1. Field of Invention
This invention relates to a leadless semiconductor package. More particularly, the present invention is related to a leadless semiconductor package with high reliability of the attachment of the encapsulation to the leadless lead-frame.
2. Related Art
Integrated circuits (chip) packaging technology is becoming a limiting factor for the development in packaged integrated circuits of higher performance. Semiconductor package designers are struggling to keep pace with the increase in pin count, size limitations, low profile, and other evolving requirements for packaging and mounting integrated circuits. Nowadays, ball grid array package (BGA) and chip scale package (CSP) are wildly applied to chip package with high I/Os and assembly package for thermal enhance integrated circuits.
However, assembly package with lead frame possesses great marketing for that it can provide low-cost solutions for current semiconductor package. Due to lead frame with long inner leads and outer leads, such conventional lead-frame assembly package can not applied to chip scale package and low profile package. Thus leadless assembly package, such as Quad-Flat-Non-lead Package which is initially developed by Matsushita, is wildly provided in the semiconductor package industry to reduce the size of the assembly package in the recent years. Referring to
As mentioned above, the chip paddle 112 of said leadless semiconductor package 100 exposes the bottom 112c and 114b of the leadless semiconductor package 100 so as to further improve the thermal performance of said leadless semiconductor package. Furthermore, due to the short leads, the impedance will be lower. Accordingly, the leadless semiconductor package is especially adapted to the assembly package with high-frequency devices, which are performed at the frequency from 10 GHz to 100 GHz, enclosed therein. In such a manner, such leadless semiconductor package has low cost and competitive price. Therefore the leadless semiconductor package is adapted to cell phone, personal digital application (PDA), digital camera and information application (IA).
As can be seen, the reliability of said leadless semiconductor package is relied upon the performance of the attachment of the encapsulation 150 to the lead frame 110. Namely, when the encapsulation 150 is able to well encapsulate the lead frame 110, the leadless semiconductor package will have a better reliability. However, usually the reliability of the leadless semiconductor package is lowered due to the change of working temperature. Namely, the encapsulation 150 is usually caused to be separated from the lead frame 110 upon the difference of the thermal coefficient of expansion of the lead frame 110 from that of the encapsulation 150 and the changes of the working temperature. Besides, referring to
Consequently, providing another leadless lead-frame to solve the mentioned-above disadvantages is the most important task in this invention.
In view of the above-mentioned problems, this invention is to provide a leadless semiconductor package with high reliability of the attachment of the encapsulation to the leadless lead-frame. Moreover, this invention is also to provide a leadless semiconductor package with high reliability of the attachment of the chip to the leadless lead-frame.
To achieve the above-mentioned, a leadless lead-frame is provided, wherein the leadless lead-frame mainly comprises a chip paddle and a plurality of leads. The chip paddle has chip disposal areas, and a grounding area surrounding the chip disposal area. The grounding area has a recession with a recession-bottom and a recession-wall connecting to the recession-bottom. An angle is formed between the recession-wall and the recession-bottom, and the angle is less than 90 degrees. The leads surround the chip paddle. The chip paddle has a cavity and the cavity has a cavity-bottom serving as the chip disposal area, and the depth of the cavity is equal to half of the thickness of the chip paddle.
To achieve the above-mentioned, a package is provided, wherein the package comprises a lead-fram and a chip. The leadless lead-frame mainly comprises a chip paddle and a plurality of leads. The chip paddle has chip disposal areas, and a grounding area surrounding the chip disposal area. The grounding area has a recession with a recession-bottom and a recession-wall connecting to the recession-bottom. An angle is formed between the recession-wall and the recession-bottom, and the angle is less than 90 degrees. The leads surround the chip paddle. The chip paddle has a cavity and the cavity has a cavity-bottom serving as the chip disposal area, and the depth of the cavity is equal to half of the thickness of the chip paddle. The chip is disposed in the cavity of the chip paddle of the lead-frame and attached to the lead-frame. The chip has an active surface and a back surface opposed to the active surface.
Besides, as mentioned above, a chip is placed in the cavity so that the total thickness of the package comprising the leadless lead-frame will become smaller. Accordingly, there is a thinner leadless semiconductor package provided.
The invention will become more fully understood from the detailed description given herein below illustrations only, and thus are not limitative of the present invention, and wherein:
The leadless lead-frame according to the preferred embodiments of this invention will be described herein below with reference to the accompanying drawings, wherein the same reference numbers refer to the same elements.
In accordance with a first preferred embodiment as shown in
Furthermore, referring to
Referring to
As mentioned above, usually the depth of the chip disposal area 312a is about half of the thickness of the chip paddle 310. Thus, when the chip 320 is placed in the chip disposal area 212a through an adhesive 330 disposed in the chip disposal area 312a, the adhesive 330 could be well controlled in the chip disposal area 312a due to the grounding area 312b be protruded from the chip disposal area 312a. In such a manner, the wires 340 will be well bonded to the grounding area 212b. In addition, because the chip 320 is placed in the chip disposal area 312a, the top of the wires connecting the leads 314 or the grounding area 312b will be lowered to shorten the length of the wires and lower the impedance of the wires. Accordingly, the electrical performance will be enhanced. Besides, the chip is placed in the chip disposal area so that the total thickness of the package will become smaller. Accordingly, there is a thinner leadless semiconductor package provided. Although the chip 320 is electrically connected to the leads 314 through the electrically conductive wires, the chip 320 is also able to be electrically connected to the leads through bumps by flip-chip bonding method, such as gold bumps and solder bumps.
Although the invention has been described in considerable detail with reference to certain preferred embodiments, it will be appreciated and understood that various changes and modifications may be made without departing from the spirit and scope of the invention as defined in the appended claims.
| Number | Date | Country | Kind |
|---|---|---|---|
| 92137725 A | Dec 2003 | TW | national |
This is a Continuation of application Ser. No. 10/876,458, filed on Jun. 28, 2004, the entire disclosure of which is hereby incorporated by reference.
| Number | Name | Date | Kind |
|---|---|---|---|
| 6713849 | Hasebe et al. | Mar 2004 | B2 |
| 7196409 | Den Ouden | Mar 2007 | B2 |
| 20020027297 | Ikenaga et al. | Mar 2002 | A1 |
| 20040041242 | Joshi | Mar 2004 | A1 |
| Number | Date | Country | |
|---|---|---|---|
| 20070164406 A1 | Jul 2007 | US |
| Number | Date | Country | |
|---|---|---|---|
| Parent | 10876458 | Jun 2004 | US |
| Child | 11704997 | US |