaces of gas dispersing channel 1128 to contaminate substrate 1110. In one example, the mean roughness (Ra) of lower surface 1160 and/or the inner surfaces of gas dispersing channel 1128 may be at least about 10 μin, such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of lower surface 1160 and/or the inner surfaces of gas dispersing channel 1128 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
Control unit 1180 may be one of any form of general purpose computer processor that can be used in an industrial setting for controlling various chambers and sub-processors. CPU 1182 may use any suitable memory 1186, such as random access memory, read only memory, floppy disk drive, hard disk, or any other form of digital storage, local or remote. Various support circuits may be coupled to CPU 1182 for supporting process chamber 1100. Control unit 1180 may be coupled to another controller that is located adjacent individual chamber components, such as programmable logic controllers 1148a, 1148b of valves 1142a, 1142b. Bi-directional communications between the control unit 1180 and various other components of process chamber 1100 are handled through numerous signal cables collectively referred to as signal buses 1188, some of which are illustrated in
Referring to
Process chamber 1100, as illustrated in
Multiple Injection Lid Assembly
Gas conduit cover 1252 contains at least one gas conduit, or may contain two, three, or more gas conduits.
Conduit 1250c is an optional conduit in some embodiments. Gas conduit 1250c may be coupled to and in fluid communication with lid cap 1272 on one end, while the other end of gas conduit 1250c extends through lid plate 1270 and may be coupled to and in fluid communication with an ALD valve and/or gas source, such as a carrier gas source, a purge gas source, a plasma gas, or a chemical precursor source. In another embodiment, conduit 1250c is may be coupled to and in fluid communication with the top surface of lid cap 1272. In another embodiment, conduit 1250c may be combined with conduit 1250b, such as with a Y-joint, and may be coupled to and in fluid communication with gas passageway 1268b.
Slots 1266a and 1266b provide fluid communication from gas annulets 1264a and 1264b to gas dispersing channel 1228. Slots 1266a and 1266b may be positioned at an angle relative to central axis 1233, such as about tangential to central axis 1233 or gas dispersing channel 1228. In one embodiment, slots 1266a and 1266b are positioned at an angle tangential to gas dispersing channel 1228, such as within a range from about 0° to about 90°, preferably, from about 0° to about 45°, and more preferably, from about 0° to about 20°.
Chamber lid assembly 1232 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1232 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1232. For example, coolant channel 1290 may be formed in chamber lid assembly 1232 to cool chamber lid assembly 1232. In another example, heating elements (not shown) may be embedded or may surround components of chamber lid assembly 1232 to heat chamber lid assembly 1232. In one embodiment, components of chamber lid assembly 1232 may be individually heated or cooled during a process. For example, referring to
Chamber lid assembly 1232 contains components that may be made of stainless steel, aluminum, nickel-plated aluminum, nickel, or other suitable materials compatible with the processing to be performed. In one embodiment, multi-injector base 1269, lid cap 1272, and lid plate 1270 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof. In one embodiment, the optional additional plate disposed therebetween contains stainless steel.
In one embodiment, inner surface 1231 of gas dispersing channel 1228 (including both inner surfaces of lid plate 1270 and lid cap 1272) and lower surface 1260 of chamber lid assembly 1232 may contain a mirror polished surface to help produce a laminar flow of a gas along gas dispersing channel 1228 and lower surface 1260 of chamber lid assembly 1232.
In an alternative embodiment, inner surface 1231 of gas dispersing channel 1228 (including both inner surfaces of lid plate 1270 and lid cap 1272) and lower surface 1260 of chamber lid assembly 1232 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surface 1231 and lower surface 1260. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surface 1231 and lower surface 1260 to contaminate substrate 1210. In one example, the mean roughness (Ra) of lower surface 1260 and/or inner surface 1231 may be at least about 10 μin, such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of lower surface 1260 and/or inner surface 1231 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
FIGS. 13A and 14A-14C depict a cross-sectional view of chamber lid assembly 1232 containing gas dispersing channel 1228 extending through a central portion of lid plate 1270. Gas annulets 1264a and 1264b annularly extend around gas dispersing channel 1228 and central axis 1233. Gas dispersing channel 1228 is usually positioned to extend perpendicular to a substrate that is positioned below chamber lid assembly 1232 during an ALD process. Gas dispersing channel 1228 extends along central axis 1233 of lid cap 1272, through lid plate 1270, and to lower surface 1260. Gas dispersing channel 1228 further extends pass lower surface 1260 and into reaction zone 1064. Lower surface 1260 extends from gas dispersing channel 1228 to choke 1262. Lower surface 1260 is sized and shaped to substantially cover the substrate that is positioned below chamber lid assembly 1232 during the ALD process.
FIGS. 13A and 14A-14C depict chamber lid assembly 1232 configured to expose a substrate to at least two gas sources or chemical precursors. In other examples, chamber lid assembly 1232 may be reconfigured to expose a substrate to a single gas source (as depicted in
Processes gases, as circular gas flow 1220 depicted in
In one example, chamber lid assembly 1232 adapted to process 300 mm diameter substrates may have the following diameters. The diameter at upper portion 1237 of gas dispersing channel 1228 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch. The diameter at point 1236 of gas dispersing channel 1228 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch. The diameter at lower portion 1235 of gas dispersing channel 1228 may be within a range from about 1 inch to about 4 inches, preferably, from about 1.5 inches to about 3 inches, and more preferably, from 1.6 inches to about 2.4 inches, for example, about 2 inches. In one embodiment, the above dimensions apply to gas dispersing channel 1228 adapted to provide a gas flow within a range from about 500 sccm and about 3,000 sccm. In other embodiments, the dimensions of gas dispersing channel 1228 may be altered to accommodate a certain gas flow therethrough.
Gas dispersing channel 1228 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1232). Gas dispersing channel 1228 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas annulets 1264a and 1264b circumvents upper portion 1237 of gas dispersing channel 1228, as depicted in
Not wishing to be bound by theory,
In one example, lower surface 1260 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1260 of chamber lid assembly 1232 and a substrate while assisting to provide uniform exposure of the surface of a substrate to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between downwardly sloping lower surface 1260 of chamber lid assembly 1232 and the surface of a substrate is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of a substrate helps provide a more uniform deposition of the gas on a substrate. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on a substrate surface. Thus, a higher velocity of a gas at a first area of the surface of a substrate versus a second area of the surface of a substrate is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1232 having lower surface 1260, downwardly sloping, provides for more uniform deposition of the gas across the surface of a substrate because lower surface 1260 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of a substrate.
Lid cap 1272, gas conduit 1250a, gas conduit cover 1252, and a portion of upper surface of lid plate 1270 may be covered by chamber lid cover 1280 having handles 1282, as illustrated in
Substrate support 1512 supports substrate 1510 on substrate receiving surface 1511 in process chamber 1500. Substrate support 1512 is mounted to lift motor 1514 for raising and lowering substrate support 1512 and substrate 1510 disposed thereon. Lift plate 1516 connected to lift motor 1518 is mounted in process chamber 1500 and raises and lowers lift pins 1520 movably disposed through substrate support 1512. Lift pins 1520 raise and lower substrate 1510 over the surface of substrate support 1512. Substrate support 1512 may include a vacuum chuck (not shown), an electrostatic chuck (not shown), or a clamp ring (not shown) for securing substrate 1510 to substrate support 1512 during a deposition process.
The temperature of substrate support 1512 may be adjusted to control the temperature of substrate 1510 disposed thereon. For example, substrate support 1512 may be heated using an embedded heating element, such as a resistive heater (not shown), or may be heated using radiant heat, such as heating lamps (not shown) disposed above substrate support 1512. Purge ring 1522 may be disposed on substrate support 1512 to define purge channel 1524 which provides a purge gas to a peripheral portion of substrate 1510 to prevent deposition thereon.
Gas delivery system 1530 is disposed at an upper portion of chamber body 1502 to provide a gas, such as a process gas and/or a purge gas, to process chamber 1500.
In one embodiment, gas delivery system 1530 contains chamber lid assembly 1532 having gas dispersing channel 1534 extending through a central portion of chamber lid assembly 1532. Gas dispersing channel 1534 extends perpendicular towards substrate receiving surface 1511 and also extends along central axis 1533 of gas dispersing channel 1534, through lid plate 1570, and to lower surface 1560. In one example, a portion of gas dispersing channel 1534 is substantially cylindrical along central axis 1533 within upper portion 1537 and a portion of gas dispersing channel 1534 that tapers away from central axis 1533 within lower portion 1535 of gas dispersing channel 1534. Gas dispersing channel 1534 further extends pass lower surface 1560 and into reaction zone 1564. Lower surface 1560 extends from lower portion 1535 of gas dispersing channel 1534 to choke 1562. Lower surface 1560 is sized and shaped to substantially cover substrate 1510 disposed on substrate receiving surface 1511 of substrate support 1512.
Processes gases, as circular gas flow 1574, are forced to make revolutions around central axis 1533 of gas dispersing channel 1534 while passing along central axis 1533. Circular gas flow 1574 may contain a flow pattern, such as a vortex pattern, a helix pattern, a spiral pattern, a twirl pattern, a twist pattern, a coil pattern, a whirlpool pattern, or derivatives thereof. Circular gas flow 1574 may extend at least about 1 revolution around central axis 1533 of gas dispersing channel 1534, preferably, at least about 1.5 revolutions, more preferably, at least about 2 revolutions, more preferably, at least about 3 revolutions, and more preferably, about 4 revolutions or more.
Gas dispersing channel 1534 has gas inlets 1536a, 1536b to provide gas flows from two similar pairs of valves 1542a/1552a, 1542b/1552b, which may be provided together and/or separately. In one configuration, valve 1542a and valve 1542b are coupled to separate reactant gas sources but are preferably coupled to the same purge gas source. For example, valve 1542a is coupled to reactant gas source 1538 and valve 1542b is coupled to reactant gas source 1539, and both valves 1542a, 1542b are coupled to purge gas source 1540. Each valve 1542a, 1542b includes delivery line 1543a, 1543b having valve seat assembly 1544a, 1544b and each valve 1552a, 1552b includes purge line 1545a, 1545b having valve seat assembly 1546a, 1546b. Delivery line 1543a, 1543b is in fluid communication with reactant gas sources 1538 and 1539 and is in fluid communication with gas inlet 1536a, 1536b of gas dispersing channel 1534. Valve seat assembly 1544a, 1544b of the delivery line 1543a, 1543b controls the flow of the reactant gas from reactant gas sources 1538 and 1539 to gas dispersing channel 1534. Purge line 1545a, 1545b is in communication with purge gas source 1540 and intersects delivery line 1543a, 1543b downstream of valve seat assembly 1544a, 1544b of delivery line 1543a, 1543b. Valve seat assembly 1546a, 1546b of purge line 1545a, 1545b controls the flow of the purge gas from purge gas source 1540 to gas dispersing channel 1534. If a carrier gas is used to deliver reactant gases from reactant gas sources 1538 and 1539, preferably the same gas is used as a carrier gas and a purge gas (i.e., an argon gas used as a carrier gas and a purge gas).
Each valve seat assembly 1544a, 1544b, 1546a, 1546b may contain a diaphragm (not shown) and a valve seat (not shown). The diaphragm may be biased open or closed and may be actuated closed or open respectively. The diaphragms may be pneumatically actuated or may be electrically actuated. Pneumatically actuated valves include pneumatically actuated valves available from Fujikin, Inc. and Veriflo Division, Parker Hannifin, Corp. Electrically actuated valves include electrically actuated valves available from Fujikin, Inc. For example, an ALD valve that may be used is the Fujikin Model No. FPR-UDDFAT-21-6.35-PI-ASN or the Fujikin Model No. FPR-NHDT-21-6.35-PA-AYT. Programmable logic controllers 1548a, 1548b may be coupled to valves 1542a, 1542b to control actuation of the diaphragms of valve seat assemblies 1544a, 1544b, 1546a, 1546b of valves 1542a, 1542b. Pneumatically actuated valves may provide pulses of gases in time periods as low as about 0.020 seconds. Electrically actuated valves may provide pulses of gases in time periods as low as about 0.005 seconds. An electrically actuated valve typically requires the use of a driver coupled between the valve and the programmable logic controller.
Each valve 1542a, 1542b may be a zero dead volume valve to enable flushing of a reactant gas from delivery line 1543a, 1543b when valve seat assembly 1544a, 1544b is closed. For example, purge line 1545a, 1545b may be positioned adjacent valve seat assembly 1544a, 1544b of delivery line 1543a, 1543b. When valve seat assembly 1544a, 1544b is closed, purge line 1545a, 1545b may provide a purge gas to flush delivery line 1543a, 1543b. In one embodiment, purge line 1545a, 1545b is positioned slightly spaced from valve seat assembly 1544a, 1544b of delivery line 1543a, 1543b so that a purge gas is not directly delivered into valve seat assembly 1544a, 1544b when open. A zero dead volume valve as used herein is defined as a valve which has negligible dead volume (i.e., not necessary zero dead volume).
Each valve pair 1542a/1552a, 1542b/1552b may be adapted to provide a combined gas flow and/or separate gas flows of the reactant gas and the purge gas. In reference to valve pair 1542a/1552a, one example of a combined gas flow of the reactant gas and the purge gas includes a continuous flow of a purge gas from purge gas source 1540 through purge line 1545a and pulses of a reactant gas from reactant gas source 1538 through delivery line 1543a. The continuous flow of the purge gas may be provided by leaving the diaphragm of valve seat assembly 1546a of purge line 1545a open. The pulses of the reactant gas from reactant gas source 1538 may be provided by opening and closing the diaphragm of valve seat assembly 1544a of delivery line 1543a. In reference to valve pair 1542a/1552a, one example of separate gas flows of the reactant gas and the purge gas includes pulses of a purge gas from purge gas source 1540 through purge line 1545a and pulses of a reactant gas from reactant gas source 1538 through delivery line 1543a. The pulses of the purge gas may be provided by opening and closing the diaphragm of valve seat assembly 1546a of purge line 1545a. The pulses of the reactant gas from reactant gas source 1538 may be provided by opening and closing the diaphragm of valve seat assembly 1544a of delivery line 1543a.
Delivery lines 1543a, 1543b of valves 1542a, 1542b may be coupled to gas inlets 1536a, 1536b through gas conduits 1550a, 1550b. Gas conduits 1550a, 1550b may be integrated or may be separate from valves 1542a, 1542b. In one aspect, valves 1542a, 1542b are coupled in close proximity to gas dispersing channel 1534 to reduce any unnecessary volume of delivery line 1543a, 1543b and gas conduits 1550a, 1550b between valves 1542a, 1542b and gas inlets 1536a, 1536b.
Not wishing to be bound by theory, it is believed that the diameter of gas dispersing channel 1534, which is constant from upper portion 1537 of gas dispersing channel 1534 to some point along central axis 1533 and increasing from this point to lower portion 1535 of gas dispersing channel 1534, allows less of an adiabatic expansion of a gas through gas dispersing channel 1534 which helps to control the temperature of the process gas contained in circular flow gas 1574. For instance, a sudden adiabatic expansion of a gas delivered into gas dispersing channel 1534 may result in a drop in the temperature of the gas which may cause condensation of the gas and formation of droplets. On the other hand, gas dispersing channel 1534 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1532). Gas dispersing channel 1534 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
Slots 1569a and 1569b provide fluid communication from gas annulets 1568a and 1568b to gas dispersing channel 1534. Slots 1569a and 1569b may be positioned at an angle relative to central axis 1533, such as about tangential to central axis 1533 or gas dispersing channel 1534. In one embodiment, slots 1569a and 1569b are positioned at an angle tangential to gas dispersing channel 1534, such as within a range from about 0° to about 90°, preferably, from about 0° to about 45°, and more preferably, from about 0° to about 20°.
Not wishing to be bound by theory,
In one embodiment,
In one example, lower surface 1560 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1560 of chamber lid assembly 1532 and substrate 1510 while assisting to provide uniform exposure of the surface of substrate 1510 to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 1560 of chamber lid assembly 1532 and the surface of substrate 1510 is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of substrate 1510 helps provide a more uniform deposition of the gas on substrate 1510. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on substrate 1510 surface. Thus, a higher velocity of a gas at a first area of the surface of substrate 1510 versus a second area of the surface of substrate 1510 is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1532 having lower surface 1560, downwardly sloping, provides for more uniform deposition of the gas across the surface of substrate 1510 because lower surface 1560 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of substrate 1510.
In one specific embodiment, the spacing between choke 1562 and substrate support 1512 is between about 0.04 inches and about 2.0 inches, and preferably between 0.04 inches and about 0.2 inches. The spacing may vary depending on the gases being delivered and the process conditions during deposition. Choke 1562 helps provide a more uniform pressure distribution within the volume or reaction zone 1564 defined between chamber lid assembly 1532 and substrate 1510 by isolating reaction zone 1564 from the non-uniform pressure distribution of pumping zone 1566 (
Referring to
Since reaction zone 1564 may contain a smaller volume when compared to the inner volume of a conventional CVD chamber, a smaller amount of gas is required to fill reaction zone 1564 for a particular process in an atomic layer deposition sequence. For example, in one embodiment, the volume of reaction zone 1564 is about 1,000 cm3 or less, preferably 500 cm3 or less, and more preferably 200 cm3 or less for a chamber adapted to process 200 mm diameter substrates. In one embodiment, the volume of reaction zone 1564 is about 3,000 cm3 or less, preferably 1,500 cm3 or less, and more preferably 600 cm3 or less for a chamber adapted to process 300 mm diameter substrates. In one embodiment, substrate support 1512 may be raised or lowered to adjust the volume of reaction zone 1564 for deposition. Because of the smaller volume of reaction zone 1564, less gas, whether a deposition gas or a purge gas, is necessary to be flowed into process chamber 1500. Therefore, the throughput of process chamber 1500 is greater and the waste may be minimized due to the smaller amount of gas used reducing the cost of operation.
Chamber lid assembly 1532 has been shown in
Chamber lid assembly 1532 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1532 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1532. For example, water channels (such as coolant channel 1290 In
The components and parts of chamber lid assembly 1532 may contain materials such as stainless steel, aluminum, nickel-plated aluminum, nickel, alloys thereof, or other suitable materials. In one embodiment, lid cap 1572 and lid plate 1570 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof.
In one embodiment, inner surface 1531 of gas dispersing channel 1534 (including both inner surfaces of lid plate 1570 and lid cap 1572) and lower surface 1560 of chamber lid assembly 1532 may contain a mirror polished surface to help produce a laminar flow of a gas along gas dispersing channel 1534 and lower surface 1560 of chamber lid assembly 1532. In another embodiment, the inner surface of gas conduits 1550a and 1550b may be electropolished to help produce a laminar flow of a gas therethrough.
In an alternative embodiment, inner surface 1531 of gas dispersing channel 1534 (including both inner surfaces of lid plate 1570 and lid cap 1572) and lower surface 1560 of chamber lid assembly 1532 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surface 1531 and lower surface 1560. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surface 1531 and lower surface 1560 to contaminate substrate 1510. In one example, the mean roughness (Ra) of lower surface 1560 and/or inner surface 1531 may be at least about 10 μin, such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of lower surface 1560 and/or inner surface 1531 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
Control unit 1580 may be one of any form of general purpose computer processor that can be used in an industrial setting for controlling various chambers and sub-processors. CPU 1582 may use any suitable memory 1586, such as random access memory, read only memory, floppy disk drive, hard disk, or any other form of digital storage, local or remote. Various support circuits may be coupled to CPU 1582 for supporting process chamber 1500. Control unit 1580 may be coupled to another controller that is located adjacent individual chamber components, such as programmable logic controllers 1548a, 1548b of valves 1542a, 1542b. Bi-directional communications between the control unit 1580 and various other components of process chamber 1500 are handled through numerous signal cables collectively referred to as signal buses 1588, some of which are illustrated in
Referring to
Circular gas flow 1574 travels through gas dispersing channel 1534 as a vortex flow which provides a sweeping action across the inner surface of gas dispersing channel 1534. Circular gas flow 1574 dissipates to a downwardly flow towards the surface of substrate 1510. The velocity of the gas flow reduces as it travels through gas dispersing channel 1534. The gas flow then travels across the surface of substrate 1510 and across lower surface 1560 of chamber lid assembly 1532. Lower surface 1560 of chamber lid assembly 1532, which is downwardly sloping, helps reduce the variation of the velocity of the gas flow across the surface of substrate 1510. The gas flow then travels by choke 1562 and into pumping zone 1566 of process chamber 1500. Excess gas, by-products, etc. flow into the pumping channel 1579 and are then exhausted from process chamber 1500 by vacuum system 1578. In one aspect, the gas flow proceeds through gas dispersing channel 1534 and between the surface of substrate 1510 and lower surface 1560 of chamber lid assembly 1532 in a laminar manner which aids in uniform exposure of a reactant gas to the surface of substrate 1510 and efficient purging of inner surfaces of chamber lid assembly 1532.
Process chamber 1500, as illustrated in
Extended Cap Lid Assembly
In another embodiment,
In one embodiment, chamber lid assembly 1632 contains lid cap 1672 positioned in a centralized portion of lid plate 1670, as illustrated in
Gas conduit cover 1652 contains at least one gas conduit, or may contain two, three, or more gas conduits.
Conduit 1650c is an optional conduit in some embodiments. Gas conduit 1650c may be coupled to and in fluid communication with lid cap 1672 on one end, while the other end of gas conduit 1650c extends through lid plate 1670 and may be coupled to and in fluid communication with an ALD valve and gas source, such as a carrier gas source, a purge gas source, a plasma gas, or a chemical precursor source. In another embodiment, conduit 1650c is may be coupled to and in fluid communication with the top surface of lid cap 1672. In another embodiment, conduit 1650c may be combined with conduit 1650b, such as with a Y-joint, and may be coupled to and in fluid communication with gas passageway 1668b.
Chamber lid assembly 1632 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1632 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1632. For example, coolant channel 1690 may be formed in chamber lid assembly 1632 to cool chamber lid assembly 1632. In another example, heating elements (not shown) may be embedded or may surround components of chamber lid assembly 1632 to heat chamber lid assembly 1632.
In one embodiment, components of chamber lid assembly 1632 may be individually heated or cooled. For example, referring to
Chamber lid assembly 1632 contains components that may be made of stainless steel, aluminum, nickel-plated aluminum, nickel, or other suitable materials. In one embodiment, lid cap 1672 and lid plate 1670 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof.
In one embodiment, inner surface 1631 of gas dispersing channel 1628 (including both inner surfaces of lid plate 1670 and lid cap 1672) and lower surface 1660 of chamber lid assembly 1632 may contain a mirror polished surface to help produce a laminar flow of a gas along expanding channel 1634 and lower surface 1660 of chamber lid assembly 1632. In another embodiment, the inner surface of gas conduits 1650a, 1650b may be electropolished to help produce a laminar flow of a gas therethrough.
In an alternative embodiment, inner surface 1631 of gas dispersing channel 1628 (including both inner surfaces of lid plate 1670 and lid cap 1672) and lower surface 1660 of chamber lid assembly 1632 may contain a roughened surface or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surface 1631 and lower surface 1660. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surface 1631 and lower surface 1660 to contaminate substrate 1610. In one example, the mean roughness (Ra) of lower surface 1660 and/or inner surface 1631 may be at least about 10 μin, such as within a range from about 10 μin (about 0.254 μm) to about 200 μin (about 5.08 μm), preferably, from about 20 μin (about 0.508 μm) to about 100 μin (about 2.54 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 80 μin (about 2.032 μm). In another example, the mean roughness of lower surface 1660 and/or inner surface 1631 may be at least about 100 μin (about 2.54 μm), preferably, within a range from about 200 μin (about 5.08 μm) to about 500 μin (about 12.7 μm).
Processes gases, as circular gas flow 1620 depicted in
In one embodiment,
In addition, the diameter of gas conduits 1650a, 1650b, and 1650c and gas passageways 1668a and 1668b may be increasing from the delivery lines or ALD valves to gas inlets 1638a and 1638b to help reduce the velocity of the gas flow prior to its entry into gas dispersing channel 1628. For example, gas conduits 1650a, 1650b, 1650c and gas passageways 1668a and 1668b may contain an inner diameter which is gradually increasing or may contain a plurality of connected conduits having increasing inner diameters.
In one example, chamber lid assembly 1632 adapted to process 300 mm diameter substrates may have the following diameters. The diameter at upper portion 1637 of gas dispersing channel 1628 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch. The diameter at point 1636 of gas dispersing channel 1628 may be within a range from about 0.5 inches to about 2 inches, preferably, from about 0.75 inches to about 1.5 inches, and more preferably, from 0.8 inches to about 1.2 inches, for example, about 1 inch. The diameter at lower portion 1635 of gas dispersing channel 1628 may be within a range from about 1 inch to about 4 inches, preferably, from about 1.5 inches to about 3 inches, and more preferably, from 1.6 inches to about 2.4 inches, for example, about 2 inches.
In general, the above dimension apply to gas dispersing channel 1628 adapted to provide a total gas flow of between about 500 sccm and about 3,000 sccm. In other specific embodiments, the dimension may be altered to accommodate a certain gas flow therethrough. In general, a larger gas flow will require a larger diameter of gas dispersing channel 1628.
Gas dispersing channel 1628 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1632). Gas dispersing channel 1628 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas inlets 1638a and 1638b are located adjacent upper portion 1637 of gas dispersing channel 1628, as depicted in
Each gas conduit 1650a, 1650b, and 1650c and gas passageways 1668a and 1668b may be positioned at an angle α from the centerline of the gas conduit and from a radius line of gas dispersing channel 1628, similarly as depicted in
Not wishing to be bound by theory,
In one example, lower surface 1660 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1660 of chamber lid assembly 1632 and a substrate while assisting to provide uniform exposure of the surface of a substrate to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 1660 of chamber lid assembly 1632 and the surface of a substrate is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of a substrate helps provide a more uniform deposition of the gas on a substrate. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on a substrate surface. Thus, a higher velocity of a gas at a first area of the surface of a substrate versus a second area of the surface of a substrate is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1632 having lower surface 1660, downwardly sloping, provides for more uniform deposition of the gas across the surface of a substrate because lower surface 1660 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of a substrate.
Lid cap 1672, gas conduit 1650a, gas conduit cover 1652, and a portion of upper surface of lid plate 1670 may be covered by chamber lid cover 1680 having handles 1682, as illustrated in
Substrate support 1712 supports substrate 1710 on substrate receiving surface 1711 in process chamber 1700. Substrate support 1712 is mounted to lift motor 1714 for raising and lowering substrate support 1712 and substrate 1710 disposed thereon. Lift plate 1716 connected to lift motor 1718 is mounted in process chamber 1700 and raises and lowers lift pins 1720 movably disposed through substrate support 1712. Lift pins 1720 raise and lower substrate 1710 over the surface of substrate support 1712. Substrate support 1712 may include a vacuum chuck (not shown), an electrostatic chuck (not shown), or a clamp ring (not shown) for securing substrate 1710 to substrate support 1712 during a deposition process.
The temperature of substrate support 1712 may be adjusted to control the temperature of substrate 1710 disposed thereon. For example, substrate support 1712 may be heated using an embedded heating element, such as a resistive heater (not shown), or may be heated using radiant heat, such as heating lamps (not shown) disposed above substrate support 1712. Purge ring 1722 may be disposed on substrate support 1712 to define purge channel 1724 which provides a purge gas to a peripheral portion of substrate 1710 to prevent deposition thereon.
Gas delivery system 1730 is disposed at an upper portion of chamber body 1702 to provide a gas, such as a process gas and/or a purge gas, to process chamber 1700.
In one embodiment, gas delivery system 1730 contains chamber lid assembly 1732 having gas dispersing channel 1734 extending through a central portion of chamber lid assembly 1732. Lid cap 1772 may contain a cylindrical portion of gas dispersing channel 1734, such as narrow portion 1754. Lid cap 1772 also contains a diverging or expanding portion of gas dispersing channel 1734, such as in expanding portion 1756. Gas dispersing channel 1734 extends towards substrate receiving surface 1711 and along central axis 1733 of gas dispersing channel 1734, through lid plate 1770, and to lower surface 1760. In one example, a portion of gas dispersing channel 1734 stays substantially cylindrical along central axis 1733 within upper portion 1737 and a portion of gas dispersing channel 1734 that tapers away from central axis 1733 within lower portion 1735 of gas dispersing channel 1734. Gas dispersing channel 1734 further extends pass lower surface 1760 and into reaction zone 1764. Lower surface 1760 extends from lower portion 1735 of gas dispersing channel 1734 to choke 1762. Lower surface 1760 is sized and shaped to substantially cover substrate 1710 disposed on substrate receiving surface 1711 of substrate support 1712.
Processes gases, as circular gas flow 1774, are forced to make revolutions around central axis 1733 of gas dispersing channel 1734 while passing along central axis 1733. Circular gas flow 1774 may contain a flow pattern, such as a vortex pattern, a helix pattern, a spiral pattern, a twirl pattern, a twist pattern, a coil pattern, a whirlpool pattern, or derivatives thereof. Circular gas flow 1774 may extend at least about 1 revolution around central axis 1733 of gas dispersing channel 1734, preferably, at least about 1.5 revolutions, more preferably, at least about 2 revolutions, more preferably, at least about 3 revolutions, and more preferably, about 4 revolutions or more.
Gas dispersing channel 1734 has gas inlets 1736a, 1736b to provide gas flows from two similar pairs of valves 1742a/1752a, 1742b/1752b, which may be provided together and/or separately. In one configuration, valve 1742a and valve 1742b are coupled to separate reactant gas sources but are preferably coupled to the same purge gas source. For example, valve 1742a is coupled to reactant gas source 1738 and valve 1742b is coupled to reactant gas source 1739, and both valves 1742a, 1742b are coupled to purge gas source 1740. Each valve 1742a, 1742b includes delivery line 1743a, 1743b having valve seat assembly 1744a, 1744b and each valve 1752a, 1752b includes purge line 1745a, 1745b having valve seat assembly 1746a, 1746b. Delivery line 1743a, 1743b is in fluid communication with reactant gas source 1738, 1739 and is in fluid communication with gas inlet 1736a, 1736b of gas dispersing channel 1734. Valve seat assembly 1744a, 1744b of the delivery line 1743a, 1743b controls the flow of the reactant gas from reactant gas source 1738, 1739 to gas dispersing channel 1734. Purge line 1745a, 1745b is in fluid communication with purge gas source 1740 and intersects delivery line 1743a, 1743b downstream of valve seat assembly 1744a, 1744b of delivery line 1743a, 1743b. Valve seat assembly 1746a, 1746b of purge line 1745a, 1745b controls the flow of the purge gas from purge gas source 1740 to gas dispersing channel 1734. If a carrier gas is used to deliver reactant gases from reactant gas source 1738, 1739, preferably the same gas is used as a carrier gas and a purge gas (i.e., an argon gas used as a carrier gas and a purge gas).
Each valve seat assembly 1744a, 1744b, 1746a, 1746b may contain a diaphragm (not shown) and a valve seat (not shown). The diaphragm may be biased open or closed and may be actuated closed or open respectively. The diaphragms may be pneumatically actuated or may be electrically actuated. Pneumatically actuated valves include pneumatically actuated valves available from Fujikin, Inc. and Veriflo Division, Parker Hannifin, Corp. Electrically actuated valves include electrically actuated valves available from Fujikin, Inc. For example, an ALD valve that may be used is the Fujikin Model No. FPR-UDDFAT-21-6.35-PI-ASN or the Fujikin Model No. FPR-NHDT-21-6.35-PA-AYT. Programmable logic controllers 1748a, 1748b may be coupled to valves 1742a, 1742b to control actuation of the diaphragms of valve seat assemblies 1744a, 1744b, 1746a, 1746b of valves 1742a, 1742b. Pneumatically actuated valves may provide pulses of gases in time periods as low as about 0.020 seconds. Electrically actuated valves may provide pulses of gases in time periods as low as about 0.005 seconds. An electrically actuated valve typically requires the use of a driver coupled between the valve and the programmable logic controller.
Each valve 1742a, 1742b may be a zero dead volume valve to enable flushing of a reactant gas from delivery line 1743a, 1743b when valve seat assembly 1744a, 1744b is closed. For example, purge line 1745a, 1745b may be positioned adjacent valve seat assembly 1744a, 1744b of delivery line 1743a, 1743b. When valve seat assembly 1744a, 1744b is closed, purge line 1745a, 1745b may provide a purge gas to flush delivery line 1743a, 1743b. In one embodiment, purge line 1745a, 1745b is positioned slightly spaced from valve seat assembly 1744a, 1744b of delivery line 1743a, 1743b so that a purge gas is not directly delivered into valve seat assembly 1744a, 1744b when open. A zero dead volume valve as used herein is defined as a valve which has negligible dead volume (i.e., not necessary zero dead volume).
Each valve pair 1742a/1752a, 1742b/1752b may be adapted to provide a combined gas flow and/or separate gas flows of the reactant gas and the purge gas. In reference to valve pair 1742a/1752a, one example of a combined gas flow of the reactant gas and the purge gas includes a continuous flow of a purge gas from purge gas source 1740 through purge line 1745a and pulses of a reactant gas from reactant gas source 1738 through delivery line 1743a. The continuous flow of the purge gas may be provided by leaving the diaphragm of valve seat assembly 1746a of purge line 1745a open. The pulses of the reactant gas from reactant gas source 1738 may be provided by opening and closing the diaphragm of valve seat assembly 1744a of delivery line 1743a. In reference to valve pair 1742a/1752a, one example of separate gas flows of the reactant gas and the purge gas includes pulses of a purge gas from purge gas source 1740 through purge line 1745a and pulses of a reactant gas from reactant gas source 1738 through delivery line 1743a. The pulses of the purge gas may be provided by opening and closing the diaphragm of valve seat assembly 1746a of purge line 1745a. The pulses of the reactant gas from reactant gas source 1738 may be provided by opening and closing the diaphragm of valve seat assembly 1744a of delivery line 1743a.
Delivery lines 1743a, 1743b of valves 1742a, 1742b may be coupled to gas inlets 1736a, 1736b through gas conduits 1750a, 1750b. Gas conduits 1750a, 1750b may be integrated or may be separate from valves 1742a, 1742b. In one aspect, valves 1742a, 1742b are coupled in close proximity to gas dispersing channel 1734 to reduce any unnecessary volume of delivery line 1743a, 1743b and gas conduits 1750a, 1750b between valves 1742a, 1742b and gas inlets 1736a, 1736b.
Not wishing to be bound by theory, it is believed that the diameter of gas dispersing channel 1734, which is constant from upper portion 1737 of gas dispersing channel 1734 to some point along central axis 1733 and increasing from this point to lower portion 1735 of gas dispersing channel 1734, allows less of an adiabatic expansion of a gas through gas dispersing channel 1734 which helps to control the temperature of the process gas contained in circular flow gas 1774. For instance, a sudden adiabatic expansion of a gas delivered through gas inlet 1736a, 1736b into gas dispersing channel 1734 may result in a drop in the temperature of the gas which may cause condensation of the gas and formation of droplets. On the other hand, gas dispersing channel 1734 that gradually tapers is believed to provide less of an adiabatic expansion of a gas. Therefore, more heat may be transferred to or from the gas, and, thus, the temperature of the gas may be more easily controlled by controlling the surrounding temperature of the gas (i.e., controlling the temperature of chamber lid assembly 1732). Gas dispersing channel 1734 may gradually taper and contain one or more tapered inner surfaces, such as a tapered straight surface, a concave surface, a convex surface, or combinations thereof or may contain sections of one or more tapered inner surfaces (i.e., a portion tapered and a portion non-tapered).
In one embodiment, gas inlets 1736a, 1736b are located adjacent upper portion 1737 of gas dispersing channel 1734. In other embodiments, one or more gas inlets 1736a, 1736b may be located along the length of gas dispersing channel 1734 between upper portion 1737 and lower portion 1735.
Not wishing to be bound by theory,
In one embodiment,
In one example, lower surface 1760 is downwardly sloping to help reduce the variation in the velocity of the process gases traveling between lower surface 1760 of chamber lid assembly 1732 and substrate 1710 while assisting to provide uniform exposure of the surface of substrate 1710 to a reactant gas. In one embodiment, the ratio of the maximum area of the flow section over the minimum area of the flow section between a downwardly sloping lower surface 1760 of chamber lid assembly 1732 and the surface of substrate 1710 is less than about 2, preferably, less than about 1.5, more preferably, less than about 1.3, and more preferably, about 1.
Not wishing to be bound by theory, it is believed that a gas flow traveling at a more uniform velocity across the surface of substrate 1710 helps provide a more uniform deposition of the gas on substrate 1710. It is believed that the velocity of the gas is directly proportional to the concentration of the gas which is in turn directly proportional to the deposition rate of the gas on substrate 1710 surface. Thus, a higher velocity of a gas at a first area of the surface of substrate 1710 versus a second area of the surface of substrate 1710 is believed to provide a higher deposition of the gas on the first area. It is believed that chamber lid assembly 1732 having lower surface 1760, downwardly sloping, provides for more uniform deposition of the gas across the surface of substrate 1710 because lower surface 1760 provides a more uniform velocity and, thus, a more uniform concentration of the gas across the surface of substrate 1710.
In one specific embodiment, the spacing between choke 1762 and substrate support 1712 is between about 0.04 inches and about 2.0 inches, and preferably between 0.04 inches and about 0.2 inches. The spacing may vary depending on the gases being delivered and the process conditions during deposition. Choke 1762 helps provide a more uniform pressure distribution within the volume or reaction zone 1764 defined between chamber lid assembly 1732 and substrate 1710 by isolating reaction zone 1764 from the non-uniform pressure distribution of pumping zone 1766.
Referring to
Since reaction zone 1764 may contain a smaller volume when compared to the inner volume of a conventional CVD chamber, a smaller amount of gas is required to fill reaction zone 1764 for a particular process in an atomic layer deposition sequence. For example, in one embodiment, the volume of reaction zone 1764 is about 1,000 cm3 or less, preferably 500 cm3 or less, and more preferably 200 cm3 or less for a chamber adapted to process 200 mm diameter substrates. In one embodiment, the volume of reaction zone 1764 is about 3,000 cm3 or less, preferably 1,500 cm3 or less, and more preferably 600 cm3 or less for a chamber adapted to process 300 mm diameter substrates. In one embodiment, substrate support 1712 may be raised or lowered to adjust the volume of reaction zone 1764 for deposition. Because of the smaller volume of reaction zone 1764, less gas, whether a deposition gas or a purge gas, is necessary to be flowed into process chamber 1700. Therefore, the throughput of process chamber 1700 is greater and the waste may be minimized due to the smaller amount of gas used reducing the cost of operation.
Chamber lid assembly 1732 has been shown in
Chamber lid assembly 1732 may include cooling elements and/or heating elements depending on the particular gas being delivered therethrough. Controlling the temperature of chamber lid assembly 1732 may be used to prevent gas decomposition, deposition, or condensation on chamber lid assembly 1732. For example, water channels (such as coolant channel 1690 shown in
The components and parts of chamber lid assembly 1732 may contain materials such as stainless steel, aluminum, nickel-plated aluminum, nickel, alloys thereof, or other suitable materials. In one embodiment, lid cap 1772 and lid plate 1770 may be independently fabricated, machined, forged, or otherwise made from a metal, such as aluminum, an aluminum alloy, steel, stainless steel, alloys thereof, or combinations thereof.
Control unit 1780 may be one of any form of general purpose computer processor that can be used in an industrial setting for controlling various chambers and sub-processors. CPU 1782 may use any suitable memory 1786, such as random access memory, read only memory, floppy disk drive, hard disk, or any other form of digital storage, local or remote. Various support circuits may be coupled to CPU 1782 for supporting process chamber 1700. Control unit 1780 may be coupled to another controller that is located adjacent individual chamber components, such as programmable logic controllers 1748a, 1748b of valves 1742a, 1742b. Bi-directional communications between the control unit 1780 and various other components of process chamber 1700 are handled through numerous signal cables collectively referred to as signal buses 1788, some of which are illustrated in
Referring to
Process chamber 1700, as illustrated in
In some embodiments, gas dispersing channel 1734 within process chamber 1700 may have roughened or machined surfaces to produce more surface area across the surfaces. Roughened surfaces provide better adhesion of undesired accumulated materials on inner surface 1790 of lid cap 1772 and lower surface 1760 of lid plate 1770. The undesired films are usually formed as a consequence of conducting a vapor deposition process and may peel or flake from inner surface 1790 and lower surface 1760 to contaminate substrate 1710.
In another embodiment, multiple surfaces form a gradient of roughened surfaces across regions R1 to R10 on inner surfaces 1790 and 1792 of lid cap 1772 and lower surface 1760 of lid plate 1770, as depicted in
In some embodiments, a mean surface roughness of gas dispersing channel 1734 may increase along central axis 1733, for example, from R1 to R10. In another example, the mean surface roughness of gas dispersing channel 1734 may increase from gas inlets 1736a and 1736b extending along central axis 1733 towards substrate receiving surface 1711. In another example, the mean surface roughness of gas dispersing channel 1734 may increase from inner surface 1790 to inner surface 1792 and further to lower surface 1760. In another example, the mean surface roughness of gas dispersing channel 1734 may increase from upper portion 1737 to lower portion 1735.
In one embodiment, narrow portion 1754 of lid cap 1772 contains inner surface 1790 having a mean roughness (Ra) of at least about 10 μin (about 0.254 μm), such as within a range from about 10 μin (about 0.254 μm) to about 50 μin (about 1.27 μm), preferably, from about 20 μin (about 0.508 μm) to about 45 μin (about 1.143 μm), and more preferably, from about 30 μin (about 0.762 μm) to about 40 μin (about 1.016 μm). Expanding portion 1756 of lid cap 1772 contains inner surface 1792 having a mean roughness of at least about 35 μin (about 0.89 μm), such as within a range from about 35 μin (about 0.89 μm) to about 70 μin (about 1.78 μm), preferably, from about 40 μin (about 1.016 μm) to about 65 μin (about 1.65 μm), and more preferably, from about 45 μin (about 1.143 μm) to about 60 μin (about 1.52 μm). Lower portion 1758 of lid plate 1770 contains lower surface 1760 having a mean roughness of at least about 35 μin (about 0.89 μm), such as within a range from about 35 μin (about 0.89 μm) to about 70 μin (about 1.78 μm), preferably, from about 40 μin (about 1.016 μm) to about 65 μin (about 1.65 μm), and more preferably, from about 45 μin (about 1.143 μm) to about 60 μin (about 1.52 μm).
In one example, narrow portion 1754 of lid cap 1772 contains region R1 having an Ra of inner surface 1790 within a range from about 32 μin to about 36 μin, such as about 34 μin, and region R2 having an Ra of inner surface 1790 within a range from about 34 μin to about 42 μin, such as about 38 μin. Expanding portion 1756 of lid cap 1772 contains region R3 having an Ra of inner surface 1792 within a range from about 40 μin to about 50 μin, such as about 45 μin, region R4 having an Ra of inner surface 1790 within a range from about 44 μin to about 60 μin, such as about 51 μin, region R5 having an Ra of inner surface 1792 within a range from about 48 μin to about 68 μin, such as about 58 μin, region R6 having an Ra of inner surface 1790 within a range from about 46 μin to about 64 μin, such as about 55 μin, region R7 having an Ra of inner surface 1792 within a range from about 48 μin to about 68 μin, such as about 57 μin, and region R8 having an Ra of inner surface 1790 within a range from about 48 μin to about 68 μin, such as about 57 μin. Also, lower portion 1758 of lid plate 1770 contains region R9 having an Ra of lower surface 1760 within a range from about 46 μin to about 64 μin, such as about 55 μin, and region R10 having an Ra of lower surface 1760 within a range from about 46 μin to about 64 μin, such as about 55 μin.
“Atomic layer deposition” (ALD), “cyclical deposition,” or “cyclical layer deposition” as used herein refers to the sequential introduction of two or more reactive compounds to deposit a layer of material on a substrate surface. The two, three, or more reactive compounds may alternatively be introduced into a reaction zone or process region of a process chamber. The reactive compounds may be in a state of gas, plasma, vapor, fluid or other state of matter useful for a vapor deposition process. Usually, each reactive compound is separated by a time delay to allow each compound to adhere and/or react on the substrate surface. In one aspect, a first precursor or compound A is pulsed into the reaction zone followed by a first time delay. Next, a second precursor or compound B is pulsed into the reaction zone followed by a second delay. Compound A and compound B react to form a deposited material. During each time delay a purge gas is introduced into the process chamber to purge the reaction zone or otherwise remove any residual reactive compound or by-products from the reaction zone. Alternatively, the purge gas may flow continuously throughout the deposition process so that only the purge gas flows during the time delay between pulses of reactive compounds. The reactive compounds are alternatively pulsed until a desired film thickness of the deposited material is formed on the substrate surface. In either scenario, the ALD process of pulsing compound A, purge gas, pulsing compound B and purge gas is a cycle. A cycle can start with either compound A or compound B and continue the respective order of the cycle until achieving a film with the desired thickness. In an alternative embodiment, a first precursor containing compound A, a second precursor containing compound B and a third precursor containing compound C are each separately pulsed into the process chamber. Alternatively, a pulse of a first precursor may overlap in time with a pulse of a second precursor while a pulse of a third precursor does not overlap in time with either pulse of the first and second precursors. “Process gas” as used herein refers to a single gas, multiple gases, a gas containing a plasma, combinations of gas(es) and/or plasma(s). A process gas may contain at least one reactive compound for a vapor deposition process. The reactive compounds may be in a state of gas, plasma, vapor, fluid or other state of matter useful for a vapor deposition process. Also, a process may contain a purge gas or a carrier gas and not contain a reactive compound.
“Substrate” or “substrate surface,” as used herein, refers to any substrate or material surface formed on a substrate upon which film processing is performed. For example, a substrate surface on which processing can be performed include materials such as silicon, silicon oxide, strained silicon, silicon on insulator (SOI), carbon doped silicon oxides, silicon nitride, doped silicon, germanium, gallium arsenide, glass, sapphire, quartz, and any other materials such as metals, metal nitrides, metal alloys, and other conductive materials, depending on the application. Barrier layers, metals or metal nitrides on a substrate surface may include titanium, titanium nitride, titanium silicide nitride, tungsten, tungsten nitride, tungsten silicide nitride, tantalum, tantalum nitride, or tantalum silicide nitride. Substrates may have various dimensions, such as 200 mm or 300 mm diameter wafers, as well as, rectangular or square panes. Substrates include semiconductor substrates, display substrates (e.g., LCD), solar panel substrates, and other types of substrates. Unless otherwise noted, embodiments and examples described herein are preferably conducted on substrates with a 200 mm diameter or a 300 mm diameter, more preferably, a 300 mm diameter. Substrates on which embodiments of the invention may be useful include, but are not limited to semiconductor wafers, such as crystalline silicon (e.g., Si<100> or Si<111>), silicon oxide, glass, quartz, strained silicon, silicon germanium, doped or undoped polysilicon, doped or undoped silicon wafers and patterned or non-patterned wafers. Substrates may be exposed to a pretreatment process to polish, etch, reduce, oxidize, hydroxylate, anneal and/or bake the substrate surface.
While foregoing is directed to the preferred embodiment of the invention, other and further embodiments of the invention may be devised without departing from the basic scope thereof, and the scope thereof is determined by the claims that follow.
This application claims benefit of U.S. Ser. No. 60/862,764 (APPM/011546L), filed Oct. 24, 2006, which is herein incorporated by reference in its entirety. This application is also a continuation-in-part of U.S. Ser. No. 11/077,753, filed Mar. 11, 2005, which is a continuation of U.S. Ser. No. 10/032,284, filed Dec. 21, 2001, and issued as U.S. Pat. No. 6,916,398, which claims benefit of U.S. Ser. No. 60/346,086, filed Oct. 26, 2001, which are herein incorporated by reference in their entirety. This application is also a continuation-in-part of U.S. Ser. No. 11/680,995, filed Mar. 1, 2007, now U.S. Pat. No. 7,402,210 which is a continuation of U.S. Ser. No. 10/712,690, filed Nov. 13, 2003, and issued as U.S. Pat. No. 7,204,886, which claims benefit of U.S. Ser. No. 60/426,134, filed Nov. 14, 2002, which are herein incorporated by reference in their entirety.
| Number | Name | Date | Kind |
|---|---|---|---|
| 5951771 | Raney et al. | Sep 1999 | A |
| 6143077 | Ikeda et al. | Nov 2000 | A |
| 6562140 | Bondestam et al. | May 2003 | B1 |
| 6734020 | Lu et al. | May 2004 | B2 |
| 6797108 | Wendling | Sep 2004 | B2 |
| 6821563 | Yudovsky | Nov 2004 | B2 |
| 6866746 | Lei et al. | Mar 2005 | B2 |
| 6916398 | Chen et al. | Jul 2005 | B2 |
| 6951804 | Seutter et al. | Oct 2005 | B2 |
| 7066194 | Ku et al. | Jun 2006 | B2 |
| 7094680 | Seutter et al. | Aug 2006 | B2 |
| 7175713 | Thakur et al. | Feb 2007 | B2 |
| 7204886 | Chen et al. | Apr 2007 | B2 |
| 7228873 | Ku et al. | Jun 2007 | B2 |
| 7402210 | Chen et al. | Jul 2008 | B2 |
| 7408225 | Shinriki et al. | Aug 2008 | B2 |
| 20020104481 | Chiang et al. | Aug 2002 | A1 |
| 20030121608 | Chen et al. | Jul 2003 | A1 |
| 20050139160 | Lei et al. | Jun 2005 | A1 |
| 20050173068 | Chen et al. | Aug 2005 | A1 |
| 20050252449 | Nguyen et al. | Nov 2005 | A1 |
| 20050271812 | Myo et al. | Dec 2005 | A1 |
| 20050271813 | Kher et al. | Dec 2005 | A1 |
| 20060030148 | Seutter et al. | Feb 2006 | A1 |
| 20060216928 | Chung et al. | Sep 2006 | A1 |
| 20070003698 | Chen et al. | Jan 2007 | A1 |
| 20070026147 | Chen et al. | Feb 2007 | A1 |
| 20070059948 | Metzner et al. | Mar 2007 | A1 |
| 20070095285 | Thakur et al. | May 2007 | A1 |
| 20070119370 | Ma et al. | May 2007 | A1 |
| 20070119371 | Ma et al. | May 2007 | A1 |
| 20070128862 | Ma et al. | Jun 2007 | A1 |
| 20070128863 | Ma et al. | Jun 2007 | A1 |
| 20070128864 | Ma et al. | Jun 2007 | A1 |
| 20080038463 | Chen et al. | Feb 2008 | A1 |
| 20080041307 | Nguyen et al. | Feb 2008 | A1 |
| 20080041313 | Chen et al. | Feb 2008 | A1 |
| 20080044569 | Myo et al. | Feb 2008 | A1 |
| 20080102203 | Wu et al. | May 2008 | A1 |
| 20080120208 | Berkooz | May 2008 | A1 |
| 20080268171 | Ma et al. | Oct 2008 | A1 |
| 20080274299 | Chen et al. | Nov 2008 | A1 |
| Number | Date | Country |
|---|---|---|
| 4087323 | Mar 1992 | JP |
| 2001020075 | Jan 2001 | JP |
| Number | Date | Country | |
|---|---|---|---|
| 20080107809 A1 | May 2008 | US |
| Number | Date | Country | |
|---|---|---|---|
| 60862764 | Oct 2006 | US | |
| 60346086 | Oct 2001 | US | |
| 60426134 | Nov 2002 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 10032284 | Dec 2001 | US |
| Child | 11077753 | US | |
| Parent | 11923589 | US | |
| Child | 11077753 | US | |
| Parent | 10712690 | Nov 2003 | US |
| Child | 11680995 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 11077753 | Mar 2005 | US |
| Child | 11923589 | US | |
| Parent | 11680995 | Mar 2007 | US |
| Child | 11923589 | US |