This application contains nucleotide sequence and/or amino acid sequence disclosure in computer readable form and a written sequence listing, the entire contents of both of which are expressly incorporated by reference in their entirety as though fully set forth herein.
The present disclosure is directed generally to inventive methods and apparatus relating to detection and measurement of one or more analytes via electronic sensors.
Electronic devices and components have found numerous applications in chemistry and biology (more generally, “life sciences”), especially for detection and measurement of various aspects of chemical reactions and substance composition. One such electronic device is referred to as an ion-sensitive field effect transistor, often denoted in the relevant literature as ISFET (or pHFET). ISFETs conventionally have been explored, primarily in the academic and research community, to facilitate measurement of the hydrogen ion concentration of a solution (commonly denoted as “pH”).
More specifically, an ISFET is an impedance transformation device that operates in a manner similar to that of a MOSFET (Metal Oxide Semiconductor Field Effect Transistor), and is particularly configured to selectively measure ion activity in a solution (e.g., hydrogen ions in the solution are the “analyte”). A detailed theory of operation of an ISFET is given in “Thirty years of ISFETOLOGY: what happened in the past 30 years and what may happen in the next 30 years,” P. Bergveld, Sens. Actuators, 88 (2003), pp. 1-20, which publication is hereby incorporated herein by reference.
Like a MOSFET, the operation of an ISFET is based on the modulation of charge concentration caused by a MOS (Metal-Oxide-Semiconductor) capacitance constituted by the polysilicon gate 64, the gate oxide 65 and the region 60 of the n-type well 54 between the source and the drain. When a negative voltage is applied across the gate and source regions (VGs<0 Volts), a “p-channel” 63 is created at the interface of the region 60 and the gate oxide 65 by depleting this area of electrons. This p-channel 63 extends between the source and the drain, and electric current is conducted through the p-channel when the gate-source potential VGS is negative enough to attract holes from the source into the channel. The gate-source potential at which the channel 63 begins to conduct current is referred to as the transistor's threshold voltage VTH (the transistor conducts when VGS has an absolute value greater than the threshold voltage VTH). The source is so named because it is the source of the charge carriers (holes for a p-channel) that flow through the channel 63; similarly, the drain is where the charge carriers leave the channel 63.
In the ISFET 50 of
As also shown in
With respect to ion sensitivity, an electric potential difference, commonly referred to as a “surface potential,” arises at the solid/liquid interface of the passivation layer 72 and the analyte solution 74 as a function of the ion concentration in the sensitive area 78 due to a chemical reaction (e.g., usually involving the dissociation of oxide surface groups by the ions in the analyte solution in proximity to the sensitive area 78). This surface potential in turn affects the threshold voltage VTH of the ISFET; thus, it is the threshold voltage VTH of the ISFET that varies with changes in ion concentration in the analyte solution 74 in proximity to the sensitive area 78.
where VDS is the voltage between the drain and the source, and β is a transconductance parameter (in units of Amps/Volts2) given by:
where μ represents the carrier mobility, Cox is the gate oxide capacitance per unit area, and the ratio W/L is the width to length ratio of the channel 63. If the reference electrode 76 provides an electrical reference or ground (VG=0 Volts), and the drain current ID and the drain-to-source voltage VDS are kept constant, variations of the source voltage VS of the ISFET directly track variations of the threshold voltage VTH, according to Eq. (1); this may be observed by rearranging Eq. (1) as:
Since the threshold voltage VTH of the ISFET is sensitive to ion concentration as discussed above, according to Eq. (3) the source voltage VS provides a signal that is directly related to the ion concentration in the analyte solution 74 in proximity to the sensitive area 78 of the ISFET. In exemplary conventional ISFETs employing a silicon nitride or silicon oxynitride passivation layer 72 for pH-sensitivity, a threshold voltage sensitivities ΔVTH (i.e., a change in threshold voltage with change in pH of the analyte solution) of approximately 30 mV/pH to 50 mV/pH have been observed (with a theoretical maximum sensitivity of 59.2 mV/pH at 298 degrees Kelvin).
Prior research efforts to fabricate ISFETs for pH measurements based on conventional CMOS processing techniques typically have aimed to achieve high signal linearity over a pH range from 1-14. Using an exemplary threshold sensitivity of approximately 50 mV/pH, and considering Eq. (3) above, this requires a linear operating range of approximately 700 mV for the source voltage VS. As discussed above in connection with
Previous efforts to fabricate two-dimensional arrays of ISFETs based on the ISFET design of
As shown in
As also shown in
In the column design of Milgrew et al. shown in
It should also be appreciated that in the column design of Milgrew et al. shown in
Furthermore, in the design of Milgrew et al., the p-channel MOSFET required to implement the transmission gate S1 in each pixel (e.g., see S11p in
The array design of Milgrew et al. was implemented using a 0.35 micrometer (μm) conventional CMOS fabrication process. In this process, various design rules dictate minimum separation distances between features. For example, according to the 0.35 μm CMOS design rules, with reference to
In sum, the ISFET pixel design of Milgrew et al. is aimed at ensuring accurate hydrogen ion concentration measurements over a pH range of 1-14. To ensure measurement linearity, the source and body of each pixel's ISFET are electrically coupled together. To ensure a full range of pH measurements, a transmission gate S1 is employed in each pixel to transmit the source voltage of an enabled pixel. Thus, each pixel of Milgrew's array requires four transistors (p-channel ISFET, p-channel MOSFET, and two n-channel MOSFETs) and two separate n-wells (
As noted earlier, individual ISFETs and arrays of ISFETs similar to those discussed above have been employed as sensing devices in a variety of applications involving chemistry and biology. In particular, ISFETs have been employed as pH sensors in various processes involving nucleic acids such as DNA. Some examples of employing ISFETs in various life-science related applications are given in the following publications, each of which is incorporated herein by reference: Massimo Barbaro, Annalisa Bonfiglio, Luigi Raffo, Andrea Alessandrini, Paolo Facci and Inrich Barak, “Fully electronic DNA hybridization detection by a standard CMOS biochip,” Sensors and Actuators B: Chemical, Volume 118, Issues 1-2, 2006, pp. 41-46; Toshinari Sakurai and Yuzuru Husimi, “Real-time monitoring of DNA polymerase reactions by a micro ISFET pH sensor,” Anal. Chem., 64(17), 1992, pp 1996-1997; S. Purushothaman, C. Toumazou, J. Georgiou, “Towards fast solid state DNA sequencing,” Circuits and Systems, vol. 4, 2002, pp. IV-169 to IV-172; S. Purushothaman, C. Toumazou, C. P. Ou, “Protons and single nucleotide polymorphism detection: A simple use for the Ion Sensitive Field Effect Transistor,” Sensors and Actuators B: Chemical, Vol. 114, no. 2, 2006, pp. 964-968; A. L. Simonian, A. W. Flounders, J. R. Wild, “FET-Based Biosensors for The Direct Detection of Organophosphate Neurotoxins,” Electroanalysis, Vol. 16, No. 22, 2004, pp. 1896-1906; C. Toumazou, S. Purushothaman, “Sensing Apparatus and Method,” United States Patent Application 2004-0134798, published Jul. 15, 2004; and T. W. Koo, S. Chan, X. Su, Z. Jingwu, M. Yamakawa, V. M. Dubin, “Sensor Arrays and Nucleic Acid Sequencing Applications,” United States Patent Application 2006-0199193, published Sep. 7, 2006.
In general, the development of rapid and sensitive nucleic acid sequencing methods utilizing automated DNA sequencers has significantly advanced the understanding of biology. The term “sequencing” refers to the determination of a primary structure (or primary sequence) of an unbranched biopolymer, which results in a symbolic linear depiction known as a “sequence” that succinctly summarizes much of the atomic-level structure of the sequenced molecule. “DNA sequencing” particularly refers to the process of determining the nucleotide order of a given DNA fragment. Analysis of entire genomes of viruses, bacteria, fungi, animals and plants is now possible, but such analysis generally is limited due to the cost and throughput of sequencing. More specifically, present conventional sequencing methods are limited in terms of the accuracy of the sequence, the length of individual templates that can be sequenced, the cost of the sequence, and the rate of sequence determination.
Despite improvements in sample preparation and sequencing technologies, none of the present conventional sequencing strategies, including those to date that may involve ISFETs, has provided the cost reductions required to increase throughput to levels required for analysis of large numbers of individual human genomes. It is necessary to sequence a large number of individual genomes to understand the genetic basis of disease and aging. In addition, a large number of cancers will need to be sequenced to understand the somatic changes underlying cancer. Some recent efforts have made significant gains in both the ability to prepare genomes for sequencing and to sequence large numbers of templates simultaneously. However, these and other efforts are still limited by the relatively large size of the reaction volumes needed to prepare templates that are detectable by these systems, as well as the need for special nucleotide analogues, and complex enzymatic or fluorescent methods to read out the bases.
Applicants have recognized and appreciated that large arrays of ISFETs may be particularly configured and employed to facilitate DNA sequencing techniques based on monitoring changes in chemical processes relating to DNA synthesis. More generally, Applicants have recognized and appreciated that large arrays of chemically-sensitive FETs may be employed to detect and measure concentrations/levels of a variety of analytes (e.g., hydrogen ions, other ions, non-ionic molecules or compounds, binding events, etc.) in a host of chemical and/or biological processes (chemical reactions, cell cultures, neural activity, nucleic acid sequencing, etc.) in which valuable information may be obtained based on such analyte measurements.
Accordingly, various embodiments of the present disclosure is directed generally to inventive methods and apparatus relating to large scale FET arrays for measuring one or more analytes. In the various embodiments disclosed herein, FET arrays include multiple “chemFETs,” or chemically-sensitive field-effect transistors, that act as chemical sensors. An ISFET, as discussed above, is a particular type of chemFET that is configured for ion detection, and ISFETs may be employed in various embodiments disclosed herein. Other types of chemFETs contemplated by the present disclosure include ENFETs, which are configured for sensing of specific enzymes. It should be appreciated, however, that the present disclosure is not limited to ISFETs and ENFETs, but more generally relates to any FET that is configured for some type of chemical sensitivity.
According to yet other embodiments, the present disclosure is directed generally to inventive methods and apparatus relating to the delivery to the above-described large scale chemFET arrays of appropriate chemical samples to evoke corresponding responses. The chemical samples may comprise (liquid) analyte samples in small reaction volumes, to facilitate high speed, high-density determination of chemical (e.g., ion or other constituent) concentration or other measurements on the analyte.
For example, some embodiments are directed to a “very large scale” two-dimensional chemFET sensor array (e.g., greater than 256 k sensors), in which one or more chemFET-containing elements or “pixels” constituting the sensors of such an array are configured to monitor one or more independent chemical reactions or events occurring in proximity to the pixels of the array. In some exemplary implementations, the array may be coupled to one or more microfluidics structures that form one or more reaction chambers, or “wells” or “microwells,” over individual sensors or groups of sensors of the array, and apparatus which delivers analyte samples to the wells and removes them from the wells between measurements. Even when microwells are not employed, the sensor array may be coupled to one or more microfluidics structures for the delivery of one or more analytes to the pixels and for removal of analyte(s) between measurements. Accordingly, inventive aspects of this disclosure, which are desired to be protected, include the various microfluidic structures which may be employed to flow reagents/analytes to and from the wells or pixels, the methods of manufacture of the array of wells, methods and structures for coupling the wells with the pixels of the array, and methods and apparatus for loading the wells with DNA-bearing beads when the apparatus is used for DNA sequencing or related analysis.
A unique reference electrode and its coupling to the flow cell are also shown.
In various embodiments, an analyte of particular interest is hydrogen ions, and large scale ISFET arrays according to the present disclosure are specifically configured to measure pH. In other embodiments, the chemical reactions being monitored may relate to DNA synthesis processes, or other chemical and/or biological processes, and chemFET arrays may be specifically configured to measure pH or one or more other analytes that provide relevant information relating to a particular chemical process of interest. In various aspects, the chemFET arrays are fabricated using conventional CMOS processing technologies, and are particularly configured to facilitate the rapid acquisition of data from the entire array (scanning all of the pixels to obtain corresponding pixel output signals).
With respect to analyte detection and measurement, it should be appreciated that in various embodiments discussed in greater detail below, one or more analytes measured by a chemFET array according to the present disclosure may include any of a variety of chemical substances that provide relevant information regarding a chemical process or chemical processes of interest (e.g., binding of multiple nucleic acid strands, binding of an antibody to an antigen, etc.). In some aspects, the ability to measure levels or concentrations of one or more analytes, in addition to merely detecting the presence of an analyte, provides valuable information in connection with the chemical process or processes. In other aspects, mere detection of the presence of an analyte or analytes of interest may provide valuable information.
A chemFET array according to various inventive embodiments of the present disclosure may be configured for sensitivity to any one or more of a variety of analytes/chemical substances. In one embodiment, one or more chemFETs of an array may be particularly configured for sensitivity to one or more analytes representing one or more binding events (e.g., associated with a nucleic acid sequencing process), and in other embodiments different chemFETs of a given array may be configured for sensitivity to different analytes. For example, in one embodiment, one or more sensors (pixels) of the array may include a first type of chemFET configured to be chemically sensitive to a first analyte, and one or more other sensors of the array may include a second type of chemFET configured to be chemically sensitive to a second analyte different from the first analyte. In one exemplary implementation, the first analyte may represent a first binding event associated with a nucleic acid sequencing process, and the second analyte may represent a second binding event associated with the nucleic acid sequencing process. Of course, it should be appreciated that more than two different types of chemFETs may be employed in any given array to detect and/or measure different types of analytes/binding events. In general, it should be appreciated in any of the embodiments of sensor arrays discussed herein that a given sensor array may be “homogeneous” and include chemFETs of substantially similar or identical types to detect and/or measure a same type of analyte (e.g., pH or other ion concentration), or a sensor array may be “heterogeneous” and include chemFETs of different types to detect and/or measure different analytes.
In yet other aspects, Applicants have specifically improved upon the ISFET array design of Milgrew et al. discussed above in connection with
With respect to chemFET array fabrication, Applicants have further recognized and appreciated that various techniques employed in a conventional CMOS fabrication process, as well as various post-fabrication processing steps (wafer handling, cleaning, dicing, packaging, etc.), may in some instances adversely affect performance of the resulting chemFET array. For example, with reference again to
Accordingly, one embodiment of the present invention is directed to an apparatus, comprising an array of CMOS-fabricated sensors, each sensor comprising one chemically-sensitive field effect transistor (chemFET) and occupying an area on a surface of the array of ten micrometers by ten micrometers or less.
Another embodiment is directed to a sensor array, comprising a two-dimensional array of electronic sensors including at least 512 rows and at least 512 columns of the electronic sensors, each sensor comprising one chemically-sensitive field effect transistor (chemFET) configured to provide at least one output signal representing a presence and/or concentration of an analyte proximate to a surface of the two-dimensional array.
Another embodiment is directed to an apparatus, comprising an array of CMOS-fabricated sensors, each sensor comprising one chemically-sensitive field effect transistor (chemFET). The array of CMOS-fabricated sensors includes more than 256 sensors, and a collection of chemFET output signals from all chemFETs of the array constitutes a frame of data. The apparatus further comprises control circuitry coupled to the array and configured to generate at least one array output signal to provide multiple frames of data from the array at a frame rate of at least 1 frame per second. In one aspect, the frame rate may be at least 10 frames per second. In another aspect, the frame rate may be at least 20 frames per second. In yet other aspects, the frame rate may be at least 30, 40, 50, 70 or up to 100 frames per second.
Another embodiment is directed to an apparatus, comprising an array of CMOS-fabricated sensors, each sensor comprising a chemically-sensitive field effect transistor (chemFET). The chemFET comprises a floating gate structure, and a source and a drain having a first semiconductor type and fabricated in a region having a second semiconductor type, wherein there is no electrical conductor that electrically connects the region having the second semiconductor type to either the source or the drain.
Another embodiment is directed to an apparatus, comprising an array of electronic sensors, each sensor consisting of three field effect transistors (FETs) including one chemically-sensitive field effect transistor (chemFET).
Another embodiment is directed to an apparatus, comprising an array of electronic sensors, each sensor comprising three or fewer field effect transistors (FETs), wherein the three or fewer FETs includes one chemically-sensitive field effect transistor (chemFET).
Another embodiment is directed to an apparatus, comprising an array of electronic sensors, each sensor comprising a plurality of field effect transistors (FETs) including one chemically-sensitive field effect transistor (chemFET), and a plurality of electrical conductors electrically connected to the plurality of FETs, wherein the plurality of FETs are arranged such that the plurality of electrical conductors includes no more than four conductors traversing an area occupied by each sensor and interconnecting multiple sensors of the array.
Another embodiment is directed to an apparatus, comprising an array of CMOS-fabricated sensors, each sensor comprising a plurality of field effect transistors (FETs) including one chemically-sensitive field effect transistor (chemFET), wherein all of the FETs in each sensor are of a same channel type and implemented in a single semiconductor region of an array substrate.
Another embodiment is directed to a sensor array, comprising a plurality of electronic sensors arranged in a plurality of rows and a plurality of columns. Each sensor comprises one chemically-sensitive field effect transistor (chemFET) configured to provide at least one output signal representing a presence and/or a concentration of an analyte proximate to a surface of the array. For each column of the plurality of columns, the array further comprises column circuitry configured to provide a constant drain current and a constant drain-to-source voltage to respective chemFETs in the column, the column circuitry including two operational amplifiers and a diode-connected FET arranged in a Kelvin bridge configuration with the respective chemFETs to provide the constant drain-to-source voltage.
Another embodiment is directed to a sensor array, comprising a plurality of electronic sensors arranged in a plurality of rows and a plurality of columns. Each sensor comprises one chemically-sensitive field effect transistor (chemFET) configured to provide at least one output signal representing a concentration of ions in an analyte proximate to a surface of the array. The array further comprises at least one row select shift register to enable respective rows of the plurality of rows, and at least one column select shift register to acquire chemFET output signals from respective columns of the plurality of columns.
Another embodiment is directed to an apparatus, comprising an array of CMOS-fabricated sensors, each sensor comprising a chemically-sensitive field effect transistor (chemFET). The chemFET comprises a floating gate structure, and a source and a drain having a first semiconductor type and fabricated in a region having a second semiconductor type, wherein there is no electrical conductor that electrically connects the region having the second semiconductor type to either the source or the drain. The array includes a two-dimensional array of at least 512 rows and at least 512 columns of the CMOS-fabricated sensors. Each sensor consists of three field effect transistors (FETs) including the chemFET, and each sensor includes a plurality of electrical conductors electrically connected to the three FETs. The three FETs are arranged such that the plurality of electrical conductors includes no more than four conductors traversing an area occupied by each sensor and interconnecting multiple sensors of the array. All of the FETs in each sensor are of a same channel type and implemented in a single semiconductor region of an array substrate. A collection of chemFET output signals from all chemFETs of the array constitutes a frame of data. The apparatus further comprises control circuitry coupled to the array and configured to generate at least one array output signal to provide multiple frames of data from the array at a frame rate of at least 20 frames per second.
Another embodiment is directed to a method for processing an array of CMOS-fabricated sensors, each sensor comprising a chemically-sensitive field effect transistor (chemFET). The method comprises: A) dicing a semiconductor wafer including the array to form at least one diced portion including the array; and B) performing a forming gas anneal on the at least one diced portion.
Another embodiment is directed to a method for processing an array of CMOS-fabricated sensors. Each sensor comprises a chemically-sensitive field effect transistor (chemFET) having a chemically-sensitive passivation layer of silicon nitride and/or silicon oxynitride deposited via plasma enhanced chemical vapor deposition (PECVD). The method comprises depositing at least one additional passivation material on the chemically-sensitive passivation layer so as to reduce a porosity and/or increase a density of the passivation layer.
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with a chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, detecting the incorporation of the one or more known nucleotide triphosphates by a change in current at the at least one chemFET. The array may be comprised of at least two, at least three, at least four, at least five, at least six, at least seven, at least eight, at least nine, at least ten, at least 100, at least 500, at least 1000, at least 104, at least 105, at least 106, at least 107, or more chemFET (or chemFET sensors, or sensors, as the terms are used interchangeably herein).
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with a chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, detecting the incorporation of the one or more known nucleotide triphosphates by a change in current at the at least one chemFET, wherein the chemFET array is any of the foregoing arrays.
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with a chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, and detecting the incorporation of the one or more known nucleotide triphosphates by a change in current at the at least one chemFET within the array, wherein a center-to-center distance between adjacent reaction chambers is 1-10 μm.
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with a chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, detecting the incorporation of the one or more known nucleotide triphosphates by the generation of sequencing reaction byproduct, wherein (a) the chemFET array comprises more than 256 sensors, or (b) a center-to-center distance between adjacent reaction chambers (or “pitch”) is 1-10 μm.
In yet another aspect, the invention provides a method for sequencing a nucleic acid comprising fragmenting a target nucleic acid to generate a plurality of fragmented nucleic acids, attaching each of the plurality of fragmented nucleic acids to individual beads to generate a plurality of beads each attached to a single fragmented nucleic acid, amplifying the number of fragmented nucleic acids on each bead, delivering the plurality of beads attached to amplified fragmented nucleic acids to a chemical-sensitive field effect transistor (chemFET) array having a separate reaction chamber for each sensor in the array, wherein only one bead is situated in each reaction chamber, and performing a sequencing reaction simultaneously in the plurality of reaction chambers.
In still another aspect, the invention provides a method for sequencing nucleic acids comprising fragmenting a target nucleic acid to generate a plurality of fragmented nucleic acids, amplifying each fragmented nucleic acid separately in the presence of a bead and binding amplified copies of the fragmented nucleic acid to the bead, thereby producing a plurality of beads each having attached multiple identical copies of a fragmented nucleic acid, delivering the plurality of beads each having attached multiple identical copies of a fragmented nucleic acid to a chemical-sensitive field effect transistor (chemFET) array having a separate reaction chamber for each chemFET sensor in the array, wherein only one bead is situated in each reaction chamber, and performing a sequencing reaction simultaneously in the plurality of reaction chambers.
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with an chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, and detecting a change in the level of a sequencing byproduct as an indicator of incorporation of the one or more known nucleotide triphosphates.
The change in the level may an increase or a decrease in a level relative to that level prior to incorporation of the one or more known nucleotide triphosphates. The change in the level may be read as a change in current at a chemFET sensor or a change in pH, but it is not so limited.
In one embodiment, the sequencing byproduct is inorganic pyrophosphate (PPi). In a related embodiment, PPi is detected by binding to a PPi receptor on the surface of one or more chemFET sensors in the array.
Various embodiments apply equally to the methods disclosed herein and they are recited once for brevity. In some embodiments, the center-to-center distance between adjacent reaction chambers is about 2-9 μm, about 2 μm, about 5 μm, or about 9 μm. In some embodiments, the chemFET array comprises more than 256 sensors (and optionally more than 256 corresponding reaction chambers (or wells), more than 103 sensors (and optionally more than 103 corresponding reaction chambers), more than 104 sensors (and optionally more than 104 corresponding reaction chambers), more than 105 sensors (and optionally more than 105 corresponding reaction chambers), or more than 106 sensors (and optionally more than 106 corresponding reaction chambers). In some embodiments, the chemFET array comprises at least 512 rows and at least 512 columns of sensors.
In some embodiments, the sequencing reaction byproduct is inorganic pyrophosphate (PPi). In some embodiments, PPi is measured directly. In some embodiments, the PPi is measured in the absence of a PPi receptor. In some embodiments, the sequencing reaction byproduct is hydrogen ions. In some embodiments, the sequencing reaction byproduct is inorganic phosphate (Pi). In still other embodiments, the chemFET detects changes in any combination of the byproducts, optionally in combination with other parameters, as described herein.
In another aspect, the invention provides a method for sequencing a nucleic acid comprising disposing a plurality of template nucleic acids into a plurality of reaction chambers, wherein the plurality of reaction chambers is in contact with an chemical-sensitive field effect transistor (chemFET) array comprising at least one chemFET for each reaction chamber, and wherein each of the template nucleic acids is hybridized to a sequencing primer and is bound to a polymerase, synthesizing a new nucleic acid strand by incorporating one or more known nucleotide triphosphates sequentially at the 3′ end of the sequencing primer, directly detecting release of inorganic pyrophosphate (PPi) as an indicator of incorporation of the one or more known nucleotide triphosphates.
In some embodiments, the PPi is directly detected by binding to a PPi receptor immobilized on the chemFET. In some embodiments, the PPi is directly detected by the chemFET in the absence of a PPi receptor.
In another aspect, the invention provides a method for sequencing nucleic acids comprising fragmenting a template nucleic acid to generate a plurality of fragmented nucleic acids, attaching one strand from each of the plurality of fragmented nucleic acids individually to beads to generate a plurality of beads each having a single stranded fragmented nucleic acid attached thereto, delivering the plurality of beads having a single stranded fragmented nucleic acid attached thereto to a chemFET array having a separate reaction chamber for each sensor in the area, and wherein only one bead is situated in each reaction chamber, and performing a sequencing reaction simultaneously in the plurality of chambers.
In another aspect, the invention provides an apparatus comprising a chemical-sensitive field effect transistor (chemFET) having disposed on its surface a PPi receptor.
In still another aspect, the invention provides an apparatus comprising a chemical-sensitive field effect transistor (chemFET) array comprising a plurality of chemFET sensors each having a PPi receptor disposed on its surface, wherein the plurality is a subset of the chemFET sensors in the array. In a related embodiment, the array comprises at least three chemFET sensors. The subset may represent 10%, 25%, 33%, 50%, 75% or more of the sensors in the array.
In some embodiments, the PPi selective receptor is Compound 1, Compound 2, Compound 3, Compound 4, Compound 5, Compound 6, Compound 7, Compound 8, Compound 9 or Compound 10 as shown in
In another aspect, the invention provides an apparatus comprising a chemical-sensitive field effect transistor (chemFET) array having disposed on its surface a biological array.
The biological array may be a nucleic acid array, a protein array including but not limited to an enzyme array, an antibody array and an antibody fragment array, a cell array, and the like. The chemical array may be an organic small molecule array, or an inorganic molecule array, but it is not so limited. The chemFET array may comprise at least 5, 10, 102, 103, 104, 105, 106 or more sensors. The biological or chemical array may be arranged into a plurality of “cells” or spatially defined regions and each of these regions is situated over a different sensor in the chemFET array, in some embodiments.
In yet another aspect, the invention provides a method for detecting a nucleic acid comprising contacting a nucleic acid array disposed on a chemFET array with a sample, and detecting binding of a nucleic acid from the sample to one or more regions on the nucleic acid array.
In another aspect, the invention provides a method for detecting a protein comprising contacting a protein array disposed on a chemFET array with a sample, and detecting binding of a protein from the sample to one or more regions on the protein array.
In yet another aspect, the invention provides a method for detecting a nucleic acid comprising contacting a protein array disposed on a chemFET array with a sample, and detecting binding of a nucleic acid from the sample to one or more regions on the protein array.
In another aspect, the invention provides a method for detecting an antigen comprising contacting an antibody array disposed on a chemFET array with a sample, and detecting binding of a antigen from the sample to one or more regions on the antibody array.
In another aspect, the invention provides a method for detecting an enzyme substrate or inhibitor comprising contacting an enzyme array disposed on a chemFET array with a sample, and detecting binding of an entity from the sample to one or more regions on the enzyme array.
It should be appreciated that all combinations of the foregoing concepts and additional concepts discussed in greater detail below (provided such concepts are not mutually inconsistent) are contemplated as being part of the inventive subject matter disclosed herein. In particular, all combinations of claimed subject matter appearing at the end of this disclosure are contemplated as being part of the inventive subject matter disclosed herein. It should also be appreciated that terminology explicitly employed herein that also may appear in any disclosure incorporated by reference should be accorded a meaning most consistent with the particular concepts disclosed herein.
In the drawings, like reference characters generally refer to the same parts throughout the different views. Also, the drawings are not necessarily to scale, emphasis instead being placed upon generally illustrating the various concepts discussed herein.
Following below are more detailed descriptions of various concepts related to, and embodiments of, inventive methods and apparatus relating to large scale chemFET arrays for analyte measurements. It should be appreciated that various concepts introduced above and discussed in greater detail below may be implemented in any of numerous ways, as the disclosed concepts are not limited to any particular manner of implementation. Examples of specific implementations and applications are provided primarily for illustrative purposes.
Various inventive embodiments according to the present disclosure are directed at least in part to a semiconductor-based/microfluidic hybrid system that combines the power of microelectronics with the biocompatibility of a microfluidic system. In some examples below, the microelectronics portion of the hybrid system is implemented in CMOS technology for purposes of illustration. It should be appreciated, however, that the disclosure is not intended to be limiting in this respect, as other semiconductor-based technologies may be utilized to implement various aspects of the microelectronics portion of the systems discussed herein.
One embodiment disclosed herein is directed to a large sensor array (e.g., a two-dimensional array) of chemically-sensitive field effect transistors (chemFETs), wherein the individual chemFET sensor elements or “pixels” of the array are configured to detect analyte concentration changes in a host of chemical and/or biological processes (chemical reactions, cell cultures, neural activity, nucleic acid sequencing processes, etc.) occurring in proximity to the array. Examples of chemFETs contemplated by various embodiments discussed in greater detail below include, but are not limited to, ion-sensitive field effect transistors (ISFETs) and enzyme-sensitive field effect transistors (ENFETs). In one exemplary implementation, one or more microfluidic structures is/are fabricated above the chemFET sensor array to provide for containment and/or confinement of a chemical reaction in which an analyte of interest may be produced. For example, in one implementation, the microfluidic structure(s) may be configured as one or more “wells” (e.g., small reaction chambers) disposed above one or more sensors of the array, such that the one or more sensors over which a given well is disposed detect and measure analyte concentration in the given well.
In some embodiments, such a chemFET array/microfluidics hybrid structure may be used to analyze solution(s)/material(s) of interest containing nucleic acids. For example, such structures may be employed to process nucleic acids in a multitude of ways that utilize sequencing of nucleic acids. In various aspects, such sequencing can be performed to determine the identity of a sequence of nucleic acids, for single nucleotide polymorphism detection in nucleic acid fragments, for nucleic acid expression profiling (comparing the nucleic acid expression profile between two or more states—e.g., comparing between diseased and normal tissue or comparing between untreated tissue and tissue treated with drug, enzymes, radiation or chemical treatment), for haplotyping (comparing genes or variations in genes on each of the two alleles present in a human subject), for karyotyping (diagnostically comparing one or more genes in a test tissue—typically from an embryo/fetus prior to conception to detect birth defects—with the same genes from “normal” karyotyped subjects), and for genotyping (comparing one or more genes in a first individual of a species with the same genes in other individuals of the same species). It should be appreciated, however, that while some illustrative examples of the concepts disclosed herein are applied in the context of nucleic acid processing, application of the concepts disclosed herein relating to chemFET sensor arrays is not limited to these examples.
In the system 1000 of
In one aspect, the flow cell 200 of the system 1000 shown in
Once a nucleic acid template is loaded into respective wells of the flow cell 200, bridge amplification can then be performed in the wells, the product denatured, and sequencing by synthesis or ligation then performed. Other methods of amplification in the wells (with the products captured in the wells) are envisioned, including rolling circle amplification, or other strategies using isothermal or non-isothermal amplification techniques such as PCR. As illustrated in
In sum, the flow cell 200 in the system of
With respect to the ISFET array 100 of the system 1000 shown in
The ISFET array 100 is not limited to any particular size, as one- or two-dimensional arrays, including as few as two to 256 pixels (e.g., 16 by 16 pixels in a two-dimensional implementation) or as many as 54 mega-pixels (e.g., 7400 by 7400 pixels in a two-dimensional implementation) or even greater may be fabricated and employed for various chemical/biological analysis purposes pursuant to the concepts disclosed herein. In one embodiment of the exemplary system shown in
More generally, a chemFET array according to various embodiments of the present disclosure may be configured for sensitivity to any one or more of a variety of analytes/chemical substances. In one embodiment, one or more chemFETs of an array may be particularly configured for sensitivity to one or more analytes representing one or more binding events (e.g., associated with a nucleic acid sequencing process), and in other embodiments different chemFETs of a given array may be configured for sensitivity to different analytes. For example, in one embodiment, one or more sensors (pixels) of the array may include a first type of chemFET configured to be chemically sensitive to a first analyte, and one or more other sensors of the array may include a second type of chemFET configured to be chemically sensitive to a second analyte different from the first analyte. In one exemplary implementation, the first analyte may represent a first binding event associated with a nucleic acid sequencing process, and the second analyte may represent a second binding event associated with the nucleic acid sequencing process. Of course, it should be appreciated that more than two different types of chemFETs may be employed in any given array to detect and/or measure different types of analytes/binding events. In general, it should be appreciated in any of the embodiments of sensor arrays discussed herein that a given sensor array may be “homogeneous” and include chemFETs of substantially similar or identical types to detect and/or measure a same type of analyte (e.g., pH or other ion concentration), or a sensor array may be “heterogeneous” and include chemFETs of different types to detect and/or measure different analytes. For simplicity of discussion, again the example of an ISFET is discussed below in various embodiments of sensor arrays, but the present disclosure is not limited in this respect, and several other options for analyte sensitivity are discussed in further detail below (e.g., in connection with
In exemplary implementations based on 0.35 micrometer CMOS processing techniques (or CMOS processing techniques capable of smaller feature sizes), each pixel of the ISFET array 100 may include an ISFET and accompanying enable/select components, and may occupy an area on a surface of the array of approximately ten micrometers by ten micrometers (i.e., 100 micrometers2) or less; stated differently, arrays having a pitch (pixel-to-pixel spacing) on the order of 10 micrometers or less may be realized. An array pitch on the order of 10 micrometers or less using a 0.35 micrometer CMOS processing technique constitutes a significant improvement in terms of size reduction with respect to prior attempts to fabricate ISFET arrays, which resulted in pixel sizes on the order of at least 12 micrometers or greater.
More specifically, in some embodiments discussed further below based on the inventive concepts disclosed herein, an array pitch of approximately nine (9) micrometers allows an ISFET array including over 256,000 pixels (i.e., a 512 by 512 array), together with associated row and column select and bias/readout electronics, to be fabricated on a 7 millimeter by 7 millimeter semiconductor die, and a similar sensor array including over four million pixels (i.e., a 2048 by 2048 array, over 4 Mega-pixels) to be fabricated on a 21 millimeter by 21 millimeter die. In other examples, an array pitch of approximately 5 micrometers allows an ISFET array including approximately 1.55 Mega-pixels (i.e., a 1348 by 1152 array) and associated electronics to be fabricated on a 9 millimeter by 9 millimeter die, and an ISFET sensor array including over 14 Mega-pixels and associated electronics on a 22 millimeter by 20 millimeter die. In yet other implementations, using a CMOS fabrication process in which feature sizes of less than 0.35 micrometers are possible (e.g., 0.18 micrometer CMOS processing techniques), ISFET sensor arrays with a pitch significantly below 5 micrometers may be fabricated (e.g., array pitch of 2.6 micrometers or pixel area of less than 8 or 9 micrometers2), providing for significantly dense ISFET arrays. Of course, it should be appreciated that pixel sizes greater than 10 micrometers (e.g., on the order of approximately 20, 50, 100 micrometers or greater) may be implemented in various embodiments of chemFET arrays according to the present disclosure.
In other aspects of the system shown in
Having provided a general overview of the role of a chemFET (e.g., ISFET) array 100 in an exemplary system 1000 for measuring one or more analytes in connection with nucleic acid processing, following below are more detailed descriptions of exemplary chemFET arrays according to various inventive embodiments of the present disclosure that may be employed in a variety of applications including, but not limited to, nucleic acid processing. Again, for purposes of illustration, chemFET arrays according to the present disclosure are discussed below using the particular example of an ISFET array, but other types of chemFETs may be employed in alternative embodiments.
An noted above, various inventive embodiments disclosed herein specifically improve upon the ISFET array design of Milgrew et al. discussed above in connection with
To this end,
In one aspect of the embodiment shown in
As illustrated in
By employing the diode-connected MOSFET Q6 in the bias/readout circuitry 110j of
In
In another aspect of the embodiment shown in
In yet another aspect of the embodiment shown in
By not tying the body connection of each ISFET to its source, the possibility of some non-zero source-to-body voltage VSB may give rise to the “body effect,” as discussed above in connection with
In the top view of
With reference now to the cross-sectional view of
In the composite cross-sectional view of
Above the substrate, gate oxide, and polysilicon layers shown in
As indicated above,
Thus, the pixel chip layout design shown in
In one exemplary implementation, the gate oxide 165 for the ISFET may be fabricated to have a thickness on the order of approximately 75 Angstroms, giving rise to a gate oxide capacitance per unit area Cox of 4.5 fF/μm2. Additionally, the polysilicon gate 164 may be fabricated with dimensions corresponding to a channel width W of 1.2 μm and a channel length L of from 0.35 to 0.6 μm (i.e., W/L ranging from approximately 2 to 3.5), and the doping of the region 160 may be selected such that the carrier mobility for the p-channel is 190 cm2/V·s (i.e., 1.9 E10 μm2/V·s). From Eq. (2) above, this results in an ISFET transconductance parameter β on the order of approximately 170 to 300 μA/V2. In other aspects of this exemplary implementation, the analog supply voltage VDDA is 3.3 Volts, and VB1 and VB2 are biased so as to provide a constant ISFET drain current IDj on the order of 5 μA (in some implementations, VB1 and VB2 may be adjusted to provide drain currents from approximately 1 μA to 20 μA). Additionally, the MOSFET Q6 (see bias/readout circuitry 110j in
With respect to the analyte-sensitive passivation layer 172 shown in
For CMOS processes involving aluminum as the metal (which has a melting point of approximately 650 degrees Celsius), a silicon nitride and/or silicon oxynitride passivation layer generally is formed via plasma-enhanced chemical vapor deposition (PECVD), in which a glow discharge at 250-350 degrees Celsius ionizes the constituent gases that form silicon nitride or silicon oxynitride, creating active species that react at the wafer surface to form a laminate of the respective materials. In one exemplary process, a passivation layer having a thickness on the order of approximately 1.0 to 1.5 μm may be formed by an initial deposition of a thin layer of silicon oxynitride (on the order of 0.2 to 0.4 μm) followed by a slighting thicker deposition of silicon oxynitride (on the order of 0.5 μm) and a final deposition of silicon nitride (on the order of 0.5 μm). Because of the low deposition temperature involved in the PECVD process, the aluminum metallization is not adversely affected.
However, Applicants have recognized and appreciated that while a low temperature PECVD process provides adequate passivation for conventional CMOS devices, the low-temperature process results in a generally low-density and somewhat porous passivation layer, which in some cases may adversely affect ISFET threshold voltage stability. In particular, during ISFET device operation, a low-density porous passivation layer over time may absorb and become saturated with ions from the solution, which may in turn cause an undesirable time-varying drift in the ISFETs threshold voltage VTH, making accurate measurements challenging.
In view of the foregoing, in one embodiment a CMOS process that uses tungsten metal instead of aluminum may be employed to fabricate ISFET arrays according to the present disclosure. The high melting temperature of Tungsten (above 3400 degrees Celsius) permits the use of a higher temperature low pressure chemical vapor deposition (LPCVD) process (e.g., approximately 700 to 800 degrees Celsius) for a silicon nitride or silicon oxynitride passivation layer. The LPCVD process typically results in significantly more dense and less porous films for the passivation layer, thereby mitigating the potentially adverse effects of ion absorption from the analyte solution leading to ISFET threshold voltage drift.
In yet another embodiment in which an aluminum-based CMOS process is employed to fabricate ISFET arrays according to the present disclosure, the passivation layer 172 shown in
Examples of materials suitable for the second portion 172B (or other additional portions) of the passivation layer 172 for particular sensitivity to hydrogen ions include, but are not limited to, silicon nitride, silicon oxynitride, aluminum oxide (Al2O3), tantalum oxide (Ta3O5), tin oxide (SnO2) and silicon dioxide (SiO2). In one aspect, the second portion 172B (or other additional portions) may be deposited via a variety of relatively low temperature processes including, but not limited to, RF sputtering, DC magnetron sputtering, thermal or e-beam evaporation, and ion-assisted depositions. In another aspect, a pre-sputtering etch process may be employed, prior to deposition of the second portion 172B, to remove any native oxide residing on the first portion 172A (alternatively, a reducing environment, such as an elevated temperature hydrogen environment, may be employed to remove native oxide residing on the first portion 172A). In yet another aspect, a thickness of the second portion 172B may be on the order of approximately 0.04 μm to 0.06 μm (400 to 600 Angstroms) and a thickness of the first portion may be on the order of 1.0 to 1.5 as discussed above. In some exemplary implementations, the first portion 172A may include multiple layers of silicon oxynitride and silicon nitride having a combined thickness of 1.0 to 1.5 and the second portion 172B may include a single layer of either aluminum oxide or tantalum oxide having a thickness of approximately 400 to 600 Angstroms. Again, it should be appreciated that the foregoing exemplary thicknesses are provided primarily for purposes of illustration, and that the disclosure is not limited in these respects.
Thus it is to be understood that the chemFET arrays described herein may be used to detect various analytes and, by doing so, may monitor a variety of reactions and/or interactions. It is also to be understood that the emphasis on hydrogen ion detection (in the form of a pH change) is for the sake of convenience and brevity and that other analytes (including other ions) can be substituted for hydrogen in these descriptions.
The chemFETs, including ISFETs, described herein are capable of detecting any analyte that is itself capable of inducing a change in electric field. The analyte need not be charged in order to be detected by the sensor. For example, depending on the embodiment, the analyte may be positively charged (i.e., a cation), negatively charged (i.e., an anion), zwitterionic (i.e., capable of having two equal and opposite charges but overall neutral), and polar yet neutral. This list is not intended as exhaustive as other analyte classes as well as species within each class will be readily contemplated by those of ordinary skill in the art based on the disclosure provided herein.
In the broadest sense of the invention, passivation layer may or may not be coated and the analyte may or may not interact with the passivation layer. As an example, the passivation layer may be comprised of silicon nitride and the analyte may be something other than hydrogen ions. As a specific example, the passivation layer may be comprised of silicon nitride and the analyte may be inorganic pyrophosphate (PPi). In these instances, PPi is detected directly (i.e., in the absence of PPi receptors attached to the passivation layer either directly or indirectly).
If the analyte being detected is hydrogen (or alternatively hydroxide), then it is preferable to use weak buffers so that changes in either ionic species can be detected at the passivation layer. If the analyte being detected is something other than hydrogen (or hydroxide) but there is some possibility of a pH change in the solution during the reaction or detection step, then it is preferable to use a strong buffer so that changes in pH do not interfere with the detection of the analyte. A buffer is an ionic molecule that resists changes in pH. Buffers are able to neutralize acids or bases added to or generated in a solution, resulting in no effective pH change in the solution. It is to be understood that any buffer is suitable provided it has a pKa in the desired range. A suitable buffer is one that functions in about the pH range of 6 to 9, and more preferably 6.5 to 8.5. The strength of a buffer is a relative term since it depends on the nature, strength and concentration of the acid or base added to or generated in the solution of interest. A weak buffer is a buffer that allows detection (and therefore is not able to otherwise control) pH changes of about at least +/−0.005, 0.01, 0.015, 0.02, 0.03, 0.04, 0.05, 0.10, 0.15, 0.20, 0.25, 0.30, 0.35, 0.45, 0.50, or more. In some embodiments, the pH change is on the order of about 0.005 (e.g., per nucleotide incorporation) and is preferably an increase in pH. A strong buffer is a buffer that controls pH changes of about at least +/−0.005, 0.01, 0.015, 0.02, 0.03, 0.04, 0.05, 0.10, 0.15, 0.20, 0.25, 0.30, 0.35, 0.45, 0.50, or more. Buffer strength can be varied by varying the concentration of the buffer species itself. Thus low concentration buffers can be low strength buffers. Examples include those having less than 1 mM (e.g., 50-100 μM) buffer species. A non-limiting example of a weak buffer suitable for the sequencing reactions described herein wherein pH change is the readout is 0.1 mM Tris or Tricine. Examples of suitable weak buffers are provided in the Examples and are also known in the art. Higher concentration buffers can be stronger buffers. Examples include those having 1-25 mM buffer species. A non-limiting example of a strong buffer suitable for the sequencing reactions described herein wherein PPi is read directly is 1, 5 or 25 mM (or more) Tris or Tricine. One of ordinary skill in the art will be able to determine the optimal buffer for use in the reactions and detection methods encompassed by the invention.
In some embodiments, the passivation layer and/or the molecules coated thereon dictate the analyte specificity of the array readout.
Detection of hydrogen ions (in the form of pH) can be carried out using a passivation layer made of silicon nitride (Si3N4), silicon oxynitride (Si2N2O), silicon oxide (SiO2), aluminum oxide (Al2O3), tantalum pentoxide (Ta2O5), tin oxide or stannic oxide (SnO2), and the like.
The passivation layer can also detect other ion species directly including but not limited to calcium, potassium, sodium, iodide, magnesium, chloride, lithium, lead, silver, cadmium, nitrate, phosphate, dihydrogen phosphate, and the like.
In some embodiments, the passivation layer is coated with a receptor for the analyte of interest. The receptor binds selectively to the analyte of interest. As used herein, a receptor that binds selectively to an analyte is a molecule that binds preferentially to that analyte (i.e., its binding affinity for that analyte is greater than its binding affinity for any other analyte). Its binding affinity for the analyte of interest may be 2-fold, 3-fold, 4-fold, 5-fold, 6-fold, 7-fold, 8-fold, 9-fold, 10-fold, 15-fold, 20-fold, 25-fold, 30-fold, 40-fold, 50-fold, 100-fold or more than its binding affinity for any other analyte. In addition to its relative binding affinity, the receptor must also have an absolute binding affinity that is sufficiently high to efficiently bind the analyte of interest (i.e., it must have a sufficient sensitivity). Receptors having binding affinities in the picomolar to micromolar range are suitable. Preferably such interaction are reversible.
The receptor may be of any nature (e.g., chemical, nucleic acid, peptide, lipid, combinations thereof and the like). The analyte too may be of any nature provided there exists a receptor that binds to it selectively and in some instances specifically. It is to be understood however that the invention further contemplates detection of analytes in the absence of a receptor. An example of this is the detection of PPi and Pi by the passivation layer in the absence of PPi or Pi receptors.
In one aspect, the invention contemplates receptors that are ionophores. As used herein, an ionophore is a molecule that binds selectively to an ionic species, whether anion or cation. In the context of the invention, the ionophore is the receptor and the ion to which it binds is the analyte. Ionophores of the invention include art-recognized carrier ionophores (i.e., small lipid-soluble molecules that bind to a particular ion) derived from microorganisms. Various ionophores are commercially available from sources such as Calbiochem.
Detection of some ions can be accomplished through using the passivation layer itself or through the use of receptors coated onto the passivation layer. For example, potassium can be detected selectively using the polysiloxane, valinomycin, or salinomycin; sodium can be detected selectively using monensin, nystatin, or SQI-Pr; calcium can be detected selectively using ionomycin, calcimycine (A23187), or CA 1001 (ETH 1001).
Receptors able to bind more than one ion can also be used in some instances.
For example, beauvericin can be used to detect calcium and/or barium ions, nigericin can be used to detect potassium, hydrogen and/or lead ions, and gramicidin can be used to detect hydrogen, sodium and/or potassium ions. One of ordinary skill in the art will recognize that these compounds can be used in applications in which single ion specificity is not required or in which it is unlikely (or impossible) that other ions which the compounds bind will be present or generated.
In other embodiments, including but not limited to nucleic acid sequencing applications, receptors that bind selectively to inorganic pyrophosphate (PPi) can be used. Examples of PPi receptors include those compounds shown in
As another example, receptors for neurotoxins are described in Simonian Electroanalysis 2004, 16: 1896-1906.
Receptors may be attached to the passivation layer covalently or non-covalently. Covalent attachment of a receptor to the passivation layer may be direct or indirect (e.g., through a linker).
The bifunctional linker may be a homo-bifunctional linker or a hetero-bifunctional linker, depending upon the nature of the molecules to be conjugated. Homo-bifunctional linkers have two identical reactive groups. Hetero-bifunctional linkers are have two different reactive groups. Various types of commercially available linkers are reactive with one or more of the following groups: primary amines, secondary amines, sulphydryls, carboxyls, carbonyls and carbohydrates. Examples of amine-specific linkers are bis(sulfosuccinimidyl)suberate, bis[2-(succinimidooxycarbonyloxy)ethyl]sulfone, disuccinimidyl suberate, disuccinimidyl tartarate, dimethyl adipimate.2HCl, dimethyl pimelimidate.2HCl, dimethyl suberimidate.2HCl, and ethylene glycolbis-[succinimidyl-[succinate]]. Linkers reactive with sulfhydryl groups include bismaleimidohexane, 1,4-di-[3′-(2′-pyridyldithio)-propionamido)]butane, 1-[p-azidosalicylamido]-4-[odoacetamido]butane, and N-[4-(p-azidosalicylamido) butyl]-3′-[2′-pyridyldithio]propionamide. Linkers preferentially reactive with carbohydrates include azidobenzoyl hydrazine. Linkers preferentially reactive with carboxyl groups include 4-[p-azidosalicylamido]butylamine.
Heterobifunctional linkers that react with amines and sulfhydryls include N-succinimidyl-3-[2-pyridyldithio]propionate, succinimidyl [4-iodoacetyl]aminobenzoate, succinimidyl 4[N-maleimidomethyl]cyclohexane-1-carboxylate, m-maleimidobenzoyl-N-hydroxysuccinimide ester, sulfosuccinimidyl 6-[3-[2-pyridyldithio]propionamido]hexanoate, and sulfosuccinimidyl 4-[N-maleimidomethyl]cyclohexane-1-carboxylate. Heterobifunctional linkers that react with carboxyl and amine groups include 1-ethyl-3-[3-dimethylaminopropyl]-carbodiimide hydrochloride. Heterobifunctional linkers that react with carbohydrates and sulfhydryls include 4-[N-maleimidomethyl]-cyclohexane-1-carboxylhydrazide.2HCl, 4-(4-N-maleimidophenyl)-butyric acid hydrazide.2HCl, and 3-[2-pyridyldithio]propionyl hydrazide.
Alternatively, receptors may be non-covalently coated onto the passivation layer. Non-covalent deposition of the receptor to the passivation layer may involve the use of a polymer matrix. The polymer may be naturally occurring or non-naturally occurring and may be of any type including but not limited to nucleic acid (e.g., DNA, RNA, PNA, LNA, and the like, or mimics, derivatives, or combinations thereof), amino acid (e.g., peptides, proteins (native or denatured), and the like, or mimics, derivatives, or combinations thereof, lipids, polysaccharides, and functionalized block copolymers. The receptor may be adsorbed onto and/or entrapped within the polymer matrix.
Alternatively, the receptor may be covalently conjugated or crosslinked to the polymer (e.g., it may be “grafted” onto a functionalized polymer).
An example of a suitable peptide polymer is poly-lysine (e.g., poly-L-lysine). Examples of other polymers include block copolymers that comprise polyethylene glycol (PEG), polyamides, polycarbonates, polyalkylenes, polyalkylene glycols, polyalkylene oxides, polyalkylene terepthalates, polyvinyl alcohols, polyvinyl ethers, polyvinyl esters, polyvinyl halides, polyvinylpyrrolidone, polyglycolides, polysiloxanes, polyurethanes, alkyl cellulose, hydroxyalkyl celluloses, cellulose ethers, cellulose esters, nitrocelluloses, polymers of acrylic and methacrylic esters, methyl cellulose, ethyl cellulose, hydroxypropyl cellulose, hydroxypropyl methyl cellulose, hydroxybutyl methyl cellulose, cellulose acetate, cellulose propionate, cellulose acetate butyrate, cellulose acetate phthalate, carboxylethyl cellulose, cellulose triacetate, cellulose sulphate sodium salt, poly(methyl methacrylate), poly(ethyl methacrylate), poly(butylmethacrylate), poly(isobutyl methacrylate), poly(hexylmethacrylate), poly(isodecyl methacrylate), poly(lauryl methacrylate), poly(phenyl methacrylate), poly(methyl acrylate), poly(isopropyl acrylate), poly(isobutyl acrylate), poly(octadecyl acrylate), polyethylene, polypropylene, poly(ethylene glycol), poly(ethylene oxide), poly(ethylene terephthalate), poly(vinyl alcohols), polyvinyl acetate, polyvinyl chloride, polystyrene, polyhyaluronic acids, casein, gelatin, glutin, polyanhydrides, polyacrylic acid, alginate, chitosan, poly(methyl methacrylates), poly(ethyl methacrylates), poly(butylmethacrylate), poly(isobutyl methacrylate), poly(hexylmethacrylate), poly(isodecyl methacrylate), poly(lauryl methacrylate), poly(phenyl methacrylate), poly(methyl acrylate), poly(isopropyl acrylate), poly(isobutyl acrylate), and poly(octadecyl acrylate), poly(lactide-glycolide), copolyoxalates, polycaprolactones, polyesteramides, polyorthoesters, polyhydroxybutyric acid, polyanhydrides, poly (styrene-b-isobutylene-b-styrene) (SIBS) block copolymer, ethylene vinyl acetate, poly(meth)acrylic acid, polymers of lactic acid and glycolic acid, polyanhydrides, poly(ortho)esters, polyurethanes, poly(butic acid), poly(valeric acid), and poly(lactide-cocaprolactone), and natural polymers such as alginate and other polysaccharides including dextran and cellulose, collagen, albumin and other hydrophilic proteins, zein and other prolamines and hydrophobic proteins, copolymers and mixtures thereof, and chemical derivatives thereof including substitutions and/or additions of chemical groups, for example, alkyl, alkylene, hydroxylations, oxidations, and other modifications routinely made by those skilled in the art.
Another issue that relates to ISFET threshold voltage stability and/or predictability involves trapped charge that may accumulate on metal layers of CMOS-fabricated devices as a result of various processing activities during or following array fabrication (e.g., back-end-of-line processing such as plasma metal etching, wafer cleaning, dicing, packaging, handling, etc.). In particular, with reference to
One opportunity for trapped charge to accumulate includes plasma etching of the topmost metal layer 304. Applicants have recognized and appreciated that other opportunities for charge to accumulate on one or more conductors of the floating gate structure includes wafer dicing, during which the abrasive process of a dicing saw cutting through a wafer generates static electricity, and/or various post-processing wafer handling/packaging steps, where automated machinery that handles/transports wafers may be sources of electrostatic discharge (ESD) to conductors of the floating gate structure. If there is no connection to the silicon substrate (or other semi-conductor substrate) to provide an electrical path to bleed off such charge accumulation, charge may build up to the point of causing undesirable changes or damage to the gate oxide 165 (e.g., charge injection into the oxide, or low-level oxide breakdown to the underlying substrate). Trapped charge in the gate oxide or at the gate oxide-semiconductor interface in turn can cause undesirable and/or unpredictable variations in ISFET operation and performance.
In view of the foregoing, other inventive embodiments of the present disclosure are directed to methods and apparatus for improving ISFET performance by reducing trapped charge or mitigating the antenna effect. In one embodiment, trapped charge may be reduced after a sensor array has been fabricated, while in other embodiments the fabrication process itself may be modified to reduce trapped charge that could be induced by some conventional process steps. In yet other embodiments, both “during fabrication” and “post fabrication” techniques may be employed in combination to reduce trapped charge and thereby improve ISFET performance.
With respect to alterations to the fabrication process itself to reduce trapped charge, in one embodiment the thickness of the gate oxide 165 shown in
In another embodiment, the topmost metal layer 304 of the ISFETs floating gate structure 170 shown in
In yet another embodiment, the metal etch process for the topmost metal layer 304 may be modified to include wet chemistry or ion-beam milling rather than plasma etching. For example, the metal layer 304 could be etched using an aqueous chemistry selective to the underlying dielectric (e.g., see http://www.transene.com/aluminum.html, hereby incorporated herein by reference). Another alternative approach employs ion-milling rather than plasma etching for the metal layer 304. Ion-milling is commonly used to etch materials that cannot be readily removed using conventional plasma or wet chemistries. The ion-milling process does not employ an oscillating electric field as does a plasma, so that charge build-up does not occur in the metal layer(s). Yet another metal etch alternative involves optimizing the plasma conditions so as to reduce the etch rate (i.e. less power density).
In yet another embodiment, architecture changes may be made to the metal layer to facilitate complete electrical isolation during definition of the floating gate. In one aspect, designing the metal stack-up so that the large area ISFET floating gate is not connected to anything during its final definition may require a subsequent metal layer serving as a “jumper” to realize the electrical connection to the floating gate of the transistor. This “jumper” connection scheme prevents charge flow from the large floating gate to the transistor. This method may be implemented as follows (M=metal layer): i) M1 contacting Poly gate electrode; ii) M2 contacting M1; iii) M3 defines floating gate and separately connects to M2 with isolated island; iv) M4 jumper, having very small area being etched over the isolated islands and connections to floating gate M3, connects the M3 floating gate to the M1/M2/M3 stack connected to the Poly gate immediately over the transistor active area; and v) M3 to M4 interlayer dielectric is removed only over the floating gate so as to expose the bare M3 floating gate. In the method outlined immediately above, step v) need not be done, as the ISFET architecture according to some embodiments discussed above leaves the M4 passivation in place over the M4 floating gate. In one aspect, removal may nonetheless improve ISFET performance in other ways (i.e. sensitivity). In any case, the final chemically-sensitive passivation layer may be a thin sputter-deposited ion-sensitive metal-oxide layer. It should be appreciated that the over-layer jumpered architecture discussed above may be implemented in the standard CMOS fabrication flow to allow any of the first three metal layers to be used as the floating gates (i.e. M1, M2 or M3).
With respect to post-fabrication processes to reduce trapped charge, in one embodiment a “forming gas anneal” may be employed as a post-fabrication process to mitigate potentially adverse effects of trapped charge. In a forming gas anneal, CMOS-fabricated ISFET devices are heated in a hydrogen and nitrogen gas mixture. The hydrogen gas in the mixture diffuses into the gate oxide 165 and neutralizes certain forms of trapped charges. In one aspect, the forming gas anneal need not necessarily remove all gate oxide damage that may result from trapped charges; rather, in some cases, a partial neutralization of some trapped charge is sufficient to significantly improve ISFET performance. In exemplary annealing processes according to the present disclosure, ISFETs may be heated for approximately 30 to 60 minutes at approximately 400 to 425 degrees Celsius in a hydrogen/nitrogen mixture that includes 10% to 15% hydrogen. In one particular implementation, annealing at 425 degrees Celsius at 30 minutes in a hydrogen/nitrogen mixture that includes 10% hydrogen is observed to be particularly effective at improving ISFET performance. For aluminum CMOS processes, the temperature of the anneal should be kept at or below 450 degrees Celsius to avoid damaging the aluminum metallurgy. In another aspect of an annealing process according to the present disclosure, the forming gas anneal is performed after wafers of fabricated ISFET arrays are diced, so as to ensure that damage due to trapped charge induced by the dicing process itself, and/or other pre-dicing processing steps (e.g., plasma etching of metals) may be effectively ameliorated.
In yet other processes for mitigating potentially adverse effects of trapped charge according to embodiments of the present disclosure, a variety of “electrostatic discharge {ESD)-sensitive protocols” may be adopted during any of a variety of wafer post-fabrication handling/packaging steps. For example, in one exemplary process, anti-static dicing tape may be employed to hold wafer substrates in place (e.g., during the dicing process). Also, although high-resistivity (e.g., 10 MΩ) deionized water conventionally is employed in connection with cooling of dicing saws, according to one embodiment of the present disclosure less resistive/more conductive water may be employed for this purpose to facilitate charge conduction via the water; for example, deionized water may be treated with carbon dioxide to lower resistivity and improve conduction of charge arising from the dicing process. Furthermore, conductive and grounded die-ejection tools may be used during various wafer dicing/handling/packaging steps, again to provide effective conduction paths for charge generated during any of these steps, and thereby reduce opportunities for charge to accumulate on one or more conductors of the floating gate structure of respective ISFETs of an array.
In yet another embodiment involving a post-fabrication process to reduce trapped charge, the gate oxide region of an ISFET may be irradiated with UV radiation. With reference again to
To facilitate a UV irradiation process to reduce trapped charge, Applicants have recognized and appreciated that materials other than silicon nitride and silicon oxynitride generally need to be employed in the passivation layer 172 shown in
In another aspect of an embodiment involving UV irradiation, each ISFET of a sensor array must be appropriately biased during a UV irradiation process to facilitate reduction of trapped charge. In particular, high energy photons from the UV irradiation, impinging upon the bulk silicon region 160 in which the ISFET conducting channel is formed, create electron-hole pairs which facilitate neutralization of trapped charge in the gate oxide as current flows through the ISFETs conducting channel. To this end, an array controller, discussed further below in connection with
Also, as discussed above, it should be appreciated that arrays according to various embodiments of the present invention may be fabricated according to conventional CMOS fabrications techniques, as well as modified CMOS fabrication techniques (e.g., to facilitate realization of various functional aspects of the chemFET arrays discussed herein, such as additional deposition of passivation materials, process steps to mitigate trapped charge, etc.) and other semiconductor fabrication techniques beyond those conventionally employed in CMOS fabrication. Additionally, various lithography techniques may be employed as part of an array fabrication process. For example, in one exemplary implementation, a lithography technique may be employed in which appropriately designed blocks are “stitched” together by overlapping the edges of a step and repeat lithography exposures on a wafer substrate by approximately 0.2 micrometers. In a single exposure, the maximum die size typically is approximately 21 millimeters by 21 millimeters. By selectively exposing different blocks (sides, top & bottoms, core, etc.) very large chips can be defined on a wafer (up to a maximum, in the extreme, of one chip per wafer, commonly referred to as “wafer scale integration”).
In one aspect of the array 100 shown in
In
Regarding the column select shift registers 1941 and 1942, these are implemented in a manner similar to that of the row select shift registers, with each column select shift register comprising 256 series-connected flip-flops and responsible for enabling readout from either the odd columns of the array or the even columns of the array. For example,
With reference again for the moment to
In the embodiment of
In one exemplary implementation, the switches of both the even and odd output drivers 1981 and 1982 (e.g., the switches 1912, 1914, . . . 191512 shown in
The ability of the bus 175 to settle quickly following enabling of successive switches in turn facilitates rapid data acquisition from the array. To this end, in some embodiments the switches 191 of the output drivers 1981 and 1982 are particularly configured to significantly reduce the settling time of the bus 175. Both the n-channel and the p-channel MOSFETs of a given switch add to the capacitance of the bus 175; however, n-channel MOSFETs generally have better frequency response and current drive capabilities than their p-channel counterparts. In view of the foregoing, Applicants have recognized and appreciated that some of the superior characteristics of n-channel MOSFETs may be exploited to improve settling time of the bus 175 by implementing “asymmetric” switches in which respective sizes for the n-channel MOSFET and p-channel MOSFET of a given switch are different.
For example, in one embodiment, with reference to
While the example above describes asymmetric switches 191 for the output drivers 1981 and 1982 in which the n-channel MOSFET is larger than the p-channel MOSFET, it should be appreciated that in another embodiment, the converse may be implemented, namely, asymmetric switches in which the p-channel MOSFET is larger than the n-channel MOSFET. In one aspect of this embodiment, with reference again to
In yet another embodiment directed to facilitating rapid settling of the bus 175 shown in
In one aspect of the array design discussed above in connection with
Generally, the array controller 250 provides various supply voltages and bias voltages to the array 100, as well as various signals relating to row and column selection, sampling of pixel outputs and data acquisition. In particular, the array controller 250 reads the two analog output signals Vout1 (odd columns) and Vout2 (even columns) including multiplexed respective pixel voltage signals from the array 100 and then digitizes these respective pixel signals to provide measurement data to the computer 260, which in turn may store and/or process the data. In some implementations, the array controller 250 also may be configured to perform or facilitate various array calibration and diagnostic functions, and an optional array UV irradiation treatment as discussed above in connection with
As illustrated in
As also shown in
Regarding data acquisition from the array 100, in one embodiment the array controller 250 of
The array controller 250 of
In the embodiment of
In one implementation, the array controller 250 controls the array 100 to enable rows successively, one at a time. For example, with reference again for the moment to
In
In addition to controlling the sensor array and ADCs, the timing generator 256 may be configured to facilitate various array calibration and diagnostic functions, as well as an optional UV irradiation treatment. To this end, the timing generator may utilize the signal LSTV indicating the selection of the last row of the array and the signal LSTH to indicate the selection of the last column of the array. The timing generator 256 also may be responsible for generating the CAL signal which applies the reference voltage VREF to the column buffer amplifiers, and generating the UV signal which grounds the drains of all ISFETs in the array during a UV irradiation process (see
With respect to the computer interface 252 of the array controller 250, in one exemplary implementation the interface is configured to facilitate a data rate of approximately 200 MB/sec to the computer 260, and may include local storage of up to 400 MB or greater. The computer 260 is configured to accept data at a rate of 200 MB/sec, and process the data so as to reconstruct an image of the pixels (e.g., which may be displayed in false-color on a monitor). For example, the computer may be configured to execute a general-purpose program with routines written in C++ or Visual Basic to manipulate the data and display is as desired.
Having discussed several aspects of an exemplary ISFET array and an array controller according to the present disclosure,
In one aspect of the embodiment shown in
In particular,
For each of the first and second groups of rows, the array 100A of
In one exemplary implementation of the array 100A of
Like the array 100 of
As noted in
While the exemplary arrays discussed above in connection with
The array 100D of
The array 100E of
Thus, in various examples of ISFET arrays based on the inventive concepts disclosed herein, an array pitch of approximately nine (9) micrometers (e.g., a sensor surface area of less than ten micrometers by ten micrometers) allows an ISFET array including over 256,000 pixels (i.e., a 512 by 512 array), together with associated row and column select and bias/readout electronics, to be fabricated on a 7 millimeter by 7 millimeter semiconductor die, and a similar sensor array including over four million pixels (i.e., a 2048 by 2048 array, over 4 Mega-pixels) to be fabricated on a 21 millimeter by 21 millimeter die. In other examples, an array pitch of approximately 5 micrometers allows an ISFET array including approximately 1.55 Mega-pixels (i.e., a 1348 by 1152 array) and associated electronics to be fabricated on a 9 millimeter by 9 millimeter die, and an ISFET sensor array including over 14 Mega-pixels and associated electronics on a 22 millimeter by 20 millimeter die. In yet other implementations, using a CMOS fabrication process in which feature sizes of less than 0.35 micrometers are possible (e.g., 0.18 micrometer CMOS processing techniques), ISFET sensor arrays with a pixel size/pitch significantly below 5 micrometers may be fabricated (e.g., array pitch of 2.6 micrometers or pixel/sensor area of less than 8 or 9 micrometers2), providing for significantly dense ISFET arrays.
In the embodiments of ISFET arrays discussed above, array pixels employ a p-channel ISFET, as discussed above in connection with
For example,
One of the primary differences between the n-channel ISFET pixel design of
In addition to the pixel designs shown in
In
In
Turning from the sensor discussion, we will now be addressing the combining of the ISFET array with a microwell array and the attendant fluidics. As most of the drawings of the microwell array structure are presented only in cross-section or showing that array as only a block in a simplified diagram,
Fluidic System: Apparatus and Method for Use with High Density Electronic Sensor Arrays
For many uses, to complete a system for sensing chemical reactions or chemical agents using the above-explained high density electronic arrays, techniques and apparatus are required for delivery to the array elements (called “pixels”) fluids containing chemical or biochemical components for sensing. In this section, exemplary techniques and methods will be illustrated, which are useful for such purposes, with desirable characteristics.
As high speed operation of the system may be desired, it is preferred that the fluid delivery system, insofar as possible, not limit the speed of operation of the overall system.
Accordingly, needs exist not only for high-speed, high-density arrays of ISFETs or other elements sensitive to ion concentrations or other chemical attributes, or changes in chemical attributes, but also for related mechanisms and techniques for supplying to the array elements the samples to be evaluated, in sufficiently small reaction volumes as to substantially advance the speed and quality of detection of the variable to be sensed.
There are two and sometimes three components or subsystems, and related methods, involved in delivery of the subject chemical samples to the array elements: (1) macrofluidic system of reagent and wash fluid supplies and appropriate valving and ancillary apparatus, (2) a flow cell and (3) in many applications, a microwell array. Each of these subsystems will be discussed, though in reverse order.
Microwell Array
As discussed elsewhere, for many uses, such as in DNA sequencing, it is desirable to provide over the array of semiconductor sensors a corresponding array of microwells, each microwell being small enough preferably to receive only one DNA-loaded bead, in connection with which an underlying pixel in the array will provide a corresponding output signal.
The use of such a microwell array involves three stages of fabrication and preparation, each of which is discussed separately: (1) creating the array of microwells to result in a chip having a coat comprising a microwell array layer; (2) mounting of the coated chip to a fluidic interface; and in the case of DNA sequencing, (3) loading DNA-loaded bead or beads into the wells. It will be understood, of course, that in other applications, beads may be unnecessary or beads having different characteristics may be employed.
Microwell Array Fabrication
Microwell fabrication may be accomplished in a number of ways. The actual details of fabrication may require some experimentation and vary with the processing capabilities that are available.
In general, fabrication of a high density array of microwells involves photo-lithographically patterning the well array configuration on a layer or layers of material such as photoresist (organic or inorganic), a dielectric, using an etching process. The patterning may be done with the material on the sensor array or it may be done separately and then transferred onto the sensor array chip, of some combination of the two. However, techniques other than photolithography are not to be excluded if they provide acceptable results.
One example of a method for forming a microwell array is now discussed, starting with reference to
After the semiconductor structures, as shown, are formed, the microwell structure is applied to the die. That is, the microwell structure can be formed right on the die or it may be formed separately and then mounted onto the die, either approach being acceptable. To form the microwell structure on the die, various processes may be used. For example, the entire die may be spin-coated with, for example, a negative photoresist such as Microchem's SU-8 2015 or a positive resist/polyimide such as HD Microsystems HD8820, to the desired height of the microwells. The desired height of the wells (e.g., about 4-12 μm in the example of one pixel per well, though not so limited as a general matter) in the photoresist layer(s) can be achieved by spinning the appropriate resist at predetermined rates (which can be found by reference to the literature and manufacturer specifications, or empirically), in one or more layers. (Well height typically may be selected in correspondence with the lateral dimension of the sensor pixel, preferably for a nominal 1:1-1.5:1 aspect ratio, height:width or diameter. Based on signal-to-noise considerations, there is a relationship between dimensions and the required data sampling rates to achieve a desired level of performance. Thus there are a number of factors that will go into selecting optimum parameters for a given application.) Alternatively, multiple layers of different photoresists may be applied or another form of dielectric material may be deposited. Various types of chemical vapor deposition may also be used to build up a layer of materials suitable for microwell formation therein.
Once the photoresist layer (the singular form “layer” is used to encompass multiple layers in the aggregate, as well) is in place, the individual wells (typically mapped to have either one or four ISFET sensors per well) may be generated by placing a mask (e.g., of chromium) over the resist-coated die and exposing the resist to cross-linking (typically UV) radiation. All resist exposed to the radiation (i.e., where the mask does not block the radiation) becomes cross-linked and as a result will form a permanent plastic layer bonded to the surface of the chip (die). Unreacted resist (i.e., resist in areas which are not exposed, due to the mask blocking the light from reaching the resist and preventing cross-linking) is removed by washing the chip in a suitable solvent (i.e., developer) such as propyleneglycolmethylethylacetate (PGMEA) or other appropriate solvent. The resultant structure defines the walls of the microwell array.
After exposure of the die/resist to the UV radiation, a second layer of resist may be coated on the surface of the chip. This layer of resist may be relatively thick, such as about 400-450 μm thick, typically. A second mask 3210 (
Other photolithographic approaches may be used for formation of the microwell array, of course, the foregoing being only one example.
For example, contact lithography of various resolutions and with various etchants and developers may be employed. Both organic and inorganic materials may be used for the layer(s) in which the microwells are formed. The layer(s) may be etched on a chip having a dielectric layer over the pixel structures in the sensor array, such as a passivation layer, or the layer(s) may be formed separately and then applied over the sensor array. The specific choice or processes will depend on factors such as array size, well size, the fabrication facility that is available, acceptable costs, and the like.
Among the various organic materials which may be used in some embodiments to form the microwell layer(s) are the above-mentioned SU-8 type of negative-acting photoresist, a conventional positive-acting photoresist and a positive-acting photodefineable polyimide. Each has its virtues and its drawbacks, well known to those familiar with the photolithographic art.
Naturally, in a production environment, modifications will be appropriate.
Contact lithography has its limitations and it may not be the production method of choice to produce the highest densities of wells—i.e., it may impose a higher than desired minimum pitch limit in the lateral directions. Other techniques, such as a deep UV step-and-repeat process, are capable of providing higher resolution lithography and can be used to produce small pitches and possibly smaller well diameters. Of course, for different desired specifications (e.g., numbers of sensors and wells per chip), different techniques may prove optimal. And pragmatic factors, such as the fabrication processes available to a manufacturer, may motivate the use of a specific fabrication method. While novel methods are discussed, various aspects of the invention are limited to use of these novel methods.
Preferably the CMOS wafer with the ISFET array will be planarized after the final metallization process. A chemical mechanical dielectric planarization prior to the silicon nitride passivation is suitable. This will allow subsequent lithographic steps to be done on very flat surfaces which are free of back-end CMOS topography.
By utilizing deep-UV step-and-repeat lithography systems, it is possible to resolve small features with superior resolution, registration, and repeatability. However, the high resolution and large numerical aperture (NA) of these systems precludes their having a large depth of focus. As such, it may be necessary, when using such a fabrication system, to use thinner photodefinable spin-on layers (i.e., resists on the order of 1-2 μm rather than the thicker layers used in contact lithography) to pattern transfer and then etch microwell features to underlying layer or layers. For example, four 1 μm plasma-enhanced chemical vapor thin-film depositions (standard fab process) may be done sequentially to render a target microwell thickness of 4 μm. High resolution lithography can then be used to pattern the microwell features and conventional SiO2 etch chemistries can be used—one each for the bondpad areas and then the microwell areas—having selective etch stops; the etch stops then can be on aluminum bondpads and silicon nitride passivation (or the like), respectively. Alternatively, other suitable substitute pattern transfer and etch processes can be employed to render microwells of inorganic materials.
Another approach is to form the microwell structure in an organic material. For example, a dual-resist “soft-mask” process may be employed, whereby a thin high-resolution deep-UV resist is used on top of a thicker organic material (e.g., cured polyimide or opposite-acting resist). The top resist layer is patterned. The pattern can be transferred using an oxygen plasma reactive ion etch process. This process sequence is sometimes referred to as the “portable conformable mask” (PCM) technique. See B. J. Lin et al., “Practicing the Novolac deep-UV portable conformable masking technique”, Journal of Vacuum Science and Technology 19, No. 4, 1313-1319 (1981); and A. Cooper et al, “Optimization of a photosensitive spin-on dielectric process for copper inductor coil and interconnect protection in RF SoC devices.”
Alternatively a “drill-focusing” technique may be employed, whereby several sequential step-and-repeat exposures are done at different focal depths to compensate for the limited depth of focus (DOF) of high-resolution steppers when patterning thick resist layers. This technique depends on the stepper NA and DOF as well as the contrast properties of the resist material.
Another PCM technique may be adapted to these purposes, such as that shown in U.S. patent application publication no. 2006/0073422 by Edwards et al. This is a three-layer PCM process and it is illustrated in
In a first step, 3320, a layer of high contrast negative-acting photoresist such as type Shipley InterVia Photodielectric Material 8021 (IV8021) 3322 is spun on the surface of a wafer, which we shall assume to be the wafer providing the substrate 3312 of
Although as shown above, the wells bottom out (i.e. terminate) on the top passivation layer of the ISFETs, it is believed that an improvement in ISFET sensor performance (i.e. such as signal-to-noise ratio) can be obtained if the active bead(s) is(are) kept slightly elevated from the ISFET passivation layer. One way to do so is to place a spacer “bump” within the boundary of the pixel microwell. An example of how this could be rendered would be not etching away a portion of the layer-or-layers used to form the microwell structure (i.e. two lithographic steps to form the microwells—one to etch part way done, the other to pattern the bump and finish the etch to bottom out), by depositing and lithographically defining and etching a separate layer to form the “bump”, or by using a permanent photo-definable material for the bump once the microwells are complete. The bump feature is shown as 3350 in
Mounting the Coated Chip to a Flow Cell (Fluidic Interface)
The process of using the assembly of an array of sensors on a chip combined with an array of microwells to sequence the DNA in a sample is referred to as an “experiment.” Executing an experiment requires loading the wells with the DNA-bound beads and the flowing of several different solutions (i.e., reagents and washes) across the wells. A fluid delivery system coupled with a fluidic interface is needed which flows the various solutions across the wells in a controlled laminar flow with acceptably small dead volumes and small cross contamination between sequential solutions. The fluidic interface is sometimes referred to as a “flow cell.”
Flow cell designs of many configurations are possible; the system and methods presented herein are not dependent on use of a specific flow cell configuration. It is desirable, though, that a suitable flow cell substantially conform to the following set of objectives:
suitable interconnections with a fluidics delivery system—e.g., via appropriately-sized tubing;
appropriate (for dna sequencing, approximately 300 μm) head space above wells;
minimization of dead volumes encountered by fluids prior to their entry to the flow chamber (i.e., the enclosed space above the microwell array).
elimination of small spaces in contact with liquid but not swept by through the flow cell (to minimize cross contamination).
uniform expansion of flow from the inlet tubing to a broad/flat front at the entry to the flow chamber.
laminar flow characteristics such that the broad/flat front profile is maintained as it traverses across the chip from inlet side to outlet side.
adaptable to placement of a removable reference electrode inside or as close to the flow chamber as possible.
easy loading of beads.
manufacturable at acceptable cost
easy assembly of flow cell and attachment to the chip package.
Each of several example designs will be discussed, meeting these criteria. In each instance, one typically may choose to implement the design in one of two ways: either by attaching the flow cell to a frame and gluing the frame (or otherwise attaching it) to the chip or by integrating the frame into the flow cell structure and attaching this unified assembly to the chip. Further, designs may be categorized by the way the reference electrode is integrated into the arrangement. Depending on the design, the reference electrode may be integrated into the flow cell (e.g., form part of the ceiling of the flow chamber) or be in the flow path (typically to the outlet or downstream side of the flow path, after the sensor array).
A first example of a suitable experiment apparatus 3410 incorporating such a fluidic interface is shown in
The apparatus comprises a semiconductor chip 3412 (indicated generally, though hidden) on or in which the arrays of wells and sensors are formed, and a fluidics assembly 3414 on top of the chip and delivering the sample to the chip for reading. The fluidics assembly includes a portion 3416 for introducing fluid containing the sample, a portion 3418 for allowing the fluid to be piped out, and a flow chamber portion 3420 for allowing the fluid to flow from inlet to outlet and along the way interact with the material in the wells. Those three portions are unified by an interface comprising a glass slide 3422 (e.g., Erie Microarray Cat #C22-5128-M20 from Erie Scientific Company, Portsmouth, N.H., cut in thirds of size about 25 mm×25 mm).
Mounted on the top face of the glass slide are two fittings, 3424 and 3426, such as nanoport fittings Part# N-333 from Upchurch Scientific of Oak Harbor, Wash. One port (e.g., 3424) serves as an inlet delivering liquids from the pumping/valving system described below but not shown here. The second port (e.g., 3426) is the outlet which pipes the liquids to waste. Each port connects to a conduit 3428, 3432 such as flexible tubing of appropriate inner diameter. The nanoports are mounted such that the tubing can penetrate corresponding holes in the glass slide. The tube apertures should be flush with the bottom surface of the slide.
On the bottom of the glass slide, flow chamber 3420 may comprise various structures for promoting a substantially laminar flow across the microwell array. For example, a series of microfluidic channels fanning out from the inlet pipe to the edge of the flow chamber may be patterned by contact lithography using positive photoresists such as SU-8 photoresist from MicroChem. Corp. of Newton, Mass. Other structures will be discussed below.
The chip 3412 will in turn be mounted to a carrier 3430, for packaging and connection to connector pins 3432.
For ease of description, to discuss fabrication starting with
A layer of photoresist 3810 is applied to the “top” of the slide (which will become the “bottom” side when the slide and its additional layers is turned over and mounted to the sensor assembly of ISFET array with microwell array on it). Layer 3810 may be about 150 μm thick in this example, and it will form the primary fluid carrying layer from the end of the tubing in the nanoports to the edge of the sensor array chip. Layer 3810 is patterned using a mask such as the mask 3910 of
A second layer of photoresist is formed quite separately, not on the resist 3810 or slide 3422. Preferably it is formed on a flat, flexible surface (not shown), to create a peel-off, patterned plastic layer. This second layer of photoresist may be formed using a mask such as mask 4010, which will leave on the flexible substrate, after patterning, the border under region 4012, two slits under regions 4014, 4016, whose use will be discussed below, and alignment marks produced by patterned regions 4018 and 4022. The second layer of photoresist is then applied to the first layer of photoresist using one alignment mark or set of alignment marks, let's say produced by pattern 4018, for alignment of these layers. Then the second layer is peeled from its flexible substrate and the latter is removed.
The other alignment mark or set of marks produced by pattern 4022 is used for alignment with a subsequent layer to be discussed.
The second layer is preferably about 150 μm deep and it will cover the fluid-carrying channel with the exception of a slit about 150 μm long at each respective edge of the sensor array chip, under slit-forming regions 4014 and 4016.
Once the second layer of photoresist is disposed on the first layer, a third patterned layer of photoresist is formed over the second layer, using a mask such as mask 4110, shown in
The fluidics assembly may be secured to the sensor array chip assembly by applying an adhesive to parts of mating surfaces of those two assemblies, and pressing them together, in alignment.
Though not illustrated in
Another way to introduce the reference electrode is shown in
In the illustrated embodiment, the reference electrode is introduced to the top of the flow chamber via a bore 4325 in the member 4320. The placement of the removable reference electrode is facilitated by a silicone sleeve 4360 and an epoxy stop ring 4370 (see the blow-up of
Yet another alternative for a fluidics assembly, as shown in
Some of the foregoing alternative embodiments also may be implemented in a hybrid plastic/PDMS configuration. For example, as shown in
The fluidic structure may also be made from glass as discussed above, such as photo-definable (PD) glass. Such a glass may have an enhanced etch rate in hydrofluoric acid once selectively exposed to UV light and features may thereby be micromachined on the top-side and back-side, which when glued together can form a three-dimensional low aspect ratio fluidic cell.
An example is shown in
Nanoports may be secured over the nanoport fluidic holes to facilitate connection of input and output tubing.
A central bore 5550 may be etched through the glass layers for receiving a reference electrode, 5560. The electrode may be secured and sealed in place with a silicone collar 5570 or like structure; or the electrode may be equipped integrally with a suitable washer for effecting the same purpose.
By using glass materials for the two-layer fluidic cell, the reference electrode may also be a conductive layer or pattern deposited on the bottom surface of the second glass layer (not shown). Or, as shown in
Still another example embodiment for a fluidic assembly is shown in
Still further examples of flow cell structures are shown in
Whether glass or plastic or other material is used to form the flow cell, it may be desirable, especially with larger arrays, to include in the inlet chamber of the flow cell, between the inlet conduit and the front edge of the array, not just a gradually expanding (fanning out) space, but also some structure to facilitate the flow across the array being suitably laminar. Using the bottom layer 5990 of an injection molded flow cell as an example, one example type of structure for this purpose, shown in
There are various other ways of providing a fluidics assembly for delivering an appropriate fluid flow across the microwell and sensor array assembly, and the forgoing examples are thus not intended to be exhaustive.
Reference Electrode
Commercial flow-type fluidic electrodes, such as silver chloride proton-permeable electrodes, may be inserted in series in a fluidic line and are generally designed to provide a stable electrical potential along the fluidic line for various electrochemical purposes. In the above-discussed system, however, such a potential must be maintained at the fluidic volume in contact with the microwell ISFET chip. With conventional silver chloride electrodes, it has been found difficult, due to an electrically long fluidic path between the chip surface and the electrode (through small channels in the flow cell), to achieve a stable potential. This led to reception of noise in the chip's electronics. Additionally, the large volume within the flow cavity of the electrode tended to trap and accumulate gas bubbles that degraded the electrical connection to the fluid. With reference to
Fluidics System
A complete system for using the sensor array will include suitable fluid sources, valving and a controller for operating the valving to low reagents and washes over the microarray or sensor array, depending on the application. These elements are readily assembled from off-the-shelf components, with and the controller may readily be programmed to perform a desired experiment.
As already discussed, the apparatus and systems of the invention can be used to detect and/or monitor interactions between various entities. These interactions include chemical or enzymatic reactions in which substrates and/or reagents are consumed and/or reaction byproducts are generated. An example of an enzymatic reaction that can be monitored according to the invention is nucleic acid sequencing, which will be discussed in greater detail herein. In the context of a sequencing reaction, the apparatus and system provided herein is able to detect nucleotide incorporation based on changes in the chemFET current. Current changes may be the result of one or more of the following events either singly or some combination thereof: generation of PPi, generation of Pi (e.g., in the presence of pyrophosphatase), generation of hydrogen (and concomitant changes in pH for example in the presence of low strength buffer), reduced concentration of unincorporated dNTP at the chemFET surface, delayed arrival of dNTP at the chemFET surface, and the like. It is to be understood that the methods provided herein are not dependent upon the mechanism by which the current change is effected. And accordingly, the invention contemplates sequencing of nucleic acids based on changes in the chemFET current. The methods provided herein in regards to sequencing can be contrasted to those in the literature including Pourmand et al. PNAS 2006 103(17):6466-6470.
Thus, in one aspect, the invention contemplates sequencing nucleic acids using a chemFET array such as an ISFET array. The method of the invention is a “sequencing by synthesis” method since it requires synthesis of a new nucleic acid strand that is complementary to the strand being sequenced.
The release of PPi following incorporation of a nucleotide in a newly synthesized nucleic acid strand is shown in
The sequencing reactions aim to maximize complete incorporation across all wells for any given dNTP, reduce or decrease the number of unincorporated dNTPs that remain in the wells, and achieve as a high a signal to noise ratio as possible.
The nucleic acid being sequenced is referred to herein as the target nucleic acid. Target nucleic acids include but are not limited to DNA such as but not limited to genomic DNA, mitochondrial DNA, cDNA and the like, and RNA such as but not limited to mRNA, miRNA, and the like. The nucleic acid may be from any source including naturally occurring sources or synthetic sources. The nucleic acids may be PCR products, cosmids, plasmids, naturally occurring or synthetic libraries, and the like. The invention is not intended to be limited in this regard. The methods provided herein can be used to sequence nucleic acids of any length. To be clear, the Examples provide a proof of principle demonstration of the sequencing of four templates of known sequence. This artificial model is intended to show that the apparatus and system are able to readout nucleotide incorporation that correlates to the known sequence of the templates. This is not intended to represent typical use of the method or system in the field. The following is a brief description of these methods.
Target nucleic acids are prepared using any manner known in the art. As an example, genomic DNA may be harvested from a sample according to techniques known in the art (see for example Sambrook et al. “Maniatis”). Following harvest, the DNA may be fragmented to yield nucleic acids of smaller length. The resulting fragments may be on the order of hundreds, thousands, or tens of thousands nucleotides in length. In some embodiments, the fragments are 200-1000 base pairs in size, or 300-800 base pairs in size, although they are not so limited. Nucleic acids may be fragmented by any means including but not limited to mechanical, enzymatic or chemical means. Examples include shearing, sonication, nebulization and endonuclease (e.g., DNase I) digestion, or any other technique known in the art to produce nucleic acid fragments, preferably of a desired length. Fragmentation can be followed by size selection techniques can be used enrich or isolate fragments of a particular length or size. Such techniques are also known in the art and include but are not limited to gel electrophoresis or SPRI.
In some embodiments, the size selected target nucleic acids are ligated to adaptor sequences on both the 5′ and 3′ ends. These adaptor sequences comprise amplification primer sequences to be used in amplifying the target nucleic acids. One adaptor sequence may also comprise a sequence complementary to the sequencing primer. The opposite adaptor sequence may comprise a moiety that facilitates binding of the nucleic acid to a solid support such as but not limited to a bead. An example of such a moiety is a biotin molecule (or a double biotin moiety, as described by Diehl et al. Nature Methods, 2006, 3(7):551-559) and such a labeled nucleic acid can therefore be bound to a solid support having avidin or streptavidin groups. The resulting nucleic acid is referred to herein as a template nucleic acid. The template nucleic acid comprises at least the target nucleic acid and usually comprises nucleotide sequences in addition to the target.
In some instances a spacer is used to distance the template nucleic acid (and in particular the target nucleic acid sequence comprised therein) from the bead. This facilitates sequencing of the end of the target closest to the bead. Examples of suitable linkers are known in the art (see Diehl et al. Nature Methods, 2006, 3(7):551-559) and include but are not limited to carbon-carbon linkers such as but not limited to iSp18.
The solid support to which the template nucleic acids are bound is referred to herein as the “capture solid support”. If the solid support is a bead, then such bead is referred to herein as a “capture bead”. The beads can be made of any material including but not limited to cellulose, cellulose derivatives, gelatin, acrylic resins, glass, silica gels, polyvinyl pyrrolidine (PVP), co-polymers of vinyl and acrylamide, polystyrene, polystyrene cross-linked with divinylbenzene or the like (see, Merrifield Biochemistry 1964, 3, 1385-1390), polyacrylamides, latex gels, dextran, crosslinked dextrans (e.g., Sephadex™), rubber, silicon, plastics, nitrocellulose, natural sponges, metal, and agarose gel (Sepharose™). In one embodiment, the beads are streptavidin-coated beads. The bead diameter will depend on the density of the ISFET and well array used with larger arrays (and thus smaller sized wells) requiring smaller beads. Generally the bead size may be about 1-10 μM, and more preferably 2-6 μM. In some embodiments, the beads are about 5.91 μM while in other embodiments the beads are about 2.8 μM. It is to be understood that the beads may or may not be perfectly spherical in shape. It is to be understood that other beads may be used and other mechanisms for attaching the nucleic acid to the beads may be utilized.
As discussed herein, the sequencing reactions are carried out in wells that are situated above the chemFETs. The wells (referred to herein interchangeably as reaction chambers or microwells) may vary in size between arrays. Preferably the width to height ratio of the well is 1:1 to 1:1.5. The bead to well size is preferably in the range of 0.6-0.8.
A homogeneous population of amplified nucleic acids are conjugated to one or more beads with the proviso that each bead will ultimately be bound to a plurality of identical nucleic acid sequences. The degree of loading of nucleic acid templates onto beads will depend on a number of factors including the bead size and the length of the nucleic acid. In most aspects, maximal loading of the beads is desired. Amplification and conjugation of nucleic acids to solid support such as beads may be accomplished in a number of ways, including but not limited to emulsion PCR as described by Margulies et al. Nature 2005 437(15):376-380 and accompanying supplemental materials. In some embodiments, the amplification is a representative amplification. A representative amplification is an amplification that does not alter the relative representation of any nucleic acid species.
Before and/or while in the wells of the flow chamber, the beads are incubated with a sequencing primer that binds to its complementary sequence located on the 3′ end of the template nucleic acid (i.e., either in the amplification primer sequence or in another adaptor sequence ligated to the 3′ end of the target nucleic acid) and with a polymerase for a time and under conditions that promote hybridization of the primer to its complementary sequence and that promote binding of the polymerase to the template nucleic acid. The primer can be of virtually any sequence provided it is long enough to be unique. The hybridization conditions are such that the primer will hybridize to only its true complement on the 3′ end of the template. Suitable conditions are disclosed in Margulies et al. Nature 2005 437(15):376-380 and accompanying supplemental materials.
Suitable polymerases include but are not limited to DNA polymerase, RNA polymerase, or a subunit thereof, provided it is capable of synthesizing a new nucleic acid strand based on the template and starting from the hybridized primer. An example of a suitable polymerase subunit is the exo-version of the Klenow fragment of E. coli DNA polymerase I which lacks 3′ to 5′ exonuclease activity. The enzyme is therefore bound to the bead (or corresponding solid support) but not to the ISFET surface itself. The template nucleic acid is also contacted with other reagents and/or cofactors including but not limited to buffer, detergent, reducing agents such as dithiothrietol (DTT, Cleland's reagent), single stranded binding proteins, and the like before and/or while in the well. In one embodiment, the template nucleic acid is contacted with the primer and the polymerase prior to its introduction into the flow chamber and wells thereof.
The nucleic acid loaded beads are introduced into the flow chamber and ultimately the wells situated above the ISFET array. The method requires that each well in the flow chamber contain only one nucleic acid loaded bead since the presence of two beads per well will yield one unusable sequencing information derived from two different nucleic acids. The Examples provides a brief description of an exemplary bead loading protocol in the context of magnetic beads. It is to be understood that a similar approach could be used to load other bead types. The protocol has been demonstrated to reduce the likelihood and incidence of trapped air in the wells of the flow chamber, uniformly distribute nucleic acid loaded beads in the totality of wells of the flow chamber, and avoid the presence and/or accumulation of excess beads in the flow chamber.
The percentage of occupied wells on the chip may vary depending on the methods being performed. If the method is aimed at extracting maximum sequence data in the shortest time possible, then higher occupancy is desirable. If speed and throughout is not as critical, then lower occupancy may be tolerated. Therefore depending on the embodiment, suitable occupancy percentages may be at least 10%, at least 20%, at least 30%, at least 40%, at least 50%, at least 60%, at least 70%, at least 80%, at least 90%, or 100% of the wells. As used herein, occupancy refers to the presence of one nucleic acid loaded bead in a well and the percentage occupancy refers to the proportion of total wells on a chip that are occupied by a single bead. Wells that are occupied by more than one bead cannot be used in the analyses contemplated by the invention.
Ultimately a homogeneous population of template nucleic acids is placed into one or more of a plurality of wells, each well situated over and thus corresponding to at least one ISFET. As discussed above, preferably the well contains at least 10, at least 100, at least 1000, at least 104, at least 105, at least 106, or more copies of an identical template nucleic acid. Identical template nucleic acids means at a minimum that the templates are identical in sequence. Most and preferably all the template nucleic acids within a well are uniformly hybridized to a primer. Uniform hybridization of the template nucleic acids to the primers means that the primer hybridizes to the template at the same location (i.e., the sequence along the template that is complementary to the primer) as every other primer-template hybrid in the well. The uniform positioning of the primer on every template allows the co-ordinated synthesis of all new nucleic acid strands within a well, thereby resulting in a greater signal-to-noise ratio.
Nucleotides are then added in flow, or by any other suitable method, in sequential order to the flow chamber and thus the wells. The nucleotides can be added in any order provided it is known and for the sake of simplicity kept constant throughout a run. If the incorporation of nucleotides is based on detection of PPi rather than detection of pH change as a result of PPi release, then it is preferable to maintain a relatively constant level and concentration of nucleotides throughout the reactions and washes. One way of accomplishing this is to add ATP to the wash buffer such that dNTPs flowing into a well are displacing ATP from the well. The ATP matches the ionic strength of the dNTPs entering the wells and it also has a similar diffusion profile as those dNTPs. In this way, influx and efflux of dNTPs during the sequencing reaction do not interfere with measurements at the chemFET. The concentration of ATP used is on the order of the concentration of dNTP used.
A typical sequencing cycle proceeds as follows: washing of the flow chamber (and wells) with wash buffer containing ATP, introduction of a first dNTP species (e.g., dATP) into the flow chamber (and wells), release and detection of PPi (by any of the mechanisms described herein), washing of the flow chamber (and wells) with wash buffer containing ATP, washing of the flow chamber (and wells) with wash buffer containing apyrase, washing of the flow chamber (and wells) with wash buffer containing ATP, and introduction of a second dNTP species. This process is continued until all 4 dNTP (i.e., dATP, dCTP, dGTP and dTTP) have been flowed through the chamber and allowed to incorporate into the newly synthesized strands. This 4-nucleotide cycle may be repeated any number of times including but not limited to 10, 25, 50, 100, 200 or more times. The number of cycles will be governed by the length of the template being sequenced and the need to replenish reaction reagents, in particular the dNTP stocks and wash buffers.
As part of the sequencing reaction, a dNTP will be ligated to (or “incorporated into” as used herein) the 3′ of the newly synthesized strand (or the 3′ end of the sequencing primer in the case of the first incorporated dNTP) if its complementary nucleotide is present at that same location on the template nucleic acid. Incorporation of the introduced dNTP (and concomitant release of PPi) therefore indicates the identity of the corresponding nucleotide in the template nucleic acid. If no change in the electric field is detected by the ISFET, then the dNTP has not been incorporated and one can conclude that the complementary nucleotide was not present in the template at that location. If a change in the electric field is detected, then the introduced dNTP has been incorporated into the newly synthesized strand. There is a positive correlation between dNTP incorporation and PPi release and the response of the ISFET, and as a result it is further possible to quantitate the number of dNTP incorporated. In other words, the voltage change registered at the ISFET is related to the number of dNTP incorporated. The result is that no sequence information is lost through the sequencing of a homopolymer stretch (e.g., poly A, poly T, poly C, or poly G) in the template. As an example, if the template nucleic acid includes a sequence of 5′ CAAAAG 3′, the ISFET will register a signal (e.g., in terms of millivolt change) upon introduction of dCTP, and then it will register a signal of greater magnitude upon the introduction of dTTP, followed by another signal upon the introduction of dGTP. The magnitude of the signals arising upon introduction of dCTP and dTTP will be essentially equivalent and will correlate with the millivoltage change resulting from a single nucleotide incorporation. The magnitude of the signal arising upon introduction of dTTP will be greater than the signals arising from single dNTP incorporation. The magnitude of these signals may be additive, and depending on the length of the homopolymer stretch may not be readily apparent in a voltage versus time (or frame) plot (such as those shown in
Apyrase is an enzyme that degrades residual unincorporated nucleotides converting them into monophosphate and releasing inorganic phosphate in the process. It is useful for degrading dNTPs that are not incorporated and/or that are in excess in any and all wells. It is important that excess and/or unreacted dNTP be washed away from any and all wells before introduction of the subsequent dNTP. Accordingly, addition of apyrase during the synthesis reaction and between the introduction of different dNTPs is useful to remove excess dNTPs that would otherwise obscure the sequencing data.
Additional sequencing reaction reagents such as those described above may be introduced throughout the reaction, although in some cases this may not be necessary. For example additional polymerase, DTT, SBB and the like may be added if necessary.
The invention therefore contemplates performing a plurality of different sequencing reactions simultaneously. A plurality of identical sequencing reactions is occurring in each occupied well simultaneously. It is this simultaneous and identical incorporation of dNTP within each well that increases the signal to noise ratio, thereby making detection of the sequencing reaction byproduct possible. By performing sequencing reactions in a plurality of wells simultaneously, a plurality of different sequencing reactions are also performed simultaneously.
The sequencing reaction can be run at a range of temperatures. Typically, the reaction is run in the range of 30-60° C., 35-55° C., or 40-45° C. It is preferable to run the reaction at temperatures that prevent formation of secondary structure in the nucleic acid. However this must be balanced with the binding of the primer (and the newly synthesized strand) to the template nucleic acid and the reduced half-life of apyrase at higher temperatures. A suitable temperature is about 41° C. The solutions including the wash buffers and the dNTP solutions are generally warmed to these temperatures in order not to alter the temperature in the wells. The wash buffer containing apyrase however is preferably maintained at a lower temperature in order to extend the half-life of the enzyme. Typically, this solution is maintained at about 4-15° C., and more preferably 4-10° C.
The nucleotide incorporation reaction can occur very rapidly. As a result, it may be desirable in some instances to slow the reaction down in order to ensure maximal data capture during the reaction. The diffusion of reagents and/or byproducts can be slowed down in a number of ways including but not limited to addition of packing beads in the wells. The packing beads also tend to increase the concentration of reagents and/or byproducts at the chemFET surface, thereby increasing the potential for signal. The presence of packing beads generally allows a greater time to sample (e.g., by 2- or 4-fold).
Data capture rates can vary and be for example anywhere from 10-100 frames per second and the choice of which rate to use will be dictated at least in part by the well size and the presence of packing beads. Smaller well sizes generally require faster data capture rates.
In some aspects of the invention that are flow-based and where the top face of the well is open and in communication with fluid over the entirety of the chip, it is important to detect the released PPi or other byproduct (e.g., H+) prior to diffusion out of the well. Diffusion of either reaction byproduct out of the well will lead to false negatives (because the byproduct is not detected in that well) and potential false positives in adjacent or downstream wells, and thus should be avoided. Packing beads may also help reduce the degree of diffusion and/or cross-talk between wells.
Thus in some embodiments packing beads are used in addition to the nucleic acid-loaded beads. The packing beads may be magnetic (including superparamagnetic) but they are not so limited. In some embodiments the packing beads and the capture beads are made of the same material (e.g., both are magnetic, both are polystyrene, etc.), while in other embodiment they are made of different materials (e.g., the packing beads are polystyrene and the capture beads are magnetic). The packing beads are generally smaller than the capture beads. The difference in size may be vary and may be 5-fold, 10-fold, 15-fold, 20-fold or more. As an example, 0.35 μm diameter packing beads have been used with 5.91 μm capture beads. Such packing beads are commercially available from sources such as Bang Labs. The placement of the packing beads relative to the capture bead may vary. For example, the packing beads may surround the capture bead and thereby prevent the capture bead from contacting the ISFET surface. As another example, the packing beads may be loaded into the wells following the capture beads in which case the capture bead is in contact with the ISFET surface. The presence of packing beads between the capture bead and the ISFET surface slows the diffusion of the sequencing byproducts such as PPi, thereby facilitating data capture.
The invention further contemplates the use of packing beads or modifications to the chemFET surface (as described herein) to prevent contact and thus interference of the chemFET surface with the template nucleic acids bound to the capture beads. A layer of packing beads that is 0.1-0.5 μm in depth or height would preclude this interaction.
The sequencing reaction may be preceded by an analysis of the arrays to determine the location of beads. It has been found that in the absence of flow the background signal (i.e., noise) is less than or equal to about 0.25 mV, but that in the presence of DNA-loaded capture beads that signal increases to about 1.0 mV +/−0.5 mV. This increase is sufficient to allow one to determine wells with beads.
The invention further contemplates kits comprising the various reagents necessary to perform a sequencing reaction and instructions of use according to the methods set forth herein.
One preferred kit comprises one or more containers housing wash buffer, one or more containers each containing one of the following reagents: dATP buffer, dCTP buffer, dGTP buffer or dTTP buffer, dATP, dCTP, dGTP and dTTP stocks, apyrase, SSB, polymerase, packing beads and optionally pyrophosphatase. Importantly the kits comprise only naturally occurring dNTPs.
The kits may also comprise one or more wash buffers comprising components as described in the Examples, but also not so limited. The kits may also comprise instructions for use including diagrams that demonstrate the methods of the invention.
It is to be understood that interactions between receptors and ligands or between two members of a binding pair or between components of a molecular complex can also be detected using the chemFET arrays. Examples of such interactions include hybridization of nucleic acids to each other, protein-nucleic acid binding, protein-protein binding, enzyme substrate binding, enzyme-inhibitor binding, antigen-antibody binding, and the like. Any binding or hybridization event that causes a change of the semiconductor charge density at the FET interface and thus changes the current that flows from the source to the drain of the sensors described herein can be detected according to the invention.
In these embodiments, the passivation layer (or possibly an intermediate layer coated onto the passivation layer) is functionalized with nucleic acids (e.g., DNA, RNA, miRNA, cDNA, and the like), antigens (which can be of any nature), proteins (e.g., enzymes, cofactors, antibodies, antibody fragments, and the like), and the like. Conjugation of these entities to the passivation layer can be direct or indirect (e.g., using bifunctional linkers that bind to both the passivation layer reactive group and the entity to be bound).
As an example, reaction groups such as amine or thiol groups may be added to a nucleic acid at any nucleotide during synthesis to provide a point of attachment for a bifunctional linker. As another example, the nucleic acid may be synthesized by incorporating conjugation-competent reagents such as Uni-Link AminoModifier, 3′-DMT-C6-Amine-ON CPG, AminoModifier II, N-TFA-C6-AminoModifier, C6-ThiolModifier, C6-Disulfide Phosphoramidite and C6-Disulfide CPG (Clontech, Palo Alto, Calif.). Other methods for attaching nucleic acids are discussed below.
In one aspect of the invention, the chemFET arrays are provided in combination with nucleic acid arrays. Nucleic acids in the form of short nucleic acids (e.g., oligonucleotides) or longer nucleic acids (e.g., full length cDNAs) can be provided on chemFET surfaces of the arrays described herein. Nucleic acid arrays generally comprise a plurality of physically defined regions on a planar surface (e.g., “spots”) each of which has conjugated to it one and more preferably more nucleic acids. The nucleic acids are usually single stranded. The nucleic acids conjugated to a given spot are usually identical. In the context of an oligonucleotide array, these nucleic acids may be on the order of less 100 nucleotides in length (including about 10, 20, 25, 30, 40, 50, 60, 70, 80, 90 or 100 nucleotides in length). If the arrays are used to detect certain genes (including mutations in such genes or expression levels of such genes), then the array may include a number of spots each of which contains oligonucleotides that span a defined and potentially different sequence of the gene. These spots are then located across the planar surface in order to exclude position related effects in the hybridization and readout means of the array.
The arrays are contacted with a sample being tested. The sample may be a genomic DNA sample, a cDNA sample from a cell, a tissue or a mass (e.g., a tumor), a population of cells that are grown on the array, potentially in a two dimensional array that corresponds to the underlying sensor array, and the like. Such arrays are therefore useful for determining presence and/or level of a particular gene or of its expression, detecting mutations within particular genes (such as but not limited to deletions, additions, substitutions, including single nucleotide polymorphisms), and the like.
The binding or hybridization of the sample nucleic acids and the immobilized nucleic acids is generally performed under stringent hybridization conditions as that term is understood in the art. (See for example Sambrook et al. “Maniatis”.) Examples of relevant conditions include (in order of increasing stringency): incubation temperatures of 25° C., 37° C., 50° C. and 68° C.; buffer concentrations of 10×SSC, 6×SSC, 4×SSC, 1×SSC, 0.1×SSC (where SSC is 0.15 M NaCl and 15 mM citrate buffer) and their equivalents using other buffer systems; formamide concentrations of 0%, 25%, 50%, and 75%; incubation times from 5 minutes to 24 hours; 1, 2, or more washing steps; wash incubation times of 1, 2, or 15 minutes; and wash solutions of 6×SSC, 1×SSC, 0.1×SSC, or deionized water. By way of example hybridization may be performed at 50% formamide and 4×SSC followed by washes of 2×SSC/formamide at 50° C. and with 1×SSC.
Nucleic acid arrays include those in which already formed nucleic acids such as cDNAs are deposited (or “spotted”) on the array in a specific location. Nucleic acids can be spotted onto a surface by piezoelectrically deposition, UV crosslinking of nucleic acids to polymer layers such as but not limited to poly-L-lysine or polypyrrole, direct conjugation to silicon coated SiO2 as described in published US patent application 2003/0186262, direct conjugation to a silanised chemFET surface (e.g., a surface treated with 3-aminopropyltriethoxysilane (APTES) as described by Uslu et al. Biosensors and Bioelectronics 2004, 19: 1723-1731, for example.
Nucleic acid arrays also include those in which nucleic acids (such as oligonucleotides of known sequence) are synthesized directly on the array. Nucleic acids can be synthesized on arrays using art-recognized techniques such as but not limited to printing with fine-pointed pins onto glass slides, photolithography using pre-made masks, photolithography using dynamic micromirror devices (such as DLP mirrors), ink-jet printing, or electrochemistry on microelectrode arrays. Reference can also be made to Nuwaysir et al. 2002 “Gene expression analysis using oligonucleotide arrays produced by maskless photolithography.”. Genome Res 12: 1749-1755. Commercial sources of this latter type of array include Agilent, Affymetrix, and NimbleGen.
Thus the chemFET passivation layer may be coated with an intermediate layer of reactive molecules (and therefore reactive groups) to which the nucleic acids are bound and/or from which they are synthesized.
The invention contemplates combining such nucleic acid arrays with the chemFET arrays and particularly the “large scale” chemFET arrays described herein. The chemFET/nucleic acid array can be used in a variety of applications, some of which will not require the wells (or microwells or reaction chambers, as they are interchangeably referred to herein). Since analyses may still be carried out in flow, including in a “closed” system (i.e., where the flow of reagents and wash solutions and the like is automated), there will be one or more flow chambers situated above and in contact with the array. The use of multiple flow chambers allows multiple samples (or nucleic acid libraries) to be analyzed simultaneously. There may be 2, 3, 4, 5, 6, 7, 8, 9, 10 or more flow chambers. This configuration applies equally to other biological arrays including those discussed herein such as protein arrays, antibody arrays, enzyme arrays, chemical arrays, and the like.
Since the binding event between binding partners or between components of a complex is detected electronically via the underlying FET, such assays may be carried out without the need to manipulate (e.g., extrinsically label) the sample being assayed. This is advantageous since such manipulation invariably results in loss of sample and generally requires increased time and work up. In addition, the present method allows binding interactions to be studied in real time.
Protein arrays used in combination with the chemFET arrays of the invention are also contemplated. Protein arrays comprise proteins or peptides or other amino acid comprising biological moiety bound to a planar surface in an organized and predetermined manner. Such proteins include but are not limited to enzymes, antibodies and antibody fragments or antibody mimics (e.g., single chain antibodies).
In one embodiment, a protein array may comprise a plurality of different proteins (or other amino acid containing biological moieties). Each protein, and preferably a plurality of proteins, is present in a predetermined region or “cell” of the array. The regions (or cells) are aligned with the sensors in the sensor array such that there is one sensor for each region (or cell). The plurality of proteins in a single region (or cell) may vary depending on the size of the protein and the size of the region (or cell) and may be but is not limited to at least 10, 50, 100, 500, 103, 104 or more. The array itself may have any number of cells, including but not limited to at least 10, 102, 103, 104, 105, 106, 107, or more. In one application, the array is exposed to a sample that is known to contain or is suspected of containing an analyte that binds to the protein. The analyte may be a substrate or an inhibitor if the protein is an enzyme. The analyte may be any molecule that binds to the protein including another protein, a nucleic acid, a chemical species (whether synthetic or naturally occurring), and the like.
It is to be understood that, like the nucleic acid arrays contemplated herein, the readout from the protein arrays will be a change in current through the chemFET and thus no additional step of labeling and/or label detection is required in these array methods.
In another embodiment, the protein array may comprise a plurality of identical proteins (or other amino acid containing biological moieties). The identical proteins may be uniformly distributed on a planar surface or they may be organized into discrete regions (or cells) on that surface. In these latter embodiments, the regions (or cells) are aligned with the sensors in the sensor array such that there is one sensor for each region (or cell).
The proteins may be synthesised off-chip, then purified and attached to the array. Alternatively they can be synthesised on-chip, similarly to the nucleic acids discussed above. Synthesis of proteins using cell-free DNA expression or chemical synthesis is amenable to on-chip synthesis. Using cell-free DNA expression, proteins are attached to the solid support once synthesized. Alternatively, proteins may be chemically synthesized on the solid support using solid phase peptide synthesis. Selective deprotection is carried out through lithographic methods or by SPOT-synthesis. Reference can be made to at least MacBeath and Schreiber, Science, 2000, 289:1760-1763, or Jones et al. Nature, 2006, 439:168-174. Reference can also be made to U.S. Pat. No. 6,919,211 to Fodor et al.
Chemical compound microarrays in combination with chemFET arrays are also envisioned. Chemical compound microarrays can be made by covalently immobilizing the compounds (e.g., organic compounds) on the solid surface with diverse linking techniques (may be referred to in the literature as “small molecule microarray”), by spotting and drying compounds (e.g., organic compounds) on the solid surface without immobilization (may be referred to in the literature as “micro arrayed compound screening (μARCS)”), or by spotting organic compounds in a homogenous solution without immobilization and drying effect (commercialized as DiscoveryDot™ technology by Reaction Biology Corporation).
Tissue microarrays in combination with chemFET arrays are further contemplated by the invention. Tissue microarrays are discussed in greater detail in Battifora Lab Invest 1986, 55:244-248; Battifora and Mehta Lab Invest 1990, 63:722-724; and Kononen et al. Nat Med 1998, 4:844-847.
The configurations of the chemFET arrays and the biological or chemical arrays are similar in each instance and the discussion of one combination array will apply to others described herein or otherwise known in the art.
In yet another aspect, the invention contemplates analysis of cell cultures (e.g., two-dimensional cells cultures) (see for example Baumann et al. Sensors and Actuators B 55 1999 77:89), and tissue sections placed in contact with the chemFET array. As an example, a brain section may be placed in contact with the chemFET array of the invention and changes in the section may be detected either in the presence or absence of stimulation such as but not limited to neurotoxins and the like. Transduction of neural processes and/or stimulation can thereby be analyzed. In these embodiments, the chemFETs may operate by detecting calcium and/or potassium fluxes via the passivation layer itself or via receptors for these ions that are coated onto the passivation layer.
In yet another aspect, the invention contemplates the use of chemFET arrays, functionalized as described herein or in another manner, for use in vivo. Such an array may be introduced into a subject (e.g., in the brain or other region that is subject to ion flux) and then analyzed for changes based on the status of the subject.
Methods for attaching nucleic acids, proteins, molecules, and the like to solid supports, particularly in the context of an array, have been described in the art. See for example Lipshutz et al. Nature Genetics (supplement) 1999 21:20-24; Li et al. Proc. Natl. Acad. Sci., 2001, 98:31-36; Lockhart et al. Nat. Biotechnol. 1996 14:1675-1680; Wodicka et al. Nat. Biotechnol. 1997 15: 1359-1367; Chen et al. Journal of Biomedical Optics 1997 2:364; Duggan et al. Nat. Genet. 1991 21(1 Suppl):10-4; Marton et al. Nat. Med. 1998 4(11):1293-301; Kononen et al. Nat Med 1998 4(7):844-847; MacBeath et al., Science 2000 289(5485):1760-1763; Haab et al. Genome Biology 2001 2(2); Pollack et al. Nat. Genet. 1999 23(1):41-6; Wang D G et al. Science 1998 280(5366):1077-82; Fodor et al. Science 1991 251:767-773; Fodor et al. Nature 1993 364:555-556; Pease et al. Proc. Natl. Acad. Sci. USA 1994 91:5022-5026; Fodor Science 1997 277:393-395; Southern et al. Genomics 1992 13: 1008-1017; Schena et al. Science 1995 270(5235):467-70; Shalon et al. Genome Res 1996 6(7):639-45; Jongsma Proteomics 2006, 6:2650-2655; Sakata, Biosensors and Bioelectronics 2007, 22: 1311-1316.
The following examples are included for purposes of illustration and are not intended to limit the scope of the invention.
The following is an example of a proof of principle for rapid sequencing of single-stranded oligonucleotides using an ISFET array.
1.1. Binding of Single-Stranded Oligonucleotides to Streptavidin-Coated Magnetic Beads.
Single-stranded DNA oligonucleotide templates with a 5′ Dual Biotin tag (HPLC purified), and a 20-base universal primer were ordered from IDT (Integrated DNA Technologies, Coralville, Ind.). Templates were 60 bases in length, and were designed to include 20 bases at the 3′ end that were complementary to the 20-base primer (Table 1, italics). The lyophilized and biotinylated templates and primer were re-suspended in TE buffer (10 mM Tris-HCl, 1 mM EDTA, pH 8) as 40 μM stock solutions and as a 400 μM stock solution, respectively, and stored at −20° C. until use.
For each template, 60 μl of magnetic 5.91 μm (Bangs Laboratories, Inc. Fishers, Ind.) streptavidin-coated beads, stored as an aqueous, buffered suspension (8.57×104 beads/μL), at 4° C., were prepared by washing with 120 μl bead wash buffer three times and then incubating with templates 1, 2, 3 and 4 (T1, T2, T3, T4: Table 1) with biotin on the 5′ end, respectively.
Due to the strong covalent binding affinity of streptavidin for biotin (Kd ˜10-15), these magnetic beads are used to immobilize the templates on a solid support, as described below. The reported binding capacity of these beads for free biotin is 0.650 pmol/μL of bead stock solution. For a small (<100 bases) biotinylated ssDNA template, it was conservatively calculated that 9.1×105 templates could be bound per bead. The beads are easily concentrated using simple magnets, as with the Dynal Magnetic Particle Concentrator or MPC-s (Invitrogen, Carlsbad, Calif.). The MPC-s was used in the described experiments.
An MPC-s was used to concentrate the beads for 1 minute between each wash, buffer was then added and the beads were resuspended. Following the third wash the beads were resuspended in 120 μL bead wash buffer plus 1 μl of each template (40 μM). Beads were incubated for 30 minutes with rotation (Labquake Tube Rotator, Barnstead, Dubuque, Iowa). Following the incubation, beads were then washed three times in 120 μL Annealing Buffer (20 mM Tris-HCl, 5 mM magnesium acetate, pH 7.5), and re-suspended in 60 μL of the same buffer.
1.2. Annealing of Sequencing Primer.
The immobilized templates, bound at the 5′ end to 5.91 μm magnetic beads, are then annealed to a 20-base primer complementary to the 3′ end of the templates (Table 1). A 1.0 μL aliquot of the 400 μM primer stock solution, representing a 20-fold excess of primer to immobilized template, is then added and then the beads plus template are incubated with primer for 15 minutes at 95° C. and the temperature was then slowly lowered to room temperature. The beads were then washed 3 times in 120 μL of 25 mM Tricine buffer (25 mM Tricine, 0.4 mg/ml PVP, 0.1% Tween 20, 8.8 mM Magnesium Acetate; ph 7.8) as described above using the MPC-s. Beads were resuspended in 25 mM Tricine buffer.
1.3. Incubation of Hybridized Templates/Primer with DNA Polymerase.
Template and primer hybrids are incubated with polymerase essentially as described by Margulies et al. Nature 2005 437(15):376-380 and accompanying supplemental materials.
2. Loading of Prepared Test Samples onto the ISFET Sensor Array.
The dimensions and density of the ISFET array and the microfluidics positioned thereon may vary depending on the application. A non-limiting example is a 512×512 array. Each grid of such an array (of which there would be 262144) has a single ISFET. Each grid also has a well (or as they may be interchangeably referred to herein as a “microwell”) positioned above it. The well (or microwell) may have any shape including columnar, conical, square, rectangular, and the like. In one exemplary conformation, the wells are square wells having dimensions of 7×7×10 μm. The center-to-center distance between wells is referred to herein as the “pitch”. The pitch may be any distance although it is preferably to have shorter pitches in order to accommodate as large of an array as possible. The pitch may be less than 50 less than 40 less than 30 less than 20 or less than 10 μm. In one embodiment, the pitch is about 9 μm. The entire chamber above the array (within which the wells are situated) may have a volume of equal to or less than about 30 μL, equal to or less than about 20 μL, equal to or less than about 15 μL, or equal to or less than 10 μL. These volumes therefore correspond to the volume of solution within the chamber as well.
2.1 Loading of Beads in an ‘Open’ System.
Beads with templates 1-4 were loaded on the chip (10 μL of each template). Briefly, an aliquot of each template was added onto the chip using an Eppendorf pipette. A magnet was then used to pull the beads into the wells.
2.2 Loading of Beads in a ‘Closed’ System.
Both the capture beads the packing beads are loaded using flow. Microliter precision of bead solution volume, as well as positioning of the bead solution through the fluidics connections, is achieved as shown in
The chip comprising the ISFET array and flow cell is seated in the ZIF (zero insertion force) socket of the loading fixture, then attaching a stainless steel capillary to one port of the flow cell and flexible nylon tubing on the other port. Both materials are microfluidic-type fluid paths (e.g., on the order of <0.01″ inner diameter). The bead loading fitting, consisting of the major and minor reservoirs, it attached to the end of the capillary. A common plastic syringe is filled with buffer solution, then connected to the free end of the nylon tubing. The electrical leads protruding from the bottom of the chip are inserted into a socket on the top of a fixture unit (not shown).
The syringe is pushed to inject the buffer solution through the tubing, across the flow cell (and chip surface) and up through the capillary as shown in
Next, a solution containing the nucleic acid-coated beads is applied with a precision pipette to the minor reservoir, as shown in
At this point, the bead solution is loaded into the fluidic path, but is not yet at the location of flow cell. Before transferring the bead solution plug, or volume of bead solution in the fluidic path, the solution in the minor reservoir is cleaned. First, approximately 1 mL of buffer solution is injected into the major reservoir, effectively diluting the bead solution left in the minor reservoir, as shown in
A volume of buffer solution is then added as droplet above the minor reservoir, as in prior bead solution application as shown in
The loading fixture is now lifted and placed over a pyramidal base, containing a magnet at its apex, as shown in
It will be appreciated that there will be other ways of drawing the beads into the wells of the flow chamber, including centrifugation or gravity. The invention is not limited in this respect.
3. DNA Sequencing using the ISFET Sensor Array.
3.1 DNA Sequencing in an ‘Open’ System.
The results shown are representative of an experiment carried out in an ‘open’ system (i.e., the ISFET chip is placed on the platform of the ISFET apparatus and then each nucleotide (5 μL resulting in 6.5 μM each) was manually added in the following order: dATP, dCTP, dGTP and dTTP (100 mM stock solutions, Pierce, Milwaukee, Wis.), by pipetting the given nucleotide into the liquid already on the surface of the chip and collecting data from the chip at a rate of 2.5 mHz. This resulted in data collection over 7.5 seconds at approximately 18 frames/second. Data were then analyzed using LabView.
Given the sequences of the templates, addition of dATP resulted in a 4 base extension in template 4. Addition of dCTP resulted in a 4 base extension in template 1. Addition of dGTP caused template 1, 2 and 4 to extend as indicated in Table 2 and addition of dTTP results in a run-off (extension of all templates as indicated).
Preferably when the method is performed in a non-automated manner (i.e., in the absence of automated flow and reagent introduction), each well contains apyrase in order to degrade the unincorporated dNTPs, or alternatively apyrase is added into each well following the addition and incorporation of each dNTP (e.g. dATP) and prior to the addition of another dNTP (e.g. dTTP). It is to be understood that apyrase can be substituted, in this embodiment or in any other embodiment discussed herein, with another compound (or enzyme) capable of degrading dNTPs.
3.2 DNA Sequencing Using Microfluidics on Sensor Chip
Sequencing in the flow regime is an extension of open application of nucleotide reagents for incorporation into DNA. Rather than add the reagents into a bulk solution on the ISFET chip, the reagents are flowed in a sequential manner across the chip surface, extending a single DNA base(s) at a time. The dNTPs are flowed sequentially, beginning with dTTP, then dATP, dCTP, and dGTP. Due to the laminar flow nature of the fluid movement over the chip, diffusion of the nucleotide into the microwells and finally around the nucleic acid loaded bead is the main mechanism for delivery. The flow regime also ensures that the vast majority of nucleotide solution is washed away between applications. This involves rinsing the chip with buffer solution and apyrase solution following every nucleotide flow. The nucleotides and wash solutions are stored in chemical bottles in the system, and are flowed over the chip using a system of fluidic tubing and automated valves. The ISFET chip is activated for sensing chemical products of the DNA extension during nucleotide flow.
While several inventive embodiments have been described and illustrated herein, those of ordinary skill in the art will readily envision a variety of other means and/or structures for performing the function and/or obtaining the results and/or one or more of the advantages described herein, and each of such variations and/or modifications is deemed to be within the scope of the inventive embodiments described herein. More generally, those skilled in the art will readily appreciate that all parameters, dimensions, materials, and configurations described herein are meant to be exemplary and that the actual parameters, dimensions, materials, and/or configurations will depend upon the specific application or applications for which the inventive teachings is/are used. Those skilled in the art will recognize, or be able to ascertain using no more than routine experimentation, many equivalents to the specific inventive embodiments described herein. It is, therefore, to be understood that the foregoing embodiments are presented by way of example only and that, within the scope of the appended claims and equivalents thereto, inventive embodiments may be practiced otherwise than as specifically described and claimed. Inventive embodiments of the present disclosure are directed to each individual feature, system, article, material, kit, and/or method described herein. In addition, any combination of two or more such features, systems, articles, materials, kits, and/or methods, if such features, systems, articles, materials, kits, and/or methods are not mutually inconsistent, is included within the inventive scope of the present disclosure.
All definitions, as defined and used herein, should be understood to control over dictionary definitions, definitions in documents incorporated by reference, and/or ordinary meanings of the defined terms.
All references, patents and patent applications disclosed herein are incorporated by reference with respect to the subject matter for which each is cited, which in some cases may encompass the entirety of the document.
The indefinite articles “a” and “an,” as used herein in the specification and in the claims, unless clearly indicated to the contrary, should be understood to mean “at least one.”
The phrase “and/or,” as used herein in the specification and in the claims, should be understood to mean “either or both” of the elements so conjoined, i.e., elements that are conjunctively present in some cases and disjunctively present in other cases. Multiple elements listed with “and/or” should be construed in the same fashion, i.e., “one or more” of the elements so conjoined. Other elements may optionally be present other than the elements specifically identified by the “and/or” clause, whether related or unrelated to those elements specifically identified. Thus, as a non-limiting example, a reference to “A and/or B”, when used in conjunction with open-ended language such as “comprising” can refer, in one embodiment, to A only (optionally including elements other than B); in another embodiment, to B only (optionally including elements other than A); in yet another embodiment, to both A and B (optionally including other elements); etc.
As used herein in the specification and in the claims, “or” should be understood to have the same meaning as “and/or” as defined above. For example, when separating items in a list, “or” or “and/or” shall be interpreted as being inclusive, i.e., the inclusion of at least one, but also including more than one, of a number or list of elements, and, optionally, additional unlisted items. Only terms clearly indicated to the contrary, such as “only one of” or “exactly one of,” or, when used in the claims, “consisting of,” will refer to the inclusion of exactly one element of a number or list of elements. In general, the term “or” as used herein shall only be interpreted as indicating exclusive alternatives (i.e. “one or the other but not both”) when preceded by terms of exclusivity, such as “either,” “one of,” “only one of,” or “exactly one of.” “Consisting essentially of,” when used in the claims, shall have its ordinary meaning as used in the field of patent law.
As used herein in the specification and in the claims, the phrase “at least one,” in reference to a list of one or more elements, should be understood to mean at least one element selected from any one or more of the elements in the list of elements, but not necessarily including at least one of each and every element specifically listed within the list of elements and not excluding any combinations of elements in the list of elements. This definition also allows that elements may optionally be present other than the elements specifically identified within the list of elements to which the phrase “at least one” refers, whether related or unrelated to those elements specifically identified. Thus, as a non-limiting example, “at least one of A and B” (or, equivalently, “at least one of A or B,” or, equivalently “at least one of A and/or B”) can refer, in one embodiment, to at least one, optionally including more than one, A, with no B present (and optionally including elements other than B); in another embodiment, to at least one, optionally including more than one, B, with no A present (and optionally including elements other than A); in yet another embodiment, to at least one, optionally including more than one, A, and at least one, optionally including more than one, B (and optionally including other elements); etc.
It should also be understood that, unless clearly indicated to the contrary, in any methods claimed herein that include more than one step or act, the order of the steps or acts of the method is not necessarily limited to the order in which the steps or acts of the method are recited.
In the claims, as well as in the specification above, all transitional phrases such as “comprising,” “including,” “carrying,” “having,” “containing,” “involving,” “holding,” “composed of,” and the like are to be understood to be open-ended, i.e., to mean including but not limited to. Only the transitional phrases “consisting of” and “consisting essentially of” shall be closed or semi-closed transitional phrases, respectively, as set forth in the United States Patent Office Manual of Patent Examining Procedures, Section 2111.03.
This application is a continuation of U.S. patent application Ser. No. 13/616,454 filed 14 Sep. 2012, which is a continuation of U.S. patent application Ser. No. 13/149,262 filed 31 May 2011, which is a continuation of U.S. patent application Ser. No. 12/002,781 filed 17 Dec. 2007, which is a continuation-in-part of U.S. application Ser. No. 12/002,291, filed 14 Dec. 2007, which claims priority to U.S. Provisional Application No. 60/956,324, filed 16 Aug. 2007, U.S. Provisional Application No. 60/948,748, filed 10 Jul. 2007, and U.S. Provisional Application No. 60/870,073, filed 14 Dec. 2007; the entire contents of each of which are incorporated herein by reference.
Number | Date | Country | |
---|---|---|---|
60956324 | Aug 2007 | US | |
60948748 | Jul 2007 | US | |
60870073 | Dec 2006 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 13616454 | Sep 2012 | US |
Child | 13794637 | US | |
Parent | 13149262 | May 2011 | US |
Child | 13616454 | US | |
Parent | 12002781 | Dec 2007 | US |
Child | 13149262 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 12002291 | Dec 2007 | US |
Child | 12002781 | US |