The present invention relates to stacked microelectronic devices and methods of manufacturing the same.
Stacked die packaging typically comes in any of three forms: pyramid configuration, inverted pyramid configuration and same size die configuration. In a pyramid configuration the top die is smaller than the bottom die. The opposite is true in the inverted pyramid configuration. Alternatively, the dies can be the same size. In all stacked die configurations, an adhesive is typically applied to attach the top and bottom die together. In the case of the inverted pyramid with a larger die on top, the inclusion of a spacer is often required which introduces two separate and additional die attach steps in package assembly processes. Spacers are made from several different types of materials that include silicon and polymer based pre-defined tapes. Electrical connections are provided by bonding electrodes on the dies to wires for connection to the base.
In accordance with embodiments of the invention, a stacked die package includes at least two microelectronic semiconductor dies, one affixed on top of the other. An adhesive wall atop the bottom die outlines an air gap between a bottom and top die. In one embodiment, the adhesive wall is in the shape of a rectangle and forms a perimeter about a hollow area centrally disposed above the die. In other embodiments, the adhesive wall may be C-shaped, V-shaped, H-shaped or X-shaped to name a few configurations. The top die is affixed on the adhesive wall to create the stacked dies. In a specific embodiment, the adhesive wall provides a thickness between the dies in a ratio of at least 1:1 with the width of the wall. The stacked dies are mounted on a base. Wire bonds connect atop surface of each of the dies to the base. The stacked die package can be encased within a non-conductive material molded over the first and second semiconductor dies. The package may further include conductive balls attached to a bottom surface of the base for facilitating electrical connections.
In accordance with a method of manufacturing, a pattern of adhesive pads is deposited on the active surface of a semiconductor wafer. Among the possible adhesive patterns are an array of rings of adhesive or an array of geometrically shaped solid blocks of adhesive. The wafer is thereafter singulated to separate it into individual first semiconductor dies, each die having an adhesive pad thereon. A rear surface of each first semiconductor die can be attached to a base. Wire bonding may be performed between the first semiconductor die and its respective base. A second semiconductor die is attached atop the adhesive pad onto the first semiconductor die to form a stacked die package. Wire bonding may be further performed to electrically attach the second semiconductor die to the base. Overmolding the first and second semiconductor die stacks with non-conductive materials encases the individual packages. In a preferred embodiment, the wafer may be backgrinded before the deposit of a pattern of adhesive. The method may further include partially curing the adhesive before singulating the wafer.
Stress on the die surface of the underlying die typically imparted by the adhesive layer is reduced by using only an adhesive wall leaving an adhesive free air gap region. Application of the adhesive to the active surface of the semiconductor wafer provides for an efficient manufacturing process. Other objects and advantages of the invention will become apparent during the following description of the presently preferred embodiments of the invention taken in conjunction with the drawings.
The foregoing features of the invention will be more readily understood by reference to the following detailed description, taken with reference to the accompanying drawings, in which:
In order to make a stacked die package in a mass production method, a starting material may be a semiconductor wafer as is well known in the art. The typical semiconductor wafer is made from silicon. An array of microelectronic circuits is formed on the semiconductor wafer. Typically, the array of circuits is formed in rows and columns of individual microelectronic circuits. The semiconductor wafer includes an active surface onto which wire connections can be made and a rear surface for mounting. When thickness is an issue, a backgrinding process may be performed on the wafer bearing the circuits to make it and, thus, the resulting dies thinner.
In accordance with an aspect of the present invention as seen in
The adhesive pads may be applied to the wafer in any of a number of methods. Such methods include screen printing or photolithography. The adhesive material may be selected from any of a number of adhesives suitable for use in making microelectronic components. Such adhesives may include, for example, polyimide or BCB (benzocyclobutene). The thickness of the adhesive to be used as a spacer depends upon the geometrical features of the silicon die for a given packaging application. For a stacked die in which the smaller die is placed on top, a smaller thickness spacer is acceptable, for example, in the range of 5 to 20 microns. In an embodiment in which a larger die is placed on top of the smaller die to form a stacked package the thickness of the adhesive may be, for example, between 50 and 75 microns. Such a thick adhesive pad may be more suitable for application through a screen printing method. The method and products of the present invention may be used with any thickness adhesive pad that can be used to produce a useable device.
In accordance with one embodiment as shown in
In accordance with an alternative embodiment such as that shown in
In accordance with a preferred embodiment, each adhesive pad is oriented over a microelectronic circuit but within boundaries set by bond pads 15 for use along the periphery of a die. Thus, the bond pads 15 for the microelectronic circuit are exposed and accessible outside the periphery of the adhesive pad. Once the adhesive pads have been deposited, an intermediate semiconductor product has been completed for further use in the manufacturing of stacked die packaging.
The method of manufacture continues with the step of partially curing 102 the adhesive to bring it to its B-stage. B-stage is an intermediate stage in a thermosetting resin reaction in which the plastic remains in a soft state. The intermediate semiconductor product is then ready for singulation. The singulation process 104 typically involves sawing the wafer into individual dies 20 as shown in
The individual dies may then be picked and placed onto a base 30. A suitable pickup nozzle is used to accommodate the circuit with adhesive pad thereon. A snap cure or low temperature curing adhesive 32 on the base 30 attaches 106 the bottom of the die 20 to the base. The base 30 may be a substrate or lead frame or other suitable base for supporting a stacked die package. The snap cure or low temperature curing adhesive 32 may then be cured without fully curing the adhesive pad 11a, 11b on the die 20. The curing may take place at a lower temperature than will cure the adhesive pad or the curing can take place in a short time span such that the adhesive pad does not cure. Standard die attach materials, such as ABLESTIK 84-1, are cured at temperatures well below full cure for adhesives such as polyimide or BCB. For example, a die attach material might be cured at temperatures between 125° C. and 150° C. for approximately one hour. The BCB or polyimide used for the adhesive pad may, on the other hand, cure at over 300° C. for more than 30 minutes to an hour.
After attaching the bottom die to the base, the adhesive attaching the die to the base is cured without curing the adhesive pad 108. Thus, the adhesive pad may remain in its B-stage during this low temperature or quick curing. At this point, wire bonding 110 can be performed to connect bond pads on the bottom die to the base, as shown in
A top die 50 is then ready for attachment 112 above the bottom die 20. The top die 50 is placed on the adhesive pad 11a, 11b as shown in
In accordance with embodiments of the invention, an air gap 80 remains disposed between the bottom die and the top die when a wall of adhesive was used to form the adhesive pad. In particular, when a ring of adhesive 11a is formed the air gap 80 is centrally disposed. This relieves that central area of stress associated with an adhesive connection.
Of course, it should be understood that various changes and modifications to the preferred embodiments described above will be apparent to those skilled in the art. For example, a stacked die package in accordance with the invention can be made with a smaller or larger top die with respect to the bottom die. Moreover, the base of the package may be a semiconductor substrate or a lead frame depending upon the desired package. Furthermore, additional layers of dies may be included so that multiple dies are stacked using the described methods. These and other changes can be made without departing from the spirit and scope of the invention and without diminishing its attendant advantages. It is therefore intended that such changes and modifications be covered by the following claims.
The present application is a divisional application of U.S. patent application Ser. No. 11/874,083, filed Oct. 17, 2007, now issued as U.S. Pat. No. ______, the full disclosure of which is hereby incorporated by reference herein.
Number | Date | Country | |
---|---|---|---|
Parent | 11874083 | Oct 2007 | US |
Child | 12896186 | US |