The disclosure of Japanese Patent Application No. 2008-92633 filed on Mar. 31, 2008 including the specification, drawings and abstract is incorporated herein by reference in its entirety.
The present invention relates to a semiconductor device and a manufacturing technology thereof. In particular, the invention pertains to a technology effective when applied to the manufacture of a semiconductor device having a conductive film formed, after a probe test step is performed by bringing a probe needle into contact with a pad, on the pad by plating.
In a probe test step (test step) of a semiconductor device equipped with a semiconductor circuit (for example, LSI), electrical properties are measured by bringing a probe needle (probe) into contact with the surface of a pad formed over a semiconductor wafer. Since this probe needle is made of a hard metal such as W (tungsten) and has a sharp top, it inevitably gives an external damage, as a probe mark, to the surface of a pad made of, for example, Al (aluminum) during the probe test step.
Japanese Patent Laid-Open No. 2007-318014 (Patent Document 1) discloses a technology of carrying out inspection by bringing a probe needle into contact with one of two regions of a pad and forming a bump electrode in the other region having no probe mark.
Manufacturing steps of a semiconductor device include a probe test step using the probe needle 4 in order to test the properties of a semiconductor circuit formed over the main surface (element formation surface) of the semiconductor wafer 1W. This probe test step is carried out while bringing the probe needle 4 into contact with a plurality of the pads 2 (
In recent years, with a reduction in the size of semiconductor devices, the pitch of pads (pad pitch) of a semiconductor chip tends to be narrow. It is therefore necessary to reduce the size of each pad in order to increase the pin count and thereby fabricate a multifunctional device. When such a pad is subjected to probe test, the probe mark seems to large relative to the pad.
For example, when a wire (which will hereinafter be called “wire” simply) is coupled onto a pad having such a large probe mark, presence of the probe mark reduces a contact area between the wire and the pad, which may lead to a poor coupling problem. Coupling of a wire to a position where the probe mark is absent as described in Patent Document 1 is considered as a measure to solve the problem.
As another measure against the pitch reduction of a semiconductor device, pitch conversion of a pad using rewiring technology is presumed to be effective. Rewiring technology (which is also called “WPP (Wafer Process Package) technology” or “WLP (Wafer Level Package) technology”) is a technology in which a typical wafer process (a front-end step) and a packaging process (a back-end step) are integrated. In this technology, after completion of packaging in the form of a semiconductor wafer, the wafer is individualized into each semiconductor chips. In short, a semiconductor chip having a widened pitch is manufactured by forming pads with a narrow pitch by utilizing a miniaturization technology of a wafer process and then forming a rewiring layer electrically coupled to the pad.
The present inventors investigated not a semiconductor device in which a wire is coupled to the pads of a semiconductor chip but a semiconductor device capable of converting the pitch of the pads of the semiconductor chip by utilizing the rewiring technology as described above. The inventors have found the following problems of such a semiconductor device.
By the rewiring technology, a seed film 6 which is a conductive film is formed by sputtering over a pad 2 formed in each device formation region and a rewiring layer 7 (interconnect layer) is formed by plating. Then, the pad 2 is led to a desired position (vacant region) over the main surface of the semiconductor wafer (which will be a semiconductor chip later) in order to couple it to the outside of the semiconductor chip. This means that the rewiring layer 7 is formed by plating so that even if the probe mark 100 is present on the pad 2, the rewiring layer 7 is formed over the pad 2 to block therewith the probe mark 100. Use of this rewiring technology therefore enables coupling between the rewiring layer 7 and the pad 2 even if the large probe mark 100 is formed over the pad 2.
The present inventors however have found another problem as described below. First, the present inventors found that as illustrated in
This pore 102 is presumed to be formed because the rewiring layer 7 formed by plating seems to block the probe mark 100 therewith, but a plating film (plating layer) grows in the rewiring layer 7 so as to block the upper portion of the probe mark 100 (recess). When a region (including a margin of the region) with which the probe 4 is brought into contact and a region (including a margin of the region) in which the seed film 6 (conductive film) is formed over the pad 2 including the margin are equal, formation of such a pore 102 in a current pathway raises the resistance of the rewiring layer as a interconnect layer and there is a fear of delay in signal transmission.
In addition, breakage of the seed film 6 due to a step difference of the probe mark 102 hampers the subsequent uniform growth of plating. There is therefore a fear of a pore being formed inside of the plating film and this may lead to a decrease in contact area, deterioration in coupling, worsening of surface flatness, deterioration in the coverage with an upper passivation film 8, and short-circuit with an adjacent portion.
An object of the invention is to provide a technology capable of achieving the size reduction of a semiconductor device, particularly, the pitch narrowing of the device.
Another object of the invention is to provide a technology capable of achieving the high pin count of a semiconductor device.
A further object of the invention is to provide a technology capable of achieving improvement in the electrical properties of a semiconductor device operated at a high speed.
A still further object of the invention is to provide a technology capable of achieving improvement in the reliability of a semiconductor device.
The above-described and the other objects and novel features of the invention will be apparent by the description herein and accompanying drawings.
The typical invention of the inventions disclosed herein will next be described briefly.
In one aspect of the invention, there is provided a manufacturing method of a semiconductor device, which includes forming, over a semiconductor wafer, a pad having a probe region and a coupling region, forming a first insulating film from which the probe region and the coupling region are exposed, bringing a probe needle to the pad in the probe region to measure electrical properties, and forming a conductive film covering therewith the first insulating film and the coupling region over the pad.
Advantages available by the typical invention disclosed herein will next be described briefly.
According to the one aspect of the invention, a rewiring layer can be formed using a conductive film free from pores due to a probe mark. This enables to provide a technology capable of achieving the size reduction, particularly pitch narrowing, of a semiconductor device; a technology capable of achieving a high pin count of a semiconductor device; a technology capable of achieving improvement in the reliability of a semiconductor device; and a technology capable of achieving improvement in electrical properties of a semiconductor device operated at a high speed.
Embodiments of the invention will hereinafter be described specifically based on accompanying drawings. In all the drawings for describing the embodiments, members having a like function will be identified by a like reference numeral and repeating description may be omitted. In the drawings for describing the following embodiments, hatching may be applied even to a plan view in order to facilitate understanding of the configuration.
The semiconductor device according to this embodiment is comprised of a semiconductor chip 1C having a BGA (Ball Grid Array) structure. The semiconductor chip 1C has, at the center portion thereof, bump electrodes 9 in the ball form arranged into a matrix. The bump electrodes 9 are each placed as an external electrode of the semiconductor chip 1C so as to protrude from a passivation film 8 which will be a surface protective film. In
A semiconductor circuit (for example, LSI) which is not illustrated in these diagrams is placed over the main surface (element formation surface) of the semiconductor chip 10 having a rectangular shape. The semiconductor circuit is formed by a known technology by the so-called front-end steps (typical wafer process) and it is comprised of, for example, MISFET (Metal Insulator Semiconductor Field Effect Transistor), resistor, capacitor and interconnects for electrically coupling these elements.
The pads 2 which are electrically coupled to interconnects configuring the semiconductor circuit and placed over the semiconductor chip 10 (semiconductor circuit) are arranged at the periphery of the semiconductor chip 10 having a rectangular shape. Each of these pads 2 has, as illustrated by two regions partitioned by a broken line in
A passivation film 3 is laid over the semiconductor chip 10 (semiconductor circuit). This passivation film 3 is made of, for example, a silicon nitride film which is an inorganic insulating film and has an opening portion 11 on the probe region 10A and the coupling region 10B of the pad 2. Over the pad 2 and the passivation film 3, a passivation film 5 is formed. This passivation film 5 is made of, for example, a polyimide film which is an organic insulating film and has an opening portion 12 having a square plane shape over the coupling region 10B of the pad 2.
As described above referring to
The interconnect layers (seed film 6 and rewiring layer 7) which are conductive members are coupled to a flat region on the surface of the pad 2 where no probe mark 100 is formed so that no probe mark (gap) 100 appears on a current pathway. Such a semiconductor device has therefore improved electrical properties. When the probe region 10A exists between the coupling region 10B and the center of the semiconductor chip 1C (below a pathway where interconnect layers (seed film 6 and rewiring layer 7) are placed), a portion of the interconnect layers are pushed up by the convex portion 101 like a hump formed over the probe region 10A as described above and exposed from the passivation film (insulating film) 8 on the uppermost surface which will be formed later. This may presumably deteriorate the reliability of the resulting semiconductor device. Even if the coupling region 10B is placed on the periphery side of the semiconductor chip 1C, there is no fear of the portion of the interconnect layers (seed film 6 and rewiring layer 7) being exposed from the passivation film 8 insofar as the interconnect layers can be led to the peripheral side of the semiconductor chip 1C from the pad 2. Since the plural pads (electrodes) 2 are placed along each side of the semiconductor chip 1C having a square plane, it is difficult to insert the one end of the interconnect layer between the pad 2 and the periphery of the semiconductor chip 1C. As shown in Embodiment 1, by placing the coupling region 10B near the short side of the pad 2 having a rectangular plane located on the center side on the main surface of the semiconductor chip 1C, exposure of a portion of the interconnect layer from the passivation film 8 can be suppressed so that the semiconductor device can have improved reliability.
The passivation film 8 serving as a protective film on the uppermost surface is formed over the rewiring layer 7 and the passivation film 5. The passivation film 8 has an opening portion 13 over a portion of the rewiring layer 7. The rewiring layer 7 has, over a portion thereof, a bump electrode 9 which is in the ball form and protrudes from the opening portion 13.
The semiconductor chip 1C having such a structure can have the bump electrodes 9 with a pitch widened by the pad 2 for realizing pitch narrowing and the rewiring layer 7 electrically coupled thereto. In other words, the semiconductor device in this embodiment can achieve size reduction, particularly pitch narrowing by electrically coupled, via the pad 2 and the rewiring layer 7, the semiconductor circuit and the bump electrode 9 serving as an external electrode.
In this embodiment, two regions are partitioned on the pad. They are the probe region 10A, that is, a region (including the margin thereof) with which the probe 4 is brought into contact and the coupling region 10B, that is, a region (including the margin thereof) in which the seed film 6 (conductive film) is formed on the pad 2 including the margin. Such a configuration makes it possible to avoid loss of the rewiring layer 7 and/or the seed film 6 as described above referring to
In this embodiment, the pad 2 has a rectangular plane with a long side extending from the periphery side to the center side of the semiconductor chip 1C. In the pad 2, the size 2a is set at, for example, 130 μm; the size b is set at, for example, 75 μm; and the pitch 2c is set at 80 μm. By using, as the pad 2, such a pad having a rectangular planar shape, size reduction, particularly, pitch narrowing can be achieved. In this Embodiment, the pads 2 are arranged in a zigzag manner at the periphery of the rectangular semiconductor chip 1C. This enables to achieve narrower pitching. For example, the pitch 2d between the outer pad 2 and the inner pad 2 is set at 40 μm.
Thus, this embodiment is useful for achieving size reduction, particularly narrow pitching of a semiconductor device so that a semiconductor circuit to be disposed on a semiconductor chip 1C can have multiple functions and a high pin count (multiple input/output) necessary for it can be realized.
As well as the method as shown in this embodiment, another method is usable for separating a probe region from a coupling region of conductive members (wire and rewiring layer). However, the more distant these regions are, the more impossible the miniaturization of the semiconductor device. In addition, the polyimide film from which a portion of the pad is exposed is an organic insulating film having a lower hardness than that of a metal so that it is inferior in processing accuracy to a metal material and the opening portion has an inclined side surface when viewed cross-sectionally. When a pad is formed while separating it into two regions, it is necessary to form a larger pad in consideration of the inferior processing accuracy of the polyimide film. Use of such a large pad is not suited for miniaturization of a semiconductor device compared with use of only one rectangular pad as described in this embodiment.
A manufacturing method of the semiconductor device according to this embodiment will next be described referring to some drawings.
A semiconductor wafer 1W as illustrated in
Described specifically, prepared is a semiconductor wafer 1W equipped with a plurality of device formation regions 50 (chip regions) having a semiconductor circuit (semiconductor element), a pad (electrode) 2 electrically coupled to the semiconductor circuit, and a passivation film (insulating film) 3 formed on the pad 2 so as to expose a portion of the pad 2. The pad 2 has a probe region (first region) 10A on the periphery side of the device formation region 50 and a coupling region (second region) 10B which is adjacent to the probe region 10A and is on the center side of the chip region relative to the probe region 10A. This semiconductor wafer 1W is, for example, a single crystal Si substrate having a circular planar shape. Each semiconductor chip 1C having a rectangular planar shape (refer to
Then, a semiconductor circuit is formed over the main surface of the semiconductor wafer 1W in a known manner (S20). The semiconductor circuit is comprised of, for example, various semiconductor elements such as n channel or p channel MISFET (Metal Insulator Semiconductor Field Effect Transistor), resistor, and capacitor and interconnects (multilayer interconnects) for electrically coupling them.
Then, the pad 2 having the probe region (first region) 10A on the periphery side of the device formation region and the coupling region (second region) 10B which is adjacent to the probe region 10A and is on the center side of the device formation region relative to the probe region 10A is formed over the semiconductor wafer 1W while electrically coupling it to an interconnect configuring the semiconductor circuit (S30). The pad 2 is in a rectangular shape having a long side extending from the periphery side to the center side of the device formation region (which will be the semiconductor chip 1C later) as illustrated in
The pad 2 has, for example, aluminum (Al) as a main conductive layer. It may have a structure in which the Al film serving as a main conductive layer is sandwiched between barrier conductive films each comprised of a film stack of a Ti film and a TiN film. Such an interconnection can be formed by successively depositing the lower barrier conductive film, the Al film, and the upper barrier conductive film and then dry etching them with a photoresist film patterned by photolithography as a mask.
Then, a passivation film 3 (first insulating film) is formed over the semiconductor wafer 1W (S40). This passivation film 3 is made of, for example, a film stack of a silicon oxide film and a silicon nitride film which are inorganic insulating films and the film stack can be formed, for example, by plasma CVD (Chemical Vapor Deposition). With a photoresist film (not illustrated) patterned by photolithography as a mask, the passivation film 3 is dry-etched to expose therefrom the probe region 10A and the coupling region 10B of the pad 2. By this exposure, the passivation film 3 has an opening portion 11. Of the opening portion 11, an exposure region of the probe region 10A is, for example, 60 μm (size 11a)×70 μm (size 11c) and an exposure region of the coupling region 10B is, for example, 60 μm (size 11b)×70 μm (size 11c). In addition, an opening portion 14 is formed on the dummy pad 2A as illustrated in
Then, a probe test of the semiconductor circuit is performed (S50). For example, as illustrated in
In this embodiment, the pad 2 has a rectangular planar shape and it has the probe region 10A on the periphery side of the semiconductor chip 1C and the coupling region 10B on the center side of the semiconductor chip 1C. The probe needle 4 is brought into contact with only the probe region 10A. The probe mark 100 is therefore present only on the pad 2 of the probe region 10A.
In this embodiment, dummy pads 2A having a similar size to that of the probe region 10A of the pad 2 and arranged in alignment are formed simultaneously with the formation of the pad 2 (refer to
The probe test includes not only tests at operation guarantee temperatures (for example, from −40 to 125° C.) at normal temperature, high temperature, and low temperature but also tests for each function because semiconductor devices have multiple functions. In a plurality of testing apparatuses (testers), the probe needle 4 is inevitably brought into contact with the same pad 2 a plurality of times. In addition, the probe test also includes a so-called wafer level burn in so that a voltage is applied to a semiconductor circuit by bringing the probe needle 4 into contact with the pad 2 of the probe region 10A for long hours (for example, several hours) under a high-temperature environment (high-temperature baking) at a temperature around the melting point of a solder (200° C. or greater). This may enlarge the probe mark 100. Even in this case, however, it is possible to limit the presence of the probe mark 100 to the pad 2 of the probe region 10A in this Embodiment.
The probe test may be performed after formation of the bump electrode 9, but in this case it is impossible to carry out a test similar to the probe test on the pad 2 because of a change in the surface condition (oxidation) of a solder due to a temperature history or limitation of the high-temperature baking temperature due to the influence of the melting point of the solder.
Then, a passivation film 5 (second insulating film) is formed over the semiconductor wafer 1W (S60). This passivation film 5 is made of, for example, a polyimide film which is an organic insulating film and can be formed, for example, by spin coating. Then, as illustrated in
Then, as illustrated in
Then, as illustrated in
A rewiring layer 7 made of a conductive film (interconnect layer, plating film) is formed over the seed film 6 by electroplating (S80). More specifically, the rewiring layer 7 is formed over the coupling region 10B and the passivation film 5 so as to extend and hug from the coupling region 10B to the center side of the semiconductor chip 1C while electrically coupling to the pad 2. The rewiring layer 7 is made of a Cu film or a Ni/Cu film. Then, the mask 16 made of the resist film is removed by asking. With the rewiring layer 7 as a mask, the seed film 6 is wet etched to leave a portion of the seed film 6 below the rewiring layer 7 and remove the other portion of the seed film 6 below the mask 16.
As illustrated in
Then, an Au film which is not illustrated is formed on the rewiring layer 7 exposed from the opening portion 13 by electroless plating at one end portion of the conductive film (interconnect layer, plating film) on the side opposite to the other end portion of the conductive film coupled to the coupling region (second region) 10B of the pad 2 as illustrated in
Then, the semiconductor wafer 1W is cut along the scribe (dicing) region between the device formation regions (between the chip regions adjacent to each other) and separated into individual semiconductor chips 1C as illustrated in
The pitch and size of the pads at the coupling portion are reduced in order to achieve multifunction (increase in the number of pins) and microfabrication (downsizing of chip). The pad size can be reduced, for example, by controlling the probing accuracy and size of a probe mark.
By the technical innovation, the pad pitch (size) is reduced, but it is difficult to drastically reduce the size of a probe mark judging from the contact property in the probe test step or influence of electrical resistance of probing
As the probing system, a cantilever system as shown in the present embodiment is being replaced by a vertically movable system. Further technical development of a probing system is however necessary judging from the cost and contact property.
As illustrated in
In this embodiment, by partitioning the probing region 10A to be probed from the coupling region 10B where the pad and the rewiring layer 7 are coupled and providing a sufficient space for these regions, limitation to probing properties is relaxed. In addition, with a view to controlling the probing position, dummy pads 2A are arranged in the same line with the probe region 10A of the pad 2. This enables to use the cantilever system probing so that the contact property can be ensured without limiting the probe test system. The performances of products including analog characteristics, requirement for which will be severer in future, can be satisfied fully.
The configuration of the semiconductor device according to this embodiment will be described first referring to some drawings.
A rectangular semiconductor chip 1C configuring the semiconductor device of this embodiment has, on the main surface thereof, a semiconductor circuit (for example, LSI) not illustrated. A pad 2 electrically coupled to an interconnect configuring the semiconductor circuit and placed on the semiconductor chip 1C (semiconductor circuit) is placed at the periphery of the rectangular semiconductor chip 1C and this pad 2 has, thereover, a bump electrode 17. As shown in
This means that it becomes possible to decrease the length of each of a plurality of wires 57 (conductive members) for electrically coupling a plurality of electrodes 56 (bonding leads) formed on the main surface (upper surface) of a substrate 55 (wiring substrate) and a plurality of pads 2 formed over the main surface (surface) of the semiconductor chip 1C mounted on the main surface (upper surface) of the substrate 55. This leads to improvement in the electrical properties of a semiconductor device.
In this Embodiment, the coupling region 10B of the wire 57 is placed on the circumferential side of the semiconductor chip 1C on the surface of the pad 2 relative to the probe region 10A. The position of the coupling region 10B is not limited to the above-described one, but may be disposed on the center side of the semiconductor chip 1C relative to the probe region 10A and one end portion (ball 20) of the wire 57 may be coupled to it via a bump electrode 17. In consideration of the distance to the electrode 56 (bonding lead) formed on the main surface of the substrate 55 (wiring substrate), the coupling region 10B and the bump electrode 17 are preferably placed on the circumferential side because the length of the wire 57 can be decreased.
A passivation film 3 is formed on the semiconductor chip 1C (semiconductor circuit). This passivation film 3 is made of, for example, a silicon nitride film which is an inorganic insulating film and has an opening portion 11 on the pad 2 in the probe region 10A and the coupling region 10B. A passivation film 18 is formed on the pad 2 and the passivation film 3. This passivation film 18 is made of, for example, a polyimide film which is an organic insulating film and it has an opening portion 21 on the pad 2 in the coupling region 10B.
On the pad 2 in the probe region 10A placed on the center side of the semiconductor chip 10 relative to the coupling region 10B, there is a probe mark 100 (external damage) caused by the contact of a probe needle 4 with the pad 2 in the probe test step as described referring to
In this embodiment, the plane shape of the pad 2 is a rectangular shape having a long side extending from the periphery side to the center side of the semiconductor chip 10. For example, the size 2a of the pad 2 is set at 130 μm, and the size 2b is set at 75 μm. The pitch 2c of the pad 2 is set at 80 μm. By using the pad having a rectangular planar shape, size reduction, particularly narrow pitching of a semiconductor device can be achieved. In this embodiment, the pads 2 are arranged in a zigzag manner at the periphery of the rectangular semiconductor chip 1C. This is useful for achieving narrow pitching. For example, the pitch 2d between the outer pad 2 and the inner pad 2 is set at 40 μm.
Electrical coupling of the wire 57, which is a conductive member, to the semiconductor chip 1C in this embodiment will next be described referring to some drawings.
In this Embodiment, the pad 2 has a rectangular shape so as to realize narrow pitching. As illustrated in
In
As illustrated in
In this embodiment, as illustrated in
Next, a manufacturing method of the semiconductor device of this embodiment will be described referring to some drawings.
As illustrated in
Then, a probe test of the semiconductor circuit is performed. For example, as illustrated in
Then, as illustrated in
Then, as illustrated in
Then the mask 23 made of a resist film is removed by asking and with the bump electrode 17 as a mask, the seed film 19 is wet etched to leave a portion of the seed film 19 below the bump electrode 17 but remove the other portion of the seed film 19 below the mask 23 (refer to
The semiconductor wafer 1W is then cut along the scribe region (dicing) between the device formation regions into individual semiconductor chips 1C as illustrated in
As illustrated in
As illustrated in
The semiconductor wafer 1W is then cut along the scribe (dicing) region between the device formation regions into individual semiconductor chips, whereby the semiconductor device according to this embodiment is completed. Various semiconductor devices can be formed, for example, by electrically coupling an external terminal to the pad 26 by wire bonding and then sealing the semiconductor chip with a resin. A contact resistance can be reduced by forming an Au film on the surface of the rewiring layer 7, followed by wire bonding to the Au film.
For example, when the entirety of the rewiring layer 7 is made of an Au film, adhesion of it with a molding resin cannot be ensured at the time of fabrication of a package. In this embodiment, therefore, the semiconductor device can have high reliability by forming the pad 26 made of an Au film only at a position where wire bonding is performed.
In the formation step of the pad 26 including an Au film, a thin film formation technology such as electroless plating, sputtering or metal printing can be employed if a mask made of, for example, a resist is formed for the formation of the pad 26 after removal of the seed film 6.
The Ni film below the Au film forms the pad 26 but it may form the rewiring layer 7. The influence of warpage of a wafer (chip) due to the Ni film having a large film stress can be reduced by configuring the pad 26 from the Ni film than by configuring the rewiring layer 7 therefrom.
The pad 26 comprised of a Cu/Ni/Au film may be formed on the rewiring layer made of a Cu film in consideration of interfacial coupling of Cu/Ni.
As illustrated in
As described referring to
Similarly, in
As illustrated in
Then, a conductive film 29 (plating film) is formed on the seed film 19 by electroplating. More specifically, the conductive film 29 is electrically coupled to a pad 2 via the seed film 19 and it is made of, for example, an Au film. The mask 27 made of the resist film is then removed by asking.
As illustrated in
The planar shape of the bump electrode 17 may be any planar shape insofar as it enables wire bonding from the bump electrode 17. It may be rectangular, polygonal or circular. It is preferably a shape permitting an increase in the contact area (maximum size shape).
As illustrated in
Various semiconductor devices can be fabricated by using the semiconductor device according to this embodiment, electrically coupling an external terminal and the bump electrode 17 by wire bonding. Upon wire bonding, Au—Au bonding can be performed at lower temperature and under a lower load compared with Al—Au bonding so that damage caused by it is lower. In other words, in the present embodiment, wire bonding can be performed at low temperature because the bump electrode 17 made of an Au film is placed on the conductive film 29 made of an Au film. An Al/Au alloy grows and becomes fragile (deteriorates) so that in this embodiment, the formation of an Al/Au alloy is avoided or suppressed by the effect of the seed film or a barrier metal layer made of a plating layer, thereby improving the reliability of wire bonding coupling.
In this embodiment, the conductive film 29 and the bump electrode 17 are stacked by plating. By coating the entire surface of the pad 2 made of Al with the conductive film 29, the pad 2 can have improved resistance to Al corrosion. In addition, the bump electrode 17 is made higher by a height 17a than the passivation film 18 serving as a surface protective film, whereby contact of a ball (stitch portion) for wire bonding with the periphery of, for example, the passivation film 18 can be prevented.
Compared with the configuration as described in Embodiment 1 referring to
In this embodiment, the probe region 10A to be probed is made smaller than the coupling region 10B wherein the pad 2 and the rewiring layer 7 are coupled to each other. For example, when cantilever system probing is employed, a probe needle 4 is brought into contact with the pad while shifting in one direction as described referring to
Thus, by making the area of the probe region 10A to be probed smaller than that of the coupling region 10B wherein the pad 2 and the rewiring layer 7 are coupled, it is possible to achieve size reduction, particularly, narrow pitching of a semiconductor device.
In the case of an area I/O (Input/Output) having a leading space at the periphery, the rewiring layer 7 can be led in both directions. As illustrated in
It is also possible to achieve size reduction, particularly, pitch narrowing by arranging the coupling via the opening portion 12 and the coupling via the opening portion 12A at intervals of two or more terminals and thereby using the coupling via the opening portion 12 for, for example, power (large current), analogue, or low-resistance coupling and the coupling via the opening portion 12A for high-resistance coupling.
The semiconductor device according to this embodiment can be obtained by forming a mask 23 with an opening portion 22 having a planar shape as illustrated in any one of
In the case of a high pin count product, a bump electrode 17 made of an Au film according to the present embodiment is advantageous over a stud bump electrode for wire bonding or flip chip from the viewpoint of securing a coupling area to the outside and relaxing the damage to a low-k layer (interlayer insulating film). When the bump electrode 17 is coupled over the probe mark 100, it is necessary to separate the probe region 10A from the coupling region 10B and completely coupling the bump electrode in the coupling region 10B in order to prevent the problem related to securement of the flatness.
For example when a bump electrode made of a solder is directly formed on a pad 2 made of an Al film, the coupling strength becomes too low to cause deterioration in the reliability of a semiconductor device. As shown in this embodiment, use of a plating film 7 made by plating between the pad 2 made of an Al film and a bump electrode 9 made of a solder enables to ensure the coupling strength and thereby improve the reliability of the semiconductor device.
When the coupling region 10B includes the probe region 10A as illustrated in
As illustrated in
One example of the coupling of the wire 33 in the stacked chips is illustrated in
In
As illustrated in
Thus, a SiP product (semiconductor device) of this embodiment can be completed. Various semiconductor devices can be obtained by mounting the SiP product of this embodiment on a mother substrate. In the method using an interposer, the electrode patterns of a mother substrate may be formed while causing them to correspond to ball electrode patterns of the interposer substrate so that a pitch between electrodes of the mother substrate can be enlarged. As a result, a mother substrate can be formed easily at a low cost.
The invention made by the present inventors was so far described specifically based on some embodiments. It should however be borne in mind that the invention is not limited to or by them. It is needless to say that various modifications or changes are possible without departing from the gist thereof.
For example, in the above embodiments, a cantilever system probe is employed for the probe test step, but it can be replaced by a vertically movable system.
In the above embodiments, the probe test step is followed by coupling of the conductive member to the coupling region. The order is not limited to it. For example, a product which must avoid application of a heat load thereto in the passivation, seed, resist or plating step after a probe test (a product from which ROM write to be performed in the probe step disappears or a product requiring fuse cut (switching of a memory bit, adjustment of variations in resistance)), probing is performed preferably after formation of a bump electrode (Au plating). When the probe test step is performed after formation of a conductive member, Cu may be used as a material of the pad because a probe needle is not brought into contact with the pad.
When the conductive member is coupled to the coupling region prior to the probe test step, there is a fear of the surface of the coupling region being contaminated due to the influence of a heat load during the probe test step. It is therefore recommended to clean the surface of the coupling region.
The present invention is utilized widely in the manufacturing industry of semiconductor devices having a conductive film formed on a pad after a probe test step, which is performed by bringing a probe needle to the pad. The invention can be applied to products with a narrow pitch, for example, mobile products, navigation products, in-vehicle products and analog products having electrical properties capable of satisfying severe requirements.
Number | Date | Country | Kind |
---|---|---|---|
2008-092633 | Mar 2008 | JP | national |
Number | Name | Date | Kind |
---|---|---|---|
5554940 | Hubacher | Sep 1996 | A |
6097082 | Sato | Aug 2000 | A |
6140149 | Wark | Oct 2000 | A |
6166556 | Wang et al. | Dec 2000 | A |
6329670 | Hu | Dec 2001 | B1 |
6380555 | Hembree et al. | Apr 2002 | B1 |
6429532 | Han | Aug 2002 | B1 |
6511901 | Lam et al. | Jan 2003 | B1 |
6812578 | Kim et al. | Nov 2004 | B2 |
6844631 | Yong et al. | Jan 2005 | B2 |
7576431 | Takahashi | Aug 2009 | B2 |
7981788 | Muto et al. | Jul 2011 | B2 |
8395260 | Matsuki et al. | Mar 2013 | B2 |
20020056901 | Ono et al. | May 2002 | A1 |
20020180026 | Liu et al. | Dec 2002 | A1 |
20030089868 | Ito et al. | May 2003 | A1 |
20040061213 | Karnezos | Apr 2004 | A1 |
20050164486 | Lua et al. | Jul 2005 | A1 |
Number | Date | Country |
---|---|---|
61-294838 | Dec 1986 | JP |
11-163055 | Jun 1999 | JP |
2000-164623 | Jun 2000 | JP |
2003-068738 | Mar 2003 | JP |
2003-152014 | May 2003 | JP |
2005-191213 | Jul 2005 | JP |
2005-317685 | Nov 2005 | JP |
2007-19415 | Jan 2007 | JP |
2007-273676 | Oct 2007 | JP |
2007-318014 | Dec 2007 | JP |
Entry |
---|
Office Action issued Jan. 17, 2012, in Japanese Patent Application No. 2008-092633. |
Office Action issued May 14, 2013, in Japanese Patent Application No. 2012-056972. |
Office Action issued Apr. 15, 2014, in Japanese Patent Application No. 2013-130933. |
Office Action issued Feb. 23, 2016, in Japanese Patent Application No. 2014-217034. |
Number | Date | Country | |
---|---|---|---|
20160336244 A1 | Nov 2016 | US |
Number | Date | Country | |
---|---|---|---|
Parent | 14876787 | Oct 2015 | US |
Child | 15219254 | US | |
Parent | 14465975 | Aug 2014 | US |
Child | 14876787 | US | |
Parent | 13802704 | Mar 2013 | US |
Child | 14465975 | US | |
Parent | 13310261 | Dec 2011 | US |
Child | 13802704 | US | |
Parent | 12413971 | Mar 2009 | US |
Child | 13310261 | US |