1. Field of the Invention
The invention relates in general to a semiconductor chip interconnection structure and a semiconductor package formed using the same, and more particularly to a semiconductor chip interconnection structure with stacked bumps and a semiconductor package formed using the same.
2. Description of the Related Art
Referring to
However, during reflow process, the solder layer 18 disposed on bump 16 often flows to the pad 14 and spoils the pad 14, largely affecting the electrical properties and reliability of the pad 14.
The invention is directed to a semiconductor chip interconnection structure and a semiconductor package formed using the same. The electrical element, having been reflown, does not contact the pad so that the electrical properties and reliability of the pad will not be affected.
According to a first aspect of the present invention, a semiconductor chip interconnection structure is provided. The semiconductor chip interconnection structure comprises a chip, a bump assembly and an electrical element. The chip comprises a pad and has a pad aperture from which the pad is exposed. The bump assembly comprises a first bump and a second bump. The first bump is disposed on the pad. The second bump is disposed on the first bump. The outer diameter of the second bump is not less than the outer diameter of the first bump. The electrical element is connected to the bump assembly.
According to a second aspect of the present invention, a semiconductor package is provided. The semiconductor package comprises a substrate and a semiconductor chip interconnection structure. The semiconductor chip interconnection structure comprises a chip, a bump assembly and an electrical element. The chip comprises a pad and has a pad aperture from which the pad is exposed. The bump assembly comprises a first bump and a second bump. The first bump is disposed on the pad. The second bump is disposed on the first bump. The outer diameter of the second bump is not less than the outer diameter of the first bump. The electrical element is connected to the bump assembly.
The above and other aspects of the invention will become better understood with regard to the following detailed description of the preferred but non-limiting embodiment(s). The following description is made with reference to the accompanying drawings.
Referring to
The semiconductor chip interconnection structure 112, such as a flip chip, a lead frame or a substrate, is electrically connected to the substrate 110 through the electrical element 108 such as solder ball or solder layer.
Referring to
The chip 126 comprises a pad 114 and has a pad aperture 116 from which the pad 114 is exposed. The electrical element 108 is connected to the bump assembly 118.
The bump assembly 118 comprises a first bump 120 and a second bump 122. The first bump 120 is disposed on the pad 114. The second bump 122 is disposed on the first bump 120. The outer diameter D12 of the second bump 122 is larger than the outer diameter D11 of the first bump 120. The “outer diameter” refers to the radial size of a bump measured from the outside, while the “inner diameter” refers to the radial size of an aperture measured from the inside.
Preferably but not restrictively, the bump assembly 118 is made from silver or copper by thermosonic wirebonding. Preferably but not restrictively, the first bump 120 is formed by silver and the second bump 122 is formed by copper. Preferably but not restrictively, the pad 114 is an aluminum pad. Preferably but not restrictively, the electrical element 108 is formed by a material selected from a group consisting of tin, silver, copper and lead.
The outer diameter D12 of the second bump 122 is larger than the outer diameter D11 of the first bump 120 and the inner diameter DP of the pad aperture 116. That is, the second bump 122 can completely shield the upper surface of the first bump 120 and the pad aperture 116. Since the outer diameter D12 of the second bump 122 is larger than the inner diameter DP of the pad aperture 116, the electrical element 108, having been reflown, can be completely formed on the second bump 122 (as indicated in
Further, by suitable design of the outer diameter D12 of the second bump 122, the upper surface 134 of the second bump 122 can be large enough so that the electrical element 108, having been reflown, can be completely formed on the second bump 122. Thus, the problem of overflowing is avoided.
Since the electrical element 108, having been reflown, can be completely formed on the second bump 122, the electrical element 108 can thus be controlled in the manufacturing process. Thus, the height, the size and the shape of the electrical element 108 can be controlled according to the needs in the manufacturing process, so that the manufacturing process is more flexible.
The size of second bump 122 is independent of the size of the pad 114. Thus, the second bump 122 can be designed to have a larger size for bearing larger electrical element 108, so that the bonding and electrical properties between the electrical element 108 and the counterpart member are enhanced.
In addition, the first bump 120 and the second bump 122 booster the substrate 110 and increase the distance between the substrate 110 and the pad 114 so as to facilitate the formation of the underfill 132 and increase the reliability of the semiconductor package 100.
The first bump 120 and the second bump 122 can be formed by different materials. For example, the first bump 120 is formed by softer and more expensive gold (Au) and is formed on the pad 114, and the second bump 122 is formed by harder and cheaper copper (Cu), so as to reduce the packaging costs and avoid the chip 126 being damaged during the formation of the first bump 120.
Referring to
The bump assembly 218 comprises a first bump 220, a second bump 222 and a third bump 224. The outer diameter D23 of the third bump 224 is larger than the outer diameter D22 of the second bump 222, the outer diameter D21 of the first bump 220, and the inner diameter DP of the pad aperture 116. The outer diameter D22 of the second bump 222 is larger than the outer diameter D21 of the first bump 220. That is, the third bump 224 can completely shield the upper surface of the second bump 222, the upper surface of the first bump 220, and the pad aperture 116.
Since the outer diameter D23 of the third bump 224 is larger than the inner diameter DP of the pad aperture 116, the electrical element 208, having been reflown, can be completely formed on the third bump 224 as indicated in
Referring to
The bump assembly 418 comprises a first bump 420, a second bump 422 and a third bump 424. The outer diameter D43 of the third bump 424 is smaller than the outer diameter D42 of the second bump 422. The outer diameter D42 of the second bump 422 is larger than the outer diameter D41 of the first bump 420 and the inner diameter DP of the pad aperture 116. That is, the second bump 422 can completely shield the upper surface of the first bump 420 and the pad aperture 116.
The third bump 424 enhances the bonding between the electrical element 408 and the second bump 422. During the reflowing process, the third bump 424 blocks the flowing electrical element 408. Since the third bump 424 changes the surface silhouette of the second bump 422, the third bump 424 avoids the electrical element 408 overflowing to the pad 114.
Referring to
In addition, the first bump 520 and the second bump 522 stacked together booster the substrate 110, facilitate the formation of the underfill 132 and further increase the reliability of the semiconductor package 100. Moreover, the first bump 520 and the second bump 522 can be formed by different materials. For example, the first bump 520 is formed by softer and more expensive gold (Au) and is formed on the pad 114, and the second bump 522 is formed by harder and cheaper copper (Cu), so as to reduce the packaging costs and avoid the chip 126 being damaged during the formation of the first bump 120.
Referring to
In the present embodiment of the invention, after the first bump 620 and the second bump 622 are formed, the coating layer 638 can be formed by sputtering technology or the electroless plating technology. In another implementation, the solder wire (not illustrated) used for forming the first bump 620 and the second bump 622 has a coating layer 638. After the wire bonding head forms the first bump 620 and the second bump 622 on the substrate, the coating layer 638 is still on the first bump 620 and the second bump 622.
Preferably but not restrictively, the coating layer 638 is formed by at least one of nickel (Ni) and gold (Au), and can be realized by such as nickel-gold alloy, chemical nickel gold (ENIG) or gold.
In the fifth embodiment, the coating layer 638 covers the first bump 620 and the second bump 622 of
Referring to
The second bump 722 is disposed on the first bump 720, and the electrical element 708 is disposed on the second bump 722.
The insulating layer 726 protects the bump assembly 718 from environmental erosion such as oxidization. The insulating layer 726 completely avoids the electrical element 708 overflowing to the pad 114, so that the electrical properties and reliability between the bump assembly 718 and the pad 114 are enhanced
In the sixth embodiment, the insulating layer 726 is formed on the semiconductor chip interconnection structure 712 of
When the insulating layer 726 is formed on the bump assembly of the second embodiment (
In another implementation (not illustrated), the bump assembly of the semiconductor chip interconnection structure 712 can form a coating layer 638 of the fifth embodiment.
Referring to
Each bump assembly 818 comprises a first bump 820 and a second bump 822. The two bump assemblies 818 are both formed on the pad 814.
If smaller first bumps 820 are used, two sets of first bumps 820 can be formed on the pad 814, so that the number of I/O contacts can be further increased.
In another implementation (not illustrated), the insulating layer 726 of the sixth embodiment can be formed on the semiconductor chip interconnection structure 812 to protect the bump assembly 818. Preferably but not restrictively, a portion (not illustrated) of the insulating layer 726 can be disposed between two bump assemblies 818.
In another implementation (not illustrated), the coating layer 638 of the fifth embodiment can be formed on the bump assembly of the semiconductor chip interconnection structure 812.
Further, the above semiconductor chip interconnection structures 212, 312, 412, 512, 612, 712 and 812 can be electrically connected to the substrate 110 of
According to the semiconductor chip interconnection structure and the semiconductor package disclosed in the above embodiments of the invention, the outer diameter of the bump contacting the electrical element is suitably designed, so that the surface of the bump contacting the electrical element is large enough. Thus, the electrical element, having been reflown, can be completely formed on the bump, and will not overflow to the pad to spoil the pad. The electrical element, having been flown, can be completely formed on the bump, so that the electrical element is more controllable in the manufacturing process. Thus, the height, the size and the shape of the electrical element 108 can be controlled according to the needs in the manufacturing process, so that the manufacturing process is more flexible. Moreover, the size of bump contacting the electrical element is independent of the size of the pad. Thus, the bump can be designed to have a larger size for bearing larger electrical element, so that the bonding and electrical properties between the electrical element and the counterpart member are enhanced.
While the invention has been described by way of example and in terms of the preferred embodiment(s), it is to be understood that the invention is not limited thereto. On the contrary, it is intended to cover various modifications and similar arrangements and procedures, and the scope of the appended claims therefore should be accorded the broadest interpretation so as to encompass all such modifications and similar arrangements and procedures.
Number | Date | Country | Kind |
---|---|---|---|
99128133 | Aug 2010 | TW | national |
101020507572.6 | Aug 2010 | CN | national |
201010264703.3 | Aug 2010 | CN | national |
This application claims the benefit of U.S. provisional application Ser. No. 61/237,370, filed Aug. 27, 2009, the subject matter of which is incorporated herein by reference.
Number | Date | Country | |
---|---|---|---|
61237370 | Aug 2009 | US |